Flame-retardant medium-voltage cable for photovoltaic power generation

By covering the flame-retardant composite material of aluminum hydroxide on the surface of Eloshi nanotubes, the problem of poor flame retardant performance of halogen-free cable materials is solved, significantly improving the flame retardant and safety performance of the cable, ensuring the photovoltaic power generation system stable operation.

CN119060439AActive Publication Date: 2024-12-03SHENZHEN DONGJIAXIN CABLE&WIRE

Patent Information

Application Number
CN202411404091.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-09
Publication Date
2024-12-03
Estimated Expiration
2044-10-09

AI Technical Summary

Technical Problem

The flame retardant performance of the cable materials prepared by existing halogen-free cable materials is poor, which affects the safety performance and reliability of the cable.

Method used

The flame retardant is prepared by high-speed mixing and extrusion granulation process using a combination of polyethylene resin, ethylene propylene ternary rubber, flame retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant and ultraviolet absorber. The material is uniformly coated with aluminum hydroxide on the surface of the Elostone nanotubes to form an efficient flame retardant composite material.

Benefits of technology

It significantly improves the flame retardant performance of the cable, ensures safe performance in fire situations and stable operation of the photovoltaic power generation system, and provides a more reliable and safe power transmission solution.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a flame-retardant medium-voltage cable for photovoltaic power generation, and belongs to the technical field of cables. Comprising a cable core, a shielding layer and a sheath layer which are sequentially arranged from inside to outside, the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps that polyethylene resin, ethylene propylene diene monomer, a flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, an antioxidant 168 and an ultraviolet light absorber UV-360 are taken and added into a high-speed mixer to be mixed, and the flame-retardant material is obtained; and extruding and granulating to obtain the flame-retardant material. The surface of the halloysite nanotube loaded flame retardant is coated with aluminum hydroxide, so that the flame-retardant effect of the prepared flame-retardant filler is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of cables, and in particular relates to a flame-retardant medium-voltage cable for photovoltaic power generation. Background Art

[0002] With the rapid development of the wire and cable industry, the demand for wires and cables has gradually increased, and their applications have become more and more extensive. Among them, aluminum alloy cable is a new type of power cable with aluminum alloy as conductor, special roll-formed wire stranding production process and annealing treatment and other advanced technologies. It has good mechanical and electrical properties and can be widely used in various fields of the national economy. With the development of society, wires and cables are increasingly widely used in various fields, such as transportation, communication, construction, etc. PVC cable material is based on polyvinyl chloride resin, which is prepared by extrusion and other methods after adding other additives. Since PVC contains a large amount of chlorine, it has excellent flame retardant properties and is the main base material of cable materials. However, PVC will produce a large amount of toxic gas when it burns, which can easily cause casualties. With people's increasing attention to environmental protection and life safety, how to reduce the incidence of fire and the mortality rate when a fire occurs, halogen-free has become the development direction of the wire and cable industry. At present, the production of halogen-free cable materials usually no longer uses PVC materials but other halogen-free polymers. However, the flame retardant properties of cable materials prepared from existing halogen-free polymers are poor. The flame retardant effect can be achieved by adding a large amount of magnesium hydroxide or other hydroxides to the halogen-free polymer matrix. However, the addition of a large amount of inorganic materials affects the physical and mechanical properties and processing performance of the cable materials. Summary of the invention

[0003] The object of the present invention is to provide a flame-retardant medium-voltage cable for photovoltaic power generation, which is used to solve the problem that the flame retardant performance of the cable material prepared by halogen-free cable material is poor.

[0004] The purpose of the present invention can be achieved by the following technical solutions: A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer arranged in sequence from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a method for preparing the flame-retardant material comprises the following steps: Polyethylene resin, EPDM rubber, flame retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 are added to a high-speed mixer, mixed, extruded and granulated to obtain the flame retardant material.

[0005] As a preferred technical solution of the present invention, the mass ratio of the polyethylene resin, EPDM rubber, flame retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 30-40:22-28:6-8:1-2:0.6-0.8:0.4-0.6:0.8-1.2.

[0006] As a preferred technical solution of the present invention, the method for preparing the flame retardant filler comprises the following steps: S1, mix halloysite nanotubes and toluene, adjust the pH to 3.5-4.5, heat in a water bath at 55-65°C with stirring for 1-2h, add methyltrimethoxysilane, continue stirring for 2-3h, filter, wash the solid phase, and vacuum dry at 80°C for 12h to obtain material A; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir for 15-25min, add N-hydroxyethyl acrylamide (purchased from Wuhan Kemik Biopharmaceutical Technology Co., Ltd.), stir for 10-15min, add carbon tetrachloride in an ice water bath, stir for 10-15h, and distill under reduced pressure to obtain material B; S3, mixing the material A and the material B, dispersing them in an ice bath with ultrasound for 30-40 min, and then treating them under a vacuum condition of 0.1 MPa for 30-40 min, centrifuging, washing the solid phase, and drying to obtain the material C; S4. Mix aluminum isopropoxide, deionized water and anhydrous ethanol, heat in a water bath at 50-60° C. with stirring for 3-4 hours, add the material C, ultrasonically disperse for 1-2 hours, let stand for 20-30 hours, filter, wash the solid phase, and dry to obtain the flame retardant filler.

[0007] As a preferred technical solution of the present invention, in step S1, the mass ratio of the halloysite nanotubes, toluene and methyltrimethoxysilane is 5-7:110-130:6-8.

[0008] As a preferred technical solution of the present invention, in step S2, the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 240-260mL: 0.1-0.12mol: 0.11-0.13mol: 0.1-0.12mol: 0.1-0.12mol.

[0009] As a preferred technical solution of the present invention, in step S3, the dosage ratio of material A to material B is 1-1.2 g: 10-12 mL.

[0010] As a preferred technical solution of the present invention, in step S4, the mass ratio of aluminum isopropoxide, deionized water, anhydrous ethanol, and material C is 0.3-0.35:400:100:0.5-0.6.

[0011] As a preferred technical solution of the present invention, in step S2, the reduced pressure distillation refers to reduced pressure distillation at 40° C. and a vacuum degree of 200 mbar for 10-12 min.

[0012] As a preferred technical solution of the present invention, the mixing refers to stirring at 120-130° C. for 8-10 minutes.

[0013] As a preferred technical solution of the present invention, the temperature of the extrusion granulation is 120-180°C.

[0014] Beneficial effects of the present invention: Disclosed in the present invention is a flame retardant medium voltage cable for a photovoltaic power generation system. The flame retardant properties of this cable are significantly improved through a unique process method. Specifically, the method involves uniformly coating aluminum hydroxide on the surface of a flame retardant loaded by halloysite nanotubes. In this way, aluminum hydroxide is combined with the flame retardant loaded by halloysite nanotubes to form a highly efficient flame retardant composite material. This composite material is introduced during the manufacturing process of the cable, so that the flame retardant cable finally obtained can show a more outstanding flame retardant effect when facing emergency situations such as fire. This improvement not only improves the safety performance of the cable, but also ensures the stable operation of the photovoltaic power generation system, thereby providing a more reliable and safe power transmission solution for the entire photovoltaic power generation system. DETAILED DESCRIPTION

[0015] In order to further illustrate the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in combination with the embodiments.

[0016] A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 120° C. for 8 min, and extruding and granulating at 120° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 30:22:6:1:0.6:0.4:0.8; The preparation method of the flame retardant filler comprises the following steps: S1, mix halloysite nanotubes and toluene, adjust the pH to 3.5, heat in a water bath at 55°C with stirring for 1 hour, add methyltrimethoxysilane, continue stirring for 2 hours, filter, wash the solid phase, and vacuum dry at 80°C for 12 hours to obtain material A; the mass ratio of the halloysite nanotubes, toluene, and methyltrimethoxysilane is 5:110:6; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir for 15 minutes, add N-hydroxyethyl acrylamide, stir for 10 minutes, add carbon tetrachloride in an ice water bath, stir for 10 hours, and distill under reduced pressure at 40°C and vacuum degree of 200 mbar for 10 minutes to obtain material B; the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 240mL: 0.1mol: 0.11mol: 0.1mol: 0.1mol; S3, taking the material A and the material B, mixing them, ultrasonically dispersing them in an ice bath for 30 minutes, and then maintaining the pressure for 30 minutes under a vacuum condition of 0.1 MPa, centrifuging, washing the solid phase, and drying to obtain material C; the dosage ratio of the material A to the material B is 1 g: 10 mL; S4. Mix aluminum isopropoxide, deionized water and anhydrous ethanol, heat and stir in a water bath at 50°C for 3 hours, add the material C, ultrasonically disperse for 1 hour, let stand for 20 hours, filter, wash the solid phase, and dry to obtain the flame retardant filler; the mass ratio of aluminum isopropoxide, deionized water, anhydrous ethanol and material C is 0.3:400:100:0.5.

[0017] A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 125° C. for 9 minutes, and extruding and granulating at 150° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 35:25:7:1.5:0.7:0.5:1; The preparation method of the flame retardant filler comprises the following steps: S1, take halloysite nanotubes and toluene, mix them, adjust the pH to 4, heat and stir in a water bath at 60°C for 1.5h, add methyltrimethoxysilane, continue stirring for 2.5h, filter, wash the solid phase, and vacuum dry at 80°C for 12h to obtain material A; the mass ratio of the halloysite nanotubes, toluene and methyltrimethoxysilane is 6:120:7; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir for 20 minutes, add N-hydroxyethyl acrylamide, stir for 12 minutes, add carbon tetrachloride in an ice water bath, stir for 12 hours, and distill under reduced pressure at 40°C and vacuum degree of 200 mbar for 11 minutes to obtain material B; the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 250mL: 0.11mol: 0.12mol: 0.11mol: 0.11mol; S3, taking the material A and the material B, mixing them, ultrasonically dispersing them in an ice bath for 35 minutes, and then maintaining the pressure for 35 minutes under a vacuum condition of 0.1 MPa, centrifuging, washing the solid phase, and drying to obtain material C; the dosage ratio of the material A to the material B is 1.1 g:11 mL; S4. Mix aluminum isopropoxide, deionized water and anhydrous ethanol, heat and stir in a water bath at 55°C for 3.5 hours, add the material C, ultrasonically disperse for 1.5 hours, let stand for 25 hours, filter, wash the solid phase, and dry to obtain the flame retardant filler; the mass ratio of the aluminum isopropoxide, deionized water, anhydrous ethanol and material C is 0.33:400:100:0.55.

[0018] A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 130° C. for 10 min, and extruding and granulating at 180° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 40:28:8:2:0.8:0.6:1.2; The preparation method of the flame retardant filler comprises the following steps: S1, take halloysite nanotubes and toluene, mix them, adjust the pH to 4.5, heat and stir in a water bath at 65°C for 2h, add methyltrimethoxysilane, continue stirring for 3h, filter, wash the solid phase, and vacuum dry at 80°C for 12h to obtain material A; the mass ratio of the halloysite nanotubes, toluene and methyltrimethoxysilane is 7:130:8; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir for 25 minutes, add N-hydroxyethyl acrylamide, stir for 15 minutes, add carbon tetrachloride in an ice water bath, stir for 15 hours, and distill under reduced pressure at 40°C and vacuum degree of 200 mbar for 12 minutes to obtain material B; the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 260mL: 0.12mol: 0.13mol: 0.12mol: 0.12mol; S3, taking the material A and the material B, mixing them, and ultrasonically dispersing them in an ice bath for 40 minutes, and then maintaining the pressure for 40 minutes under a vacuum condition of 0.1 MPa, centrifuging, washing the solid phase, and drying to obtain material C; the dosage ratio of the material A to the material B is 1.2 g:12 mL; S4. Mix aluminum isopropoxide, deionized water and anhydrous ethanol, heat and stir in a water bath at 60°C for 4 hours, add the material C, ultrasonically disperse for 2 hours, let stand for 30 hours, filter, wash the solid phase, and dry to obtain the flame retardant filler; the mass ratio of aluminum isopropoxide, deionized water, anhydrous ethanol and material C is 0.35:400:100:0.6.

[0019] Comparative Example 1 A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 125° C. for 9 minutes, and extruding and granulating at 150° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 35:25:7:1.5:0.7:0.5:1; The preparation method of the flame retardant filler comprises the following steps: S1, taking halloysite nanotubes and material B (preparation process is the same as that in Example 2) and mixing them, dispersing them ultrasonically in an ice bath for 35 minutes, and then maintaining the pressure for 35 minutes under 0.1 MPa vacuum conditions, centrifuging and washing the solid phase, and drying to obtain material C; the dosage ratio of the halloysite nanotubes to material B is 1.1 g:11 mL; S2. Mix aluminum isopropoxide, deionized water and anhydrous ethanol, heat and stir in a water bath at 55°C for 3.5 hours, add the material C, ultrasonically disperse for 1.5 hours, let stand for 25 hours, filter, wash the solid phase, and dry to obtain the flame retardant filler; the mass ratio of the aluminum isopropoxide, deionized water, anhydrous ethanol and material C is 0.33:400:100:0.55.

[0020] Comparative Example 2 A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 125° C. for 9 minutes, and extruding and granulating at 150° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 35:25:7:1.5:0.7:0.5:1; The preparation method of the flame retardant filler comprises the following steps: S1, take halloysite nanotubes and toluene, mix them, adjust the pH to 4, heat and stir in a water bath at 60°C for 1.5h, add methyltrimethoxysilane, continue stirring for 2.5h, filter, wash the solid phase, and vacuum dry at 80°C for 12h to obtain material A; the mass ratio of the halloysite nanotubes, toluene and methyltrimethoxysilane is 6:120:7; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir for 20 minutes, add N-hydroxyethyl acrylamide, stir for 12 minutes, add carbon tetrachloride in an ice water bath, stir for 12 hours, and distill under reduced pressure at 40°C and vacuum degree of 200 mbar for 11 minutes to obtain material B; the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 250mL: 0.11mol: 0.12mol: 0.11mol: 0.11mol; S3. Mix the material A and the material B, disperse them in an ice bath with ultrasonic waves for 35 minutes, and then maintain the pressure for 35 minutes under 0.1 MPa vacuum conditions, centrifuge, wash the solid phase, and dry to obtain material C, which is the flame retardant filler; the dosage ratio of the material A to the material B is 1.1 g:11 mL.

[0021] Comparative Example 3 A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 125° C. for 9 minutes, and extruding and granulating at 150° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, ethylene propylene rubber, flame-retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 35:25:7:1.5:0.7:0.5:1; The preparation method of the flame retardant filler comprises the following steps: S1, take halloysite nanotubes and toluene, mix them, adjust the pH to 4, heat and stir in a water bath at 60°C for 1.5h, add methyltrimethoxysilane, continue stirring for 2.5h, filter, wash the solid phase, and vacuum dry at 80°C for 12h to obtain material A; the mass ratio of the halloysite nanotubes, toluene and methyltrimethoxysilane is 6:120:7; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir for 20 minutes, add N-hydroxyethyl acrylamide, stir for 12 minutes, add carbon tetrachloride in an ice water bath, stir for 12 hours, and distill under reduced pressure at 40°C and vacuum degree of 200 mbar for 11 minutes to obtain material B; the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 250mL: 0.11mol: 0.12mol: 0.11mol: 0.11mol; S3, taking the material A and the material B, mixing them, ultrasonically dispersing them in an ice bath for 35 minutes, and then maintaining the pressure for 35 minutes under a vacuum condition of 0.1 MPa, centrifuging, washing the solid phase, and drying to obtain material C; the dosage ratio of the material A to the material B is 1.1 g:11 mL; S4. Take aluminum hydroxide and the material C and mix them to obtain the flame retardant filler; the mass ratio of the aluminum hydroxide and the material C is 0.33:0.55.

[0022] Comparative Example 4 A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, EPDM rubber, material B, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 125° C. for 9 minutes, and extruding and granulating at 150° C. to obtain the flame-retardant material; the mass ratio of the polyethylene resin, EPDM rubber, material B, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 is 35:25:7:1.5:0.7:0.5:1; The preparation method of material B comprises the following steps: Take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide and triethylamine, mix them, stir for 20 minutes, add N-hydroxyethyl acrylamide, stir for 12 minutes, add carbon tetrachloride in an ice water bath, stir for 12 hours, and distill under reduced pressure at 40°C and a vacuum degree of 200 mbar for 11 minutes to obtain material B; the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide and carbon tetrachloride is 250mL: 0.11mol: 0.12mol: 0.11mol: 0.11mol.

[0023] Comparative Example 5 A flame-retardant medium-voltage cable for photovoltaic power generation comprises a cable core, a shielding layer and a sheath layer which are sequentially arranged from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, and a preparation method of the flame-retardant material comprises the following steps: adding polyethylene resin, EPDM rubber, halloysite nanotubes, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168 and ultraviolet light absorber UV-360 to a high-speed mixer, stirring at 125°C for 9 minutes, and extruding and granulating at 150°C to obtain the flame-retardant material; the mass ratio of the polyethylene resin, EPDM rubber, halloysite nanotubes, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168 and ultraviolet light absorber UV-360 is 35:25:7:1.5:0.7:0.5:1.

[0024] Performance Testing The flame retardant materials prepared in Examples 1-3 and Comparative Examples 1-5 were subjected to performance tests. They were dried in a drying oven at 55° C. for 24 h, and samples were prepared using a tablet press: the temperature was 170° C., the time was 15 min, and the pressure was 16.5 MPa. Then, an oxygen index test was performed using a BK-JF-3 oxygen index tester; a vertical burning grade test was performed in accordance with standard GB / T 10707-2008, and the results are shown in Table 1.

[0025] Table 1 Vertical burning level Oxygen index (%) Example 1 V0 36.4 Example 2 V0 37.1 Example 3 V0 36.8 Comparative Example 1 V1 33.4 Comparative Example 2 V1 30.7 Comparative Example 3 V2 29.3 Comparative Example 4 V2 27.2 Comparative Example 5 V2 25.7 It can be seen from Table 1 that the flame retardant materials prepared in Examples 1-3 of the present application have excellent flame retardant properties; in Comparative Example 1, the halloysite nanotubes were not surface treated, resulting in a decrease in the flame retardant loading of the prepared flame retardant filler, resulting in a decrease in the flame retardant effect; in Comparative Examples 2-3, aluminum hydroxide was not coated on the surface of the halloysite nanotubes or aluminum hydroxide was only added through a physical process, resulting in poor interfacial compatibility of the flame retardant filler, resulting in a decrease in the flame retardant effect; It can be seen from Comparative Examples 4-5 that the flame retardant effect of the flame retardant filler can be improved through the synergistic effect of the flame retardant loaded on the halloysite nanotubes.

[0026] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A flame-retardant medium-voltage cable for photovoltaic power generation, comprising a cable core, a shielding layer and a sheath layer arranged in sequence from the inside to the outside, wherein the sheath layer is made of a flame-retardant material, characterized in that: The method for preparing the flame retardant material comprises the following steps: Polyethylene resin, EPDM rubber, flame retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168, and ultraviolet light absorber UV-360 are added to a high-speed mixer, mixed, extruded and granulated to obtain the flame retardant material.

2. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 1, characterized in that: The mass ratio of the polyethylene resin, EPDM rubber, flame retardant filler, stearic acid, maleic anhydride grafted polyethylene, antioxidant 168 and ultraviolet light absorber UV-360 is 30-40: 22-28: 6-8: 1-2: 0.6-0.8: 0.4-0.6: 0.8-1.

2.

3. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 1, characterized in that: The preparation method of the flame retardant filler comprises the following steps: S1, mix halloysite nanotubes and toluene, adjust the pH, heat in a water bath with stirring, add methyltrimethoxysilane, continue stirring, filter, wash the solid phase, and vacuum dry to obtain material A; S2, take dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, mix, stir, add N-hydroxyethyl acrylamide, stir, add carbon tetrachloride in an ice water bath, stir, and distill under reduced pressure to obtain material B; S3, mixing the material A and the material B, performing ultrasonic dispersion in an ice bath, performing vacuum pressure treatment, performing centrifugal separation, washing the solid phase, and drying to obtain the material C; S4. Mix aluminum isopropoxide, deionized water and anhydrous ethanol, heat and stir in a water bath, add the material C, disperse by ultrasonic, let stand, filter, wash and dry the solid phase to obtain the flame retardant filler.

4. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 3, characterized in that: In step S1, the mass ratio of the halloysite nanotubes, toluene and methyltrimethoxysilane is 5-7:110-130:6-8.

5. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 3, characterized in that: In step S2, the dosage ratio of dichloromethane, flame retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide, triethylamine, N-hydroxyethyl acrylamide, and carbon tetrachloride is 240-260 mL: 0.1-0.12 mol: 0.11-0.13 mol: 0.1-0.12 mol: 0.1-0.12 mol.

6. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 3, characterized in that: In step S3, the dosage ratio of material A to material B is 1-1.2 g: 10-12 mL.

7. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 3, characterized in that: In step S4, the mass ratio of aluminum isopropoxide, deionized water, anhydrous ethanol, and material C is 0.3-0.35:400:100:0.5-0.

6.

8. The flame-retardant medium voltage cable for photovoltaic power generation according to claim 3, characterized in that: In step S2, the reduced pressure distillation refers to reduced pressure distillation at 40° C. and a vacuum degree of 200 mbar for 10-12 min.

9. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 1, characterized in that: The mixing refers to stirring at 120-130° C. for 8-10 minutes.

10. A flame-retardant medium voltage cable for photovoltaic power generation according to claim 1, characterized in that: The temperature of the extrusion granulation is 120-180°C.

Citation Information

Patent Citations

  • Manufacture of dihydroxy aromatic compounds by alcoholysis of flame retardant-containing polycarbonate compositions

    CN104870418A

  • Low-smoke halogen-free flame retardant and preparation method and application thereof

    CN112759795A

  • Halogen-free flame-retardant cable material for aluminum alloy cable and preparation method thereof

    CN117004111A

  • Flame-retardant antistatic polyurethane elastomer and preparation method thereof

    CN118222085A

Cited By

  • Flame-retardant unsaturated polyester resin-based fiber composite material with low volume shrinkage

    CN119331178A

  • Oil-resistant and aging-resistant drag chain cable special for robot and preparation method of oil-resistant and aging-resistant drag chain cable

    CN121460277A