Ingot mold for industrial silicon breaking process

By designing an ingot die with a rectangular array cavity and vertical cooling hole, combining a chute and a compressed air cooling system, the problems of long cooling time and complex crushing process of traditional ingot die are solved, and efficient silicon ingot cooling and crushing are achieved, improving the efficiency of the ingot die. productivity.

CN119035472APending Publication Date: 2024-11-29INNER MONGOLIA UNIV OF SCI & TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411175487.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The traditional ferrosilicon ingot molds have a long cooling time during the casting process, and the crushing process is complicated and the efficiency is low.

Method used

Design an ingot die for industrial silicon de-crumbing process, including rectangular array arrangement of cavity and vertical cooling holes, equipped with chutes and compressed air cooling systems, cavity sizes suitable for the inlet size of jaw crusher, slide chutes Designed for natural breakage, base and hoist structures for easy movement and cooling.

Benefits of technology

It significantly shortens the cooling time of silicon ingots, saves manual crushing process, and improves production efficiency. The size of the silicon block meets the entrance requirements of the jaw crusher and directly enters the crusher for secondary crushing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0005010603710000011
    Figure HDA0005010603710000011
  • Figure HDA0005010603710000012
    Figure HDA0005010603710000012
  • Figure HDA0005010603710000013
    Figure HDA0005010603710000013
Patent Text Reader

Abstract

The ingot mold comprises a mold body, an opening is formed in the upper end of the mold body, a plurality of cavities are formed in the mold body and distributed in the mold body in a rectangular array mode, and sliding grooves are formed in the cavity walls between the adjacent cavities; and cooling holes which are vertically formed from top to bottom are formed in four circumferential corners of a cavity body of the cavity. Compared with an existing traditional ingot mold, compressed air is introduced into the cavities of the ingot mold and the cooling holes between the cavities, the cooling time of a silicon ingot can be shortened, the silicon ingot obtained after casting molding of the ingot mold meets the inlet size of a jaw crusher, a traditional crushing process can be omitted, and the productivity is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of molds, in particular to an ingot mold used in an industrial silicon de-crushing process. Background Art

[0002] The photovoltaic industry, which uses silicon materials as its main raw material, is a typical sunrise industry and is thriving. Industrial silicon is the basic raw material for the development of the photovoltaic industry and is mainly used in the production of polysilicon, organic silicon, and aluminum alloy products. In the industrial silicon smelting workshop, the ingot mold is the mold used by the silicon smelting industry to cast silicon ingots. The existing production process for refined industrial silicon is to invert the molten liquid silicon in the silicon bag into the ingot mold. The casting is mainly long-plate type, and it is cooled and formed in the ingot mold. After demolding and manual crushing, it is sent to the jaw crusher for secondary crushing. The traditional ferrosilicon ingot mold has the following defects: during the casting process, the cooling time of the long-plate ingot mold is relatively long, and during the cooling process, the center of the ingot mold cools slowly, accompanied by silicon flow. After cooling is completed, a crushing process is required, which is complicated and inefficient. Summary of the invention

[0003] In view of the problems of slow cooling of ingot molds and complicated subsequent crushing process in the prior art, the present invention proposes to design an ingot mold for industrial silicon crushing process, which has good cooling effect and more efficient crushing. The technical solutions adopted by the present invention to solve the problems in the prior art are as follows:

[0004] An ingot mold for an industrial silicon de-crushing process comprises a mold body, the upper end of the mold body is open, a plurality of cavities are arranged inside the mold body in a rectangular array, slide grooves are provided on the cavity walls between adjacent cavities, and cooling holes are provided at the four circumferential corners of the cavity body and are vertically opened from top to bottom.

[0005] The cavity is a cavity with a certain draft angle.

[0006] The included angles between the bottom surface of the cavity and each side wall are 104.04°, and the resulting draft angle facilitates demoulding.

[0007] The cavity size meets the inlet size of the jaw crusher, eliminating the crushing process of the silicon powder production process. The maximum feed size of the jaw crusher is 300×300mm. After the traditional process is cast, it is a silicon plate, which needs to be naturally cooled and then manually crushed to meet the maximum feed size. The size of the silicon block made by the mold of the present invention is less than 300×300mm, and can enter the inlet of the jaw crusher without manual crushing.

[0008] The bottom of the chute is a U-shaped structure, and the upper opening is flush with the upper end surface of the cavity wall, which facilitates the flow of silicone water into the edge cavity during casting.

[0009] The opening depth of the chute is 100mm, and the width of the chute is relatively thin. When the silicon water is cast to a level higher than the chute and lower than the upper end surface of the mold, the casting is stopped; after cooling is completed, due to the thin design of the chute, the silicon blocks in the mold will be subjected to a certain impact when demolding, and large silicon blocks will naturally break and shatter along the internal chute to form several small silicon blocks.

[0010] A forklift slot is provided at the bottom of the mold body, which is convenient for moving the ingot mold as a whole from the bottom. The forklift slot spacing and slot size are compatible with commonly used forklifts.

[0011] A plurality of lifting ears are arranged on the upper end surface of the side wall of the mold body, which are used for a crane to lift the ingot mold from above and move it.

[0012] There are three lifting ears, which are respectively arranged at the upper ends of the three side walls of the mold body. The lifting ear structure arranged in a triangle is used to ensure the lifting stability.

[0013] The ingot mold is provided with a matching base, which has a stepped groove inside. The upper dimension of the groove is adapted to the outer dimension of the ingot mold, and the lower dimension of the groove is smaller than the outer dimension of the ingot mold and larger than the spacing between the outermost cooling holes. After the silicon block in the ingot mold is cast, it is cooled during transportation. The cooling process can be completed on the transfer vehicle by introducing compressed air into the lower layer of the base and dispersing the compressed air through a number of cooling holes on the ingot mold to accelerate the cooling of the silicon block.

[0014] The present invention has the following advantages:

[0015] Compared with the existing traditional ingot molds, the cavity of the ingot mold of the present invention and the cooling holes between the cavities are filled with compressed air, which can reduce the cooling time of the silicon ingot. The silicon ingot obtained after the ingot mold of the present invention is cast and molded meets the inlet size of the jaw crusher, which can save the traditional crushing process and improve productivity. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the overall structure of the ingot mold of the present invention;

[0017] Figure 2 It is a cross-sectional view of the ingot mold EE of the present invention;

[0018] Figure 3 It is a cross-sectional view of the cooling hole of the present invention;

[0019] Figure 4 It is a front view of the ingot mold of the present invention;

[0020] Figure 5 A top view of an ingot mold of the present invention;

[0021] Figure 6 This is a state diagram of the ingot mold of the present invention being cooled by compressed air;

[0022] Among them: 1- cavity, 2- lifting ear, 3- chute, 4- forklift slot, 5- cooling hole. DETAILED DESCRIPTION

[0023] The technical solution of the present invention is further specifically described below through embodiments and in conjunction with the accompanying drawings. Figure 1-5 As shown, an ingot mold for industrial silicon crushing process includes a mold body, the upper end of the mold body is open, and a plurality of cavities 1 are arranged inside the mold body in a rectangular array. The angles between the bottom surface of the cavity 1 and each side wall are 104.04°, and the draft angle formed is convenient for demoulding; the size of the cavity 1 meets the inlet size of the jaw crusher, eliminating the crushing process of the silicon powder production process, the maximum feed size of the jaw crusher is 300×300mm, and the traditional process is a silicon plate after casting, which needs to be naturally cooled and then manually crushed to meet the maximum feed size. The size of the silicon block made based on the mold of the present invention is less than 300×300mm, and can enter the inlet of the jaw crusher without manual crushing.

[0024] A chute 3 is provided on the cavity wall between adjacent cavities 1. The bottom of the chute 3 is a U-shaped structure, and the upper opening is flush with the upper end surface of the cavity wall, which is convenient for the flow of silicon water into the edge cavity during casting. The opening depth of the chute 3 is 100mm, and the width of the chute 3 is relatively thin. When the silicon water is cast to a level higher than the chute 3 and lower than the upper end surface of the mold, the casting is stopped; after cooling, due to the thin design of the chute, the silicon block in the mold will be subjected to a certain impact when demolding, and the large silicon block will naturally break and shatter along the internal chute to form several small silicon blocks.

[0025] A forklift slot 4 is provided at the bottom of the mold body to facilitate the overall movement of the ingot mold from the bottom. The spacing and slot size of the forklift slot 4 are compatible with common forklifts. Three lifting ears 2 are provided on the upper end surface of the side wall of the mold body for a crane to lift the ingot mold from above and move it. The three lifting ears 2 are respectively arranged at the upper ends of the three side walls of the mold body, and the lifting stability is ensured by using a lifting ear structure arranged in a triangle.

[0026] like Figure 3 and Figure 6 As shown, the four corners of the cavity 1 are provided with cooling holes 5 vertically opened from top to bottom. The ingot mold is also provided with a matching base, which has a stepped groove inside. The upper dimension of the groove is adapted to the outer dimension of the ingot mold, and the lower dimension of the groove is smaller than the outer dimension of the ingot mold, and larger than the spacing between the outermost cooling holes. After the silicon block in the ingot mold is cast, it is cooled during the transportation process. The cooling process can be completed on the transfer vehicle. By introducing compressed air into the lower layer of the base, the compressed air is dispersed through several cooling holes on the ingot mold to accelerate the cooling of the silicon block.

[0027] The protection scope of the present invention is not limited to the above-mentioned embodiments. Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the scope and spirit of the present invention. If these changes and modifications fall within the scope of the claims of the present invention and their equivalents, the present invention is intended to include these changes and modifications.

Claims

1. An ingot mold for industrial silicon de-crushing process, characterized in that: The mold body comprises a mold main body, the upper end of which is open and a plurality of cavities are arranged inside. The plurality of cavities are arranged in a rectangular array inside the mold main body, and slide grooves are opened on the cavity walls between adjacent cavities. The four circumferential corners of the cavity are provided with cooling holes opened vertically from top to bottom.

2. An ingot mold for industrial silicon de-crushing process according to claim 1, characterized in that: The cavity is a cavity with a certain draft angle.

3. An ingot mold for industrial silicon de-fragmentation process as claimed in claim 2, characterized in that: The included angles between the bottom surface of the cavity and each side wall are 104.04°, and the resulting draft angle facilitates demoulding.

4. An ingot mold for industrial silicon de-fragmentation process according to claim 1, characterized in that: The cavity size is less than 300×300 mm, meeting the inlet size of the jaw crusher.

5. An ingot mold for industrial silicon de-fragmentation process according to claim 1, characterized in that: The bottom of the slide groove is a U-shaped structure, and the upper opening is flush with the upper end surface of the cavity wall.

6. An ingot mold for industrial silicon de-fragmentation process according to claim 1, characterized in that: The opening depth of the chute is 100 mm, and the chute width is relatively thin.

7. An ingot mold for industrial silicon de-fragmentation process according to claim 1, characterized in that: A forklift groove is provided at the bottom of the mold body, and the forklift groove spacing and slot size are compatible with commonly used forklifts.

8. An ingot mold for industrial silicon de-crushing process as claimed in claim 1, characterized in that: A plurality of lifting ears are arranged on the upper end surface of the side wall of the mold body.

9. An ingot mold for industrial silicon de-fragmentation process according to claim 1, characterized in that: There are three lifting ears, which are respectively arranged on the upper ends of the three side walls of the mold body.

10. An ingot mold for industrial silicon de-crushing process according to claim 1, characterized in that: The ingot mold is provided with a matching base, and a stepped groove is opened inside the base. The upper dimension of the groove is adapted to the outer dimension of the ingot mold, and the lower dimension of the groove is smaller than the outer dimension of the ingot mold and larger than the spacing between the outermost cooling holes. Compressed air can be introduced into the lower layer of the base.

Citation Information

Cited By

  • Method for forming industrial silicon melt stepped solidification reinforced Si8Al6Fe4Ca

    CN119911912A