3D model printing forming method

By printing layer by layer in a 3D printer and degreasing and sintering, the problem of insufficient structural stability in 3D model printing and forming technology is solved, and the stability and quality of the product are improved.

CN119078175APending Publication Date: 2024-12-06KUNSHAN HAOMITE TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411231881.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

In the existing 3D model printing and forming technology, the structural stability of the molded products is insufficient, resulting in inconsistent with the actual product and initial modeling, affecting the product quality and service life.

Method used

By establishing a three-dimensional model in a 3D printer, preparing resin materials and adding binder, printing layer by layer to form intermediate molding materials, and printing continues to be carried out after curing, and finally degreasing and sintering treatment are carried out to form a stable 3D model product.

Benefits of technology

It effectively improves the molding stability of printing materials, avoids the inconsistency of appearance caused by product deformation, and improves product quality and service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119078175A_ABST
    Figure CN119078175A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of 3D model printing, and particularly relates to a 3D model printing forming method which comprises the following steps that S1, a 3D model of an object needing to be printed is established, and a 3D model printing path is set through the 3D model; s2, a printing raw material is prepared, a printing material used for the to-be-printed object is obtained, and the printing material used for the to-be-printed object is added into a material groove in a 3D printer; s3, a 3D printer is started, a printing material used for heating and melting the to-be-printed article is conveyed to a 3D printing head, and the 3D printer automatically extrudes the printing material onto a movable working platform of the 3D printer according to model information and three-dimensional model data of the imported article and a 3D model printing path; in this way, the stability of the printing material in the forming process can be effectively improved, and the situation that due to deformation, an actual product is inconsistent with an initially-modeled product in appearance, and the quality and the service life of the product are affected is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of 3D model printing, and in particular to a 3D model printing and forming method. Background Art

[0002] 3D printing is an advanced technology for manufacturing three-dimensional objects. Compared with traditional industrial manufacturing, it does not require molds or large production lines. Simply put, 3D printing is to build objects by stacking materials layer by layer on a machine according to a computer-generated three-dimensional model. The working principle of a 3D printer is to cut the digital model into thin slices, then print these slices layer by layer, stack them layer by layer, and finally form a complete physical object. It is easy to operate. Just send the 3D model to the printer through computer software and select the appropriate material, and the printer will be able to automatically complete the printing process. It is often used to make models in the fields of mold manufacturing and industrial design, and then gradually used for the direct manufacturing of some products. There are already parts printed using this technology. This technology has been used in jewelry, footwear, industrial design, architecture, engineering and construction (AEC), automobiles, aerospace, dental and medical industries, education, geographic information systems, civil engineering and other fields.

[0003] In the existing 3D model printing and molding technology, the structural stability of the molded product needs to be further improved. During the printing process of the molded product, the lack of stability can easily lead to inconsistency between the actual product and the initial modeled product appearance, affecting the quality and service life of the product. Therefore, the present invention provides a 3D model printing and molding method. Summary of the invention

[0004] The purpose of the present invention is to provide a 3D model printing method to solve the above problems raised in the above background technology.

[0005] To achieve the above object, the present invention provides the following technical solution: a 3D model printing method, comprising the following steps: S1: Establish a three-dimensional model of the object to be printed, set a 3D model printing path through the three-dimensional model, and import the three-dimensional model data and the corresponding 3D model printing path into the 3D printer; S2: preparing printing raw materials to obtain printing materials for the object to be printed, and adding the printing materials for the object to be printed into a material tank in the 3D printer; S3: Turn on the 3D printer, heat and melt the printing material for the object to be printed and deliver it to the 3D printing head. The 3D printer automatically extrude the printing material onto its movable working platform according to the imported 3D model data of the object and the 3D model printing path, thereby obtaining a first intermediate molding material. S4: After the first intermediate molding material is solidified, the upper layer of the first intermediate molding material is continuously printed to obtain the second intermediate molding material. After the second intermediate molding material is solidified, the upper layer of the second intermediate molding material is continuously printed, and so on, to finally obtain the desired three-dimensional solid green body of the printed object; S5: Degreasing and carbonizing the obtained three-dimensional solid green body of the printed object to obtain the desired 3D model product.

[0006] Preferably, in step S2, the printing material used for the object to be printed is resin, and a binder is mixed into the resin.

[0007] Preferably, in step S5, the method for degreasing and carbonizing the obtained three-dimensional solid green body of the printed object is to place the three-dimensional solid green body of the printed object into a degreasing furnace for a primary degreasing treatment, and then perform a secondary degreasing treatment on the three-dimensional solid green body of the printed object after the primary degreasing treatment by high-temperature sintering, so as to finally obtain the desired 3D model product.

[0008] Preferably, the binder is at least one of paraffin wax, polyethylene wax, polypropylene, stearic acid, polystyrene, aniline, boric acid, and polyethylene glycol.

[0009] Preferably, the three-dimensional solid green body of the printed object is placed in a degreasing furnace for a degreasing treatment, and the degreasing is carried out in a catalytic degreasing furnace using concentrated nitric acid as a medium, the degreasing temperature is 90-110° C., and the degreasing time is 7-8 hours.

[0010] Preferably, the method of performing a secondary degreasing treatment on the three-dimensional solid green body of the printed object after the primary degreasing treatment by high-temperature sintering is to place the three-dimensional solid green body of the printed object after the primary degreasing treatment into a sintering furnace, perform sintering and degreasing by a step-by-step heating method, and cool down with the furnace after the heating is completed.

[0011] Preferably, the step-by-step heating method is as follows: heating to 800°C at a heating rate of 1°C / min to 10°C / min, and keeping warm for 2-3 hours; heating to 1000°C at a heating rate of 1°C / min to 4°C / min, and keeping warm for 2-3 hours; heating to 1100°C-1200°C at a heating rate of 0.5°C / min to 2°C / min, and keeping warm for 2-3 hours.

[0012] Preferably, the working platform is moved in the X and Y directions by means of a screw drive, and the 3D printing head is moved in the Z direction by means of a hydraulic cylinder or an electric push rod.

[0013] Compared with the prior art, the present invention has the following beneficial effects: During the 3D model printing process, the 3D printer automatically extrude the printing material onto its movable working platform according to the model information based on the imported 3D model data of the object and the 3D model printing path, to obtain a first intermediate molding material. After the first intermediate molding material is solidified, the upper layer of the first intermediate molding material is continued to be printed to obtain a second intermediate molding material. After the second intermediate molding material is solidified, the upper layer of the second intermediate molding material is continued to be printed, and so on, to finally obtain the desired three-dimensional solid green body of the printed object. The obtained three-dimensional solid green body of the printed object is degreased and carbonized to obtain the desired 3D model product. In this way, the stability of the printing material molding process can be effectively improved, and the situation in which the actual product is inconsistent with the initial modeling product appearance due to deformation, which affects the quality and service life of the product, can be avoided. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a flow chart of the steps of the present invention. DETAILED DESCRIPTION

[0015] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0016] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "top / bottom" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.

[0017] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "mounted / connected", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. Example

[0018] See also Figure 1The present invention provides a technical solution: a 3D model printing method, comprising the following steps: S1: Building a three-dimensional model of the object to be printed. The three-dimensional model can be built using existing conventional three-dimensional model software. The 3D model printing path is set through the three-dimensional model, and the three-dimensional model data and the corresponding 3D model printing path are imported into the 3D printer; S2: preparing printing raw materials to obtain printing materials for the object to be printed, and adding the printing materials for the object to be printed into a material tank in the 3D printer; S3: Turn on the 3D printer, heat and melt the printing material for the object to be printed and deliver it to the 3D printing head. The 3D printer automatically extrude the printing material onto its movable working platform according to the imported 3D model data of the object and the 3D model printing path, thereby obtaining a first intermediate molding material. S4: After the first intermediate molding material is solidified, the upper layer of the first intermediate molding material is continuously printed to obtain the second intermediate molding material. After the second intermediate molding material is solidified, the solidification time is set according to the properties of the printing material, and the upper layer of the second intermediate molding material is continuously printed, and so on, to finally obtain the desired three-dimensional solid green body of the printed object; S5: Degreasing and carbonizing the obtained three-dimensional solid green body of the printed object to obtain the desired 3D model product.

[0019] In step S2 of the invention, the printing material used for the object to be printed is resin, and a binder is mixed into the resin.

[0020] In step S5 of the invention, the method for degreasing and carbonizing the obtained three-dimensional solid green body of the printed object is to place the three-dimensional solid green body of the printed object into a degreasing furnace for a primary degreasing treatment, and then perform a secondary degreasing treatment on the three-dimensional solid green body of the printed object after the primary degreasing treatment by high-temperature sintering, so as to finally obtain the desired 3D model product.

[0021] The binder of the invention is at least one of paraffin wax, polyethylene wax, polypropylene, stearic acid, polystyrene, aniline, boric acid and polyethylene glycol.

[0022] The method of placing the printed three-dimensional solid green body into a degreasing furnace for a degreasing treatment is to degrease it in a catalytic degreasing furnace using concentrated nitric acid as a medium, the degreasing temperature is 90-110°C, and the degreasing time is 7-8h.

[0023] The method of performing a secondary degreasing treatment on the three-dimensional solid green body of the printed object after the primary degreasing treatment by high-temperature sintering is to put the three-dimensional solid green body of the printed object after the primary degreasing treatment into a sintering furnace, perform sintering and degreasing by a step-by-step heating method, and cool down with the furnace after the heating is completed.

[0024] The step-by-step heating method of the invention is specifically as follows: heating to 800°C at a heating rate of 1°C / min to 10°C / min, and keeping warm for 2-3 hours; heating to 1000°C at a heating rate of 1°C / min to 4°C / min, and keeping warm for 2-3 hours; heating to 1100°C-1200°C at a heating rate of 0.5°C / min to 2°C / min, and keeping warm for 2-3 hours.

[0025] The working platform of the invention is moved in the X direction and the Y direction by means of a screw drive, and the 3D printing head of the invention is moved in the Z direction by means of a hydraulic cylinder or an electric push rod drive.

[0026] The complete 3D model printing process is: A three-dimensional model of an object to be printed is established, a 3D model printing path is set through the three-dimensional model, the three-dimensional model data and the corresponding 3D model printing path are imported into a 3D printer, a binder is added to a resin mixture and placed in a material tank in the 3D printer, the binder is at least one of paraffin wax, polyethylene wax, polypropylene, stearic acid, polystyrene, aniline, boric acid, and polyethylene glycol, the 3D printer is turned on, and the printing material for the object to be printed after heating and melting is transported to the 3D printing head, and the 3D printer automatically extrude the printing material onto its movable working platform according to the imported three-dimensional model data of the object and the 3D model printing path according to the model information, to obtain a first intermediate molding material, and the first intermediate molding material is to be molded. After the solidification of an intermediate molding material is completed, the upper layer of the first intermediate molding material is continuously printed to obtain a second intermediate molding material. After the solidification of the second intermediate molding material is completed, the upper layer of the second intermediate molding material is continuously printed, and so on, finally obtaining the desired three-dimensional solid green body of the printed object, and the obtained three-dimensional solid green body of the printed object is degreased once in a catalytic degreasing furnace using concentrated nitric acid as a medium, the degreasing temperature is 100°C, and the degreasing time is 7h. The three-dimensional solid green body of the printed object after the first degreasing treatment is placed in a sintering furnace, and sintered and degreased by a step-by-step heating method, specifically, heating to 800°C at a heating rate of 10°C / min, and keeping warm for 3h; heating to 1000°C at a heating rate of 4°C / min, and keeping warm for 3h; heating to 1200°C at a heating rate of 2°C / min, and keeping warm for 3h. After the insulation is completed, the temperature is lowered with the furnace to obtain the desired 3D model product.

[0027] Working principle: During the 3D model printing process, the 3D printer automatically extrude the printing material onto its movable working platform according to the model information based on the imported 3D model data of the object and the 3D model printing path, to obtain the first intermediate molding material. After the first intermediate molding material is solidified, the upper layer of the first intermediate molding material is continuously printed to obtain the second intermediate molding material. After the second intermediate molding material is solidified, the upper layer of the second intermediate molding material is continuously printed, and so on, to finally obtain the desired three-dimensional solid green body of the printed object. The obtained three-dimensional solid green body of the printed object is degreased and carbonized to obtain the desired 3D model product. In this way, the stability of the printing material molding process can be effectively improved, and the situation that the actual product is inconsistent with the initial modeling product appearance due to deformation, which affects the quality and service life of the product, can be avoided.

[0028] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. For those skilled in the art, it is obvious that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention; therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is limited by the attached claims rather than the above description. Therefore, it is intended to include all changes within the meaning and scope of the equivalent elements of the claims in the present invention, and any figure marks in the claims should not be regarded as limiting the claims involved.

[0029] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A 3D model printing method, characterized in that: The following steps are involved: S1: Establish a three-dimensional model of the object to be printed, set a 3D model printing path through the three-dimensional model, and import the three-dimensional model data and the corresponding 3D model printing path into the 3D printer; S2: preparing printing raw materials to obtain printing materials for the object to be printed, and adding the printing materials for the object to be printed into a material tank in the 3D printer; S3: Turn on the 3D printer, heat and melt the printing material for the object to be printed and deliver it to the 3D printing head. The 3D printer automatically extrude the printing material onto its movable working platform according to the imported 3D model data of the object and the 3D model printing path, thereby obtaining a first intermediate molding material. S4: After the first intermediate molding material is solidified, the upper layer of the first intermediate molding material is continuously printed to obtain the second intermediate molding material. After the second intermediate molding material is solidified, the upper layer of the second intermediate molding material is continuously printed, and so on, to finally obtain the desired three-dimensional solid green body of the printed object; S5: Degreasing and carbonizing the obtained three-dimensional solid green body of the printed object to obtain the desired 3D model product.

2. The 3D model printing method according to claim 1, characterized in that: In step S2, the printing material used for the object to be printed is resin, and a binder is mixed into the resin.

3. The 3D model printing method according to claim 2, characterized in that: In step S5, the method for degreasing and carbonizing the obtained three-dimensional solid green body of the printed object is to place the three-dimensional solid green body of the printed object into a degreasing furnace for a primary degreasing treatment, and then perform a secondary degreasing treatment on the three-dimensional solid green body of the printed object after the primary degreasing treatment by high-temperature sintering, so as to finally obtain the desired 3D model product.

4. The 3D model printing method according to claim 2, characterized in that: The binder is at least one of paraffin wax, polyethylene wax, polypropylene, stearic acid, polystyrene, aniline, boric acid and polyethylene glycol.

5. The 3D model printing method according to claim 3, characterized in that: The method of placing the printed three-dimensional solid green body into a degreasing furnace for a degreasing treatment is to degrease it in a catalytic degreasing furnace using concentrated nitric acid as a medium, the degreasing temperature is 90-110°C, and the degreasing time is 7-8h.

6. The 3D model printing method according to claim 3, characterized in that: The method of performing a secondary degreasing treatment on the three-dimensional solid green body of the printed object after the primary degreasing treatment by high-temperature sintering is to put the three-dimensional solid green body of the printed object after the primary degreasing treatment into a sintering furnace, perform sintering and degreasing by a step-by-step heating method, and cool down with the furnace after the heating is completed.

7. The 3D model printing method according to claim 6, characterized in that: The step-by-step heating method is specifically as follows: heating to 800°C at a heating rate of 1°C / min to 10°C / min, and keeping warm for 2-3 hours; heating to 1000°C at a heating rate of 1°C / min to 4°C / min, and keeping warm for 2-3 hours; heating to 1100°C-1200°C at a heating rate of 0.5°C / min to 2°C / min, and keeping warm for 2-3 hours.

8. The 3D model printing method according to claim 1, characterized in that: The working platform is driven by a screw to move in the X and Y directions, and the 3D printing head is driven by a hydraulic cylinder or an electric push rod to move in the Z direction.