Sodium ion battery

By introducing manganese element into sodium ion batteries to catalyze the sulfur-containing compound SH to form a dense passivation film, the problem that organic electrolyte salts cannot be formed on the surface of the positive electrode current collector is solved, and the cycle life and high-temperature performance of the battery are improved.

CN119069632APending Publication Date: 2024-12-03LIYANG HINA BATTERY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411207078.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

When using organic electrolyte salts in sodium ion batteries under high temperature and high pressure conditions, a dense passivation film cannot be formed on the surface of the positive electrode current collector, resulting in positive electrode corrosion and a decrease in the battery cycle life.

Method used

The surface of the positive electrode current collector is introduced to catalyze the sulfur-containing compound SH to form a dense interface passivation film rich in inorganic components. By regulating the distribution of manganese elements and organic electrolyte salts, the sulfur-containing compound SH in the electrolyte solution is ensured in the positive electrode current collector by regulating the distribution of manganese elements and organic electrolyte salts. A passivation film that is resistant to high temperature and corrosion is generated on the surface.

Benefits of technology

It significantly improves the cycle life of the battery and capacity retention ability at high temperatures, reduces impedance growth, and enhances the overall performance of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_5
    Figure SMS_5
  • Figure SMS_6
    Figure SMS_6
Patent Text Reader

Abstract

The invention discloses a sodium ion battery, which comprises a positive electrode containing a manganese element and an electrolyte containing an organic electrolyte salt and an additive, the manganese element in the positive electrode is distributed in a positive electrode active material and a current collector, and the additive comprises one or more of sulfur compounds SH; the sodium ion battery meets the conditions that 1 < = d / (ab + 100ac) < = 125, 0.1% < = a < = 5%, 10% < = b < = 35%, 0.01% < = c < = 0.1% and 0.5% < = d < = 12%, a is the mass percentage content of the additive (namely the sulfur-containing compound SH) in the electrolyte, b is the mass percentage content of the manganese element in the positive electrode active material, c is the mass percentage content of the manganese element in the positive electrode current collector, and c is the mass percentage content of the manganese element in the negative electrode current collector. And d is the mass percentage content of the organic electrolyte salt in the electrolyte. The manganese element catalyzes the sulfur-containing compound SH to construct a passivation film on the surface of the positive electrode current collector, so that the capacity retention ratio of the battery at high temperature is improved, the impedance growth rate is reduced, and the battery performance is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of sodium ion batteries, and in particular to a sodium ion battery which utilizes the interaction between a sulfur-containing compound and manganese elements at different distribution positions in a positive electrode to generate a good passivation film. Background Art

[0002] Sodium-ion batteries have the same principle and similar structure as lithium-ion batteries, and have the characteristics of wide resources, low cost, wide temperature range and high safety. They have become an important development target for the next generation of secondary batteries. At present, the positive electrode materials of sodium-ion batteries mainly include transition metal oxides, polyanions, Prussian blue materials, etc. Among them, the layered oxide positive electrode materials have compaction density, high gram capacity and high voltage platform, which can enable sodium-ion batteries to achieve higher energy density, so they are considered to be the most promising positive electrode materials for large-scale application.

[0003] In order to achieve large-scale application of sodium-ion batteries, it is necessary to further improve the multiple energy density and cycle life. However, although the gram capacity and voltage platform of layered oxides as positive electrode materials can be improved by increasing the upper limit of charging voltage, NaPF6, which is often used as an electrolyte salt, will decompose under high or low pressure or high temperature conditions, poisoning the positive and negative solid electrolyte interface films (SEI and CEI) and causing battery performance degradation. Compared with NaPF6, organic electrolyte salts often have better high temperature and high pressure stability, higher conductivity and cation migration number in electrolytes, and are expected to become another widely used electrolyte salt after NaPF6. However, in sodium-ion batteries with high-voltage layered oxide positive electrodes, organic electrolyte salt anions cannot form a dense passivation film on the surface of the aluminum current collector to protect the positive electrode, which will cause corrosion of the positive electrode current collector and deteriorate the cycle life of the battery.

[0004] If we want to develop high-voltage, high-energy-density sodium-ion batteries containing organic electrolyte salts, we must solve the problem of corrosion of the positive electrode current collector. Summary of the invention

[0005] In view of the problems existing in the prior art, the present invention utilizes manganese to catalyze the sulfur-containing compound SH to form a dense interfacial passivation film containing sulfur-rich inorganic components on the surface of the positive electrode current collector, thereby solving the corrosion problem caused by the inability of organic electrolyte salts to form SEI and CEI. By regulating the organic electrolyte salt, the manganese element in the positive electrode and the sulfur-containing compound SH, a uniform and dense passivation film can be formed on the surface of the positive electrode current collector, which greatly improves the capacity retention ability of the battery at high temperature and reduces the impedance growth.

[0006] A sodium ion battery proposed in the present invention comprises a positive electrode containing manganese elements and an electrolyte containing an organic electrolyte salt and an additive, wherein the manganese elements in the positive electrode are distributed in the positive electrode active material and the current collector, and the additive comprises a sulfur-containing compound SH having a structure of formula I:

[0007]

[0008] wherein R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from C1-C3 halogenated or non-halogenated alkylene, R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 is located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 is located on the ring and directly connected to S. R3 is selected from H, F, C1-C3 halogenated or non-halogenated alkyl.

[0009] The sodium ion battery of the present invention satisfies 1≤d / (ab+100ac)≤125, and 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%, wherein a is the mass percentage of the compound represented by structural formula I in the electrolyte, b is the mass percentage of the Mn element in the positive electrode material, c is the mass percentage of the Mn element in the positive electrode current collector, and d is the mass percentage of the organic electrolyte salt in the electrolyte.

[0010] As some exemplary preferred solutions, we have preferred the range of 4≤d / (ab+100ac)≤24 on the basis of ensuring 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%. The above preferred range helps to further optimize the cycle stability and ion transport performance of the passivation film, not only maintaining the cycle stability under high temperature conditions, but also effectively reducing the amplitude of impedance growth.

[0011] As some exemplary preferred schemes, we prefer the single dosage of each component (1%≤a≤3.5%, 12.5%≤b≤25%, 0.03%≤c≤0.09%, 2.5%≤d≤10%), and at the same time prefer the range of 4≤d / (ab+100ac)≤24.

[0012] As a further solution, the positive electrode includes a positive electrode material layer and a positive electrode current collector containing manganese elements.

[0013] As a further embodiment, the positive electrode material layer includes a positive electrode active material containing manganese, a positive electrode binder and a positive electrode conductor.

[0014] As a further embodiment, the positive electrode active material containing a manganese element is an O3-phase metal layered oxide containing a manganese element, and the general formula of the O3-phase metal layered oxide containing a manganese element is Na x Mn y TM z O2, where 0.95 < x ≤ 1.05, 0.01 ≤ y ≤ 0.6, y + z = 1, and TM represents a transition metal element with an unfilled d electron orbital, specifically including one or more of scandium (Sc), yttrium (Y), lanthanide elements (from lanthanum (La) to lutetium (Lu)), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), copper (Cu), technetium (Tc), rhenium (Re), iron (Fe), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), nickel (Ni), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), mercury (Hg).

[0015] As a further embodiment, in the positive electrode active material Na x Mn y TM z O2, 0.95 < x ≤ 1.05, 0.01 ≤ y ≤ 0.55, and y + z = 1.

[0016] As a further embodiment, in the positive electrode active material Na x Mn y TM z O2, 0.95 < x ≤ 1.05, 0.1 ≤ y ≤ 0.5, y + z = 1, and TM includes Ni, Fe, and Cu.

[0017] As a further embodiment, the positive electrode active material of copper element is Na x Cu fa Ni b Fe c Mn y M dO2, where 0.95 < x ≤ 1.05, 0.02 ≤ a ≤ 0.19, 0.2 ≤ b ≤ 0.34, 0.2 ≤ c ≤ 0.4, 0.2 ≤ y ≤ 0.5, 0 ≤ d ≤ 0.2, and a + b + c + d = 1, and M is one or more of scandium (Sc), yttrium (Y), lanthanide elements (from lanthanum (La) to lutetium (Lu)), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), technetium (Tc), rhenium (Re), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), mercury (Hg).

[0018] As a further solution, the positive electrode binder includes at least one of a thermoplastic resin, an acrylic resin, sodium carboxymethyl cellulose, and styrene-butadiene rubber.

[0019] As a further solution, the positive electrode conductive agent includes a crystalline carbon material and an amorphous carbon material.

[0020] As a further solution, the positive electrode current collector containing a manganese element is a metal foil layer containing a manganese element.

[0021] As a further solution, the metal in the metal foil layer containing a manganese element can be selected from one or several of aluminum, nickel, tin, copper, and stainless steel.

[0022] As a further solution, the introduction method of the manganese element in the positive electrode current collector is not limited, and those skilled in the art can select according to actual needs, and can be selected from any one of mechanical alloying method, chemical vapor deposition method, physical vapor deposition (PVD) method, electroplating method, and alloying method.

[0023] As a still further solution, in the formula I structure of the sulfur-containing compound SH, R1 is selected from O, a C1-C3 alkylene group or an oxygen-containing alkylene group, and R2 is selected from R4 is selected from C or O, R5 is selected from O, a C1-C3 alkylene group or an oxygen-containing alkylene group, and at least one of R4 and R5 contains an O located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, a C1-C3 alkylene group or an oxygen-containing alkylene group, and at least one of R6 and R7 includes an O located on the ring and directly connected to S; R3 is selected from H, F, a C1-C3 halogenated or non-halogenated hydrocarbon group.

[0024] As a still further solution, in the formula I structure of the sulfur-containing compound SH, R1 is selected from O, a C1-C3 alkylene group or an oxygen-containing alkylene group, and R2 is selected from R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 includes O located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 includes O located on the ring and directly connected to S; R3 is selected from H, F, C1~C3 halogenated or non-halogenated hydrocarbon group.

[0025] As a further embodiment, the sulfur-containing compound SH has the structural formula II:

[0026]

[0027] Among them, R8, R 11 Selected from O, R9, R 10 A alkylene group selected from C1-C3.

[0028] As a further solution, the additive may further include a second additive.

[0029] As a further solution, the second additive is selected from at least one of cyclic carbonate compounds or fluorine-containing inorganic salt compounds.

[0030] As a further solution, the second additive contains an O=T structure, wherein T can be any one of S, P, B, and C.

[0031] As a further solution, the content of the second additive in the electrolyte is 0.1%-1.5%.

[0032] As a further embodiment, the electrolyte further includes an inorganic electrolyte salt, an organic electrolyte salt and a solvent.

[0033] As a further embodiment, the inorganic electrolyte salt is selected from borates, phosphates, sulfates, nitrates, antimonates, arsenates, and chlorates.

[0034] As a further embodiment, the inorganic electrolyte salt is substituted with fluorine.

[0035] As yet a further aspect, the inorganic electrolyte salt includes NaPF6.

[0036] As a further solution, the content of NaPF6 in the electrolyte is 1%≤NaPF6≤15%.

[0037] As a further solution, the content of NaPF6 in the electrolyte is 4%≤NaPF6≤11%.

[0038] As a further embodiment, the organic electrolyte salt includes an organic sulfonyl sodium salt.

[0039] As a further embodiment, the organic sulfonyl sodium salt includes an organic sulfonyl sodium salt substituted or halogenated with a halogen element or an organic sulfonyl sodium salt not substituted or halogenated with a halogen element.

[0040] As a further embodiment, the halogen element in the organic sulfonyl sodium salt substituted or halogenated with a halogen element is selected from F;

[0041] As a further embodiment, the organic sulfonyl sodium salt includes at least one of sulfonimide sodium salt, sulfonic acid sodium salt, sulfonyl chloride sodium salt, sulfonamide sodium salt, sulfonic acid ester sodium salt, sulfonylurea sodium salt, and sulfonamide methyl ester sodium salt.

[0042] As a further embodiment, the organic sulfonyl sodium salt includes at least one of sulfonimide sodium salt and sulfonic acid sodium salt.

[0043] As a further solution, the content of the organic electrolyte salt in the electrolyte is 5%-10%.

[0044] As a further solution, the solvent includes at least one of a linear carbonate solvent, a carboxylate solvent, and a phosphate solvent.

[0045] The sodium ion battery provided by the present invention also includes a negative electrode and a separator.

[0046] Compared with the prior art, the present invention has at least the following beneficial effects:

[0047] The sodium ion battery provided by the present invention uses a sulfur-containing compound SH as an additive and a manganese element as a catalyst, and utilizes the manganese element introduced into the positive electrode material to catalyze the sulfur-containing compound SH to form a dense interface passivation film containing sulfur-rich inorganic components on the surface of the positive electrode current collector. By adjusting 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%, and 1≤d / (ab+100ac)≤125, the sulfur-containing compound SH is catalyzed to form a high-temperature resistant and corrosion-resistant dense passivation film on the surface of the positive electrode current collector, thereby solving the problem that organic electrolyte salts cannot form SEI and CEI in sodium batteries, and improving the battery cycle life.

[0048] The passivation film of the present invention exhibits excellent chemical stability, and can provide long-lasting and reliable protection for the positive electrode current collector even in a high temperature environment, ensuring the stability of the contact surface between the positive electrode material and the current collector, thereby enhancing the capacity retention of the battery under high temperature conditions, reducing the increase in resistance, and significantly improving the overall performance of the battery. In addition, the organic electrolyte salt introduced in the present invention can significantly improve the conductivity and cation migration efficiency of the battery, thereby increasing the capacity of the battery. DETAILED DESCRIPTION

[0049] For ease of understanding, the battery electrolyte of the present invention will be described in more detail below, and examples of the present invention will be given, but the scope of the present invention is not limited thereby.

[0050] A sodium ion battery proposed in the present invention comprises a positive electrode containing manganese elements and an electrolyte containing an organic electrolyte salt and an additive, wherein the manganese elements in the positive electrode are distributed in the positive electrode active material and the current collector, and the additive comprises a sulfur-containing compound SH having a structure of formula I:

[0051]

[0052] wherein R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from C1-C3 halogenated or non-halogenated alkylene, R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 is located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 is located on the ring and directly connected to S. R3 is selected from H, F, C1-C3 halogenated or non-halogenated alkyl.

[0053] The sodium ion battery of the present invention satisfies 1≤d / (ab+100ac)≤125, and 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%, wherein a is the mass percentage of the compound represented by structural formula I in the electrolyte, b is the mass percentage of the Mn element in the positive electrode material, c is the mass percentage of the Mn element in the positive electrode current collector, and d is the mass percentage of the organic electrolyte salt in the electrolyte.

[0054] The sulfur-containing compound SH is used as an additive to introduce manganese into the positive electrode active material and the positive electrode current collector. The manganese element is used to catalyze the sulfur-containing compound containing structural formula I to form a dense interfacial passivation film containing sulfur-rich inorganic components on the surface of the aluminum alloy positive electrode current collector, effectively inhibiting the corrosion of the organic electrolyte salt in the non-aqueous electrolyte to the aluminum positive electrode current collector. The Mn element introduced into the positive electrode active material can not only catalyze the sulfur-containing compound to form a passivation film, but also serve as a transition metal element with a stable structure in the positive electrode material, providing a stable two-dimensional layered structure for the positive electrode material. The trace Mn element introduced into the positive electrode current collector can catalyze the formation of the passivation film while giving the current collector higher hardness, strength and corrosion resistance. When the manganese element, sulfur-containing compound and organic electrolyte salt introduced into the positive electrode active material and the positive electrode current collector meet the conditions: 1≤d / (ab+100ac)≤125, and 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%, it can not only inhibit the corrosion of the positive electrode current collector, but also significantly improve the capacity retention rate of the battery at high temperature and improve the battery cycle life.

[0055] Under the catalysis of manganese in the positive electrode, sulfur-containing compounds SH gather on the surface of the positive electrode current collector and react bidirectionally from the inside out and from the outside in, forming a dense composite passivation film rich in inorganic components, which effectively inhibits the corrosion of organic electrolyte salts on the positive electrode current collector, reduces the occurrence of battery side reactions and reduces the overall ohmic impedance.

[0056] Due to the special multivalent characteristics of Mn, after introducing it into the positive electrode material, it can give the positive electrode material a higher energy density; at the same time, the introduction of manganese can effectively improve the stability of the battery under high temperature conditions and improve battery performance; during the first charging process, the Mn element in the positive electrode material migrates to the surface of the current collector, catalyzing the sulfur-containing compound SH to form a dense passivation film rich in inorganic components from the outside to the inside on the surface of the positive electrode current collector, protecting the positive electrode current collector.

[0057] When manganese is introduced into the positive electrode current collector, it not only enhances the mechanical properties of the positive electrode current collector material, but the Mn element on the surface of the current collector can also catalyze the sulfur-containing compounds SH in the electrolyte during the first charging process to form a dense sulfur-containing composite passivation film rich in inorganic components from the inside out, further protecting the positive electrode current collector.

[0058] The present invention comprehensively considers the addition and distribution state of manganese elements and the influence of additives on the reactivity of manganese elements under different distribution conditions, and analyzes in detail the independent influence and interaction of the addition amount of each component on the battery performance. By constructing and revealing the influence of the addition amount and stoichiometric relationship of each component on the formation of the passivation film, the component relationship is optimized, thereby significantly improving the electrochemical performance of sodium ion batteries under high temperature conditions.

[0059] Specifically, we first determined the single dosage of each component (0.1% ≤ a ≤ 5%, 10% ≤ b ≤ 35%, 0.01% ≤ c ≤ 0.1%, 0.5% ≤ d ≤ 12%) to ensure that the sodium ion battery with manganese and additives can achieve the corresponding basic performance. Further, d / (ab+100ac) reflects the influence of the concentration of organic electrolyte salt in the electrolyte relative to other key components in the battery (compound A, the content of manganese in the positive electrode material and the current collector), and reflects the influence of the corresponding content relationship on the reaction degree of sulfur-containing compound SH with the manganese in the positive electrode active material and the positive electrode current collector, as well as the influence of the distribution position of manganese. We found that when the value of a*(b+100c) / d is 1≤d / (ab+100ac)≤125, the sodium ion battery can obtain better high-temperature electrochemical performance. d / (ab+100ac)≤1 or 125≤d / (ab+100ac) may cause the content and distribution of sulfur-containing compounds SH and manganese elements in the positive electrode material to be mismatched, resulting in the generated passivation film being insufficient to adapt to the content of organic electrolyte salts. Through d / (ab+100ac), we can better understand and optimize the synergistic effect of different materials and components in the battery to achieve optimal electrochemical performance and stability. On the basis of the above, the appropriate mass ratio of each component material ensures the density and efficiency of the passivation film generated in the battery system, providing the premise and guarantee for obtaining batteries with improved comprehensive performance.

[0060] As some exemplary preferred solutions, we have preferred the range of 4≤d / (ab+100ac)≤24 on the basis of ensuring 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%. The above preferred range helps to further optimize the cycle stability and ion transport performance of the passivation film, not only maintaining the cycle stability under high temperature conditions, but also effectively reducing the amplitude of impedance growth.

[0061] As some exemplary preferred schemes, we prefer the single dosage of each component (1%≤a≤3.5%, 12.5%≤b≤25%, 0.03%≤c≤0.09%, 2.5%≤d≤10%), and at the same time prefer the range of 4≤d / (ab+100ac)≤24.

[0062] As a further solution, the positive electrode includes a positive electrode material layer and a positive electrode current collector containing manganese elements.

[0063] As a further embodiment, the positive electrode material layer includes a positive electrode active material containing manganese, a positive electrode binder and a positive electrode conductor.

[0064] As a further solution, the manganese-containing positive electrode active material is an O3-phase metal layered oxide containing manganese, and the general formula of the O3-phase metal layered oxide containing manganese is Nax Mn y TM z O₂, where 0.95 < x ≤ 1.05, 0.01 ≤ y ≤ 0.6, y + z = 1, and TM represents a transition metal element with unfilled d electron orbitals, specifically including one or more of scandium (Sc), yttrium (Y), lanthanide elements (from lanthanum (La) to lutetium (Lu)), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), copper (Cu), technetium (Tc), rhenium (Re), iron (Fe), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), nickel (Ni), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), and mercury (Hg).

[0065] As a further embodiment, the manganese-containing cathode active material Na x Mn y TM z O₂ has 0.95 < x ≤ 1.05, 0.01 ≤ y ≤ 0.55, and y + z = 1.

[0066] As a further embodiment, the manganese-containing cathode active material Na x Mn y TM z O₂ has 0.95 < x ≤ 1.05, 0.1 ≤ y ≤ 0.5, y + z = 1, and TM includes Ni, Fe, and Cu.

[0067] As a further embodiment, the copper-containing cathode active material Na x Cu fa Ni b Fe c Mn y M d O₂, where 0.95 < x ≤ 1.05, 0.02 ≤ a ≤ 0.19, 0.2 ≤ b ≤ 0.34, 0.2 ≤ c ≤ 0.4, 0.2 ≤ y ≤ 0.5, 0 ≤ d ≤ 0.2, and a + b + c + d = 1, and M is one or more of scandium (Sc), yttrium (Y), lanthanide elements (from lanthanum (La) to lutetium (Lu)), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), technetium (Tc), rhenium (Re), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), and mercury (Hg).

[0068] As a further solution, the manganese-containing positive electrode active material includes NaCu 1 / 9 Ni 2 / 9 Fe 1 / 3 Mn 1 / 3 O2.

[0069] As a further solution, the positive electrode binder includes at least one of thermoplastic resin, acrylic resin, sodium carboxymethyl cellulose and styrene butadiene rubber.

[0070] As a further embodiment, the thermoplastic resin includes at least one of polyvinylidene fluoride, copolymers of vinylidene fluoride, polytetrafluoroethylene, copolymers of vinylidene fluoride-hexafluoropropylene, copolymers of tetrafluoroethylene-hexafluoropropylene, copolymers of tetrafluoroethylene-perfluoroalkyl vinyl ether, copolymers of ethylene-tetrafluoroethylene, copolymers of vinylidene fluoride-tetrafluoroethylene, copolymers of vinylidene fluoride-trifluoroethylene, copolymers of vinylidene fluoride-trichloroethylene, copolymers of vinylidene fluoride-fluoroethylene, copolymers of vinylidene fluoride-hexafluoropropylene-tetrafluoroethylene, thermoplastic polyimide, polyethylene and polypropylene.

[0071] As a further embodiment, the acrylic resin includes at least one of vinyl acrylate resin, methyl acrylate resin, butyl acrylate resin, acrylic styrene resin, acrylate resin, acrylate copolymer resin, acrylic resin, and acrylic emulsion resin.

[0072] As a further embodiment, the positive electrode conductor includes a crystalline carbon material and an amorphous carbon material.

[0073] As a further solution, the crystalline carbon material includes at least one of conductive graphite, carbon nanotubes, graphene, and reduced graphene oxide.

[0074] As a further solution, the amorphous carbon material includes at least one of conductive carbon black, conductive carbon balls, and conductive carbon fibers.

[0075] As a further solution, the positive electrode current collector containing manganese element is a metal foil layer containing manganese element.

[0076] As a further solution, the metal in the metal foil layer containing manganese element can be selected from one or more of aluminum, nickel, tin, copper and stainless steel.

[0077] As a further solution, the method of introducing the manganese element into the positive electrode current collector is not limited, and technicians can choose according to actual needs, and can be selected from any one of mechanical alloying, chemical vapor deposition, physical vapor deposition (PVD), electroplating, and alloying.

[0078] As a further embodiment, in the structure of formula I of the sulfur-containing compound SH, R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 includes O located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 includes O located on the ring and directly connected to S; R3 is selected from H, F, C1~C3 halogenated or non-halogenated hydrocarbon group.

[0079] As a further embodiment, in the structure of formula I of the sulfur-containing compound SH, R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 includes O located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 includes O located on the ring and directly connected to S; R3 is selected from H, F, C1~C3 halogenated or non-halogenated hydrocarbon group.

[0080] As a further embodiment, the sulfur-containing compound SH has the structural formula II:

[0081]

[0082] Among them, R8, R 11 Selected from O, R9, R 10 A alkylene group selected from C1-C3.

[0083] As a further embodiment, the present invention also provides a sulfur-containing compound SH selected from

[0084]

[0085] One of them.

[0086] As a further solution, the additive may further include a second additive.

[0087] As a further solution, the second additive is selected from at least one of cyclic carbonate compounds or fluorine-containing inorganic salt compounds.

[0088] As a further solution, the second additive contains an O=T structure, wherein T can be any one of S, P, B, and C.

[0089] As a further embodiment, the cyclic carbonate compound is at least one selected from vinylene carbonate (VC), vinyl ethylene carbonate, methylene carbonate, fluoroethylene carbonate (FEC), trifluoromethylethylene carbonate, and bisfluoroethylene carbonate.

[0090] As a further solution, the fluorine-containing inorganic salt compound includes any one of sodium difluorophosphate (NaPO2F2), sodium difluorooxalatoborate (NaDFOB), and sodium fluorosulfonate (NaFSO3).

[0091] As a further solution, the content of the second additive in the electrolyte is 0.1%-1.5%.

[0092] As a further solution, the electrolyte also includes an inorganic electrolyte salt, an organic electrolyte salt and a solvent. Inorganic electrolyte salts are usually composed of inorganic anions and sodium cations. These salts usually have a higher melting point and a lower solubility in organic solvents when in solid state, so sodium batteries using inorganic electrolyte salts are usually more stable at high temperatures. However, inorganic electrolyte salts may react with positive electrode materials or solvents under high temperature and high voltage conditions, resulting in a decrease in the performance of sodium batteries. In contrast, organic electrolyte salts composed of organic anions and sodium cations have good compatibility with organic solvents, and can provide higher conductivity and cation migration number when used as battery electrolytes, but organic electrolyte salt anions cannot form a dense passivation film on the surface of the positive electrode current collector, so it may cause corrosion of the current collector. In order to solve these problems, the present invention combines an organic electrolyte with an inorganic electrolyte, and constructs a composite passivation film on the surface of the positive electrode current collector by using a boron-containing compound A and the manganese element in the positive electrode, ensuring thermal stability while avoiding the corrosion of the organic electrolyte to the positive electrode current collector, thereby significantly improving the performance of the sodium battery.

[0093] As a further embodiment, the inorganic electrolyte salt is selected from borates, phosphates, sulfates, nitrates, antimonates, arsenates, and chlorates.

[0094] As a further embodiment, the inorganic electrolyte salt is substituted with fluorine.

[0095] As yet a further aspect, the inorganic electrolyte salt includes NaPF6.

[0096] As a further solution, the content of NaPF6 in the electrolyte is 1%≤NaPF6≤15%.

[0097] As a further solution, the content of NaPF6 in the electrolyte is 4%≤NaPF6≤11%. When 4%≤NaPF6≤11%, the ionic conductivity of the electrolyte can be further improved, the stability of the high-temperature sodium battery at high temperature can be enhanced, and the battery performance can be improved.

[0098] As a further embodiment, the organic electrolyte salt includes an organic sulfonyl sodium salt.

[0099] As a further embodiment, the organic sulfonyl sodium salt includes an organic sulfonyl sodium salt substituted or halogenated with a halogen element or an organic sulfonyl sodium salt not substituted or halogenated with a halogen element.

[0100] As a further embodiment, the halogen element in the organic sulfonyl sodium salt substituted or halogenated with a halogen element is selected from F.

[0101] As a further embodiment, the organic sulfonyl includes at least one of sulfonimide sodium salt, sulfonic acid sodium salt, sulfonyl chloride sodium salt, sulfonamide sodium salt, sulfonic acid ester sodium salt, sulfonylurea sodium salt, and sulfonamide methyl ester sodium salt.

[0102] As a further embodiment, the organic sulfonyl includes at least one of sodium sulfonimide salt and sodium sulfonate salt.

[0103] As a further embodiment, the sodium sulfonyl imide salt includes at least one of sodium bis(trifluoromethanesulfonyl)imide (NaTFSI), sodium bis(pentafluoroethanesulfonyl)imide, sodium bis(perfluorobutanesulfonyl)imide, sodium bis(perfluorohexanesulfonyl)imide, sodium bis(fluorosulfonyl)imide, and sodium bis(pentafluoroethylsulfonyl)imide.

[0104] As a further embodiment, the sodium sulfonate salt includes at least one of sodium trifluoromethanesulfonate, sodium pentafluoroethanesulfonate, and sodium perfluorooctanesulfonate.

[0105] As a further solution, the content of the organic electrolyte salt in the electrolyte is 5%-10%.

[0106] As a further solution, the solvent includes at least one of a linear carbonate solvent, a carboxylate solvent, and a phosphate solvent.

[0107] As a further embodiment, the linear carbonate solvent includes at least one of dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate and methyl propyl carbonate.

[0108] As a further embodiment, the carboxylic acid ester solvent includes at least one of methyl acetate, ethyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, methyl isobutyrate, ethyl butyrate, methyl trimethylacetate and ethyl trimethylacetate.

[0109] As a further embodiment, the phosphate solvent includes at least one of trimethyl phosphate, triethyl phosphate, tripropyl phosphate, triphenyl phosphate, tris(2,2,2-trifluoroethyl)phosphite and ethoxy(pentafluoro)cyclotriphosphazene.

[0110] The sodium ion battery provided by the present invention also includes a negative electrode and a separator.

[0111] As a further solution, the negative electrode includes a negative electrode material layer and a negative electrode current collector, and the negative electrode material layer is formed on the surface of the negative electrode current collector.

[0112] As a further solution, the negative electrode material layer includes a negative electrode active material, a negative electrode binder, a negative electrode conductor and a thickener.

[0113] As a further solution, the negative electrode active material includes at least one of a carbon-based material, a titanium-based material, an alloy material and an organic compound material.

[0114] As a further aspect, the carbon-based material includes a crystalline carbon-based material and an amorphous carbon-based material.

[0115] As a further solution, the crystalline carbon-based material includes graphite and graphene. Graphite is preferred in the present invention, and when used with a positive electrode sheet of a sodium transition metal oxide positive electrode active material, the sodium ion battery can have high conductivity and structural stability.

[0116] As a further solution, the amorphous carbon-based material includes hard carbon, soft carbon, carbon nanotubes, carbon black and carbon aerogel.

[0117] As a further solution, the type of the negative electrode binder is not limited, and technicians can choose it according to actual needs, including at least one of styrene butadiene rubber (SBR), styrene-butadiene rubber, water-based acrylic resin and carboxymethyl cellulose (CMC).

[0118] As a further solution, the type of the negative electrode conductive agent is not limited, and technicians can choose according to actual needs, including at least one of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphene, conductive carbon black and carbon nanofibers.

[0119] As a further solution, the negative electrode current collector is selected from any one of a metal material capable of conducting electrons, a carbon-coated metal foil or a porous metal plate.

[0120] As a further solution, the metal material capable of conducting electrons used as the negative electrode current collector is a metal foil layer, and the metal of the foil layer includes at least one of aluminum, nickel, tin, copper and stainless steel, preferably copper or aluminum.

[0121] As a further solution, the type of thickener is not limited, and technicians can choose according to actual needs, such as using carboxymethyl cellulose as a thickener.

[0122] As a further solution, the average pore radius distribution range of the negative electrode material layer is 0.01 to 100 μm.

[0123] As a further solution, the present invention does not specifically limit the type of diaphragm, and any known porous structure diaphragm with electrochemical stability and mechanical stability can be selected according to actual needs. For example, it can be a single-layer or multi-layer film containing at least one of glass fiber, non-woven fabric, polyethylene, polypropylene and polyvinylidene fluoride (PVDF).

[0124] As a further solution, the thickness of the separator is 6 to 12 μm.

[0125] The following will be combined with the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0126] The chemical raw materials involved in the following examples and comparative examples are all prior art and are commercially available. The experimental devices, test devices, etc. involved in the following examples and comparative examples are all conventional devices in the art, without special requirements and limitations.

[0127] Example 1

[0128] The present embodiment provides a sodium ion battery, the sodium ion battery comprising a positive electrode, a negative electrode, a separator and a non-aqueous electrolyte; The present embodiment provides a sodium ion battery, the sodium ion battery comprising a positive electrode, a negative electrode, a separator and a non-aqueous electrolyte;

[0129] The positive electrode comprises a positive electrode material layer and a positive electrode current collector aluminum foil containing manganese elements, wherein the positive electrode material layer comprises a positive electrode active material NaCu 1 / 9 Ni 2 / 9 Fe 1 / 3 Mn 1 / 3 O2, conductive carbon black Super-P, binder polyvinylidene fluoride (PVDF) and positive electrode current collector aluminum foil, the average radius distribution range of the positive electrode sheet pores is 6 μm;

[0130] The negative electrode comprises a negative electrode material layer and a negative electrode current collector copper foil, wherein the negative electrode material layer comprises negative electrode active material graphite, conductive carbon black Super-P, binder styrene-butadiene rubber (SBR) and carboxymethyl cellulose (CMC), and the average pore radius distribution range of the negative electrode sheet is 50 μm;

[0131] Preparation of the electrolyte: Ethylene carbonate and ethyl methyl carbonate are mixed in a volume ratio of 1:1, and then an electrolyte salt is added to the mixed non-aqueous organic solvent to a mass concentration as described in the table, and then a sulfur-containing compound SH and a second additive are added to obtain the non-aqueous electrolyte;

[0132] Preparation of positive electrode: Mix NaCu in a mass ratio of 97:1.5:1.5 1 / 9 Ni 2 / 9 Fe 1 / 3 Mn 1 / 3 O2, Super-P and PVDF are then dispersed in N-methyl-2-pyrrolidone (NMP) to obtain a positive electrode slurry; the positive electrode slurry is evenly coated on the surface of a manganese-containing aluminum foil prepared by a mechanical alloying method, and after drying, rolling and vacuum drying, an aluminum lead wire is welded with an ultrasonic welder to obtain a positive electrode sheet;

[0133] Preparation of negative electrode: Graphite, Super-P, SBR and CMC are mixed in a mass ratio of 94:1.5:3:1.5, and then dispersed in deionized water to obtain negative electrode slurry; the negative electrode slurry is coated on both sides of copper foil, and after drying, rolling and vacuum drying, a nickel lead wire is welded with an ultrasonic welder to obtain a negative electrode sheet;

[0134] Preparation of battery cells: a separator with a thickness of 7 μm is placed between the positive electrode sheet and the negative electrode sheet, and then the sandwich structure consisting of the positive electrode sheet, the negative electrode sheet and the separator is wound, and then the wound body is flattened and placed in an aluminum foil packaging bag, and vacuum baked at 75°C for 48 hours to obtain a battery cell to be injected with liquid;

[0135] In a glove box with water and oxygen contents below 20ppm and 50ppm respectively, the prepared electrolyte was injected into the battery cell, and after vacuum packaging, it was left at 45°C for 24h; then the conventional formation of the first charge was carried out according to the following steps: 0.1C constant current charging for 180min, 0.2C constant current charging for 120min, after aging at 45°C for 48h, the battery was vacuum sealed for the second time, and then further charged to 4.0V at a constant current of 0.2C, and discharged to 2V at a constant current of 0.2C.

[0136] The type and content of the above sulfur-containing compound SH, the type and content of the second additive, or \ and, the manganese content in the positive electrode material, the manganese content in the positive electrode current collector, the type and content of the organic electrolyte salt, and the d / (ab+100ac) value are shown in Table 1.

[0137] Example 2-16

[0138] A sodium battery was prepared by changing some parameters in Example 1 and the rest of the parameters were the same as in Example 1. The parameter changes and results are listed in Table 1.

[0139] Comparative Example 1

[0140] A sodium battery was prepared by changing some parameters in Example 1 and the rest of the parameters were the same as in Example 1. The parameter changes and results are listed in Table 2.

[0141] The sodium ion batteries prepared in the embodiments and comparative examples were repeatedly charged at 1C CCCV between 2-4V and then discharged at 1CCC at a high temperature of 45°C for charge-discharge cycle performance testing. The discharge capacity retention rate and impedance growth rate of the battery at high temperature were calculated according to the following formula:

[0142] Capacity retention rate after 1000 cycles at 45℃ = 1000th discharge capacity after 45℃ cycle / first cycle discharge capacity × 100%;

[0143] Impedance growth rate after 1000 cycles at 45℃ = (discharge DCIR after 1000 cycles at 45℃ - discharge DCIR after the first cycle at 45℃) / discharge DCIR after the first cycle at 45℃ × 100%;

[0144] The test results obtained for Examples 1 to 27 and Comparative Examples 1 to 16 are shown in Table 2.

[0145] Table 1

[0146]

[0147]

[0148] Table 2

[0149]

[0150]

[0151] From Examples 1-9 and Comparative Examples 1-8, it can be observed that when the positive electrode of the battery satisfies 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, and 0.5%≤d≤12%, the battery has a capacity retention rate of more than 84% after 1000 cycles at 45°C, and an impedance growth rate of less than 87%. This indicates that the basic performance of the sodium battery can be guaranteed by satisfying 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, and 0.5%≤d≤12%. From Examples 10-11 and Comparative Examples 9-16, it can be seen that when satisfying 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, and 0.5%≤d≤12%, it is also necessary to ensure that 1≤d / (ab+100ac)≤125. When d / (ab+100ac)>125, excessive organic electrolyte salt in the electrolyte may break through the passivation film, corrode the current collector, and reduce the effective contact area between the current collector and the positive electrode active material, thereby increasing the contact resistance; on the other hand, d / (ab+100ac)>125 may also indicate that the content of sulfur-containing compound SH or manganese element in the battery is too low, and the existing content is not enough to cooperate with the sulfur-containing compound SH and the manganese element in the positive electrode material to build a uniform passivation film. From Comparative Examples 13-16, it can be seen that when d / (ab+100ac)>125, the impedance growth rate of 1000 cycles at 45°C exceeds 125%. Compared with d / (ab+100ac)>125, d / (ab+100ac)<1 shows a higher impedance growth rate and a lower capacity retention rate. This may be because the mismatched sulfur-containing compound SH and manganese element are difficult to form a uniform, dense, and moderately thick passivation film on the surface of the positive electrode current collector, resulting in a rapid increase in impedance growth rate. At the same time, d / (ab+100ac)<1 may also mean that the content of organic electrolyte salt in the electrolyte is too low, resulting in too low electrolyte conductivity or poor thermal stability, which in turn leads to increased battery impedance and capacity decay; therefore, calculating d / (ab+100ac) has important practical significance for the design of sodium battery performance.

[0152] According to Examples 1-9 relative to Examples 10 and 11, when 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12% are satisfied, 4≤d / (ab+100ac)≤24 may be preferred.

[0153] According to Example 2, 1%≤a≤3.5%, 12.5%≤b≤25%, 0.03%≤c≤0.09%, 2.5%≤d≤10% can be preferably selected. On the basis of satisfying the above conditions, 4≤d / (ab+100ac)≤24 is further selected according to Example 2, which is helpful to significantly improve the capacity retention rate and reduce the impedance growth rate after 1000 cycles at 45°C. By synergistically optimizing the ion transfer efficiency and the performance of the dense passivation film, the growth rate of the impedance is effectively reduced, thereby enhancing the overall performance of the sodium battery.

[0154] Examples 2, 12-17 show the effects of different sulfur-containing compounds SH on the performance of sodium batteries. It can be observed from Examples 2, 12-17 that compared with sulfur-containing compounds SH (Examples 2, 12, 16) with only a single ring structure (heteroatoms are S and O) in the structure, the capacity retention rate of Examples 13-15 and 17 with at least two ring structures (heteroatoms are S and O) after 1000 cycles at 45°C is significantly better than that of only a single ring structure. At the same time, the impedance growth rate is also better than that of only a single ring structure. This may be because sulfur-containing compounds SH containing two ring structures can provide more active sites, which helps to improve the efficiency and uniformity of electrochemical reactions, reduce the loss of the battery during the charge and discharge process, and thus improve the cycle performance of the battery. In addition, from the comparison of Examples 13-15 and Example 17, it can be seen that the sulfur-containing compound SH in which the heterocyclic rings are connected by bridge bonds can slow down the growth of impedance to a greater extent (<63%) when used as an additive. This may be because the bridge bond structure can often give the molecule a higher thermal stability, which helps to maintain the stability of the molecule during the battery cycle, thereby improving the battery performance.

[0155] Examples 2, 21-25 also compare the capacity retention rate and impedance growth rate of the sodium battery after 1000 cycles at 45°C when the second additive is added. Compared with Example 2, the overall capacity retention rate of the sodium battery with the second additive after 1000 cycles at 45°C is higher than 89%, and the impedance growth rate is lower than 57%. This may be because the second additive containing the O=T structure can effectively assist the manganese element in catalyzing the sulfur-containing compound SH to construct a dense passivation film, and it itself also participates in the construction of the interface film on the electrode surface, so the battery energy is further improved.

[0156] The type of organic electrolyte salt in the electrolyte will also affect the performance of the sodium battery. It can be seen from Examples 2, 18-20 that when the type of organic electrolyte salt in the electrolyte is sulfonimide salt and sulfonate, the sodium battery shows a capacity retention rate of about 88% in 1000 cycles. However, after 1000 cycles at 45°C, the embodiment in which the organic electrolyte salt is sulfonimide salt shows a lower impedance growth rate (<68%). This may be because sulfonimide anions generally have higher chemical stability and are not easy to decompose or react with electrode materials. Therefore, they show a lower impedance growth effect in 1000 cycles at high temperature.

[0157] According to the test results of Example 2 and Examples 26 to 27, the electrolyte of the provided sodium ion battery must also contain an appropriate amount of NaPF6 to ensure that the battery has good cycle performance. According to Example 2, 4%≤NaPF6≤11% can be preferably used to further reduce the impedance growth rate after 1000 cycles at 45°C, thereby improving the battery cycle capacity.

[0158] The technical features of the above-described embodiments can be combined arbitrarily. In order to make the description concise, all possible combinations of the technical features in the above-described embodiments are not described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification. Although the embodiments of the present invention have been shown and described above, it can be understood that the above-described embodiments are exemplary and cannot be understood as limitations of the present invention. Those of ordinary skill in the art can change, modify, replace and deform the above-described embodiments within the scope of the present invention. In addition, those of ordinary skill in the art can combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples without contradiction.

Claims

1. A sodium ion battery, characterized in that: The invention comprises a positive electrode containing manganese element and an electrolyte containing an organic electrolyte salt and an additive, wherein the manganese element in the positive electrode is distributed in the positive electrode active material and the current collector, and the additive comprises a sulfur-containing compound SH having a structure of formula I: wherein R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from C1-C3 halogenated or non-halogenated alkylene, R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 is located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 is located on the ring and directly connected to S. R3 is selected from H, F, C1-C3 halogenated or non-halogenated alkyl; When the sodium ion battery satisfies 1≤d / (ab+100ac)≤125, and 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, and 0.5%≤d≤12%, a is the mass percentage of the compound represented by structural formula I in the electrolyte, b is the mass percentage of the Mn element in the positive electrode material, c is the mass percentage of the Mn element in the positive electrode current collector, and d is the mass percentage of the organic electrolyte salt in the electrolyte.

2. The sodium ion battery according to claim 1, characterized in that The a, b, c, and d also satisfy 0.1%≤a≤5%, 10%≤b≤35%, 0.01%≤c≤0.1%, 0.5%≤d≤12%, and 4≤d / (ab+100ac)≤24; Further preferably, it is characterized in that the sodium ion battery satisfies 1%≤a≤3.5%, 12.5%≤b≤25%, 0.03%≤c≤0.09%, 2.5%≤d≤10%, and 4≤d / (ab+100ac)≤24.

3. The sodium ion battery according to claim 1, characterized in that: The positive electrode comprises a positive electrode material layer and a positive electrode current collector containing manganese elements; Further preferably, it is characterized in that the positive electrode material layer comprises a positive electrode active material containing manganese element, a positive electrode binder and a positive electrode conductive agent; Further preferably, it is characterized in that the positive electrode binder includes at least one of thermoplastic resin, acrylic resin, sodium carboxymethyl cellulose and styrene butadiene rubber; Further preferably, it is characterized in that the positive electrode conductor includes crystalline carbon material and amorphous carbon material.

4. The manganese-containing positive electrode active material according to claim 3, characterized in that: The manganese element-containing positive electrode active material is an O3-phase metal layered oxide containing manganese element, and the general formula of the O3-phase metal layered oxide containing manganese element is Na x Mn y TM z O2, where 0.95 < x ≤ 1.05, 0.01 ≤ y ≤ 0.6, y + z = 1, and TM represents a transition metal element with unfilled d electron orbitals, specifically including one or more of scandium (Sc), yttrium (Y), lanthanide elements (from lanthanum (La) to lutetium (Lu)), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), copper (Cu), technetium (Tc), rhenium (Re), iron (Fe), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), nickel (Ni), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), mercury (Hg); Further preferably, it is characterized in that the positive electrode active material containing manganese element Na x Mn y TM z O2 0.95 <x≤1.05,0.01≤y≤0.55,y+z=1; More preferably, it is characterized in that in the positive electrode active material Na x Mn y TM z O2, 0.95 < x ≤ 1.05, 0.1 ≤ y ≤ 0.5, y + z = 1, and TM includes Ni, Fe, and Cu; Further preferably, it is characterized in that the positive electrode active material of copper element is Na x Cu fa Ni b Fe c Mn y M d O2, where 0.95 < x ≤ 1.05, 0.02 ≤ a ≤ 0.19, 0.2 ≤ b ≤ 0.34, 0.2 ≤ c ≤ 0.4, 0.2 ≤ y ≤ 0.5, 0 ≤ d ≤ 0.2, and a + b + c + d = 1, and M is one or more of scandium (Sc), yttrium (Y), lanthanide elements (from lanthanum (La) to lutetium (Lu)), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), technetium (Tc), rhenium (Re), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), mercury (Hg).

5. The positive electrode current collector containing manganese element according to claim 3 is a metal foil layer containing manganese element; More preferably, it is characterized in that The metal in the metal foil layer containing manganese element can be selected from one or more of aluminum, nickel, tin, copper and stainless steel; Further preferably, it is characterized in that the method of introducing the manganese element into the positive electrode current collector is not limited, and the technicians can choose it according to actual needs, and it can be selected from any one of mechanical alloying method, chemical vapor deposition method, physical vapor deposition (PVD) method, electroplating method, and alloying method.

6. The sodium ion battery according to claim 1, characterized in that: In the structure of formula I of the sulfur-containing compound SH, R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 contains O located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 contains O located on the ring and directly connected to S; R3 is selected from H, F, C1-C3 halogenated or non-halogenated alkyl; Further preferably, it is characterized in that, in the structure of formula I of the sulfur-containing compound SH, R1 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and R2 is selected from R4 is selected from C or O, R5 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R4 and R5 contains O located on the ring and directly connected to S, R6 is selected from C or O, R7 is selected from O, C1-C3 alkylene or oxygen-containing alkylene, and at least one of R6 and R7 contains O located on the ring and directly connected to S; R3 is selected from H, F, C1-C3 halogenated or non-halogenated alkyl; Further preferably, it is characterized in that the sulfur-containing compound SH has the structural formula II: Among them, R8, R 11 Selected from O, R9, R 10 A alkylene group selected from C1-C3.

7. The sodium ion battery according to claim 1, characterized in that: The additive may also include a second additive; Further preferably, it is characterized in that the second additive is selected from at least one of cyclic carbonate compounds or fluorine-containing inorganic salt compounds; Further preferably, the second additive contains an O=T structure, wherein T can be any one of S, P, B and C; Further preferably, it is characterized in that the content of the second additive in the electrolyte is 0.1%-1.5%.

8. The sodium ion battery according to claim 1, characterized in that: The electrolyte solution also includes an inorganic electrolyte salt, an organic electrolyte salt and a solvent; Further preferably, it is characterized in that the inorganic electrolyte salt is selected from borates, phosphates, sulfates, nitrates, antimonates, arsenates, and chlorates; Further preferably, it is characterized in that the inorganic electrolyte salt is substituted with fluorine; Further preferably, it is characterized in that the inorganic electrolyte salt includes NaPF6; Further preferably, it is characterized in that the content of NaPF6 in the electrolyte is 1%≤NaPF6≤15%; Further preferably, it is characterized in that the content of NaPF6 in the electrolyte is 4%≤NaPF6≤11%.

9. The organic electrolyte salt according to claim 8, characterized in that The organic electrolyte salt includes an organic sulfonyl sodium salt; Further preferably, it is characterized in that the organic sulfonyl sodium salt includes an organic sulfonyl sodium salt substituted or halogenated by a halogen element or an organic sulfonyl sodium salt not substituted or halogenated by a halogen element; Further preferably, it is characterized in that the halogen element in the organic sulfonyl sodium salt substituted or halogenated with a halogen element is selected from F; Further preferably, it is characterized in that the organic sulfonyl sodium salt includes at least one of sulfonimide sodium salt, sulfonic acid sodium salt, sulfonyl chloride sodium salt, sulfonamide sodium salt, sulfonic acid ester sodium salt, sulfonylurea sodium salt, and sulfonamide methyl ester sodium salt; Further preferably, it is characterized in that the organic sulfonyl sodium salt comprises at least one of sulfonimide sodium salt and sulfonic acid sodium salt; Further preferably, it is characterized in that the content of the organic electrolyte salt in the electrolyte is 5%-10%.

10. The solvent according to claim 8, characterized in that The solvent includes at least one of a chain carbonate solvent, a carboxylate solvent, and a phosphate solvent.