Optimization method of multi-chip dispensing mode

By adopting multi-chip dispensing method in semiconductor packaging, the bottom filling process is omitted and through-silicon holes are filled with metal materials, the problem of gaps between holes and bumps caused by poor material fluidity in traditional packaging processes is solved, and the reliability of the product is improved and yield.

CN119028910APending Publication Date: 2024-11-26HUATIAN TECHNOLOGY (KUNSHAN) ELECTRONICS CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411158510.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In traditional packaging processes, the bottom filler material of the capillary tube has poor fluidity, which makes it difficult to fully fill the chip bottom, which can easily cause voids, especially in the layer gap of high-bandwidth memory, affecting product yield.

Method used

Multi-chip dispensing method is adopted, including preparing a rewiring structure on the wafer, connecting functional chips, forming a plastic seal, grinding and thinning, opening through-silicon holes and filling metal materials, forming a metal conductive structure, omitting the bottom filling process, and customizing it Dispensing method to make up for the shortcomings of insufficient flow capacity.

Benefits of technology

It improves the reliability and yield of the product, reduces the bottom filling process, and improves the offset problem between bumps. It has simple process and low cost, which is suitable for industrial promotion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028910A_ABST
    Figure CN119028910A_ABST
Patent Text Reader

Abstract

The invention discloses an optimization method of a multi-chip dispensing mode. The optimization method comprises the following steps: step 1, preparing a rewiring structure on a wafer; 2, connecting a functional chip on the rewiring structure; 3, packaging the functional chip to form a plastic package body; 4, grinding and thinning the plastic package body until the functional chip is exposed; 5, forming a silicon through hole in one surface, far away from the functional chip, of the wafer; 6, filling the silicon through hole with a metal material; and 7, wiring on one surface, far away from the functional chip, of the wafer to form a metal conductive structure. According to the optimization method for the multi-chip dispensing mode, the bottom filling process can be omitted, the dispensing mode can be self-defined according to the arrangement mode of the chips, the defect caused by the limited flowing capacity of a plastic packaging material can be overcome, the bottom cavity phenomenon and the problem of offset between bumps can be solved, the product yield can be improved, the overall process is simple, the cost is low, and the method is suitable for large-scale popularization and application. And the method is low in cost and suitable for industrial popularization and application.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of semiconductor packaging, and in particular relates to an optimization method for a multi-chip glue dispensing mode. Background Art

[0002] As the micro-interconnection pitch decreases, the packaging structure becomes more and more complex, and the spacing range of the stacked interconnections between chips is gradually shrinking. The traditional packaging process requires bottom filling and then curing to protect the chip, but the fluidity of the traditional capillary bottom filling material is poor, which reduces the reliability of the product. The current plastic encapsulation MUF method and center dispensing method are not conducive to flowing into the bottom of each chip, which is easy to cause voids, especially the gap between each layer of DRAM (Dynamic Random Access Memory) of the stacked HBM (High Bandwidth Memory), which is easy to cause offset between bumps and affect the yield. Summary of the invention

[0003] In order to solve the technical problems existing in the prior art, the purpose of the present invention is to provide an optimization method for multi-chip dispensing.

[0004] In order to achieve the above purpose and the above technical effect, the technical solution adopted by the present invention is:

[0005] A method for optimizing a multi-chip dispensing method comprises the following steps:

[0006] Step 1: preparing a redistribution structure on a wafer;

[0007] Step 2: Connecting the functional chip to the rewiring structure;

[0008] Step 3: Encapsulate the functional chip to form a plastic package;

[0009] Step 4: Grind and thin the plastic package until the functional chip is exposed;

[0010] Step 5: Opening a through silicon via on the side of the wafer away from the functional chip;

[0011] Step 6: Filling the through silicon via with metal material;

[0012] Step 7: Conduct wiring on the side of the wafer away from the functional chip to form a metal conductive structure.

[0013] Furthermore, in step one, the surface of the redistribution structure has a conductive structure, and the conductive structure is made of Cu, Ni, Sn or Ag.

[0014] Furthermore, in step 2, the types of the functional chips are at least two and the number is at least two, and the functional chips are bonded to the rewiring structure by flip chip bonding technology.

[0015] Furthermore, the functional chip includes at least one functional chip I and at least one functional chip II, and the functional chip I and the functional chip II are respectively bonded to the conductive structure of the rewiring structure by flip chip bonding technology.

[0016] Furthermore, non-electrical chips are mounted on both sides of the functional chip II on the rewiring structure to improve the warping.

[0017] Furthermore, in step three, the plastic sealing body is formed by dispensing glue on a plurality of plastic sealing units according to a certain pattern.

[0018] Furthermore, the plastic package body is made by the following steps:

[0019] First, add plastic sealing material to the same outer side of the plastic sealing units in the first row, then add plastic sealing material between the same inner side of the plastic sealing units in the first row and the same outer side of the plastic sealing units in the second row, then add plastic sealing material between the same inner side of the plastic sealing units in the second row and the same outer side of the plastic sealing units in the third row, and then add plastic sealing material between the same inner side of the plastic sealing units in the third row and the same outer side of the plastic sealing units in the fourth row. Repeat this cycle to complete the dispensing work, and then perform plastic sealing to form a plastic sealing body.

[0020] Furthermore, the plastic package body is made by the following steps:

[0021] First, add plastic sealing material to the outer side of the first plastic sealing unit in the first row, then add plastic sealing material to the inner side of the second plastic sealing unit in the first row, and then add plastic sealing material to the outer side of the third plastic sealing unit in the first row, and repeat this cycle to complete the plastic sealing work of the first row in a wave-like manner. Then enter the second row and add plastic sealing material to the outer side and inner side of the plastic sealing units in the adjacent second row in turn, and then add plastic sealing material to the outer side of the next plastic sealing unit in the second row, and repeat this cycle to complete the plastic sealing work of the second row in a wave-like manner. In this cycle, the dispensing work is completed, and then plastic sealing is carried out to form a plastic sealing body.

[0022] Furthermore, the plastic package body is made by the following steps:

[0023] According to the placement order, first complete the plastic sealing work of all chips in the previous row in a wave shape, then enter the next row and complete the plastic sealing work of all chips in the next row in a wave shape, and repeat this cycle to complete the dispensing work, and then perform plastic sealing to form a plastic sealing body.

[0024] Furthermore, in step five, a through silicon via is formed on the side of the wafer away from the functional chip through a silicon etching process, and then a metal layer is sputtered on the inner wall of the through silicon via and the surface of the wafer to achieve signal interconnection.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] The present invention discloses an optimization method for a multi-chip dispensing method, comprising the following steps: step one: preparing a rewiring structure on a wafer; step two: connecting a functional chip on the rewiring structure; step three: encapsulating the functional chip to form a plastic package; step four: grinding and thinning the plastic package until the functional chip is exposed; step five: opening a through silicon via on the side of the wafer away from the functional chip; step six: filling the through silicon via with a metal material; step seven: wiring on the side of the wafer away from the functional chip to form a metal conductive structure. The optimization method for the multi-chip dispensing method provided by the present invention can omit the bottom filling process, and can customize the dispensing method according to the arrangement of the chips, can make up for the defects caused by the limited flow capacity of the plastic package material, and can also improve the bottom void phenomenon and the problem of offset between bumps, which is conducive to improving the product yield, the overall process is simple, the cost is low, and it is suitable for industrial promotion and use. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 It is a structural schematic diagram of step 1 of the present invention;

[0028] Figure 2 This is a schematic diagram of the structure of step 2 of embodiment 1 of the present invention;

[0029] Figure 3 This is a schematic diagram of the structure of step three of embodiment 1 of the present invention;

[0030] Figure 4 This is a schematic diagram of the structure of step 4 of embodiment 1 of the present invention;

[0031] Figure 5 This is a schematic diagram of the structure of step 5 of embodiment 1 of the present invention;

[0032] Figure 6 This is a schematic diagram of the structure of step six of embodiment 1 of the present invention;

[0033] Figure 7 This is a schematic diagram of the structure of step seven of embodiment 1 of the present invention;

[0034] Figure 8-9 They are respectively structural schematic diagrams of step 2 of embodiment 2 of the present invention;

[0035] Fig.10 This is a schematic diagram of the structure of step 3 of embodiment 2 of the present invention;

[0036] Fig.11 This is a schematic diagram of the structure of step 3 of embodiment 3 of the present invention;

[0037] Fig.12 This is a schematic diagram of the structure of step 3 of embodiment 4 of the present invention;

[0038] Fig.13 It is a structural schematic diagram of step three of the prior art;

[0039] Figure 14-15 They are respectively structural schematic diagrams of step 3 of embodiment 5 of the present invention;

[0040] Fig.16 Schematic diagram of the structure forming a cavity between bumps. DETAILED DESCRIPTION

[0041] The present invention is described in detail below so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.

[0042] A brief summary of one or more aspects is given below to provide a basic understanding of these aspects. This summary is not an exhaustive overview of all conceived aspects, and is neither intended to identify the key or critical elements of all aspects nor to define the scope of any or all aspects. Its only purpose is to give some concepts of one or more aspects in a simplified form as a prelude to a more detailed description that will be given later.

[0043] Example 1

[0044] like Figure 1-7 As shown, a method for optimizing a multi-chip dispensing method includes the following steps:

[0045] Step 1: If Figure 1 As shown, a rewiring structure 2 is prepared on the surface of a wafer 1 by conventional processes such as yellow light, electroplating, and PVD, and then a conductive structure 201 is formed on the surface of the rewiring structure 2. The rewiring structure 2 can be two or more layers, usually copper lines. The rewiring structure 2 is formed in a passivation layer, and the passivation layer can be a solid dry film or PI glue.

[0046] Step 2: If Figure 2As shown, at least one functional chip I3 and at least one functional chip II4 are connected to the rewiring structure 2. Specifically, the functional chip I3 and the functional chip II4 are respectively bonded to the conductive structure 201 of the rewiring structure 2 by flip-chip bonding technology, and then the wafer reconstruction is achieved by thermal reflow. Due to the large number of blank areas, it is possible to choose to mount a non-electrical chip 5 on both sides of the rewiring structure 2 and the functional chip II4 to effectively improve the warping phenomenon. The non-electrical chip 5 may be added or not;

[0047] Step 3: If Figure 3 As shown, the functional chip I3 and the functional chip II4 are packaged through the plastic packaging MUF process to form a plastic packaging body 6, which protects the chip and supports the entire reconstructed wafer; Fig.13 Schematic diagram of the central dispensing method in the prior art. This method has the problem of uneven distribution of the surface of the plastic packaging material, which may cause voids when the bump pitch is small. To solve this problem, the following steps are used in this embodiment to form the plastic packaging body 6:

[0048] According to the placement order, firstly complete the plastic sealing work of all chips in the previous row in a wave-like manner, then enter the next row and complete the plastic sealing work of all chips in the next row in a wave-like manner, and repeat this cycle to complete all the dispensing work, and then perform plastic sealing to form a plastic sealing body 6. This method makes the plastic sealing material evenly distributed on the surface of the wafer, which is more conducive to automatically flowing into the bump structure, which can not only reduce the bottom filling process, but also ensure product reliability and improve product yield;

[0049] Step 4: If Figure 4 As shown, the plastic package body 6 is ground and thinned until the functional chip I3 and the functional chip II4 are exposed, which is beneficial to improving the heat dissipation effect of the chip;

[0050] Step 5: If Figure 5 As shown, a through silicon via 7 is formed on a side of the wafer 1 away from the functional chip I3 and the functional chip II4 through a silicon etching process, and then a metal layer 701 is sputtered on the inner wall of the through silicon via 7 and the surface of the wafer 1 to realize signal interconnection;

[0051] Step 6: If Figure 6 As shown, the through silicon via 7 is filled with metal copper material through an electroplating process, and the metal copper on the surface can be removed by wet etching or chemical mechanical polishing (CMP);

[0052] Step 7: If Figure 7As shown, through magnetron sputtering process, photolithography process and electroplating process, wiring is performed on the side of wafer 1 away from functional chip Ⅰ3 and functional chip Ⅱ4, and a metal conductive structure is formed at the position of the metal pad formed in the last layer, and the component of the metal conductive structure is Sn.

[0053] The rest is the same as in Example 1.

[0054] Example 2

[0055] like Figure 1 , Figure 8-10 As shown, a method for optimizing a multi-chip dispensing method includes the following steps:

[0056] Step 1: If Figure 1 As shown, a rewiring structure 2 is prepared on the surface of the wafer 1 by conventional processes such as yellow light, electroplating, and PVD, and then a conductive structure 201 is formed on the surface of the rewiring structure 2. The rewiring structure 2 has two layers.

[0057] Step 2: If Figure 8-9 As shown, at least one functional chip I3 and at least one functional chip II4 are connected to the rewiring structure 2. Specifically, the functional chip I3 and the functional chip II4 are respectively bonded to the conductive structure 201 of the rewiring structure 2 by flip-chip bonding technology, and then the wafer is reconstructed by thermal reflow. Due to the large number of blank areas, this embodiment specifically mounts non-electrical chips 5 on both sides of the rewiring structure 2 and the functional chip II4 to effectively improve the warping phenomenon;

[0058] Step 3: If Fig.10 As shown, the functional chip I3 and the functional chip II4 are packaged through the plastic packaging MUF process to form a plastic packaging body 6, which protects the chip and supports the entire reconstructed wafer;

[0059] Fig.13 Schematic diagram of the central dispensing method in the prior art. This method has the problem of uneven distribution of the surface of the plastic packaging material, which may cause voids when the bump pitch is small. To solve this problem, the following steps are used in this embodiment to form the plastic packaging body 6:

[0060] First, plastic molding compound is added to the same outer side of the plastic molding units in the first row, and then plastic molding compound is added between the same inner side of the plastic molding units in the first row and the same outer side of the plastic molding units in the second row, and then plastic molding compound is added between the same inner side of the plastic molding units in the second row and the same outer side of the plastic molding units in the third row, and then plastic molding compound is added between the same inner side of the plastic molding units in the third row and the same outer side of the plastic molding units in the fourth row, and this cycle is repeated to complete the dispensing work, and then plastic molding is performed to form a plastic molding body 6. This method makes the plastic molding compound evenly distributed on the surface of the wafer, which is more conducive to automatically flowing into the bump structure, which can not only reduce the bottom filling process, but also ensure product reliability and improve product yield;

[0061] Step 4: Grind and thin the plastic package 6 until the functional chip I3 and the functional chip II4 are exposed, which is beneficial to improve the heat dissipation effect of the chip;

[0062] Step 5: Through silicon via 7 is formed on the side of wafer 1 away from functional chip I3 and functional chip II4 by silicon etching process, and then a metal layer 701 is sputtered on the inner wall of through silicon via 7 and the surface of wafer 1 to realize signal interconnection;

[0063] Step 6: Fill the through silicon via 7 with metal copper material through an electroplating process, and the metal copper on the surface can be removed by a wet etching method;

[0064] Step 7: Through magnetron sputtering, photolithography and electroplating processes, wiring is performed on the side of the wafer 1 away from the functional chip I3 and the functional chip II4, and a metal conductive structure is formed at the position of the metal pad formed in the last layer, and the composition of the metal conductive structure is Sn.

[0065] The rest is the same as in Example 1.

[0066] Example 3

[0067] like Figure 1 , 8 , 9, and 11, a method for optimizing a multi-chip dispensing method comprises the following steps:

[0068] Step 1: If Figure 1 As shown, a rewiring structure 2 is prepared on the surface of the wafer 1 by conventional processes such as yellow light, electroplating, and PVD, and then a conductive structure 201 is formed on the surface of the rewiring structure 2. The rewiring structure 2 has two layers.

[0069] Step 2: If Figure 8-9As shown, at least one functional chip I3 and at least one functional chip II4 are connected to the rewiring structure 2. Specifically, the functional chip I3 and the functional chip II4 are respectively bonded to the conductive structure 201 of the rewiring structure 2 by flip-chip bonding technology, and then the wafer is reconstructed by thermal reflow. Due to the large number of blank areas, this embodiment specifically mounts non-electrical chips 5 on both sides of the rewiring structure 2 and the functional chip II4 to effectively improve the warping phenomenon;

[0070] Step 3: If Fig.11 As shown, the functional chip I3 and the functional chip II4 are packaged through the plastic packaging MUF process to form a plastic packaging body 6, which protects the chip and supports the entire reconstructed wafer; Fig.13 Schematic diagram of the central dispensing method in the prior art. This method has the problem of uneven distribution of the surface of the plastic packaging material, which may cause voids when the bump pitch is small. To solve this problem, the following steps are used in this embodiment to form the plastic packaging body 6:

[0071] First, plastic sealing material is added to the outer side of the first plastic sealing unit in the first row, and then plastic sealing material is added to the inner side of the second plastic sealing unit in the first row, and then plastic sealing material is added to the outer side of the third plastic sealing unit in the first row, and this cycle is repeated to complete the plastic sealing work of the first row in a wave-like manner, and then the second row is entered and plastic sealing material is added to the outer side and inner side of the adjacent plastic sealing unit in the second row in turn, and then plastic sealing material is added to the outer side of the next plastic sealing unit in the second row, and this cycle is repeated to complete the plastic sealing work of the second row in a wave-like manner, and this cycle is repeated to complete the dispensing work, and then plastic sealing is performed to form a plastic sealing body 6. This method makes the plastic sealing material evenly distributed on the surface of the wafer, which is more conducive to automatically flowing into the bump structure, which can not only reduce the bottom filling process, but also ensure product reliability and improve product yield;

[0072] Step 4: Grind and thin the plastic package 6 until the functional chip I3 and the functional chip II4 are exposed, which is beneficial to improve the heat dissipation effect of the chip;

[0073] Step 5: Through silicon via 7 is formed on the side of wafer 1 away from functional chip I3 and functional chip II4 by silicon etching process, and then a metal layer 701 is sputtered on the inner wall of through silicon via 7 and the surface of wafer 1 to realize signal interconnection;

[0074] Step 6: Fill the through silicon via 7 with metal copper material through an electroplating process, and the metal copper on the surface can be removed by a wet etching method;

[0075] Step 7: Through magnetron sputtering, photolithography and electroplating processes, wiring is performed on the side of the wafer 1 away from the functional chip I3 and the functional chip II4, and a metal conductive structure is formed at the position of the metal pad formed in the last layer, and the composition of the metal conductive structure is Sn.

[0076] The rest is the same as in Example 1.

[0077] Example 4

[0078] like Figure 1 , 8 , 9, and 12, a method for optimizing a multi-chip dispensing method comprises the following steps:

[0079] Step 1: If Figure 1 As shown, a rewiring structure 2 is prepared on the surface of the wafer 1 by conventional processes such as yellow light, electroplating, and PVD, and then a conductive structure 201 is formed on the surface of the rewiring structure 2. The rewiring structure 2 has two layers.

[0080] Step 2: If Figure 8-9 As shown, at least one functional chip I3 and at least one functional chip II4 are connected to the rewiring structure 2. Specifically, the functional chip I3 and the functional chip II4 are respectively bonded to the conductive structure 201 of the rewiring structure 2 by flip-chip bonding technology, and then the wafer is reconstructed by thermal reflow. Due to the large number of blank areas, this embodiment specifically mounts non-electrical chips 5 on both sides of the rewiring structure 2 and the functional chip II4 to effectively improve the warping phenomenon;

[0081] Step 3: If Fig.12 As shown, the functional chip I3 and the functional chip II4 are packaged through the plastic packaging MUF process to form a plastic packaging body 6, which protects the chip and supports the entire reconstructed wafer; Fig.13 Schematic diagram of the central dispensing method in the prior art. This method has the problem of uneven distribution of the surface of the plastic packaging material, which may cause voids when the bump pitch is small. To solve this problem, the following steps are used in this embodiment to form the plastic packaging body 6:

[0082] According to the placement order, firstly complete the plastic sealing work of all the chips in the previous row in a wave-like manner, then enter the next row and complete the plastic sealing work of all the chips in the next row in a wave-like manner, and repeat this cycle to complete the dispensing work, and then perform plastic sealing to form a plastic sealing body 6. This method makes the plastic sealing material evenly distributed on the surface of the wafer, which is more conducive to automatically flowing into the bump structure, which can not only reduce the bottom filling process, but also ensure product reliability and improve product yield;

[0083] Step 4: Grind and thin the plastic package 6 until the functional chip I3 and the functional chip II4 are exposed, which is beneficial to improve the heat dissipation effect of the chip;

[0084] Step 5: Through silicon via 7 is formed on the side of wafer 1 away from functional chip I3 and functional chip II4 by silicon etching process, and then a metal layer 701 is sputtered on the inner wall of through silicon via 7 and the surface of wafer 1 to realize signal interconnection;

[0085] Step 6: Fill the through silicon via 7 with metal copper material through an electroplating process, and the metal copper on the surface can be removed by a wet etching method;

[0086] Step 7: Through magnetron sputtering, photolithography and electroplating processes, wiring is performed on the side of the wafer 1 away from the functional chip I3 and the functional chip II4, and a metal conductive structure is formed at the position of the metal pad formed in the last layer, and the composition of the metal conductive structure is Sn.

[0087] The rest is the same as in Example 1.

[0088] Example 5

[0089] The difference between this embodiment and embodiment 1 is that in step 3, this embodiment adopts a surrounding convection dispensing method to form the plastic package 6. Fig.14 As shown in FIG. 1 , the plastic encapsulation material flows into between each layer of DRAM of HBM, such as Fig.15 As shown in the figure, this method can effectively reduce the offset between DRAMs and increase product yield. The test found that if glue is not dispensed between the gaps before molding, voids may form between the bumps, such as Fig.16 As shown, therefore, this embodiment requires dispensing glue between the gaps before molding.

[0090] The rest is the same as in Example 1.

[0091] Parts or structures not specifically described in the present invention may adopt existing technologies or existing products and will not be described in detail here.

[0092] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for optimizing a multi-chip dispensing method, characterized in that: The following steps are involved: Step 1: preparing a redistribution structure on a wafer; Step 2: Connecting the functional chip to the rewiring structure; Step 3: Encapsulate the functional chip to form a plastic package; Step 4: Grind and thin the plastic package until the functional chip is exposed; Step 5: Opening a through silicon via on the side of the wafer away from the functional chip; Step 6: Filling the through silicon via with metal material; Step 7: Conduct wiring on the side of the wafer away from the functional chip to form a metal conductive structure.

2. The optimization method of a multi-chip dispensing method according to claim 1, characterized in that: In step 1, the surface of the redistribution structure has a conductive structure, and the conductive structure is made of Cu, Ni, Sn or Ag.

3. The optimization method of a multi-chip dispensing method according to claim 1, characterized in that: In step 2, there are at least two types of functional chips and at least two functional chips in number, and the functional chips are bonded to the redistribution structure by flip chip bonding technology.

4. The optimization method of a multi-chip dispensing method according to claim 3, characterized in that: The functional chip includes at least one functional chip I and at least one functional chip II, and the functional chip I and the functional chip II are respectively bonded to the conductive structure of the rewiring structure by flip chip bonding technology.

5. The optimization method for multi-chip dispensing method according to claim 4, characterized in that: Non-electrical chips are also mounted on the rewiring structure and on both sides of the functional chip II to improve the warping.

6. The optimization method for multi-chip dispensing method according to claim 1, characterized in that: In step three, the plastic encapsulation body is formed by dispensing glue on a plurality of plastic encapsulation units according to a certain pattern.

7. The optimization method for multi-chip dispensing according to claim 6, characterized in that: The plastic package body is made by the following steps: First, add plastic sealing material to the same outer side of the plastic sealing units in the first row, then add plastic sealing material between the same inner side of the plastic sealing units in the first row and the same outer side of the plastic sealing units in the second row, then add plastic sealing material between the same inner side of the plastic sealing units in the second row and the same outer side of the plastic sealing units in the third row, and then add plastic sealing material between the same inner side of the plastic sealing units in the third row and the same outer side of the plastic sealing units in the fourth row. Repeat this cycle to complete the dispensing work, and then perform plastic sealing to form a plastic sealing body.

8. The optimization method for multi-chip dispensing method according to claim 6, characterized in that: The plastic package body is made by the following steps: First, add plastic sealing material to the outer side of the first plastic sealing unit in the first row, then add plastic sealing material to the inner side of the second plastic sealing unit in the first row, and then add plastic sealing material to the outer side of the third plastic sealing unit in the first row, and repeat this cycle to complete the plastic sealing work of the first row in a wave-like manner. Then enter the second row and add plastic sealing material to the outer side and inner side of the plastic sealing units in the adjacent second row in turn, and then add plastic sealing material to the outer side of the next plastic sealing unit in the second row, and repeat this cycle to complete the plastic sealing work of the second row in a wave-like manner. In this cycle, the dispensing work is completed, and then plastic sealing is carried out to form a plastic sealing body.

9. The optimization method for multi-chip dispensing according to claim 6, characterized in that: The plastic package body is made by the following steps: According to the placement order, first complete the plastic sealing work of all chips in the previous row in a wave shape, then enter the next row and complete the plastic sealing work of all chips in the next row in a wave shape, and repeat this cycle to complete the dispensing work, and then perform plastic sealing to form a plastic sealing body.

10. The optimization method for multi-chip dispensing method according to claim 1, characterized in that: In step five, a through silicon via is formed on the side of the wafer away from the functional chip through a silicon etching process, and then a metal layer is sputtered on the inner wall of the through silicon via and the surface of the wafer to achieve signal interconnection.

Citation Information

Cited By

  • Multi-chip flip chip ball grid array packaging method and packaging structure

    CN120834017A