Method for controlling deformation of high-quality nuclear-grade zirconium alloy super-long plate in cold rolling process and application
By controlling parameters such as pass deformation, rolling speed and rolling pressure, and using continuous deviation correction control method, the problem of excessive welds and risk of strip breakage during cold rolling of nuclear-grade zirconium alloy ultra-long plates is solved, and production is improved Efficiency and product quality reduce costs.
Patent Information
- Application Number
- CN202411318700.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-12-03
AI Technical Summary
In the prior art, there are problems of excessive welds, high risk of broken strips and poor product control during the cold rolling process of nuclear-grade zirconium alloy ultra-long plates, resulting in low production efficiency and high metal loss.
By controlling the pass deformation amount, rolling speed, rolling pressure and bending force, the continuous deviation correction control method is used to adjust the rolling parameters to reduce uneven deformation, and dynamic correction of ultra-long plates is achieved, which is suitable for lengths of more than 5 meters. plate rolling.
Significantly reduce welds, improve welding process efficiency, reduce the chance of breaking belts and metal losses, reduce electricity costs, and is suitable for mass industrial production and form economic value.
Smart Images

Figure CN119056868A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of nuclear-grade nonferrous metal processing, and in particular to a method and application for controlling deformation during cold rolling of high-quality nuclear-grade zirconium alloy ultra-long plates. Background Art
[0002] Zirconium alloys are used as positioning bearing materials for reactor cores due to their low thermal neutron absorption cross section, good comprehensive mechanical properties, pressure processing forming properties, welding properties, and high temperature and high pressure water vapor corrosion resistance. The simple production process of nuclear grade zirconium alloys is: hot-rolled slabs → cold rolling of plates → welding into coils → cold rolling of strips → punching of grids. The process flow shows that the strips are welded from multiple sheets of plates. The length of the welded plates in the early stage of production is between 3.5 and 4 meters, resulting in too many welds after coiling. Too many welds increase the risk of strip breaking during the strip rolling process and have a significant adverse effect on the control of grid punching products. Increasing the length of a single sheet is a direct and effective means to solve the problem of too many welds. The conventional product length of cold-rolled plates with a width of 450 to 600 mm is less than 5 meters, so the length of more than 5 meters is defined as an extra-long plate. When rolling extra-long plates, the length of the semi-finished billet and the equipment roller table needs to meet the finished product length requirements, and the uneven deformation of the plate needs to be controlled. Summary of the invention
[0003] The present invention aims to solve one of the technical problems in the related art at least to a certain extent.
[0004] To this end, an embodiment of the present invention provides a method and application for controlling deformation during cold rolling of high-quality nuclear-grade zirconium alloy ultra-long plates.
[0005] In a first aspect, the present invention provides a method for controlling deformation during cold rolling of high-quality nuclear-grade zirconium alloy ultra-long plates, comprising the following steps:
[0006] (a) Select the correct position for feeding;
[0007] (b) When the plate does not have side bending, the rolling is carried out at a pass deformation of 3% to 5% and a rolling speed of 15 to 25 m / min in the early stage of rolling, and at a pass deformation of 1% to 3% and a rolling speed of 5 to 10 m / min in the middle and late stages of rolling;
[0008] (c) When the plate is bent sideways, the deviation is corrected by adjusting the deformation amount, rolling speed, rolling pressure and bending roll force.
[0009] Furthermore, it also includes 2 to 3 passes before the finished product, and the deformation of the passes is controlled within 0.5% to 1.0%.
[0010] Furthermore, the correct position selected in step (a) is to align the center line of the head and tail of the incoming plate material with the center line of the working roller, and the length of the incoming plate material is more than 5m.
[0011] Furthermore, in the step (c), when the side bending depth is below 80 mm, the deformation amount per pass is adjusted to 0.5% to 1%, and the rolling speed is within 10 m / min.
[0012] Furthermore, in the step (c), when the side bending depth is below 80 mm, the single-side rolling pressure is continuously adjusted between 100 and 900 KN in the early and middle stages of rolling.
[0013] Furthermore, when the side bending depth in step (c) is below 80 mm, the single-side rolling pressure is continuously adjusted between 50 and 100 KN in the later stage of rolling.
[0014] Furthermore, in the step (c), when the side bending depth is above 80 mm, the rolling speed is adjusted to 5-10 m / min, the rolling pressure is increased to 200±5 KN, the bending roll force is 0 KN, and the alignment is gradually performed through 2-3 passes.
[0015] Furthermore, in the step (c), when the side bending depth is above 80 mm and dynamic correction cannot be achieved by adjusting the rolling speed, rolling pressure and bending roll force, the machine is stopped and the rolling pressure is completely unloaded, and the plate position is corrected before continuing rolling.
[0016] Furthermore, the side bend in step (c) includes a unilateral bend, an S-bend and a compound bend. When correcting the compound bend, the compound bend is first corrected to the unilateral bend, and then the unilateral bend is aligned.
[0017] In a second aspect, the present invention proposes the application of the method proposed in the first aspect in the cold rolling process of high-quality nuclear-grade zirconium alloy ultra-long plates.
[0018] Compared with the prior art, the beneficial effects of the present invention are:
[0019] The method of the present invention is applied in the cold rolling process of high-quality nuclear-grade zirconium alloy ultra-long plates, which can reduce welds, improve welding process efficiency, reduce the probability of strip breakage, significantly reduce metal loss and electricity costs, and can be easily applied to mass industrial production, thereby generating considerable economic value.
[0020] The present invention adopts a continuous deviation correction control method to continuously correct the deviation of the plate caused by uneven deformation during the dynamic rolling process. It is suitable for the rolling process of ultra-long plates and achieves the purpose of improving product quality and reducing various costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the following description of the embodiments in conjunction with the accompanying drawings, in which:
[0022] Figure 1 This is a flow chart of a method for controlling deformation during cold rolling of high-quality nuclear-grade zirconium alloy ultra-long plates according to the present invention;
[0023] Figure 2 It is a schematic diagram of the structure of the single-side bend of the present invention;
[0024] Figure 3 This is a schematic diagram of the structure of the S-bend of the present invention;
[0025] Figure 4 It is a schematic structural diagram of the composite bend of the present invention. DETAILED DESCRIPTION
[0026] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0027] like Figures 1 to 4 As shown, the method for controlling deformation during cold rolling of high-quality nuclear-grade zirconium alloy ultra-long plates of the present invention comprises the following steps:
[0028] (a) Select the correct position for feeding;
[0029] (b) When the plate does not have side bending, the rolling is carried out at a pass deformation of 3% to 5% and a rolling speed of 15 to 25 m / min in the early stage of rolling, and at a pass deformation of 1% to 3% and a rolling speed of 5 to 10 m / min in the middle and late stages of rolling;
[0030] (c) When the plate is bent sideways, the deviation is corrected by adjusting the deformation amount, rolling speed, rolling pressure and bending roll force.
[0031] In step (a), when unloading, the center line of the semi-finished plate material is aligned with the center line of the working roller to prevent uneven deformation. The length of the plate material is more than 5m.
[0032] In some embodiments, in the first 2 to 3 passes of the finished product, the deformation amount is controlled within 0.5% to 1.0%.
[0033] In step (b), when the plate does not bend sideways, the rolling is carried out at a pass deformation of 3% to 5% and a rolling speed of 15 to 25 m / min in the early stage of rolling, and at a pass deformation of 1% to 3% and a rolling speed of 5 to 10 m / min in the middle and late stages of rolling, which is the overall control strategy for the rolling process.
[0034] After feeding, as the plate is continuously bitten by the roller, the transverse movement has the characteristic of acceleration. The thickness difference between the two sides can reach 0.10-0.20mm or 7%-12%, which can cause the plate to be pulled or the edge torn, so it must be corrected in time at the initial stage of transverse movement.
[0035] In step (c), when the side bending depth is below 80 mm, the pass deformation is adjusted to 0.5% to 1%, and the rolling speed is within 10 m / min to improve the uneven deformation.
[0036] In some embodiments, moderate and continuous adjustment of the unilateral rolling pressure can effectively reduce or improve the degree of deviation of the plate. In the early and middle stages of rolling, the deviation adjustment pressure value range is 100-900KN. Exceeding this range may cause reverse deviation, thus forming a compound bend. After the deviation correction is completed, the unilateral rolling pressure is restored to the initial setting value. In the late stage of rolling, the unilateral rolling pressure is continuously adjusted between 50 and 100KN. Exceeding this range may cause reverse deviation, thus forming a compound bend. After the deviation correction is completed, the unilateral rolling pressure is restored to the initial setting value.
[0037] When the side bending depth in step (c) is above 80 mm, the rolling speed is adjusted to 5-10 m / min, the rolling pressure is raised to 200±5 KN, the bending roll force is 0 KN, and the alignment is gradually performed through 2-3 passes.
[0038] In step (c), when the side bending depth is above 80 mm and dynamic correction cannot be achieved by adjusting the rolling speed, rolling pressure and bending roll force, the machine is stopped and the rolling pressure is completely unloaded, and the plate position is corrected before continuing rolling.
[0039] Among them, the types of lateral bends include single-sided bends, S-bends and compound bends. When correcting compound bends, first correct the compound bends to single-sided bends, and then align the single-sided bends. In addition, it is more difficult to bend the head of the plate than the tail. When correcting lateral bends, correct the head first and then the tail to reduce the workload.
[0040] The method of the present invention is applied in the cold rolling process of high-quality nuclear-grade zirconium alloy ultra-long plates, which can reduce welds, improve the efficiency of the welding process by about 50%, reduce the probability of strip breakage by more than 90%, significantly reduce metal loss and electricity costs, and can be easily applied to mass industrial production, thereby generating considerable economic value.
[0041] The present method is specifically described below in conjunction with embodiments.
[0042] The preparation process of high-quality nuclear-grade zirconium alloy ultra-long plates includes:
[0043] Place the semi-finished material with the specification of δ3.60×L2880mm on the rolling mill roller table, align the center line of the head and tail of the material with the center line of the working roll. Set the rolling parameters to rolling pressure 2000KN, bending roll force 30KN and rolling speed 20m / min for the first rolling;
[0044] When the plate has obvious lateral deviation in the roll gap, the single-side pressure of the rolling mill is continuously adjusted in the range of 100 to 900 KN. During the process, the correction effect is evaluated in real time. When the lateral deviation is significantly corrected, the adjustment value needs to be restored to the initial setting value to avoid reverse deviation.
[0045] When the rolling thickness reaches δ1.7mm and the length reaches 6m, the lateral shift caused by uneven deformation will occur frequently, and the rolling speed is reduced to 5-10m / min to provide effective time for the completion of the deviation adjustment operation;
[0046] In the first 2 to 3 passes of the finished product, the deformation of the pass is controlled in the range of 0.5% to 1.0%, which can effectively control the degree of deviation and improve the plate shape. Finally, the δ1.22mm nuclear-grade zirconium alloy ultra-long plate is obtained. Due to the effective increase in length, it shows its many advantages in subsequent production and processing.
[0047] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms may be for different embodiments or examples. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.
[0048] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0049] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A method for controlling deformation during cold rolling of high-quality nuclear-grade zirconium alloy ultra-long plates, characterized in that: The following steps are involved: (a) Select the correct position for feeding; (b) When the plate does not have side bending, the rolling is carried out at a pass deformation of 3% to 5% and a rolling speed of 15 to 25 m / min in the early stage of rolling, and at a pass deformation of 1% to 3% and a rolling speed of 5 to 10 m / min in the middle and late stages of rolling; (c) When the plate is bent sideways, the deviation is corrected by adjusting the deformation amount, rolling speed, rolling pressure and bending roll force.
2. The method according to claim 1, characterized in that It also includes the first 2 to 3 passes of the finished product, controlling the deformation of each pass within 0.5% to 1.0%.
3. The method according to claim 1, characterized in that The correct position selected in step (a) is to align the center line of the head and tail of the incoming plate material with the center line of the working roller, and the length of the incoming plate material is more than 5m.
4. The method according to claim 1, characterized in that In the step (c), when the side bending depth is below 80 mm, the deformation amount per pass is adjusted to 0.5% to 1%, and the rolling speed is within 10 m / min.
5. The method according to claim 4, characterized in that When the side bending depth in the step (c) is below 80 mm, the single-side rolling pressure is continuously adjusted between 100 and 900 KN in the early and middle stages of rolling.
6. The method according to claim 4, characterized in that When the side bending depth in the step (c) is below 80 mm, the single-side rolling pressure is continuously adjusted between 50 and 100 KN in the later stage of rolling.
7. The method according to claim 1, characterized in that When the side bending depth in step (c) is above 80 mm, the rolling speed is adjusted to 5-10 m / min, the rolling pressure is raised to 200±5 KN, the bending roll force is 0 KN, and the alignment is gradually performed through 2-3 passes.
8. The method according to claim 7, characterized in that In the step (c), when the side bending depth is above 80 mm and dynamic correction cannot be achieved by adjusting the rolling speed, rolling pressure and bending roll force, the machine is stopped and the rolling pressure is completely unloaded, and the plate position is corrected before continuing rolling.
9. The method according to claim 1, characterized in that The side bend in step (c) includes a unilateral bend, an S-bend and a compound bend. When correcting the compound bend, the compound bend is first corrected to the unilateral bend, and then the unilateral bend is aligned.
10. Use of the method according to any one of claims 1 to 9 in the cold rolling process of high-quality nuclear-grade zirconium alloy ultra-long plates.
Citation Information
Patent Citations
Method for correcting error of middle blank for pass-reversible rolling
CN101376140A
High-precision zirconium alloy plate rolling method
CN109108072A
Al-Mg-Mn-Zr-Cr alloy and preparation method thereof
CN115233050A
Preparation method of close-packed hexagonal metal material containing ultrahigh-density twin crystals
CN115747690A
Method for improving hydrogen embrittlement resistance of zirconium alloy by using deformation twin crystal
CN116356233A