Thickening agent molecular weight optimization method, device and equipment for improving resistance reduction rate and medium

By dividing and optimizing the molecular weight of polyacrylamide during fracturing and forming the optimal mixed conformation, the problem of insufficient resistance reduction of existing thickeners in deep and ultra-deep reservoir fracturing is solved, and more efficient reduction is achieved Resistance effect.

CN119069008APending Publication Date: 2024-12-03BETTER OILFIELD TECH +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411152595.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The existing thickeners for fracturing are blind and arbitrary in raw material processing and suspension emulsion preparation, and cannot meet the ultra-high resistance reduction requirements for deep and ultra-deep reservoir fracturing transformation.

Method used

By dividing the molecular weight range of polyacrylamide, input temperature, pressure and molecular weight into the preset pipeline model, determine the single-molecular conformation and proportional conformation, combine to form a mixed conformation, and screen out the optimal conformation to improve the resistance reduction.

Benefits of technology

The molecular weight of the thickener is optimized, the resistance reduction is improved, and the ultra-high resistance reduction requirements for deep and ultra-deep reservoir fracturing transformation is met, avoiding the blindness and arbitrary nature of raw material processing and suspension emulsion preparation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069008A_ABST
    Figure CN119069008A_ABST
Patent Text Reader

Abstract

The invention discloses a thickening agent molecular weight optimization method, a thickening agent molecular weight optimization device, thickening agent molecular weight optimization equipment and a medium for improving resistance reduction rate. The method comprises the following steps: dividing to obtain a plurality of polyacrylamide molecular weight ranges; obtaining a first single-molecule conformation corresponding to the molecular weight of the polyacrylamide; obtaining a second proportion conformation under the proportion of the molecular weight range of the polyacrylamide; determining a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportion conformations; determining an optimal third mixed conformation and the resistance reduction rate of the optimal third mixed conformation from the plurality of third mixed conformations; and determining whether the optimal third mixed conformation is the target conformation or not according to the resistance reduction rate of the first single-molecule conformation and the resistance reduction rate of the second proportion conformation which form the optimal third mixed conformation and the resistance reduction rate of the optimal third mixed conformation. The invention belongs to the field of thickening agent molecule optimization. The thickening agent for fracturing can be prevented from having great blindness and randomness in the aspects of raw material processing and suspension emulsion preparation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to thickener molecule optimization, and in particular to a thickener molecular weight optimization method, device, equipment and medium for improving drag reduction rate. Background Art

[0002] Fracturing construction is an important measure to increase the production of oil and gas reservoirs. The most commonly used fracturing fluid in fracturing construction is water-based fracturing fluid. Thickener is the main component of water-based fracturing fluid. Thickener can improve the fluidity of fracturing fluid, increase the ability of liquid to suspend solid particles, and help to generate greater osmotic pressure in underground rock cracks, thereby enhancing the production capacity of oil and gas reservoirs. The commonly used polyacrylamide suspension emulsion thickener has an important function in addition to increasing viscosity in fracturing fluid and reducing fracturing fluid filtration, namely reducing fracturing fluid friction. Improving the drag reduction rate can increase the net construction pressure to create the prerequisite for forming the optimal complex fracture network and reduce the construction pressure, thereby improving the efficiency of oil and gas production.

[0003] During the fracturing construction process, due to the large displacement and fast pumping speed, in order to improve the short-term hydration viscosity and high temperature and salt resistance of the thickener, large molecular weight polyacrylamide is completely used as the solid particles of the suspension emulsion. Some wells have high construction pressure in the middle and choose to reduce the displacement, resulting in slow and incomplete stretching of the long chain of large molecular weight polyacrylamide during the fracturing fluid pumping process. It is difficult to disturb the water molecules at low displacement, so the dynamic volume is small, the fluid friction is still high, and the drag reduction rate is basically ≤70%, which cannot meet the ultra-high drag reduction rate requirements of the current deep and ultra-deep reservoir fracturing transformation. At present, the thickener for fracturing has great blindness and arbitrariness in raw material processing and suspension emulsion preparation, which cannot meet the ultra-high drag reduction rate requirements of the deep and ultra-deep reservoir fracturing transformation. In view of this, how to optimize the molecular weight of the thickener to improve the drag reduction rate is an urgent problem to be solved. Summary of the invention

[0004] The embodiments of the present application provide a method, device, equipment and medium for optimizing the molecular weight of a thickener for improving the drag reduction rate, thereby solving the technical problem in the prior art that thickeners for fracturing have great blindness and arbitrariness in raw material processing and suspension emulsion preparation, and achieving the technical effect of optimizing the molecular weight of the thickener and improving the drag reduction rate.

[0005] In a first aspect, the present application provides a method for optimizing the molecular weight of a thickener for improving drag reduction, the method comprising:

[0006] Several polyacrylamide molecular weight ranges are obtained by division;

[0007] Inputting a preset temperature, a preset pressure and a molecular weight of polyacrylamide into a preset pipeline model, and obtaining a first single-molecule conformation corresponding to the molecular weight of polyacrylamide;

[0008] Input a preset temperature, a preset pressure, and a molecular weight range ratio of polyacrylamide into a preset pipeline model to obtain a second ratio conformation under the molecular weight range ratio of polyacrylamide;

[0009] Determining a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportioned conformations;

[0010] Determining an optimal third hybrid conformation and a drag reduction rate of the optimal third hybrid conformation from a plurality of third hybrid conformations;

[0011] According to the drag reduction rate of the first single-molecule conformation constituting the optimal third hybrid conformation and the drag reduction rate of the second proportion conformation, and the drag reduction rate of the optimal third hybrid conformation, it is determined whether the optimal third hybrid conformation is the target conformation.

[0012] Further, according to the drag reduction rate of the first single-molecule conformation constituting the optimal third hybrid conformation and the drag reduction rate of the second proportion conformation, and the drag reduction rate of the optimal third hybrid conformation, determining whether the optimal third hybrid conformation is the target conformation includes:

[0013] If the drag reduction rate of the optimal third hybrid conformation is greater than the drag reduction rate of the first single-molecule conformation constituting the optimal third hybrid conformation, and greater than the drag reduction rate of the second proportion conformation constituting the optimal third hybrid conformation, then the optimal third hybrid conformation is the target conformation.

[0014] Further, an optimal third hybrid conformation is determined from a plurality of third hybrid conformations, including:

[0015] The maximum value among several third hybrid conformations is taken as the optimal third hybrid conformation.

[0016] Further, according to the plurality of first single-molecule conformations and the plurality of second proportion conformations, a plurality of third mixed conformations are determined, including:

[0017] Combining a number of first single-molecule conformations and a number of second proportion conformations respectively to obtain a number of combined conformations;

[0018] Several combination conformations of disorder, oblique entanglement and curling were eliminated, and the combination conformations that were not eliminated were taken as the third mixed conformation.

[0019] Furthermore, it includes: the conformation includes hydrodynamic volume, perturbation elastic strength, main chain stretching speed and main chain stretching length.

[0020] Further, it includes: the molecular weight range of polyacrylamide includes a first range, a second range and a third range, wherein the molecular weight of polyacrylamide in the first range is 1 million to 10 million, the molecular weight of polyacrylamide in the second range is 10 million to 20 million, and the molecular weight of polyacrylamide in the third range is 20 million to 30 million.

[0021] Furthermore, a preset pipeline model is constructed, including:

[0022] Input pre-set parameters into the preset molecular dynamics simulation software to construct a preset pipeline model. The pre-set parameters include the volume of water molecules, the viscosity of water molecules, and the flow rate of water molecules.

[0023] In a second aspect, the present application provides a thickener molecular weight optimization device for improving drag reduction, the device comprising:

[0024] A partitioning module, used for obtaining several molecular weight ranges of polyacrylamide by partitioning;

[0025] A first conformation module, used to input a preset temperature, a preset pressure and a molecular weight of polyacrylamide in a preset pipeline model, and obtain a first single-molecule conformation corresponding to the molecular weight of polyacrylamide;

[0026] A second conformation module is used to input a preset temperature, a preset pressure and a molecular weight range proportion of polyacrylamide in a preset pipeline model to obtain a second conformation under the molecular weight range proportion of polyacrylamide;

[0027] A third conformation module, used for determining a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportion conformations;

[0028] An optimal conformation module, used to determine an optimal third hybrid conformation and a drag reduction rate of the optimal third hybrid conformation from a plurality of third hybrid conformations;

[0029] The target conformation module is used to determine whether the optimal third mixed conformation is the target conformation based on the drag reduction rate of the first single molecule conformation and the drag reduction rate of the second proportion conformation that constitute the optimal third mixed conformation, as well as the drag reduction rate of the optimal third mixed conformation.

[0030] In a third aspect, the present application provides an electronic device, including:

[0031] processor;

[0032] a memory for storing processor-executable instructions;

[0033] The processor is configured to execute to implement a method for optimizing the molecular weight of a thickener for improving the drag reduction rate as provided in the first aspect.

[0034] In a fourth aspect, the present application provides a non-temporary computer-readable storage medium. When the instructions in the storage medium are executed by a processor of an electronic device, the electronic device is enabled to implement a method for optimizing the molecular weight of a thickener for improving the drag reduction rate as provided in the first aspect.

[0035] One or more technical solutions provided in the embodiments of the present application have at least the following technical effects or advantages:

[0036] The present application provides a thickener molecular weight optimization method for improving drag reduction rate, comprising: obtaining a plurality of polyacrylamide molecular weight ranges by division; inputting a preset temperature, a preset pressure and a polyacrylamide molecular weight in a preset pipeline model to obtain a first single molecule conformation corresponding to the polyacrylamide molecular weight; inputting a preset temperature, a preset pressure and a polyacrylamide molecular weight range proportion in the preset pipeline model to obtain a second proportion conformation under the polyacrylamide molecular weight range proportion; determining a plurality of third mixed conformations according to the plurality of first single molecule conformations and the plurality of second proportion conformations; determining an optimal third mixed conformation and a drag reduction rate of the optimal third mixed conformation from the plurality of third mixed conformations; determining whether the optimal third mixed conformation is a target conformation according to the drag reduction rate of the first single molecule conformation constituting the optimal third mixed conformation and the drag reduction rate of the second proportion conformation, as well as the drag reduction rate of the optimal third mixed conformation. The present application combines the first single molecule conformation and the second proportion conformation to obtain a plurality of third mixed conformations, and obtains the target conformation through screening and comparison, thereby avoiding the great blindness and arbitrariness of the thickener for fracturing in the raw material processing and suspension emulsion preparation, realizing the optimization of the thickener molecular weight, improving the drag reduction rate, and meeting the ultra-high drag reduction rate requirements for the current deep and ultra-deep reservoir fracturing transformation. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0038] Figure 1 A schematic diagram of a flow chart of a method for optimizing the molecular weight of a thickener for improving drag reduction provided in the present application;

[0039] Figure 2 A schematic diagram of the structure of a thickener molecular weight optimization device for improving drag reduction provided in the present application;

[0040] Figure 3 A schematic diagram of the structure of an electronic device provided in this application. DETAILED DESCRIPTION

[0041] The embodiment of the present application solves the technical problem in the prior art that thickeners for fracturing have great blindness and arbitrariness in raw material processing and suspension emulsion preparation by providing a method for optimizing the molecular weight of the thickener for improving the drag reduction rate.

[0042] The technical solution of the embodiment of the present application is to solve the above technical problems, and the overall idea is as follows:

[0043] A method for optimizing the molecular weight of a thickener for improving drag reduction rate comprises: obtaining a plurality of polyacrylamide molecular weight ranges by division; inputting a preset temperature, a preset pressure and a polyacrylamide molecular weight into a preset pipeline model to obtain a first single molecule conformation corresponding to the polyacrylamide molecular weight; inputting a preset temperature, a preset pressure and a polyacrylamide molecular weight range proportion into the preset pipeline model to obtain a second proportion conformation under the polyacrylamide molecular weight range proportion; determining a plurality of third mixed conformations according to the plurality of first single molecule conformations and the plurality of second proportion conformations; determining an optimal third mixed conformation and a drag reduction rate of the optimal third mixed conformation from the plurality of third mixed conformations; determining whether the optimal third mixed conformation is a target conformation according to the drag reduction rate of the first single molecule conformation constituting the optimal third mixed conformation, the drag reduction rate of the second proportion conformation, and the drag reduction rate of the optimal third mixed conformation.

[0044] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0045] First of all, the term "and / or" in this article is only a description of the association relationship of the associated objects, indicating that there can be three relationships. For example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.

[0046] This application provides Figure 1 A method for optimizing the molecular weight of a thickener for improving drag reduction rate is shown, comprising steps S11-S16:

[0047] Regarding step S11, several polyacrylamide molecular weight ranges are obtained by division.

[0048] Each polyacrylamide molecule corresponds to a polyacrylamide molecular weight. For example, the molecular weight of a polyacrylamide molecule is 200. The molecular weight range of polyacrylamide can be divided according to actual needs. The present application provides a division method, including: a first range, a second range and a third range, wherein the molecular weight of the polyacrylamide molecules in the first range is 1 million to 10 million; the molecular weight of the polyacrylamide molecules in the second range is 10 million to 20 million; the molecular weight of the polyacrylamide molecules in the third range is 20 million to 30 million.

[0049] Regarding step S12, a preset temperature, a preset pressure and a molecular weight of polyacrylamide are input into a preset pipeline model to obtain a first single molecule conformation corresponding to the molecular weight of polyacrylamide.

[0050] Before inputting the preset temperature, preset pressure, and molecular weight of polyacrylamide into the preset pipeline model, the preset pipeline model may be constructed first, including:

[0051] Input pre-set parameters into the preset molecular dynamics simulation software to construct a preset pipeline model. The pre-set parameters include the volume of water molecules, the viscosity of water molecules, and the flow rate of water molecules.

[0052] The molecular dynamics simulation software used in this application is Materials Studio. The purpose of building a preset pipeline model can be achieved by inputting the volume of water molecules, the viscosity of water molecules, and the flow rate of water molecules into Materials Studio.

[0053] After constructing the preset pipeline model, the preset temperature, preset pressure and the molecular weight of a single polyacrylamide molecule are input into the preset pipeline model in the molecular dynamics simulation software to obtain the first single-molecule conformation corresponding to the molecular weight of the single polyacrylamide molecule. The first single-molecule conformation includes the hydrodynamic volume, the perturbation elastic strength, the main chain stretching speed and the main chain stretching length.

[0054] Among them, the preset temperature and the preset pressure can be determined according to the actual situation, and the preset temperature and the preset pressure in the present application are the same. For example, by inputting a polyacrylamide molecule with a molecular weight of 600, the hydrodynamic volume, perturbation elastic strength, main chain stretching speed and main chain stretching length corresponding to the polyacrylamide molecule with a molecular weight of 600 can be obtained. It can be seen that each polyacrylamide molecular weight corresponds to a first single molecule conformation, that is, corresponds to a set of hydrodynamic volume, perturbation elastic strength, main chain stretching speed and main chain stretching length.

[0055] Regarding step S13, a preset temperature, a preset pressure and a molecular weight range ratio of polyacrylamide are input into a preset pipeline model to obtain a second ratio conformation under the molecular weight range ratio of polyacrylamide.

[0056] The difference between step S13 and step S12 is that the molecular weight range ratio of polyacrylamide inputted in step S13 refers to the ratio of the first range, the second range, or the third range mentioned above.

[0057] It should be understood that the percentage of the first range, the second range, or the third range does not include a specific molecular weight of polyacrylamide.

[0058] For example, the proportions of the first range, the second range, and the third range are 20%, 30%, and 50%, respectively, and the proportions (the proportions of the molecular weight range of the polyacrylamide) correspond to the second proportion conformation A;

[0059] For another example, the first range and the second range account for 50% and 50% respectively, corresponding to the second accounting conformation B;

[0060] For another example, the proportion of the third range is 100%, corresponding to the second proportion conformation C.

[0061] It can be seen that the combination of the proportions of the first range, the second range, or the third range can be various, and each range does not include a specific molecular weight of polyacrylamide.

[0062] Regarding step S14, a plurality of third mixed conformations are determined according to the plurality of first single-molecule conformations and the plurality of second proportion conformations.

[0063] In step S13, only the second proportion conformation corresponding to the proportion of the molecular weight range of polyacrylamide is obtained, but the second proportion conformation does not include the specific molecular weight of polyacrylamide, so the first single molecule conformation and the second proportion conformation can be combined.

[0064] It should be particularly noted that when the first single molecule conformation and the second proportional conformation are combined, there is only one molecular weight of polyacrylamide in each range.

[0065] For example, the first single molecular weight is 6 million, 15 million, and 25 million, and the corresponding first single molecule conformations are D, E, and F, respectively. The proportions of the first range, the second range, and the third range are 20%, 30%, and 50%, respectively, and the corresponding second proportion conformations are A. A, D, E, and F together constitute the third mixed conformation, among which the first range corresponds to only one first single molecular weight of 600, the second range corresponds to only one first single molecular weight of 15 million, and the third range corresponds to only one first single molecular weight of 25 million.

[0066] In addition, in order to improve efficiency and avoid interference from some conformations, it also includes:

[0067] Several first single-molecule conformations and several second proportioning conformations are combined respectively to obtain several combined conformations; several disordered, obliquely entangled and curled combined conformations are eliminated, and the combined conformations that are not eliminated are used as the third mixed conformation.

[0068] Regarding step S15, an optimal third mixing configuration and a drag reduction rate of the optimal third mixing configuration are determined from a plurality of third mixing configurations.

[0069] Specifically, the maximum value among several third hybrid conformations can be taken as the optimal third hybrid conformation.

[0070] It can be understood that the third hybrid conformation includes hydrodynamic volume, perturbation elastic strength, main chain stretching speed and main chain stretching length. The values ​​of hydrodynamic volume, perturbation elastic strength, main chain stretching speed and main chain stretching length can be added to obtain the value of the third hybrid conformation, and then the maximum value in the third hybrid conformation can be taken as the optimal third hybrid conformation.

[0071] Regarding step S16, it is determined whether the optimal third hybrid conformation is the target conformation based on the drag reduction rate of the first single molecule conformation and the drag reduction rate of the second proportion conformation constituting the optimal third hybrid conformation, as well as the drag reduction rate of the optimal third hybrid conformation.

[0072] If the drag reduction rate of the optimal third hybrid conformation is greater than the drag reduction rate of the first single-molecule conformation constituting the optimal third hybrid conformation, and greater than the drag reduction rate of the second proportion conformation constituting the optimal third hybrid conformation, then the optimal third hybrid conformation is the target conformation.

[0073] For example, the third hybrid conformation F is the optimal third hybrid conformation, the first single-molecule conformations constituting the third hybrid conformation F are D, E and F respectively, and the second proportion conformation constituting the third hybrid conformation F is A. The drag reduction rate of the third hybrid conformation F is compared with the drag reduction rates corresponding to D, E, F and A respectively. If the drag reduction rate of F is greater than the drag reduction rate corresponding to D, E, F and A, the third hybrid conformation F is taken as the target conformation, proving that the third hybrid conformation F can achieve the optimal drag reduction, and this design is the design that can achieve the optimal drag reduction. Specific embodiment 1:

[0075] For a certain Wei 20XH63-16 well:

[0076] Well Wei 20XH63-16 has a depth of 3176.52m (vertical depth) / 5505.00m (inclined depth), a formation pressure coefficient of about 1.71-1.81, a maximum horizontal principal stress of 89MPa, a minimum horizontal principal stress of 76MPa, a vertical stress of 80.4MPa, a horizontal stress difference of about 13MPa, and a construction displacement of 11-14m 3 / min, casing inner diameter 114.3mm, liquid viscosity 4.8Mpa·s, bottom temperature 118.62℃. The total amount of liquid entering the ground during the 29th stage of fracturing was 1636.58 3 , the amount of sand added is 170.38t, 100 mesh silt sand is 135.58t, and 40 / 70 mesh expanded clay is 34.8t.

[0077] Under the same well conditions, the construction pressure of the adjacent well is as high as 89Mpa, and the drag reduction rate is only 72%. The on-site well conditions require that the construction pressure of this well be lower than 78Mpa. Combined with the working conditions of this well, the molecular weight of polyacrylamide is optimized and analyzed through the POLYMORYH module of the molecular dynamics simulation software Materials Studio, and the molecular weight of the most active conformation under the well conditions and the proportion of each molecular weight addition are obtained. Among them, 20% of the 5 million low molecular weight polyacrylamide, 40% of the 12 million medium molecular weight polyacrylamide and 40% of the 28 million high molecular weight polyacrylamide, the drag reduction rate is measured by the indoor pipeline friction meter to reach 87.1%, realizing the optimization of the molecular weight of the thickener with ultra-high drag reduction rate under the well conditions and meeting the on-site construction requirements. Specific embodiment 2:

[0079] For a certain Wei 20XH63-15 well:

[0080] Well Wei 20XH63-15 has a depth of 3214.44 (vertical depth) / 5428.00m (inclined depth), a formation pressure coefficient of about 1.71-1.81, a maximum horizontal principal stress of 87MPa, a minimum horizontal principal stress of 74MPa, a vertical stress of 82.4MPa, a horizontal stress difference of about 13MPa, and a construction displacement of 12-16m 3 / min, casing inner diameter 114.3mm, liquid viscosity 4.7Mpa·s, bottom temperature 116.55℃. The total liquid volume entering the ground during the 16th stage of fracturing was 1366.07m 3 , the amount of sand added is 140.22t, 70 / 140 mesh quartz sand is 115.98t, 40 / 70 mesh ceramsite is 24.24t. Under the same well conditions, the construction pressure of the adjacent well is as high as 90Mpa, and the resistance reduction rate is only 73%. The construction pressure of this well is required to be lower than 80Mpa.

[0081] The molecular weight of the most active conformation under the well conditions and the proportion of each molecular weight added were obtained through the POLYMORYH module of the molecular dynamics simulation software Materials Studio. Among them, 30% of the 4 million low molecular weight polyacrylamide, 32% of the 14 million medium molecular weight polyacrylamide and 38% of the 24 million high molecular weight polyacrylamide, measured by the indoor pipeline friction meter, had a drag reduction rate of 85.3%, achieving the optimization of the molecular weight of the thickener with ultra-high drag reduction rate under the well conditions and meeting the on-site construction requirements. Specific embodiment 3:

[0083] For large 2X1 wells:

[0084] The depth of the 2X1 well is 4471.47 (vertical depth) / 6960.00m (inclined depth), the formation pressure coefficient is about 1.8-2.0, the maximum horizontal principal stress is 118MPa, the minimum horizontal principal stress is 102MPa, the vertical stress is 114.5MPa, the horizontal stress difference is about 16MPa, and the construction displacement is 16-18m 3 / min, casing inner diameter 114.3mm, liquid viscosity 4.9mPa·s, bottom temperature 108.02℃. The total liquid volume entering the ground during the 6th stage fracturing operation was 2763.9m 3 , the amount of sand added is 256.22t, 70 / 140 mesh quartz sand is 142.7t, and 40 / 70 mesh expanded clay is 113.52t.

[0085] Under the same well conditions, the construction pressure of the adjacent well is as high as 125MPa, and the drag reduction rate is only 75%. The construction pressure of this well is required to be lower than 115MPa. The molecular weight of the most active conformation under the well conditions and the proportion of each molecular weight addition are obtained through the POLYMORYH module of the molecular dynamics simulation software Materials Studio. Among them, 18% of 8 million low molecular weight polyacrylamide, 32% of 12 million medium molecular weight polyacrylamide and 50% of 26 million high molecular weight polyacrylamide, the drag reduction rate is measured by the indoor pipeline friction meter to reach 84%, realizing the optimization of the molecular weight of the thickener with ultra-high drag reduction rate under the well conditions and meeting the on-site construction requirements.

[0086] In summary, the present application provides a method for optimizing the molecular weight of a thickener for improving the drag reduction rate, comprising: obtaining a plurality of polyacrylamide molecular weight ranges by division; inputting a preset temperature, a preset pressure and a polyacrylamide molecular weight in a preset pipeline model to obtain a first single molecule conformation corresponding to the polyacrylamide molecular weight; inputting a preset temperature, a preset pressure and a polyacrylamide molecular weight range proportion in the preset pipeline model to obtain a second proportion conformation under the proportion of the polyacrylamide molecular weight range; determining a plurality of third mixed conformations according to the plurality of first single molecule conformations and the plurality of second proportion conformations; determining an optimal third mixed conformation and a drag reduction rate of the optimal third mixed conformation from the plurality of third mixed conformations; determining whether the optimal third mixed conformation is a target conformation according to the drag reduction rate of the first single molecule conformation constituting the optimal third mixed conformation and the drag reduction rate of the second proportion conformation, as well as the drag reduction rate of the optimal third mixed conformation. The present application combines the first single molecule conformation and the second proportion conformation to obtain a plurality of third mixed conformations, and obtains the target conformation through screening and comparison, thereby avoiding the great blindness and arbitrariness of the thickener for fracturing in the raw material processing and suspension emulsion preparation, realizing the optimization of the thickener molecular weight, improving the drag reduction rate, and meeting the ultra-high drag reduction rate requirements for the current deep and ultra-deep reservoir fracturing transformation.

[0087] Based on the same inventive concept, the present application provides Figure 2 A thickener molecular weight optimization device for improving drag reduction rate is shown, comprising:

[0088] A division module 21, used for obtaining a number of polyacrylamide molecular weight ranges by division;

[0089] A first conformation module 22, for inputting a preset temperature, a preset pressure and a molecular weight of polyacrylamide into a preset pipeline model, and obtaining a first single molecule conformation corresponding to the molecular weight of polyacrylamide;

[0090] The second conformation module 23 is used to input a preset temperature, a preset pressure and a molecular weight range ratio of polyacrylamide in a preset pipeline model to obtain a second conformation under the molecular weight range ratio of polyacrylamide;

[0091] A third conformation module 24, used to determine a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportion conformations;

[0092] An optimal configuration module 25, used to determine an optimal third hybrid configuration and a drag reduction rate of the optimal third hybrid configuration from a plurality of third hybrid configurations;

[0093] The target conformation module 26 is used to determine whether the optimal third mixed conformation is the target conformation according to the drag reduction rate of the first single molecule conformation and the drag reduction rate of the second proportion conformation constituting the optimal third mixed conformation, and the drag reduction rate of the optimal third mixed conformation.

[0094] Based on the same inventive concept, the present application also provides Figure 3 An electronic device as shown includes:

[0095] Processor 31;

[0096] A memory 32 for storing instructions executable by the processor 31;

[0097] The processor 31 is configured to execute to implement a thickener molecular weight optimization method for improving drag reduction rate as provided above.

[0098] Based on the same inventive concept, the present application also provides a non-temporary computer-readable storage medium. When the instructions in the storage medium are executed by the processor 31 of the electronic device, the electronic device can execute a thickener molecular weight optimization method for improving the drag reduction rate as provided above.

[0099] Since the electronic device introduced in this embodiment is an electronic device used to implement the information processing method in the embodiment of the present application, based on the information processing method introduced in the embodiment of the present application, a person skilled in the art can understand the specific implementation of the electronic device of the present embodiment and its various variations, so how the electronic device implements the method in the embodiment of the present application is not described in detail here. As long as a person skilled in the art implements the electronic device used by the information processing method in the embodiment of the present application, it belongs to the scope of protection of this application.

[0100] Those skilled in the art will appreciate that embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.

[0101] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (systems), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0102] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0103] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1The steps for the functions specified in one or more boxes.

[0104] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.

[0105] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A method for optimizing the molecular weight of a thickener for improving drag reduction, characterized in that: The method comprises: Several polyacrylamide molecular weight ranges are obtained by division; Inputting a preset temperature, a preset pressure and a molecular weight of polyacrylamide into a preset pipeline model, and obtaining a first single-molecule conformation corresponding to the molecular weight of polyacrylamide; Inputting the preset temperature, the preset pressure and the molecular weight range proportion of polyacrylamide into the preset pipeline model to obtain a second proportion conformation under the molecular weight range proportion of polyacrylamide; Determining a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportioned conformations; Determining an optimal third mixing conformation and a drag reduction rate of the optimal third mixing conformation from a plurality of third mixing conformations; According to the drag reduction rate of the first single-molecule conformation and the drag reduction rate of the second proportion conformation constituting the optimal third hybrid conformation, and the drag reduction rate of the optimal third hybrid conformation, it is determined whether the optimal third hybrid conformation is the target conformation.

2. A method for optimizing the molecular weight of a thickener for improving drag reduction as claimed in claim 1, characterized in that: The determining whether the optimal third mixed conformation is a target conformation according to the drag reduction rate of the first single-molecule conformation constituting the optimal third mixed conformation and the drag reduction rate of the second proportion conformation, and the drag reduction rate of the optimal third mixed conformation, comprises: If the drag reduction rate of the optimal third hybrid conformation is greater than the drag reduction rate of the first single-molecule conformation constituting the optimal third hybrid conformation, and greater than the drag reduction rate of the second proportion conformation constituting the optimal third hybrid conformation, then the optimal third hybrid conformation is the target conformation.

3. A method for optimizing the molecular weight of a thickener for improving drag reduction as claimed in claim 1, characterized in that: The optimal third hybrid conformation is determined from a number of third hybrid conformations, including: The maximum value among several third mixed conformations is taken as the optimal third mixed conformation.

4. A method for optimizing the molecular weight of a thickener for improving drag reduction as claimed in claim 1, characterized in that: The step of determining a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportion conformations comprises: Combining a number of first single-molecule conformations and a number of second proportion conformations respectively to obtain a number of combined conformations; Several combination conformations of disorder, oblique entanglement and curling were eliminated, and the combination conformations that were not eliminated were taken as the third mixed conformation.

5. A method for optimizing the molecular weight of a thickener for improving drag reduction as claimed in claim 1, characterized in that: include: The conformation includes hydrodynamic volume, perturbation elastic strength, main chain stretching speed and main chain stretching length.

6. A method for optimizing the molecular weight of a thickener for improving drag reduction as claimed in claim 1, characterized in that: include: The molecular weight range of polyacrylamide includes a first range, a second range and a third range, wherein the molecular weight of polyacrylamide in the first range is 1-10 million, the molecular weight of polyacrylamide in the second range is 10-20 million, and the molecular weight of polyacrylamide in the third range is 20-30 million.

7. A method for optimizing the molecular weight of a thickener for improving drag reduction as claimed in claim 1, characterized in that: Build a preset pipeline model, including: Inputting pre-set parameters into the preset molecular dynamics simulation software to construct the preset pipeline model, the pre-set parameters include the volume of water molecules, the viscosity of water molecules and the flow rate of water molecules.

8. A device for optimizing the molecular weight of a thickener for improving drag reduction, characterized in that: The device comprises: A partitioning module, used for obtaining several molecular weight ranges of polyacrylamide by partitioning; A first conformation module, used to input a preset temperature, a preset pressure and a molecular weight of polyacrylamide in a preset pipeline model, and obtain a first single-molecule conformation corresponding to the molecular weight of polyacrylamide; A second conformation module is used to input the preset temperature, the preset pressure and the molecular weight range proportion of polyacrylamide into the preset pipeline model to obtain a second proportion conformation under the molecular weight range proportion of polyacrylamide; A third conformation module, used for determining a plurality of third mixed conformations according to the plurality of first single-molecule conformations and the plurality of second proportion conformations; An optimal conformation module, used to determine an optimal third hybrid conformation and a drag reduction rate of the optimal third hybrid conformation from a plurality of third hybrid conformations; The target conformation module is used to determine whether the optimal third mixed conformation is the target conformation based on the drag reduction rate of the first single-molecule conformation and the drag reduction rate of the second proportion conformation constituting the optimal third mixed conformation, as well as the drag reduction rate of the optimal third mixed conformation.

9. An electronic device, characterized in that: include: processor; a memory for storing instructions executable by the processor; The processor is configured to execute a method for optimizing the molecular weight of a thickener for improving drag reduction rate as described in any one of claims 1 to 7.

10. A non-transitory computer-readable storage medium, characterized in that: When the instructions in the storage medium are executed by a processor of an electronic device, the electronic device is enabled to implement a method for optimizing the molecular weight of a thickener for improving drag reduction rate as described in any one of claims 1 to 7.