Preparation method of composite film with inner layer coated with antifogging agent
Through the preparation method of composite film coated with anti-fog agent in the inner layer, the initial curing and air-drying of anti-fog agent are used to form a protective layer, which solves the problem of insufficient anti-fog capacity of the existing film material and realizes the prevention under refrigeration conditions Fog effect.
Patent Information
- Application Number
- CN202411096080.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-12-06
AI Technical Summary
The existing packaging film materials have insufficient anti-fog resistance, which causes water vapor to condense into water droplets on the inner surface of the sealed container during refrigeration, affecting the sealing effect.
The composite film preparation method of inner layer coated anti-fog agent is used to prepare, through unwinding, coating, air-drying and winding steps, the first hot air nozzle is used to initially cure and air-dry the anti-fog protective layer to ensure the anti-fog agent. Evenly distributed and cured.
Under refrigeration conditions, it is achieved to prevent mist from forming water droplets on the inner surface of the composite film, improve the anti-fog effect of packaging seal, and avoid the problem of uneven distribution of anti-fog agents.
Smart Images

Figure CN119076346A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of film material manufacturing, and in particular to a method for preparing a composite film with an inner layer coated with an anti-fogging agent. Background Art
[0002] During the production, storage, cold chain transportation and refrigerated sales of fresh food, a sealed container is usually formed by adding a printed cover film to a plastic container to seal and package the product. For example, Chinese Patent 202021994790.7 discloses a multi-format high-temperature resistant food lunch box, including a box body with three accommodating cavities for placing food, with a gap between each of the accommodating cavities, the cavity wall of each of the accommodating cavities extending downward and integrally formed with its bottom, the bottom area of the accommodating cavity is smaller than its top area, the bottom of the cavity wall is connected to the bottom through a first arc surface, and two adjacent cavity walls are connected through a second arc surface, and the upper surface of each of the accommodating cavities forms a flat sealing surface, and a sealing film for sealing each of the accommodating cavities is affixed to the sealing surface.
[0003] Due to the temperature difference between the product in the sealed container and the external environment, the water vapor in the container condenses into tiny water droplets on the inner surface of the printed cover film, so the film material used for packaging needs to have anti-fog properties. Summary of the invention
[0004] The purpose of the present invention is to provide a method for preparing a composite film with an inner layer coated with an anti-fogging agent, so as to solve the problem that the anti-fogging ability of existing packaging film materials is insufficient.
[0005] In order to achieve the above object, the present invention adopts the following technical scheme: a method for preparing a composite film with an inner layer coated with an anti-fogging agent, comprising the following steps:
[0006] S1, unwinding: the film-based material roll is unwinded through the unwinding mechanism;
[0007] S2, coating: the film substrate is transported to the bottom of the coating nozzle for coating with the anti-fogging agent, a first hot air nozzle is arranged in front of the coating nozzle, and the hot air blown by the first hot air nozzle is directed toward the film substrate below the coating nozzle to preliminarily cure the anti-fogging agent;
[0008] S3, air drying: the film substrate coated with the antifogging agent continues to be transported, and the antifogging agent is dried by hot air during the transportation process, and the antifogging agent forms an antifogging protective layer on the surface of the film substrate to form a composite film;
[0009] S4, winding: After the temperature of the composite film drops to room temperature, it is wound up.
[0010] As a further description of the above technical solution:
[0011] In step S2, before the film substrate is conveyed to the bottom of the coating nozzle for coating with the anti-fogging agent, the surface of the film substrate is pre-heated.
[0012] As a further description of the above technical solution:
[0013] In step S2, when the film substrate is conveyed to the bottom of the coating nozzle for coating with the anti-fogging agent, the film substrate is arranged at an inclination.
[0014] As a further description of the above technical solution:
[0015] A strip-shaped air outlet is arranged at the bottom of the first hot air nozzle, and the hot air blown out of the strip-shaped air outlet is directed toward the film substrate below the coating nozzle.
[0016] As a further description of the above technical solution:
[0017] The first hot air nozzle is rotatably mounted on the mounting frame.
[0018] As a further description of the above technical solution:
[0019] An infrared thermal imaging device is arranged at the rear side of the coating nozzle.
[0020] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:
[0021] 1. In the present invention, a certain proportion of anti-fog agent is coated on the inner layer of the composite film, and then heated and air-dried to form a protective layer on the substrate. At this time, when the composite film is used to package products, the anti-fog agent forms an anti-fog protective layer on the surface of the film substrate, so that the fog generated after refrigeration cannot form water droplets on the inner surface of the composite film, thereby achieving an anti-fog effect.
[0022] 2. In the present invention, during the processing of the composite film, after the film substrate is coated with the antifog agent by the coating nozzle, the antifog agent on the film substrate is immediately heated and air-dried by the first hot air nozzle to achieve preliminary air drying to prevent the antifog agent from flowing on the film substrate and causing uneven distribution. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0024] Figure 1 The figure is a schematic diagram of coating of a coating nozzle in a method for preparing a composite film with an inner layer coated with an anti-fogging agent.
[0025] Legend:
[0026] 1. Coating nozzle; 2. First hot air nozzle; 21. Mounting frame. DETAILED DESCRIPTION
[0027] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0028] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0030] In the description of the embodiments of the present invention, it should be noted that the terms "upper", "inner", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are directions or positional relationships in which the inventive product is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.
[0031] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0032] Example 1
[0033] See also Figure 1 The present invention provides a technical solution: a method for preparing a composite film with an inner layer coated with an anti-fogging agent, comprising the following steps:
[0034] S1, unwinding: the film-based material roll is unwinded through the unwinding mechanism;
[0035] S2, coating: the film substrate is transported to the bottom of the coating nozzle 1 for coating of the antifogging agent. A first hot air nozzle 2 is arranged in front of the coating nozzle 1. The hot air blown by the first hot air nozzle 2 is directed toward the film substrate below the coating nozzle 1 to preliminarily cure the antifogging agent.
[0036] S3, air drying: the film substrate coated with the antifogging agent continues to be transported, and the antifogging agent is dried by hot air during the transportation process, and the antifogging agent forms an antifogging protective layer on the surface of the film substrate to form a composite film;
[0037] S4, winding: After the temperature of the composite film drops to room temperature, it is wound up.
[0038] A strip-shaped air outlet is provided at the bottom of the first hot air nozzle 2, and the hot air blown out of the strip-shaped air outlet is directed toward the film substrate below the coating nozzle 1, effectively ensuring that the anti-fogging agent is heated and dried uniformly.
[0039] The first hot air nozzle 2 is rotatably mounted on the mounting frame 21. The first hot air nozzle 2 can be rotated to adjust the blowing angle of the heating head and the heating effect, so as to timely and effectively cure the anti-fogging agent.
[0040] An infrared thermal imaging device is provided at the rear side of the coating nozzle 1. The infrared thermal imaging device detects the temperature distribution on the surface of the film substrate. Since the temperature rise of the heated film substrate and the antifogging agent is different from the temperature rise of the heated film substrate alone, by detecting the temperature distribution on the film surface, it can be judged whether the antifogging agent is sprayed uniformly, so as to timely find out whether the coating nozzle 1 is working normally, and subsequently remove the composite film material that is not coated properly, so as to improve the processing quality of the composite film.
[0041] Working principle: A certain proportion of anti-fog agent is applied to the inner layer of the composite film, and then heated and air-dried to form a protective layer on the substrate. At this time, when the composite film is used to package products, the anti-fog agent forms an anti-fog protective layer on the surface of the film substrate, so that the fog generated after refrigeration cannot form water droplets on the inner surface of the composite film, thereby achieving an anti-fog effect. During the composite film processing, after the film substrate is coated with the anti-fog agent by the coating nozzle 1, the anti-fog agent on the film substrate is immediately heated and air-dried by the first hot air nozzle 2 to achieve preliminary air drying and prevent the anti-fog agent from flowing on the film substrate and causing uneven distribution.
[0042] Example 2
[0043] The other steps are the same as those of Example 1, except that: in step S2, before the film substrate is conveyed to the bottom of the coating nozzle 1 for coating with the antifogging agent, the surface of the film substrate is preheated to improve the bonding effect between the film substrate and the antifogging agent.
[0044] Example 3
[0045] The other steps are the same as those of Example 2, except that: in step S2, when the film substrate is conveyed to the bottom of the coating nozzle 1 for coating with the antifogging agent, the film substrate is arranged obliquely, and when the film substrate is conveyed to the bottom of the coating nozzle 1 for coating with the antifogging agent, the film substrate is conveyed obliquely upward. This allows the coated antifogging agent to improve its bonding effect with the film substrate under the action of gravity, and the hot air blown out by the first hot air nozzle 2 can prevent the antifogging agent from flowing, effectively achieving the initial solidification of the antifogging agent.
[0046] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for preparing a composite film with an inner layer coated with an antifogging agent, characterized in that: The following steps are involved: S1, unwinding: the film-based material roll is unwinded through the unwinding mechanism; S2, coating: the film substrate is transported to the bottom of the coating nozzle for coating with the anti-fogging agent, a first hot air nozzle is arranged in front of the coating nozzle, and the hot air blown by the first hot air nozzle is directed toward the film substrate below the coating nozzle to preliminarily cure the anti-fogging agent; S3, air drying: the film substrate coated with the antifogging agent continues to be transported, and the antifogging agent is dried by hot air during the transportation process, and the antifogging agent forms an antifogging protective layer on the surface of the film substrate to form a composite film; S4, winding: After the temperature of the composite film drops to room temperature, it is wound up.
2. The method for preparing a composite film with an inner layer coated with an anti-fogging agent according to claim 1, characterized in that: In the step S2, before the film substrate is conveyed to the bottom of the coating nozzle for coating with the anti-fogging agent, the surface of the film substrate is preheated.
3. The method for preparing a composite film with an inner layer coated with an anti-fogging agent according to claim 2, characterized in that: In the step S2, when the film substrate is conveyed to the bottom of the coating nozzle for coating with the anti-fogging agent, the film substrate is arranged at an inclination.
4. The method for preparing a composite film with an inner layer coated with an anti-fogging agent according to claim 1, characterized in that: A strip-shaped air outlet is provided at the bottom of the first hot air nozzle, and the hot air blown out of the strip-shaped air outlet is directed toward the film substrate below the coating nozzle.
5. The method for preparing a composite film with an inner layer coated with an anti-fogging agent according to claim 4, characterized in that: The first hot air nozzle is rotatably mounted on the mounting frame.
6. The method for preparing a composite film with an inner layer coated with an anti-fogging agent according to claim 1, characterized in that: An infrared thermal imaging device is arranged at the rear side of the coating nozzle.