Photoetching method and photoresist mask
By forming channels on the photoresist layer and dividing them into independent units, the problem of cracking caused by excessive stress on large-sized wafer photoresist is solved, and the preparation quality of circuit components and the performance of integrated circuits are improved.
Patent Information
- Application Number
- CN202310618854.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-25
- Publication Date
- 2024-11-26
AI Technical Summary
When lithography is performed on large-sized wafers, large-area photoresist coated on the photoresist is prone to cracking due to excessive stress, which affects the preparation of circuit components and the performance of integrated circuits.
By forming a channel on the photoresist layer, it is divided into multiple independent and separate photoresist units, stress is released and the risk of cracking is reduced.
It effectively reduces the risk of cracking caused by stress accumulation during large-area coating of photoresist, and improves the preparation quality of circuit components and the performance of integrated circuits.
Smart Images

Figure CN119024645A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of integrated circuit technology, especially the field of photolithography technology, and in particular, the present application relates to a photolithography method and a photoresist mask. Background Art
[0002] The photolithography process in integrated circuit technology mainly includes the steps of coating - pre-baking - exposure - development - hardening - etching - stripping. It mainly uses the photosensitive anti-corrosion coating to undergo photochemical reaction, combined with the corrosion method to prepare the required patterns on various thin films or silicon, and uses the pattern for etching or material deposition, so as to achieve the purpose of making various circuit components, selective doping, forming metal electrodes and wiring, etc.
[0003] However, in some process scenarios, it is inevitable to perform photolithography on large-size wafers (for example, to create bumps on wafers, such as indium pillars for flip-chip interconnections), and photoresist coated over a large area is very prone to cracking due to excessive stress, which affects the preparation of circuit components and, in turn, the performance of integrated circuits. Invention content
[0004] The purpose of the present application is to provide a photolithography method and a photoresist mask, which divide the photoresist layer into multiple independent and separated photoresist units to release stress, thereby reducing the risk of cracking caused by stress accumulation when the photoresist is coated on a large area.
[0005] An embodiment of the present application provides a photolithography method, comprising: forming a photoresist layer to cover the surface of a wafer; forming channels in the photoresist layer to divide the photoresist layer into a plurality of independent and separate photoresist units; and forming a photolithography pattern in the photoresist unit, and using the photolithography pattern to form an element with a corresponding pattern on the wafer.
[0006] In the photolithography method as described above, in some embodiments, the step of forming channels in the photoresist layer to divide the photoresist layer into a plurality of independent and separate photoresist units includes: determining an area on the wafer for forming a chip; and patterning the photoresist according to the area to form a photoresist unit on each of the areas, and each of the photoresist units is independent and separate from each other.
[0007] In some embodiments of the photolithography method as described above, before the step of forming a photoresist layer to cover the surface of the wafer, the method further includes: forming a stopper on the surface of the wafer.
[0008] In the above-mentioned photolithography method, in some embodiments, there are a plurality of the blocking blocks, and the plurality of the blocking blocks are distributed at the boundaries of the region.
[0009] In the above-mentioned photolithography method, in some embodiments, the photoresist layer includes at least two layers of photoresist.
[0010] As described above in the photolithography method, in some embodiments, the sensitivity of the photoresist in each layer is different.
[0011] Another embodiment of the present application provides a photoresist mask, comprising: a plurality of independent and separated photoresist units formed on a surface of a wafer, wherein the photoresist units have photolithographic patterns for forming corresponding elements on the wafer.
[0012] In the photoresist mask as described above, in some embodiments, the photoresist unit includes at least two layers of photoresist.
[0013] In the photoresist mask described above, in some embodiments, the sensitivity of the photoresist at each layer is different.
[0014] In some embodiments of the photoresist mask as described above, a stopper is formed on the wafer, and a plurality of the stoppers are distributed at the boundaries of the region.
[0015] Compared with the prior art, the present application first forms a photoresist layer to cover the surface of the wafer, then forms channels in the photoresist layer to divide the photoresist layer into a plurality of independent and separate photoresist units, finally forms a photoresist pattern in the photoresist unit, and uses the photoresist pattern to form an element with a corresponding pattern on the wafer. The present application divides the photoresist layer into a plurality of independent and separate photoresist units to release stress, thereby reducing the risk of cracking caused by stress accumulation when the photoresist is coated on a large area. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A schematic diagram of a photolithography method provided for one embodiment of the present application;
[0017] Figure 2 A schematic diagram of a photoresist layer covering a wafer surface provided in accordance with an embodiment of the present application;
[0018] Figure 3 A schematic diagram of a photoresist unit forming a photolithography pattern according to an embodiment of the present application.
[0019] In the figure:
[0020] 1. Wafer; 10. Chip; 2. Photoresist layer; 20. Photoresist unit; 21. Channel area photoresist; 22. Redundant area photoresist; 201. Photolithography pattern. DETAILED DESCRIPTION
[0021] To make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the embodiments of the present application will be described in detail below in conjunction with the accompanying drawings. However, it will be appreciated by those skilled in the art that in the present application, many technical details are proposed in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can also be implemented. The division of the following embodiments is for the convenience of description, and the specific implementation of the present application should not be construed as any limitation, and the various embodiments can be combined and referenced with each other under the premise of no contradiction.
[0022] It should be noted that the terms "including" and "having" and any variations thereof in the specification and claims of the present application and the above-mentioned drawings are intended to cover non-exclusive inclusions. For example, a process, method, system, product or apparatus comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or apparatuses.
[0023] In addition, it should be understood that when a layer (or film), region, pattern or structure is referred to as being "on" a substrate, layer (or film), region and / or pattern, it can be directly on another layer or substrate, and / or there can also be intervening layers. In addition, it should be understood that when a layer is referred to as being "under" another layer, it can be directly under another layer, and / or there can also be one or more intervening layers. In addition, references to being "on" and "under" each layer can be made based on the accompanying drawings.
[0024] In addition, it should be understood that when a layer (or film), region, pattern or structure is referred to as being "on" a substrate, layer (or film), region and / or pattern, it can be directly on another layer or substrate, and / or there can also be intervening layers. In addition, it should be understood that when a layer is referred to as being "under" another layer, it can be directly under another layer, and / or there can also be one or more intervening layers. In addition, references to being "on" and "under" each layer can be made based on the accompanying drawings.
[0025] In the existing semiconductor process, a wafer is generally divided into several chip areas arranged at intervals. The manufacture of semiconductor devices requires hundreds of processes, and the photolithography process, as the main process step of patterning, plays a pivotal role in the manufacturing process of semiconductor devices.
[0026] The photolithography process forms a photoresist on the surface of the wafer, exposes and develops the photoresist to form a mask pattern, and then performs subsequent processing on the surface of the wafer according to the mask pattern. The subsequent processing may be to image the pattern on the wafer substrate through an etching step, or to complete the optional doping of the pattern area of the wafer substrate through an ion implantation step. The various patterns of the photoresist layer determine many features of the final semiconductor device, such as through holes, necessary interconnects between layers, and silicon doped areas. Among them, etching is the technology of transferring the mask pattern to the silicon wafer, which is used to etch away the surface material of the silicon wafer that is not protected by the photoresist. Specifically, a dry etching process or a wet etching process may be used, and the etching pattern includes grooves and / or etching holes.
[0027] Based on the above description, the photolithography process is to dissolve some areas on the photoresist through steps such as exposure, development, fixing, and hardening to form a mask with a layout pattern for subsequent steps. With the expansion of the scale of components, it is inevitable to implement photolithography for large-size wafers, and the photoresist coated on a large area is very easy to crack due to excessive stress, which affects the preparation of circuit components and further affects the performance of integrated circuits.
[0028] To address this, the present application proposes a photolithography method and a photoresist mask, which divide the photoresist layer into multiple independent and separate photoresist units to release stress, thereby reducing the risk of cracking caused by stress accumulation when the photoresist is coated over a large area.
[0029] Figure 1 A schematic flow chart of a photolithography method provided for one embodiment of the present application.
[0030] Figure 2 A schematic diagram of a photoresist layer covering a wafer surface provided in accordance with an embodiment of the present application.
[0031] Figure 3 A schematic diagram of a photoresist unit forming a photolithography pattern according to an embodiment of the present application.
[0032] Figures 1 to 3 , schematically shows a process of coating a photoresist layer 2 on the surface of a wafer 1, using the photoresist layer 2 to form a photoresist unit 20 with a layout pattern as a mask, and then preparing a circuit element (such as an air bridge) based on the photoresist unit 20.
[0033] Combination Figures 1 to 3 As shown, a photolithography method provided in an embodiment of the present application includes steps S100 to S300:
[0034] Step S100, forming a photoresist layer 2 to cover the surface of the wafer 1, wherein the wafer 1 can be a semiconductor substrate, such as silicon, sapphire, etc., and this embodiment uses a silicon wafer. After the surface of the wafer 1 is coated with glue, it can also be baked and cooled to shape, for example, baked at 160-200°C for 2-10 minutes and then cooled to shape. For example, it can be baked at 180°C for 3 minutes and then cooled to room temperature.
[0035] Step S200 , forming a channel in the photoresist layer 2 to divide the photoresist layer 2 into a plurality of photoresist units 20 that are independent and separated from each other, and separating the photoresist units through the channel.
[0036] Step S300, forming a photolithography pattern 201 in the photoresist unit 20, and using the photolithography pattern 201 to form a component with a corresponding pattern on the wafer 1. The component can be obtained by subsequent processing the surface of the wafer 1 according to the photolithography pattern 201, specifically, the pattern can be imaged on the wafer 1 through an etching step, or the pattern area of the wafer 1 can be selectively doped by an ion implantation step.
[0037] Among them, the photoresist involved in this embodiment can be selected from positive photoresist or negative photoresist. The photoresist is formed on the surface of the wafer 1 by a spin coating process. The process of the spin coating process includes dripping glue on the surface of the wafer 1, slow glue leveling and fast glue leveling. In the process of fast glue leveling, under the action of centrifugal force, the photoresist diffuses to the edge of the wafer 1. The components with corresponding patterns include grooves and / or etched holes, etc., and the depths of the grooves and etched holes are different, which is caused by the different etching times of the grooves and the etched holes. When the etching depth of a single etching is the same, the more etching times, the greater the etching depth for the wafer 1.
[0038] Based on the above description of the embodiment of the present application, it can be understood that compared with the related art, the present application forms a photoresist layer 2 to cover the surface of the wafer 1, then forms a channel in the photoresist layer 2 to divide the photoresist layer 2 into a plurality of photoresist units 20 that are independent and separated from each other, and finally forms a photoresist pattern 201 in the photoresist unit 20, and uses the photoresist pattern 201 to form a component with a corresponding pattern on the wafer 1. The present application divides the photoresist layer 2 into a plurality of photoresist units 20 that are independent and separated from each other to release stress, thereby reducing the risk of cracking caused by stress accumulation when the photoresist is coated over a large area. It should be noted that coating a thick photoresist over a large area is particularly prone to stress accumulation. In addition, the difference in thermal expansion coefficients between the wafer and the photoresist is also one of the factors that cause stress accumulation.
[0039] Before forming the photoresist layer 2 to cover the surface of the wafer 1, the wafer surface can be purged with nitrogen to remove particles on the surface of the wafer 1, such as foreign particles, contamination, natural oxide layer, etc., so as not to affect the adhesion of the photoresist; then the wafer 1 is pre-baked to dry the surface of the wafer 1 so as to increase the adhesion between the photoresist layer 2 and the surface of the wafer 1. Specifically, the moisture on the surface of the wafer 1 can be pre-baked and dried at 150°C to 200°C and then cooled; photoresist is coated on the wafer 1. In this embodiment, the photoresist can be 20000P. The photoresist can be coated by static coating. For example, this embodiment adopts a spin coating method. Specifically, after the wafer 1 is rotated at a first speed of 850r / min, 20000P of photoresist is dripped into the rotation center of the wafer 1, and then Then, the wafer 1 is rotated at a uniform speed of 3500r / min until the photoresist 20000P is spread to the edge of the wafer 1, wherein the first speed can also be 880r / min, 900r / min, 950r / min, 1000r / min, as long as it is between 850 and 1000r / min, and the second speed can also be 3900r / min, 4200r / min, 4500r / min, as long as the second speed is between 3500 and 4500r / min; it should be noted that, compared with the static coating method, the aforementioned rotary coating method is not easy to accumulate photoresist and is easier to spread evenly. After shaping, a photoresist layer 2 with relatively uniform thickness is formed, thereby avoiding the accumulation of glue in local areas when coating the photoresist and causing stress accumulation.
[0040] The method of dividing the photoresist layer 2 is not limited to one method in the specific implementation, as long as the photoresist layer 2 can be divided as a whole to form a plurality of photoresist units 20 that are independent of each other and separated from each other. In the embodiment of the present application, the channel is used as the dividing line between the photoresist units, and the communication can be formed by the exposure-development method in the specific implementation. In some embodiments, the step of forming a channel in the photoresist layer 2 to divide the photoresist layer 2 into a plurality of photoresist units 20 that are independent of each other and separated from each other includes: determining the area on the wafer 1 for forming the chip 10; and according to the area for forming the chip 10, patterning the photoresist to form a photoresist unit 20 on each of the areas, and each of the photoresist units 20 is independent of each other and separated from each other. After the development operation, the hardening film can be performed first and then the metal material can be deposited. The hardening film is to bake the photoresist dissolved by the development so that the photoresist is firmly adhered to the surface of the chip 10. Each photoresist unit 20 corresponds to a region covered on the chip 10 , and the region between adjacent chips 10 is exposed through the channel. This not only fully utilizes the region between the chips 10 to form a stress buffer structure, but also fully protects the surface of the chip 10 by utilizing the photoresist unit 20 .
[0041] In this step, a developer is used to dissolve and remove a portion of the photoresist layer 2, and the trench described above is formed between adjacent chip 10 regions. In this embodiment, the developer can also be placed in an ice-water mixture during the development operation so that the development operation is performed in a constant low-temperature environment. In specific implementation, the developer can also be placed in liquid nitrogen so that the ambient temperature of the developer drops to a lower level, such as -20°C. The lower temperature environment reduces the sensitivity of the photoresist to the developer. The development and dissolution process is easy to operate and control to reduce the deviation of the trench morphology, which helps to improve the reliability and repeatability of the trench shape and maintain the stability and controllability of the development and dissolution process. Specifically, development at a low temperature helps to control the formed graphic morphology by controlling the development time. In this step, a developer is used to dissolve and remove a portion of the photoresist (i.e., the trench region photoresist 21), and trenches are formed between the regions where the adjacent chips 10 are located as the boundary of the adjacent photoresist units 20, and part of the wafer 1 is exposed through the formed trench. It should be noted that, in addition to the area used as the chip 10 and the area between the chips 10 (for example, as the space for dicing), there is also a redundant area on the wafer 1, which is also covered with photoresist, as shown by the redundant area photoresist 22 in the figure.
[0042] In some embodiments, before the step of forming the photoresist layer 2 to cover the surface of the wafer 1, it also includes: forming a stopper on the surface of the wafer 1. In one embodiment, there are multiple stoppers, and the multiple stoppers are distributed at the boundary of the region. The tensile stress of the photoresist can be reduced by the enclosure of the stoppers, which helps to reduce the risk of photoresist tearing. In specific implementation, the stoppers located between the chips 10 can be exposed through the channels formed on the photoresist layer 2.
[0043] In some embodiments, the photoresist layer 2 includes at least two layers. It should be noted that after the first photoresist is first coated on the surface of the wafer 1, due to the high solvent content, the overall thickness of the glue layer is relatively thick, and the first photoresist has poor adhesion to the surface of the wafer 1 during spin coating, and it is easy to cause the two layers of glue to penetrate and fuse when the second photoresist is coated, which affects the graphic morphology formed after exposure and development. To this end, in one embodiment, the solvent in the first photoresist can be evaporated by baking, so that the thickness of the coated first photoresist is reduced by 10% to 20%, and the film stress formed by rotation can be relatively reduced to enhance the adhesion of the first photoresist, and the first photoresist is not only thin and uniform but also can avoid mutual dissolution with the second photoresist. In this embodiment, the thickness of the first photoresist finally formed is controlled to be between 180nm and 200nm.
[0044] Exemplarily, a method for forming another layer of photoresist (second photoresist) on a previously formed photoresist (first photoresist), that is, a method for constructing a second photoresist on the first photoresist, may include: coating the second photoresist on the first photoresist. Specifically, in this embodiment, after the wafer is uniformly rotated at a third speed, the second photoresist is dripped into the rotation center of the first photoresist, and then the wafer 1 is uniformly rotated at a fourth speed until the second photoresist spreads to the edge of the first photoresist. It should be noted that the third speed and the fourth speed can be determined according to the properties of the photoresist such as the viscosity and the requirements for uniform coating; then, the second photoresist layer is obtained by baking and cooling.
[0045] It should be noted that, according to the different exposure wavelengths, photoresists can be divided into ultraviolet (300-450nm) photoresists, deep ultraviolet (160-280nm) photoresists, extreme ultraviolet (EUV, 13.5nm) photoresists, electron beam photoresists, ion beam photoresists, X-ray photoresists and other types. In order to achieve the effect of exposing two layers of photoresists at one time, in this application, the first photoresist and the second photoresist must be the same type of photoresist, and the sensitivity of the photoresists located in each layer is different. Exemplarily, the sensitivity of the second photoresist is lower than that of the first photoresist, that is, the sensitivity of the second photoresist layer is lower than that of the first photoresist layer, so as to ensure that the exposed area on the first photoresist layer is larger than the exposed area on the second photoresist layer. It is understandable that when selecting different types of photoresists, the exposure wavelength and the developer used for dissolution also need to be adjusted accordingly.
[0046] In this embodiment, the first photoresist and the second photoresist can be electron beam photoresists. In specific implementation, the first photoresist and the second photoresist can also be ultraviolet photoresists, deep ultraviolet photoresists, extreme ultraviolet photoresists, or the above photoresists in combination with other glues that are easily developed and dissolved. Compared with ultraviolet photoresists, deep ultraviolet photoresists, and extreme ultraviolet photoresists, electron beam photoresists have short exposure wavelengths and high resolutions.
[0047] As described above, sensitivity refers to the minimum light energy (for UV photoresist) or minimum charge (for electron beam photoresist) incident on a unit area that causes the entire photoresist to react. The smaller the value, the higher the sensitivity, the smaller the dose required for exposure, and the faster the exposure process.
[0048] In one embodiment of the present application, after the second photoresist and the first photoresist are exposed, the second photoresist and the first photoresist are immediately baked at 100°C for 1 to 2 minutes to fix the first photoresist and the second photoresist, that is, the polymer compounds at the photosensitive and non-photosensitive boundaries of the first photoresist and the second photoresist are redistributed by baking. It should be noted that the baking temperature and baking time vary depending on the type and thickness of the photoresist, and generally baking at 80 to 120°C for 1 to 3 minutes is sufficient.
[0049] An embodiment of the present application also provides a photoresist mask, which can be used to form a component with a corresponding pattern on a wafer 1. The component can be obtained by subsequent processing of the surface of the wafer 1 according to the photoresist pattern 201 possessed by the photoresist unit 20 serving as a mask. Specifically, the pattern can be imaged on the wafer 1 through an etching step, or the selective doping of the pattern area of the wafer 1 can be completed through an ion implantation step.
[0050] Combination Figures 1 to 3 As shown, a photoresist mask provided in an embodiment of the present application includes: a plurality of independent and separated photoresist units 20 formed on the surface of a wafer 1, and the photoresist units 20 have a photolithography pattern 201 for forming corresponding elements on the wafer 1.
[0051] In one embodiment, the photoresist layer 2 includes at least two layers. Exemplarily, the sensitivity of the photoresist in each layer is different. In another embodiment, in order to avoid cracking of the flip-chip photoresist due to excessive stress, a stopper is formed on the wafer 1, and a plurality of the stoppers are distributed at the boundaries of the region.
[0052] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
[0053] The above describes in detail the structure, features and effects of the present application based on the embodiments shown in the drawings. The above is only a preferred embodiment of the present application, but the present application does not limit the scope of implementation to what is shown in the drawings. Any changes made in accordance with the concept of the present application, or modifications to equivalent embodiments with equivalent changes, which still do not exceed the spirit covered by the description and drawings, should be within the protection scope of the present application.
Claims
1. A photolithography method, characterized in that: include: forming a photoresist layer to cover the surface of the wafer; forming channels in the photoresist layer to divide the photoresist layer into a plurality of photoresist units that are independent and separated from each other; as well as, A photolithography pattern is formed in the photoresist unit, and a component having a corresponding pattern is formed on the wafer using the photolithography pattern.
2. The photolithography method according to claim 1, characterized in that: The step of forming a channel in the photoresist layer to divide the photoresist layer into a plurality of photoresist units that are independent and separated from each other comprises: determining the area on the wafer for forming the chips; The photoresist is patterned according to the regions to form photoresist units on each of the regions, and each of the photoresist units is independent and separated from each other.
3. The photolithography method according to claim 2, characterized in that: Before the step of forming a photoresist layer to cover the surface of the wafer, the method further includes: A stopper is formed on the surface of the wafer.
4. The photolithography method according to claim 3, characterized in that: There are a plurality of stoppers, and the plurality of stoppers are distributed at the boundaries of the area.
5. The photolithography method according to claim 1, characterized in that: The photoresist layer includes at least two layers.
6. The photolithography method according to claim 5, characterized in that: The sensitivity of the photoresist in each layer is different.
7. A photoresist mask, characterized in that: include: A plurality of independent and separated photoresist units are formed on the surface of a wafer, and the photoresist units have photolithographic patterns for forming corresponding elements on the wafer.
8. The photoresist mask according to claim 7, characterized in that: The photoresist unit includes at least two layers.
9. The photoresist mask according to claim 8, characterized in that: The sensitivity of the photoresist in each layer is different.
10. The photoresist mask according to claim 7, characterized in that: A stopper is formed on the wafer, and a plurality of the stoppers are distributed at the boundary of the region.
Citation Information
Patent Citations
Photolithography method, etching method and semiconductor structure
CN109062011A
Photolithography mask
CN210721012U
Mask pattern generation method
JP2003309054A
Mask, semiconductor device, and manufacturing method therefor
JP2003338457A
Stencil mask, and stencil mask blanks
JP2006073869A
Cited By
Mask pattern generation method, mask, semiconductor structure and manufacturing method thereof
CN121742116A