Preparation method of semiconductor device and semiconductor device

By forming an anti-permeable film on the side walls of the signal line contact groove, the performance problems of semiconductor devices caused by alignment errors during etching are solved, the preparation yield and performance are improved, and the cost is reduced.

CN119028912APending Publication Date: 2024-11-26CHENGDU HIGH-TECH JIN SCI&TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411113932.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In memory semiconductor manufacturing process, the difference in the shape and position of the accommodation groove caused by poor control of dislocation and etching amount during the etching process affects the performance and yield of the semiconductor device.

Method used

在信号线接触槽的侧壁形成防渗透膜,防止掺杂离子渗透并覆盖预设有源区,避免信号线接触结构与相邻有源区接触,防止离子扩散,从而提升制备精度和性能。

Benefits of technology

It improves the production yield and performance of semiconductor devices, reduces the production cost, and simplifies the etching accuracy requirements of signal line contact slots.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028912A_ABST
    Figure CN119028912A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a semiconductor device and the semiconductor device, and the preparation method of the semiconductor device comprises the steps: providing a substrate, forming isolation structures on the substrate, and forming an active region between the adjacent isolation structures; forming a hard mask layer on the surface of one side of the substrate, and patterning the hard mask layer to form a through hole exposing part of the active region; forming a signal line contact groove in the active region exposed by the through hole, wherein the signal line contact groove is communicated with the through hole; an anti-osmosis membrane is formed on the side wall of the signal line contact groove; a signal line contact structure is formed, and at least part of the signal line contact structure is located in the signal line contact groove. According to the preparation method of the semiconductor device, the preparation yield of the semiconductor device can be improved, and the yield and the performance of the semiconductor device are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of semiconductor technology, and in particular, relates to a method for preparing a semiconductor device and a semiconductor device. Background Art

[0002] In the memory semiconductor manufacturing process, the semiconductor substrate includes multiple active areas and isolation areas for isolating the active areas. A receiving groove for a contact structure for connecting a data line needs to be formed above some of the active areas. The receiving groove is formed by an etching process. Due to misalignment during the etching process and poor control of the etching amount of the etching process, the shape and position of the formed receiving groove are easily different from the ideal state, which makes the prepared semiconductor device prone to defects, seriously affecting the performance of the semiconductor device. Summary of the invention

[0003] The purpose of the present application is to at least solve the problem of low yield of semiconductor devices caused by the preparation method of semiconductor devices. This purpose is achieved through the following technical solutions:

[0004] The first aspect of the present application provides a method for preparing a semiconductor device, comprising:

[0005] Providing a substrate, and forming an isolation structure on the substrate, and forming an active region between adjacent isolation structures;

[0006] forming a hard mask layer on a surface of one side of the substrate, and patterning the hard mask layer to form a through hole exposing a portion of the active area;

[0007] forming a signal line contact groove in the active area exposed by the through hole, wherein the signal line contact groove is connected to the through hole;

[0008] forming an anti-permeability film on the sidewall of the signal line contact groove;

[0009] A signal line contact structure is formed, wherein the signal line contact structure is at least partially located in the signal line contact groove.

[0010] In the preparation method of the semiconductor device provided in the present application, an anti-penetration film is formed on the side wall of the signal line contact groove, so that in the subsequent preparation process, the doped ions can be prevented from penetrating into the active area adjacent to the preset active area. After the isolation structure is over-etched due to the limitation of the preparation process accuracy, thereby exposing the active area adjacent to the preset active area, the surface of the active area adjacent to the preset active area facing the signal line contact groove can be covered by forming an anti-penetration film to prevent the signal line contact structure in the signal line contact groove from contacting the adjacent active area, and to prevent the ions in the process of forming the signal line contact structure from diffusing into the adjacent active area, thereby improving the preparation yield of the semiconductor device and improving the yield and performance of the semiconductor device.

[0011] The second aspect of the present application also provides a semiconductor device, characterized in that it is prepared by the semiconductor device preparation method provided by the first aspect of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present application. Moreover, the same reference numerals are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0013] Figure 1 It is a schematic diagram of an ideal state of a semiconductor device in the preparation process in the prior art;

[0014] Figure 2 It is a partial schematic diagram of a semiconductor device in the prior art during the preparation process;

[0015] Figure 3 A flow chart of a method for preparing a semiconductor device provided in an embodiment of the present application;

[0016] Figure 4 It is a structural schematic diagram of a semiconductor device during the preparation process provided by an embodiment of the present application;

[0017] Figure 5 yes Figure 4 A magnified image of area A;

[0018] Figure 6 It is a schematic diagram of a local structure of a semiconductor device during the preparation process provided by an embodiment of the present application;

[0019] Figure 7 It is a schematic diagram of a local structure of a semiconductor device during the preparation process provided by an embodiment of the present application;

[0020] Figure 8 It is a structural schematic diagram of a semiconductor device during the preparation process provided in an embodiment of the present application.

[0021] The reference numerals are as follows:

[0022] 1. Substrate; 11. Active area; 2. Isolation structure; 21. Isolation groove; 22. Isolation material; 3. Hard mask layer; 31. Through hole; 4. Signal line contact groove; 5. Anti-penetration membrane; 6. Oxide layer; 7. Mask layer; 01. Semiconductor substrate; 02. Active area; 03. Isolation area; 04. Receiving groove. DETAILED DESCRIPTION

[0023] The exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.

[0024] It should be understood that the terms used herein are only for the purpose of describing specific example embodiments and are not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms "one", "an" and "said" as used herein may also be meant to include plural forms. The terms "include", "comprise", "contain", and "have" are inclusive, and therefore specify the existence of stated features, steps, operations, elements and / or parts, but do not exclude the existence or addition of one or more other features, steps, operations, elements, parts, and / or combinations thereof. The method steps, processes, and operations described herein are not interpreted as necessarily requiring them to be performed in the specific order described or illustrated, unless the execution order is clearly indicated. It should also be understood that additional or alternative steps may be used.

[0025] Although the terms first, second, third, etc. can be used in the text to describe multiple elements, components, regions, layers and / or sections, these elements, components, regions, layers and / or sections should not be limited by these terms. These terms can only be used to distinguish an element, component, region, layer or section from another region, layer or section. Unless the context clearly indicates, terms such as "first", "second" and other numerical terms do not imply order or sequence when used in the text. Therefore, the first element, component, region, layer or section discussed below can be referred to as the second element, component, region, layer or section without departing from the teaching of the example embodiments.

[0026] For ease of description, spatial relative terms may be used herein to describe the relationship of one element or feature relative to another element or feature as shown in the figure, such as "inside", "outside", "inner side", "outer side", "below", "below", "above", "above", etc. Such spatial relative terms are intended to include different orientations of the device in use or operation in addition to the orientation depicted in the figure. For example, if the device in the figure is turned over, then the elements described as "below other elements or features" or "below other elements or features" will subsequently be oriented as "above other elements or features" or "above other elements or features". Therefore, the example term "below..." can include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or in other directions) and the spatial relative descriptors used in the text are interpreted accordingly.

[0027] The research found that Figure 1 and Figure 2 As shown, in the memory semiconductor manufacturing process, the semiconductor substrate 01 includes a plurality of active regions 02 and an isolation region 03 for isolating the active regions 02. A receiving groove 04 for connecting a contact structure of a data line needs to be formed above some of the active regions 02. The contact structure is located in the receiving groove 04 and contacts the active region 02 below. The receiving groove 04 is formed by an etching process. Due to the misalignment during the etching process and the poor control of the etching amount of the etching process, the shape and position of the formed receiving groove 04 are easily different from the ideal state. Figure 1 As shown, in an ideal state, the center of the receiving groove 04 should coincide with the center of the active area 02 below, so that in an ideal shape, only the remaining isolation portion will be etched, and the isolation area 03 will not be overetched in a direction perpendicular to the thickness of the semiconductor substrate 01. In an ideal state, the etching amount should be precisely controlled so that the thickness of the remaining portion of the isolation structure 2 is a preset value, for example, a is 0.77nm. When the etching amount is not well controlled and the etching amount is large, the isolation area 03 will also be overetched in a direction perpendicular to the thickness of the semiconductor substrate 01. That is, when there is a deviation in the alignment or the etching amount is large, such as Figure 2As shown, it is easy to cause over-etching of the isolation region 03 in a direction perpendicular to the thickness of the semiconductor substrate 01, thereby exposing the adjacent active region 02. In the subsequent contact structure preparation process, the doping ions of the contact structure are easy to diffuse into the adjacent active region 02, so that the prepared semiconductor device is prone to defects, which seriously affects the performance of the semiconductor device. In order to improve the above-mentioned defects, the related technology adopts methods such as improving the alignment accuracy and reducing the alignment error when etching to form the receiving groove 04, and cutting the cross section after the etching process to check whether the size of the receiving groove 04 is in an ideal state, so as to more accurately manage the size of the receiving groove 04 in the subsequent preparation process to prevent the adjacent active region 02 from being exposed, but on the one hand, the effect is not ideal, and on the other hand, it will cause an increase in the preparation cost. Based on the above problems, the present application provides a method for preparing a semiconductor device and a semiconductor device to improve the preparation accuracy of the semiconductor device.

[0028] like Figure 3 As shown, according to an embodiment of the present application, a method for preparing a semiconductor device is proposed, comprising:

[0029] S200, such as Figure 4 As shown, a substrate 1 is provided, and isolation structures 2 are formed on the substrate 1 , and active regions 11 are formed between adjacent isolation structures 2 .

[0030] Specifically, the substrate 1 includes a semiconductor material, and the semiconductor material may be silicon, germanium, a silicon-germanium alloy or gallium nitride.

[0031] Specifically, a plurality of isolation structures 2 are arranged at intervals, and the isolation structures 2 separate a plurality of active regions 11 in the substrate 1, and the isolation structures 2 are used to achieve isolation and insulation between adjacent active regions 11. The depth of the isolation structures 2 is less than the thickness of the substrate 1. The isolation structures 2 include insulating materials.

[0032] S400, such as Figure 4 As shown, a hard mask layer 3 is formed on one surface of the substrate 1 , and the hard mask layer 7 is patterned to form a through hole 31 exposing a portion of the active area 11 .

[0033] Specifically, the hard mask layer 3 may include multiple layers stacked, for example, four layers. The hard mask layer 7 is used as a mask when patterning the substrate 1, and can limit the position and shape of subsequent film layers. A through hole 31 is formed in the hard mask layer 3, and the through hole 31 penetrates the hard mask layer 3 along the thickness direction of the hard mask layer 3. The through hole 31 exposes part of the active area 11. The through hole 31 defines the position of the signal line contact groove 4 and the signal line contact structure. The substrate 1 can be patterned based on the patterned hard mask layer 3 to form the signal line contact groove 4. The signal line contact groove 4 exposes part of the active area 11, so that the active area 11 can be contacted with the signal line contact structure later.

[0034] S600, such as Figure 5 As shown, a signal line contact groove 4 is formed in the active area 11 exposed by the through hole 31 , and the signal line contact groove 4 is connected to the through hole 31 .

[0035] Specifically, the area of ​​the substrate 1 opposite to the through hole 31 is etched to form a signal line contact groove 4, which is connected to the through hole 31, so that the active area 11 is exposed for subsequent connection with the signal line contact structure.

[0036] S800, such as Figure 5 As shown, an anti-permeation film 5 is formed on the side wall of the signal line contact groove 4.

[0037] Specifically, the anti-permeation membrane 5 can prevent the doping ions from penetrating, that is, can block the doping ions.

[0038] S1000 , forming a signal line contact structure (not shown in the figure), wherein the signal line contact structure is at least partially located in the signal line contact groove 4 .

[0039] Specifically, the signal line contact structure may be a data line contact structure, which may be located in the signal line contact groove 4, or may be partially located in the signal line contact groove 4 and partially located in the through hole 31. The signal line contact structure contacts the active area 11 and is used to realize the connection between the signal line and the active area 11.

[0040] Specifically, the semiconductor device in the present application may be a memory semiconductor device.

[0041] The reading and writing function of data in the memory semiconductor device is the core function. The substrate 1 of the semiconductor device includes active components for controlling the reading and writing functions. The malfunction of the active components will cause the electrical characteristics of the active components to change, thereby affecting the yield of the semiconductor device. The active components include the above-mentioned active area 11.

[0042] The signal line contact groove 4, under ideal conditions, etches the portion of the preset active area 11 opposite to the through hole 31 and the portion of the isolation structure 2 on both sides of the preset active area 11, but the isolation structure 2 does not expose the active area 11 adjacent to the preset active area 11, so as to avoid adverse effects on the adjacent active area 11 when the signal line contact structure is subsequently formed. Limited by the process precision, in the process of preparing the signal line contact groove 4, due to the position of the through hole 31 and the alignment of the formation of the signal line contact groove 4 in the process of preparing by the etching process, the finally formed signal line contact groove 4 may over-etch the isolation structure 2, thereby exposing the active area 11 adjacent to the preset active area 11. When the signal line contact structure is subsequently formed, it will have an adverse effect on the active area 11 adjacent to the preset active area 11, thereby affecting the preparation yield of the semiconductor device. In the preparation method of the semiconductor device provided in the present application, by forming an anti-permeability film 5 on the side wall of the signal line contact groove 4, it is possible to prevent doped ions from penetrating into the active area 11 adjacent to the preset active area 11 in the subsequent preparation process. After the isolation structure 2 is over-etched due to the limitation of the preparation process accuracy, thereby exposing the active area 11 adjacent to the preset active area 11, the surface of the active area 11 adjacent to the preset active area 11 facing the signal line contact groove 4 can be covered by forming an anti-permeability film 5 to prevent the signal line contact structure in the signal line contact groove 4 from contacting the adjacent active area 11, and to prevent ions in the process of forming the signal line contact structure from diffusing into the adjacent active area 11, thereby improving the preparation yield of the semiconductor device and improving the yield and performance of the semiconductor device.

[0043] In the method for preparing a semiconductor device provided by the present application, improvements are made on the basis of the existing process, and the existing preparation process can be maintained, and only the preparation process of the anti-permeation membrane 5 is newly added, and the other preparation processes can continue to use the previous preparation processes, thereby reducing costs. In addition, the method for preparing a semiconductor device provided by the present application can reduce the requirements for the etching accuracy of the signal line contact groove 4, thereby helping to reduce the preparation cost.

[0044] In the method for preparing a semiconductor device provided in the present application, the anti-permeability film 5 can be removed in a subsequent preparation process, specifically, can be removed simultaneously with other film layers.

[0045] In a feasible implementation manner, step S800 includes:

[0046] S810, such as Figure 6 As shown, the signal line contact groove 4 penetrates the isolation structure 2 along a direction perpendicular to the thickness of the substrate 1 and exposes the active area 11 .

[0047] S820, such as Figure 6As shown, the sidewalls and bottom walls of the signal line contact groove 4 are processed by a rapid thermal oxidation process, so that the portion of the active area 11 exposed through the signal line contact groove 4 is oxidized to form an oxide layer 6 .

[0048] Specifically, when the active region 11 is subjected to high-speed high-temperature heat treatment, oxygen conditions and pressure conditions are supplied so that the surface of the active region 11 is oxidized to form an oxide layer 6 with a certain thickness.

[0049] S830, such as Figure 6 and Figure 7 As shown, the portion of the oxide layer 6 located at the bottom wall of the signal line contact groove 4 is removed, and the portion of the protective layer located at the side wall of the signal line contact groove 4 is retained to form an anti-permeation film 5.

[0050] In the above-mentioned embodiment, the anti-permeability film 5 is formed by subjecting the active area 11 to a rapid thermal oxidation process, without introducing new materials, thereby saving preparation steps and reducing preparation costs. Specifically, the signal line contact groove 4 penetrates the isolation structure 2 in a direction perpendicular to the thickness of the substrate 1 and exposes the active area 11, and the portion of the active area 11 exposed by the signal line contact groove 4 can form an oxide layer 6 after being subjected to a rapid thermal oxidation process. In order to ensure that the signal line contact structure in the signal line contact groove 4 is in contact with the active area 11 below, it is necessary to remove the portion of the oxide layer 6 located at the bottom wall of the signal line contact groove 4. In order to protect the active area 11 exposed laterally by the signal line contact groove 4, it is necessary to retain the portion of the oxide film located at the side wall of the signal line contact groove 4 and use it as the anti-permeability film 5.

[0051] In a feasible implementation manner, the processing temperature of the rapid thermal oxidation process is T, 900° C. ≤ T ≤ 1100° C.; and / or,

[0052] The oxygen volume flow rate in the rapid thermal oxidation process is L, 30sccm≤L≤80sccm; and / or,

[0053] The rapid thermal oxidation process has a processing time t, 2s≤t≤30s; and / or,

[0054] The pressure of the rapid thermal oxidation process is P, 5Torr≤P≤760Torr.

[0055] In the above embodiment, the processing temperature T of the rapid thermal oxidation process may be 900° C., 930° C., 980° C., 990° C., 1000° C., 1020° C., 1090° C., 1100° C., etc. The oxygen volume flow rate L in the rapid thermal oxidation process may be 30 sccm, 32 sccm, 39 sccm, 40 sccm, 48 sccm, 52 sccm, 64 sccm, 77 sccm, 80 sccm, etc. The processing time t of the rapid thermal oxidation process may be 2 s, 5 s, 9 s, 10 s, 15 s, 20 s, 21 s, 28 s, 30 s, etc. The pressure P of the rapid thermal oxidation process may be 5 Torr, 15 Torr, 50 Torr, 75 Torr, 80 Torr, 92 Torr, 100 Torr, 150 Torr, 280 Torr, 360 Torr, 450 Torr, 520 Torr, 630 Torr, 760 Torr, etc.

[0056] In a feasible implementation manner, the step of removing the portion of the oxide layer 6 located at the bottom wall of the signal line contact groove 4 includes:

[0057] The portion of the oxide layer 6 located at the bottom wall of the signal line contact groove 4 is removed by etching using a dry etching process, and the portion of the oxide layer 6 located at the side wall of the signal line contact groove 4 is retained.

[0058] In the above embodiment, the oxide layer 6 is patterned by dry etching process, and the oxide layer 6 on the bottom wall of the signal line contact groove 4 is anisotropically etched away, while ensuring that the curing layer on the side wall of the signal line contact groove 4 is retained. This etching method has a better control effect on etching accuracy.

[0059] In a feasible embodiment, the thickness of the anti-permeation membrane 5 is greater than or equal to 10 angstroms.

[0060] In the above embodiment, the thickness of the anti-permeability film 5 is greater than or equal to 10 angstroms to prevent the doped ions in the signal line contact structure from diffusing to the adjacent active area 11 through the side wall of the signal line contact groove 4, thereby helping to improve the electrical characteristics of the semiconductor device and improve the yield and performance of the semiconductor device.

[0061] In another possible implementation, if Figure 5 As shown, a new oxide film may be added to form an anti-permeation film 5 in the signal line contact groove 4. The new oxide film may be formed by deposition and patterning to form the anti-permeation film 5.

[0062] In a feasible implementation manner, forming the isolation structure 2 on the substrate 1 includes:

[0063] An isolation groove 21 is formed on the substrate 1, and an active area 11 is formed between adjacent isolation grooves 21. Along the thickness direction of the substrate 1, the size of the isolation groove 21 is smaller than the thickness of the substrate 1;

[0064] The isolation trench 21 is filled with an isolation material 22 .

[0065] In the above embodiment, the isolation structure 2 may be a shallow trench isolation (STI) structure, wherein the isolation trench 21 may be formed by an etching process and is used to fill the isolation material 22 to achieve insulation of the adjacent active region 11. The isolation material 22 includes an insulating material, specifically silicon oxide, silicon nitride or silicon oxynitride.

[0066] In a feasible implementation manner, the material of the signal line contact structure includes polysilicon doped with phosphine.

[0067] In the above embodiment, the signal line contact structure may include polysilicon doped with phosphine, and the anti-permeability film 5 may prevent the phosphine from penetrating into the adjacent active area 11, thereby reducing the adverse effects on the adjacent active area 11 and improving the manufacturing yield.

[0068] In a possible implementation, Figure 8 As shown, the step of patterning the hard mask layer 7 includes:

[0069] A mask layer 7 is formed on a surface of the hard mask layer 3 facing away from the substrate 1, wherein the mask layer 7 includes a via hole;

[0070] The region H of the hard mask layer 3 exposed through the hole is etched to form a through hole 31 .

[0071] In the above embodiment, the mask layer 7 may include an optical glue (PR glue), which may form a via hole at a position for forming a signal line contact structure, and maintain a certain thickness at a position where no signal line contact is formed, thereby realizing a mask. In the subsequent process of patterning the hard mask layer 3, a through hole 31 may be formed at a position opposite to the via hole, so as to form a signal line contact structure opposite to the through hole 31. The subsequent process also includes forming a signal line contact groove 4, which may be formed by the same preparation process as the through hole 31, thereby simplifying the preparation process and saving preparation costs.

[0072] The present application also provides a semiconductor device, which is prepared by any one of the semiconductor device preparation methods provided in the above embodiments of the present application.

[0073] In the semiconductor device, by forming an anti-permeability film 5 on the side wall of the signal line contact groove 4, the signal line contact structure can be made to contact only the active area 11 below, and not to contact the active area 11 adjacent to the substrate 1 in a direction perpendicular to the thickness of the substrate 1, and can prevent the doped ions in the signal line contact structure from diffusing into the active area 11 adjacent to the substrate 1 in a direction perpendicular to the thickness of the substrate 1, thereby improving the yield and performance of the semiconductor device.

[0074] The above are only preferred specific implementations of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be based on the protection scope of the claims.

Claims

1. A method for preparing a semiconductor device, characterized in that: include: Providing a substrate, and forming an isolation structure on the substrate, and forming an active region between adjacent isolation structures; forming a hard mask layer on a surface of one side of the substrate, and patterning the hard mask layer to form a through hole exposing a portion of the active area; forming a signal line contact groove in the active area exposed by the through hole, wherein the signal line contact groove is connected to the through hole; forming an anti-permeability film on the sidewall of the signal line contact groove; A signal line contact structure is formed, wherein the signal line contact structure is at least partially located in the signal line contact groove.

2. The method for preparing a semiconductor device according to claim 1, wherein: The step of forming an anti-permeation film on the sidewall of the signal line contact groove comprises: The signal line contact groove penetrates the isolation structure in a direction perpendicular to the thickness of the substrate and exposes the active area; Processing the sidewalls and bottom wall of the signal line contact groove by a rapid thermal oxidation process so that the portion of the active area exposed by the signal line contact groove is oxidized to form an oxide layer; The portion of the oxide layer located at the bottom wall of the signal line contact groove is removed, and the portion of the oxide layer located at the side wall of the signal line contact groove is retained to form an anti-permeation film.

3. The method for preparing a semiconductor device according to claim 2, characterized in that: The processing temperature of the rapid thermal oxidation process is T, 900°C ≤ T ≤ 1100°C; and / or, The oxygen volume flow rate in the rapid thermal oxidation process is L, 30 sccm≤L≤80 sccm; and / or, The rapid thermal oxidation process has a treatment time of t, 2s≤t≤30s; and / or, The pressure of the rapid thermal oxidation process is P, 5Torr≤P≤760Torr.

4. The method for preparing a semiconductor device according to claim 2, characterized in that: The step of removing the portion of the oxide layer located at the bottom wall of the signal line contact groove comprises: A dry etching process is adopted to etch and remove a portion of the oxide layer located at the bottom wall of the signal line contact groove, and a portion of the oxide layer located at the side wall of the signal line contact groove is retained.

5. The method for preparing a semiconductor device according to claim 1, characterized in that: The thickness of the anti-permeation membrane is greater than or equal to 10 angstroms.

6. The method for preparing a semiconductor device according to claim 1, wherein: The forming of an isolation structure on the substrate comprises: Forming isolation grooves on the substrate, forming active areas between adjacent isolation grooves, and along the thickness direction of the substrate, the size of the isolation grooves is smaller than the thickness of the substrate; The isolation grooves are filled with isolation materials.

7. The method for preparing a semiconductor device according to claim 6, characterized in that: The isolation material includes silicon oxide, silicon nitride or silicon oxynitride.

8. The method for preparing a semiconductor device according to claim 1, characterized in that: The material of the signal line contact structure includes polysilicon doped with phosphine.

9. The method for preparing a semiconductor device according to claim 1, wherein: The step of patterning the hard mask layer comprises: forming a mask layer on a surface of the hard mask layer facing away from the substrate, wherein the mask layer includes a via hole; The area of ​​the hard mask layer exposed by the via hole is etched to form the through hole.

10. A semiconductor device, characterized in that: The semiconductor device is prepared by the method for preparing the semiconductor device according to any one of claims 1 to 9.