Isolating membrane and preparation method thereof, secondary battery and electric device
By using an isolation film with ion trapping agent in secondary batteries, the problem of transition metal ion dissolution is solved, the circulation performance and life of the battery are improved, and more stable electrolyte and interface mask are achieved.
Patent Information
- Application Number
- CN202310640959.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-31
- Publication Date
- 2024-12-03
AI Technical Summary
Existing secondary batteries have transition metal ion dissolution problems in the electrochemical environment, resulting in reduced structural stability of the positive electrode material and decomposition of the negative electrode interface mask, affecting battery life and performance.
Using an isolation film containing an ion trapping agent, the reduction potential of the ion trapping agent relative to the lithium metal is 0 to 2V, which can reduce the transition metal ions to a low-valent state or a metal element, reduce the presence of H+, and reduce the active materials with positive and negative electrodes. Direct contact to improve battery circulation performance.
It significantly improves the cycling performance and life of the secondary battery, reduces the migration and catalytic decomposition of transition metal ions, enhances the stability of the electrolyte, and extends the service life of the battery.
Smart Images

Figure CN119069953A_ABST
Abstract
Description
Technical Field The present application relates to the field of battery technology, and in particular to an isolation membrane and a preparation method thereof, a secondary battery and an electrical device. Background Art In recent years, secondary batteries have been widely used in energy storage power systems such as hydropower, thermal power, wind power and solar power stations, as well as power tools, electric bicycles, electric motorcycles, electric vehicles, military equipment, aerospace and other fields due to their high energy density and recyclability. With the great development and wide application of secondary batteries, higher requirements have been put forward for their electrochemical performance. Therefore, how to provide a secondary battery with good performance is a technical problem that needs to be solved urgently. Summary of the invention The present application is made in view of the above-mentioned technical problems, and its purpose is to provide an isolation membrane and a preparation method thereof, a secondary battery and an electrical device, wherein the cycle performance of the secondary battery containing the isolation membrane is improved. In a first aspect, the present application provides an isolation membrane, comprising: a base film; a coating, the coating being disposed on the surface of at least one side of the base film, the coating comprising an ion capture agent, the reduction potential of the ion capture agent relative to lithium metal being 0 to 2 V; and an insulating layer, the insulating layer being disposed on the coating. In the embodiment of the present application, the isolation film includes a base film, a coating disposed on the surface of at least one side of the base film, and an insulating layer disposed on the coating, wherein the coating includes an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2 V. The positive electrode material is an important component of the secondary battery and directly affects the performance of the secondary battery. The positive electrode material containing transition metals will inevitably undergo the phenomenon of transition metal ion dissolution in the electrochemical environment. On the one hand, the dissolved transition metal ions destroy the structural stability of the original positive electrode material and thus affect the life of the secondary battery. On the other hand, the dissolved transition metal ions will migrate and deposit on the surface of the negative electrode material, catalyzing the decomposition and regeneration of the electrolyte and the negative electrode interface film, continuously consuming reversible active metals, and ultimately leading to a decrease in the performance of the secondary battery. In the technical solution of the embodiment of the present application, the reduction potential of the ion capture agent in the isolation membrane relative to lithium metal is 0-2V, while the reduction potential of transition metal ions relative to lithium metal is generally above 2V. Therefore, the ion capture agent can reduce the transition metal ions dissolved in the secondary battery into low-valent ions that are not easily dissolved, or into metal elements, thereby improving the situation where the transition metal ions catalyze the decomposition of the electrolyte and the negative electrode interface film, thereby improving the cycle performance of the secondary battery. In addition, due to H + The reduction potential of ions relative to lithium metal is higher than that of transition metal ions relative to lithium metal, so the ion scavenger can also convert H in the battery cell into +Reduction, that is, removing acidic substances in the electrolyte (such as HF, organic acid RH + , H· free radicals, etc.), further improving the performance of the secondary battery. The coating layer including the ion capture agent is arranged between the base film and the insulating layer. In this way, when the positive electrode sheet, the separator, and the negative electrode sheet are sequentially stacked and wound into an electrode assembly, the possibility of direct contact between the ion capture agent and the positive and negative electrode active materials is reduced, thereby reducing the risk of the ion capture agent losing its redox activity and also reducing the risk of the ion capture agent affecting the performance of the positive and negative electrode active materials. In a possible implementation, the ion capture agent includes at least one of an active metal and an alkali metal compound. Optionally, the active metal includes at least one of Li, Na, K, Rb, Cs, Fr, Mg, Ca, Sr, Ba, Al, Ti or V; Optionally, the active metal includes at least one of Li, Na, Mg, Al, Ti or V; Optionally, the alkali metal compound includes A 1 x B, A 2 y Ti5O 12 , and at least one of the compounds represented by formula (I), formula (II) or formula (III): RA 3 (I) Among them, A 1 , A 2 , A 3 , A 4 , A 5 , A 6 Each independently includes at least one of Li, Na or K, B includes C, Si or Sn, x≥0.05, y>4, R, R1, R2, R3, and R4 independently include a hydrogen atom, an alkyl group having 1 to 20 carbon atoms, an alkyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an alkenyl group having 2 to 20 carbon atoms, an alkenyl group having 2 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an alkenyl group having 6 to 8 carbon atoms, The present invention further comprises at least one of an aryl group having 6 to 26 carbon atoms, an aryl group having 6 to 26 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, a carboxyl group having 1 to 20 carbon atoms, a carboxyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, a carbonyl group having 1 to 20 carbon atoms, a carbonyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an aryloxy group having 6 to 26 carbon atoms, and an aryloxy group having 6 to 26 carbon atoms substituted by a sulfonic acid group or a sulfonyl group. In a possible implementation, the A 1 x B includes Li 1 / 6 C. Na 1 / 6 C.K 1 / 8 C. Li4.4 Si, or Li 4.4 At least one of Sn. In a possible implementation, 5≤y≤7, the A 2 y Ti5O 12 Including Li7Ti5O 12 or Na7Ti5O 12 At least one of . In a possible implementation, the compound represented by formula (I) includes at least one of n-butyl lithium, naphthyl lithium or biphenyl lithium. In a possible implementation, the compound represented by formula (II) comprises At least one of . In a possible implementation, the compound represented by formula (III) comprises At least one of . The ion capture agent in the coating layer can be bonded to the base film through the adhesive, so that there is good bonding force between the ion capture agent and the base film, so as to improve the overall structural strength of the isolation membrane. In a possible implementation, the mass proportion of the ion capture agent in the coating is 50% to 99%. Optionally, the mass proportion of the ion capture agent in the coating is 80% to 98%. The mass proportion of the ion capture agent in the coating is within the given range, and the ion capture agent can play a good role in reducing transition metal ions, thereby further improving the cycle performance of the battery. In a possible implementation, the thickness d1 of the coating is 0.5 μm to 30 μm. Optionally, d1 is 2 μm to 20 μm. If the coating thickness is too small, the content of the ion capture agent in the separator is too small, and the ion capture agent cannot play a good role in reducing the transition metal ions through chemical reactions; if the coating thickness is too large, more pores of the base film will be blocked, resulting in a significant reduction in the migration channels of active metal ions in the separator, thereby significantly increasing the internal resistance of the secondary battery and deteriorating the performance of the secondary battery, for example, affecting the cycle performance of the secondary battery. Therefore, setting the coating thickness to 0.5μm to 30μm is conducive to improving the performance of the secondary battery. In a possible implementation manner, the thickness d2 of the insulating layer is 0.01 μm to 20 μm. Optionally, d2 is 0.1 μm to 10 μm. If the thickness of the insulating layer is too small, it cannot play a good role in isolating the ion capture agent and the electrode active material; if the thickness of the insulating layer is too large, it will hinder the migration of active metal ions in the active material of the electrode plate, deteriorating the performance of the secondary battery, for example, affecting the cycle performance of the secondary battery. Therefore, setting the thickness of the insulating layer to 0.01μm to 20μm is conducive to improving the performance of the secondary battery. In one possible implementation, the base film includes at least one of polyolefins and their derivatives, halogenated polyolefins and their derivatives, polyethers and their derivatives, polyetheretherketones and their derivatives, polyesters and their derivatives, polyimides and their derivatives, and polyvinyl alcohols and their derivatives; optionally, the halogenated polyolefins and their derivatives include at least one of polytetrafluoroethylene and their derivatives, polyvinyl fluoride and their derivatives, and polyvinylidene fluoride and their derivatives; optionally, the polyesters and their derivatives include at least one of polyethylene terephthalate and their derivatives, and polybutylene terephthalate and their derivatives. In one possible implementation, the insulating layer includes at least one of an electronic insulating inorganic substance and an electronic insulating organic substance; optionally, the electronic insulating inorganic substance includes at least one of Al3O2, TiO2, MgO, SiO2, SnO2, CeO2, ZrO2, BaTiO3, Y2O3 or boehmite; optionally, the electronic insulating organic substance includes at least one of polyethylene, polypropylene, cellulose, polyimide, polyethylene oxide, polymethyl methacrylate, polyvinyl chloride, polyacrylonitrile, polyvinylidene fluoride, polypropylene oxide, polyvinylidene chloride or polycarbonate. In one possible implementation, the coating also includes a binder; optionally, the binder includes at least one of polyacrylate, polyacrylic acid, polytetrafluoroethylene, polyvinylidene fluoride, vinylidene fluoride-trichloroethylene copolymer, polyvinyl pyrrolidone, polyvinyl acetate, ethylene-vinyl acetate copolymer, polyethylene oxide, polyarylate, carboxymethyl cellulose, hydroxypropyl cellulose, regenerated cellulose, cellulose acetate, cellulose acetate propionate, cellulose acetate butyrate, polyacrylonitrile, polyvinyl alcohol, polyethylene, polypropylene, starch, or cyanoethyl pullulan. In a possible implementation, the coating further includes a filler; optionally, the filler includes at least one of inorganic particles, organic particles, or an organic-metal framework material; optionally, the inorganic particles include at least one of inorganic particles having a dielectric constant of 5 or more or inorganic particles having ion conductivity but not storing ions; optionally, the organic particles include at least one of polycarbonate, polythiophene, polypyridine, polystyrene, polyacrylic wax, polyethylene, polypropylene, cellulose, cellulose modifier, melamine resin, phenolic resin, polyester, silicone resin, polyimide, polyamideimide, polyaromatic amide, polyphenylene sulfide, polysulfone, polyethersulfone, polyetheretherketone, polyaryletherketone, or a copolymer of butyl acrylate and ethyl methacrylate; optionally, the organic-metal framework material includes at least one of a nitrogen-containing heterocyclic ligand building structure, an organic carboxylic acid ligand building structure, and a nitrogen-oxygen mixed ligand building structure. In a possible implementation manner, the porosity of the base film is 30% to 60%. If the porosity of the base film is too small, there are too few paths for metal ions to migrate through, which inhibits the transmission of metal ions and affects the cycle performance of the secondary battery. If the porosity of the base film is too large, the base film material accounts for a small proportion and cannot play a good role in isolating the positive electrode and the negative electrode. Therefore, setting the porosity of the base film to 30% to 60% is conducive to improving the overall performance of the secondary battery. In the second aspect, a method for preparing an isolation film is provided, comprising: providing a base film; providing a coating slurry, wherein the coating slurry comprises an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2 V, and the coating slurry is coated on the base film to form a coating; providing an insulating slurry, and the insulating slurry is coated on the coating to obtain the isolation film. In a third aspect, a secondary battery is provided, comprising the isolation membrane in the first aspect and any possible implementation thereof. In a fourth aspect, an electrical device is provided, comprising the secondary battery described in the third aspect. The embodiment of the present application provides a separation membrane, which includes a base membrane, a coating disposed on the surface of at least one side of the base membrane, and an insulating layer disposed on the coating, wherein the coating includes an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2 V. The positive electrode material is an important component of the secondary battery and directly affects the performance of the secondary battery. The positive electrode material containing transition metals will inevitably undergo the phenomenon of transition metal ion dissolution in the electrochemical environment. On the one hand, the dissolved transition metal ions destroy the structural stability of the original positive electrode material and thus affect the life of the secondary battery. On the other hand, the dissolved transition metal ions will migrate and deposit on the surface of the negative electrode material, catalyzing the decomposition and regeneration of the electrolyte and the negative electrode interface film, continuously consuming reversible active metals, and ultimately leading to a decrease in the performance of the secondary battery. In the technical solution of the embodiment of the present application, the reduction potential of the ion capture agent in the isolation membrane relative to lithium metal is 0-2V, while the reduction potential of transition metal ions relative to lithium metal is generally above 2V. Therefore, the ion capture agent can reduce the transition metal ions dissolved in the secondary battery into low-valent ions that are not easily dissolved, or into metal elements, thereby improving the situation where the transition metal ions catalyze the decomposition of the electrolyte and the negative electrode interface film, thereby improving the cycle performance of the secondary battery. In addition, due to H + The reduction potential of ions relative to lithium metal is higher than that of transition metal ions relative to lithium metal, so the ion scavenger can also convert H in the battery cell into + Reduction, that is, removing acidic substances in the electrolyte (such as HF, organic acid RH + , H· free radicals, etc.), further improving the performance of the secondary battery. The coating layer including the ion capture agent is arranged between the base film and the insulating layer. In this way, when the positive electrode sheet, the separator, and the negative electrode sheet are sequentially stacked and wound into an electrode assembly, the possibility of direct contact between the ion capture agent and the positive and negative electrode active materials is reduced, thereby reducing the risk of the ion capture agent losing its redox activity and also reducing the risk of the ion capture agent affecting the performance of the positive and negative electrode active materials. BRIEF DESCRIPTION OF THE DRAWINGS In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the drawings without paying creative work. Figure 1 A schematic diagram of an isolation membrane according to an embodiment of the present application; Figure 2 A schematic diagram of an isolation membrane according to an embodiment of the present application; Figure 3 A schematic diagram of a method for preparing an isolation film according to an embodiment of the present application; Figure 4is a schematic diagram of a secondary battery disclosed in one embodiment of the present application; Figure 5 is a schematic diagram of the exploded structure of a secondary battery disclosed in one embodiment of the present application; Figure 6 is a structural schematic diagram of a battery module disclosed in an embodiment of the present application; Figure 7 is a schematic diagram of the exploded structure of a battery pack disclosed in one embodiment of the present application; Figure 8 It is a schematic diagram of an electrical device disclosed in one embodiment of the present application. In the drawings, the drawings are not drawn to scale. DETAILED DESCRIPTION Hereinafter, the embodiments of the isolation membrane and its preparation method, battery cell, battery and electrical device of the present application are specifically disclosed in detail with appropriate reference to the accompanying drawings. However, there may be cases where unnecessary detailed descriptions are omitted. For example, there are cases where detailed descriptions of well-known matters and repeated descriptions of actually the same structures are omitted. This is to avoid the following description from becoming unnecessarily lengthy and to facilitate the understanding of those skilled in the art. In addition, the drawings and the following descriptions are provided for those skilled in the art to fully understand the present application and are not intended to limit the subject matter described in the claims. In the description of this application, it should be noted that, unless otherwise specified, "multiple" means more than two; the terms "upper", "lower", "left", "right", "inner", "outer", etc., indicating directions or positional relationships, are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting this application. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance. "Scope" disclosed in the present application is limited in the form of lower limit and upper limit, and a given range is limited by selecting a lower limit and an upper limit, and the selected lower limit and upper limit define the boundary of a special range. The scope limited in this way can be including end values or not including end values, and can be arbitrarily combined, that is, any lower limit can be combined with any upper limit to form a scope. For example, if the scope of 60-120 and 80-110 is listed for a specific parameter, it is understood that the scope of 60-110 and 80-120 is also expected. In addition, if the minimum range values 1 and 2 are listed, and if the maximum range values 3, 4 and 5 are listed, the following scope can be all expected: 1-3, 1-4, 1-5, 2-3, 2-4 and 2-5. In the present application, unless otherwise specified, the numerical range "ab" represents the abbreviation of any real number combination between a and b, wherein a and b are real numbers. For example, the numerical range "0-5" means that all real numbers between "0-5" are listed in this document, and "0-5" is just an abbreviation of these numerical combinations. In addition, when a parameter is expressed as an integer ≥ 2, it is equivalent to disclosing that the parameter is, for example, an integer of 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, etc. If there is no special explanation, all steps of the present application can be performed sequentially or randomly, preferably sequentially. For example, the method includes steps (a) and (b), which means that the method may include steps (a) and (b) performed sequentially, or may include steps (b) and (a) performed sequentially. For example, the method may further include step (c), which means that step (c) may be added to the method in any order. For example, the method may include steps (a), (b) and (c), or may include steps (a), (c) and (b), or may include steps (c), (a) and (b), etc. If there is no special explanation, the "include" and "comprising" mentioned in this application represent open-ended. For example, the "include" and "comprising" may mean including or comprising other components not listed. If not specifically stated, in this application, the term "and / or" is inclusive. For example, the phrase "A and / or B" means "A, B, or both A and B". More specifically, any of the following conditions satisfies the condition "A and / or B": A is true (or exists) and B is false (or does not exist); A is false (or does not exist) and B is true (or exists); or both A and B are true (or exist). Unless otherwise specified, all embodiments and optional embodiments of the present application can be combined with each other to form a new technical solution. Unless otherwise specified, all technical features and optional technical features of this application can be combined with each other to form a new technical solution. Unless otherwise specified, the following terms have the following meanings. Any undefined terms have their generally accepted meanings in the art. "Alkyl" refers to a monovalent saturated hydrocarbon group having one or more carbon atoms, optionally with a carbon number of 1 to 20. For example, alkyl includes straight chain hydrocarbon groups and branched hydrocarbon groups, such as methyl (CH3-), ethyl (CH3CH2-), n-propyl (CH3CH2CH2-), isopropyl ((CH3)2CH-), n-butyl (CH3CH2CH2CH2-), isobutyl ((CH3)2CHCH2-), sec-butyl ((CH3)(CH3CH2)CH-), tert-butyl ((CH3)3C-), n-pentyl (CH3CH2CH2CH2CH2-), neopentyl ((CH3)3CCH2-), etc. "Alkenyl" refers to a straight or branched hydrocarbon group having one or more carbon atoms and at least one double bond unsaturated site, optionally with 2 to 20 carbon atoms, such as vinyl (CH2=CH-), propenyl (CH3CH=CH-), allyl (CH2=CH-CH2-), n-butenyl (-CH3CH2CH=CH-), etc. "Aryl" refers to an aromatic compound having a single ring or multiple condensed rings, optionally with 6 to 26 carbon atoms. For example, aryl includes phenyl, naphthyl, indenyl, etc. Aryl also includes a single ring fused to an aryl, for example, tetrahydronaphthyl, 2,3-dihydroindanyl, etc. "Carboxyl" refers to a group having one or more carbon atoms and having a -CO2H functional group, and optionally, the number of carbon atoms is 1 to 20. "Carbonyl" refers to a group having one or more carbon atoms and having a -CO- functional group, and optionally, the number of carbon atoms is 1 to 20. "Aryloxy" refers to a group formed by connecting at least one carbon atom on the aromatic ring of an aryl group to an oxygen atom, and optionally, the number of carbon atoms is 6 to 26. "Sulfonic acid" refers to -SO3H. "Sulfonyl" refers to RS(=O)2-, wherein R includes hydrogen atom, alkyl, alkenyl, alkynyl, aryl, cycloalkyl, cycloalkenyl, heteroaryl, heterocyclic group and the like. A secondary battery is a battery that can be used again after being discharged by recharging the active materials. Usually, a secondary battery includes a positive electrode, a negative electrode, a separator and an electrolyte. During the battery charging and discharging process, active ions are embedded and released back and forth between the positive electrode and the negative electrode. The separator is set between the positive electrode and the negative electrode to play an isolating role. The electrolyte plays the role of conducting ions between the positive electrode and the negative electrode. Due to their high energy density and recyclability, secondary batteries are widely used in energy storage power systems such as hydropower, thermal power, wind power and solar power stations, as well as power tools, electric bicycles, electric motorcycles, electric vehicles, military equipment, aerospace and other fields. With the great development and wide application of secondary batteries, higher requirements are also put forward for their energy density, cycle performance, discharge capacity and other performance. Positive electrode materials are one of the key materials that determine the performance of secondary batteries, mainly including metal oxides and polyanion salts, among which layered metal oxides and spinel metal oxides containing transition metals are widely used as positive electrode materials. The above-mentioned positive electrode materials containing transition metals have the advantages of high energy density and good cycle performance, which are beneficial to improving the performance of secondary batteries. However, transition metal ions will inevitably dissolve in the electrochemical environment of positive electrode materials containing transition metals. On the one hand, the dissolved transition metal ions destroy the structural stability of the original positive electrode materials and thus affect the life of the secondary battery. On the other hand, the dissolved transition metal ions will migrate and deposit on the surface of the negative electrode material, catalyzing the decomposition and regeneration of the electrolyte and the negative electrode interface film, continuously consuming reversible active metals, and ultimately leading to a decline in the performance of the secondary battery. In view of this, an embodiment of the present application provides an isolation membrane, which includes a base membrane and a coating disposed on the surface of at least one side of the base membrane, wherein the coating includes an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2V, while the reduction potential of transition metal ions relative to lithium metal is generally above 2V, so the ion capture agent can reduce the transition metal ions dissolved in the secondary battery into low-valent ions that are not easily dissolved, or into metal elements, thereby improving the situation where the transition metal ions catalyze the decomposition of the electrolyte and the negative electrode interface film, thereby improving the cycle performance of the secondary battery. In addition, due to H + The reduction potential of ions relative to lithium metal is higher than that of transition metal ions relative to lithium metal, so the ion scavenger can also convert H in the battery cell into + Reduction, that is, removing acidic substances in the electrolyte (such as HF, organic acid RH + , H· free radicals, etc.), further improving the performance of secondary batteries. [Isolation film] Figure 1 FIG. 1 is a schematic diagram of an isolation membrane according to an embodiment of the present application. Figure 1 As shown, the isolation film 1 includes a base film 12, a coating 11 and an insulating layer 13. The coating 11 is disposed on at least one side of the base film 12, and the insulating layer 13 is disposed on the coating 11. For example, along the thickness direction of the isolation film 1 (eg Figure 1 The base film 12, the coating layer 11 and the insulating layer 13 are sequentially arranged. The coating layer 11 includes an ion trapping agent, and the reduction potential of the ion trapping agent relative to lithium metal is 0 to 2V. The ion capture agent mentioned here refers to a class of substances that can consume free transition metal ions in secondary batteries. The reduction potential of the ion capture agent relative to lithium metal is 0 to 2V, while the reduction potential of transition metal ions relative to lithium metal is generally above 2V. Therefore, the reducibility of the ion capture agent is stronger than that of the transition metal ions. The ion capture agent can reduce the free transition metal ions into low-valent ions that are not easily dissolved from the positive electrode material, or reduce them into metal elements. The positive electrode material is an important component of the secondary battery and directly affects the performance of the secondary battery. The positive electrode material containing transition metals will inevitably undergo the phenomenon of transition metal ion dissolution in the electrochemical environment. On the one hand, the dissolved transition metal ions destroy the structural stability of the original positive electrode material and thus affect the life of the secondary battery. On the other hand, the dissolved transition metal ions will migrate and deposit on the surface of the negative electrode material, catalyzing the decomposition and regeneration of the electrolyte and the negative electrode interface film, continuously consuming reversible active metals, and ultimately leading to a decline in the performance of the secondary battery. For example, the positive electrode material may include a phosphate material with an olivine structure, a material with a spinel structure, and a transition metal oxide with a layered structure. Specifically, for example, lithium iron phosphate (LiFePO4), lithium iron manganese phosphate (LiMnFePO4), lithium manganate (LiMn2O4), ternary materials, etc. The iron ions, nickel ions, manganese ions, etc. in the above positive electrode materials all have the phenomenon of dissolving from the positive electrode materials. The coating 11 of the isolation membrane 1 provided in the embodiment of the present application includes an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2V, while the reduction potential of transition metal ions relative to lithium metal is generally above 2V. Therefore, the ion capture agent can reduce the transition metal ions dissolved in the secondary battery into low-valent ions that are not easily dissolved, or into metal elements, thereby improving the situation where the transition metal ions catalyze the decomposition of the electrolyte and the negative electrode interface film, thereby improving the cycle performance of the secondary battery. In addition, due to H + The reduction potential of ions relative to lithium metal is higher than that of transition metal ions relative to lithium metal, so the ion scavenger can also convert H in the battery cell into + Reduction, that is, removing acidic substances in the electrolyte (such as HF, organic acid RH + , H· free radicals, etc.), further improving the performance of the secondary battery. The coating 11 including the ion capture agent is arranged between the base film 12 and the insulating layer 13. In this way, when the positive electrode sheet, the separator, and the negative electrode sheet are sequentially stacked and wound into an electrode assembly, the possibility of direct contact between the ion capture agent and the positive and negative electrode active materials is reduced, thereby reducing the risk of the ion capture agent losing its redox activity and also reducing the risk of the ion capture agent affecting the performance of the positive and negative electrode active materials. It should be understood that in the embodiments of the present application, different types of ion capture agents can be selected according to different types of free transition metal ions dissolved in the secondary battery. Optionally, in some embodiments, the ion capture agent includes at least one of a compound of an active metal and an alkali metal. Specifically, the active metal may include at least one of Li, Na, K, Rb, Cs, Fr, Mg, Ca, Sr, Ba, Al, Ti or V. Optionally, the active metal includes at least one of Li, Na, Mg, Al, Ti or V. Optionally, the alkali metal compound comprises A 1 x B, A 2 y Ti5O 12 , and at least one of the compounds represented by formula (I), formula (II) or formula (III): RA 3 (I) Among them, A 1 , A 2 , A 3 , A 4 , A 5 , A 6 Each independently includes at least one of Li, Na or K, B includes C, Si or Sn, x≥0.05, y>4, R, R1, R2, R3, and R4 independently include a hydrogen atom, an alkyl group having 1 to 20 carbon atoms, an alkyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an alkenyl group having 2 to 20 carbon atoms, an alkenyl group having 2 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an alkenyl group having 6 to 8 carbon atoms, The present invention further comprises at least one of an aryl group having 6 to 26 carbon atoms, an aryl group having 6 to 26 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, a carboxyl group having 1 to 20 carbon atoms, a carboxyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, a carbonyl group having 1 to 20 carbon atoms, a carbonyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an aryloxy group having 6 to 26 carbon atoms, and an aryloxy group having 6 to 26 carbon atoms substituted by a sulfonic acid group or a sulfonyl group. In the embodiments of the present application, the dotted line in formula (II) indicates that R1 and R2 may be connected to form a ring or may not be connected; the dotted line in formula (III) indicates that R3 and R4 may be connected to form a ring or may not be connected. Optionally, A 1 x B includes LiC6, NaC6, KC8, Li 4.4 Si、Li 4.4 Sn or Li 22 At least one of Si5. In the present application embodiment, A 1 x The value of x in B is related to the specific substance selected for B. For example, when B is carbon (C), the upper limit of the value of x is 1 / 6; for another example, when B is silicon (Si) or tin (Sn), the upper limit of the value of x is 4.4. Optionally, 5≤y≤7, A 2 y Ti5O 12 Including Li7Ti5O 12 or Na7Ti5O 12 At least one of . Optionally, the compound represented by formula (I) includes at least one of n-butyllithium, naphthyllithium or biphenyllithium. Optionally, the compound represented by formula (II) comprises At least one of . Optionally, the compound represented by formula (III) comprises At least one of . The base film 12 has two surfaces arranged along its thickness direction. Figure 1 As shown, both surfaces of the base film 12 are provided with coating layers 11 , and the surfaces of the coating layers 11 on both sides of the base film 12 away from the base film 12 are provided with insulating layers 13 . Figure 2 Schematic diagram of an isolation membrane according to an embodiment of the present application. In some other embodiments, such as Figure 2 As shown, one of the two surfaces of the base film 12 that are opposite to each other in the thickness direction is provided with a coating 11 , and an insulating layer 13 is provided on the coating 11 , that is, the coating 11 and the insulating layer 13 are provided on the same side of the base film 12 . Optionally, in some embodiments, the mass proportion of the ion capture agent in the coating 11 is 50% to 99%. Optionally, the mass proportion of the ion capture agent in the coating 11 is 80% to 98%. Specifically, the mass proportion of the ion capture agent in the coating 11 can be 50%, 60%, 70%, 80%, 90%, 96%, 98%, 99%, or a value between any two of the above values. The mass proportion of the ion capture agent in the coating 11 is within the given range, and the ion capture agent can play a good role in reducing transition metal ions, thereby further improving the cycle performance of the battery. Optionally, in some embodiments, Figure 1 and Figure 2 As shown, the thickness d1 of the coating 11 is 0.5 μm to 30 μm, and optionally, d1 is 2 μm to 20 μm. Specifically, the thickness d1 of the coating 11 may be 0.5 μm, 1 μm, 2 μm, 5 μm, 10 μm, 15 μm, 20 μm, 25 μm, 30 μm, or a value between any two of the above values. If the thickness of the coating 11 is too small, the content of the ion capture agent in the separator 1 is too small, and the ion capture agent cannot play a good role in reducing the transition metal ions through chemical reactions; if the thickness of the coating 11 is too large, more pores of the base film 12 will be blocked, resulting in a significant reduction in the migration channels of the active metal ions in the separator 1, which will significantly increase the internal resistance of the secondary battery and deteriorate the performance of the secondary battery, for example, affecting the cycle performance of the secondary battery. Therefore, setting the thickness of the coating 11 to 0.5μm to 30μm is conducive to improving the performance of the secondary battery. Optionally, in some embodiments, Figure 1 and Figure 2 As shown, the thickness d2 of the insulating layer 13 is 0.01 μm to 20 μm, and optionally, d2 is 0.1 μm to 10 μm. Specifically, the thickness d2 of the insulating layer 13 may be 0.01 μm, 0.1 μm, 1 μm, 5 μm, 10 μm, 15 μm, 20 μm, or a value between any two of the above values. If the thickness of the insulating layer 13 is too small, it cannot play a good role in isolating the ion capture agent and the electrode active material; if the thickness of the insulating layer is too large, it will hinder the migration of active metal ions in the active material of the electrode plate, deteriorating the performance of the secondary battery, for example, affecting the cycle performance of the secondary battery. Therefore, setting the thickness of the insulating layer 13 to 0.01μm to 20μm is conducive to improving the performance of the secondary battery. As mentioned above, the thickness of the material can be measured by a micrometer. The thickness of the material at multiple different positions is measured using the micrometer, and the average value of the multiple measurement results is recorded as the final thickness. The material thickness in the embodiment of the present application can be measured by the above method, but is not limited to the above method. For example, it can also be measured by spectroscopy. The specific detection method can refer to the well-known method of measuring thickness by spectroscopy. Optionally, in some embodiments, the base film includes at least one of polyolefins and their derivatives, halogenated polyolefins and their derivatives, polyethers and their derivatives, polyetheretherketones and their derivatives, polyesters and their derivatives, polyimides and their derivatives, and polyvinyl alcohols and their derivatives; optionally, the halogenated polyolefins and their derivatives include at least one of polytetrafluoroethylene and their derivatives, polyvinyl fluoride and their derivatives, and polyvinylidene fluoride and their derivatives; optionally, the polyesters and their derivatives include at least one of polyethylene terephthalate and their derivatives, and polybutylene terephthalate and their derivatives. Optionally, in some embodiments, the insulating layer includes at least one of an electronic insulating inorganic substance and an electronic insulating organic substance. Optionally, the electronically insulating inorganic substance includes at least one of Al3O2, TiO2, MgO, SiO2, SnO2, CeO2, ZrO2, BaTiO3, Y2O3 or boehmite. Optionally, the electronically insulating organic material includes at least one of polyethylene, polypropylene, cellulose, polyimide, polyethylene oxide, polymethyl methacrylate, polyvinyl chloride, polyacrylonitrile, polyvinylidene fluoride, polypropylene oxide, polyvinylidene chloride or polycarbonate. Optionally, in some embodiments, the coating 11 further includes a binder. Optionally, the binder includes at least one of polyacrylate, polyacrylic acid, polytetrafluoroethylene, polyvinylidene fluoride, vinylidene fluoride-trichloroethylene copolymer, polyvinyl pyrrolidone, polyvinyl acetate, ethylene-vinyl acetate copolymer, polyethylene oxide, polyarylate, carboxymethyl cellulose, hydroxypropyl cellulose, regenerated cellulose, cellulose acetate, cellulose acetate propionate, cellulose acetate butyrate, polyacrylonitrile, polyvinyl alcohol, polyethylene, polypropylene, starch, or cyanoethyl pullulan. Optionally, in some embodiments, the coating 11 further includes a filler. Optionally, the filler includes at least one of inorganic particles, organic particles, or organic-metal framework materials; optionally, the inorganic particles include at least one of inorganic particles having a dielectric constant of 5 or more or inorganic particles having ion conductivity but not storing ions. Optionally, the organic particles include at least one of polycarbonate, polythiophene, polypyridine, polystyrene, polyacrylic wax, polyethylene, polypropylene, cellulose, cellulose modifier, melamine resin, phenolic resin, polyester, silicone resin, polyimide, polyamideimide, polyaramid, polyphenylene sulfide, polysulfone, polyethersulfone, polyetheretherketone, polyaryletherketone, or a copolymer of butyl acrylate and ethyl methacrylate. Optionally, the organic-metal framework material includes at least one of a nitrogen-containing heterocyclic ligand building structure, an organic carboxylic acid ligand building structure, and a nitrogen-oxygen mixed ligand building structure. Optionally, in some embodiments, the porosity of the base film is 30% to 60%. Porosity refers to the percentage of the pore volume in a material to the total volume of the material in its natural state. The porosity of the base film can be calculated by using an empty weight method, an air permeation method, a pressure method, etc. The specific detection steps of the above test methods can refer to the known test steps for the porosity of materials. Specifically, the porosity of the base film may be 30%, 35%, 40%, 45%, 50%, 55%, 60%, or a value between any two of the above values. If the porosity of the base film is too small, there are too few paths for metal ions to migrate through, which inhibits the transmission of metal ions and affects the cycle performance of the secondary battery. If the porosity of the base film is too large, the base film material accounts for a small proportion and cannot play a good role in isolating the positive electrode and the negative electrode. Therefore, setting the porosity of the base film to 30% to 60% is conducive to improving the overall performance of the secondary battery. [Method for preparing isolation film] Figure 3 This is a method for preparing an isolation film according to an embodiment of the present application. Figure 3 As shown, the method 300 includes the following steps. Step 310, providing a base film; Step 320, providing a coating slurry, and applying the coating slurry on the base film to form a coating; The coating layer includes an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2V. Step 330 , providing an insulating slurry, and coating the insulating slurry on the coating to obtain an isolation film. The separator prepared by the above method can improve the cycle performance of the secondary battery when applied to the secondary battery. [Positive electrode] The positive electrode sheet includes a positive electrode current collector and a positive electrode film layer arranged on at least one surface of the positive electrode current collector, and the positive electrode film layer includes a positive electrode active material. As an example, the positive electrode current collector has two surfaces opposite to each other in its thickness direction, and the positive electrode film layer is disposed on any one or both of the two opposite surfaces of the positive electrode current collector. In some embodiments, the positive electrode current collector may be a metal foil or a composite current collector. For example, aluminum foil may be used as the metal foil. The composite current collector may include a polymer material base and a metal layer formed on at least one surface of the polymer material base. The composite current collector may be formed by forming a metal material (aluminum, aluminum alloy, nickel, nickel alloy, titanium, titanium alloy, silver and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene (PP), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polystyrene (PS), polyethylene (PE), etc.). In some embodiments, the positive electrode active material may adopt the positive electrode active material for lithium ion batteries known in the art. As an example, the positive electrode active material may include at least one of the following materials: lithium phosphates containing olivine structure, lithium transition metal oxides and their respective modified compounds. However, the present application is not limited to these materials, and other traditional materials that can be used as positive electrode active materials for lithium ion batteries can also be used. These positive electrode active materials can be used alone or in combination of two or more. Among them, examples of lithium transition metal oxides may include, but are not limited to, lithium cobalt oxide (such as LiCoO2), lithium nickel oxide (such as LiNiO2), lithium manganese oxide (such as LiMnO2, LiMn2O4), lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide (such as LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2 (also referred to as NCM333), LiNi 0.5 Co 0.2 Mn 0.3 O2 (also referred to as NCM523), LiNi 0.5 Co 0.25 Mn 0.25 O2 (also referred to as NCM211), LiNi 0.6 Co 0.2 Mn 0.2 O2 (also referred to as NCM622), LiNi 0.8 Co 0.1 Mn 0.1 O2 (also referred to as NCM811), lithium nickel cobalt aluminum oxide (such as LiNi 0.85 Co 0.15 Al 0.05 O2) and its modified compounds, etc. Examples of lithium-containing phosphates with an olivine structure may include, but are not limited to, at least one of lithium iron phosphate (such as LiFePO4 (also referred to as LFP)), a composite material of lithium iron phosphate and carbon, lithium manganese phosphate (such as LiMnPO4), a composite material of lithium manganese phosphate and carbon, lithium iron manganese phosphate, and a composite material of lithium iron manganese phosphate and carbon. In some embodiments, the positive electrode film layer may also optionally include a binder. As an example, the binder may include at least one of polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), vinylidene fluoride-tetrafluoroethylene-propylene terpolymer, vinylidene fluoride-hexafluoropropylene-tetrafluoroethylene terpolymer, tetrafluoroethylene-hexafluoropropylene copolymer, and fluorine-containing acrylate resin. In some embodiments, the positive electrode film layer may further include a conductive agent, for example, the conductive agent may include at least one of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphene and carbon nanofibers. In some embodiments, the positive electrode sheet can be prepared in the following manner: the components for preparing the positive electrode sheet, such as the positive electrode active material, the conductive agent, the binder and any other components are dispersed in a solvent (such as N-methylpyrrolidone) to form a positive electrode slurry; the positive electrode slurry is coated on the positive electrode collector, and after drying, cold pressing and other processes, the positive electrode sheet can be obtained. [Negative electrode] The negative electrode sheet includes a negative electrode current collector and a negative electrode film layer disposed on at least one surface of the negative electrode current collector, wherein the negative electrode film layer includes a negative electrode active material. As an example, the negative electrode current collector has two surfaces opposite to each other in its thickness direction, and the negative electrode film layer is disposed on any one or both of the two opposite surfaces of the negative electrode current collector. In some embodiments, the negative electrode current collector may be a metal foil or a composite current collector. For example, as the metal foil, copper foil may be used. The composite current collector may include a polymer material base layer and a metal layer formed on at least one surface of the polymer material substrate. The composite current collector may be formed by forming a metal material (copper, copper alloy, nickel, nickel alloy, titanium, titanium alloy, silver and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene (PP), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polystyrene (PS), polyethylene (PE), etc.). In some embodiments, the negative electrode active material may adopt the negative electrode active material for the battery known in the art. As an example, the negative electrode active material may include at least one of the following materials: artificial graphite, natural graphite, soft carbon, hard carbon, silicon-based materials, tin-based materials, lithium titanate, etc. The silicon-based material may be selected from at least one of elemental silicon, silicon oxide compounds, silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. The tin-based material may be selected from at least one of elemental tin, tin oxide compounds, and tin alloys. However, the present application is not limited to these materials, and other traditional materials that can be used as negative electrode active materials for batteries may also be used. These negative electrode active materials may be used alone or in combination of two or more. In some embodiments, the negative electrode film layer may further include a binder. The binder may be selected from at least one of styrene-butadiene rubber (SBR), polyacrylic acid (PAA), sodium polyacrylate (PAAS), polyacrylamide (PAM), polyvinyl alcohol (PVA), sodium alginate (SA), polymethacrylic acid (PMAA) and carboxymethyl chitosan (CMCS). In some embodiments, the negative electrode film layer may further include a conductive agent, which may be selected from at least one of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphene and carbon nanofibers. In some embodiments, the negative electrode film layer may optionally include other additives, such as a thickener (eg, sodium carboxymethyl cellulose (CMC-Na)). In some embodiments, the negative electrode sheet can be prepared in the following manner: the components for preparing the negative electrode sheet, such as the negative electrode active material, the conductive agent, the binder and any other components are dispersed in a solvent (such as deionized water) to form a negative electrode slurry; the negative electrode slurry is coated on the negative electrode collector, and after drying, cold pressing and other processes, the negative electrode sheet can be obtained. [Electrolytes] The electrolyte plays the role of conducting ions between the positive electrode and the negative electrode. The present application has no specific restrictions on the type of electrolyte, which can be selected according to needs. For example, the electrolyte can be liquid, gel or all-solid. In some embodiments, the electrolyte is an electrolyte solution, which includes an electrolyte salt and a solvent. In some embodiments, the electrolyte salt can be selected from at least one of lithium hexafluorophosphate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluoroarsenate, lithium bis(fluorosulfonyl)imide, lithium bis(trifluoromethanesulfonyl)imide, lithium trifluoromethanesulfonate, lithium difluorophosphate, lithium difluorooxalatoborate, lithium dioxalatoborate, lithium difluorodioxalatophosphate, and lithium tetrafluorooxalatophosphate. In some embodiments, the solvent can be selected from at least one of ethylene carbonate, propylene carbonate, ethyl methyl carbonate, diethyl carbonate, dimethyl carbonate, dipropyl carbonate, methyl propyl carbonate, ethyl propyl carbonate, butylene carbonate, fluoroethylene carbonate, methyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, 1,4-butyrolactone, cyclopentane sulfone, dimethyl sulfone, methyl ethyl sulfone and diethyl sulfone. In some embodiments, the electrolyte may further include additives, such as negative electrode film-forming additives, positive electrode film-forming additives, and additives that can improve certain battery properties, such as additives that improve battery overcharge performance, additives that improve battery high or low temperature performance, etc. In some embodiments, the positive electrode sheet, the negative electrode sheet, and the separator may be formed into an electrode assembly by a winding process or a lamination process. In some embodiments, the secondary battery may include an outer package, which may be used to encapsulate the electrode assembly and the electrolyte. In some embodiments, the outer packaging of the secondary battery may be a hard shell, such as a hard plastic shell, an aluminum shell, a steel shell, etc. The outer packaging of the battery cell may also be a soft package, such as a bag-type soft package. The material of the soft package may be plastic, and examples of the plastic include polypropylene, polybutylene terephthalate, and polybutylene succinate. The present application has no particular limitation on the shape of the secondary battery, which may be cylindrical, square or any other shape. Figure 4 The secondary battery 20 is a square structure as an example. In some embodiments, reference Figure 5 , the outer packaging may include a shell 21 and a cover plate 23. Among them, the shell 21 may include a bottom plate and a side plate connected to the bottom plate, and the bottom plate and the side plate enclose a receiving cavity. The shell 21 has an opening connected to the receiving cavity, and the cover plate 23 can be covered on the opening to close the receiving cavity. The positive electrode sheet, the negative electrode sheet and the isolation membrane can form an electrode assembly 22 through a winding process or a lamination process. The electrode assembly 22 is encapsulated in the receiving cavity. The electrolyte is infiltrated in the electrode assembly 22. The number of electrode assemblies 22 contained in the secondary battery 20 can be one or more, and those skilled in the art can select according to specific actual needs. Figure 6 40 is an example of a battery module. Figure 6 In the battery module 40, a plurality of secondary batteries 20 may be included. The plurality of secondary batteries 20 may be arranged in sequence along the length direction of the battery module 40. Of course, they may also be arranged in any other manner. Further, the plurality of secondary batteries 20 may be fixed by fasteners. The battery module 40 may further include a housing having an accommodation space in which the plurality of secondary batteries 20 are accommodated. In some embodiments, the battery modules described above may also be assembled into a battery pack, and the number of battery modules contained in the battery pack may be adjusted according to the application and capacity of the battery pack. Figure 7 50 is an example of a battery pack. Figure 7 The battery pack 50 may include a box body 51, the inside of the box body 51 is a hollow structure, and a plurality of battery modules 40 are accommodated in the box body 51. The plurality of battery modules 40 may be arranged in the box body 51 in any manner. In addition, the present application also provides an electrical device, which includes at least one of the secondary battery, battery module or battery pack provided in the present application. The secondary battery, battery module or battery pack can be used as a power source for the electrical device, and can also be used as an energy storage unit for the electrical device. The electrical device may include mobile devices (such as mobile phones, laptops, etc.), electric vehicles (such as pure electric vehicles, hybrid electric vehicles, plug-in hybrid electric vehicles, electric bicycles, electric scooters, electric golf carts, electric trucks, etc.), electric trains, ships and satellites, energy storage systems, etc., but are not limited to these. As the electrical device, a secondary battery, a battery module or a battery pack may be selected according to its usage requirements. Figure 8 The power consumption device is taken as an example. The power consumption device is a pure electric vehicle, a hybrid electric vehicle, or a plug-in hybrid electric vehicle. In order to meet the high power and high energy density requirements of the power consumption device for battery cells, batteries or battery modules can be used. As another example, the device may be a mobile phone, a tablet computer, a notebook computer, etc. The device is usually required to be light and thin, and a battery cell may be used as a power source. [Example] Hereinafter, the embodiments of the present application will be described. The embodiments described below are exemplary and are only used to explain the present application, and should not be construed as limiting the present application. If no specific techniques or conditions are indicated in the embodiments, the techniques or conditions described in the literature in this area or the product specifications are used. If the manufacturer is not indicated in the reagents or instruments used, they are all conventional products that can be obtained commercially. 1. Preparation of isolation film Isolation film 1: A base film is provided, wherein the material includes polyethylene (PE) and the thickness is 7 μm. Provide coating slurry: add ion capture agent Li7Ti5O 12 , the binder polyvinylidene fluoride (PVDF) is fully stirred and mixed in an N-methylpyrrolidone solvent system in a mass ratio of 90%:10% to form a coating slurry, which is applied on the above-mentioned PE base film to form a coating, wherein the coating has a thickness of 5 μm. Providing insulating slurry: dissolving Al2O3 ceramic particles and binder styrene polybutadiene rubber in a solvent NMP at a mass ratio of 90%:10%, stirring and mixing thoroughly to form an insulating slurry, applying it on the surface of the above coating to form an insulating layer, and then drying to obtain an isolation film 1, wherein the thickness of the insulating layer is 2μm. Isolation membrane 2: The preparation of isolation membrane 2 is similar to that of isolation membrane 1, except that the coating thickness in isolation membrane 2 is 0.5 μm. Separator 3: Separator 3 is prepared similarly to separator 1, except that the coating thickness in separator 3 is 2 μm. Separator 4: Separator 4 is prepared similarly to separator 1, except that the coating thickness in separator 4 is 20 μm. Separator 5: Separator 5 is prepared similarly to separator 1, except that the coating thickness in separator 5 is 30 μm. Isolation film 6: The preparation of isolation film 6 is similar to that of isolation film 1, except that the thickness of the insulating layer in isolation film 6 is 0.01 μm. Isolation film 7: The preparation of isolation film 7 is similar to that of isolation film 1, except that the thickness of the insulating layer in isolation film 7 is 0.1 μm. Isolation film 8: The preparation of isolation film 8 is similar to that of isolation film 1, except that the thickness of the insulating layer in isolation film 8 is 10 μm. Isolation film 9: The preparation of isolation film 9 is similar to that of isolation film 1, except that the thickness of the insulating layer in isolation film 9 is 20 μm. Isolation membrane 10: The preparation of isolation membrane 10 is similar to that of isolation membrane 1, except that the ion capture agent in the coating of isolation membrane 10 is Li 1 / 6 C. Isolation membrane 11: The preparation of isolation membrane 13 is similar to that of isolation membrane 1, except that the ion capture agent in the coating of isolation membrane 11 is Na 1 / 6 C. Isolation membrane 12: The preparation of isolation membrane 12 is similar to that of isolation membrane 1, except that the ion capture agent in the coating of isolation membrane 12 is Li 4.4 Four. Isolation membrane 13: The preparation of isolation membrane 13 is similar to that of isolation membrane 1, except that the ion capture agent in the coating of isolation membrane 13 is Li 4.4 Sn. Separator 14: The preparation of separator 14 is similar to that of separator 1, except that the ion capture agent in the coating of separator 14 is Li powder. Separator 15: The preparation of separator 15 is similar to that of separator 1, except that the ion capture agent in the coating layer of separator 15 is n-butyl lithium. Isolation membrane 16: The preparation of isolation membrane 16 is similar to that of isolation membrane 1, except that the ion capture agent in the coating of isolation membrane 16 is Isolation membrane 17: The preparation of isolation membrane 17 is similar to that of isolation membrane 1, except that the ion capture agent in the coating of isolation membrane 17 is Isolation membrane 18: The preparation of isolation membrane 18 is similar to that of isolation membrane 1, except that the coating in isolation membrane 18 contains inorganic Al2O3 ceramic particles, wherein the ion capture agent Li7Ti5O 12 The mass ratio of inorganic Al2O3 ceramic particles and binder PVDF is 50%:40%:10%.
[0001] Separator 19: Separator 19 is prepared similarly to separator 1, except that the coating of separator 19 contains only the binder PVDF but no ion scavenger. 2. Preparation of secondary batteries [Example 1] (1) Preparation of positive electrode sheet Active material lithium manganate (LiMn2O4), conductive agent acetylene black, and binder PVDF are fully stirred and mixed in an N-methylpyrrolidone solvent system in a mass ratio of 90%:5%:5%, and then coated on Al foil, dried, and cold pressed to obtain a positive electrode sheet. (2) Preparation of negative electrode sheet Active material artificial graphite, conductive agent acetylene black and binder PVDF were fully stirred and mixed in an N-methylpyrrolidone solvent system in a mass ratio of 90%:5%:5%, and then coated on a Cu foil, dried and cold pressed to obtain a negative electrode sheet. (3) Isolation film The isolation film adopts the isolation film 1 prepared above. (4) Preparation of electrolyte Ethylene carbonate (EC) and ethyl methyl carbonate (EMC) were mixed at a mass ratio of 30:70, and 1 M lithium hexafluorophosphate (LiPF6) electrolyte salt was dissolved to obtain an electrolyte solution. (5) Assembly of lithium-ion batteries The positive electrode sheet, the isolation film 1, and the negative electrode sheet are stacked in order, so that the isolation film 1 is placed between the positive electrode sheet and the negative electrode sheet to play an isolating role, and then wound to obtain an electrode assembly; the electrode assembly is placed in a battery casing, and after drying, the electrolyte is injected, and then a lithium-ion battery 1 is obtained through processes such as formation and standing, which is Example 1. The preparation methods of the secondary batteries of Examples 2-18 and Comparative Example 1 are similar to that of the secondary battery of Example 1, except that different isolation membranes are used (among which, Examples 1-18 use isolation membranes 1-18, and Comparative Example 1 uses isolation membrane 19), as shown in Table 1 for details. 3. Battery performance test (1) Battery capacity retention test At 45°C, the lithium-ion secondary battery is charged at a constant current of 1C to the upper voltage limit, then charged at a constant voltage at the upper voltage limit until the current is less than 0.05C, and then discharged at a constant current of 1C to the lower voltage limit. This is a charge and discharge process. Repeat the charge and discharge in this way, and calculate the capacity retention rate of the lithium-ion secondary battery after 500 cycles. The capacity retention rate (%) of the lithium ion secondary battery after 500 cycles at 45° C.=(discharge capacity at the 500th cycle / discharge capacity at the first cycle)×100%. (2) Negative electrode transition metal content test after 500 cycles at 45°C The lithium-ion secondary battery after 500 cycles at 45° C. was disassembled, the negative electrode piece was taken out, and then the total content of transition metals (such as Ni, Co, Mn or Fe) on the negative electrode piece was tested by inductively coupled plasma atomic emission spectrometry according to EPA 6010D-2014. The voltage upper and lower limits of the above lithium manganese oxide system battery performance test are selected to be 3 to 4.3V. Please refer to Table 1 for product parameters of different embodiments and comparative examples, as well as test results of battery performance tests conducted on Comparative Example 1 and Embodiments 1-18 prepared according to the above method. Table 1: Product parameters and test results of comparative examples and different embodiments From the comparison between the results of comparative example 1 and examples 1-18, it can be seen that the coating of the isolation membrane includes an ion capture agent, and the corresponding cycle performance of the lithium manganese oxide battery is significantly improved, and the transition metal content on the negative electrode plate is also significantly reduced. From the comparison of the results of comparative example 1 and examples 1, 10-18, it can be seen that the ion capture agent Li7Ti5O provided in the examples of the present application 12 、、Li 1 / 6 C. Na 1 / 6 C. Li 4.4 Si、Li 4.4 Sn, metallic Li (powder), n-butyl lithium, When added to lithium manganese oxide batteries respectively, the cycle performance of lithium manganese oxide batteries is significantly improved, and the transition metal content on the negative electrode plate is also significantly reduced. From the comparison of the results of Examples 1-5, it can be seen that when the thickness of the coating is within an appropriate range, the corresponding cycle performance improvement effect of the lithium manganese oxide battery is better. In the embodiments of the present application, when other conditions are the same, the thickness of the coating is within the range of 0.5 μm to 30 μm, and the cycle performance of the lithium manganese oxide battery is better. From the comparison of the results of Example 1 and Examples 6-9, it can be seen that when the thickness of the insulating layer is within an appropriate range, the corresponding cycle performance improvement effect of the lithium manganese oxide battery is better. In the embodiment of the present application, when other conditions are the same, the thickness of the insulating layer is within the range of 0.01μm to 20μm, and the cycle performance of the lithium manganese oxide battery is better. Although the present application has been described with reference to preferred embodiments, various modifications may be made thereto and parts thereof may be replaced with equivalents without departing from the scope of the present application. In particular, the various technical features mentioned in the various embodiments may be combined in any manner as long as there are no structural conflicts. The present application is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.
Claims
1. A separation film, include: Basement membrane; A coating layer, the coating layer is disposed on the surface of at least one side of the base film, the coating layer includes an ion capture agent, and the reduction potential of the ion capture agent relative to lithium metal is 0 to 2V; An insulating layer is disposed on the coating layer.
2. The isolation film according to claim 1, in, The ion capture agent includes at least one of active metal and alkali metal compounds; Optionally, the active metal includes at least one of Li, Na, K, Rb, Cs, Fr, Mg, Ca, Sr, Ba, Al, Ti or V. Optionally, the active metal includes at least one of Li, Na, Mg, Al, Ti or V. Optionally, the alkali metal compound comprises A 1 x B. A 2 y Ti 5 O 12 , at least one of the compounds represented by formula (I), formula (II) or formula (III): RA 3 (I)、 Among them, A 1 , A 2 , A 3 , A 4 , A 5 , A 6 Each independently includes at least one of Li, Na, or K, B includes C, Si, or Sn, x≥0.05, y>4, R, R 1 , R 2 , R 3 , R 4 Each independently includes at least one of a hydrogen atom, an alkyl group having 1 to 20 carbon atoms, an alkyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an alkenyl group having 2 to 20 carbon atoms, an alkenyl group having 2 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an aryl group having 6 to 26 carbon atoms, an aryl group having 6 to 26 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, a carboxyl group having 1 to 20 carbon atoms, a carboxyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, a carbonyl group having 1 to 20 carbon atoms, a carbonyl group having 1 to 20 carbon atoms substituted by a sulfonic acid group or a sulfonyl group, an aryloxy group having 6 to 26 carbon atoms, and an aryloxy group having 6 to 26 carbon atoms substituted by a sulfonic acid group or a sulfonyl group.
3. The isolation film according to claim 2, in, The A 1 x B includes Li 1 / 6 C. Na 1 / 6 C.K 1 / 8 C. Li 4.4 Si or Li 4.4 At least one of Sn.
4. The isolation film according to claim 2 or 3, in, 5≤y≤7; Optionally, the A 2 y Ti 5 O 12 Including Li 7 Ti 5 O 12 Or Na 7 Ti 5 O 12 At least one of .
5. The separator according to any one of claims 2 to 4, in, The compound represented by formula (I) includes at least one of n-butyllithium, naphthyllithium or biphenyllithium.
6. The separator according to any one of claims 2 to 5, in, The compounds represented by formula (II) include At least one of .
7. The separator according to any one of claims 2 to 6, in, The compounds represented by formula (III) include At least one of .
8. The separator according to any one of claims 1 to 7, in, The mass proportion of the ion capture agent in the coating is 50% to 99%. Optionally, the mass proportion of the ion capture agent in the coating is 80% to 98%.
9. The separator according to any one of claims 1 to 8, in, The thickness d1 of the coating is 0.5 μm to 30 μm, and optionally, d1 is 2 μm to 20 μm.
10. The separator according to any one of claims 1 to 9, in, The thickness d2 of the insulating layer is 0.01 μm to 20 μm, and optionally, d2 is 0.1 μm to 10 μm.
11. The separator according to any one of claims 1 to 10, in, The base film comprises at least one of polyolefins and their derivatives, halogenated polyolefins and their derivatives, polyethers and their derivatives, polyetheretherketones and their derivatives, polyesters and their derivatives, polyimides and their derivatives, and polyvinyl alcohols and their derivatives; Optionally, the halogenated polyolefin and its derivatives include at least one of polytetrafluoroethylene and its derivatives, polyvinyl fluoride and its derivatives, polyvinylidene fluoride and its derivatives; Optionally, the polyester and its derivatives include at least one of polyethylene terephthalate and its derivatives, polybutylene terephthalate and its derivatives.
12. The separator according to any one of claims 1 to 11, in, The insulating layer includes at least one of an electronic insulating inorganic substance and an electronic insulating organic substance; Optionally, the electronic insulating inorganic substance comprises Al 3 O 2 、TiO 2 、MgO、SiO 2 SnO 2 、CeO 2 、ZrO 2 、BaTiO 3 , Y 2 O 3 or at least one of boehmite; Optionally, the electronically insulating organic substance includes at least one of polyethylene, polypropylene, cellulose, polyimide, polyethylene oxide, polymethyl methacrylate, polyvinyl chloride, polyacrylonitrile, polyvinylidene fluoride, polypropylene oxide, polyvinylidene chloride or polycarbonate.
13. The separator according to any one of claims 1 to 12, in, The coating also includes a binder; Optionally, the binder includes at least one of polyacrylate, polyacrylic acid, polytetrafluoroethylene, polyvinylidene fluoride, vinylidene fluoride-trichloroethylene copolymer, polyvinyl pyrrolidone, polyvinyl acetate, ethylene-vinyl acetate copolymer, polyethylene oxide, polyarylate, carboxymethyl cellulose, hydroxypropyl cellulose, regenerated cellulose, cellulose acetate, cellulose acetate propionate, cellulose acetate butyrate, polyacrylonitrile, polyvinyl alcohol, polyethylene, polypropylene, starch, or cyanoethyl pullulan.
14. The separator according to any one of claims 1 to 13, in, The coating further comprises a filler; Optionally, the filler includes at least one of inorganic particles, organic particles, or organic-metal framework materials; Optionally, the inorganic particles include at least one of inorganic particles having a dielectric constant of 5 or more or inorganic particles having ion conductivity but not storing ions; Optionally, the organic particles include at least one of polycarbonate, polythiophene, polypyridine, polystyrene, polyacrylic wax, polyethylene, polypropylene, cellulose, cellulose modifier, melamine resin, phenolic resin, polyester, silicone resin, polyimide, polyamideimide, polyaramid, polyphenylene sulfide, polysulfone, polyethersulfone, polyetheretherketone, polyaryletherketone, or a copolymer of butyl acrylate and ethyl methacrylate; Optionally, the organic-metal framework material includes at least one of a nitrogen-containing heterocyclic ligand building structure, an organic carboxylic acid ligand building structure, and a nitrogen-oxygen mixed ligand building structure.
15. The separator according to any one of claims 1 to 14, in, The porosity of the base film is 30% to 60%.
16. A method for preparing an isolation film, include: providing a basement membrane; Providing a coating slurry, the coating slurry comprising an ion capture agent, the ion capture agent having a reduction potential of 0 to 2 V relative to lithium metal, and coating the coating slurry on the base film to form a coating; An insulating slurry is provided, and the insulating slurry is coated on the coating layer to obtain the isolation film. 17 . A secondary battery comprising the separator according to claim 1 .
18. An electric device comprising the secondary battery according to claim 17.
Citation Information
Cited By
Battery monomer, battery device, power utilization device and energy storage device
CN121885720A
A battery cell, a battery device, a power consumption device, an energy storage device
CN121885720B