Thin-wall waveguide tube butt welding device and method

Through the design of the thin-wall waveguide butt welding device, combined with the boss stop, pin screw and support tool assembly, the problem of poor deformation and positioning accuracy in manual welding of thin-wall waveguide is solved, and high-precision welding molding is achieved.

CN119077079APending Publication Date: 2024-12-06BEIJING INST OF RADIO MEASUREMENT
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411595317.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-11
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

During manual welding of thin-walled waveguides, thin-walled pipe fittings are prone to deform, resulting in poor positioning accuracy and cannot meet the high-precision requirements.

Method used

A thin-wall waveguide butt welding device is designed, including a thin-wall waveguide assembly and a supporting tool assembly. Through the combination of boss stops, pin screw positioning holes and support tool assembly, high-precision positioning and deformation control are achieved, and manual Flame brazing method for welding.

Benefits of technology

High-precision butt welding of thin-wall waveguides is realized, reducing the risk of deformation during welding, and welding forming that meets the requirements of high precision.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119077079A_ABST
    Figure CN119077079A_ABST
Patent Text Reader

Abstract

The invention discloses a thin-wall waveguide tube butt welding device and method.The device comprises a thin-wall waveguide tube assembly and a supporting tool assembly, the thin-wall waveguide tube assembly is formed by combining and assembling a left-side waveguide tube, a right-side waveguide tube and a pin screw, and a boss spigot and a pin positioning hole are formed in the left-side waveguide tube; the right waveguide tube is provided with a butt joint spigot and a pin screw positioning hole; the boss seam allowance is in clearance fit with the butt joint seam allowance, and a pin screw penetrates through a pin positioning hole and a pin screw positioning hole to be connected with the left waveguide tube and the right waveguide tube in a fastening mode. The supporting tool assemblies are symmetrically arranged on the two sides of the thin-wall waveguide tube assembly and comprise fixed baffles, adjustable baffles, top plates, double-end studs and nuts, the fixed baffles and the adjustable baffles are used for supporting the two sides of the left-side waveguide tube and the two sides of the right-side waveguide tube, the double-end studs penetrate through the top plates, the fixed baffles and the adjustable baffles, and the two ends of each double-end stud are fixed through the nuts. According to the invention, high-precision positioning and deformation control of butt welding of the thin-wall waveguide tube can be realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of high-difficulty manual flame brazing forming and deformation control, and in particular relates to a thin-wall waveguide butt welding device and method. Background Art

[0002] At present, in the process of butt welding multiple sections of thin-walled waveguide tubes to form waveguide products, manual welding is more economical than welding methods such as vacuum furnace brazing. However, since thin-walled pipes are easily deformed by heat, thin-walled waveguide tubes are very prone to deformation and poor positioning accuracy during the manual welding process, which cannot meet the high-precision requirements of thin-walled waveguide products. Summary of the invention

[0003] The purpose of the present invention is to provide a thin-wall waveguide butt welding device and method, which can perform high-precision positioning and deformation control of thin-wall waveguide butt welding, and realize thin-wall waveguide welding forming with high-precision requirements.

[0004] In order to achieve the above-mentioned purpose, one aspect of the present invention provides a thin-walled waveguide butt welding device, including a thin-walled waveguide assembly and a supporting tooling assembly, wherein the thin-walled waveguide assembly is assembled by a left waveguide, a right waveguide and a pin screw assembly, wherein a boss stop and pin positioning holes separated on both sides of the boss stop are provided on the butt surface of the left waveguide, and a butt stop and pin screw positioning holes are provided on the butt surface of the right waveguide, wherein the butt stop is an intermittent boss stop, and gaps are reserved at the four corners to form a gap, and the pin screw positioning holes are separated on both sides of the butt stop; The boss stopper and the docking stopper are matched with each other to realize the stopper positioning between the left waveguide and the right waveguide. The pin screw passes through the pin positioning hole and the pin screw positioning hole to fasten and connect the left waveguide and the right waveguide. There are multiple supporting tooling components, which are symmetrically arranged on both sides of the thin-walled waveguide tube component, including a fixed baffle, an adjustable baffle, a top plate, studs and nuts. The fixed baffle and the adjustable baffle are used to support both sides of the left waveguide tube and the right waveguide tube. The top plate is used to connect the fixed baffle and the adjustable baffle. The studs pass through the top plate, the fixed baffle and the adjustable baffle, and are fixed at both ends by nuts.

[0005] Preferably, a first oblong hole, a side limit hole, and a bottom limit hole are provided on the fixed baffle plate, and a second oblong hole, a side limit platform, and a bottom limit platform are provided on the adjustable baffle plate. The side limit platform is plugged into the side limit hole, and the bottom limit platform is plugged into the bottom limit hole. A through hole is provided on the top plate, and the stud bolt passes through the through hole and the first oblong hole and the second oblong hole, thereby fastening the top plate to the fixed baffle plate and the adjustable baffle plate.

[0006] Preferably, the pin screw comprises a pin portion and a threaded portion, the pin portion is longer than the threaded portion, the pin positioning hole is used to position the pin portion, and the pin screw positioning hole is used to position the pin portion and the threaded portion.

[0007] Preferably, the fixed baffle, the adjustable baffle and the top plate are all made of machinable ceramics.

[0008] Preferably, the boss stopper and the docking stopper have a clearance fit, and the clearance is between 0.01-0.02 mm.

[0009] Another aspect of the present invention provides a method for butt welding a thin-walled waveguide tube, wherein the thin-walled waveguide tube is butt welded using the above-mentioned device, and the method comprises: Step S1: machining a thin-wall waveguide blank to form a boss stop and a pin positioning hole to form a left waveguide; Step S2: machining the thin-walled waveguide blank into intermittent boss stops and pin screw positioning holes to form a right waveguide; Step S3: Assemble and tighten the left waveguide and the right waveguide with pin screws to form a thin-wall waveguide assembly; Step S4: symmetrically placing fixed baffles at both ends of the thin-walled waveguide assembly, and screwing and fastening the adjustable baffles, the top plate, the studs, and the nuts to form a symmetrically supported support fixture assembly; Step S5: butt-welding the thin-walled waveguide assembly by manual flame brazing to complete the welding and forming of the thin-walled waveguide. After the welding is completed, the supporting tooling assembly is removed.

[0010] The thin-walled waveguide butt welding device and method according to the above aspects of the present invention can perform high-precision positioning and deformation control of thin-walled waveguide butt welding, thereby achieving high-precision thin-walled waveguide welding forming. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] In order to more clearly illustrate the technical solution of the present invention, the following briefly introduces the drawings used in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work: Figure 1 2 is a schematic structural diagram of a thin-wall waveguide butt welding device according to an embodiment of the present invention; Figure 2 is a schematic structural diagram of a thin-wall waveguide assembly according to an embodiment of the present invention; Figure 3 It is a schematic diagram of the structure of the left waveguide and the docking surface of an embodiment of the present invention; Figure 4It is a schematic diagram of the structure of the right waveguide and the docking surface of an embodiment of the present invention; Figure 5 is a schematic structural diagram of a pin screw according to an embodiment of the present invention; Figure 6 is a schematic structural diagram of a supporting tooling assembly according to an embodiment of the present invention; Figure 7 Detailed description of the invention is provided in detail. DETAILED DESCRIPTION

[0012] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0013] One embodiment of the present invention provides a thin-wall waveguide butt welding device, such as Figure 1 As shown, the thin-wall waveguide butt welding device of the embodiment of the present invention comprises a thin-wall waveguide assembly 1 and a supporting tooling assembly 2. Figure 2-5 As shown, the thin-walled waveguide tube assembly 1 is assembled by a left waveguide tube 11, a right waveguide tube 12 and a pin screw 13. The docking surface of the left waveguide tube 11 is provided with a boss stop 112 and a pin positioning hole 111, which are symmetrically distributed and evenly stressed. The docking surface of the right waveguide tube 12 is provided with a docking stop 122 and a pin screw positioning hole 121. The docking stop 122 is an intermittent boss stop, and gaps are reserved at the four corners to form a gap, which is convenient for prefabricated solder and solder flow, fully ensuring the welding strength, and also avoiding over-positioning and assembly difficulties when docking with the left waveguide tube 11, and deformation affecting the docking position accuracy. The pin screw positioning holes 121 are separated on both sides of the docking stop 122, fully ensuring high positioning accuracy.

[0014] The pin screw 13 includes a pin portion 131 and a threaded portion 132, wherein the pin portion 131 is longer than the threaded portion 132. The pin screw 13 passes through the pin positioning hole 111 and the pin screw positioning hole 121, and is used to fasten and connect the left waveguide 11 and the right waveguide 12. The pin positioning hole 111 is used to position the pin portion 131, and the pin screw positioning hole 121 is a combination of a positioning hole and a threaded hole, with a positioning hole first and a threaded hole later, thereby positioning both the pin portion 131 and the threaded portion 132. The boss stop 112 and the docking stop 122 are clearance-matched to achieve stop positioning between the left waveguide 11 and the right waveguide 12, and the clearance is controlled between 0.01-0.02mm. For 1mm thin-walled waveguide products, the thinnest size of the boss stop 112 and the docking stop 122 can be 0.5mm, or it can be appropriately enlarged to set the stop thickness to not less than 0.5mm. A 0.5mm wide gap is reserved at the four corners of the docking stop 122, which can also be adjusted appropriately according to the situation. The pin positioning hole 111 and the pin screw positioning hole 121 ensure that the two sides are accurately positioned when fastened by the pin screw 13, and the fastening purpose can be achieved. Thereby, a double insurance positioning method is realized. The stopper positioning can ensure the positioning accuracy of the waveguide cavity docking, and is also convenient for pre-welding of solder, avoiding the direct accumulation of solder flow at the docking interface in the case of direct docking. In addition, due to the low welding strength of the thin-walled weld surface, the increase of the stopper also increases the spreading area of ​​the solder, increases the welding strength, reduces the difficulty of solder control, and improves the docking accuracy in the cavity. In addition, the pin screw positioning reduces the deformation of the thin-walled welding deformation, which causes the stopper deformation and affects the welding positioning and deformation accuracy. In addition, the symmetrical arrangement of the force application points greatly reduces the impact of welding deformation.

[0015] like Figure 6 As shown, the support fixture assembly 2 includes a fixed baffle 21, an adjustable baffle 22, a top plate 23, a stud 24, and a nut 25. The fixed baffle 21 and the adjustable baffle 22 are used to support both sides of the left waveguide 11 and the right waveguide 12. The top plate 23 is used to connect the fixed baffle 21 and the adjustable baffle 22. The stud 24 passes through the top plate 23, the fixed baffle 21, and the adjustable baffle 22, and the two ends are fixed by nuts 25. During welding, on the welding workbench, the fixed baffle 21 is first fixed, the thin-walled waveguide is placed, and the adjustable baffle 22 is installed on the right side, and is fastened and fixed by the top plate 23, the stud 24, and the nut 25. The support fixture assembly 2 is symmetrically arranged on both sides of the thin-walled waveguide assembly 1. By fixing the support position of the thin-walled waveguide assembly 1, the risk of large-angle deformation during welding is reduced, and the straightness and verticality requirements of the welding waveguide are ensured. The fixed baffle 21, the adjustable baffle 22, and the top plate 23 are all made of machinable ceramics to prevent the heat concentration of the supporting tooling assembly 2 from affecting the waveguide welding deformation. The machinable ceramic material itself has a low thermal expansion coefficient and high thermal stability, and has the advantages of high temperature resistance and high hardness, and is suitable for manual welding and other welding auxiliary tooling.

[0016] like Figure 7As shown, the fixed baffle 21 is provided with a first oblong hole 211, a side end limiting hole 212, and a bottom surface limiting hole 213, and the adjustable baffle 22 is provided with a second oblong hole 221, a side end limiting platform 222, and a bottom surface limiting platform 223, the side end limiting platform 222 cooperates with the side end limiting hole 212, and the bottom surface limiting platform 223 cooperates with the bottom surface limiting hole 213, and a through hole 231 is provided on the top plate 23, and the stud 24 passes through the through hole 231 and the first oblong hole 211 and the second oblong hole 221, so as to fasten the top plate 23 to the fixed baffle 21 and the adjustable baffle 22.

[0017] Specifically, the side end limit table 222 is plugged into the side end limit hole 212 to perform high-precision clearance matching, and the tolerance gap is 0.01-0.02mm, which is used to ensure the stability of the fixed baffle 21 and the adjustable baffle 22 during assembly and use, and the external force of the wall affects the welding process. The two sides of the fixed baffle 21 and the adjustable baffle 22 are in contact with the outer wall of the waveguide, the bottom surface of the top plate 23 is in contact with the upper surface of the waveguide, and the upper side of the inner wall of the fixed baffle 21 is in contact with the lower side of the waveguide, fixing the welding position to ensure welding in a natural state. The bottom surface limit table 223 is plugged into the bottom surface limit hole 213 to ensure that the support fixture assembly 2 does not rotate and is perpendicular to the workbench, ensuring the verticality and parallelism of the waveguide during the assembly welding process. The two side support fixture assemblies 2 are symmetrically arranged on both sides of the thin-walled waveguide assembly 1 to avoid uneven force due to welding deformation. The number of support fixture assemblies 2 used can be adjusted according to the length of the waveguide to ensure the position accuracy and size requirements, but at least they need to be arranged on both sides of the weld and the end of the waveguide.

[0018] An embodiment of the present invention further provides a method for butt welding a thin-walled waveguide tube, wherein the thin-walled waveguide tube is butt welded using the above-mentioned device, and the method comprises the following steps: Step S1: Processing a thin-walled waveguide blank to form a boss stop 112 and a pin positioning hole 111 of, for example, 0.5 mm, to form a left waveguide 11. The thin-walled waveguide blank is formed by a method not limited to machining, drawing, extrusion, or other part forming methods. Step S2: processing the thin-walled waveguide blank into, for example, 0.5 mm intermittent boss stop 122 and pin screw positioning hole 121 to form the right waveguide 12. The thin-walled waveguide blank is formed by a method not limited to machining, drawing, extrusion or other part forming methods. Step S3: Assemble and tighten the left waveguide 11 and the right waveguide 12 with the pin screws 13 to form a thin-walled waveguide assembly 1; Step S4: placing fixed baffles 21 at symmetrical positions at both ends of the thin-walled waveguide assembly 1, and screwing and fastening the adjustable baffles 22, the top plate 23, the studs 24, and the nuts 25 to form a symmetrically supported support fixture assembly 2; Step S5: pre-place solder wire at the weld position and fix it by laser spot welding, then butt weld the thin-walled waveguide assembly 1 by manual flame brazing to complete the welding of the thin-walled waveguide. After welding is completed, remove the support fixture assembly 2.

[0019] After welding is completed, the welded thin-walled waveguide tube can be placed on the processing equipment, and the pin screw connection at the joint can be removed by wire cutting or CNC processing to form a long straight waveguide tube with a uniform appearance, or it can be retained according to design requirements.

[0020] In summary, the thin-walled waveguide butt welding device and method of the embodiment of the present invention is designed to combine thin-walled stop butt welding and pin screw fastening on the basis of conventional stop positioning. Before welding, the thin-walled stop and the pin screws on both sides are fastened to ensure that the deformation risk of thin-walled parts is reduced when the internal stress is concentrated and deformed during the welding process. In order to greatly reduce the deformation of thin-walled parts, a support tooling assembly is added outside the heat-affected zone of the manual welding thin-walled waveguide as a thin-walled waveguide manual welding placement and deformation control device, which not only achieves the purpose of easy welding of the exposed weld position of the thin-walled waveguide, but also supports and fixes the shape of the waveguide without affecting the welding process, thereby reducing the risk of thermal deformation of the waveguide.

[0021] The thin-walled waveguide butt welding device and method of the embodiment of the present invention can be applied to thin-walled waveguides with a wall thickness of ≥1mm, can achieve high-precision positioning of thin-walled waveguide butt welding, solve the problems of thin-walled waveguide manual welding support and natural deformation welding control, and meet the straightness and verticality accuracy requirements of parts after welding. The present invention can be applied to the butt welding needs of various thin-walled waveguide products with complex waveguide caliber, length or inner cavity, special shape, etc., and can be extended to the butt welding of multiple sections of waveguides, not limited to one weld, and the middle section is supported and positioned by the support tooling assembly of the present invention.

[0022] The above description is only by way of illustration of certain exemplary embodiments of the present invention. It is undoubted that those skilled in the art can modify the described embodiments in various ways without departing from the spirit and scope of the present invention. Therefore, the above drawings and descriptions are illustrative in nature and should not be construed as limiting the scope of protection of the claims of the present invention.

Claims

1. A thin-wall waveguide butt welding device, It is characterized in that It includes a thin-walled waveguide assembly and a supporting tooling assembly. The thin-walled waveguide assembly is assembled by a left waveguide, a right waveguide and a pin screw. The docking surface of the left waveguide is provided with a boss stop and pin positioning holes separated on both sides of the boss stop. The docking surface of the right waveguide is provided with a docking stop and a pin screw positioning hole. The docking stop is an intermittent boss stop, and gaps are reserved at the four corners to form a gap. The pin screw positioning holes are separated on both sides of the docking stop. The boss stopper and the docking stopper are matched with each other to realize the stopper positioning between the left waveguide and the right waveguide. The pin screw passes through the pin positioning hole and the pin screw positioning hole to fasten and connect the left waveguide and the right waveguide. There are multiple supporting tooling components, which are symmetrically arranged on both sides of the thin-walled waveguide tube component, including a fixed baffle, an adjustable baffle, a top plate, studs and nuts. The fixed baffle and the adjustable baffle are used to support both sides of the left waveguide tube and the right waveguide tube. The top plate is used to connect the fixed baffle and the adjustable baffle. The studs pass through the top plate, the fixed baffle and the adjustable baffle, and are fixed at both ends by nuts.

2. The device according to claim 1, It is characterized in that The fixed baffle is provided with a first oblong hole, a side limit hole, and a bottom limit hole; the adjustable baffle is provided with a second oblong hole, a side limit platform, and a bottom limit platform; the side limit platform is plugged into the side limit hole, and the bottom limit platform is plugged into the bottom limit hole; a through hole is provided on the top plate, and the stud passes through the through hole and the first oblong hole and the second oblong hole, thereby fastening the top plate to the fixed baffle and the adjustable baffle.

3. The device according to claim 1 or 2, It is characterized in that The pin screw comprises a pin portion and a threaded portion, the pin portion is longer than the threaded portion, the pin positioning hole is used to position the pin portion, and the pin screw positioning hole is used to position the pin portion and the threaded portion.

4. The device according to claim 1 or 2, It is characterized in that The fixed baffle, adjustable baffle and top plate are all machined from machinable ceramic.

5. The device according to claim 1 or 2, It is characterized in that The boss stop and the docking stop have a clearance fit, with the clearance being between 0.01-0.02mm.

6. A method for butt welding of thin-walled waveguide tubes, It is characterized in that Butt welding a thin-walled waveguide tube using the device described in any one of claims 1 to 5, the method comprising: Step S1: machining a thin-wall waveguide blank to form a boss stop and a pin positioning hole to form a left waveguide; Step S2: machining the thin-walled waveguide blank into intermittent boss stops and pin screw positioning holes to form a right waveguide; Step S3: Assemble and tighten the left waveguide and the right waveguide with pin screws to form a thin-wall waveguide assembly; Step S4: symmetrically placing fixed baffles at both ends of the thin-walled waveguide assembly, and screwing and fastening the adjustable baffles, the top plate, the studs, and the nuts to form a symmetrically supported support fixture assembly; Step S5: butt-welding the thin-walled waveguide assembly by manual flame brazing to complete the welding and forming of the thin-walled waveguide. After the welding is completed, the supporting tooling assembly is removed.