Battery cap laser welding method capable of preventing tab fracture

By using smooth guide zone and magnetic column technology in the battery cap laser welding system, the problem of pole ears being prone to break during welding is solved, and the quality and yield of welding are improved.

CN119035761AActive Publication Date: 2024-11-29GUANGDONG NUODA SMART ENERGY TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411417619.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-11
Publication Date
2024-11-29
Estimated Expiration
2044-10-11

AI Technical Summary

Technical Problem

Existing battery cap welding systems can easily cause the electrode ear to break when pressing the electrode ear, resulting in a low welding yield.

Method used

Using a laser welding method for battery caps including laser welding parts, fixing seats, compression mechanisms and demagnetization mechanisms, the caps are moved to aligned with the pole ears through magnetic columns and horizontal drive members, and the pole is made by using a smooth guide area. The ear bend angle is reduced to avoid breakage and welding is achieved through laser welds.

Benefits of technology

It effectively avoids the breakage of the extreme ear, improves the yield of welding, and ensures stable connection of the battery cap.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035761A_ABST
    Figure CN119035761A_ABST
Patent Text Reader

Abstract

The invention provides a battery cap laser welding method capable of preventing tab breakage. According to the battery cap laser welding method capable of preventing tab breakage, a battery cap welding device is adopted for welding, the battery cap welding device comprises a laser welding piece, a fixing base, a pressing mechanism, a cap fixing mechanism and a demagnetizing mechanism, and the cap fixing mechanism is used for being in magnetic attraction with a cap; the pressing mechanism comprises a second horizontal driving piece, a connecting plate and a pressing boss, a smooth guide area is arranged on the side face, close to the magnetic attraction column, of the pressing boss, and when the second horizontal driving piece drives the pressing boss to move, the smooth guide area abuts against the electrode lug; the demagnetizing mechanism comprises a connecting frame, a vertical driving part and a barrier plate, the vertical driving part is connected with the connecting frame, the power output end of the vertical driving part is connected with the barrier plate, and the vertical driving part drives the barrier plate to abut against the cap so that the cap can be separated from the magnetic attraction column.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of battery technology, and in particular to a laser welding method for a battery cap that prevents tab breakage. Background Art

[0002] With the continuous consumption of non-renewable resources and the increasing prominence of environmental problems, new energy has developed rapidly in recent years, especially the development and application of lithium-ion batteries have become more mature and extensive. In order to facilitate the modular production of lithium-ion batteries, lithium-ion batteries are usually split into several core components such as the cap as the positive electrode, the battery cell and the shell as the negative electrode for separate mass production, and then the battery cell is installed in the shell and packaged through the cap. Before packaging, the cap must be electrically connected to the battery cell. Generally, the cap is welded to the pole ear on the corresponding battery cell through a welding device to achieve conduction. When welding the pole ear and the cap, the pole ear must be pressed against the cap to avoid the contact surface between the pole ear and the cap being not flat enough, which may lead to fire and welding through the pole ear during welding.

[0003] For example, a Chinese patent with application number CN202320842292.8 discloses a battery cap welding system, including a tab correction assembly and a tab pressing assembly. The tab pressing assembly includes an actuating rack, a gear, a passive rack and a pressing rod. The actuating rack, the gear and the passive rack cooperate to drive the pressing rod to move backward to press the tab onto the cap.

[0004] However, the structural design of the above-mentioned cap welding system has the following problems during use:

[0005] In the above-mentioned cap welding system, the battery cell is fixed under the cap, and the actuating rack, gear and passive rack cooperate to drive the clamping rod to move, so as to press the pole ear on the battery cell to the inner side of the cap. However, since the inner side of the cap has a step and the side where the clamping rod abuts the pole ear is a flat structure, when the clamping rod presses the pole ear to the cap, the pole ear is bent at a large angle by force, which can easily cause the pole ear to break, thereby resulting in a low welding yield.

[0006] Therefore, there is an urgent need for a welding device and method that can provide sufficient pressing force and avoid breakage of the tab during welding. Summary of the invention

[0007] The purpose of the present disclosure is to overcome the deficiencies in the prior art and to provide a battery cap laser welding method that can provide sufficient pressing force and prevent the tab from breaking during welding.

[0008] The purpose of this disclosure is achieved through the following technical solutions:

[0009] A battery cap laser welding method for preventing tab breakage, using a battery cap welding device for welding, the battery cap welding device comprising:

[0010] A laser welding part, a fixing seat, a pressing mechanism, a cap fixing mechanism and a demagnetizing mechanism, wherein the fixing seat is provided with an embedding groove, wherein the embedding groove is used to embed the battery core, and the cap fixing mechanism comprises a first horizontal driving member and a magnetic column, wherein the first horizontal driving member is installed on the fixing seat, wherein the power output end of the first horizontal driving member is connected to the magnetic column, and the magnetic column is used to magnetically engage with the cap;

[0011] The clamping mechanism includes a second horizontal driving member, a connecting plate and a clamping boss, the second horizontal driving member is installed on the fixing seat, the power output end of the second horizontal driving member is connected to the connecting plate, the connecting plate is fixedly connected to the clamping boss, the clamping boss is arranged opposite to the cap fixing mechanism, a smooth guiding area is provided on a side of the clamping boss adjacent to the magnetic suction column, when the second horizontal driving member drives the clamping boss to move, the smooth guiding area abuts against the pole ear, the connecting plate is provided with a first avoiding hole, the clamping boss is provided with a second avoiding hole corresponding to the first avoiding hole, and the light beam emitted by the laser welding member passes through the first avoiding hole and the second avoiding hole to weld the pole ear to the cap;

[0012] The demagnetization mechanism comprises a connecting frame, a vertical driving member and a blocking plate, wherein the connecting frame is mounted on the fixing seat, the vertical driving member is connected to the connecting frame, the power output end of the vertical driving member is connected to the blocking plate, and the vertical driving member drives the blocking plate to abut against the cap, so that the cap is separated from the magnetic column;

[0013] The battery cap laser welding method for preventing tab breakage comprises the following steps:

[0014] Embed the battery cell in the embedding groove;

[0015] The cap is attracted to the magnetic column, and the first horizontal driving member is started to drive the magnetic column to move so that the cap is arranged opposite to the pole ear of the battery cell;

[0016] The second horizontal driving member is started to drive the pressing boss to move along the direction of the pole ear, so that the pressing boss abuts against the pole ear, and when the pressing boss presses the pole ear against the cap, the pole ear is bent along the direction of the smooth guide area;

[0017] Starting the laser welding part to perform laser welding operation on the cap and the tab;

[0018] The vertical drive member is started to drive the blocking plate to move to the side of the cap away from the clamping boss, and the first horizontal drive member is simultaneously started to drive the magnetic column to move in the direction away from the clamping boss. When the cap abuts against the blocking plate, the forward working power of the first horizontal drive member is increased to provide acceleration for the magnetic column away from the clamping boss, so that the cap can be separated from the magnetic column.

[0019] In one embodiment, the second horizontal driving member drives the pressing boss to move along the direction of the pole ear, so that the pressing boss abuts against the pole ear, and when the pressing boss slowly presses the pole ear against the cap, the pole ear bends along the direction of the smooth guide area, specifically comprising the following steps:

[0020] When the second horizontal driving member drives the pressing boss to abut against the pole ear, the positive working power of the second horizontal driving member is increased to provide acceleration of the pressing boss toward the capping direction, so that the pole ear is closely fitted with the smooth guiding area, and the pole ear is quickly bent along the smooth guiding area;

[0021] When the pole ear is bent along the smooth guide area, the reverse working power of the second horizontal driving member is increased to provide acceleration of the pressing boss in a direction away from the cap, so that the pressing boss slowly presses the pole ear against the cap.

[0022] In one embodiment, the vertical driving member drives the blocking plate to be arranged opposite to the cap, and the first horizontal driving member drives the magnetic column to move in a direction away from the pressing boss. When the cap abuts against the blocking plate, the first horizontal driving member forms an acceleration in a direction away from the pressing boss to make the cap detach from the magnetic column, which specifically includes the following steps:

[0023] When the cap and the pole ear are welded and before the cap and the blocking plate are butted, the vertical driving member is started to drive the blocking plate to move in the direction of the cap, so that the blocking plate and the cap are arranged opposite to each other, and the first horizontal driving member is started at the same time to drive the magnetic column to move at a constant speed in a direction away from the pressing boss, so that the cap and the blocking plate are butted;

[0024] When the cap abuts against the blocking plate, the forward working power of the first horizontal driving member is increased to provide acceleration in a direction in which the magnetic column moves away from the pressing boss, so that the cap is separated from the magnetic column.

[0025] In one embodiment, the cap is attracted to the magnetic column, and the first horizontal driving member drives the magnetic column to move so that the cap is arranged opposite to the tab of the battery cell, which specifically includes the following steps:

[0026] The outer side of the cap is sleeved on the magnetic column, so that the cap and the magnetic column are attracted to each other, and the inner side of the cap is arranged toward the pole ear;

[0027] The first horizontal driving member is activated to drive the magnetic column to move toward the pole ear, so that the pole ear is located between the pressing boss and the cap.

[0028] In one embodiment, the smooth guide area is located at the lower side of the pressing boss.

[0029] In one embodiment, the connecting plate is provided with an avoidance groove, the connecting frame passes through the avoidance groove and is connected to the fixing seat, and the vertical driving member drives the blocking plate to pass through the avoidance groove and then abut against the cover cap.

[0030] In one embodiment, the blocking plate is provided with a blocking groove, and the diameter of the groove wall of the blocking groove is smaller than the diameter of the cap, so that the outer wall of the blocking groove abuts against the cap.

[0031] In one embodiment, the magnetic column includes a magnetic column body and a moving plate, one side of the moving plate is connected to the power output end of the first horizontal driving member, and the other side of the moving plate is connected to the magnetic column body.

[0032] In one embodiment, a first guide rail is disposed on a side of the movable plate adjacent to the connecting plate, the connecting plate is provided with a first guide groove, and the first guide rail is embedded in the first guide groove so that the connecting plate slides along an extension direction of the first guide rail; and / or,

[0033] A second guide rail is disposed on a side of the fixing seat adjacent to the movable plate. The movable plate is provided with a second guide groove. The second guide rail is embedded in the second guide groove so that the movable plate slides along the extending direction of the second guide rail.

[0034] In one of the embodiments, a surface of the smooth guide area is provided with an electroplating layer.

[0035] Compared with the prior art, the present invention has at least the following advantages:

[0036] In the above-mentioned laser welding method for battery caps to prevent the pole ear from breaking, the battery cell is embedded in the embedding groove of the fixing seat, the cap is attracted to the magnetic column, the first horizontal driving member drives the magnetic column to move the cap to a position opposite to the pole ear, the second horizontal driving member drives the connecting plate to move, and then drives the clamping boss to move, so that the clamping boss abuts against the pole ear on the battery cell, and then the pole ear is pressed against the cap. Since a smooth guide area is provided on the side of the clamping boss adjacent to the cap fixing mechanism, and the end of the pole ear is fixed to the battery cell, in the process of the clamping boss pressing the pole ear, the pole ear is tightly attached to the inclined surface of the smooth guide area, so that the bending amplitude of the pole ear is smaller, thereby avoiding the breakage of the pole ear and improving the yield of the pole ear welding. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the technical solutions of the embodiments of the present disclosure, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present disclosure and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0038] Figure 1 A schematic structural diagram of a battery cap welding device according to an embodiment;

[0039] Figure 2 for Figure 1 Another structural schematic diagram of the battery cap welding device shown;

[0040] Figure 3 for Figure 1 A structural schematic diagram of a pressing mechanism of a battery cap welding device shown;

[0041] Figure 4 for Figure 1 Another structural schematic diagram of the battery cap welding device shown;

[0042] Figure 5 for Figure 1 A structural schematic diagram of a demagnetization mechanism of a battery cap welding device shown;

[0043] Figure 6 A process flow chart of a laser welding method for a battery cap to prevent tab breakage according to an embodiment;

[0044] Figure 7 This is a schematic structural diagram of a magnetic column according to an embodiment;

[0045] Figure 8 A schematic structural diagram of a heat dissipation assembly of a battery cap welding device according to an embodiment;

[0046] Fig. 9 for Figure 1 Another structural schematic diagram of the battery cap welding device shown;

[0047] Fig.10 It is a schematic diagram of a bent tab in the prior art;

[0048] Fig.11 A schematic diagram of a tab after bending in a battery cap laser welding method for preventing tab breakage according to an embodiment;

[0049] Fig.12 for Figure 1 A physical picture of the battery cap welding device shown;

[0050] Fig.13 for Figure 1Another pictorial diagram of the battery cap welding device shown. DETAILED DESCRIPTION

[0051] In order to facilitate the understanding of the present disclosure, the present disclosure will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present disclosure are given in the drawings. However, the present disclosure can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present disclosure more thoroughly and comprehensively understood.

[0052] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0053] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present disclosure. The terms used herein in the specification of the present disclosure are only for the purpose of describing specific embodiments and are not intended to limit the present disclosure. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0054] The present invention provides a method for laser welding a battery cap to prevent the tab from breaking, and adopts a battery cap welding device for welding, wherein the battery cap welding device comprises: a laser welding part, a fixing seat, a clamping mechanism, a cap fixing mechanism and a demagnetization mechanism, wherein the fixing seat is provided with an embedding groove, and the embedding groove is used to embed the battery cell, and the cap fixing mechanism comprises a first horizontal driving member and a magnetic suction column, wherein the first horizontal driving member is installed on the fixing seat, and the power output end of the first horizontal driving member is connected to the magnetic suction column, and the magnetic suction column is used to magnetically engage with the cap; the clamping mechanism comprises a second horizontal driving member, a connecting plate and a clamping boss, wherein the second horizontal driving member is installed on the fixing seat, and the power output end of the second horizontal driving member is connected to the connecting plate, and the connecting plate is fixedly connected to the clamping boss, and the The clamping boss is arranged opposite to the cap fixing mechanism, and a smooth guiding area is provided on a side of the clamping boss adjacent to the magnetic suction column. When the second horizontal driving member drives the clamping boss to move, the smooth guiding area abuts against the pole ear, the connecting plate is provided with a first avoiding hole, and the clamping boss is provided with a second avoiding hole corresponding to the first avoiding hole. The light beam emitted by the laser welding member passes through the first avoiding hole and the second avoiding hole to weld the pole ear to the cap; the demagnetization mechanism includes a connecting frame, a vertical driving member and a blocking plate, the connecting frame is installed on the fixing seat, the vertical driving member is connected to the connecting frame, the power output end of the vertical driving member is connected to the blocking plate, and the vertical driving member drives the blocking plate to abut against the cap to separate the cap from the magnetic suction column;

[0055] The laser welding method for preventing the tab breakage of a battery cap comprises the following steps: embedding the battery cell into the embedding groove; engaging the cap with the magnetic column, and the first horizontal driving member drives the magnetic column to move so that the cap and the tab of the battery cell are arranged relative to each other; the second horizontal driving member drives the clamping boss to move in the direction of the tab so that the clamping boss abuts against the tab, and when the clamping boss slowly presses the tab against the cap, the tab bends in the direction of the smooth guide area; starting the laser welding member to weld the cap to the tab; when the welding of the cap and the tab is completed, the vertical driving member drives the blocking plate to be arranged relative to the cap, and the first horizontal driving member drives the magnetic column to move in the direction away from the clamping boss, and when the cap abuts against the blocking plate, the first horizontal driving member forms an acceleration in the direction away from the clamping boss so that the cap is separated from the magnetic column.

[0056] In the above-mentioned laser welding method for battery caps to prevent the pole ear from breaking, the battery cell is embedded in the embedding groove of the fixing seat, the cap is attracted to the magnetic column, the first horizontal driving member drives the magnetic column to move the cap to a position opposite to the pole ear, the second horizontal driving member drives the connecting plate to move, and then drives the clamping boss to move, so that the clamping boss abuts against the pole ear on the battery cell, and then the pole ear is pressed against the cap. Since a smooth guide area is provided on the side of the clamping boss adjacent to the cap fixing mechanism, and the end of the pole ear is fixed to the battery cell, in the process of the clamping boss pressing the pole ear, the pole ear is tightly attached to the inclined surface of the smooth guide area, so that the bending amplitude of the pole ear is smaller, thereby avoiding the breakage of the pole ear and improving the yield of the pole ear welding.

[0057] In order to better understand the technical solutions and beneficial effects of the present invention, the present invention is further described in detail below in conjunction with specific embodiments:

[0058] like Figures 1 to 4 As shown, a laser welding method for a battery cap to prevent the tab from breaking in one embodiment adopts a battery cap welding device 10 for welding, and the battery cap welding device 10 comprises: a laser welding part 100, a fixing seat 200, a clamping mechanism 300, a cap fixing mechanism 400 and a demagnetization mechanism 500, the fixing seat 200 is provided with an embedding groove 210, the embedding groove 210 is used to embed the battery cell 10a, the cap fixing mechanism 400 comprises a first horizontal driving member 410 and a magnetic column 420, the first horizontal driving member 410 is installed on the fixing seat 200, the power output end of the first horizontal driving member 410 is connected to the magnetic column 420, and the magnetic column 420 is used to magnetically engage with the cap 10b, so that the first horizontal driving member 410 drives the magnetic column 420 to move the cap 10b to a position opposite to the tab 10c.

[0059] Furthermore, the clamping mechanism 300 includes a second horizontal driving member 310, a connecting plate 320 and a clamping boss 330, the second horizontal driving member 310 is installed on the fixing seat 200, the power output end of the second horizontal driving member 310 is connected to the connecting plate 320, the connecting plate 320 is fixedly connected to the clamping boss 330, the clamping boss 330 is arranged opposite to the cap fixing mechanism 400, and a smooth guide area 331 is provided on a side of the clamping boss 330 adjacent to the magnetic suction column 420, when the second horizontal driving member 410 drives the clamping boss 330 to move, the smooth guide area 331 abuts against the pole ear 10c, the connecting plate 320 is provided with a first avoidance hole, the clamping boss 330 is provided with a second avoidance hole corresponding to the first avoidance hole, and the light beam emitted by the laser welding member 100 passes through the first avoidance hole and the second avoidance hole to weld the pole ear to the cap.

[0060] Furthermore, the demagnetization mechanism 500 includes a connecting frame 510, a vertical driving member 520 and a blocking plate 530. The connecting frame 510 is installed on the fixed seat 200, the vertical driving member 520 is connected to the connecting frame 510, the power output end of the vertical driving member 520 is connected to the blocking plate 530, and the vertical driving member 520 drives the blocking plate 530 to abut against the cap 10b to separate the cap 10b from the magnetic suction column 420.

[0061] In this embodiment, the battery cell 10a is embedded in the embedding groove 210, and the magnetic column 420 attracts and fixes the cap 10b. The first horizontal driving member 410 drives the magnetic column 420 to move to move the cap 10b to a position opposite to the pole ear 10c. The second horizontal driving member 310 drives the clamping boss 330 to press the pole ear 10c against the inner side of the cap 10b. Since a smooth guide area 331 is provided on a side of the clamping boss 330 adjacent to the magnetic column 420, and the end of the pole ear 10c is fixed in the battery cell 10a, when the clamping boss 330 presses the pole ear 10c against the cap 10b, the pole ear 10c fits tightly with the smooth guide area 331, so that the pole ear 10c is bent along the inclined surface of the smooth guide area 331, thereby making the bending angle of the pole ear 10c smaller to avoid the pole ear 10c from breaking during the welding process.

[0062] like Figures 1 to 6 As shown, the battery cap laser welding method for preventing tab breakage comprises the following steps:

[0063] S100: embed the battery cell 10a into the embedding groove 210. In this embodiment, the battery cell 10a is embedded into the embedding groove 210, so that the battery cell 10a is fixed on the fixing seat 200, and the tab 10c on the battery cell 10a is arranged opposite to the cap 10b.

[0064] S200: The cap 10b is attracted to the magnetic column 420, and the first horizontal driving member 410 is activated to drive the magnetic column 420 to move, so that the cap 10b is arranged opposite to the tab 10c of the battery cell 10a.

[0065] In this embodiment, since the cap 10b is made of metal, after the cap 10b is magnetically fixed by the magnetic column 420, the first horizontal driving member 410 drives the magnetic column 420 to move in the horizontal direction, and when the magnetic column 420 moves to a preset position, the cap 10b is arranged opposite to the tab 10c of the battery cell 10a. Further, the first horizontal driving member 410 can be a cylinder or a motor.

[0066] S300: Start the second horizontal driving member 310 to drive the pressing boss 330 to move along the direction of the pole lug 10c, so that the pressing boss 330 abuts against the pole lug 10c, and when the pressing boss 330 presses the pole lug 10c against the cap 10b, the pole lug 10c bends along the direction of the smooth guide area 331.

[0067] In this embodiment, the second horizontal driving member 310 drives the connecting plate 320 to move horizontally, thereby driving the clamping boss 330 to move along the direction of the pole ear 10c, so that the clamping boss 330 abuts against the pole ear 10c. In the process of the clamping boss 330 clamping the pole ear 10c against the cap 10b, the pole ear 10c is closely fitted with the smooth guide area 331, so that the pole ear 10c is bent along the inclined surface of the smooth guide area 331, so as to reduce the bending angle of the pole ear 10c and avoid the breakage of the pole ear 10c. It should be noted that when the clamping boss 330 clamps the pole ear 10c against the inner side of the cap 10b, the force of the clamping boss 330 on the pole ear 10c is reduced, so that the clamping boss 330 slowly clamps the pole ear 10c against the inner side of the cap 10b, avoiding damage to the pole ear 10c and the cap 10b. Furthermore, the second horizontal driving member 310 is a cylinder or a motor.

[0068] S400: Start the laser welding unit 100 to perform laser welding operation on the cap 10b and the tab 10c.

[0069] In this embodiment, the laser welding component 100 is a laser device. After the clamping boss 330 presses the pole ear 10c against the inner side of the cap 10b, the laser welding component 100 is started. Since the connecting plate 320 is provided with a first avoidance hole, the clamping boss 330 is provided with a second avoidance hole corresponding to the first avoidance hole, and the first avoidance hole is connected to the second avoidance hole, the light beam emitted by the laser welding component 100 passes through the first avoidance hole and the second avoidance hole in sequence, and then acts on the inner side of the pole ear 10c and the cap 10b, so that the cap 10b and the pole ear 10c are welded.

[0070] S500: Start the vertical drive member 520 to drive the blocking plate 530 to move to the side of the cap 10b away from the clamping boss 330, and simultaneously start the first horizontal drive member 410 to drive the magnetic column 420 to move in the direction away from the clamping boss 330. When the cap 10b abuts against the blocking plate 530, the forward working power of the first horizontal drive member 410 is increased to provide acceleration in the direction of the magnetic column away from the clamping boss 330, so that the cap 10b is separated from the magnetic column 420.

[0071] In this embodiment, after the cap 10 b and the tab 10 c are welded, the cap 10 b is attracted to the magnetic post 420 , and the cap 10 b needs to be demagnetized to separate the cap 10 b from the magnetic post 420 . Specifically, the vertical driving member 520 drives the blocking plate 530 to move in the vertical direction so that the blocking plate 530 moves to a position opposite to the cap 10b, that is, the blocking plate 530 is arranged adjacent to the cap 10b. At this time, the first horizontal driving member 410 drives the magnetic column 420 to move in a direction away from the clamping boss 330, thereby driving the blocking plate 530 to move together. When the cap 10b abuts against the blocking plate 530, the first horizontal driving member 410 increases the forward working power, so that the force of the magnetic column 420 moving toward the cap 10b increases, so that the first horizontal driving member 410 forms an acceleration away from the clamping boss 330, that is, the first horizontal driving member 410 increases the force when the cap 10b and the blocking plate 530 abut instantly, so that the cap 10b can quickly detach from the magnetic column 420, so as to prevent the cap 10b from tearing off the pole ear 10c during the process of detaching from the magnetic column 420.

[0072] In the above-mentioned laser welding method for preventing the tab from breaking, the battery cell 10a is embedded in the embedding groove 210 of the fixing seat 200, and the cap 10b is attracted to the magnetic column 420. The first horizontal driving member 410 drives the magnetic column 420 to move the cap 10b to a position opposite to the tab 10c. The second horizontal driving member 310 drives the connecting plate 320 to move, thereby driving the pressing boss 330 to move, so that the pressing boss 330 abuts against the tab 10c on the battery cell 10a, thereby The pole lug 10c is pressed against the cap 10b. Since a smooth guide area 331 is provided on one side of the pressing boss 330 adjacent to the cap fixing mechanism 400, and the end of the pole lug 10c is fixed to the battery cell 10a, when the pressing boss 330 presses the pole lug 10c, the pole lug 10c is tightly attached to the inclined surface of the smooth guide area 331, thereby reducing the bending amplitude of the pole lug 10c, avoiding breakage of the pole lug 10c, and improving the welding yield of the pole lug 10c.

[0073] In one embodiment, the second horizontal driving member 310 drives the pressing boss 330 to move along the direction of the pole ear 10c, so that the pressing boss 330 abuts against the pole ear 10c, and when the pressing boss 330 slowly presses the pole ear 10c against the cap 10b, the pole ear 10c bends along the direction of the smooth guide area 331, specifically including the following steps:

[0074] When the second horizontal driving member 310 drives the pressing boss 330 to abut against the pole ear 10c, the forward working power of the second horizontal driving member 310 is increased to provide acceleration of the pressing boss 330 toward the cap 10b, so that the pole ear 10c is closely fitted with the smooth guide area 331, and the pole ear 10c is quickly bent along the smooth guide area 331;

[0075] When the pole lug 10c is bent along the smooth guide area 331, the reverse working power of the second horizontal driving member 310 is increased to provide acceleration of the pressing boss away from the cap 10b, so that the pressing boss 330 slowly presses the pole lug 10c against the cap 10b.

[0076] In this embodiment, when the clamping boss 330 abuts against the pole lug 10c, the forward working power of the second horizontal driving member 310 is increased, so that the second horizontal driving member 310 forms an acceleration along the direction of the cap 10b, that is, the second horizontal driving member 310 increases the force of the clamping boss 330 on the pole lug 10c, so that the pole lug 10c bends quickly along the inclined surface of the smooth guide area 331 to avoid the pole lug 10c from breaking during the bending process. Furthermore, after the pole lug 10c is bent along the inclined surface of the smooth guide area 331, the reverse working power of the second horizontal driving member 310 is increased, so that the second horizontal driving member 310 forms an acceleration away from the direction of the cap 10b, that is, the force of the clamping boss 330 on the pole lug 10c is reduced, so that the speed of the pole lug 10c is smaller when it abuts against the cap 10b, and the clamping boss 330 has a smaller force when pressing the pole lug 10c against the inner side surface of the cap 10b, thereby preventing the pole lug 10c from hitting the inner side surface of the cap 10b, and thus preventing the pole lug 10c and the cap 10b from being damaged.

[0077] In one embodiment, the vertical driving member 520 drives the blocking plate 530 to be arranged opposite to the cap 10b, and the first horizontal driving member 410 drives the magnetic column 420 to move in a direction away from the pressing boss 330. When the cap 10b abuts against the blocking plate 530, the first horizontal driving member 410 forms an acceleration in a direction away from the pressing boss 330, so that the cap 10b is separated from the magnetic column 420, which specifically includes the following steps:

[0078] After the cap 10b and the pole ear 10c are welded and before the cap abuts against the blocking plate, the vertical driving member 520 is started to drive the blocking plate 530 to move in the direction of the cap 10b, so that the blocking plate 530 and the cap 10b are arranged opposite to each other, and the first horizontal driving member 410 is started at the same time to drive the magnetic column 420 to move at a constant speed in a direction away from the pressing boss 330, so that the cap 10b abuts against the blocking plate 530;

[0079] When the cap 10 b contacts the blocking plate 530 , the forward working power of the first horizontal driving member 410 is increased to provide acceleration in the direction of the magnetic column moving away from the pressing boss 330 , so that the cap 10 b is separated from the magnetic column 420 .

[0080] In this embodiment, before the cap 10b abuts against the blocking plate 530, the first horizontal driving member 410 drives the magnetic column 420 to move at a uniform speed in the direction of the clamping boss 330. At this time, the force exerted by the first horizontal driving member 410 on the magnetic column 420 is relatively small, so that the instantaneous speed when the cap 10b abuts against the blocking plate 530 is relatively small, so that when the cap 10b abuts against the blocking plate 530, the force between the cap 10b and the blocking plate 530 is relatively small, thereby avoiding the cap 10b hitting the blocking plate 530 and causing damage to the cap 10b. Furthermore, when the cap 10b abuts against the blocking plate 530, the forward working power of the first horizontal driving member 410 is increased, so that the first horizontal driving member 410 forms an acceleration in the direction away from the clamping boss 330, that is, the first horizontal driving member 410 increases the force of the magnetic column 420 along the direction of the blocking plate 530, so that at the moment the cap 10b abuts against the blocking plate 530, the force between the cap 10b and the blocking plate 530 increases, thereby causing the cap 10b to quickly detach from the magnetic column 420.

[0081] In one embodiment, the cap 10b is attracted to the magnetic column 420, and the first horizontal driving member 410 drives the magnetic column 420 to move so that the cap 10b is arranged opposite to the tab 10c of the battery cell 10a, which specifically includes the following steps:

[0082] The outer side of the cap 10b is sleeved on the magnetic pole 420, so that the cap 10b and the magnetic pole 420 are attracted to each other, and the inner side of the cap 10b is arranged toward the pole ear 10c;

[0083] The first horizontal driving member 410 is activated to drive the magnetic pole 420 to move toward the pole tab 10 c , so that the pole tab 10 c is located between the pressing boss 330 and the cap 10 b .

[0084] In this embodiment, the inner side of the cap 10b needs to be welded with the pole ear 10c. By sleeved the outer side of the cap 10b on the magnetic column 420, the diameter of the cap 10b is adapted to the diameter of the magnetic column 420. When the outer side of the cap 10b is sleeved on the magnetic column 420, the inner side of the cap 10b just corresponds to the position of the laser welding part 100, thereby improving the accuracy of the welding between the cap 10b and the pole ear 10c and reducing the need for repositioning. Further, the first horizontal driving member 410 drives the magnetic column 420 to move along the direction of the pole ear 10c to adjust the welding distance between the cap 10b and the laser welding part 100.

[0085] like Figure 3 As shown, in one embodiment, the smooth guide area 331 is located at the lower side of the clamping boss 330. In this embodiment, the battery cell 10a is located below the clamping boss 330, and the pole lug 10c is located between the clamping boss 330 and the magnetic column 420. By setting the smooth guide area 331 on the lower side of the clamping boss 330, when the clamping boss 330 presses the pole lug 10c onto the cap 10b, the pole lug 10c is pressed against the chamfered surface of the smooth guide area 331 to reduce the bending angle of the pole lug 10c, thereby avoiding the breakage of the pole lug 10c. Furthermore, the position of the smooth guide area 331 should be adapted to the position between the battery cell 10a and the clamping boss 330. For example, when the battery cell 10a is located on the side of the clamping boss 330, the smooth guide area 331 should be set on the side of the clamping boss 330.

[0086] like Figure 2 As shown, in one embodiment, the connecting plate 320 is provided with a position-avoiding groove 321, the connecting frame 510 passes through the position-avoiding groove 321 to connect with the fixing seat 200, and the vertical driving member 520 drives the blocking plate 530 to pass through the position-avoiding groove 321 and then abuts against the cap 10b. It can be understood that by providing the position-avoiding groove 321 on the connecting plate 320, and the connecting frame 510 passes through the position-avoiding groove 321 and is installed on the fixing seat 200, when the vertical driving member 520 drives the blocking plate 530 to move to a position opposite to the cap 10b, the blocking plate 530 is located between the pressing boss 330 and the connecting frame 510, so that the blocking plate 530 separates the cap 10b from the magnetic column 420, and the design of the position-avoiding groove 321 of the connecting plate 320 makes the structure of the cap fixing mechanism 400 more compact.

[0087] like Figure 5 As shown, in one embodiment, the blocking plate 530 is provided with a blocking groove 531, and the groove wall diameter of the blocking groove 531 is smaller than the diameter of the cap 10b, so that the outer wall of the blocking groove 531 abuts against the cap 10b. It can be understood that the blocking plate 530 is provided with a blocking groove 531, and the groove wall diameter of the blocking groove 531 is smaller than the diameter of the cap 10b. When the vertical driving member 520 drives the blocking plate to move to a position opposite to the cap 10b, the first horizontal driving member 410 drives the magnetic column 420 to move. At this time, the outer wall of the blocking groove 531 abuts against the periphery of the cap 10b. Under the blocking action of the blocking plate 530, the cap 10b is separated from the magnetic column 420, and the magnetic column 420 passes through the blocking groove 531 and returns to its original position. Furthermore, the blocking groove 531 may be U-shaped or semicircular, so that the outer wall of the blocking groove 531 and the cap 10 b may abut over a larger area, thereby better blocking and separating the cap 10 b from the magnetic column 420 .

[0088] like Figure 4 As shown, in one embodiment, the magnetic column 420 includes a magnetic column body 421 and a moving plate 422, one side of the moving plate 422 is connected to the power output end of the first horizontal driving member 410, and the other side of the moving plate 422 is connected to the magnetic column body 421. It can be understood that one side of the moving plate 422 is connected to the power output end of the first horizontal driving member 410, and the other side of the moving plate 422 is connected to the magnetic column body 421, so that the first horizontal driving member 410 drives the moving plate 422 to move, thereby driving the magnetic column body 421 to move, and the magnetic column body 421 is used to magnetically attract and close the cap 10b.

[0089] like Figure 4 As shown, in one embodiment, the first guide rail 422a is provided on a side of the movable plate 422 adjacent to the connecting plate 320, and the connecting plate 320 is provided with a first guide groove, and the first guide rail 422a is embedded in the first guide groove, so that the connecting plate 320 slides along the extending direction of the first guide rail 422a. It can be understood that the movable plate 422 and the connecting plate 320 are slidably connected through the first guide rail 422a, so that the movable plate 422 plays a supporting and fixing role on the connecting plate 320, reduces the gravity on the power output end of the first horizontal driving member 410, and improves the service life of the device.

[0090] like Figure 4 As shown, in one embodiment, the second guide rail 220 is provided on a side of the fixed seat 200 adjacent to the moving plate 422, and the moving plate 422 is provided with a second guide groove, and the second guide rail 220 is embedded in the second guide groove, so that the moving plate 422 slides along the extension direction of the second guide rail 220. It can be understood that the moving plate 422 and the fixed seat 200 are slidably connected through the second guide rail 220, so that the fixed seat 200 supports and fixes the moving plate 422, reduces the gravity on the power output end of the second horizontal driving member 310, and improves the service life of the device.

[0091] In one embodiment, the surface of the smooth guide area 331 is provided with an electroplated layer. It is understandable that the surface of the smooth guide area 331 is attached with an electroplated metal layer, such as a silver layer or a copper layer, which is attached to the surface of the smooth guide area 331 through an electroplating process, so that the surface of the smooth guide area 331 is smooth and has no burrs, so that when the smooth guide area 331 abuts against the pole ear 10c, the pole ear 10c will not be damaged, and the pole ear 10c can be better bent along the chamfered inclined surface of the smooth guide area 331, thereby making the welding effect of the pole ear 10c and the cap 10b better.

[0092] It is understandable that since the outer side of the cap is sleeved on the magnetic column and is magnetically attracted to the magnetic column to play a positioning and fixing role, that is, the outer periphery of the cap is adapted to the diameter of the magnetic column, when it comes to caps of different sizes, the adaptability of the magnetic column is poor, which in turn leads to poor fixing and positioning effects of the magnetic column. Therefore, in order to improve the adaptability of the magnetic column, in one implementation, the cap fixing mechanism also includes a fastener, the magnetic column is provided with a first connecting hole, the power output end of the first horizontal drive member is provided with a second connecting hole, the first connecting hole and the second connecting hole are correspondingly arranged, and the fastener passes through the first connecting hole and the second connecting hole in sequence, so that the power output end of the first horizontal drive member is connected to the magnetic column through the fastener. In this embodiment, the fastener is a screw, and the screw passes through the first connection hole and the second connection hole in sequence, so that the first horizontal driving member is screwed to the magnetic column, that is, the power output end of the first horizontal driving member is detachably connected to the magnetic column, and the disassembly and assembly of the magnetic column is more convenient. When it comes to caps of different sizes, the magnetic columns of different models and sizes can be replaced to make the magnetic column compatible with the cap, thereby making the adaptability of the magnetic column higher. Furthermore, in other embodiments, the magnetic column can also be connected to the power output end of the first horizontal driving member by snapping, such as the magnetic column is provided with a slot, the power output end of the first horizontal driving member is provided with a snap column, and the snap column is snapped into the slot, so that the disassembly and assembly of the magnetic column is more convenient.

[0093] Furthermore, since the magnetic column 420 uses a permanent magnet, that is, the magnetic attraction force of the magnetic column 420 cannot be changed, when it comes to caps with greater thickness and weight, the magnetic attraction force of the magnetic column 420 is smaller, resulting in the cap not being completely attracted to the magnetic column 420, and thus causing the cap to fall off the magnetic column 420. Therefore, in order to improve the adaptability of the magnetic column 420 to caps of different thicknesses and weights, as Figure 7As shown, in one embodiment, the magnetic pole 420 includes a metal rod 420a, an electromagnetic body 420b, a sliding paddle 420c, a coil 420d, a first terminal 420e and a second terminal 420f, the coil 420d is wound along the length direction of the electromagnetic body 420b, the electromagnetic body 420b is connected to the metal rod 420a, one end of the sliding paddle 420c is slidably arranged on the metal rod 420a, and the other end of the sliding paddle 420c is abutted against the coil 420d, the first terminal 420e is connected to the coil 420d, and the second terminal 420f is connected to the sliding paddle 420c. In this embodiment, the coil 420d is wound along the length direction of the electromagnetic body 420b, the sliding paddle 420c is slidably set on the metal rod 420a, the sliding paddle 420c is in contact with the coil 420d, the first terminal 420e is connected to the coil 420d, and the second terminal 420f is connected to the sliding paddle 420c. When the current connected to the first terminal 420e is fixed, the first terminal 420e, the coil 420d, the sliding paddle 420c and the second terminal 420f form a loop, and by sliding the sliding paddle 420c The position makes the sliding paddle 420c slide along the length direction of the electromagnetic body 420b, so that the sliding paddle 420c abuts against the coil 420d with different numbers of turns, and the magnetic force of the electromagnetic body 420b is proportional to the number of turns of the coil 420d, that is, the larger the number of turns of the coil 420d, the larger the magnetic force of the electromagnetic body 420b, thereby realizing the adjustment of the magnetic force of the electromagnetic body 420b. In this way, the electromagnetic body 420b is more adaptable to caps of different thicknesses and weights, so that the magnetic attraction effect of the electromagnetic body 420b on the cap is better.

[0094] Furthermore, when the laser welding part welds the pole ear and the cap, the instantaneous heat generated is relatively large, and the heat is transferred from the welding point between the pole ear and the cap to the periphery of the cap. In particular, when the cap is adsorbed by an electromagnet, the electromagnet will also generate heat when it is energized, which further increases the heat transferred to the cap. The high temperature easily causes the cap to deform, resulting in a decrease in the product yield of the cap. Therefore, in order to improve the heat dissipation performance of the cap, such as Figure 8As shown, in one embodiment, the cap fixing mechanism 400 also includes a heat dissipation component 430, and the heat dissipation component 430 includes a heat dissipation base 431 and a plurality of heat dissipation fins 432. The heat dissipation base 431 is connected to the inner side surface of the magnetic column facing away from the cap, and the outer side surface of the magnetic column is used to be attracted to the cap. A plurality of heat dissipation fins 432 are sequentially and spaced apart on a side surface of the heat dissipation base 431 facing away from the cap. The heat dissipation fin 432 located in the middle of the heat dissipation base 431 has the largest length, and the length of the plurality of heat dissipation fins 432 gradually decreases from the middle of the heat dissipation base 431 to both sides, and the heat dissipation fins 432 located on both sides of the middle heat dissipation fin 432 have a preset angle with the heat dissipation base 431; each of the heat dissipation fins 432 is provided with a heat dissipation hole 432a, and the heat dissipation holes 432a of two adjacent heat dissipation fins 432 are staggered. In this embodiment, a vent hole is provided on a side of the magnetic column away from the heat dissipation component 430, and the vent hole is arranged opposite to the heat dissipation component 430. The heat dissipation base 431 in the heat dissipation component 430 is connected to the inner side of the magnetic column, and a plurality of heat dissipation fins 432 are arranged at intervals on the heat dissipation base 431, so that heat is transferred from the magnetic column to the heat dissipation base 431, and then from the heat dissipation base 431 to the heat dissipation fins 432, thereby increasing the heat dissipation area of ​​the magnetic column and achieving a better heat dissipation effect of the magnetic column. Furthermore, the light beam emitted by the laser welding part acts on the pole ear and the cap, and the position where the pole ear and the cap are welded abuts against the middle of the magnetic column. During the welding process, the heat is first transferred to the middle of the magnetic column, that is, the heat in the middle of the magnetic column is the largest, so the heat dissipation performance requirement of the middle of the magnetic column is higher, by providing a plurality of heat dissipation fins 432 on the heat dissipation base 431, and the heat dissipation fins 432 located in the middle of the heat dissipation base 431 are the longest, and the heat dissipation fins 432 in the middle of the heat dissipation base 431 are longer than the heat dissipation base 431. The length of the periphery gradually decreases, and the length of the plurality of heat sink fins 432 gradually decreases from the middle of the heat sink base 431 to the periphery of the heat sink base 431, that is, the plurality of heat sink fins 432 are distributed in a stepped manner. Since the heat sink fins 432 located in the middle of the heat sink base 431 have the largest length, that is, the heat dissipation area in the middle of the heat sink base 431 is the largest, when the heat in the middle of the magnetic column is transferred to the middle of the heat sink base 431, the heat sink fins 432 located in the middle can dissipate the heat in time, thereby improving the heat dissipation effect on the middle of the magnetic column. Furthermore, the heat sink fins 432 located on both sides of the middle heat sink fin 432 are at a preset angle with the heat sink base 431, which is 45°-60°. The heat sink fins 432 on both sides are symmetrically arranged relative to the middle heat sink fin 432, thereby reducing the air flow resistance, and the heat dissipation holes 432a of two adjacent heat sink fins 432 are staggered, which increases the turbulence of the heat sink fins 432 on the air, thereby increasing the contact area between the heat sink fins 432 and the flowing air, further improving the heat dissipation effect on the magnetic column, thereby avoiding the deformation problem of the cap magnetically attracted to the magnetic column due to high temperature.It is understandable that after the welding of the pole ear and the cap is completed, the cap needs to be separated from the magnetic column by the demagnetization mechanism, that is, when the vertical driving member drives the blocking plate to move to a position opposite to the cap, the first horizontal driving member drives the magnetic column to move along the direction of the blocking plate, so that the cap on the magnetic column collides with the blocking plate, and then the cap is separated from the magnetic column. However, since the force when the cap collides with the blocking plate is difficult to control, the cap is easily damaged, resulting in a decrease in product yield. Therefore, in order to improve the product yield, in one embodiment, the demagnetization mechanism also includes a first buffer elastic sheet, which is connected to a side of the blocking plate adjacent to the clamping boss, so that when the first horizontal driving member drives the magnetic column to move, the first buffer elastic sheet abuts against the cap. In this embodiment, the first buffer elastic sheet can be made of elastic materials such as silicone or rubber, and is bonded to a side of the blocking plate adjacent to the clamping boss through an adhesive layer. When the first horizontal driving member drives the magnetic column to move, the cap on the magnetic column moves together until the cap abuts against the first buffer elastic sheet. Since the first buffer elastic sheet has elastic properties, when the cap collides with the first buffer elastic sheet, the rigidity of the cap can be reduced, thereby avoiding damage to the cap due to collision during demagnetization, thereby improving the yield of the product.

[0095] Furthermore, when the pole ear 10c is welded to the cap 10b, the pole ear 10c needs to be pressed against the inner side of the cap 10b by the pressing boss 330, and the outer side of the cap 10b abuts against the magnetic column 420. In this way, when the pressing boss 330 applies a large force to press the pole ear 10c, the rigid force between the outer side of the cap 10b and the magnetic column 420 is large, which causes damage to the cap 10b. After long-term use, the magnetic column 420 is easily damaged and cracked, resulting in a reduction in the magnetic attraction force of the magnetic column 420. Therefore, in order to avoid the above problems, Figure 2 and Fig. 9As shown, in one embodiment, the clamping mechanism 300 also includes a second buffer elastic sheet 340, and a receiving groove 423 is opened in the middle of a side surface of the magnetic column 420 adjacent to the clamping boss 330, the second buffer elastic sheet 340 is located in the receiving groove 423 and is connected to the magnetic column 420, the thickness of the second buffer elastic sheet 340 is the same as the depth of the receiving groove 423, and there is a preset gap between the periphery of the second buffer elastic sheet 340 and the groove wall of the receiving groove 423. In this embodiment, the accommodating groove 423 is opened in the middle part of the magnetic column 420, and the second buffer elastic sheet 340 is located in the accommodating groove 423 and connected to the magnetic column 420, so that when the clamping boss 330 presses the pole ear 10c to the inner side of the cap 10b, the outer side of the cap 10b abuts against the second buffer elastic sheet 340. The second buffer elastic sheet 340 is made of materials such as silicone or rubber and has elastic properties, thereby reducing the rigid force on the outer side of the cap 10b and avoiding damage to the cap 10b. Furthermore, the thickness of the second buffer elastic sheet 340 is the same as the depth of the accommodating groove 423, so that the side structure of the magnetic column 420 adjacent to the clamping boss 330 is flat. When the clamping boss 330 presses the pole ear 10c to the inner side of the cap 10b, the second buffer elastic sheet 340 is deformed, and the deformation amount of the second buffer elastic sheet 340 is small, thereby ensuring the flatness of the contact between the pole ear 10c and the inner side of the cap 10b, so that the welding effect of the pole ear 10c and the cap 10b is better. Furthermore, there is a preset gap between the periphery of the second buffer elastic sheet 340 and the groove wall of the accommodating groove 423. The second buffer elastic sheet 340 is bonded to the bottom wall of the accommodating groove 423 by an adhesive layer. When the second buffer elastic sheet 340 is damaged due to long-term use, it is necessary to replace the second buffer elastic sheet 340 to ensure the accuracy of welding between the pole ear 10c and the inner side of the cap 10b. The second buffer elastic sheet 340 is scraped off by a scraper through the preset gap, and then a new second buffer elastic sheet 340 is bonded to the accommodating groove 423. This makes the replacement of the second buffer elastic sheet 340 more convenient.

[0096] Compared with the prior art, the present invention has at least the following advantages:

[0097] In the above-mentioned laser welding method for preventing the tab from breaking, the battery cell 10a is embedded in the embedding groove 210 of the fixing seat 200, and the cap 10b is attracted to the magnetic column 420. The first horizontal driving member 410 drives the magnetic column 420 to move the cap 10b to a position opposite to the tab 10c. The second horizontal driving member 310 drives the connecting plate 320 to move, thereby driving the pressing boss 330 to move, so that the pressing boss 330 abuts against the tab 10c on the battery cell 10a, thereby The pole lug 10c is pressed against the cap 10b. Since a smooth guide area 331 is provided on one side of the pressing boss 330 adjacent to the cap fixing mechanism 400, and the end of the pole lug 10c is fixed to the battery cell 10a, when the pressing boss 330 presses the pole lug 10c, the pole lug 10c is tightly attached to the inclined surface of the smooth guide area 331, thereby reducing the bending amplitude of the pole lug 10c, avoiding breakage of the pole lug 10c, and improving the welding yield of the pole lug 10c.

[0098] The above-mentioned embodiments only express several implementation methods of the present disclosure, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present disclosure, and these all belong to the protection scope of the present disclosure. Therefore, the protection scope of the patent of the present disclosure shall be subject to the attached claims.

Claims

1. A laser welding method for battery caps to prevent tab breakage, characterized in that: Laser welding is performed using a battery cap welding device, the battery cap welding device comprising: A laser welding part, a fixing seat, a pressing mechanism, a cap fixing mechanism and a demagnetizing mechanism, wherein the fixing seat is provided with an embedding groove, wherein the embedding groove is used to embed the battery core, and the cap fixing mechanism comprises a first horizontal driving member and a magnetic column, wherein the first horizontal driving member is installed on the fixing seat, wherein the power output end of the first horizontal driving member is connected to the magnetic column, and the magnetic column is used to magnetically engage with the cap; The clamping mechanism includes a second horizontal driving member, a connecting plate and a clamping boss, the second horizontal driving member is installed on the fixing seat, the power output end of the second horizontal driving member is connected to the connecting plate, the connecting plate is fixedly connected to the clamping boss, the clamping boss is arranged opposite to the cap fixing mechanism, a smooth guiding area is provided on a side of the clamping boss adjacent to the magnetic suction column, when the second horizontal driving member drives the clamping boss to move, the smooth guiding area abuts against the pole ear, the connecting plate is provided with a first avoiding hole, the clamping boss is provided with a second avoiding hole corresponding to the first avoiding hole, and the light beam emitted by the laser welding member passes through the first avoiding hole and the second avoiding hole to weld the pole ear to the cap; The demagnetization mechanism comprises a connecting frame, a vertical driving member and a blocking plate, wherein the connecting frame is mounted on the fixing seat, the vertical driving member is connected to the connecting frame, the power output end of the vertical driving member is connected to the blocking plate, and the vertical driving member drives the blocking plate to abut against the cap, so that the cap is separated from the magnetic column; The battery cap laser welding method for preventing tab breakage comprises the following steps: Embed the battery cell in the embedding groove; The cap is attracted to the magnetic column, and the first horizontal driving member is started to drive the magnetic column to move so that the cap is arranged opposite to the pole ear of the battery cell; The second horizontal driving member is started to drive the pressing boss to move along the direction of the pole ear, so that the pressing boss abuts against the pole ear, and when the pressing boss presses the pole ear against the cap, the pole ear is bent along the direction of the smooth guide area; Starting the laser welding part to perform laser welding operation on the cap and the tab; The vertical drive member is started to drive the blocking plate to move to the side of the cap away from the clamping boss, and the first horizontal drive member is simultaneously started to drive the magnetic column to move in the direction away from the clamping boss. When the cap abuts against the blocking plate, the forward working power of the first horizontal drive member is increased to provide acceleration for the magnetic column away from the clamping boss, so that the cap can be separated from the magnetic column.

2. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The second horizontal driving member drives the pressing boss to move along the direction of the pole ear, so that the pressing boss abuts against the pole ear, and when the pressing boss slowly presses the pole ear against the cap, the pole ear bends along the direction of the smooth guide area, specifically including the following steps: When the second horizontal driving member drives the pressing boss to abut against the pole ear, the positive working power of the second horizontal driving member is increased to provide acceleration of the pressing boss toward the capping direction, so that the pole ear is closely fitted with the smooth guiding area, and the pole ear is quickly bent along the smooth guiding area; When the pole ear is bent along the smooth guide area, the reverse working power of the second horizontal driving member is increased to provide acceleration of the pressing boss in a direction away from the cap, so that the pressing boss slowly presses the pole ear against the cap.

3. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The vertical driving member drives the blocking plate to be arranged opposite to the cap, and the first horizontal driving member drives the magnetic column to move in a direction away from the pressing boss. When the cap abuts against the blocking plate, the first horizontal driving member generates an acceleration in a direction away from the pressing boss, so that the cap is separated from the magnetic column, which specifically includes the following steps: When the cap and the pole ear are welded and before the cap and the blocking plate are butted, the vertical driving member is started to drive the blocking plate to move in the direction of the cap, so that the blocking plate and the cap are arranged opposite to each other, and the first horizontal driving member is started at the same time to drive the magnetic column to move at a constant speed in a direction away from the pressing boss, so that the cap and the blocking plate are butted; When the cap abuts against the blocking plate, the forward working power of the first horizontal driving member is increased to provide acceleration in a direction in which the magnetic column moves away from the pressing boss, so that the cap is separated from the magnetic column.

4. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The cap is attracted to the magnetic column, and the first horizontal driving member drives the magnetic column to move so that the cap is arranged opposite to the tab of the battery cell, specifically comprising the following steps: The outer side of the cap is sleeved on the magnetic column, so that the cap and the magnetic column are attracted to each other, and the inner side of the cap is arranged toward the pole ear; The first horizontal driving member is activated to drive the magnetic column to move toward the pole ear, so that the pole ear is located between the pressing boss and the cap.

5. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The smooth guide area is located at the lower side of the pressing boss.

6. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The connecting plate is provided with a position-avoiding groove, the connecting frame passes through the position-avoiding groove and is connected with the fixing seat, and the vertical driving member drives the blocking plate to pass through the position-avoiding groove and then abuts against the cover cap.

7. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The blocking plate is provided with a blocking groove, and the groove wall diameter of the blocking groove is smaller than the diameter of the cover cap, so that the outer wall of the blocking groove abuts against the cover cap.

8. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The magnetic column comprises a magnetic column body and a moving plate, one side of the moving plate is connected to the power output end of the first horizontal driving member, and the other side of the moving plate is connected to the magnetic column body.

9. The battery cap laser welding method for preventing tab breakage according to claim 8, characterized in that: A first guide rail is disposed on a side of the movable plate adjacent to the connecting plate, and a first guide groove is formed on the connecting plate. The first guide rail is embedded in the first guide groove so that the connecting plate slides along the extending direction of the first guide rail; and / or, A second guide rail is disposed on a side of the fixing seat adjacent to the movable plate. The movable plate is provided with a second guide groove. The second guide rail is embedded in the second guide groove so that the movable plate slides along the extending direction of the second guide rail.

10. The battery cap laser welding method for preventing tab breakage according to claim 1, characterized in that: The surface of the smooth guide area is provided with an electroplating layer.

Citation Information

Patent Citations

  • Sealed battery and producing method therefor

    CN101908652A

  • Automatic cylindrical battery cap welding machine

    CN104505486A

  • Automatic welding mechanism for cap tab of lithium battery

    CN215698879U

  • DEVICE FOR AUTOMATICALLY ASSEMBLING THE COMPONENTS OF ELECTROCHEMICAL CELLS AND SYSTEM FOR PERFORMING PRODUCTION WORKS ON ELECTROCHEMICAL CELLS

    DE3025508A1

  • Ultrasonic welder for automatically welding safety end cap, tab and punched plate of power battery

    WO2018192249A1