Anode tank inner arc supporting plate structure for electrolytic copper foil and connecting method
By designing the structure and connection method of the anode slot in the anode slot for electrolytic copper foil, using the elastic anode and irregularly distributed anode fixing device treated with platinum and iridium coatings, the low bonding rate of the anode plate in the prior art is solved and the The problem of liquid leakage risk improves the conductivity and replacement efficiency.
Patent Information
- Application Number
- CN202411145165.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-26
AI Technical Summary
The existing electrolytic copper foil back-pull anode structure has too low bonding rate between the anode plate and the arc plate, resulting in excessive groove pressure, high energy consumption and risk of liquid leakage. The labor intensity of the operator during replacement is high, which improves the Difficult to replace.
Design an arc support plate structure in the anode groove for electrolytic copper foil, including an electrolytic box, support plate, anode fixing device and elastic anode. Through platinum and iridium coatings, irregularly distributed anode fixing device and J-type card are provided. The groove adopts a variety of fixing methods such as bolts, nuts, mortise and tenon or welding to ensure that the anode fixing device is closely fitted with the support plate, improves conductive efficiency and reduces the risk of liquid leakage.
The conductivity efficiency between the anode groove and the anode fixing device is improved, the groove pressure during production is reduced, the risk of liquid leakage is avoided, and the labor intensity of the operator during replacement is reduced, and the replacement efficiency is improved.
Smart Images

Figure CN119020830A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of electrolytic processing, and specifically relates to an arc support plate structure in an anode tank for electrolytic copper foil and a connection method, and also specifically designs a connection method. Background Art
[0002] The anode tank in the copper foil production machine mainly provides a reaction chamber and carries positive charges to form a positive electric field. The fitting rate between the anode plate installed inside the anode tank and the mother plate will directly lead to the electrochemical rate of the entire equipment. When the anode plate and the mother plate can be fully fitted, the tank pressure of the anode tank will be minimized. There are currently two types of anode plates for copper foil: one is an embedded anode plate, and the other is a back-pull anode plate, which is locked by fasteners inside the anode tank by setting a series of threaded blind holes inside the mother plate to achieve conductivity; the other is a back-pull anode plate, which is a corresponding through hole set on the anode tank mother plate, and the anode plate is fixed to the mother plate from the back through a sealing component, a pressing component, and a locking component to ensure fitting and sealing.
[0003] Publication No. "CN216514193U" discloses an electrolytic copper foil back-pull anode structure. The utility model discloses an electrolytic copper foil back-pull anode plate structure, comprising: an anode plate body (6) and an anode slot, a plurality of screw rods (8) are fixedly connected to the back of the anode plate body, the screw rods include a base section and an extension section, the outer diameter of the extension section is smaller than the outer diameter of the base section, a sealing cap (4) is sleeved on the base section, a locking nut (2) is sleeved on the extension section, a sealing nut (1) is provided on the outer sleeve of the locking nut, a sealing gasket (3) is adapted between the sealing cap and the sealing nut, and the anode slot is penetrated on the base section between the sealing cap and the anode plate body. The beneficial effect of the utility model is that there is no processing mark on the front of the anode plate, which plays an important role in the uniformity of the current and the extension of the life of the anode plate, the sealing device has a simple structure and a reasonable design, and can effectively prevent leakage and crystallization; it is easy to assemble and disassemble, can be recycled, and effectively reduces the production cost.
[0004] The above-mentioned electrolytic copper foil back-pull anode structure has problems such as excessive cell pressure and high energy consumption during the foil production process due to the low bonding rate between the anode plate and the arc plate. At the same time, the back-pull anode has the risk of leakage when installed improperly. It also reduces the labor intensity of the operators when replacing the anode plates in the traditional anode cell and improves the replacement efficiency. Therefore, an inner arc support plate structure and connection method for the anode cell of electrolytic copper foil are needed to assist in solving this problem. Summary of the invention
[0005] (1) Technical issues to be solved
[0006] In view of the deficiencies in the prior art, the object of the present invention is to provide an inner arc support plate structure and a connection method for an anode tank for electrolytic copper foil, which can increase the fitting rate of the anode fixing device to improve the conductivity efficiency between the anode tank and the anode fixing device, reduce the tank pressure of the anode tank during production, and avoid the risk of leakage caused by improper installation of the back-pull anode fixing device. At the same time, it also reduces the labor intensity of operators when replacing the anode fixing device in the traditional anode tank, thereby improving the replacement efficiency.
[0007] (2) Technical solution
[0008] In order to solve the above technical problems, the present invention provides such an inner arc support plate structure of an anode tank for electrolytic copper foil, the inner arc support plate structure of an anode tank for electrolytic copper foil comprising:
[0009] An electrolysis box, which is used for mounting the support plate and provides an anode tank for electrolysis in the subsequent electrolysis process to ensure that the subsequent electrolysis can proceed stably;
[0010] A support plate, the support plate is fitted in the anode tank and is used to provide a mounting layer for the anode fixture to be mounted;
[0011] an anode fixing device, the anode fixing device being fixed at the inner edge of the support plate, and the anode fixing device being provided with a slot for installing the elastic anode;
[0012] The elastic anode is used to achieve uniform discharge after the power supply device is turned on, thereby facilitating subsequent electrolysis operations.
[0013] Furthermore, the elastic anode is an elastic component capable of maintaining or restoring its original state, the contact portion of the elastic anode with the support plate is subjected to platinum plating, and the non-contact side of the elastic anode with the support plate is subjected to iridium coating.
[0014] Furthermore, the elastic anode may be one or more of a mesh, a filament or a foam structure.
[0015] Furthermore, a plurality of anode fixing devices are arranged at the inner edge of the support plate, and the plurality of anode fixing devices are irregularly distributed at the inner edge of the support plate. When arranging, it is necessary to ensure that the anode fixing devices are aligned with each other or have equal offset spacing.
[0016] Furthermore, the height of the anode fixing device is less than or equal to the thickness of the elastic anode, and the anode fixing device is an arc-shaped rod structure as a whole.
[0017] Furthermore, the clamping slot is a J-shaped slot structure, and a plurality of the clamping slots are arranged on the anode fixing device, and the plurality of the clamping slots are symmetrically and equidistantly distributed on the anode fixing device.
[0018] Furthermore, the anode fixing device can be installed on the support plate by a variety of fixing methods, including connection and fixing by fixing parts, such as bolt and nut fixing, mutual clamping of mortise and tenon structures, etc., and the fixing method can also be connected and fixed by welding, etc.
[0019] Furthermore, the support plate is a whole plate rolled into a circle, and the support plate has an arc-shaped plate structure.
[0020] A connection method comprises the following steps:
[0021] S1. Take a titanium plate of appropriate size, roll it into a circle, and then assemble it with other parts of the anode tank and in the electrolytic box. After completion, fine boring of the arc support plate is performed to ensure the radius size of the arc plate;
[0022] S2. After the fine boring is completed, the entire arc support plate surface needs to be polished;
[0023] S3, fixing the elastic anode fixing device to the arc support plate accordingly;
[0024] S4. Install the elastic anodes on the arc support plate in sequence, and arrange the elastic anodes according to the corresponding rules to ensure that each anode is completely flat;
[0025] S5. Tighten the elastic anode to the elastic anode fixing device starting from the liquid inlet position and inspect;
[0026] S6. Re-tighten the unfixed parts to ensure that the elastic anode and each anode fixing device can be effectively fastened, and at the same time ensure that the elastic anode and the arc support plate are closely fitted.
[0027] Furthermore, the surface roughness of the S2 needs to be Ra1.6, and the fixing method of the S3 is vertical, oblique, etc. but is not limited to these methods.
[0028] (3) Beneficial effects
[0029] Compared with the prior art, the present invention has the following beneficial effects:
[0030] The present invention arranges the elastic anode into a non-whole plate structure such as a filament, mesh or foam shape, the contact portion of the elastic anode with the support plate is subjected to platinum plating, and the non-contact side of the elastic anode with the support plate is subjected to iridium coating, so that uniform and efficient discharge can be performed after conduction, and at the same time, the anode fixture bonding rate can be increased to improve the conduction efficiency between the anode tank and the anode fixture, and the tank pressure of the anode tank during production can be reduced, and at the same time, the risk of leakage of the back-pull anode fixture when improperly installed can be avoided, and at the same time, the labor intensity of the operator when replacing the anode fixture in the traditional anode tank is reduced, thereby improving the replacement efficiency;
[0031] The present invention distributes the anode fixing device irregularly on the support plate in a vertical, horizontal or oblique distribution manner, including but not limited to these manners, so as to keep the anode fixing device in a fixed position and a fixed state in the anode tank, and facilitate auxiliary pulling and fixing of the elastic anode in the subsequent process.
[0032] The present invention provides a plurality of slots on the anode fixing device, and the slots are symmetrically and equidistantly distributed on the anode fixing device, so that the anode slots can completely and tightly fit the arc support plate and conduct electricity. Each anode fixing device has slots in opposite directions, which are used to firmly fix the elastic anode so that it will not be displaced due to the flow direction of the electrolyte, thereby ensuring the stability of the subsequent overall discharge of the elastic anode. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without paying any creative work.
[0034] Figure 1 It is a partial structural schematic diagram of the present invention;
[0035] Figure 2 A longitudinal cross-sectional view of the support plate and the anode fixing device of the present invention after installation;
[0036] Figure 3 A longitudinal cross-sectional view of another perspective after the corresponding support plate and the anode fixing device of the present invention are installed;
[0037] Figure 4 It is a partial structural schematic diagram of the elastic anode of the present invention after being installed in the anode fixing device;
[0038] Figure 5 It is a structural schematic diagram of the anode fixing device of the present invention;
[0039] Figure 6 This is a front view of the anode fixing device of the present invention after installing the elastic anode;
[0040] Figure 7 It is a method flow chart of the connection method in the present invention.
[0041] The markings in the attached drawings are: 1. elastic anode; 2. anode fixing device; 21. slot; 3. support plate; 4. electrolytic box. DETAILED DESCRIPTION
[0042] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0043] This specific embodiment is an arc support plate structure in an anode tank for electrolytic copper foil, such as Figure 1 As shown, the arc support plate structure in the anode tank for electrolytic copper foil includes an electrolytic box 4, which is used for installing the support plate 3 and providing an anode tank for electrolysis in the subsequent electrolysis process to ensure that the subsequent electrolysis can be carried out stably. The support plate 3 is fitted and installed in the anode tank, which is used to provide a mounting layer for the anode fixing device 2 to be installed. The support plate 3 is a whole plate rolled into a circle, and the support plate 3 is an arc-shaped plate structure. Through the arrangement of the electrolytic box 4, an electrolysis space can be provided during the electrolysis process for subsequent electrolysis reactions.
[0044] The above-mentioned anode fixing device 2 is fixed at the inner edge of the support plate 3. A slot 21 for installing the elastic anode 1 is provided on the anode fixing device 2. Several anode fixing devices 2 are arranged at the inner edge of the support plate 3. Several anode fixing devices 2 are irregularly distributed at the inner edge of the support plate 3. When arranging, it is necessary to ensure that the anode fixing devices 2 are aligned with the anode fixing devices 2 or have equal offset spacing.
[0045] By distributing the anode fixing device 2 irregularly on the support plate 3 in a vertical, horizontal or oblique manner, including but not limited to these manners, the anode fixing device 2 is fixed in a fixed position and state in the anode tank, and it is convenient to assist in pulling and fixing the elastic anode 1 later.
[0046] The above-mentioned slot 21 is in a J-shaped slot structure. A plurality of slots 21 are provided on the anode fixing device 2 , and the plurality of slots 21 are symmetrically and equidistantly distributed on the anode fixing device 2 .
[0047] By providing a plurality of slots 21 on the anode fixture 2, the slots 21 are symmetrically and equidistantly distributed on the anode fixture 2, so that the anode slot can completely and tightly fit the arc support plate 3 and conduct electricity. Each anode fixture 2 has slots 21 in opposite directions, which are used to firmly fix the elastic anode 1 so that it will not be displaced due to the flow direction of the electrolyte, thereby ensuring the stability of the subsequent overall discharge of the elastic anode 1.
[0048] The anode fixing device 2 can be installed on the support plate 3 by a variety of fixing methods, including fixing by connection through fixing parts, such as bolt and nut fixing, mutual clamping of mortise and tenon structures, etc. The fixing method can also be connected and fixed by welding, etc., and the overall installation of different fixing methods can be achieved by a variety of different methods. Different types of installation processing can be implemented on the anode fixing device 2 according to different installation requirements during work, ensuring that the anode fixing device 2 can be stably fixed on the support plate 3.
[0049] The elastic anode 1 may be one or more of a mesh, a filament or a foam structure. The elastic anode 1 is an elastic member capable of maintaining or restoring its original state. The contact portion of the elastic anode 1 with the support plate 3 is subjected to platinum plating, and the non-contact side of the elastic anode 1 and the support plate 3 is subjected to iridium coating. The elastic anode 1 is used to achieve uniform discharge after the power supply device is turned on, thereby facilitating subsequent electrolysis operations.
[0050] By configuring the elastic anode 1 to be a non-whole plate structure such as a filament, mesh or foam shape, the contact portion of the elastic anode 1 and the support plate 3 is platinum-plated, and the non-contact side of the elastic anode 1 and the support plate 3 is iridium-coated, uniform and efficient discharge can be performed after conduction, and at the same time, the fitting rate of the anode fixture 2 can be increased to improve the conduction efficiency between the anode tank and the anode fixture 2, reduce the tank pressure of the anode tank during production, and avoid the risk of leakage caused by improper installation of the back-pull anode fixture 2. At the same time, the labor intensity of the operator when replacing the anode fixture 2 in the traditional anode tank is reduced, thereby improving the replacement efficiency.
[0051] A connection method comprises the following steps:
[0052] S1. Take a titanium plate of suitable size, roll it into a circle, and then assemble it with other parts of the anode tank and in the electrolytic box 4. After completion, fine boring of the arc support plate 3 is performed to ensure the radius size of the arc plate;
[0053] S2. After fine boring is completed, the entire arc support plate 3 needs to be polished and ground. The surface roughness in S2 needs to reach Ra1.6;
[0054] S3, fixing the elastic anode fixing device 2 to the arc support plate 3 accordingly, the fixing method in S3 adopts vertical, oblique and other methods but is not limited to these methods;
[0055] S4, install the elastic anodes 1 on the arc support plate 3 in sequence, and arrange the elastic anodes 1 according to the corresponding rules to ensure that each anode is completely flat;
[0056] S5, tightening the elastic anode 1 to the elastic anode fixing device 2 starting from the liquid inlet position and inspecting;
[0057] S6. Re-tighten the unfixed parts to ensure that the elastic anode 1 and each anode fixing device 2 can be effectively fastened, and at the same time ensure that the elastic anode 1 and the arc support plate 3 are closely fitted.
[0058] All technical features in this embodiment can be freely combined according to actual needs.
[0059] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. An inner arc support plate structure of an anode tank for electrolytic copper foil, the inner arc support plate structure of an anode tank for electrolytic copper foil comprising: An electrolysis box (4), the electrolysis box (4) is used for mounting the support plate (3) and providing an anode tank for electrolysis in the subsequent electrolysis process to ensure that the subsequent electrolysis can be carried out stably; A support plate (3), the support plate (3) being fitted in the anode tank and used to provide a mounting layer for mounting the anode fixture (2); an anode fixing device (2), the anode fixing device (2) being fixed to the inner edge of the support plate (3), and the anode fixing device (2) being provided with a slot (21) for mounting the elastic anode (1); An elastic anode (1) is used to achieve uniform discharge after a power supply device is turned on, thereby facilitating subsequent electrolysis operations.
2. The inner arc support plate structure of an anode tank for electrolytic copper foil according to claim 1, characterized in that: The elastic anode (1) is an elastic component capable of maintaining or restoring its original state. The contact portion of the elastic anode (1) with the support plate (3) is subjected to platinum plating, and the non-contact side of the elastic anode (1) and the support plate (3) is subjected to iridium coating.
3. The inner arc support plate structure of an anode tank for electrolytic copper foil according to claim 2, characterized in that: The elastic anode (1) may be one or more of a mesh, a filament or a foam structure.
4. The inner arc support plate structure of an anode tank for electrolytic copper foil according to claim 1, characterized in that: A plurality of anode fixing devices (2) are arranged at the inner edge of the support plate (3), and the plurality of anode fixing devices (2) are irregularly distributed at the inner edge of the support plate (3). When arranging, it is necessary to ensure that the anode fixing devices (2) are aligned with each other or have equal offset spacing.
5. The inner arc support plate structure of an anode tank for electrolytic copper foil according to claim 4, characterized in that: The height of the anode fixing device (2) is less than or equal to the thickness of the elastic anode (1), and the anode fixing device (2) is an arc-shaped rod structure as a whole.
6. The inner arc support plate structure of the anode tank for electrolytic copper foil according to claim 5, characterized in that: The clamping groove (21) is in a J-shaped groove structure, and a plurality of the clamping grooves (21) are arranged on the anode fixing device (2), and the plurality of the clamping grooves (21) are symmetrically and equidistantly distributed on the anode fixing device (2).
7. The inner arc support plate structure of an anode tank for electrolytic copper foil according to claim 1, characterized in that: The anode fixing device (2) can be installed on the support plate (3) by various fixing methods, including connection and fixing by fixing parts, such as bolt and nut fixing, mutual clamping of mortise and tenon structures, etc., and the fixing method can also be connected and fixed by welding, etc.
8. The inner arc support plate structure of an anode tank for electrolytic copper foil according to claim 1, characterized in that: The support plate (3) is a whole plate rolled into a circle, and the support plate (3) is an arc-shaped plate structure.
9. A connection method, used for the inner arc support plate structure of an anode tank for electrolytic copper foil according to any one of claims 1 to 8, characterized in that: The following steps are involved: S1. Take a titanium plate of suitable size, roll it into a circle, and then assemble it with other parts of the anode tank and in the electrolytic box (4). After completion, fine boring of the arc support plate (3) is performed to ensure the radius size of the arc plate; S2. After the fine boring is completed, the entire arc surface of the arc support plate (3) needs to be polished and ground; S3, fixing the elastic anode (1) fixing device to the arc support plate (3) accordingly; S4, installing the elastic anodes (1) on the arc support plate (3) in sequence, and arranging the elastic anodes (1) according to a corresponding rule to ensure that each anode is completely flat; S5, tightening the elastic anode (1) to the elastic anode fixing device (2) starting from the liquid inlet position and inspecting; S6. Re-tighten the unfixed parts to ensure that the elastic anode (1) and each anode fixing device (2) can be effectively fastened, and at the same time ensure that the elastic anode (1) and the arc support plate 3 are tightly fitted.
10. A connection method according to claim 9, characterized in that: The surface roughness of the S2 needs to reach Ra1.6, and the fixing method of the S3 is vertical, oblique, etc. but is not limited to these methods.
Citation Information
Patent Citations
Electrolytic copper foil back pull type anode plate structure
CN216514193U