Method and related device for qualitatively representing durability of 2D NAND FLASH memory
By introducing a trap mechanism in the simulation model, the reduction of write charge efficiency is simulated, and the linear relationship between the program threshold voltage change amount and the trap charge amount is obtained, solving the problem of difficult to quickly and accurately characterize the durability of 2D NAND FLASH memory in the prior art. , realizes efficient and accurate durability characterization and process impact analysis.
Patent Information
- Application Number
- CN202411138250.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-26
AI Technical Summary
The prior art is difficult to quickly and accurately characterize the durability of 2D NAND FLASH memory. The traditional methods consume time, consume high resources, and are costly, and it is difficult to explore the impact of different processes on durability.
By introducing a trap mechanism in the simulation model, the reduction of write charge efficiency is simulated, the linear relationship between the program threshold voltage change and the trap charge amount is obtained, and the durability of the 2D NAND FLASH memory is qualitatively characterized, and the device is predicted by using the program threshold voltage change amount. Service life.
It realizes the durability of 2D NAND FLASH memory fast, accurate and resource-saving characterization, reduces the actual characterization time, improves the efficiency and accuracy of characterization, and can more conveniently explore the impact of different processes on durability.
Smart Images

Figure CN119028403A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of FLASH memory durability evaluation, and relates to a method for qualitatively characterizing the durability of a 2D NAND FLASH memory and a related device. Background Art
[0002] In the current information and digital age, the integrated circuit industry plays an irreplaceable role in promoting economic and social development. The market share of the semiconductor memory industry accounts for about one-third of the overall semiconductor market, and storage technology is becoming an indispensable part of supporting the operation of modern society.
[0003] Semiconductor memory can be mainly divided into two categories: volatile and non-volatile. Volatile memory cannot maintain data storage after the power is turned off. Common examples include dynamic random access memory (DRAM) and static random access memory (SRAM). Non-volatile memory (NVM) or non-volatile storage is a type of computer memory that retains stored information even after power is turned off. Examples of non-volatile memory include flash memory, read-only memory, ferroelectric random access memory, etc. DRAM and NAND FLASH are the two types of memory that dominate the market.
[0004] The core advantage of 2D NAND FLASH technology lies in its continuously improving integration density, which significantly increases the storage capacity of each chip. The increase in 2D NAND flash storage capacity is often achieved at the cost of increased process and system complexity. This is mainly due to the need to not only reduce the technical feature size, but also to deal with a series of increasingly deteriorating physical problems that may damage the reliability of the array and thus have an adverse effect on performance. For example, the storage density of 2D NAND FLASH is getting larger and larger, and the corresponding core device size is getting smaller and smaller. The reduction in device size means that the device's voltage resistance also becomes worse. When 2D NAND FLASH develops to advanced process nodes (Sub-28nm), how to improve the reliability of advanced process products (such as erase and write times, high-temperature data retention, etc.) becomes particularly important.
[0005] In practical applications, 2D NAND FLASH faces severe challenges in terms of durability. The most prominent problem is the limitation of the number of erase and write cycles. Each 2D NAND FLASH storage cell has a certain erase and write threshold. Once this threshold is exceeded, the storage cell may fail. This performance degradation phenomenon caused by frequent erase and write operations is called "erase fatigue". The device has a good durability when it reaches 100,000 erase and write times. The cause of erase fatigue is that during the programming process, electron injection will damage the tunnel layer; at the same time, the anode hot hole injection will damage the barrier layer, and the traps generated by the hot hole injection of the substrate during the erase process will also damage the barrier or tunnel layer. The formation of these interface traps is the main reason for the decrease in the durability of 2D NAND FLASH. They will capture electrons in shallow traps, resulting in a decrease in charge, thereby increasing the risk of read errors. Therefore, how to improve and quickly and accurately characterize the durability of 2D NAND flash memory is an important research direction.
[0006] The traditional method of characterizing the durability of 2D NAND FLASH memory is to detect the change of threshold voltage under tens of thousands of erase and write cycles, use computers to simulate hundreds of thousands of erase and write cycles, and detect the threshold voltage under each erase and write number to obtain a curve chart of the relationship between threshold voltage and erase and write number. This method is inefficient and time-consuming, consumes a lot of computing resources, is costly, and the characterization relationship is nonlinear. When exploring the impact of different processes on durability, it is difficult to quickly and conveniently characterize durability. Summary of the invention
[0007] The object of the present invention is to provide a method and related device for qualitatively characterizing the endurance of a 2D NAND FLASH memory, so as to solve the technical problem that it is difficult to quickly and accurately characterize the endurance of a 2D NAND FLASH memory in the prior art.
[0008] In order to achieve the above object, the present invention adopts the following technical solutions:
[0009] In a first aspect, the present invention provides a method for qualitatively characterizing the endurance of a 2D NAND FLASH memory, comprising the following steps:
[0010] Obtain relevant configuration parameters of the 2D NAND FLASH memory to be tested;
[0011] Input relevant configuration parameters of the 2D NAND FLASH memory to be tested into the simulation model, and introduce a trap mechanism into the simulation model;
[0012] According to the simulation model, the programming threshold voltage change ΔV during several erase and write cycles is obtained tp and the trapped charge Q oxThe linear relationship between 2D NAND FLASH and 2D NAND FLASH is used to qualitatively characterize the endurance of 2D NAND FLASH memory.
[0013] Furthermore, in the step of obtaining relevant configuration parameters of the 2D NAND FLASH memory to be tested, the relevant configuration parameters include: physical parameters of the initial substrate Si, tunnel oxide SiO2, polysilicon floating gate, barrier layer, polysilicon control gate, source and drain.
[0014] Furthermore, the relevant configuration parameters of the 2D NAND FLASH memory to be tested are input into the simulation model. In the step of introducing a trap mechanism into the simulation model, the simulation process of the simulation model is completed through the SILVACO TCAD platform, and the reduction of the write charge efficiency is simulated by introducing traps along the SiO2 / Si interface.
[0015] Furthermore, the programming threshold voltage change ΔV is obtained according to the simulation model. tp and the trapped charge Q ox The steps to qualitatively characterize the endurance of 2D NAND FLASH memory include:
[0016] As the amount of trapped charge introduced increases, the programming threshold voltage changes by ΔV tp The programming threshold voltage change ΔV is also gradually increased according to the simulation results of the simulation model. tp and the trapped charge Q ox The relationship curve diagram of the programming threshold voltage change ΔV is plotted by converting the horizontal and vertical coordinates in the curve diagram into logarithmic coordinates. tp and the trapped charge Q ox Take the log and get a value about the change in programming threshold voltage ΔV tp and the trapped charge Q ox The linear relationship of is as follows:
[0017] lg(ΔV tp )=Alg(Q ox )+B
[0018] Where ΔV tp is the programming threshold voltage change; Q ox is the trapped charge; A is the slope of the fitting curve; B is the intercept of the fitting curve.
[0019] Furthermore, the method further comprises: according to the obtained programming threshold voltage change ΔV tp and the trapped charge Q ox The linear relationship between the programming threshold voltage and the set trap concentration is introduced to predict the change in programming threshold voltage ΔV tp .
[0020] Furthermore, the method further comprises: when the programming threshold voltage change amount ΔV tp When the preset failure standard is reached, it means that the device fails. According to the obtained programming threshold voltage change ΔV tp and the trapped charge Q ox The linear relationship between the introduced trap concentration and the erase and write cycles is obtained, thereby qualitatively characterizing the durability and calculating the service life of the device.
[0021] In a second aspect, the present invention provides a system for qualitatively characterizing the endurance of a 2D NAND FLASH memory, comprising:
[0022] A parameter acquisition module is used to obtain relevant configuration parameters of the 2D NAND FLASH memory to be tested;
[0023] A trap introduction module is used to input relevant configuration parameters of the 2D NAND FLASH memory to be tested into the simulation model, and introduce a trap mechanism into the simulation model;
[0024] A simulation module is used to obtain the programming threshold voltage change ΔV according to the simulation model tp and the trapped charge Q ox The linear relationship between 2D NAND FLASH and 2D NAND FLASH is used to qualitatively characterize the endurance of 2D NAND FLASH memory.
[0025] In a third aspect, the present invention provides a computer device, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of the above method when executing the computer program.
[0026] In a fourth aspect, the present invention provides a computer-readable storage medium, wherein the computer-readable storage medium stores a computer program, and when the computer program is executed by a processor, the steps of the above method are implemented.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] The present invention discloses a method and related device for qualitatively characterizing the durability of 2D NAND FLASH memory. In the process of simulating the durability degradation of 2D NAND FLASH memory, by introducing a trap mechanism, the increase of drain current after durability degradation and the subsequent decrease of write charge efficiency (programming efficiency) are reproduced in the model. The relevant configuration parameters of the 2D NAND FLASH memory are input into the simulation model to obtain the programming threshold voltage change ΔV tp and the trapped charge Q oxThe linear relationship is used to qualitatively characterize the durability of 2D NAND FLASH memory. The present invention will introduce traps for electrical simulation of programming and erasing steps. When simulating the durability of the device, the reduction in write charge efficiency (programming efficiency) will be simulated by introducing traps along the SiO2 / Si interface. These traps can capture electrons that should have been injected into the floating gate, resulting in a reduction in the number of electrons actually injected into the floating gate, thereby reproducing the phenomenon that the write charge efficiency (programming efficiency) of the actual flash memory device is reduced after the durability is degraded. The introduction of traps greatly reduces the time spent in actually characterizing the durability, and has the advantages of high efficiency, accuracy, speed, and resource conservation. In addition, the present invention converts the programming threshold voltage change ΔV tp As the main parameter for simulating endurance, the relationship between the change in programming threshold voltage and the change in trap charge is used to qualitatively characterize the endurance of 2D NAND flash, which is more accurate. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0030] Figure 1 is a flow chart of the method of the present invention;
[0031] Figure 2 is a schematic diagram of the system of the present invention;
[0032] Figure 3 A method for qualitatively characterizing the durability of 2D NAND flash memory under different tunnel oxide (SiO2) preparation processes according to an embodiment of the present invention;
[0033] Figure 4 The programming and erasing threshold voltages of the device with a tunnel oxide (SiO2) thickness of 7.0 nm according to the embodiment of the present invention vary with the amount of trapped charge;
[0034] Figure 5 The variation of the programming threshold voltage variation with the amount of trapped charge in the embodiment of the present invention;
[0035] Figure 6 The comparison results of the durability of tunnel oxide (SiO2) grown by direct deposition, wet oxygen, and dry oxygen in the embodiment of the present invention;
[0036] Figure 7 It is a schematic diagram of the computer device structure of the present invention. DETAILED DESCRIPTION
[0037] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0038] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0039] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0040] In the description of the embodiments of the present invention, it should be noted that if the terms "upper", "lower", "horizontal", "inner", etc. indicate an orientation or positional relationship based on the orientation or positional relationship shown in the drawings, or the orientation or positional relationship in which the product of the invention is usually placed when in use, it is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, the terms "first", "second", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.
[0041] In addition, if the term "horizontal" appears, it does not mean that the component must be absolutely horizontal, but can be slightly tilted. For example, "horizontal" only means that its direction is more horizontal than "vertical", which does not mean that the structure must be completely horizontal, but can be slightly tilted.
[0042] In the description of the embodiments of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal connection of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0043] The present invention is further described in detail below in conjunction with the accompanying drawings:
[0044] See also Figure 1 The embodiment of the present invention discloses a method for qualitatively characterizing the endurance of a 2D NAND FLASH memory, comprising the following steps:
[0045] S1, obtaining relevant configuration parameters of the 2D NAND FLASH memory to be tested;
[0046] The relevant configuration parameters include physical parameters of the initial substrate Si, tunnel oxide SiO2, polysilicon floating gate, barrier layer, polysilicon control gate, source and drain. In a feasible embodiment of the present invention, the concentration of B (boron) in the initial substrate Si is 1×10 14 cm -3 , the crystal orientation is (100); the thickness of the tunnel oxide SiO2 is 7.0nm; the thickness of the floating gate polysilicon is 65nm, and the concentration of P (phosphorus) injected into the floating gate is 1×10 21 cm -3 The gate length of the floating gate is 19nm; the barrier layer is SiO2, Si3N4, and SiO2, with thicknesses of 4.0nm, 3.5nm, and 4.5nm respectively; the thickness of the polysilicon control gate is 85nm and the gate length is 19nm; the thickness of the TiSi layer on the control gate is 20nm; the source and drain are formed by injecting a concentration of 1×10 12 cm -3 As (arsenic) is diffused at 930°C for 10 minutes; the formed memory cell junction depth is 0.18μm.
[0047] S2, inputting relevant configuration parameters of the 2D NAND FLASH memory to be tested into the simulation model, and introducing a trap mechanism into the simulation model to replace a huge number of erase and write cycles;
[0048] It should be noted that the simulation process of the simulation model is completed through the SILVACO TCAD platform and is applicable to other simulation platforms. In the simulation of the durability degradation of the 19nm process 2D NAND FLASH memory, by introducing the trap mechanism, the increase in drain current after durability degradation and the subsequent decrease in write charge efficiency (programming efficiency) are reproduced in the model. The introduction of this trap is based on a deep understanding of the actual physical process. Specifically, with the degradation of durability, the energy and speed of hot electrons will decrease. This is because with the repeated use of flash memory, the physical properties of its internal materials, such as the adjustment of the band structure or the formation of traps, will affect the transmission characteristics of hot electrons. Due to the reduction in the energy of hot electrons, their ability to be injected into the floating gate will be weakened, resulting in a reduction in electron injection in the floating gate. Traps will be introduced for electrical simulation of programming and erasing steps. When simulating the durability of the device, traps will be introduced along the SiO2 / Si interface to simulate the decrease in write charge efficiency (programming efficiency). These traps can capture electrons that should have been injected into the floating gate, resulting in a reduction in the number of electrons actually injected into the floating gate, thereby reproducing the phenomenon that the write charge efficiency (programming efficiency) of actual flash memory devices decreases after endurance degradation. The introduction of traps greatly reduces the time spent on actual endurance characterization, and has the advantages of high efficiency, accuracy, speed, and resource conservation.
[0049] S3, obtaining the programming threshold voltage change ΔV during several erase and write cycles according to the simulation model tp and the trapped charge Q ox The linear relationship between 2D NAND FLASH and 2D NAND FLASH is used to qualitatively characterize the endurance of 2D NAND FLASH memory.
[0050] As the amount of trapped charge introduced increases, the programming threshold voltage changes by ΔV tp The programming threshold voltage change ΔV is also gradually increased according to the simulation results of the simulation model. tp and the trapped charge Q ox The relationship curve diagram of the programming threshold voltage change ΔV is plotted by converting the horizontal and vertical coordinates in the curve diagram into logarithmic coordinates. tp and the trapped charge Q ox Take the log and get a value about the change in programming threshold voltage ΔV tp and the trapped charge Q ox The linear relationship of is as follows:
[0051] lg(ΔV tp )=Alg(Q ox )+B
[0052] Where ΔV tp is the programming threshold voltage change; Q oxis the trapped charge; A is the slope of the fitting curve; B is the intercept of the fitting curve.
[0053] According to the obtained programming threshold voltage change ΔV tp and the trapped charge Q ox The linear relationship between the programming threshold voltage and the set trap concentration is introduced to predict the change in programming threshold voltage ΔV tp .
[0054] When the programming threshold voltage changes by ΔV tp When the preset failure standard is reached, it means that the device fails. According to the obtained programming threshold voltage change ΔV tp and the trapped charge Q ox The linear relationship between the introduced trap concentration and the erase and write cycles is obtained, thereby qualitatively characterizing the durability and calculating the service life of the device.
[0055] See also Figure 2 The embodiment of the present invention discloses a system for qualitatively characterizing the durability of a 2D NAND FLASH memory, comprising a parameter acquisition module, a trap introduction module and a simulation module; wherein the parameter acquisition module is used to acquire relevant configuration parameters of the 2D NAND FLASH memory to be tested; the trap introduction module is used to input the relevant configuration parameters of the 2D NAND FLASH memory to be tested into a simulation model, and introduce a trap mechanism into the simulation model; the simulation module is used to obtain a programming threshold voltage change ΔV according to the simulation model tp and the trapped charge Q ox The linear relationship between 2D NAND FLASH and 2D NAND FLASH is used to qualitatively characterize the endurance of 2D NAND FLASH memory.
[0056] Example:
[0057] like Figure 4 As shown in the figure, the programming and erasing threshold voltages of a device with a tunnel oxide (SiO2) thickness of 7.0nm vary with the amount of trapped charge. It shows that as the amount of trapped charge increases, the storage window (V tp -V te , that is, programming threshold voltage minus erasing threshold voltage) decreases, and durability decreases. During degradation, the erase voltage has been increasing, but erasing plays a smaller role than programming. In addition, the programming threshold voltage decreases linearly with the increase of the amount of trapped charge, which verifies the conclusion that the programming threshold voltage can be used to simulate degradation. The range of trap charge is 0 to 2.00E-13C / cm 2 The method uses the change in programming threshold voltage to simulate the degradation of the storage window, thereby qualitatively characterizing the durability. The greater the change in programming threshold voltage, the worse the durability of the device. Figure 5 is the change in programming threshold voltage as the amount of trapped charge changes. Figure 5 As shown in a, ΔV tp and the trapped charge Q ox The relationship is linear, and the range of trapped charge is 0~3.3E-13C·cm -2 , ΔV tp The corresponding variation range is about 0 to 5 V. When the slope of the curve with the change of the trapped charge amount is larger, ΔV tp The larger the value (that is, for the same amount of trapped charge, ΔV tp The larger the value, the worse the durability of the device. When the slope of the curve is difficult to clearly distinguish the durability, both the horizontal and vertical axes can be converted to logarithmic coordinates, that is, the trap charge and ΔV tp Take the log respectively. In this way, we can get a tp and the trapped charge Q ox The linear relationship is lg(ΔV tp )=Alg(Q ox )+B, such as Figure 5 According to the corresponding relationship between trap concentration and erase-write cycle number, the set trap concentration is introduced, that is, under the limited erase-write cycle number, the programming threshold voltage change (ΔV tp ). Conversely, when the programming threshold voltage changes to a preset failure standard, it means that the device has failed. At this time, the number of erase and write cycles can be calculated based on the introduced trap concentration, thereby qualitatively characterizing the durability and estimating the service life of the device.
[0058] See also Figure 3 The method for qualitatively characterizing the durability of 2D NAND flash is used to further optimize the chip preparation process and improve chip performance; the relationship between the change in programming threshold voltage and the change in trap charge density is used to qualitatively characterize the durability of 2D NAND flash, which can be conveniently used to explore the impact of process factors on durability, such as the impact of tunnel oxide thickness, floating gate thickness, temperature, tunnel oxide preparation process, diffused nitrided tunnel oxide, etc. on durability.
[0059] There are many methods for preparing tunnel oxide SiO2, including thermal oxidation, thermal decomposition, sputtering, anodization, etc. At present, thermal oxidation is one of the most widely used preparation methods because of its advantages such as simple process, high quality of oxide film, and stability of film. The thermal oxidation process of silicon is that the silicon material is converted into silicon dioxide through oxidation reaction under a high temperature environment of 900-1200°C. This process can be subdivided into several types such as dry oxygen oxidation, wet oxygen oxidation and water vapor oxidation according to different oxidation conditions. In the dry oxygen oxidation process, dry and pure oxygen is used as the oxidizing atmosphere, and oxygen directly reacts with silicon at high temperature to form silicon dioxide. Although the oxidation speed is slow, the generated oxide layer has the densest structure, and its surface presents a non-polar siloxane structure. This structural characteristic makes it have excellent adhesion to the photoresist and effectively avoids the occurrence of floating glue. Water vapor oxidation uses high-purity water vapor as the oxidation atmosphere, and silicon atoms and water molecules on the surface of the silicon wafer react to generate silicon dioxide. Water vapor oxidation accelerates the oxidation reaction due to the participation of water vapor, but it also causes the oxide layer structure to become loose, and the quality is lower than that of dry oxygen oxidation. Wet oxygen oxidation combines the characteristics of dry oxygen and water vapor, and its oxidation speed and quality are between dry oxygen oxidation and water vapor oxidation.
[0060] The relationship between the change in programming threshold voltage and the amount of trapped charge is used to qualitatively characterize the durability of 19nm process 2D NAND flash, and to guide the preparation methods of tunnel oxide (SiO2) in different processes. For all tunnel oxide (SiO2) thicknesses of 7.0nm, a comparative study of direct deposition, wet oxygen growth, and dry oxygen growth was conducted, and the range of trapped charge was controlled in the range of 0 to 2.00E-13C / cm 2 The tunnel oxide (SiO2) dielectric layers prepared by the three processes are all oriented (110) and doped with a boron concentration of 1×10 14 cm -3 on a single crystal silicon substrate.
[0061] Dry oxygen growth: During dry oxygen growth preparation, the diffusion temperature is controlled to be 1000°C and the time is 30 minutes;
[0062] Wet oxygen growth: During wet oxygen growth, the diffusion temperature is controlled to be 800°C and the time is 20 minutes;
[0063] Direct deposition: Direct deposition deposits a 7.0nm thick silicon dioxide layer directly on the substrate;
[0064] Figure 6 As a guide to the results, it is shown that the slope of the curve is the largest when directly deposited, the slope of the curve is second when wet oxygen is prepared, and the slope of the curve is the smallest when dry oxygen is prepared, indicating that when the thickness of the tunnel oxide (SiO2) is 7.0nm, at the same trap charge amount, the trap charge amount is 1.25E-13C / cm 2For example, the programming threshold voltage change of 19nm process 2D NAND flash obtained by dry oxygen preparation of tunnel oxide (SiO2) is the smallest, ΔV tp The programming threshold voltage change of 19nm process 2D NAND flash obtained by preparing tunnel oxide (SiO2) with wet oxygen is second, ΔV tp The programming threshold voltage change of 19nm 2D NAND flash obtained by directly depositing tunnel oxide (SiO2) is the largest, ΔV tp The result is ~2.25V. It shows that the 19nm process 2D NAND flash with dry oxygen preparation of tunnel oxide (SiO2) has the best durability, followed by wet oxygen growth, while direct deposition has the worst effect. This qualitative characterization result obtains the high-durability 2D NAND flash tunnel oxide (SiO2) layer preparation process, that is, the dry oxygen method is used to prepare a 7.0nm thick tunnel oxide (SiO2) dielectric layer, and the trapped charge is controlled at 2.00E-13C / cm 2 This discovery suggests that the use of dry oxygen growth methods under specific conditions can significantly improve the durability of flash memory devices, providing a valuable reference for the optimization of flash memory technology.
[0065] The present invention simulates the reduction of write charge efficiency (programming efficiency) by introducing traps, replaces a huge number of erase and write cycles, greatly shortens the time for characterizing durability, and is efficient and fast; at the same time, the change in programming threshold voltage is used as the main durability indicator, rather than using the threshold voltage as the main durability indicator, and the relationship with the trap charge is a linear relationship, and the slope of the curve can be used to conveniently and intuitively judge the durability quality under different process conditions; using trap charges to simulate the reduction of write charge efficiency (programming efficiency) and using the change in programming threshold voltage as the main parameter indicator of durability has a physical theoretical basis and relevant theoretical support, and the method is accurate and reliable for qualitatively characterizing durability; in addition, due to the replacement of a huge number of erase and write cycles, the consumption of computing resources is reduced, and the cost of characterizing durability is reduced; when the trap charge range is controlled within 0 to 2.00E-13C / cm 2By comparing different tunnel oxide (SiO2) dielectric layer preparation processes, namely dry oxygen method, wet oxygen method, and direct deposition, under the same amount of trapped charge, the programming threshold voltage change of the 19nm process 2D NAND flash memory obtained by the dry oxygen method to prepare a 7.0nm thick tunnel oxide (SiO2) dielectric layer is the smallest, followed by wet oxygen, and the largest by direct deposition, indicating that the 19nm process 2D NAND flash prepared by dry oxygen tunnel oxide (SiO2) exhibits the best durability, followed by wet oxygen growth, while direct deposition exhibits the worst effect. Through this qualitative characterization result, the high durability 19nm process 2D NAND flash prepared by the dry oxygen method (controlling the diffusion temperature to 1000℃, time to 30min) with a 7.0nm thick tunnel oxide (SiO2) is obtained, and the trap charge range is controlled in the range of 0 to 2.00E-13C / cm 2 This method can further guide simulation and optimize the actual preparation process, provide reference and application value, improve chip durability and thus improve chip performance.
[0066] In one embodiment of the present invention, see Figure 7 , a computer device is provided, the computer device includes a processor and a memory, the memory is used to store a computer program, the computer program includes program instructions, and the processor is used to execute the program instructions stored in the computer storage medium. The processor may be a central processing unit (CPU), or other general-purpose processors, digital signal processors (DSP), application-specific integrated circuits (ASIC), field-programmable gate arrays (FPGA) or other programmable logic devices, discrete gates or transistor logic devices, discrete hardware components, etc. It is the computing core and control core of the terminal, which is suitable for implementing one or more instructions, and is specifically suitable for loading and executing one or more instructions in a computer storage medium to implement a corresponding method flow or a corresponding function; the processor described in the embodiment of the present invention can be used for the operation of the method for qualitatively characterizing the durability of 2D NAND FLASH memory.
[0067] The present invention also provides a storage medium, specifically a computer-readable storage medium (Memory), which is a memory device in a computer device for storing programs and data. It is understandable that the computer-readable storage medium here can include both built-in storage media in a computer device and, of course, extended storage media supported by the computer device. The computer-readable storage medium provides a storage space that stores the operating system of the terminal. In addition, one or more instructions suitable for being loaded and executed by a processor are also stored in the storage space, and these instructions can be one or more computer programs (including program codes). It should be noted that the computer-readable storage medium here can be a high-speed RAM memory or a non-volatile memory (non-volatile memory), such as at least one disk memory. The processor can load and execute one or more instructions stored in the computer-readable storage medium to implement the corresponding steps of the method for qualitatively characterizing the durability of the 2D NAND FLASH memory in the above embodiment.
[0068] Those skilled in the art will appreciate that embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.
[0069] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (systems), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0070] These computer program instructions may also be stored in a computer readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer readable memory produce an article of manufacture including an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0071] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 A step that specifies a function in one or more boxes.
[0072] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.
Claims
1. A method for qualitatively characterizing the endurance of 2D NAND FLASH memory, characterized in that: The following steps are involved: Obtain relevant configuration parameters of the 2D NAND FLASH memory to be tested; Input relevant configuration parameters of the 2D NAND FLASH memory to be tested into the simulation model, and introduce a trap mechanism into the simulation model; According to the simulation model, the programming threshold voltage change ΔV during several erase and write cycles is obtained tp and the trapped charge Q ox The linear relationship between 2D NAND FLASH and 2D NAND FLASH is used to qualitatively characterize the endurance of 2D NAND FLASH memory.
2. The method for qualitatively characterizing the endurance of a 2D NAND FLASH memory according to claim 1, characterized in that: In the step of obtaining relevant configuration parameters of the 2D NAND FLASH memory to be tested, the relevant configuration parameters include: physical parameters of the initial substrate Si, tunnel oxide SiO2, polysilicon floating gate, barrier layer, polysilicon control gate, source and drain.
3. The method for qualitatively characterizing the endurance of a 2D NAND FLASH memory according to claim 1, characterized in that: In the step of inputting the relevant configuration parameters of the 2D NAND FLASH memory to be tested into the simulation model and introducing the trap mechanism into the simulation model, the simulation process of the simulation model is completed through the SILVACO TCAD platform, and the reduction of the write charge efficiency is simulated by introducing traps along the SiO2 / Si interface.
4. The method for qualitatively characterizing the endurance of a 2D NAND FLASH memory according to claim 1, characterized in that: The programming threshold voltage change ΔV is obtained according to the simulation model tp and the trapped charge Q ox The steps to qualitatively characterize the endurance of 2D NAND FLASH memory include: As the amount of trapped charge introduced increases, the programming threshold voltage changes by ΔV tp The programming threshold voltage change ΔV is also gradually increased according to the simulation results of the simulation model. tp and the trapped charge Q ox The relationship curve diagram of the programming threshold voltage change ΔV is plotted by converting the horizontal and vertical coordinates in the curve diagram into logarithmic coordinates. tp and the trapped charge Q ox Take the log and get a value about the change in programming threshold voltage ΔV tp and the trapped charge Q ox The linear relationship of is as follows: lg(ΔV tp )=Alg(Q ox )+B Where, ΔV tp is the programming threshold voltage change; Q ox is the trapped charge; A is the slope of the fitting curve; B is the intercept of the fitting curve.
5. The method for qualitatively characterizing the endurance of a 2D NAND FLASH memory according to claim 4, characterized in that: Also includes: According to the obtained programming threshold voltage change ΔV tp and the trapped charge Q ox The linear relationship between the programming threshold voltage and the set trap concentration is introduced to predict the change in programming threshold voltage ΔV tp .
6. The method for qualitatively characterizing the endurance of a 2D NAND FLASH memory according to claim 4, characterized in that: Also includes: When the programming threshold voltage changes by ΔV tp When the preset failure standard is reached, it means that the device fails. According to the obtained programming threshold voltage change ΔV tp and the trapped charge Q ox The linear relationship between the introduced trap concentration and the erase and write cycles is obtained, thereby qualitatively characterizing the durability and calculating the service life of the device.
7. A system for qualitatively characterizing the endurance of a 2D NAND FLASH memory, characterized in that: include: A parameter acquisition module is used to obtain relevant configuration parameters of the 2D NAND FLASH memory to be tested; A trap introduction module is used to input relevant configuration parameters of the 2D NAND FLASH memory to be tested into the simulation model, and introduce a trap mechanism into the simulation model; A simulation module is used to obtain the programming threshold voltage change ΔV according to the simulation model tp and the trapped charge Q ox The linear relationship between 2D NAND FLASH and 2D NAND FLASH is used to qualitatively characterize the endurance of 2D NAND FLASH memory.
8. A computer device comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that: When the processor executes the computer program, the steps of the method according to any one of claims 1 to 6 are implemented.
9. A computer-readable storage medium storing a computer program, characterized in that: When the computer program is executed by a processor, the steps of the method according to any one of claims 1 to 6 are implemented.