Recycling system and method for polycrystalline silicon slag slurry
By using a titanium removal evaporator, titanium removal evaporation tower and condenser system in the polycrystalline silicon production process, combined with a composite ester titanium removal agent, efficiently removes Ti impurities in the slurry, solving the problem of difficult removal of Ti impurities in the polycrystalline silicon slurry , improves the purity and resource utilization of chlorosilane.
Patent Information
- Application Number
- CN202410969626.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-07-19
AI Technical Summary
It is difficult to efficiently remove Ti impurities from the slurry produced during the existing polycrystalline silicon production process, resulting in the recovered chlorosilane containing a large amount of Ti impurities, which is not conducive to its utilization.
The system including a titanium removal evaporation kettle, a titanium removal evaporation tower and a condenser is adopted to evaporate and condense the gas phase and liquid phase generated by high boiling substance treatment, and combined with a composite ester titanium removal agent to achieve effective removal of Ti impurities.
It improves the purity of chlorosilane, reduces the content of Ti impurities, improves the utilization rate of resources, and is suitable for resource reuse in the polysilicon industry.
Smart Images

Figure CN119034224A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a polysilicon slurry recovery system and method, belonging to the technical field of chemical separation. Background Art
[0002] With the increase in demand, the photovoltaic industry and the integrated circuit industry have developed rapidly. Polysilicon is the core raw material of the photovoltaic industry and the integrated circuit industry, so more and more companies have begun to produce polysilicon.
[0003] At present, almost all polysilicon production enterprises adopt the modified Siemens method. In the process of producing polysilicon by the modified Siemens method, a large amount of slurry will be generated. For example, a certain amount of slurry will be generated in the chlorine hydrogenation section of polysilicon production. The slurry mainly includes chlorosilane, silicon powder and metal chloride (for example, TiCl3), etc. The treatment and utilization of the slurry is a difficult problem that the polysilicon industry must face. At present, chlorosilane is mainly recovered by removing silicon powder and metal chloride in the slurry. However, the existing method is difficult to achieve efficient removal of Ti impurities in the slurry, so that the recovered chlorosilane contains more Ti impurities, which is not conducive to the utilization of chlorosilane. Summary of the invention
[0004] The invention provides a polysilicon slurry recovery system, which can efficiently remove Ti impurities in the slurry, reduce the titanium impurity content in the recovered chlorosilane, and improve resource utilization.
[0005] The present invention provides a method for recovering polysilicon slurry. The method is carried out using the above-mentioned system, so Ti impurities in the slurry can be removed efficiently, thereby obtaining recovered chlorosilane with higher purity, which is beneficial to the reuse of chlorosilane.
[0006] The present invention provides a polysilicon slurry recovery system, which comprises a titanium removal evaporator, a titanium removal evaporation tower and a condenser;
[0007] The gas phase outlet of the titanium removal evaporation kettle is communicated with the inlet of the titanium removal evaporation tower, and the top outlet of the titanium removal evaporation tower is communicated with the inlet of the condenser;
[0008] The titanium removal evaporator at least contains high boiling substances generated by slurry treatment.
[0009] The recovery system as described above, wherein, further comprises a titanium removal hydrolysis tank;
[0010] The liquid phase outlet of the titanium removal evaporator is communicated with the inlet of the titanium removal hydrolysis tank.
[0011] The recovery system as described above, wherein, further comprises a titanium removal residual liquid recovery tank;
[0012] The liquid phase outlet of the titanium removal evaporator is communicated with the inlet of the titanium removal residual liquid recovery tank, and the outlet of the titanium removal residual liquid recovery tank is communicated with the inlet of the titanium removal residual liquid hydrolysis tank.
[0013] In the above-mentioned recovery system, the temperature in the titanium removal residual liquid hydrolysis tank is 50-80° C. and the pressure is 0.02-0.06 MPaG.
[0014] The recovery system as described above, wherein it further comprises a titanium removal agent tank, wherein the outlet of the titanium removal agent tank is connected to the inlet of the titanium removal evaporator;
[0015] The titanium removal agent is a complex ester.
[0016] In the recovery system as described above, the addition amount of the titanium removal agent is 0.1-0.4 kg / t high boiling point.
[0017] In the recovery system as described above, the bottom outlet of the titanium removal evaporation tower is communicated with the inlet of the titanium removal evaporation kettle.
[0018] The recovery system as described above, wherein, further comprises a titanium removal reflux tank,
[0019] The outlet of the condenser is communicated with the inlet of the titanium removal reflux tank, and the outlet of the titanium removal reflux tank is communicated with the inlet of the titanium removal evaporation tower.
[0020] The recovery system as described above, wherein the temperature in the titanium removal evaporator is 150-200° C. and the pressure is 0.05-0.15 MPaG; and / or,
[0021] In the titanium removal evaporation tower, the temperature is 130-180° C. and the pressure is 0.05-0.15 MPaG.
[0022] The present invention provides a method for recovering polysilicon slurry, wherein the method is carried out using the recovery system as described above.
[0023] The present invention provides a polysilicon slurry recovery system, which can efficiently remove Ti impurities in the slurry, reduce the Ti impurity content in recovered chlorosilane, and improve resource utilization through the organic connection of a titanium removal evaporator, a titanium removal evaporation tower and a condenser.
[0024] The present invention provides a method for recovering polysilicon slurry. The method is carried out using the above-mentioned recovery system. The method can efficiently remove Ti impurities in the slurry, thereby obtaining recovered chlorosilane with higher purity, which is beneficial to the reuse of chlorosilane. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solutions in the embodiments of the present invention or related technologies, the following briefly introduces the drawings required for use in the embodiments of the present invention or related technologies. Obviously, the drawings described below are only some embodiments of the present invention, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0026] Figure 1 Schematic diagram of a polysilicon slurry recovery system in some embodiments of the present invention.
[0027] Description of reference numerals:
[0028] 1: Titanium removal evaporator;
[0029] 2: Titanium removal evaporation tower;
[0030] 3: Condenser;
[0031] 4: Titanium removal tank;
[0032] 5: Remove titanium reflux tank;
[0033] 6: Titanium removal reflux pump;
[0034] 7: Remove the titanium buffer tank. DETAILED DESCRIPTION
[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] Figure 1 Schematic diagram of a polysilicon slurry recovery system in some embodiments of the present invention. Figure 1 As shown, the first aspect of the present invention provides a polysilicon slurry recovery system, which includes a titanium removal evaporation kettle 1, a titanium removal evaporation tower 2 and a condenser 3;
[0037] The gas phase outlet of the titanium removal evaporator 1 is connected to the inlet of the titanium removal evaporation tower 2, and the top outlet of the titanium removal evaporation tower 2 is connected to the inlet of the condenser 3;
[0038] The titanium removal evaporator 1 contains at least high boiling substances generated by slurry treatment.
[0039] In the present invention, the high boiling products produced by the slurry treatment mainly include Si2Cl6, Si2OCl6, AlCl3, SiCl4, SiHCl3, iron-containing chloride, titanium-containing chloride and boron-containing chloride, wherein the mass percentage of Si2Cl6 is 55-70%, the mass percentage of Si2OCl6 is 3-8%, the mass percentage of AlCl3 is 0-10ppm, the mass percentage of SiCl4 is 15-25%, the mass percentage of SiHCl3 is 0.5-3%, the mass percentage of iron-containing chloride is not higher than 50ppm, the mass percentage of titanium-containing chloride is not higher than 20ppm, and the mass percentage of boron-containing chloride is not higher than 20ppm. In some embodiments, the high boiling products of the present invention can be high boiling products after aluminum removal, which mainly include Si2Cl6, Si2OCl6, SiCl4, SiHCl3, iron-containing chloride, titanium-containing chloride and boron-containing chloride. It can be understood that the titanium removal evaporator 1 may also include a titanium removal agent, which is used to remove titanium from high boiling materials.
[0040] In a specific implementation manner, the high boiling products generated by the slurry treatment are subjected to titanium removal evaporation treatment in the titanium removal evaporator 1. After being treated in the titanium removal evaporator 1, a gas phase mainly including Si2Cl6, Si2OCl6, SiCl4, SiHCl3, AlCl3, iron-containing chloride and boron-containing chloride and a liquid phase mainly including a titanium removal agent, titanium-containing chloride and unreacted high boiling products are obtained;
[0041] The liquid phase is discharged through the liquid phase outlet of the titanium removal evaporator 1; the gas phase is output through the gas phase outlet of the titanium removal evaporator 1, and enters the titanium removal evaporation tower 2 through the inlet of the titanium removal evaporation tower 2, and the gas phase is evaporated in the titanium removal evaporation tower 2 to obtain titanium removal high boiling products including Si2Cl6 and Si2OCl6 and titanium removal low boiling products including SiCl4, SiHCl3 and a small amount of titanium-containing chloride, and the titanium removal high boiling products are output through the top outlet of the titanium removal evaporation tower 2, and enter the condenser 3 through the inlet of the condenser 3. After condensation in the condenser 3, the titanium removal chlorosilane solution is obtained, and the obtained chlorosilane solution can be reused after cracking.
[0042] The polysilicon slurry recovery system of the present invention can efficiently remove Ti impurities in the slurry, reduce the titanium impurity content in the recovered chlorosilane, and improve resource utilization by allowing the high-boiling products generated by slurry treatment to enter the organically combined titanium removal evaporator 1, titanium removal evaporation tower 2 and condenser 3 in sequence.
[0043] In some embodiments of the present invention, the recovery system further comprises a titanium removal hydrolysis tank;
[0044] The liquid phase outlet of the titanium removal evaporator 1 is communicated with the inlet of the titanium removal hydrolysis tank.
[0045] Specifically, the liquid phase produced by the titanium removal evaporator 1 is output through the liquid phase outlet of the titanium removal evaporator 1, and enters the titanium removal residual liquid hydrolysis tank through the inlet of the titanium removal residual liquid hydrolysis tank. The liquid phase is hydrolyzed under the action of lime milk (lime milk is a lime milk aqueous solution with a mass percentage of 3 to 10%) in the titanium removal residual liquid hydrolysis tank, and the waste water obtained by hydrolysis enters the waste water main pipe, and the obtained tail gas (HCl, H2, water) enters the tail gas tower for treatment.
[0046] The recovery system of the present invention can also recover and reuse other components (HCl, H2, water) in the high-boiling product, has excellent economic benefits, and is suitable for wide promotion and application.
[0047] Furthermore, the recovery system also includes a titanium removal residual liquid recovery tank;
[0048] The liquid phase outlet of the titanium removal evaporator 1 is communicated with the inlet of the titanium removal residual liquid recovery tank, and the outlet of the titanium removal residual liquid recovery tank is communicated with the inlet of the titanium removal residual liquid hydrolysis tank.
[0049] In a specific embodiment, the liquid phase obtained by the titanium removal evaporator 1 is output through the outlet of the titanium removal evaporator 1, enters the titanium removal residual liquid recovery tank through the inlet of the titanium removal residual liquid recovery tank, and is stored in the titanium removal residual liquid recovery tank, wherein a part of the liquid phase is then output through the outlet of the titanium removal residual liquid recovery tank, enters the titanium removal residual liquid hydrolysis tank through the inlet of the titanium removal residual liquid hydrolysis tank for hydrolysis; the other part of the liquid phase is output through the outlet of the titanium removal residual liquid recovery tank, and enters the titanium removal evaporator 1 through the inlet of the titanium removal evaporator 1.
[0050] By setting up a titanium removal residual liquid recovery tank, the liquid phase produced by the titanium removal evaporator 1 can be stored more conveniently, the amount of the liquid phase to be hydrolyzed can be controlled, and the liquid phase can be allowed to enter the titanium removal evaporator 1 again, so that the titanium in the liquid phase can be further removed, and the useful components in the liquid phase can be further utilized to improve the utilization rate of resources.
[0051] In some embodiments, a hydrolysis tank cooler is further included, and the hydrolysis tank cooler is used to condense the tail gas generated by the hydrolysis tank. The obtained condensate enters the titanium removal residual liquid hydrolysis tank again for hydrolysis to improve the hydrolysis degree of the liquid phase.
[0052] The invention also includes a hydrolyzate circulation pump, the outlet of the titanium removal residual liquid hydrolysis tank is connected to the inlet of the hydrolyzate circulation pump, and the outlet of the hydrolyzate circulation pump is connected to the inlet of the hydrolyzate cooler. The invention uses the hydrolyzate circulation pump to make the waste water obtained by the titanium removal residual liquid hydrolysis tank as the cold source of the hydrolyzate cooler, which can further save water resources and improve resource utilization.
[0053] Furthermore, when the temperature in the titanium removal residual liquid hydrolysis tank is 50-80° C. and the pressure is 0.02-0.06 MPaG, the hydrolysis efficiency of the titanium removal residual liquid hydrolysis tank can be further improved while saving energy consumption, thereby increasing the recycling rate of resources.
[0054] For example, in the titanium removal residual liquid hydrolysis tank, the temperature may be any one of 50°C, 60°C, 65°C, 70°C, 75°C and 80°C, or a range consisting of any two thereof;
[0055] The pressure may be any one of 0.02 MPaG, 0.03 MPaG, 0.04 MPaG, 0.05 MPaG, and 0.06 MPaG, or a range consisting of any two of them.
[0056] In some embodiments of the present invention, the recovery system further comprises a titanium removal agent tank 4, the outlet of the titanium removal agent tank 4 is connected to the inlet of the titanium removal evaporator 1;
[0057] The titanium remover is a complex ester.
[0058] In a specific embodiment, the titanium removal agent is outputted from the outlet of the titanium removal agent tank 4 and enters the titanium removal evaporator 1 through the inlet of the titanium removal evaporator 1. In the titanium removal evaporator 1, the titanium removal agent reacts with high boiling materials to perform titanium removal treatment.
[0059] By using the titanium removal agent tank 4 to add the titanium removal agent to the titanium removal evaporator 1, the amount of the titanium removal agent added can be adjusted in real time to control the reaction progress, thereby improving the titanium removal efficiency while saving the titanium removal agent. In addition, composite esters are used for titanium removal, and the composite esters have strong selectivity, and the resulting complex is stable and easy to separate.
[0060] In some embodiments, a titanium removal buffer tank 7 is further included, the outlet of the titanium removal agent tank 4 is communicated with the inlet of the titanium removal buffer tank 7, the outlet of the titanium removal buffer tank 7 is communicated with the inlet of the titanium removal evaporator 1, and the high boiling products enter the titanium removal buffer tank 7 through the inlet of the titanium removal buffer tank 7. By arranging the titanium removal buffer tank 7 between the titanium removal agent tank 4 and the titanium removal evaporator 1, the titanium removal agent and the high boiling products can be mixed in advance, and the amount of the titanium removal agent and the high boiling products added can be controlled, thereby improving the processing efficiency of the titanium removal evaporator 1.
[0061] Furthermore, when the addition amount of the titanium removal agent is 0.1-0.4 kg / t high boiling point, the titanium removal agent can fully play its role and improve the titanium removal effect.
[0062] Exemplarily, the addition amount of the titanium removal agent can be any one of 0.1 kg / t high boiling point, 0.15 kg / t high boiling point, 0.2 kg / t high boiling point, 0.3 kg / t high boiling point, 0.35 kg / t high boiling point, 0.4 kg / t high boiling point, or any two of them.
[0063] In some embodiments of the present invention, the bottom outlet of the titanium removal evaporation tower 2 is connected to the inlet of the titanium removal evaporation kettle 1 .
[0064] Specifically, the titanium removal low-boiling products (including SiCl4, SiHCl3 and a small amount of titanium-containing chloride) produced by the titanium removal evaporation tower 2 are output through the bottom outlet of the titanium removal evaporation tower 2, enter the titanium removal evaporation kettle 1 through the inlet of the titanium removal evaporation kettle 1, and further titanium removal is carried out in the titanium removal evaporation kettle 1.
[0065] Through this setting, titanium can be removed better while saving materials, thus improving resource utilization efficiency.
[0066] Furthermore, it also includes a titanium removal reflux tank 5,
[0067] The outlet of the condenser 3 is communicated with the inlet of the titanium removal reflux tank 5 , and the outlet of the titanium removal reflux tank 5 is communicated with the inlet of the titanium removal evaporation tower 2 .
[0068] Specifically, the liquid chlorosilane obtained after condensation in the condenser 3 is output through the outlet of the condenser 3, and enters the titanium removal reflux tank 5 through the inlet of the titanium removal reflux tank 5. The liquid chlorosilane is stored in the titanium removal reflux tank 5. A part of the liquid chlorosilane can be output through the outlet of the titanium removal reflux tank 5, and enter the titanium removal evaporation tower 2 through the inlet of the titanium removal evaporation tower 2 for reflux, and the other part of the liquid chlorosilane can enter other sections for reuse.
[0069] By providing the titanium removal reflux tank 5, on the one hand, liquid-phase chlorosilane can be stored more conveniently, and chlorosilane can be used as reflux liquid of the titanium removal evaporation tower 2, thereby improving resource utilization.
[0070] In some embodiments, a titanium removal reflux pump 6 is further included, the outlet of the titanium removal reflux tank 5 is connected to the inlet of the titanium removal reflux pump 6, and the outlet of the titanium removal reflux pump 6 is connected to the inlet of the titanium removal evaporation tower 2. The present invention can reflux chlorosilane through the titanium removal reflux pump 6 to improve the utilization efficiency of chlorosilane.
[0071] In some embodiments of the present invention, when the temperature in the titanium removal evaporator 1 is 150-200° C. and the pressure is 0.05-0.15 MPaG, the titanium removal efficiency can be improved while saving energy consumption.
[0072] Furthermore, when the temperature in the titanium removal evaporation tower 2 is 130-180° C. and the pressure is 0.05-0.15 MPaG, the titanium removal efficiency can be further improved while saving energy consumption, and the resource recycling rate can be increased.
[0073] A second aspect of the present invention provides a method for recovering polysilicon slurry, wherein the method is carried out using the recovery system of the first aspect.
[0074] Since the recovery method is carried out using the above-mentioned recovery system, Ti impurities in the slurry can be removed efficiently, thereby obtaining recovered chlorosilane with higher purity, which is beneficial to the reuse of chlorosilane.
[0075] The technical solution of the present invention will be further described below in conjunction with specific embodiments.
[0076] Example 1
[0077] The polysilicon slurry recovery system of this embodiment is as follows: Figure 1 As shown, it includes: a titanium removal evaporator 1, a titanium removal evaporation tower 2, a titanium removal residual liquid hydrolysis tank, a titanium removal agent tank 4, a titanium removal residual liquid recovery tank, a titanium removal reflux tank 5, a titanium removal buffer tank 7, a hydrolysis tank cooler, a hydrolyzate circulation pump, a titanium removal reflux pump 6 and a condenser 3;
[0078] The outlet of the titanium removal agent tank 4 is communicated with the inlet of the titanium removal buffer tank 7, the outlet of the titanium removal agent tank 4 is communicated with the inlet of the titanium removal evaporator 1, the gas phase outlet of the titanium removal evaporator 1 is communicated with the inlet of the titanium removal evaporation tower 2, the top outlet of the titanium removal evaporation tower 2 is communicated with the inlet of the condenser 3, the outlet of the condenser 3 is communicated with the inlet of the titanium removal reflux tank 5, the outlet of the titanium removal reflux tank 5 is communicated with the inlet of the titanium removal reflux pump 6, the outlet of the titanium removal reflux pump 6 is communicated with the inlet of the titanium removal evaporation tower 2, and the bottom outlet of the titanium removal evaporation tower 2 is communicated with the inlet of the titanium removal evaporation tank 1;
[0079] The liquid phase outlet of the titanium removal evaporator 1 is connected to the inlet of the titanium removal residual liquid recovery tank, the outlet of the titanium removal residual liquid recovery tank is connected to the inlet of the titanium removal residual liquid hydrolysis tank, the liquid phase outlet of the titanium removal residual liquid hydrolysis tank is connected to the inlet of the hydrolyzed liquid circulation pump, the outlet of the hydrolyzed liquid circulation pump is connected to the cold source inlet of the hydrolyzed liquid cooler, and the gas phase outlet of the titanium removal residual liquid hydrolysis tank is connected to the heat source inlet of the hydrolyzed liquid cooler;
[0080] The outlet of the titanium removal residual liquid recovery tank is connected to the inlet of the titanium removal evaporator 1;
[0081] The high boiling materials enter the titanium removal buffer tank 7 through the inlet of the titanium removal buffer tank 7 .
[0082] Example 2
[0083] The method for recovering polysilicon slurry in this embodiment is carried out using the system in Embodiment 1, and specifically comprises:
[0084] 1) allowing the titanium removal agent to enter the titanium removal buffer tank 7 through the titanium removal agent tank 4, allowing the high boiling point to enter the titanium removal buffer tank 7, and then allowing the premix of the titanium removal agent and the high boiling point to enter the titanium removal evaporator 1 through the titanium removal buffer tank 7, allowing the high boiling point and the titanium removal agent to undergo titanium removal treatment in the titanium removal evaporator 1, and obtaining a liquid phase and a gas phase after the titanium removal treatment;
[0085] 2) the gas phase is output through the outlet of the titanium removal evaporator 1, enters the titanium removal evaporation tower 2 through the inlet of the titanium removal evaporation tower 2, after being processed by the titanium removal evaporation tower 2, the obtained titanium removal high boiling products are output through the top outlet of the titanium removal evaporation tower 2, enter the condenser 3 through the inlet of the condenser 3, and obtain liquid chlorosilane after condensation by the condenser 3, the liquid chlorosilane is output through the outlet of the condenser 3, enters the titanium removal reflux tank 5 through the inlet of the titanium removal reflux tank 5, part of the liquid chlorosilane in the titanium removal reflux tank 5 is output through the outlet of the titanium removal reflux tank 5, enters the titanium removal reflux pump 6 through the inlet of the titanium removal reflux pump 6, the outlet of the titanium removal reflux pump 6 is connected to the inlet of the titanium removal evaporation tower 2, and the bottom outlet of the titanium removal evaporation tower 2 is connected to the inlet of the titanium removal evaporation kettle 1;
[0086] 3) The liquid phase is outputted through the liquid phase outlet of the titanium removal evaporator 1, and enters the titanium removal residual liquid recovery tank through the inlet of the titanium removal residual liquid recovery tank. The liquid phase in the titanium removal residual liquid recovery tank is outputted through the outlet of the titanium removal residual liquid recovery tank, and enters the titanium removal residual liquid hydrolysis tank through the inlet of the titanium removal residual liquid hydrolysis tank. The liquid is hydrolyzed with 8% lime milk in the titanium removal residual liquid hydrolysis tank to obtain waste water and tail gas;
[0087] Part of the tail gas is cooled in the hydrolyzed liquid cooler and then enters the titanium removal residual liquid hydrolysis tank again, and part of the tail gas enters the tail gas tower for treatment;
[0088] Part of the wastewater enters the wastewater main, and part of the wastewater is connected to the inlet of the hydrolyzate circulation pump, and then transported to the hydrolyzate tank cooler through the outlet of the hydrolyzate circulation pump to cool the tail gas as a cold source of the hydrolyzate cooler;
[0089] The high boiling substances include: Si2Cl6, Si2OCl6, SiCl4, SiHCl3, iron-containing chloride, titanium-containing chloride and boron-containing chloride, and the mass percentage of Si2Cl6 is 67.4%, the mass percentage of Si2OCl6 is 6.4%, the mass percentage of SiCl4 is 24.7%, the mass percentage of SiHCl3 is 1.4%, the mass percentage of iron-containing chloride is 15ppm, the mass percentage of titanium-containing chloride is 5ppm and the mass percentage of boron-containing chloride is 5ppm;
[0090] Liquid chlorosilanes include: SiCl4, SiHCl 3、 Si2Cl6, Si2OCl6, the mass percentage of SiCl4 is 25.9%, the mass percentage of SiHCl3 is 1.4%, the mass percentage of Si2Cl6 is 66.2%, and the mass percentage of Si2OCl6 is 6.4%;
[0091] The tail gas includes HCl, H2, water, and N2, wherein the mass percentage of HCl is 0.1%, the mass percentage of H2 is 0.01%, the mass percentage of water is 0.05%, and the mass percentage of nitrogen is 99.84%;
[0092] The titanium removal agent is a complex ester, and the addition amount of the titanium removal agent is 0.3kg / t high boiling point;
[0093] In the titanium removal evaporator 1, the temperature is 152°C and the pressure is 0.07MPaG;
[0094] In the titanium removal evaporation tower 2, the temperature is 142°C and the pressure is 0.04 MPaG;
[0095] In the titanium removal residual liquid hydrolysis tank, the temperature is 45°C and the pressure is 0.05MPaG.
[0096] Comparative Example 1
[0097] The method for recovering polysilicon slurry of this comparative example comprises the following steps:
[0098] 1) The titanium removal agent enters the titanium removal agent buffer tank 7 through the titanium removal agent feeding tank 4, and enters the titanium removal evaporator 1 through the titanium removal agent buffer tank 7, so that the high boiling point and the titanium removal agent are subjected to titanium removal treatment in the titanium removal evaporator 1, and a liquid phase and a gas phase are obtained after the titanium removal treatment;
[0099] 2) The gas phase is outputted from the outlet of the titanium removal evaporator 1, enters the condenser 3 through the inlet of the condenser 3, and is condensed in the condenser 3 to obtain liquid chlorosilane;
[0100] 3) The liquid phase is outputted through the liquid phase outlet of the titanium removal evaporator 1, and the chlorosilane enters the titanium removal residual liquid recovery tank through the inlet of the titanium removal residual liquid recovery tank. The liquid phase in the titanium removal residual liquid recovery tank is outputted through the outlet of the titanium removal residual liquid recovery tank, and enters the titanium removal residual liquid hydrolysis tank through the inlet of the titanium removal residual liquid hydrolysis tank, and is hydrolyzed with 8% lime milk in the titanium removal residual liquid hydrolysis tank to obtain waste water and tail gas;
[0101] Part of the tail gas is cooled in the hydrolyzed liquid cooler and then enters the titanium removal residual liquid hydrolysis tank again, and part of the tail gas enters the tail gas tower for treatment;
[0102] The high boiling substances include: Si2Cl6, Si2OCl6, AlCl3, SiCl4, SiHCl3, iron-containing chloride, titanium-containing chloride and boron-containing chloride, and the mass percentage of Si2Cl6 is 67.4%, the mass percentage of Si2OCl6 is 6.4%, the mass percentage of SiCl4 is 24.7%, the mass percentage of SiHCl3 is 1.4%, the mass percentage of iron-containing chloride is 15ppm, the mass percentage of titanium-containing chloride is 5ppm and the mass percentage of boron-containing chloride is 5ppm;
[0103] Liquid chlorosilane includes: SiCl4, SiHCl3, Si2Cl6, Si2OCl6, AlCl3, the mass percentage of SiCl4 is 26.2%, the mass percentage of SiHCl3 is 1.5%, the mass percentage of Si2Cl6 is 65.9%, the mass percentage of Si2OCl6 is 6.4%, and other impurities are 10ppm;
[0104] The tail gas includes HCl, H2, water, and N2, wherein the mass percentage of HCl is 0.1%, the mass percentage of H2 is 0.01%, the mass percentage of water is 0.05%, and the mass percentage of nitrogen is 99.84%;
[0105] The titanium removal agent is a complex ester, and the addition amount of the titanium removal agent is 0.3kg / t high boiling point;
[0106] In the titanium removal evaporator 1, the temperature is 152°C and the pressure is 0.07MPaG;
[0107] In the titanium removal residual liquid hydrolysis tank, the temperature is 45°C and the pressure is 0.05MPaG.
[0108] It can be seen that compared with Comparative Example 1, the liquid chlorosilane obtained by the polycrystalline silicon slurry recovery method in Example 2 of the present invention has higher purity and contains almost no other impurities, indicating that the polycrystalline silicon slurry recovery system and recovery method of the present invention can efficiently remove Ti impurities in the slurry, reduce the Ti impurity content in the recovered chlorosilane, and improve resource utilization.
[0109] Each embodiment in this specification is described in a related manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. The above are only preferred embodiments of the present invention and are not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention are included in the scope of protection of the present invention.
Claims
1. A polysilicon slurry recovery system, characterized in that: It includes a titanium removal evaporator, a titanium removal evaporator tower and a condenser; The gas phase outlet of the titanium removal evaporation kettle is communicated with the inlet of the titanium removal evaporation tower, and the top outlet of the titanium removal evaporation tower is communicated with the inlet of the condenser; The titanium removal evaporator at least contains high boiling substances generated by slurry treatment.
2. The recovery system according to claim 1, characterized in that: Also included is a titanium removal hydrolysis tank; The liquid phase outlet of the titanium removal evaporator is communicated with the inlet of the titanium removal hydrolysis tank.
3. The recovery system according to claim 2, characterized in that: It also includes a titanium removal residual liquid recovery tank; The liquid phase outlet of the titanium removal evaporator is communicated with the inlet of the titanium removal residual liquid recovery tank, and the outlet of the titanium removal residual liquid recovery tank is communicated with the inlet of the titanium removal residual liquid hydrolysis tank.
4. The recovery system according to claim 2 or 3, characterized in that: In the titanium removal residual liquid hydrolysis tank, the temperature is 50-80° C. and the pressure is 0.02-0.06 MPaG.
5. The recycling system according to any one of claims 1 to 4, characterized in that: It also includes a titanium removal agent tank, the outlet of which is connected to the inlet of the titanium removal evaporator; The titanium removal agent is a complex ester.
6. The recovery system according to claim 5, characterized in that: The addition amount of the titanium removal agent is 0.1-0.4 kg / t high boiling matter.
7. The recycling system according to any one of claims 1 to 6, characterized in that: The bottom outlet of the titanium removal evaporation tower is communicated with the inlet of the titanium removal evaporation kettle.
8. The recycling system according to any one of claims 1 to 7, characterized in that: Also includes titanium removal reflux tank, The outlet of the condenser is communicated with the inlet of the titanium removal reflux tank, and the outlet of the titanium removal reflux tank is communicated with the inlet of the titanium removal evaporation tower.
9. The recycling system according to any one of claims 1 to 8, characterized in that: In the titanium removal evaporator, the temperature is 150-200°C and the pressure is 0.05-0.15MPaG; and / or, In the titanium removal evaporation tower, the temperature is 130-180° C. and the pressure is 0.05-0.15 MPaG.
10. A method for recovering polysilicon slurry, characterized in that: The method is carried out using the recovery system described in any one of claims 1 to 9.
Citation Information
Patent Citations
Low-cost SCR denitration catalyst and preparation method thereof
CN105478133A
Energy-saving titanium tetrachloride refining method
CN108328652A
Disilane preparation method
CN109399644A
Resourceful treatment method for olefin polymerization industrial waste acid residues
CN112678866A
Method and device for treating chlorosilane slag slurry
CN114590811A