Powder metallurgy side hole forming die
The powder metallurgy side hole forming mold addresses the need for secondary processing by using sliding and rotating side molds to apply radial and axial pressure, ensuring uniform molding and easy demolding without additional processing steps.
Patent Information
- Application Number
- CN202411225815.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-12-06
AI Technical Summary
Existing powder metallurgy dies require secondary processing to form side holes, limiting the shape of the green compact and complicating the demolding process.
A powder metallurgy side hole forming mold with a mold frame and symmetrical side molds that can slide and rotate, allowing for simultaneous radial and axial pressure during pressing, and facilitating easy demolding without secondary processing.
Enables uniform molding force and straightforward formation of side holes without secondary processing, enhancing the ease of demolding and reducing damage to the product.
Smart Images

Figure CN119076947A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of powder metallurgy, and more specifically to a powder metallurgy side hole forming die. Background Art
[0002] Powder metallurgy is a process technology that produces metal powder or uses metal powder (or a mixture of metal powder and non-metal powder) as raw material, and then forms and sinters it to produce metal materials, composite materials and various types of products. Powder metallurgy is similar to the production of ceramics, both of which belong to powder sintering technology. Therefore, a series of new powder metallurgy technologies can also be used to prepare ceramic materials. Due to the advantages of powder metallurgy technology, it has become the key to solving new material problems and plays a vital role in the development of new materials.
[0003] Compression molding is the most widely used technology in powder metallurgy forming. It is a process in which metal powder is fed into a mold cavity at room temperature with a specified filling coefficient, and the powder is pressed into a green compact with a predetermined shape, size, density and strength by die punching. The green compact is then ejected from the mold by pressure. It usually consists of three steps: powder loading, pressing and demolding. There are three main pressing methods for compression molding technology: unidirectional pressing, bidirectional pressing and floating pressing. Regardless of the pressing method, the pressing pressure applied to the powder metallurgy forming press is always axial, and the pressing is carried out along the axial direction of the green compact. Therefore, the shape of the green compact is limited, and the side holes in the powder metallurgy product cannot be directly pressed and formed, but need to be formed after sintering.
[0004] Therefore, a new solution needs to be proposed to solve this problem. Summary of the invention
[0005] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a powder metallurgy side hole forming die, which solves the problem that the side holes of the existing powder metallurgy dies need secondary processing.
[0006] The above technical objectives of the present invention are achieved through the following technical solutions: The embodiment of the present application provides a powder metallurgy side hole forming mold, including a mold frame, the mold frame is provided with an upper mold assembly and a lower mold assembly, the lower mold assembly includes a lower shell, the lower shell includes a bottom plate, a lower mold frame is fixedly connected to the bottom plate, the lower mold frame includes a pressing cavity, two symmetrical side molds are provided on the left and right sides of the pressing cavity, the side molds are slidably connected to the lower mold frame, one of the side molds is provided with a hole forming axis, the two side molds can be combined to form a female mold, a first driving assembly that can drive the two side molds to slide toward or away from each other is provided on the lower shell, a lower die head is provided at the bottom of the lower mold frame, a second driving assembly that can drive the lower die head to rise and fall is provided on the bottom plate, the upper mold assembly includes an upper mold frame, an upper die head is provided on the upper mold frame, a third driving assembly that can drive the upper mold frame to press down is provided on the mold frame, and a fourth driving assembly that can drive the upper die head to press down is provided on the upper mold frame.
[0007] In one of the embodiments, a mold core is fixedly connected to the bottom plate, a first clearance hole for the mold core to pass through is provided at the bottom of the lower mold frame, and the lower mold head is located at the periphery of the mold core and can be slidably connected to the mold core.
[0008] In one of the embodiments, a connecting hole is provided on the side mold for the hole-making shaft to pass through, a limiting groove is provided on the outer periphery of the connecting hole, a limiting ring is provided on the hole-making shaft to match the limiting hole, the limiting ring is rotatably connected to the limiting groove, a first screw is provided on the end of the hole-making shaft away from the mold core, a first threaded hole is provided on the side of the lower mold frame close to the first screw, the first screw is threadedly connected to the first threaded hole, an axial groove matched with the hole-making shaft is provided on the mold core, and the end of the hole-making shaft close to the axial groove can extend into the axial groove.
[0009] In one of the embodiments, the top of the lower mold frame is flush with the top plate, a push block is slidably connected to the top plate, and a fifth driving component that can drive the push block to slide back and forth is provided on the top plate.
[0010] In one of the embodiments, a ventilation cavity is provided on the push block, and a partition is provided on the push block for dividing the ventilation cavity into an air inlet cavity and an air outlet cavity, the push block includes a left plate and a right plate, two ends of the partition are respectively connected to the left plate and the right plate, an air inlet is provided on the side of the air inlet cavity close to the top plate, and an air outlet is provided on the side of the air outlet cavity close to the top plate, a cold air fan is provided on one side of the mold frame, the cold air fan includes a cold air outlet, and the cold air outlet is connected to the air inlet cavity, a collecting box is provided on the other side of the mold frame, a connecting port is provided on the collecting box, and the connecting port is connected to the air outlet cavity, an exhaust fan is provided on the collecting box, the exhaust fan includes an exhaust port and an exhaust port, the exhaust port is connected to the collecting box, and a filter is provided between the exhaust port and the connecting port.
[0011] In one of the embodiments, an opening is provided on the air inlet chamber, the air cooler is connected to the opening, an adjusting groove is provided on one side of the push block close to the opening, a strip groove connected to the adjusting groove is provided on the side wall of the air inlet chamber, the strip groove extends from one end of the push block close to the top plate to the end away from the top plate, an adjusting block is slidably connected in the strip groove, two ends of the adjusting block extend into the air inlet chamber and the adjusting groove respectively, a wind shield that can cover the opening is provided on the adjusting block located in the air inlet chamber, a top cover is provided on the top of the air inlet chamber, a spring that can press the wind shield down to below the opening is provided on the top cover, and a resist block that can resist the adjusting block to make the wind shield rise and fall is provided on the top plate.
[0012] In one embodiment, the stop block includes an adjustment slope that gradually rises from front to back.
[0013] In one embodiment, the fifth driving assembly includes a second screw, a first connecting block is fixedly connected to the top plate, a motor is fixedly connected to the first connecting block, an output end of the motor is fixedly connected to the second screw, an end of the second screw away from the motor is rotatably connected to the mold frame, a second threaded hole is provided on the push block, the second screw is threadedly connected to the second threaded hole, a second connecting block is fixedly connected to the top plate, a guide rod parallel to the second screw is fixedly connected to the second connecting block, and the push block is slidably connected to the guide rod.
[0014] In one embodiment, the first driving assembly includes two first hydraulic cylinders, the two first hydraulic cylinders are symmetrically arranged on the lower shell, the lower mold frame is provided with two second make way holes, the output ends of the two first hydraulic cylinders pass through the two second make way holes respectively and are connected to the two side molds, the second driving assembly includes a second hydraulic cylinder fixedly connected to the base plate, the output end of the second hydraulic cylinder is fixedly connected to the lower mold head, the third driving assembly includes a third hydraulic cylinder fixedly connected to the mold frame, the output end of the third hydraulic cylinder is fixedly connected to the upper mold frame, and the fourth driving assembly includes a fourth hydraulic cylinder fixedly connected to the upper mold frame, the output end of the fourth hydraulic cylinder is fixedly connected to the upper mold head.
[0015] In summary, the present invention has the following beneficial effects: the present invention provides a lower mold frame with a pressing cavity, and two side molds are provided in the pressing cavity, and the two side molds are provided to be close to each other to form a female mold, so that when pressing the blank, the two side molds are first brought close to each other to pre-press the metal powder on the side, and after the two side molds form the female mold, the upper mold head and the lower mold head press the metal powder in the up and down directions to press the metal powder into shape, so that the metal powder is subjected to both radial pressure and axial pressure during the pressing process, so that the force of the metal powder molding is more uniform, and at the same time, a hole axis is provided on one side mold, and when the pressing is completed, the two side molds move to both sides, and the side mold pulls the hole axis out of the blank to obtain the side hole, so that the formation of the side hole is simple and convenient, and no secondary processing is required, and on the other hand, after pressing and molding, the two side molds move to both sides, and the upper mold head moves upward, so that the blank is easy to demold, and at the same time, the damage to the blank caused by ejection and demolding is avoided. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 The structure of the powder metallurgy side hole forming die of the embodiment of the present application is shown in FIG. Figure 1 ;
[0017] Figure 2 This is a schematic diagram of the structure inside the lower shell of the powder metallurgy side hole forming die of an embodiment of the present application;
[0018] Figure 3 The structure of the powder metallurgy side hole forming die of the embodiment of the present application is shown in FIG. Figure 2 ;
[0019] Figure 4 It is a schematic structural diagram of a hole forming shaft in a powder metallurgy side hole forming die according to an embodiment of the present application;
[0020] Figure 5 It is a schematic structural diagram of a push block in a powder metallurgy side hole forming die according to an embodiment of the present application;
[0021] Figure 6 for Figure 1 Magnified view of part A.
[0022] In the figure: 1, mold frame; 2, lower shell; 21, bottom plate; 211, mold core; 22, lower mold frame; 221, pressing cavity; 222, side mold; 2221, hole forming shaft; 22211, limit ring; 22212, first screw; 223, lower die head; 23, top plate; 231, push block; 23111, air inlet cavity; 231112, wind shield; 23112, air outlet cavity; 23113, partition; 2312, adjustment Groove; 23121, adjustment block; 2313, opening; 232, first connecting block; 2321, motor; 2322, second screw; 233, second connecting block; 2331, guide rod; 234, stop block; 2341, adjustment slope; 3, upper mold frame; 31, upper mold head; 4, collection box; 41, exhaust fan; 5, cooling fan; 6, first hydraulic cylinder; 7, second hydraulic cylinder; 8, third hydraulic cylinder; 9, fourth hydraulic cylinder. DETAILED DESCRIPTION
[0023] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] like Figures 1 to 3 As shown, an embodiment of the present application provides a powder metallurgy side hole forming mold, including a mold frame 1, on which an upper mold assembly and a lower mold assembly are arranged, the lower mold assembly includes a lower shell 2, the lower shell 2 includes a bottom plate 21, a lower mold frame 22 is fixedly connected to the bottom plate 21, the lower mold frame 22 includes a pressing cavity 221, and two symmetrical side molds 222 are arranged on the left and right sides of the pressing cavity 221, and the side molds 222 are slidably connected to the lower mold frame 22, one of the side molds 222 is provided with a hole forming shaft 2221, and the two The side molds 222 can be combined to form a female mold, and the lower shell 2 is provided with a first driving component that can drive the two side molds 222 to slide toward or away from each other, and the bottom of the lower mold frame 22 is provided with a lower mold head 223, and the bottom plate 21 is provided with a second driving component that can drive the lower mold head 223 to rise and fall, and the upper mold assembly includes an upper mold frame 3, and the upper mold frame 3 is provided with an upper mold head 31, and the mold frame 1 is provided with a third driving component that can drive the upper mold frame 3 to press down, and the upper mold frame 3 is provided with a fourth driving component that can drive the upper mold head 31 to press down.
[0025] Specifically, slide grooves can be set on the front and rear sides of the lower mold frame 22, and sliders corresponding to the slide grooves are set on the front and rear sides of the side molds 222. The sliders are slidably connected to the slide grooves. The position where one side mold 222 contacts the other side mold 222 can be set as a slope to prevent excessive metal powder from remaining at the joint of the two side molds 222.
[0026] During operation, the two side molds 222 are first moved to the two sides of the pressing cavity 221 respectively, and then the powder is poured into the pressing cavity 221, and the upper mold frame 3 is pressed down so that the upper mold frame 3 closes the pressing cavity 221, and then the first driving component drives the two side molds 222 to approach each other, and the metal powder is squeezed as the two side molds 222 approach each other. When the two side molds 222 are close to form a female mold, the second driving component drives the lower die head 223 to press upward, and the fourth driving component drives the upper die head 31 to press downward, so that the metal powder is pressed and formed by the upper and lower pressures at the same time. After pressing and forming, the two side molds 222 move to both sides respectively, and the upper die head 31 also moves upward, so that the pressed green sheet is demolded, and the lower die head 223 pushes the pressed green sheet upward to take out the pressed green sheet.
[0027] The above structure is set up by setting a lower mold frame 22 with a pressing cavity 221, setting two side molds 222 in the pressing cavity 221, and setting the two side molds 222 to be close to form a female mold, so that when pressing the compact, the two side molds 222 are first brought close to each other to pre-press the metal powder on the side. After the two side molds 222 form a female mold, the upper mold head 31 and the lower mold head 223 press the metal powder in the up and down directions to press the metal powder into shape, so that the metal powder is subjected to radial pressure during the pressing process. It is also subjected to axial pressure, so that the force of metal powder molding is more uniform. At the same time, a hole axis 2221 is set on a side mold 222. When the pressing is completed, the two side molds 222 move to both sides, and the side mold 222 pulls the hole axis 2221 out of the pressed billet to obtain a side hole, making the formation of the side hole simple and convenient without the need for secondary processing. On the other hand, after pressing and molding, the two side molds 222 move to both sides, and the upper mold head 31 moves upward, making it easy to demold the pressed billet and avoiding damage to the pressed billet during ejection and demolding.
[0028] In this embodiment, Figure 1 As shown, a mold core 211 is fixedly connected to the bottom plate 21 , a first clearance hole for the mold core 211 to pass through is provided at the bottom of the lower mold frame 22 , and the lower mold head 223 is located at the outer periphery of the mold core 211 and can be slidably connected to the mold core 211 .
[0029] The above structure is provided with a mold core 211 penetrating the lower mold frame 22, so that the pressed blank is ring-shaped.
[0030] In this embodiment, Figure 2 and Figure 4As shown, the side mold 222 is provided with a connecting hole for the hole-making shaft 2221 to pass through, and a limiting groove is provided on the outer periphery of the connecting hole. The hole-making shaft 2221 is provided with a limiting ring 22211 matched with the limiting hole, and the limiting ring 22211 is rotatably connected with the limiting groove. A first screw 22212 is provided at the end of the hole-making shaft 2221 away from the mold core 211, and a first threaded hole is provided on the side of the lower mold frame 22 close to the first screw 22212. The first screw 22212 is threadedly connected with the first threaded hole, and an axial groove matched with the hole-making shaft 2221 is provided on the mold core 211, and the end of the hole-making shaft 2221 close to the axial groove can extend into the axial groove.
[0031] During operation, when the two side molds 222 approach the mold core 211, the hole forming shaft 2221 extends into the axial groove of the mold core 211. When the side molds 222 move away from the mold core 211, the side molds 222 move to the left and right sides of the lower mold frame 22. Since the hole forming shaft 2221 is rotatably connected to the side molds 222 and is threadedly connected to one side of the lower mold frame 22, the hole forming shaft 2221 rotates under the action of the thread force when the side molds 222 move, which facilitates the separation of the hole forming shaft 2221 from the pressed blank.
[0032] The above-mentioned structure is arranged to rotatably connect the hole forming shaft 2221 with the side mold 222, and threadably connect the end of the hole forming shaft 2221 close to the lower mold frame 22 to the lower mold frame 22, so that when the hole forming shaft 2221 moves with the side mold 222, it rotates under the action of the thread force, so that the hole forming shaft 2221 is separated from the pressed blank while rotating, making separation convenient and preventing burrs from being generated in the side hole.
[0033] In this embodiment, Figure 1 As shown, the top of the lower mold frame 22 is flush with the top plate 23, a push block 231 is slidably connected to the top plate 23, and a fifth driving component that can drive the push block 231 to slide forward and backward is provided on the top plate 23.
[0034] During operation, when the pressing of the green compact is completed, the lower die head 223 can eject the green compact, and the upper surface of the lower die head 223 is parallel to the top plate 23. When the lower die head 223 moves upward until the lower die head 223 is flush with the top plate 23, the fifth driving assembly drives the push block 231 to move from back to front, so that the push block 231 passes over the pressing cavity 221 to push the green compact forward.
[0035] The above structure is arranged by arranging a push block 231 on the top plate 23 and arranging a fifth driving assembly that can drive the push block 231 to move, so that the push block 231 can push the green compact out when the green compact is pressed.
[0036] In this embodiment, Figure 5As shown, the push block 231 is provided with a ventilation cavity, and the push block 231 is provided with a partition 23113 which can separate the ventilation cavity into an air inlet cavity 23111 and an air outlet cavity 23112. The push block 231 includes a left plate and a right plate, and the two ends of the partition 23113 are respectively connected to the left plate and the right plate. The air inlet cavity 23111 is provided with an air inlet on one side close to the top plate 23, and the air outlet cavity 23112 is provided with an air outlet on one side close to the top plate 23. A cooling fan 5 is provided on one side of the mold frame 1, and the cooling fan 5 includes a cold air outlet, and the cold air outlet is connected to the air inlet chamber 23111. A collecting box is provided on the other side of the mold frame 1, and a connecting port is provided on the collecting box, and the connecting port is connected to the air outlet chamber 23112. An exhaust fan 41 is provided on the collecting box, and the exhaust fan 41 includes an exhaust port and an exhaust port, and the exhaust port is connected to the collecting box 4. A filter is provided between the exhaust port and the connecting port.
[0037] During operation, before pressing, the push block 231 can be moved to the front of the pressing chamber 221. When pressing is completed, the upper mold frame 3 is moved up first, and then the push block 231 moves from front to back, so that the push block 231 gradually passes through the pressing chamber 221. At this time, the air cooler 5 and the exhaust fan 41 are both turned on, and the air inlet chamber 23111 of the push block 231 transports cold air into the pressing chamber 221, so that the pressed green sheet is well cooled, which is convenient for subsequent demolding. The air outlet chamber 23112 of the push block 231 extracts the residual powder in the pressing chamber 221 and on the surface of the pressed green sheet, which is convenient for the next pressing work.
[0038] The above-mentioned structure is arranged by arranging an air inlet chamber 23111 and an air outlet chamber 23112 on the push block 231, and arranging a cold air fan 5 connected with the air inlet chamber 23111, so that when the push block 231 moves to the top of the pressing chamber 221, cold air can be sent into the pressing chamber 221, so that the pressed green body can be cooled quickly and the pressed green body can be demolded conveniently, and a collecting box and an exhaust fan 41 are arranged to be connected with the air outlet chamber 23112, so that when the push block 231 passes above the pressing chamber 221, the residual powder in the pressing chamber 221 can be absorbed and collected for the next pressing work.
[0039] In this embodiment, Figure 5 and Figure 6As shown, the air inlet cavity 23111 is provided with an opening 2313, the air cooler 5 is connected to the opening 2313, an adjustment groove 2312 is provided on one side of the push block 231 close to the opening 2313, a strip groove connected to the adjustment groove 2312 is provided on the side wall of the air inlet cavity 23111, an adjustment block 23121 is slidably connected in the strip groove, and both ends of the adjustment block 23121 extend to the air inlet cavity 23111 and the In the adjusting slot 2312, a wind shield 231112 which can block the opening 2313 is arranged on the adjusting block 23121 located in the air inlet chamber 23111, a top cover is arranged on the top of the air inlet chamber 23111, a spring which can press the wind shield 231112 down to below the opening 2313 is arranged on the top cover, and a resisting block 234 which can resist the adjusting block 23121 to make the wind shield 231112 rise and fall is arranged on the top plate 23.
[0040] During operation, when the push block 231 moves from front to back, the cold air from the push block 231 can cool the green sheet. However, since the push block 231 reaches different parts of the green sheet at different times, the temperatures of different parts of the green sheet are different. By setting a wind shield 231112 and a spring so that the wind shield 231112 is located below the opening 2313, and by setting a stop block 234 on the top plate 23, the wind shield 231112 can rise to block a portion of the opening 2313, thereby reducing the air output and weakening the cooling effect.
[0041] In this embodiment, Figure 6 As shown, the stopper 234 includes an adjusting slope 2341 which gradually rises from front to back.
[0042] During operation, when the push block 231 moves from front to back, the adjusting slope 2341 abuts against one side of the adjusting block 23121. When the adjusting block 23121 abuts against the high point of the adjusting slope 2341, the adjusting block 23121 is lifted up, so that the adjusting block 23121 partially blocks the opening 2313. Since the adjusting slope 2341 gradually rises from front to back, when the push block 231 moves from front to back, the height to which the adjusting block 23121 is lifted up becomes higher and higher, so that the blocked part of the opening 2313 becomes larger and the air output is reduced.
[0043] The above-mentioned structure is arranged by arranging the wind shield 231112, the adjusting block 23121 and the stop block 234, so that the cooling effect of the push block 231 gradually weakens when it moves from front to back. Since the front part of the billet is first cooled by the push block 231, when the push block 231 moves to above the rear part of the billet, the rear part of the billet has been partially cooled by the air or other factors, so the amount of cold air required for the rear part of the billet is less than that for the front part of the billet. By arranging the wind shield 231112, the adjusting block 23121 and the stop block 234, the cooling effect of the push block 231 is weakened from front to back, which can offset some temperature differences between the front and rear parts of the billet, so that the temperature of each part of the billet after cooling is roughly balanced, so that the molding and demolding effects of the billet are better.
[0044] In this embodiment, Figure 2 As shown, the fifth driving assembly includes a second screw 2322, a first connecting block 232 is fixedly connected to the top plate 23, a motor 2321 is fixedly connected to the first connecting block 232, an output end of the motor 2321 is fixedly connected to the second screw 2322, an end of the second screw 2322 away from the motor 2321 is rotatably connected to the mold frame 1, a second threaded hole is provided on the push block 231, the second screw 2322 is threadedly connected to the second threaded hole, a second connecting block 233 is fixedly connected to the top plate 23, a guide rod 2331 parallel to the second screw 2322 is fixedly connected to the second connecting block 233, and the push block 231 is slidably connected to the guide rod 2331.
[0045] During operation, the motor 2321 drives the second screw rod 2322 to rotate, and the push block 231 slides along the guide rod 2331 under the action of the thread force. The direction of the guide rod 2331 is set to be parallel to the Y axis, and the push block 231 slides along the length direction of the guide rod 2331.
[0046] In this embodiment, the first driving assembly includes two first hydraulic cylinders 6, and the two first hydraulic cylinders 6 are symmetrically arranged on the lower shell 2. Two second make way holes are arranged on the lower mold frame 22. The output ends of the two first hydraulic cylinders 6 pass through the two second make way holes respectively and are connected to the two side molds 222. The second driving assembly includes a second hydraulic cylinder 7 fixedly connected to the bottom plate 21, and the output end of the second hydraulic cylinder 7 is fixedly connected to the lower mold head 223. The third driving assembly includes a third hydraulic cylinder 8 fixedly connected to the mold frame 1, and the output end of the third hydraulic cylinder 8 is fixedly connected to the upper mold frame 3. The fourth driving assembly includes a fourth hydraulic cylinder 9 fixedly connected to the upper mold frame 3, and the output end of the fourth hydraulic cylinder 9 is fixedly connected to the upper mold head 31.
[0047] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A powder metallurgy side hole forming die, comprising a die frame (1), wherein an upper die assembly and a lower die assembly are arranged on the die frame (1), characterized in that: The lower mold assembly comprises a lower shell (2), the lower shell (2) comprises a top plate (23) and a bottom plate (21), the bottom plate (21) is fixedly connected to a lower mold frame (22), the lower mold frame (22) comprises a pressing cavity (221), two symmetrical side molds (222) are arranged on the left and right sides of the pressing cavity (221), the side molds (222) are slidably connected to the lower mold frame (22), one of the side molds (222) is provided with a hole-forming shaft (2221), the two side molds (222) can be combined to form a female mold, and the lower shell (2) is provided with a A first driving component is provided which can drive the two side molds (222) to slide towards or away from each other; a lower mold head (223) is provided at the bottom of the lower mold frame (22); a second driving component which can drive the lower mold head (223) to rise and fall is provided on the bottom plate (21); the upper mold component comprises an upper mold frame (3); an upper mold head (31) is provided on the upper mold frame (3); a third driving component which can drive the upper mold frame (3) to press downward is provided on the mold frame (1); and a fourth driving component which can drive the upper mold head (31) to press downward is provided on the upper mold frame (3).
2. The powder metallurgy side hole forming die according to claim 1, characterized in that: A mold core (211) is fixedly connected to the bottom plate (21), a first clearance hole for the mold core (211) to pass through is provided at the bottom of the lower mold frame (22), and the lower mold head (223) is annular and is located on the outer periphery of the mold core (211) and can be slidably connected to the mold core (211).
3. The powder metallurgy side hole forming die according to claim 2, characterized in that: The side mold (222) is provided with a connecting hole for the hole-forming shaft (2221) to pass through, and a limiting groove is provided on the outer periphery of the connecting hole. The hole-forming shaft (2221) is provided with a limiting ring (22211) adapted to the limiting hole, and the limiting ring (22211) is rotatably connected to the limiting groove. The hole-forming shaft (2221) is provided with a first screw rod (22212) at one end away from the mold core (211), and a first threaded hole is provided on a side of the lower mold frame (22) close to the first screw rod (22212), and the first screw rod (22212) is threadedly connected to the first threaded hole. The mold core (211) is provided with an axial groove adapted to the hole-forming shaft (2221), and the end of the hole-forming shaft (2221) close to the mold core (211) can extend into the axial groove.
4. The powder metallurgy side hole forming die according to claim 1, characterized in that: The top of the lower mold frame (22) is flush with the top plate (23), a push block (231) is slidably connected to the top plate (23), and a fifth driving component capable of driving the push block (231) to slide forward and backward is arranged on the top plate (23).
5. The powder metallurgy side hole forming die according to claim 4, characterized in that: The push block (231) is provided with a ventilation cavity, and the push block (231) is provided with a partition (23113) capable of dividing the ventilation cavity into an air inlet cavity (23111) and an air outlet cavity (23112). The push block (231) comprises a left side plate and a right side plate, and two ends of the partition (23113) are respectively connected to the left side plate and the right side plate. The air inlet cavity (23111) is provided with an air inlet on a side close to the top plate (23), and the air outlet cavity (23112) is provided with an air outlet on a side close to the top plate (23). The mold frame A cooling fan (5) is arranged on one side of the mold frame (1), the cooling fan (5) comprising a cooling air outlet, the cooling air outlet being connected to the air inlet chamber (23111), a collecting box (4) is arranged on the other side of the mold frame (1), a connecting port is arranged on the collecting box (4), the connecting port is connected to the air outlet chamber (23112), an exhaust fan (41) is arranged on the collecting box (4), the exhaust fan (41) comprises an exhaust port and an exhaust port, the exhaust port is connected to the collecting box (4), and a filter is arranged between the exhaust port and the connecting port.
6. The powder metallurgy side hole forming die according to claim 5, characterized in that: An opening (2313) is provided on the side wall of the air inlet chamber (23111), the air cooler (5) is connected to the opening (2313), an adjustment groove (2312) is provided on one side of the push block (231) close to the opening (2313), a strip groove connected to the adjustment groove (2312) is provided on the side wall of the air inlet chamber (23111), the strip groove extends from one end of the push block (231) close to the top plate (23) to one end away from the top plate (23), an adjustment block (23121) is slidably connected in the strip groove, and the two ends of the adjustment block (23121) are respectively The windshield (231112) is fixedly connected to the adjusting block (23121) in the air inlet cavity (23111) and is capable of shielding the opening (2313). A top cover is arranged on the top of the air inlet cavity (23111). A spring is arranged on the top cover and is capable of pressing the windshield (231112) down to below the opening (2313). The top plate (23) is provided with a resisting block (234) which can resist the adjusting block (23121) to lift the windshield (231112).
7. The powder metallurgy side hole forming die according to claim 6, characterized in that: The stop block (234) comprises an adjusting inclined surface (2341) which gradually rises from front to back.
8. The powder metallurgy side hole forming die according to claim 4, characterized in that: The fifth driving assembly comprises a second screw rod (2322), a first connecting block (232) fixedly connected to the top plate (23), a motor (2321) fixedly connected to the first connecting block (232), an output end of the motor (2321) fixedly connected to the second screw rod (2322), an end of the second screw rod (2322) away from the motor (2321) rotatably connected to the mold frame (1), a second threaded hole is provided on the push block (231), the second screw rod (2322) is threadedly connected to the second threaded hole, a second connecting block (233) fixedly connected to the top plate (23), a guide rod (2331) parallel to the second screw rod (2322) fixedly connected to the second connecting block (233), and the push block (231) is slidably connected to the guide rod (2331).
9. The powder metallurgy side hole forming die according to claim 1, characterized in that: The first drive assembly comprises two first hydraulic cylinders (6), the two first hydraulic cylinders (6) are symmetrically arranged on the lower shell (2), the lower mold frame (22) is provided with two second clearance holes, the output ends of the two first hydraulic cylinders (6) respectively pass through the two second clearance holes and are connected to the two side molds (222), the second drive assembly comprises a second hydraulic cylinder (7) fixedly connected to the bottom plate (21), the output end of the second hydraulic cylinder (7) is fixedly connected to the lower mold head (223), the third drive assembly comprises a third hydraulic cylinder (8) fixedly connected to the mold frame (1), the output end of the third hydraulic cylinder (8) is fixedly connected to the upper mold frame (3), and the fourth drive assembly comprises a fourth hydraulic cylinder (9) fixedly connected to the upper mold frame (3), the output end of the fourth hydraulic cylinder (9) is fixedly connected to the upper mold head (31).
Citation Information
Cited By
High-precision continuous pressing forming device and method for powder metallurgy blank with inner sinking groove