Production process of difluoroethyl acetate

Difluoroethyl acetate was prepared by reacting 1,2,2-trichloro-1,1-difluoroethane with hydrogen using a composite catalyst in a tubular reactor, and the costly raw materials in the prior art were solved Problem, high-efficiency and low-cost production of difluoroethyl acetate has been achieved.

CN119080614APending Publication Date: 2024-12-06NANTONG BAOKAI CHEM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411176647.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The existing difluoroethyl acetate synthesis methods rely on expensive difluoroethanol, resulting in high production cost and complex process, and urgently need a new production process.

Method used

The crude product of 2-chloro-1,1-difluoroethane is prepared by reacting 1,2,2-trichloro-1,1-difluoroethane with hydrogen in a tubular reactor, and reacts with acetate. , difluoroethyl acetate is prepared by synergistic action of composite catalysts such as copper-zinc catalysts and palladium-carbon catalysts.

Benefits of technology

It significantly reduces raw material costs, simplifies the process flow, improves production efficiency, achieves high conversion and selectivity, avoids the use of expensive raw materials, and has mild reaction conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005010899200000021
    Figure BDA0005010899200000021
  • Figure BDA0005010899200000031
    Figure BDA0005010899200000031
Patent Text Reader

Abstract

The invention discloses a production process of difluoroethyl acetate, and relates to the technical field of chemical synthesis. When the difluoroethyl acetate is prepared, the copper-zinc catalyst is firstly prepared by using a coprecipitation method, and then the copper-zinc catalyst is mixed with the palladium-carbon catalyst to prepare the composite catalyst; filling the composite catalyst into a metal pipeline, and adjusting by using hydrogen and helium mixed gas to prepare a tubular reactor; the method comprises the following steps: mixing a raw material 1, 2, 2-trichloro-1, 1-difluoroethane with hydrogen, introducing the mixture into a tubular reactor, and carrying out catalytic hydrodechlorination to prepare a 2-chloro-1, 1-difluoroethane crude product; the 2-chloro-1, 1-difluoroethane crude product is rectified and purified and then reacts with acetate, and difluoroethyl acetate is prepared. The difluoroethyl acetate is prepared by adopting a novel synthesis route, the raw material conversion rate is high, the product selectivity is good, and the target product purity is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of chemical synthesis, in particular to a production process of difluoroethyl acetate. Background Art

[0002] With the development of new energy technology, lithium-ion batteries have gradually taken a leading position in the chemical power market. Electrolyte is an important component of lithium-ion batteries, affecting many of the main properties of the battery. Fluorine has strong electronegativity and weak polarity. Fluorinated solvents or fluorine-containing additives have the advantages of low melting point, high flash point, high oxidation decomposition voltage, and good wettability with electrode materials. Difluoroethyl acetate is an excellent electrolyte additive. In addition, difluoroethyl acetate can also be used in the synthesis of important intermediates such as new medicines, pesticides, functional materials, etc., and can be used to synthesize difluoroethanol and difluoroacetic acid. It has a wide range of applications, great market potential, and development value.

[0003] The existing methods for synthesizing difluoroethyl acetate mostly use difluoroethanol and acetyl chloride for preparation. Difluoroethanol is expensive and the preparation process is not worth the effort. There is an urgent need to develop a new production process for difluoroethyl acetate. Summary of the invention

[0004] The object of the present invention is to provide a production process of difluoroethyl acetate to solve the problems existing in the prior art.

[0005] In order to solve the above technical problems, the present invention provides the following technical solutions:

[0006] A production process of difluoroethyl acetate mainly comprises the following preparation steps: mixing 1,2,2-trichloro-1,1-difluoroethane and hydrogen and introducing them into a tubular reactor to react to obtain a crude 2-chloro-1,1-difluoroethane product; distilling and purifying the crude 2-chloro-1,1-difluoroethane product to obtain a 2-chloro-1,1-difluoroethane solution; reacting the 2-chloro-1,1-difluoroethane solution with acetate to obtain difluoroethyl acetate;

[0007] The tubular reactor comprises a metal pipeline and a composite catalyst.

[0008] As an optimization, the production process of difluoroethyl acetate mainly includes the following preparation steps:

[0009] (1) At 200-220°C, 3×10 5 Pa, mixing 1,2,2-trichloro-1,1-difluoroethane and hydrogen in a certain molar ratio and feeding them into a tubular reactor to obtain a crude 2-chloro-1,1-difluoroethane product;

[0010] (2) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with a solvent at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution;

[0011] (3) Under a nitrogen atmosphere, the acetate and the solvent are mixed uniformly in a mass ratio of 1:(2-3), heated to 115-125° C., stirred at a speed of 200-300 r / min, connected to a dry ice condenser, and a 0.75-fold molar amount of 2-chloro-1,1-difluoroethane solution of the acetate is added dropwise over 1-1.5 h. After the addition is complete, the mixture is refluxed at 300-400 r / min and 115-125° C. for 2-3 h, cooled naturally to room temperature, and purified by distillation to obtain difluoroethyl acetate.

[0012] As an optimization, the preparation method of the tubular reactor in step (1) is as follows: the composite catalyst is filled into the metal pipe, and the filling amount of the composite catalyst is 1.2 to 1.4 cm 3 , at 200~220℃, at 40cm 3 / min, a hydrogen-helium mixed gas is introduced for 2-2.5h to prepare a tubular reactor.

[0013] As an optimization, the composite catalyst is mainly prepared according to the following preparation steps:

[0014] (a) copper nitrate trihydrate, zinc nitrate hexahydrate and pure water are mixed uniformly in a mass ratio of 1:(0.36-0.38):(8-10), heated to 50°C, stirred at 200-300 r / min for 20-30 min to obtain a mixed solution, the mixed solution is added dropwise to a 10 wt% sodium carbonate solution at 50°C with a mass 1.5 times that of the mixed solution for 1-1.5 h, the stirring is maintained at 200-300 r / min during the dropping process, the end point pH is controlled to be between 7 and 8 with a 5 wt% sodium hydroxide solution, the mixture is allowed to stand for 3-4 h, filtered, washed with pure water until neutral, vacuum dried at 70-80°C for 8-10 h, calcined at 350°C for 3 h, ground with a high-speed ball mill at 50-60 r / min for 1-2 h, and passed through a 350 mesh sieve to obtain a copper-zinc catalyst;

[0015] (b) The copper-zinc catalyst and the palladium-carbon catalyst are uniformly mixed in a mass ratio of 1:(0.22-0.28), ground in a high-speed ball mill at 50-60 r / min for 1-2 h, and passed through a 350-mesh sieve to obtain a composite catalyst.

[0016] As an optimization, the palladium-carbon catalyst brand is Kaixi catalyst, containing 5wt% palladium and having a particle size of 350 mesh.

[0017] As an optimization, the inner diameter of the metal pipe is 5 mm and the length is 1000-2000 mm;

[0018] The volume ratio of hydrogen to helium in the hydrogen-helium mixed gas is 1:9.

[0019] As an optimization, the molar ratio of 1,2,2-trichloro-1,1-difluoroethane to hydrogen in step (1) is 1:8.7.

[0020] As an optimization, the reaction process for preparing the crude 2-chloro-1,1-difluoroethane product in step (1) is as follows:

[0021]

[0022] As an optimization, the solvent in steps (2) and (3) is a polar aprotic solvent, including cyclopentane, dimethyl sulfoxide, tetramethylene sulfoxide, dipropyl sulfoxide, benzyl methyl sulfoxide, diisobutyl sulfoxide, dibutyl sulfoxide, diisoamyl sulfoxide, N-methylformamide, N,N-dimethylformamide, N,N-dimethylacetamide, N,N-dimethylpropionamide, N,N-dipropylformamide, N,N-dibutylformamide, N-methylpyrrolidone, N-methylcaprolactam and mixtures thereof.

[0023] As an optimization, the acetate in step (3) is one of potassium acetate and sodium acetate.

[0024] As an optimization, the reaction process for preparing difluoroethyl acetate in step (3) is as follows:

[0025]

[0026] Compared with the prior art, the beneficial effects achieved by the present invention are:

[0027] When preparing difluoroethyl acetate, the present invention comprises the following steps: firstly preparing a copper-zinc catalyst by a coprecipitation method, and then mixing a palladium-carbon catalyst to obtain a composite catalyst; filling the composite catalyst into a metal pipe, adjusting the mixture with a hydrogen-helium mixed gas to obtain a tubular reactor; mixing a raw material 1,2,2-trichloro-1,1-difluoroethane with hydrogen, and introducing the mixture into the tubular reactor to obtain a crude 2-chloro-1,1-difluoroethane product by catalytic hydrogenation and dechlorination; and reacting the crude 2-chloro-1,1-difluoroethane product with acetate after distillation and purification to obtain difluoroethyl acetate.

[0028] First, the appropriate proportion of copper and zinc content can effectively improve the catalytic activity and selectivity of the catalyst. In the present invention, the ratio of copper to zinc content is 10:3. In the process of preparing 2-chloro-1,1-difluoroethane by catalytic hydrodechlorination of 1,2,2-trichloro-1,1-difluoroethane, a conversion rate of 99% to 100% can be achieved, and the selectivity is 90% to 93%. The comprehensive yield is between 89% and 93%. Compared with expensive difluoroethanol, using 1,2,2-trichloro-1,1-difluoroethane as a raw material for preparation can significantly reduce costs, and the preparation process is short in process flow and reaction time, which greatly improves production efficiency.

[0029] Secondly, 2-chloro-1,1-difluoroethane is reacted with acetate to prepare difluoroethanol acetate. The reaction process is simple and the product conversion rate is high, which avoids the use of expensive difluoroethanol. In addition, the reaction conditions are mild and the reaction can be carried out under normal pressure. DETAILED DESCRIPTION

[0030] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0031] Example 1

[0032] A production process of difluoroethyl acetate, the production process of difluoroethyl acetate comprising the following preparation steps:

[0033] (1) Copper nitrate trihydrate, zinc nitrate hexahydrate and pure water were mixed uniformly in a mass ratio of 1:0.36:8, heated to 50° C., stirred at 200 r / min for 30 min to obtain a mixed solution, and the mixed solution was added dropwise to a 10 wt % sodium carbonate solution at 50° C. with a mass 1.5 times that of the mixed solution for 1 h, with stirring maintained at 200 r / min during the dropping process, and the end point pH was controlled to 7 with a 5 wt % sodium hydroxide solution, allowed to stand for 3 h, filtered, washed with pure water until neutral, vacuum dried at 70° C. for 10 h, calcined at 350° C. for 3 h, ground with a high-speed ball mill at 50 r / min for 2 h, and passed through a 350-mesh sieve to obtain a copper-zinc catalyst;

[0034] (2) mixing the copper-zinc catalyst and the palladium-carbon catalyst in a mass ratio of 1:0.22, grinding them in a high-speed ball mill at 50 r / min for 2 h, and passing them through a 350-mesh sieve to obtain a composite catalyst;

[0035] (3) Fill the composite catalyst into a metal pipe with a length of 1300 mm and an inner diameter of 5 mm. The amount of composite catalyst filled is 1.2 cm 3, at 200°C, with a 40cm 3 / min, a hydrogen-helium mixed gas was introduced for 2.5h to prepare a tubular reactor;

[0036] (4) At 200°C, 3×10 5 Pa, 1,2,2-trichloro-1,1-difluoroethane and hydrogen were mixed in a molar ratio of 1:8.7 and fed into a tubular reactor, with a contact time of 4.9 s to obtain a crude 2-chloro-1,1-difluoroethane product, with a reaction raw material conversion rate of 99.24%, a selectivity of 90.76%, and a yield of 90.07%;

[0037] (5) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with N,N-dimethylacetamide at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution;

[0038] (6) Under a nitrogen atmosphere, acetate and N,N-dimethylacetamide were mixed uniformly in a mass ratio of 1:2, heated to 115°C, stirred at a speed of 200 r / min, connected to a dry ice condenser, and 0.75 times the molar amount of 2-chloro-1,1-difluoroethane solution of acetate was added dropwise over 1 h. After the addition was completed, the mixture was refluxed at 300 r / min and 115°C for 3 h, naturally cooled to room temperature, and purified by distillation to obtain difluoroethyl acetate. The conversion rate of 2-chloro-1,1-difluoroethane was 100%, the yield was 92.64%, and the purity of the distillation product was 99.94%.

[0039] Example 2

[0040] A production process of difluoroethyl acetate, the production process of difluoroethyl acetate comprising the following preparation steps:

[0041] (1) Copper nitrate trihydrate, zinc nitrate hexahydrate and pure water were mixed uniformly in a mass ratio of 1:0.37:9, heated to 50°C, stirred at 250 r / min for 25 min to obtain a mixed solution, and the mixed solution was added dropwise to a 50°C 10wt% sodium carbonate solution with a mass 1.5 times that of the mixed solution over 1.2 h, with stirring maintained at 250 r / min during the addition process, and the end point pH was controlled to 7.5 with a 5wt% sodium hydroxide solution, allowed to stand for 3.5 h, filtered, washed with pure water until neutral, vacuum dried at 75°C for 9 h, calcined at 350°C for 3 h, ground with a high-speed ball mill at 55 r / min for 1.5 h, and passed through a 350-mesh sieve to obtain a copper-zinc catalyst;

[0042] (2) mixing the copper-zinc catalyst and the palladium-carbon catalyst in a mass ratio of 1:0.25, grinding them in a high-speed ball mill at 55 r / min for 1.5 h, and passing them through a 350-mesh sieve to obtain a composite catalyst;

[0043] (3) Fill the composite catalyst into a metal pipe with a length of 1300 mm and an inner diameter of 5 mm. The amount of composite catalyst filled is 1.3 cm 3 , at 210°C, at 40 cm 3 / min, a hydrogen-helium mixed gas was introduced for 2.2 h to prepare a tubular reactor;

[0044] (4) At 210°C, 3×10 5 Pa, 1,2,2-trichloro-1,1-difluoroethane and hydrogen were mixed in a molar ratio of 1:8.7 and fed into a tubular reactor, with a contact time of 4.9 s to obtain a crude 2-chloro-1,1-difluoroethane product, with a reaction raw material conversion rate of 99.67%, a selectivity of 92.88%, and a yield of 92.57%;

[0045] (5) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with N,N-dimethylacetamide at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution;

[0046] (6) Under nitrogen atmosphere, acetate and N,N-dimethylacetamide were mixed uniformly in a mass ratio of 1:2.5, heated to 120°C, stirred at 250 r / min, connected to a dry ice condenser, and 0.75 times the molar amount of 2-chloro-1,1-difluoroethane solution of acetate was added dropwise over 1.2 h. After the addition was completed, the mixture was refluxed at 350 r / min and 120°C for 2.5 h, naturally cooled to room temperature, and purified by distillation to obtain difluoroethyl acetate. The conversion rate of 2-chloro-1,1-difluoroethane was 100%, the yield was 93.43%, and the purity of the distillation product was 99.92%.

[0047] Example 3

[0048] A production process of difluoroethyl acetate, the production process of difluoroethyl acetate comprising the following preparation steps:

[0049] (1) Copper nitrate trihydrate, zinc nitrate hexahydrate and pure water were mixed uniformly in a mass ratio of 1:0.38:10, heated to 50°C, and stirred at 300 r / min for 20 min to obtain a mixed solution, and the mixed solution was added dropwise to a 50°C 10wt% sodium carbonate solution with a mass 1.5 times that of the mixed solution over 1.5 hours, with stirring maintained at 300 r / min during the dropping process, and the end point pH was controlled to 8 with a 5wt% sodium hydroxide solution, allowed to stand for 4 hours, filtered, washed with pure water until neutral, vacuum dried at 80°C for 8 hours, calcined at 350°C for 3 hours, ground with a high-speed ball mill at 60 r / min for 1 hour, and passed through a 350-mesh sieve to obtain a copper-zinc catalyst;

[0050] (2) mixing the copper-zinc catalyst and the palladium-carbon catalyst in a mass ratio of 1:0.28, grinding them in a high-speed ball mill at 60 r / min for 1 h, and passing them through a 350-mesh sieve to obtain a composite catalyst;

[0051] (3) Fill the composite catalyst into a metal pipe with a length of 1300 mm and an inner diameter of 5 mm. The amount of composite catalyst filled is 1.4 cm 3 , at 220°C, at 40 cm 3 / min, a hydrogen-helium mixed gas was introduced for 2.5h to prepare a tubular reactor;

[0052] (4) At 220°C, 3×10 5 Pa, 1,2,2-trichloro-1,1-difluoroethane and hydrogen were mixed in a molar ratio of 1:8.7 and fed into a tubular reactor, with a contact time of 4.9 s to obtain a crude 2-chloro-1,1-difluoroethane product, with a reaction raw material conversion rate of 99.14%, a selectivity of 91.59%, and a yield of 90.80%;

[0053] (5) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with N,N-dimethylacetamide at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution;

[0054] (6) Under a nitrogen atmosphere, acetate and N,N-dimethylacetamide were mixed uniformly in a mass ratio of 1:3, heated to 125°C, stirred at a speed of 300 r / min, connected to a dry ice condenser, and 0.75 times the molar amount of 2-chloro-1,1-difluoroethane solution of acetate was added dropwise over 1.5 h. After the addition was completed, the mixture was refluxed at 400 r / min and 125°C for 2 h, naturally cooled to room temperature, and purified by distillation to obtain difluoroethyl acetate. The conversion rate of 2-chloro-1,1-difluoroethane was 100%, the yield was 91.86%, and the purity of the distillation product was 99.95%.

[0055] Comparative Example 1

[0056] A production process of difluoroethyl acetate, the production process of difluoroethyl acetate comprising the following preparation steps:

[0057] (1) Copper nitrate trihydrate, zinc nitrate hexahydrate and pure water were mixed uniformly in a mass ratio of 1:0.12:9, heated to 50°C, stirred at 250 r / min for 25 min to obtain a mixed solution, and the mixed solution was added dropwise to a 50°C 10wt% sodium carbonate solution with a mass 1.5 times that of the mixed solution over 1.2 h, with stirring maintained at 250 r / min during the addition process, and the end point pH was controlled to 7.5 with a 5wt% sodium hydroxide solution, allowed to stand for 3.5 h, filtered, washed with pure water until neutral, vacuum dried at 75°C for 9 h, calcined at 350°C for 3 h, ground with a high-speed ball mill at 55 r / min for 1.5 h, and passed through a 350-mesh sieve to obtain a copper-zinc catalyst;

[0058] (2) mixing the copper-zinc catalyst and the palladium-carbon catalyst in a mass ratio of 1:0.25, grinding them in a high-speed ball mill at 55 r / min for 1.5 h, and passing them through a 350-mesh sieve to obtain a composite catalyst;

[0059] (3) Fill the composite catalyst into a metal pipe with a length of 1300 mm and an inner diameter of 5 mm. The amount of composite catalyst filled is 1.3 cm 3 , at 210°C, at 40 cm 3 / min, a hydrogen-helium mixed gas was introduced for 2.2 h to prepare a tubular reactor;

[0060] (4) At 210°C, 3×10 5 Pa, 1,2,2-trichloro-1,1-difluoroethane and hydrogen were mixed in a molar ratio of 1:8.7 and fed into a tubular reactor, with a contact time of 4.9 s to obtain a crude 2-chloro-1,1-difluoroethane product, with a reaction raw material conversion rate of 95.46%, a selectivity of 42.38%, and a yield of 40.46%;

[0061] (5) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with N,N-dimethylacetamide at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution;

[0062] (6) Under nitrogen atmosphere, acetate and N,N-dimethylacetamide were mixed uniformly in a mass ratio of 1:2.5, heated to 120°C, stirred at 250 r / min, connected to a dry ice condenser, and 0.75 times the molar amount of 2-chloro-1,1-difluoroethane solution of acetate was added dropwise over 1.2 h. After the addition was completed, the mixture was refluxed at 350 r / min and 120°C for 2.5 h, naturally cooled to room temperature, and purified by distillation to obtain difluoroethyl acetate. The conversion rate of 2-chloro-1,1-difluoroethane was 100%, the yield was 90.26%, and the purity of the distillation product was 99.89%.

[0063] Comparative Example 2

[0064] A production process of difluoroethyl acetate, the production process of difluoroethyl acetate comprising the following preparation steps:

[0065] (1) Copper nitrate trihydrate, zinc nitrate hexahydrate and pure water were mixed uniformly in a mass ratio of 1:0.62:9, heated to 50° C., stirred at 250 r / min for 25 min to obtain a mixed solution, and the mixed solution was added dropwise to a 10 wt % sodium carbonate solution at 50° C. with a mass 1.5 times that of the mixed solution over 1.2 h, with stirring maintained at 250 r / min during the addition, and the end point pH was controlled to 7.5 with a 5 wt % sodium hydroxide solution, allowed to stand for 3.5 h, filtered, washed with pure water until neutral, vacuum dried at 75° C. for 9 h, calcined at 350° C. for 3 h, ground with a high-speed ball mill at 55 r / min for 1.5 h, and passed through a 350-mesh sieve to obtain a copper-zinc catalyst;

[0066] (2) mixing the copper-zinc catalyst and the palladium-carbon catalyst in a mass ratio of 1:0.25, grinding them in a high-speed ball mill at 55 r / min for 1.5 h, and passing them through a 350-mesh sieve to obtain a composite catalyst;

[0067] (3) Fill the composite catalyst into a metal pipe with a length of 1300 mm and an inner diameter of 5 mm. The amount of composite catalyst filled is 1.3 cm 3 , at 210°C, at 40 cm 3 / min, a hydrogen-helium mixed gas was introduced for 2.2 h to prepare a tubular reactor;

[0068] (4) At 210°C, 3×10 5 Pa, 1,2,2-trichloro-1,1-difluoroethane and hydrogen were mixed in a molar ratio of 1:8.7 and fed into a tubular reactor, with a contact time of 4.9 s to obtain a crude 2-chloro-1,1-difluoroethane product, with a reaction raw material conversion rate of 99.81%, a selectivity of 53.49%, and a yield of 53.39%;

[0069] (5) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with N,N-dimethylacetamide at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution;

[0070] (6) Under nitrogen atmosphere, acetate and N,N-dimethylacetamide were mixed uniformly in a mass ratio of 1:2.5, heated to 120°C, stirred at 250 r / min, connected to a dry ice condenser, and 0.75 times the molar amount of 2-chloro-1,1-difluoroethane solution of acetate was added dropwise over 1.2 h. After the addition was completed, the mixture was refluxed at 350 r / min and 120°C for 2.5 h, cooled naturally to room temperature, and purified by distillation to obtain difluoroethyl acetate. The conversion rate of 2-chloro-1,1-difluoroethane was 100%, the yield was 91.15%, and the purity of the distillation product was 99.91%.

[0071] The specific implementation methods described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific implementation method of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. A production process for difluoroethyl acetate, characterized in that, The method mainly comprises the following preparation steps: mixing 1,2,2-trichloro-1,1-difluoroethane and hydrogen and introducing them into a tubular reactor for reaction to obtain a crude 2-chloro-1,1-difluoroethane product; distilling and purifying the crude 2-chloro-1,1-difluoroethane product to obtain a 2-chloro-1,1-difluoroethane solution; reacting the 2-chloro-1,1-difluoroethane solution with acetate to obtain difluoroethyl acetate; The tubular reactor comprises a metal pipeline and a composite catalyst.

2. A production process for difluoroethyl acetate according to claim 1, characterized in that, The production process of difluoroethyl acetate mainly comprises the following preparation steps: (1) At 200-220°C, 3×10 5 Pa, mixing 1,2,2-trichloro-1,1-difluoroethane and hydrogen in a certain molar ratio and feeding them into a tubular reactor to obtain a crude 2-chloro-1,1-difluoroethane product; (2) distilling and purifying the crude 2-chloro-1,1-difluoroethane product until the 2-chloro-1,1-difluoroethane content is greater than 99%, and then mixing it with a solvent at a mass ratio of 1:1 to obtain a 2-chloro-1,1-difluoroethane solution; (3) Under a nitrogen atmosphere, the acetate and the solvent are mixed uniformly in a mass ratio of 1:(2-3), heated to 115-125° C., stirred at a speed of 200-300 r / min, connected to a dry ice condenser, and a 0.75-fold molar amount of 2-chloro-1,1-difluoroethane solution of the acetate is added dropwise over 1-1.5 h. After the addition is complete, the mixture is refluxed at 300-400 r / min and 115-125° C. for 2-3 h, cooled naturally to room temperature, and purified by distillation to obtain difluoroethyl acetate.

3. A production process for difluoroethyl acetate according to claim 2, characterized in that, The preparation method of the tubular reactor in step (1) is as follows: the composite catalyst is filled into a metal pipe, and the amount of the composite catalyst filled is 1.2 to 1.4 cm 3 , at 200~220℃, at 40cm 3 / min, a hydrogen-helium mixed gas is introduced for 2-2.5h to obtain a tubular reactor.

4. A production process for difluoroethyl acetate according to claim 3, characterized in that, The composite catalyst is mainly prepared according to the following preparation steps: (a) copper nitrate trihydrate, zinc nitrate hexahydrate and pure water are mixed uniformly in a mass ratio of 1:(0.36-0.38):(8-10), heated to 50°C, stirred at 200-300 r / min for 20-30 min to obtain a mixed solution, the mixed solution is added dropwise to a 10 wt% sodium carbonate solution at 50°C with a mass 1.5 times that of the mixed solution for 1-1.5 h, the stirring is maintained at 200-300 r / min during the dropping process, the end point pH is controlled to be between 7 and 8 with a 5 wt% sodium hydroxide solution, the mixture is allowed to stand for 3-4 h, filtered, washed with pure water until neutral, vacuum dried at 70-80°C for 8-10 h, calcined at 350°C for 3 h, ground with a high-speed ball mill at 50-60 r / min for 1-2 h, and passed through a 350 mesh sieve to obtain a copper-zinc catalyst; (b) The copper-zinc catalyst and the palladium-carbon catalyst are uniformly mixed in a mass ratio of 1:(0.22-0.28), ground in a high-speed ball mill at 50-60 r / min for 1-2 h, and passed through a 350-mesh sieve to obtain a composite catalyst.

5. A production process for difluoroethyl acetate according to claim 4, characterized in that, The palladium-carbon catalyst is of Kaixi catalyst brand, contains 5wt% palladium, and has a particle size of 350 meshes.

6. A production process for difluoroethyl acetate according to claim 3, characterized in that, The metal pipe has an inner diameter of 5 mm and a length of 1000 to 2000 mm; The volume ratio of hydrogen to helium in the hydrogen-helium mixed gas is 1:

9.

7. A production process for difluoroethyl acetate according to claim 2, characterized in that, The molar ratio of 1,2,2-trichloro-1,1-difluoroethane to hydrogen in step (1) is 1:8.

7.

8. A production process for difluoroethyl acetate according to claim 2, characterized in that, The solvent in steps (2) and (3) is a polar aprotic solvent, including cyclopentane, dimethyl sulfoxide, tetramethylene sulfoxide, dipropyl sulfoxide, benzyl methyl sulfoxide, diisobutyl sulfoxide, dibutyl sulfoxide, diisoamyl sulfoxide, N-methylformamide, N,N-dimethylformamide, N,N-dimethylacetamide, N,N-dimethylpropionamide, N,N-dipropylformamide, N,N-dibutylformamide, N-methylpyrrolidone, N-methylcaprolactam and mixtures thereof.

9. A production process for difluoroethyl acetate according to claim 2, characterized in that, The acetate in step (3) is one of potassium acetate and sodium acetate.