Welding seam defect inspection method

By using a combination of a compensator and a radiation source between the bushing and the casing of the voltage regulator electric heater to perform multi-angle double-wall radiography, the problem of internal quality inspection being impossible in the prior art has been solved, and efficient and accurate inspection of fillet welds has been achieved.

CN119023714APending Publication Date: 2024-11-26CHINA NUCLEAR POWER DESIGN COMPANY +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411277448.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-12
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Existing testing technologies cannot perform internal quality inspections on the fillet welds between the bushing and the casing of the voltage regulator electric heater; they can only perform surface quality inspections, which cannot meet the stringent weld quality requirements.

Method used

A compensator is fitted around the outer periphery of the casing, flush with the outer periphery of the electric heater sleeve. Double-wall irradiation is performed by adjusting the X-ray source to a first preset angle with the sleeve axis. Multi-angle detection is performed by combining multiple rotations. Multiple double-wall irradiations are performed using a combination of Ir192 X-ray source and compensator.

Benefits of technology

It effectively eliminates the influence of thickness differences, improves the accuracy of weld internal quality inspection and defect detection rate, avoids interference from false defects, and ensures the reliability of weld internal quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119023714A_ABST
    Figure CN119023714A_ABST
Patent Text Reader

Abstract

The invention provides a weld defect inspection method, and relates to the technical field of weld defect inspection. The weld defect inspection method comprises the steps that a compensation body is provided, the compensation body is arranged outside the cladding in a sleeving mode, and the periphery of the compensation body is flush with the periphery of the electric heater sleeve; a ray source is adjusted to form a first preset angle alpha with the axis of the sleeve, and double-wall transillumination is conducted on the fillet weld; after a combined body of the sleeve and the compensation body or the ray source is rotated by a second preset angle beta in the circumferential direction of the sleeve, double-wall transillumination is conducted on the fillet weld; and after the combined body of the sleeve and the compensation body or the ray source is continuously rotated by a third preset angle delta in the circumferential direction of the sleeve, double-wall transillumination is conducted on the fillet weld. The compensation body is provided, and the periphery of the compensation body is flush with the periphery of the electric heater sleeve, so that the influence of large thickness difference between the electric heater sleeve and a cladding can be eliminated during radiographic inspection, and the internal quality of a welding seam can be conveniently detected.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of weld defect volume inspection, and in particular to a weld defect inspection method. Background Art

[0002] The pressurizer is one of the key equipment in a pressurized water reactor nuclear power plant. It regulates and controls the pressure and volume of the primary circuit main system and plays a very important role in ensuring the integrity of the pressure boundary of the primary circuit main system. The main function of the pressurizer electric heater is to heat the reactor coolant in the pressurizer under rated conditions and variable load operation of the nuclear power plant to maintain it at a saturated temperature that meets the operating pressure, thereby controlling and regulating the pressure fluctuation of the reactor coolant system.

[0003] The assembly structure of the electric heater, sleeve and lower head of the pressurizer is as follows: A vertically arranged electric heater is installed at the lower head of the pressurizer, wherein the electric heater is composed of a cladding and a heating wire, and the heating wire is placed inside the cladding of the electric heater. When the electric heater is working, the heating wire is energized to generate heat to heat the water in the pressurizer. In order to protect the service life of the electric heater, an electric heater sleeve is designed on the outside of the electric heater in the structural design. The electric heater sleeve is inserted into the lower head of the pressurizer and connected to the inner wall cladding layer of the lower head of the pressurizer by welding, and the electric heater cladding and the electric heater sleeve are connected by a fillet weld structure. The fillet weld between the electric heater cladding and the electric heater sleeve is different from the general plug-in weld. It is a special-shaped weld. The bevel is machined on the inner side of the sleeve for welding. The electric heater cladding and the electric heater sleeve are both austenitic stainless steel. During the service of a nuclear power plant, when an electric heater is damaged, the weld can be cut and replaced with a new electric heater.

[0004] The fillet weld between the electric heater cladding and the electric heater sleeve of the pressurizer is an important nuclear primary pressure-bearing weld in the primary pressure boundary, and needs to bear the sealing function, and has strict requirements on the quality of the weld. In the manufacturing process of the fillet weld between the electric heater cladding and the electric heater sleeve of the pressurizer, it is currently limited by the special structure of the fillet weld, such as the small size of the sleeve and cladding, the special-shaped structure of the weld, and the large thickness difference on both sides of the weld. The existing inspection technology and process can only use the penetration inspection method to inspect the surface quality of the fillet weld between the electric heater cladding and the electric heater sleeve, and cannot perform volume inspection (such as UT or RT inspection) on the internal quality of the fillet weld, and lacks effective inspection means for the internal quality of the weld. Summary of the invention

[0005] In view of the above shortcomings of the prior art, the present invention provides a method for inspecting weld defects to improve the technical problem that only the penetration inspection method can be used to inspect the surface quality of the weld between the stabilizer electric heater sleeve and the cladding, and there is a lack of effective inspection means for the internal quality of the weld.

[0006] To achieve the above-mentioned purpose and other related purposes, the present invention provides a method for inspecting weld defects, which is used for inspecting internal defects of the corner weld between the sleeve of a voltage regulator electric heater and the cladding, comprising: providing a compensating body, sleeved the compensating body outside the cladding, and the outer periphery of the compensating body is flush with the outer periphery of the electric heater sleeve; adjusting the radiation source to form a first preset angle α with the axis of the sleeve, and performing double-wall radiography on the corner weld; rotating the combination of the sleeve and the compensating body or the radiation source along the circumference of the sleeve by a second preset angle β, and performing double-wall radiography on the corner weld; continuing to rotate the combination of the sleeve and the compensating body or the radiation source along the circumference of the sleeve by a third preset angle δ, and performing double-wall radiography on the corner weld.

[0007] In an exemplary embodiment of the present application, the first preset angle α is 70° to 80°.

[0008] In an exemplary embodiment of the present application, factors affecting the first preset angle α include an outer diameter D of the cladding and a length L of the fillet weld along the axial direction of the cladding.

[0009] In an exemplary embodiment of the present application, the outer diameter D of the cladding multiplied by tanα is greater than or equal to the length L of the weld along the axial direction of the cladding.

[0010] In an exemplary embodiment of the present application, the second preset angle β is in the same direction as the third preset angle δ, and the sum of the second preset angle β and the third preset angle δ is 90°.

[0011] In an exemplary embodiment of the present application, the second preset angle β is equal to the third preset angle δ.

[0012] In an exemplary embodiment of the present application, the compensating body includes two rotatably connected semi-annular tubes, which are buckled together to form a hollow tube, and an avoidance portion is provided on the inner wall of one end of the hollow tube, and the avoidance portion is in contact with the fillet weld.

[0013] In an exemplary embodiment of the present application, a locking portion is provided on the semi-annular tube, and after the two semi-annular tubes are buckled together, the relative rotation of the semi-annular tubes is limited by the locking portion.

[0014] In an exemplary embodiment of the present application, the ray source is an Ir192 ray source, a focal spot size φ of the ray source is less than or equal to 3 mm, and a focal length f is 250 mm to 350 mm.

[0015] In an exemplary embodiment of the present application, the compensating body and the electric heater sleeve are made of the same material.

[0016] In combination with the prior art, the beneficial effects of the present invention are:

[0017] The existing weld inspection process can only perform surface inspection on the weld between the electric heater cladding and the electric heater sleeve, but cannot complete deep inspection, resulting in the inability to monitor the quality of the weld. The present application provides a compensating body, which is sleeved outside the cladding, and the outer circumference of the compensating body is flush with the outer circumference of the electric heater sleeve. When performing radiographic inspection, the influence of the large thickness difference between the electric heater sleeve and the cladding can be eliminated, thereby facilitating the internal quality inspection of the weld.

[0018] By aligning the ray source with the axis of the sleeve at a first preset angle α, the fillet weld is double-walled for transillumination, thereby reducing the effect of the inherent gap between the compensating body and the heater sleeve on the film causing pseudo defects and reducing interference with the flat top of the film defect.

[0019] By performing radiographic inspection on the weld at three different positions through the initial position, rotating the combination of the sleeve and the compensating body or the radiation source along the circumference of the sleeve by a second preset angle β, and rotating the combination of the sleeve and the compensating body or the radiation source along the circumference of the sleeve by a third preset angle δ, the defect detection rate at any circumferential position can be improved, and the risk of missed defect detection can be effectively avoided. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0021] Figure 1 A schematic diagram of an exemplary voltage regulator electric heater of the present application;

[0022] Figure 2 This is a schematic diagram of an exemplary welding point between an electric heater sleeve and a cladding of the present application;

[0023] Figure 3 This is a schematic diagram of an exemplary electric heater sleeve groove of the present application;

[0024] Figure 4 This is a schematic diagram of an exemplary weld inspection method of the present application;

[0025] Figure 5 This is a schematic diagram of an exemplary radiographic inspection transillumination of the present application;

[0026] Figure 6 This is a schematic cross-sectional view of an exemplary X-ray inspection of a fillet weld in the present application.

[0027] Component number description:

[0028] 100. Electric heater sleeve; 200. Cladding; 300. Electric heater; 400. X-ray source; 500. Fillet weld; 600. Compensating body. DETAILED DESCRIPTION

[0029] The following is an explanation of the embodiments of the present invention by specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the features in the following embodiments and the embodiments can be combined with each other without conflict. It should also be understood that the terms used in the embodiments of the present invention are intended to describe specific embodiments, rather than to limit the scope of protection of the present invention. The test methods for which specific conditions are not specified in the following examples are usually carried out under conventional conditions or according to the conditions recommended by the manufacturers.

[0030] When numerical ranges are given in the embodiments, it should be understood that, unless otherwise specified in the present invention, both endpoints of each numerical range and any value between the two endpoints can be selected. Unless otherwise defined, all technical and scientific terms used in the present invention are familiar to those skilled in the art and the description of the present invention, and any methods, equipment and materials of the prior art similar or equivalent to the methods, equipment and materials described in the embodiments of the present invention can also be used to implement the present invention.

[0031] It should be noted that the terms such as "upper", "lower", "left", "right", "middle" and "one" etc. used in this specification are only for the convenience of description and are not intended to limit the scope of implementation of the present invention. Changes or adjustments to their relative relationships, without substantially changing the technical content, should also be regarded as the scope of implementation of the present invention.

[0032] The pressurizer is one of the key equipment in a pressurized water reactor nuclear power plant. It regulates and controls the pressure and volume of the primary circuit main system and plays a very important role in ensuring the integrity of the pressure boundary of the primary circuit main system. The main function of the pressurizer electric heater is to heat the reactor coolant in the pressurizer under rated conditions and variable load operation of the nuclear power plant to maintain it at a saturated temperature that meets the operating pressure, thereby controlling and regulating the pressure fluctuation of the reactor coolant system.

[0033] The assembly structure of the voltage stabilizer electric heater 300, the casing and the lower head is as follows: Figures 1 to 3As shown, a vertically arranged electric heater 300 is installed at the lower end of the pressurizer, wherein the electric heater is composed of a cladding 200 and a heating wire, etc., and the heating wire is placed inside the electric heater cladding 200. When the electric heater 300 is working, the heating wire is powered on to generate heat, thereby heating the water in the pressurizer. In order to protect the service life of the electric heater 300, in terms of structural design, an electric heater sleeve 100 is designed outside the electric heater 300, and the electric heater sleeve 100 is inserted into the lower end of the pressurizer and connected to the inner wall cladding layer of the lower end of the pressurizer by welding, and the electric heater cladding 200 and the electric heater sleeve 100 are connected by a fillet weld 500 welding structure. The fillet weld 500 between the electric heater cladding 200 and the electric heater sleeve 100 is different from the general plug-in weld, and is a special-shaped weld. The groove is machined on the inner side of the sleeve for welding. The outer diameter of the electric heater cladding 200 at the connection of the fillet weld 500 is 22.1mm and the wall thickness is 3.2mm. The inner and outer diameters of the electric heater sleeve 100 are 22.9mm and 45mm respectively, and both are austenitic stainless steel. During the service of the nuclear power plant, when an electric heater 300 is damaged, the weld can be cut and replaced with a new electric heater 300.

[0034] The fillet weld 500 between the pressurizer electric heater cladding 200 and the electric heater sleeve 100 is an important nuclear primary pressure-bearing weld in the primary pressure boundary, and needs to assume a sealing function, which places strict requirements on the weld quality. In the manufacturing process of the fillet weld 500 between the pressurizer electric heater cladding 200 and the electric heater sleeve 100, it is currently limited by the special structure of the fillet weld 500, such as the small size of the sleeve and the cladding 200, the special-shaped structure of the weld, and the large thickness difference on both sides of the weld. As a result, the existing inspection technology and process can only use the penetration inspection method to perform surface quality inspection on the fillet weld 500 between the electric heater cladding 200 and the electric heater sleeve 100, and cannot perform volume inspection on the internal quality of the fillet weld 500.

[0035] In view of this, the present invention provides a method for inspecting weld defects, which is used for volume inspection of internal defects of the corner weld 500 between the stabilizer electric heater sleeve 100 and the cladding 200, so as to improve the control of the internal quality of the corner weld 500, increase the defect detection rate, accurately judge the nature of the defects, and ensure the quality of the product weld.

[0036] See also Figure 4 , Figure 4 The flow chart of a weld defect inspection method is shown, and the specific steps are as follows:

[0037] Step S110 , providing a compensating body 600 , and sleeve the compensating body 600 outside the cladding shell 200 , so that the outer periphery of the compensating body 600 is flush with the outer periphery of the electric heater sleeve 100 .

[0038] By arranging a compensating body 600 outside the cladding 200, the outer periphery of the compensating body 600 is flush with the outer periphery of the electric heater sleeve 100, so that the fillet weld 500 can be inspected for suspected volume, and the internal defects of the fillet weld 500 can be effectively inspected, avoiding the problem of being unable to perform X-ray volume inspection due to the large height difference between the cladding 200 and the electric heater sleeve 100.

[0039] In one embodiment, the compensating body 600 is a tubular structure that can be sleeved and closely or substantially closely attached to the cladding 200. The compensating body 600 includes two semi-annular tubes, which are buckled together to form a chamber that is closely attached to the outer periphery of the cladding 200. The two semi-annular tubes can be two independent parts, which are then directly buckled together to form a tubular structure; the two semi-annular tubes can also be rotatably connected, and after one of the semi-annular tubes is close to the cladding 200, the other semi-annular tube is rotated so that the other semi-annular tube is also close to the cladding 200. Preferably, the two semi-annular tubes are rotatably connected to facilitate the placement and storage of the compensating body 600. The two semi-annular tubes can be rotatably connected by means including but not limited to hinges.

[0040] In one embodiment, a locking portion is provided on the semi-annular tube, and after the two semi-annular tubes are buckled, the locking portion limits the relative rotation of the semi-annular tubes, thereby facilitating the X-ray volume inspection. In another embodiment of the present application, the two semi-annular tubes are two unconnected parts, and after the two semi-annular tubes are buckled, the locking portion limits the relative movement of the two semi-annular tubes, thereby ensuring the X-ray volume inspection of the fillet weld 500.

[0041] In one embodiment, the semi-annular tubes are buckled together to form a hollow tube, and an avoidance portion is provided on the inner wall of one end of the hollow tube, which is fitted with the fillet weld 500, thereby preventing interference between the compensation body 600 and the fillet weld 500, affecting the detection of the fillet weld 500, and improving the detection quality of the fillet weld 500.

[0042] In one embodiment, the compensating body 600 is made of the same material as the electric heater sleeve 100 to prevent the different materials from affecting the X-ray detection and improve the accuracy of the defect detection result.

[0043] Step S120 , adjusting the radiation source 400 to form a first preset angle α with the axis of the sleeve, and performing double-wall radiography on the fillet weld 500 .

[0044] See also Figure 5 and Figure 6 By adjusting the ray source 400 so that the ray source 400 and the axis of the sleeve are at a first preset angle α, the influence of the inherent gap between the compensating body 600 and the electric heater sleeve 100 on the detection of the fillet weld 500 can be effectively reduced, thereby improving the accuracy of defect detection of the fillet weld 500.

[0045] Furthermore, in order to improve the accuracy of the weld inspection results, the fillet weld 500 is inspected by double-wall transillumination. In order to obtain better results, a first preset angle α is obtained comprehensively based on factors including the outer diameter D of the cladding 200, the axial length L of the weld along the cladding 200, etc., to ensure the accuracy of the inspection results.

[0046] Furthermore, the outer diameter D of the cladding 200 multiplied by tanα is greater than or equal to the length L of the weld along the axial direction of the cladding 200, so that when the double wall is transilluminated, the fillet welds 500 arranged on both sides of the electric heater cladding 200 do not overlap or the overlapping area is reduced, so that the defect position can be obtained more accurately, thereby improving the accuracy of defect detection.

[0047] Furthermore, the first preset angle α is 70° to 80°, which not only avoids the overlap of the fillet welds 500 on both sides of the electric heater shell 200, but also effectively reduces the influence of the gap between the fillet welds 500 and the compensation body 600 on the detection result.

[0048] Double-wall transillumination can improve the detection efficiency of the fillet weld 500. In one embodiment, the ray source 400 is an Ir192 ray source 400, the focus size φ is less than or equal to 3 mm, and the focal length f is 250 mm to 350 mm, thereby effectively ensuring the volume detection of the fillet weld 500.

[0049] Step S130 , rotating the combination of the sleeve 100 and the compensating body 600 or the radiation source 400 along the circumference of the sleeve 100 by a second preset angle β, and performing double-wall radiography on the fillet weld 500 .

[0050] By rotating the radiation source 400 along the circumference of the sleeve 100, or rotating the combination of the sleeve 100 and the compensating body 600, the rotation angle is a second preset angle β, and the corner weld 500 is double-walled for the second time to obtain the second radiation irradiation result, thereby improving the accuracy of the detection and reducing the error of the radiation detection. Preferably, the combination of the sleeve 100 and the compensating body 600 is more convenient to rotate than the radiation source 400, which is conducive to the multi-angle irradiation detection.

[0051] Step S140 , continue to rotate the combination of the sleeve 100 and the compensating body 600 or the radiation source along the circumference of the sleeve 100 by a third preset angle δ to perform double-wall radiography on the fillet weld 500 .

[0052] By rotating the radiation source 400 along the circumference of the sleeve, or rotating the combination of the sleeve 100 and the compensating body 600, the rotation angle is the third preset angle δ, and the corner weld 500 is double-walled for the third time to obtain the third radiation irradiation result. Through detection at different angles, the accuracy of detection is improved and the error of radiation detection is reduced. The three radiation irradiation results are obtained by three double-walled transilluminations, and the angles of the first irradiation and the third irradiation are perpendicular, so that the three radiation irradiation results can completely cover the corner weld 500, avoid the radiation irradiation blind area of ​​the corner weld 500, and improve the accuracy of the internal defect detection of the corner weld 500. The three irradiation results are compared to obtain the internal defect inspection result of the corner weld 500, which effectively solves the problem that the existing corner weld 500 inspection can only inspect the surface and cannot inspect the internal quality of the corner weld 500.

[0053] Furthermore, the second preset angle β and the third preset angle δ are in the same direction. For example, when the combination of the sleeve 100 and the compensating body 600 is rotated for the first time, the second preset angle β is rotated clockwise around the circumference of the sleeve 100. When the combination of the sleeve 100 and the compensating body 600 is rotated for the second time, the third preset angle δ is continued to be rotated clockwise around the circumference of the sleeve 100.

[0054] Furthermore, the sum of the second preset angle β and the third preset angle δ is 90°, that is, the angle between the third penetration and the first penetration is 90°, avoiding the blind area of ​​the corner weld 500 radiation penetration, ensuring the accuracy of radiation detection, and improving the accuracy of defect positioning and defect structure judgment.

[0055] Furthermore, the second preset angle β is equal to the third preset angle δ, that is, the second preset angle β and the third preset angle δ are both 45°, so as to better perform radiographic detection on different angles of the corner weld 500 and improve the detection accuracy.

[0056] In order to reduce the impact of excessive differences in blackness in the film assessment area on defect assessment, the method of double-film transillumination, double-film assessment + local area single-film observation assistance is adopted to effectively ensure accurate detection of each area of ​​the fillet weld 500, which is convenient for monitoring the quality of the fillet weld 500. In other words, each double-wall transillumination uses two films with different sensitivities and contrast characteristics for transillumination, and the quality of the fillet weld 500 is assessed by superimposing and observing the two films. Single-film auxiliary observation is performed for local areas, such as single-film observation for areas with larger blackness, which effectively ensures the accuracy of the quality assessment of the fillet weld 500.

[0057] The present invention provides a method for inspecting weld defects. By providing a compensating body 600, the problem of large thickness difference between the cladding 200 and the casing and inability to perform volume detection is avoided. The avoidance portion of the compensating body 600 is fitted with the fillet weld 500, which solves the influence of weld irregularity on radiographic detection. The ray source 400 forms a first preset angle α with the axis of the cladding 200, which facilitates double-wall transillumination of the fillet weld 500. Through multiple transilluminations, each area of ​​the weld is effectively inspected, and at the same time, it is convenient to locate weld defects and determine the weld structure. Therefore, the present invention effectively overcomes some practical problems in the prior art and has high utilization value and use significance. The above embodiments are only illustrative of the principles and effects of the present invention, and are not used to limit the present invention. Any person familiar with this technology can modify or change the above embodiments without violating the spirit and scope of the present invention. Therefore, all equivalent modifications or changes made by those with ordinary knowledge in the relevant technical field without departing from the spirit and technical ideas disclosed by the present invention should still be covered by the claims of the present invention.

Claims

1. A method for inspecting weld defects, used for inspecting internal defects of fillet welds between a voltage stabilizer electric heater sleeve and a cladding, characterized in that: include: Providing a compensating body, and sleeved the compensating body outside the cladding, so that the outer periphery of the compensating body is flush with the outer periphery of the electric heater sleeve; Adjusting the radiation source to form a first preset angle α with the axis of the sleeve to perform double-wall radiography on the fillet weld; After rotating the combination of the sleeve and the compensating body or the radiation source along the circumference of the sleeve by a second preset angle β, double-wall radiography is performed on the fillet weld; After the combination of the sleeve and the compensating body or the radiation source is continuously rotated by a third preset angle δ along the circumference of the sleeve, double-wall radiography is performed on the fillet weld.

2. The method for inspecting weld defects according to claim 1, characterized in that: The first preset angle α is 70° to 80°.

3. The method for inspecting weld defects according to claim 1, characterized in that: Factors affecting the first preset angle α include the outer diameter D of the cladding and the length L of the fillet weld along the axial direction of the cladding.

4. The method for inspecting weld defects according to claim 3, characterized in that: The outer diameter D of the cladding multiplied by tanα is greater than or equal to the length L of the fillet weld along the axial direction of the cladding.

5. The method for inspecting weld defects according to claim 1, characterized in that: The second preset angle β is in the same direction as the third preset angle δ, and the sum of the second preset angle β and the third preset angle δ is 90°.

6. The method for inspecting weld defects according to claim 5, characterized in that: The second preset angle β is equal to the third preset angle δ.

7. The method for inspecting weld defects according to claim 1, characterized in that: The compensating body comprises two rotatably connected semi-annular tubes, wherein the semi-annular tubes are buckled together to form a hollow tube, and an escape portion is arranged on the inner wall of one end of the hollow tube, and the escape portion is fitted with the fillet weld.

8. The method for inspecting weld defects according to claim 7, characterized in that: The semi-annular tubes are provided with locking parts, and after the two semi-annular tubes are buckled together, the relative rotation of the semi-annular tubes is restricted by the locking parts.

9. The method for inspecting weld defects according to claim 1, characterized in that: The ray source is an Ir192 ray source, the focal point size φ of the ray source is less than or equal to 3 mm, and the focal length f is 250 mm to 350 mm.

10. The method for inspecting weld defects according to claim 1, characterized in that: The compensating body is made of the same material as the electric heater sleeve.