High-strength antioxidant iron-nickel alloy valve steel material and preparation process thereof
The high-strength, oxidation-resistant iron-nickel alloy valve steel addresses the oxidation and corrosion issues of titanium-nickel alloys by incorporating specific elements and a tailored preparation process, enhancing the material's durability and mechanical properties.
Patent Information
- Application Number
- CN202411393407.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-08
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing titanium-nickel alloy valve steels exhibit average strength and are prone to oxidation and corrosion, affecting their service life due to the harsh corrosive environment in engine intake and exhaust systems.
A high-strength, oxidation-resistant iron-nickel alloy valve steel material is developed, comprising specific proportions of carbon, silicon, phosphorus, sulfur, chromium, vanadium, manganese, and molybdenum, with a preparation process involving vacuum induction smelting, forging, and heat treatment to enhance corrosion resistance and strength.
The alloy significantly improves oxidation resistance and corrosion resistance, extending the service life and enhancing the mechanical properties of the valve steel, including strength, hardness, and toughness.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of valve steel, and in particular to a high-strength oxidation-resistant iron-nickel alloy valve steel material and a preparation process thereof. Background Art
[0002] The engine intake and exhaust valves control the intake and exhaust of the combustion chamber and operate at very high temperatures. The combustion of fuel produces highly corrosive ions such as CO32-, SO42- and Cl-, thus forming a highly corrosive environment.
[0003] Therefore, the valve material must have very high high temperature strength and hardness to avoid creep, and must also have high tensile strength and elongation after fracture. In recent years, the engine has developed towards high speed, high power and low fuel consumption. With the continuous improvement of automobile service life requirements and the continuous improvement of exhaust emission standards, the requirements for valve materials are getting higher and higher.
[0004] The existing titanium-nickel alloy valve steel has average strength during use and is easily oxidized and corroded by the external environment, which affects the service life of the valve steel. Summary of the invention
[0005] The present invention proposes a high-strength, oxidation-resistant iron-nickel alloy valve steel material and a preparation process to solve the problem that the titanium-nickel alloy valve steel has average strength during use and is easily oxidized and corroded by the external environment, which affects the service life of the valve steel.
[0006] In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme: a high-strength, oxidation-resistant iron-nickel alloy valve steel material, comprising carbon, silicon, phosphorus, sulfur, chromium, vanadium, nickel, molybdenum, and manganese, wherein the element proportions of the iron-nickel alloy valve steel material are as follows: the carbon proportion is 0.3-0.91%, the silicon proportion is 0.1-0.45%, the manganese proportion is 0.22-0.7%, the phosphorus proportion is 0.01-0.03%, the sulfur proportion is 0.012-0.03%, the chromium proportion is 4.7-8.9%, the vanadium proportion is 0.65-1.2%, the molybdenum proportion is 0.43-0.85%, the nickel proportion is 43.5-47.23%, the iron proportion is 42.8-47.6%, and the remainder is unavoidable impurity elements.
[0007] The effects achieved by the above components are: Nickel has good corrosion resistance and thermal stability, and can improve the corrosion resistance of the alloy. Iron is a common structural material. After alloying with nickel, a nickel-iron alloy material with excellent performance can be obtained. These elements, as impurities or alloying elements, have an important influence on the performance of the alloy. By adding alloying elements such as chromium, silicon and molybdenum to iron-nickel alloy valve steel, its oxidation resistance can be significantly improved, and the corrosion resistance and heat resistance of the material can be enhanced, thereby extending the service life and improving safety.
[0008] Preferably, the chromium accounts for 7.48% and the molybdenum accounts for 0.67%.
[0009] The effects achieved by the above components are as follows: adding alloy elements such as chromium, silicon and molybdenum to the iron-nickel alloy valve steel can enhance its antioxidant properties. Chromium is one of the effective elements for improving the antioxidant properties of steel. It can form a dense oxide protective film on the surface of the steel to prevent oxygen and moisture from further corroding the steel, thereby improving the corrosion resistance and heat resistance of the steel. Molybdenum in steel can improve hardenability and thermal strength, prevent temper brittleness, increase remanence and coercive force, and corrosion resistance in certain media. Molybdenum can further improve corrosion resistance to organic acids and hydrogen peroxide, sulfuric acid, sulfurous acid, sulfates, acid dyes, bleaching powder solution, etc., especially preventing the pitting corrosion tendency caused by the presence of chloride ions.
[0010] Preferably, the silicon accounts for 0.28%, the carbon accounts for 0.36%, and the manganese accounts for 0.48%.
[0011] The effects achieved by the above components are as follows: Silicon is an important reducing agent and deoxidizing agent in the steelmaking process, which can improve the hardness and strength of steel. When silicon-containing steel is heated in an oxidizing atmosphere, a layer of SiO2 film will form on the surface, which helps to improve the oxidation resistance of steel at high temperatures. At the same time, silicon is also an effective element for improving the strength of steel. Adding an appropriate amount of silicon to steel can refine the grains and improve the hardness and strength of steel. Carbon is one of the most effective strengthening elements. It forms carbides with iron or alloys, which can significantly improve the strength of steel. The quenching and tempering process during the treatment process can change the morphology of carbides in the steel, refine the grains, and further improve the strength of the steel. Manganese is a weak carbide-forming element that can reduce the Ar1 and martensite transformation temperature of the steel, improve the hardenability of the steel, and increase the residual austenite content, thereby enhancing the strength of the steel. By adding manganese, silicon and an appropriate amount of carbon and other elements to the iron-nickel alloy valve steel, its strength can be effectively improved. At the same time, the addition of these elements can also improve other mechanical properties of the steel, such as hardness, toughness and wear resistance.
[0012] Preferably, the phosphorus accounts for 0.02% and the vanadium accounts for 0.87%.
[0013] The effects achieved by the above components are: vanadium has good ductility and hardness, is non-magnetic, can resist corrosion from hydrochloric acid and sulfuric acid, improves the strength and toughness of steel, refines grains, increases grain coarsening temperature, and thus increases the strength, toughness and wear resistance of steel. As an impurity element, phosphorus has a complex effect in steel. On the one hand, phosphorus can increase the tensile strength of steel, but it also increases the brittleness of steel, especially under low temperature conditions, phosphorus reduces the strength of steel, increases the hardness of steel, and reduces the plasticity and toughness of steel.
[0014] Preferably, the sulfur accounts for 0.01%.
[0015] The effects achieved by the above components are as follows: Sulfur is a harmful element in valve steel, which mainly causes hot brittleness, reduces the ductility, toughness and corrosion resistance of steel, and also has an adverse effect on welding and weldability. Therefore, the sulfur content in ordinary steel is generally controlled at ≤0.050%, and in high-quality steel it is controlled at ≤0.030%, while the requirement for high-quality steel is even lower in order to achieve better mechanical properties and corrosion resistance. In the production and use of valve steel, the sulfur content needs to be strictly controlled to ensure that the performance of the valve steel meets specific application requirements.
[0016] Preferably, a method for preparing high-strength, oxidation-resistant iron-nickel alloy valve steel is characterized in that: the specific steps of the method for preparing the iron-nickel alloy valve steel are as follows: ① Raw material preparation and smelting: prepare qualified ingredients according to the raw material proportions shown in claims 1-5 above, and then smelt the raw materials into molten steel by vacuum induction smelting; ② Forging: The smelted molten steel is poured into a specific jig to form a steel ingot, and then the formed steel ingot is forged at a high temperature of 1030°C, and then the forged steel ingot is cooled and placed in a heating chamber; ③ Heat treatment: The steel ingot is placed in a heating chamber for tempering treatment. The tempering temperature is maintained between 600-850°C and the tempering holding time is between 1-3 hours. Then, the valve steel is obtained after the steel ingot is cooled.
[0017] In summary, the beneficial effects of the present invention are: By adding alloying elements such as chromium, silicon and molybdenum to iron-nickel alloy valve steel, its oxidation resistance can be significantly improved, and the corrosion resistance and heat resistance of the material can be enhanced. By adding elements such as manganese, silicon and an appropriate amount of carbon to iron-nickel alloy valve steel, its strength can be effectively improved, thereby extending the service life of iron-nickel alloy valve steel and improving safety. DETAILED DESCRIPTION
[0018] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] The present embodiment discloses a high-strength, oxidation-resistant iron-nickel alloy valve steel material, including carbon, silicon, phosphorus, sulfur, chromium, vanadium, nickel, molybdenum, and manganese. The element proportions of the iron-nickel alloy valve steel material are as follows: carbon accounts for 0.3-0.91%, silicon accounts for 0.1-0.45%, manganese accounts for 0.22-0.7%, phosphorus accounts for 0.01-0.03%, sulfur accounts for 0.012-0.03%, chromium accounts for 4.7-8.9%, vanadium accounts for 0.65-1.2%, molybdenum accounts for 0.43-0.85%, and nickel accounts for 43.5-4. 7.23%, iron accounts for 42.8-47.6%, and the rest are inevitable impurity elements. Nickel has good corrosion resistance and thermal stability, and can improve the corrosion resistance of the alloy. Iron is a common structural material. After alloying with nickel, nickel-iron alloy materials with excellent performance can be obtained. These elements, as impurities or alloying elements, have an important influence on the performance of the alloy. By adding alloying elements such as chromium, silicon and molybdenum to iron-nickel alloy valve steel, its oxidation resistance can be significantly improved, and the corrosion resistance and heat resistance of the material can be enhanced, thereby extending the service life and improving safety.
[0020] For example, chromium accounts for 7.48% and molybdenum accounts for 0.67%. Adding alloy elements such as chromium, silicon and molybdenum to iron-nickel alloy valve steel can enhance its antioxidant properties. Chromium is one of the effective elements to improve the antioxidant properties of steel. It can form a dense oxide protective film on the surface of steel to prevent oxygen and moisture from further corroding the steel, thereby improving the corrosion resistance and heat resistance of the steel. Molybdenum in steel can improve hardenability and thermal strength, prevent temper brittleness, increase remanence and coercive force, as well as corrosion resistance in certain media. Molybdenum can further improve corrosion resistance to organic acids and hydrogen peroxide, sulfuric acid, sulfurous acid, sulfates, acid dyes, bleaching powder solution, etc., especially preventing the pitting corrosion tendency caused by the presence of chloride ions.
[0021] For example, silicon accounts for 0.28%, carbon accounts for 0.36%, and manganese accounts for 0.48%. Silicon is an important reducing agent and deoxidizer in the steelmaking process, which can improve the hardness and strength of steel. When silicon-containing steel is heated in an oxidizing atmosphere, a layer of SiO2 film will form on the surface, which helps to improve the oxidation resistance of steel at high temperatures. At the same time, silicon is also an effective element for improving the strength of steel. Adding an appropriate amount of silicon to steel can refine the grains and improve the hardness and strength of steel. Carbon is one of the most effective strengthening elements. It forms carbides with iron or alloys and can significantly It can significantly improve the strength of steel. Through the quenching and tempering process in the heat treatment process, the morphology of carbides in steel can be changed, the grains can be refined, and the strength of steel can be further improved. Manganese is a weak carbide-forming element, which can reduce the Ar1 and martensite transformation temperature of steel, improve the hardenability of steel, increase the residual austenite content, and thus enhance the strength of steel. By adding manganese, silicon and an appropriate amount of carbon and other elements to iron-nickel alloy valve steel, its strength can be effectively improved. At the same time, the addition of these elements can also improve other mechanical properties of steel, such as hardness, toughness and wear resistance.
[0022] For example, phosphorus accounts for 0.02% and vanadium accounts for 0.87%. Vanadium has good ductility and hardness, is non-magnetic, can resist corrosion from hydrochloric acid and sulfuric acid, improves the strength and toughness of steel, refines grains, and increases grain coarsening temperature, thereby increasing the strength, toughness and wear resistance of steel. As an impurity element, phosphorus has a complex role in steel. On the one hand, phosphorus can increase the tensile strength of steel, but it also increases the brittleness of steel, especially under low temperature conditions. Phosphorus reduces the strength of steel, increases the hardness of steel, and reduces the plasticity of steel. , toughness, sulfur accounts for 0.01%. Sulfur is a harmful element in valve steel, which mainly causes hot brittleness, reduces the ductility, toughness and corrosion resistance of steel, and also has an adverse effect on welding and weldability. Therefore, the sulfur content in ordinary steel is generally controlled at ≤0.050%, and in high-quality steel it is controlled at ≤0.030%, while the requirements for high-quality steel are lower, in order to achieve better mechanical properties and corrosion resistance. In the production and use of valve steel, the sulfur content needs to be strictly controlled to ensure that the performance of valve steel meets specific application requirements.
[0023] This embodiment discloses a method for preparing a high-strength, oxidation-resistant iron-nickel alloy valve steel, which is characterized in that the method comprises the following specific steps: ① Raw material preparation and smelting: prepare qualified ingredients according to the raw material proportions shown in claims 1-5 above, and then smelt the raw materials into molten steel by vacuum induction smelting; ② Forging: The molten steel is poured into a specific jig to form a steel ingot, and then the formed steel ingot is forged at a high temperature of 1030°C. The forged steel ingot is then cooled and placed in a heating chamber. ③ Heat treatment: The steel ingot is placed in a heating chamber for tempering treatment. The tempering temperature is maintained between 600-850°C and the tempering holding time is between 1-3 hours. Then, the valve steel is obtained after the steel ingot is cooled.
[0024] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0025] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A high-strength, oxidation-resistant iron-nickel alloy valve steel material, comprising carbon, silicon, phosphorus, sulfur, chromium, vanadium, nickel, molybdenum and manganese, characterized in that: The element proportions of the iron-nickel alloy valve steel material are as follows: carbon accounts for 0.3-0.91%, silicon accounts for 0.1-0.45%, manganese accounts for 0.22-0.7%, phosphorus accounts for 0.01-0.03%, sulfur accounts for 0.012-0.03%, chromium accounts for 4.7-8.9%, vanadium accounts for 0.65-1.2%, molybdenum accounts for 0.43-0.85%, nickel accounts for 43.5-47.23%, iron accounts for 42.8-47.6%, and the remainder is unavoidable impurity elements.
2. The high-strength, oxidation-resistant iron-nickel alloy valve steel material according to claim 1, characterized in that: The chromium accounts for 7.48% and the molybdenum accounts for 0.67%.
3. The high-strength, oxidation-resistant iron-nickel alloy valve steel material according to claim 1, characterized in that: The silicon accounts for 0.28%, the carbon accounts for 0.36%, and the manganese accounts for 0.48%.
4. The high-strength, oxidation-resistant iron-nickel alloy valve steel material according to claim 1, characterized in that: The phosphorus accounts for 0.02%, and the vanadium accounts for 0.87%.
5. The high-strength, oxidation-resistant iron-nickel alloy valve steel material according to claim 1, characterized in that: The sulfur content is 0.01%.
6. The method for preparing a high-strength, oxidation-resistant iron-nickel alloy valve steel according to claim 1, characterized in that: The specific steps of the preparation method of the iron-nickel alloy valve steel are as follows: ① Raw material preparation and smelting: prepare qualified ingredients according to the raw material proportions shown in claims 1-5 above, and then smelt the raw materials into molten steel by vacuum induction smelting; ② Forging: The smelted molten steel is poured into a specific jig to form a steel ingot, and then the formed steel ingot is forged at a high temperature of 1030°C, and then the forged steel ingot is cooled and placed in a heating chamber; ③ Heat treatment: The steel ingot is placed in a heating chamber for tempering treatment. The tempering temperature is maintained between 600-850°C and the tempering holding time is between 1-3 hours. Then, the valve steel is obtained after the steel ingot is cooled.