Beta-radiovolt effect nuclear battery based on carbon-14 diamond and manufacturing method

By adopting a combination design of carbon-14 diamond and graphene supercapacitors in β-radiation volt effect nuclear batteries, the problems of low power and insufficient radiation resistance of traditional nuclear batteries are solved, high power output and stable operation are achieved, and energy is improved Conversion efficiency and mechanical properties.

CN119028622APending Publication Date: 2024-11-26ELECTRIC POWER RES INST OF GUANGXI POWER GRID CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410863051.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-29
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing β-radiation volt effect nuclear batteries have a narrow bandwidth and poor radiation resistance due to the narrow bandwidth of Si and GaAs used, which leads to low power, insufficient stability and radiation resistance, and the separation of radiation sources and semiconductor transducer devices. Energy wasted and conversion efficiency is inefficient.

Method used

Using a β-radiation volt-effect nuclear battery based on carbon-14 diamond, including power generation units and energy storage units. The power generation units are composed of Schottky metal layer, carbon-14 diamond film, P+ diamond film, diamond substrate and ohmic contact layer. , combined with graphene supercapacitors, are prepared by microwave plasma vapor deposition and magnetron sputtering processes to form an efficient power generation and energy storage structure.

Benefits of technology

It achieves high power output and stable operation, overcomes the problems of insufficient low power and radiation resistance of traditional nuclear batteries, improves energy conversion efficiency, and improves mechanical strength and heat dissipation performance through the design of graphene supercapacitors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028622A_ABST
    Figure CN119028622A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of energy storage and utilization of nuclear batteries, and discloses a carbon-14 diamond-based beta-radiovolt effect nuclear battery and a manufacturing method thereof.The nuclear battery comprises a power generation unit and an energy storage unit, and the power generation unit comprises at least one group of power generation structural bodies; the power generation structural body comprises a Schottky metal layer, a carbon-14 diamond film, a P + type diamond film, a diamond substrate and an ohmic contact layer which are sequentially distributed in a layered structure; the nuclear battery disclosed by the invention is based on a carbon-14 diamond transducer and is combined with a graphene supercapacitor to form radiation-volt conversion and storage integrated equipment, decay energy of radioactive isotopes is converted into electric energy, and the electric energy is stored; the diamond Schottky junction beta radiation volt effect nuclear battery forms the charging bin of the graphene supercapacitor, the mechanical strength is high, the heat dissipation performance is good, the work is stable, and the large power output of the milliwatt level can be realized by accumulating the charge quantity through time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of nuclear battery energy storage and utilization, and in particular to a carbon-14 diamond-based beta radiation voltaic effect nuclear battery and a manufacturing method thereof. Background Art

[0002] With the rapid development and high integration of miniaturized and self-powered electronic systems, there is an urgent need to develop electrochemical micro energy storage devices, mainly including micro batteries and micro supercapacitors. Among them, planar micro batteries and micro supercapacitors have attracted widespread attention because they can be directly integrated with microelectronic devices on a single substrate and can become independent or supplementary micro power sources.

[0003] Nuclear batteries have the advantages of long life and high energy density. They are highly adaptable to the environment and do not require human intervention. Therefore, they are widely used in aerospace, military defense, deep sea, deep earth, polar exploration, biomedicine and micro-electromechanical systems. Among them, the β-radiation voltaic effect nuclear battery itself is a semiconductor component, which is easy to integrate with other electronic components. It is small in size, stable in operation, and does not contain moving parts. It is an ideal micro power source for micro-electromechanical systems (MEMS).

[0004] Traditional β-radiation voltaic effect nuclear batteries use materials such as Si and GaAs, which have narrow bandgap widths and poor radiation resistance, resulting in low open circuit voltages and long-term performance degradation of nuclear batteries due to radiation damage. The separate structure of the radiation source and the semiconductor transducer device causes a large portion of the radiation source's energy to be wasted due to the self-absorption effect, resulting in reduced short-circuit current and low conversion efficiency. Therefore, it is urgent to improve existing nuclear batteries to meet today's application needs. Summary of the invention

[0005] The purpose of this section is to summarize some aspects of embodiments of the present invention and briefly introduce some preferred embodiments. Some simplifications or omissions may be made in this section and the specification abstract and the invention title of this application to avoid blurring the purpose of this section, the specification abstract and the invention title, and such simplifications or omissions cannot be used to limit the scope of the present invention.

[0006] In view of the above-mentioned problems existing in the existing nuclear batteries, the present invention is proposed.

[0007] Therefore, one object of the present invention is to provide a beta radiation voltaic effect nuclear battery based on carbon-14 diamond, so as to solve the problems of low power, stability and weak radiation resistance of existing nuclear batteries.

[0008] In order to solve the above technical problems, the present invention provides the following technical solutions: a beta-radiation voltaic effect nuclear battery based on carbon-14 diamond, the nuclear battery comprising a power generation unit and an energy storage unit, wherein the power generation unit comprises at least one power generation structure; the power generation structure comprises a Schottky metal layer, a carbon-14 diamond film, a P + type diamond film, diamond substrate and ohmic contact layer.

[0009] As a preferred solution of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery described in the present invention, the power generation unit also includes a first electrode connected to the Schottky metal layer in each group of the power generation structure through a wire, and a second electrode connected to the ohmic contact layer.

[0010] As a preferred solution of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery of the present invention, wherein: the thickness of the Schottky metal layer is 50-100 nm; the carbon-14 diamond film is a boron-doped P-type diamond with a doping concentration of N A =10 14 cm -3 , with a thickness of 100 to 500 nm; the P + The diamond film is a boron-doped P-type diamond with a doping concentration of N A =10 20 cm -3 , with a thickness of 1 to 2 μm; the diamond substrate is a type Ib diamond substrate with a thickness of 0.4 mm; the ohmic contact layer adopts Ti / Au alloy electrodes with thicknesses of 50 nm and 80 nm respectively.

[0011] As a preferred solution of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery described in the present invention, it also includes an energy storage unit, which includes no less than one graphene supercapacitor, the first electrode is connected to the negative electrode of the graphene supercapacitor, and the second electrode is connected to the positive electrode of the graphene supercapacitor.

[0012] Another object of the present invention is to provide a method for manufacturing a carbon-14 diamond-based beta-radiation voltaic effect nuclear battery, so as to prepare the above-mentioned nuclear battery.

[0013] In order to solve the above technical problems, the present invention provides the following technical solutions: a method for manufacturing a carbon-14 diamond-based beta radiation voltaic effect nuclear battery, the manufacturing method comprising the following steps:

[0014] S1: Using type Ib diamond as substrate, P was homoepitaxially grown by microwave plasma vapor deposition. + Type diamond film;

[0015] S2: After the growth of P + On the type diamond film, a carbon-14 diamond film is homoepitaxially grown by microwave plasma vapor deposition to form a diamond epitaxial wafer;

[0016] S3: cleaning the prepared diamond epitaxial wafer; treating it with an acid solution to form an oxygen-terminated surface, and then cleaning and drying it;

[0017] S4: Preparation of Schottky electrode on the surface of carbon-14 diamond film of diamond epitaxial wafer;

[0018] S5: preparing an ohmic contact electrode on a side of the diamond epitaxial wafer away from the carbon-14 diamond film;

[0019] S6: cutting the diamond epitaxial wafer assembly and welding wires at the Schottky electrode and the ohmic contact electrode;

[0020] S7: Connect the wires to the positive electrode and the negative electrode of the graphene supercapacitor respectively, and arrange multiple groups of diamond epitaxial wafer assemblies on the periphery of the graphene supercapacitor.

[0021] As a preferred embodiment of the method for manufacturing a carbon-14 diamond-based beta-radiation voltaic effect nuclear battery according to the present invention, wherein: the P + type diamond film, using CH4, TMB and H2 as reaction gases, CH4 gas flow rate 5sccm, TMB gas flow rate 5sccm, H2 gas flow rate 500sccm, substrate temperature 950℃, gas pressure 1000Pa, microwave power 4kW, and growth time 5h.

[0022] As a preferred embodiment of the method for manufacturing a carbon-14 diamond-based beta-radiation voltaic effect nuclear battery according to the present invention, the carbon-14 diamond film is homoepitaxially grown by microwave plasma vapor deposition. 14 CH4, TMB, H2 are used as reaction gases, among which 14 CH4 provides the carbon source for diamond growth, and TMB serves as the p-type doping B source. 14 CH4 gas flow rate is 5 sccm, H2 gas flow rate is 500 sccm, substrate temperature is 900°C, TMB gas flow rate is 3 sccm, gas pressure is 1000 Pa, microwave power is 4 kW, and growth time is 2 h.

[0023] As a preferred embodiment of the method for manufacturing a carbon-14 diamond-based beta-radiation voltaic effect nuclear battery of the present invention, the cleaning treatment of the prepared diamond epitaxial wafer comprises ultrasonic cleaning with methanol, acetone and ethanol for 15 minutes respectively, and then rinsing with deionized water;

[0024] The acid solution treatment includes placing the diamond epitaxial wafer in a mixture of 300° C. sulfuric acid and nitric acid (volume mixing ratio 1:1) for 3 hours to remove the hydrogen terminal surface conductive layer.

[0025] As a preferred embodiment of the manufacturing method of the carbon-14 diamond-based beta-radiation voltaic effect nuclear battery of the present invention, wherein: the Schottky electrode is prepared on the surface of the carbon-14 diamond film of the diamond epitaxial wafer, and the Schottky contact metal Ni is sputtered by a magnetron sputtering process, and the sputtering gas pressure is 10 -7 Pa and annealed at 500 °C in nitrogen for 1 h.

[0026] As a preferred embodiment of the manufacturing method of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery of the present invention, an ohmic contact electrode is prepared on the side of the diamond epitaxial wafer away from the carbon-14 diamond film, and the ohmic contact metal Ti and metal Au are sputtered in sequence by a magnetron sputtering process, followed by annealing at 700°C in nitrogen for 1 hour.

[0027] Beneficial effects of the present invention:

[0028] The nuclear battery of the present invention is based on a carbon-14 diamond transducer device, combined with a graphene supercapacitor to form an integrated radiovoltaic conversion and storage device, which converts the decay energy of radioactive isotopes into electrical energy and stores it; the diamond Schottky junction β-radiovoltaic effect nuclear battery constitutes the charging compartment of the graphene supercapacitor, which has high mechanical strength, good heat dissipation performance, stable operation, and can achieve high-power output of milliwatts to the outside by accumulating charge over time. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative labor. Among them:

[0030] Figure 1 The figure is a schematic diagram of the construction principle of the beta radiation voltaic effect nuclear battery based on carbon-14 diamond of the present invention.

[0031] Figure 2 This is a schematic diagram of the power generation unit layer structure of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery of the present invention.

[0032] Figure 3 It is a schematic diagram of the internal electron flow of the beta radiation voltaic effect nuclear battery based on carbon-14 diamond of the present invention.

[0033] Figure 4 This is a schematic diagram of the power generation structure of the carbon-14 diamond-based beta radiation voltaic effect nuclear battery of the present invention, which is placed sideways and surrounds the periphery of the capacitor.

[0034] Figure 5 This is a schematic diagram of the power generation structure of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery of the present invention being stacked flatly on the periphery of a capacitor.

[0035] Figure 6 This is a schematic diagram of the power generation structure of the carbon-14 diamond-based β-radiation voltaic effect nuclear battery of the present invention, which is placed sideways and radially distributed around the capacitor. DETAILED DESCRIPTION

[0036] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are described in detail below in conjunction with the accompanying drawings.

[0037] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0038] Secondly, the term "one embodiment" or "embodiment" as used herein refers to a specific feature, structure, or characteristic that may be included in at least one implementation of the present invention. The term "in one embodiment" that appears in different places in this specification does not necessarily refer to the same embodiment, nor does it refer to a separate or selective embodiment that is mutually exclusive with other embodiments.

[0039] Secondly, the present invention is described in detail with reference to the schematic diagram. When describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.

[0040] Example 1

[0041] Reference Figures 1 to 6 , which is the first embodiment of the present invention, provides a beta radiation voltaic effect nuclear battery based on carbon-14 diamond, and the nuclear battery includes a power generation unit 100 and an energy storage unit 200, wherein the power generation unit 100 is used to generate electrical energy and transmit the generated electrical energy to the energy storage unit 200 for storage; the energy storage unit 200 discharges to the outside in a centralized manner.

[0042] Specifically, the power generation unit 100 includes at least one power generation structure 101, each power generation structure 101 is independent of each other, and a relatively stable power generation unit 100 is formed by combining multiple power generation structures 101; and the power generation structure 101, as shown in the attached Figure 2 As shown in FIG. 1 , the structure is layered, and from top to bottom, the Schottky metal layer 101a, the carbon-14 diamond film 101b, the P + The Schottky metal layer 101a, the carbon-14 diamond film 101b and the P + The type diamond film 101c constitutes the power generation structure of the nuclear battery; and the Schottky metal layer 101a and the ohmic contact layer 101e respectively form the negative electrode and the positive electrode of the power generation structure 101.

[0043] Furthermore, in this nuclear battery structure, the thickness of the Schottky metal layer 101a is 50-100 nm; the carbon-14 diamond film 101b is a boron-doped P-type diamond with a doping concentration of N A =10 14 cm -3 , thickness is 100~500nm; P + The diamond film 101c is a P-type diamond doped with boron, with a doping concentration of N A =10 20 cm -3 , with a thickness of 1 to 2 μm; the diamond substrate 101d is a type Ib diamond substrate with a thickness of 0.4 mm; the ohmic contact layer 101e uses a Ti / Au alloy electrode with thicknesses of 50 nm and 80 nm respectively.

[0044] Different from Si, GaAs and other materials used in traditional β-radiation voltaic effect nuclear batteries, diamond is an ultra-wide bandgap semiconductor material with a bandgap width of 5.5eV. It has extremely strong radiation resistance, high carrier mobility, high thermal conductivity, and strong stability. It is an ideal choice for energy conversion materials in β-radiation voltaic effect nuclear batteries.

[0045] Among them, non-radioactive diamonds are mainly composed of 12 C (carbon-12), while radioactive isotopes 14 C (Carbon-14) has pure β radioactivity, with average β particle energy of 49.47keV and 156.475keV. It has moderate energy and does not contain accompanying γ rays, making it suitable for use as a radiation source for β radiation voltaic effect nuclear batteries. 14 The C diamond film has both β radioactivity and semiconductor properties, and can be used as a β radiation source and a transducer material at the same time, which can overcome the negative impact of the self-absorption effect of the low-energy β source.

[0046] In the power generation structure 101, the carbon-14 diamond film 101b contains a large amount of radioactive isotope carbon-14, which constantly emits beta particles in all directions in the structure, generating radiation-generated electron-hole pairs through the radiovoltaic effect; and the Schottky metal layer 101a and the carbon-14 diamond film 101b form a Schottky barrier at the interface between the Schottky metal layer 101a, the carbon-14 diamond film 101b and the P + Under the action of the built-in electric field formed by the type diamond film 101c, electrons and holes are separated and move in a directional manner, the electrons move to the Schottky metal layer 101a, and the holes move to the ohmic contact layer 101e, thereby forming a current.

[0047] Furthermore, the first electrode 102 is connected to the Schottky metal layer 101a in each power generation structure 101 through a wire to form the negative electrode of the nuclear battery; the second electrode 103 is connected to the ohmic contact layer 101e in each power generation structure 101 through a wire to form the positive electrode of the nuclear battery; this facilitates the power generation unit 100 to output electrical energy to the outside.

[0048] The energy storage unit 200 includes at least one graphene supercapacitor 201 , the first electrode 102 is connected to the positive electrode of the graphene supercapacitor 201 , and the second electrode 103 is connected to the negative electrode of the graphene supercapacitor 201 .

[0049] The energy storage unit 200 may be composed of a single graphene supercapacitor or a plurality of graphene capacitor groups, and the specific configuration may be determined by actual application requirements. The capacitor may be charged by correspondingly connecting the second electrode 103 and the first electrode 102 in the power generation unit 100 to the positive and negative plates of the capacitor.

[0050] Graphene supercapacitors have excellent electrical and thermal conductivity, and their internal structure design is flexible, so the capacitors can be made into various shapes. In addition, it is convenient to match graphene supercapacitors with different numbers of power generation structures 101, and to adjust the distribution state of the combination of each power generation structure 101 and graphene supercapacitor 201 based on the installation position. Figures 4 to 6 As shown in , if the sheet-like power generation structure 101 is arranged in a polygonal, radial or stacked shape on the periphery of the capacitor, the overall structural strength of the nuclear battery can be effectively improved, the energy utilization rate of the nuclear battery can be improved, and the installation space can be saved.

[0051] The integrated beta radiation voltaic effect nuclear battery composed of carbon-14 diamond ultra-wide bandgap semiconductor transducer devices has the advantage of high output voltage, which can continuously charge the graphene supercapacitor and store the decay energy of the radioactive source in the capacitor. Instantaneous milliwatt-level power output can be achieved for different application scenarios. On the one hand, it improves the energy conversion efficiency of the beta radiation voltaic effect nuclear battery; on the other hand, it overcomes the disadvantage of low power of the beta radiation voltaic effect nuclear battery.

[0052] Example 2

[0053] As a second embodiment of the present invention, a method for manufacturing a beta radiation voltaic effect nuclear battery based on carbon-14 diamond is provided, which is used to manufacture the beta radiation voltaic effect nuclear battery as in embodiment 1. The manufacturing method comprises the following steps:

[0054] S1: Using type Ib diamond as substrate, P was homoepitaxially grown by microwave plasma vapor deposition. + type diamond film 101c; wherein, in the microwave plasma vapor deposition process, CH4 (methane), TMB (B(CH3)3, trimethylboron), and H2 (hydrogen) are used as reaction gases, the CH4 gas flow rate is 5sccm (sccm is milliliters per minute under standard conditions), the TMB gas flow rate is 5sccm, the H2 gas flow rate is 500sccm, the substrate temperature is 950°C, the gas pressure is 1000Pa, the microwave power is 4kW, and the growth time is 5h.

[0055] S2: After the growth of P + On the type diamond film 101c, a carbon-14 diamond film 101b is homoepitaxially grown by microwave plasma vapor deposition to form a diamond epitaxial wafer; wherein, in the microwave plasma vapor deposition process, 14 CH4, TMB, H2 are used as reaction gases, among which 14 CH4 provides the carbon source for diamond growth, and TMB serves as the p-type doping B source. 14 CH4 gas flow rate is 5 sccm, H2 gas flow rate is 500 sccm, substrate temperature is 900°C, TMB gas flow rate is 3 sccm, gas pressure is 1000 Pa, microwave power is 4 kW, and growth time is 2 h.

[0056] S3: Clean the prepared diamond epitaxial wafer; then treat it with an acid solution to form an oxygen terminal surface, and then clean and dry it; specifically, the cleaning treatment includes ultrasonic cleaning with methanol, acetone and ethanol for 15 minutes respectively, and then rinsing with deionized water; the acid solution treatment includes placing the diamond epitaxial wafer in a mixed solution of 300℃ sulfuric acid and nitric acid in a volume ratio of 1:1 for 3 hours to remove the hydrogen terminal surface conductive layer. Then rinse it with deionized water.

[0057] S4: Prepare a Schottky electrode on the surface of the carbon-14 diamond film 101b of the diamond epitaxial wafer; specifically, use a magnetron sputtering process to sputter the Schottky contact metal Ni, and the sputtering pressure is 10 -7 Pa and annealed at 500 °C in nitrogen for 1 h to obtain a good Schottky contact.

[0058] S5: preparing an ohmic contact electrode on the side of the diamond epitaxial wafer away from the carbon-14 diamond film 101b; specifically, using a magnetron sputtering process to sputter ohmic contact metal Ti and metal Au in sequence, followed by annealing at 700°C in nitrogen for 1 hour to obtain a good ohmic contact.

[0059] S6: cutting the diamond epitaxial wafer assembly and welding wires at the Schottky electrodes and the ohmic contact electrodes to form each power generation structure 101;

[0060] S7: Connect the wires to the positive and negative plates of the graphene supercapacitor 201, and arrange multiple groups of diamond epitaxial wafer assemblies (i.e., power generation structures 101) on the periphery of the graphene supercapacitor 201. Specifically, the arrangement of the power generation structures 101 can be determined according to the shape and space size of the installed battery compartment, and the maximum energy utilization rate can be achieved as much as possible.

[0061] Finally, the positive and negative plates of the graphene supercapacitor 201 supply power to the external circuit.

[0062] It should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solutions of the present invention may be modified or replaced by equivalents without departing from the spirit and scope of the technical solutions of the present invention, which should all be included in the scope of the claims of the present invention.

Claims

1. A beta radiation voltaic effect nuclear battery based on carbon-14 diamond, characterized in that: include, A power generation unit (100), comprising at least one group of power generation structures (101); The power generation structure (101) comprises a Schottky metal layer (101a), a carbon-14 diamond film (101b), a P + type diamond film (101c), a diamond substrate (101d) and an ohmic contact layer (101e).

2. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 1, characterized in that: The power generation unit (100) further comprises a first electrode (102) connected to the Schottky metal layer (101a) in each group of the power generation structure (101) through a wire, and a second electrode (103) connected to the ohmic contact layer (101e).

3. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 2, characterized in that: The thickness of the Schottky metal layer (101a) is 50-100 nm; The carbon-14 diamond film (101b) is a P-type diamond doped with boron, with a doping concentration of N A =10 14 cm -3 , thickness is 100~500nm; The P + The diamond film (101c) is a boron-doped P-type diamond with a doping concentration of N A =10 20 cm -3 , thickness is 1 to 2 μm; The diamond substrate (101d) is a type Ib diamond substrate with a thickness of 0.4 mm; The ohmic contact layer (101e) uses a Ti / Au alloy electrode with thicknesses of 50nm and 80nm respectively.

4. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 3, characterized in that: It also includes an energy storage unit (200), which includes no less than one graphene supercapacitor (201), wherein the first electrode (102) is connected to the negative electrode of the graphene supercapacitor (201), and the second electrode (103) is connected to the positive electrode of the graphene supercapacitor (201).

5. A method for manufacturing a carbon-14 diamond-based beta radiation voltaic effect nuclear battery as claimed in any one of claims 1 to 4, characterized in that: The steps include: Using type Ib diamond as substrate, P + Type diamond film (101c); After the growth of P + On the type diamond film (101c), a carbon-14 diamond film (101b) is homoepitaxially grown by microwave plasma vapor deposition to form a diamond epitaxial wafer; Cleaning the prepared diamond epitaxial wafer; Then it is treated with an acid solution to form an oxygen terminal surface, and then cleaned and dried; A Schottky electrode is prepared on the surface of a carbon-14 diamond film (101b) of a diamond epitaxial wafer; An ohmic contact electrode is prepared on a side of the diamond epitaxial wafer away from the carbon-14 diamond film (101b); Cutting the diamond epitaxial wafer assembly and welding wires at the Schottky electrode and the ohmic contact electrode; The wires are connected to the positive electrode and the negative electrode of the graphene supercapacitor (201) respectively, and a plurality of groups of diamond epitaxial wafer assemblies are arranged on the periphery of the graphene supercapacitor (201).

6. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 5, characterized in that: The microwave plasma vapor deposition homoepitaxially grows P + type diamond film (101c), using CH4, TMB and H2 as reaction gases, CH4 gas flow rate 5sccm, TMB gas flow rate 5sccm, H2 gas flow rate 500sccm, substrate temperature 950°C, gas pressure 1000Pa, microwave power 4kW, and growth time 5h.

7. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 6, characterized in that: The carbon-14 diamond film (101b) is homoepitaxially grown by microwave plasma vapor deposition. 14 CH4, TMB, H2 are used as reaction gases. 14 CH4 gas flow rate is 5 sccm, H2 gas flow rate is 500 sccm, substrate temperature is 900°C, TMB gas flow rate is 3 sccm, gas pressure is 1000 Pa, microwave power is 4 kW, and growth time is 2 h.

8. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 7, characterized in that: The cleaning treatment of the prepared diamond epitaxial wafer includes ultrasonic cleaning with methanol, acetone and ethanol for 15 minutes respectively, and then rinsing with deionized water; The acid solution treatment includes placing the diamond epitaxial wafer in a mixture of 300° C. sulfuric acid and nitric acid (volume mixing ratio 1:1) for 3 hours to remove the hydrogen terminal surface conductive layer.

9. The beta radiation voltaic effect nuclear battery based on carbon-14 diamond according to claim 8, characterized in that: The Schottky electrode is prepared on the surface of the carbon-14 diamond film (101b) of the diamond epitaxial wafer, and the Schottky contact metal Ni is sputtered by a magnetron sputtering process, and the sputtering pressure is 10 -7 Pa and annealed at 500 °C in nitrogen for 1 h.

10. The carbon-14 diamond-based beta radiation voltaic effect nuclear battery according to claim 9, characterized in that: The ohmic contact electrode is prepared on the side of the diamond epitaxial wafer away from the carbon-14 diamond film (101b), and the ohmic contact metal Ti and metal Au are sputtered in sequence by a magnetron sputtering process, followed by annealing at 700°C in nitrogen for 1 hour.

Citation Information

Cited By

  • Magnetic suspension heart pump system based on nuclear battery energy supply and control method thereof

    CN120022526A