Novel pulp-preparing gypsum board covering paper production process

By dividing wood pulp and waste paper into long fiber and short fiber slurry, and using pressure screens in the flow delivery system, the problem of long fiber flocculation in the wood pulp is solved, and the tensile strength and stability of gypsum board protective paper is improved. sex.

CN119061722AActive Publication Date: 2024-12-03SHANXI QIANG WEI PAPER CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411179492.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-12-03
Estimated Expiration
2044-08-27

AI Technical Summary

Technical Problem

The long fibers of wood pulp in gypsum board protective paper are prone to flocculation, affecting the mixing effect of wood pulp and waste pulp, resulting in poor paper strength and uniformity, which makes it difficult to meet the requirements of high tensile strength.

Method used

Using a new pulping process, by dividing wood pulp and waste paper into long fiber pulp and short fiber pulp, and using a pressure screen in the flow delivery system for dispersion treatment, reducing fiber flocculation, improving mixing uniformity, and combining glue application Use agent, retention filter aid and aluminum sulfate to adjust the pH value of the slurry to ensure the fiber dispersion effect.

Benefits of technology

It effectively reduces the flocculation of long fibers in wood pulp, improves the mixing effect of wood pulp and waste pulp, improves the strength and stability of the paper, and meets the requirements of high tensile strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005011683180000041
    Figure BDA0005011683180000041
  • Figure HDA0005011683190000011
    Figure HDA0005011683190000011
Patent Text Reader

Abstract

The invention relates to a novel pulp-preparing gypsum board covering paper production process which comprises the following steps: respectively preparing a natural color softwood pulp board and waste paper into pulp, and dividing the waste paper pulp into long fiber pulp and short fiber pulp; and mixing the wood pulp, the long fiber pulp and the short fiber pulp, passing through a pressurized screen, dispersing in a drifting system, and spraying on a net for forming to obtain finished paper. The pressurized screen is arranged in front of the drifting system, the fiber dispersion effect can be improved through the pressurized screen, wood pulp, long fiber pulp and short fiber pulp obtained after the pressurized screen is used can be better mixed, wood pulp long fiber flocculation is reduced, the mixing effect uniformity is improved, and the paper forming strength is improved and stabilized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of gypsum board facing papers, and particularly relates to a production process of a new type of gypsum board facing paper with slurry preparation. Background Art

[0002] Gypsum board is a material made of building gypsum as the main raw material. It is a building material with light weight, high strength, thin thickness, easy processing, good sound insulation, heat insulation and fire resistance. It is one of the new lightweight boards that are currently being developed. Gypsum board has been widely used in various buildings such as residences, office buildings, shops, hotels and industrial plants for interior partitions, wall coverings (instead of wall plastering), ceilings, sound-absorbing panels, ground base panels and various decorative panels.

[0003] The breaking load of gypsum board is one of its important performance indicators, which is directly related to the quality and safety of gypsum board. According to the current national standard GB / T 9775-2008 "Gypsum Board", the average longitudinal breaking load of gypsum board should be ≥400N, the minimum value should be ≥360N, and the average transverse breaking load should be ≥160N, the minimum value should be ≥140N. This standard ensures that the gypsum board can maintain a certain strength when subjected to external forces and is not easy to crack or break, thereby ensuring the safety and stability of the building structure.

[0004] 60% of the breaking load strength of gypsum board comes from the tensile strength of the gypsum board face paper covering both sides. Therefore, with the development and changes of the market, the gypsum board face paper is developing towards low quantity and high strength. The tensile strength of the face paper is used as a decisive indicator to measure the quality of the product. The main factors affecting the tensile strength are: the strength of the fiber itself, the bonding strength between the fibers, and the uniformity.

[0005] In order to improve the tensile strength index of gypsum board facing paper, paper mills generally need to add a certain proportion of long coniferous wood fibers. However, the inventors found in production that the long fibers of wood pulp are easy to flocculate, affecting the mixing of wood pulp and waste paper pulp, thereby affecting the strength and uniformity of the finished paper. Summary of the invention

[0006] The purpose of the present invention is to provide a new type of gypsum board face paper production process, which can reduce the flocculation of wood pulp long fibers and achieve a better mixing effect of wood pulp and waste paper pulp;

[0007] In order to achieve the above object, the technical solution adopted by the present invention is:

[0008] A new type of gypsum board facing paper production process includes the following steps:

[0009] (1) Pulping: The natural softwood pulpboard and waste paper are separately made into pulp, and the waste paper pulp is divided into long fiber pulp and short fiber pulp;

[0010] (2) Papermaking: Wood pulp, long fiber pulp and short fiber pulp are mixed, passed through a pressure screen, and then dispersed in a flow conveying system and sprayed onto a net to form finished paper.

[0011] Preferably, in step (1), preparing the unbleached coniferous pulp board into pulp comprises the following steps: conveying the unbleached coniferous pulp board with a wet weight ≥ 15 g to a pulper, adding water and crushing it to prepare a pulp with a concentration of 4 to 5%, and then removing impurities through a high-consistency cleaner, and then entering a disc grinder for pulping until the beating degree is 35±2°SR.

[0012] Preferably, in step (1), waste paper is made into pulp, and the waste paper pulp is divided into long fiber pulp and short fiber pulp, comprising the following steps: the waste paper is transported to a pulper, water is added and crushed to form a pulp with a concentration of 3.5% to 4%, impurities are removed by a high-concentration cleaner and a coarse screen, and the pulp is divided into long fiber pulp and short fiber pulp by fiber grading screening, wherein the sieve gap of the fiber grading screen is 0.15 mm.

[0013] Preferably, the long fiber pulp passes through a low-concentration cleaner and fine screen, and then enters a multi-disc concentrator to be concentrated to a concentration of 8 to 10%, and then is transported to a heat dispersion treatment, and then is beaten to 30±2°SR by a double-disc refiner; the short fiber pulp passes through a low-concentration cleaner, and then enters a multi-disc concentrator to be concentrated to a concentration of 8 to 10%.

[0014] Preferably, the pore size of the pressure screen is 8 mm.

[0015] Preferably, in step (2), the mixed slurry enters the flow system to form a slurry with a concentration of 0.4%-0.8%, which is dispersed and sprayed onto the screen through a headbox.

[0016] Preferably, in step (2), the lining layer of the mesh uses a mixed pulp of 10% to 40% wood pulp slurry, 20 to 50% long fiber slurry and 0 to 20% short fiber slurry, the core layer of the mesh uses a mixed pulp of 10% to 40% wood pulp slurry, 0 to 30% long fiber slurry and 20 to 40% short fiber slurry, and the bottom layer of the mesh uses a mixed pulp of 10% to 40% wood pulp slurry, 20 to 50% long fiber slurry and 0 to 20% short fiber slurry.

[0017] Preferably, sizing agent, retention and drainage aid, aluminum sulfate and starch in the slurry are added to the flow system, and the amount of aluminum sulfate added is adjusted to ensure that the pH of the slurry in the headbox does not exceed 6.8.

[0018] Preferably, in step (2), the mixed slurry enters the flow conveying system for dispersion and is then sprayed onto the wire surface, and is subjected to gravity dehydration or vacuum dehydration on the wire to reach a dryness of 10%-14%. After pressing, pre-drying, surface bonding, post-drying, and winding, a finished paper is obtained.

[0019] The present invention arranges a pressure screen before the flow conveying system, which can improve the fiber dispersion effect. After using the pressure screen, the wood pulp, OCC long fibers and OCC short fibers can obtain a better mixing effect, reduce the flocculation of the wood pulp long fibers, improve the uniformity of the mixing effect, and improve and stabilize the paper strength. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is a schematic diagram of the structure of the pressure screen for wood pulp, long fiber pulp and short fiber pulp. DETAILED DESCRIPTION

[0021] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0022] The present invention discloses a novel gypsum board facing paper production process, comprising the following steps:

[0023] (1) Pulping: The natural softwood pulpboard and waste paper are pulped separately, and the waste paper pulp is divided into long fiber pulp and short fiber pulp.

[0024] Specifically, the raw material is natural coniferous wood pulp board, with wet weight ≥15g. It is transported to the pulper via a chain conveyor, and water is added to break it up to make a pulp with a concentration of 4-5%. Then, it is passed through a high-concentration remover to remove some heavy impurities such as sand to prevent impurities such as iron wire from entering the system. The wood pulp is sent to the pre-beating pulp tower after the high-concentration remover, and finally is beaten by a disc grinder to a beating degree of 35±2°SR. After the disc grinder treatment, the wood pulp is properly cut and fibrillated, and then stored in the post-beating tower for pulping of each layer of papermaking.

[0025] Specifically, the OCC waste is conveyed to a pulper via a chain conveyor for water-addition and crushing. In this embodiment, a Kaydon D-type pulping system is used to make a pulp with a concentration of 3.5% to 4%. Some heavy impurities in the waste paper are removed by a high-concentration cleaner and a coarse screen. The waste paper is then screened into long fiber pulp and short fiber pulp through fiber grading. The fiber grading screen has a sieve gap of 0.15 mm and a grading ratio of 40% short fiber + 60% long fiber.

[0026] More specifically, the long fiber pulp is further removed from the pulp by a low-concentration cleaner and a fine screen to remove impurities such as foam, plastic, and adhesives, wherein the fine screen is a three-stage fine screen, i.e., after the long fiber pulp passes through the low-concentration cleaner, it enters three pressure screens in sequence, and then enters a multi-disc thickener to be concentrated to a concentration of 8%, and is transported to a heat dispersion treatment by an inclined screw conveyor to disperse the adhesives in the pulp to an invisible level to the naked eye, and then is beaten to 30±2°SR by a double-disc refiner, and the refined pulp is stored in a pulp tower for papermaking pulping; the short fiber pulp passes through a low-concentration cleaner, enters a multi-disc thickener to be concentrated to a concentration of 8%, and is then stored in a pulp tower.

[0027] (2) Papermaking: Wood pulp, long fiber pulp and short fiber pulp are mixed, passed through a pressure screen, and then dispersed in a flow conveying system and sprayed onto a net to form finished paper.

[0028] Specifically, Figure 1 As shown, the wood pulp, long fiber pulp and short fiber pulp from the pulping workshop are respectively passed into the feed pipe of the pressure screen and enter the pressure screen. The pressure screen adopts a hole screen with an aperture of 8mm. The larger aperture makes the pressure screen mainly play a dispersing role instead of screening and removing slag. During the rotation of the rotor and the screen drum, the pulp is fully mixed from the pulp inlet point to the pulp outlet point, and positive and negative pressure pulses are formed at the front and tail of the rotor blade to improve the fiber dispersion effect. At this time, the pressure screen no longer removes impurities in the pulp, and the slag discharge port of the pressure screen no longer discharges impurities. After using the pressure screen, the wood pulp, OCC long fiber and OCC short fiber can get a better mixing effect, as shown in Table 1, reducing the flocculation of wood pulp long fibers, improving the uniformity of the mixing effect, and improving and stabilizing the paper strength;

[0029] The three kinds of pulps pass through the pressure screen and enter the pulping pool. After that, they pass through the flow system, i.e., the pulp pump and the pre-net screen to form a pulp with a concentration of 0.4%-0.8%. Functional additives such as sizing agent, retention and filtration aid, aluminum sulfate and starch in the pulp are added to the flow system. The amount of aluminum sulfate added is adjusted to ensure that the pH of the pulp in the headbox does not exceed 6.8.

[0030] The slurry is sprayed evenly onto the mesh surface along the entire banner direction through the headbox. The mesh part adopts 4 layers of mesh (surface, lining, core, bottom). The surface layer is hung with ONP slurry, and the lining layer, core layer and bottom layer are the above mixed slurry. The mixed slurry used in the lining layer is 30% wood pulp slurry, 50% long fiber slurry and 20% short fiber slurry. The mixed slurry used in the core layer is 30% wood pulp slurry, 30% long fiber slurry and 40% short fiber slurry. The mixed slurry used in the bottom layer is 30 % wood pulp, 50% long fiber pulp and 20% short fiber pulp are dehydrated by gravity or vacuum dehydration of the wire section to reach a dryness of 10-14%, and then go through pressing, front drying, surface glue, post drying, calendering and winding. The pressing section is composed of 2 shoe presses, and the dryness of the outlet section is about 48%. Starch is used to control the glue concentration of 18% on the front side and 8% on the back side. Finally, it is rewound into paper rolls of required specifications and diameters by a rewinder and stored in the warehouse via a chain conveyor.

[0031] Table 1

[0032]

[0033] As shown in Table 1, after the pressure screen was put into use, the strength of the same paper type increased, the strength fluctuation decreased, and the product quality stability was improved.

Claims

1. A new type of gypsum board facing paper production process, characterized in that: The following steps are involved: (1) Pulping: The natural softwood pulpboard and waste paper are separately made into pulp, and the waste paper pulp is divided into long fiber pulp and short fiber pulp; (2) Papermaking: Wood pulp, long fiber pulp and short fiber pulp are mixed, passed through a pressure screen, and then dispersed in a flow conveying system and sprayed onto a net to form finished paper.

2. The production process of the new type of gypsum board facing paper according to claim 1 is characterized in that: In step (1), the process of preparing the natural coniferous wood pulp board into pulp comprises the following steps: conveying the natural coniferous wood pulp board with a wet weight of ≥15g to a pulper, adding water and crushing it to prepare a pulp with a concentration of 4 to 5%, then passing through a high-consistency cleaner to remove impurities, and then entering a disc grinder for pulping until the pulping degree is 35±2°SR.

3. The production process of the new type of gypsum board facing paper according to claim 1 is characterized in that: In step (1), waste paper is made into pulp, and the waste paper pulp is divided into long fiber pulp and short fiber pulp, which comprises the following steps: the waste paper is transported to a pulper, water is added to disintegrate the waste paper, and a pulp with a concentration of 3.5% to 4% is made; impurities are removed by a high-concentration cleaner and a coarse screen; and the pulp is divided into long fiber pulp and short fiber pulp by fiber classification screening.

4. The production process of the new type of gypsum board facing paper according to claim 1 or 3, characterized in that: After passing through a low-concentration cleaner and fine screen, the long-fiber pulp enters a multi-disc thickener to be concentrated to a concentration of 8 to 10%, and then is transported to a heat dispersion treatment, and then is beaten to 30±2°SR by a double-disc refiner; after passing through a low-concentration cleaner, the short-fiber pulp enters a multi-disc thickener to be concentrated to a concentration of 8 to 10%.

5. The production process of the new type of gypsum board facing paper according to claim 1 is characterized in that: The pore size of the pressure screen is 8 mm.

6. The production process of the new type of gypsum board facing paper according to claim 1 is characterized in that: In step (2), the mixed slurry enters the flow system to form a slurry with a concentration of 0.4%-0.8%, which is dispersed and sprayed onto the screen through a headbox.

7. The production process of the new type of gypsum board facing paper according to any one of claims 1 to 4, characterized in that: In step (2), the lining layer of the mesh uses a mixed pulp of 10% to 40% wood pulp slurry, 20% to 50% long fiber slurry and 0% to 20% short fiber slurry, the core layer of the mesh uses a mixed pulp of 10% to 40% wood pulp slurry, 0% to 30% long fiber slurry and 20% to 40% short fiber slurry, and the bottom layer of the mesh uses a mixed pulp of 10% to 40% wood pulp slurry, 20% to 50% long fiber slurry and 0% to 20% short fiber slurry.

8. The production process of the new type of gypsum board facing paper according to claim 1 or 6, characterized in that: Add sizing agent, retention and filtration aid, aluminum sulfate and starch in the pulp into the flow system, and adjust the amount of aluminum sulfate added to ensure that the pH of the pulp in the headbox does not exceed 6.

8.

9. The production process of the new type of gypsum board facing paper according to claim 1 is characterized in that: In step (2), the mixed slurry enters the flow conveying system for dispersion and is then sprayed onto the wire surface. It is then dehydrated by gravity or vacuum on the wire to a dryness of 10%-14%. After being pressed, pre-dried, coated with glue, post-dried, and rolled up, the finished paper is obtained.

Citation Information

Patent Citations

  • Composite decorative paper for artificial board and preparation method thereof

    CN104313936A

  • Production technique for improving strength of gypsum board covering paper

    CN106555359A

  • Production process of low-basis-weight damp-proof waterproof coveying paper

    CN107313300A

  • Method for making high-grade packaging paper by mixing and pulping high-calorie pulp and waste paper

    CN116536968A

  • Manufacturing process of bleached wood pulp fine dried noodle gypsum board covering paper

    CN117488594A