Continuous anode aluminum electrolysis cell
By adopting a built-in conductor structure and fixing device in the aluminum electrolytic cell, the problems of high anode replacement frequency and uneven current distribution are solved, the efficiency and accuracy of electrolytic aluminum production are improved, and continuous production is achieved.
Patent Information
- Application Number
- CN202411484817.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-23
- Publication Date
- 2024-12-06
AI Technical Summary
The prior art is unable to achieve continuous electrolytic aluminum production due to the large anode replacement frequency and uneven current distribution of carbon blocks, which affects efficiency and accuracy.
It adopts a continuous anode aluminum electrolytic cell design including a top structure, anode structure, fixing device and cathode structure. It is connected by steel beams, spreaders, anode carbon blocks, guide rods, clamps and claws. It has a built-in conductor structure to reduce the anode replacement frequency. Improve the sealing effect of the electrolytic cell.
It effectively reduces the anode replacement frequency, improves the efficiency and accuracy of electrolytic aluminum production, and realizes the continuous electrolytic aluminum production process.
Smart Images

Figure CN119082804A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of molten salt aluminum electrolytic metallurgy production, and in particular to a continuous anode aluminum electrolytic cell. Background Art
[0002] Since 1886, the process and principles of molten salt electrolysis for aluminum smelting have remained unchanged. However, electrolytic cells, based on anode characteristics, have evolved from small prebaked anodes to side-inserted self-baked anodes, to top-inserted self-baked anodes, and finally to prebaked anodes. Early electrolytic cells had high power consumption and low current efficiency. With continuous technological advancements, the structure of electrolytic cells has been gradually optimized, significantly improving power consumption and current efficiency.
[0003] Traditional self-baking cells utilize plug-and-play electrodes, resulting in uneven current distribution and complex anode operation, making automation and intelligentization difficult. The workshop environment is harsh due to high fluoride concentrations in the air. Current efficiency is typically 88%-90%, resulting in a high DC power consumption of approximately 14,900 kWh per ton of aluminum. Cell types are typically in the 60-90 kA range, making further scaling difficult. While prebaked cell technology has made significant progress in terms of scale-up and automation, the prebaked anode process, which involves baking long carbon blocks, cutting them, and then casting the anode steel claws, still presents significant drawbacks, such as a lengthy process and interference with cell stability during the electrode change process.
[0004] In summary, the existing technology cannot realize the continuous electrolytic aluminum production process due to the high replacement frequency of anodes and the uneven current distribution of carbon blocks, which further affects the efficiency and accuracy of electrolytic aluminum production. Summary of the Invention
[0005] The purpose of this application is to provide a continuous anode aluminum electrolytic cell to solve the problem in the prior art that the electrolytic aluminum production process cannot be continuous due to the high frequency of anode replacement and uneven current distribution of carbon blocks.
[0006] In view of the above problems, the present application provides a continuous anode aluminum electrolysis cell.
[0007] The present application provides a continuous anode aluminum electrolytic cell, wherein the continuous anode aluminum electrolytic cell comprises: a top structure, comprising a steel beam, on which a first sling, a second sling, and an intermediate sling are installed; an anode structure, comprising an anode carbon block, wherein the anode carbon block is penetrated by a plurality of side anode guide rods, and the plurality of side anode guide rods extend out of the anode carbon block, and the plurality of side anode guide rods include an anode busbar, and the anode carbon block also includes a top anode guide rod, and the top anode guide rod extends out of the anode carbon block; a fixing device, comprising an anode clamp and a metal claw; the anode carbon block is fixed to the first sling and the second sling by the anode clamp; the anode carbon block is connected to the intermediate sling by the metal claw; an electrolytic cell, wherein the electrolytic cell can be filled with electrolyte; a cathode structure, located on the other side of the electrolytic cell, comprising a cathode carbon block and a cathode lining, which together with the electrolytic cell constitute the cathode part of the electrolytic reaction.
[0008] One or more technical solutions provided in this application have at least the following technical effects or advantages:
[0009] The top structure includes a steel beam, on which a first sling, a second sling and an intermediate sling are installed; the anode structure includes an anode carbon block, the anode carbon block is penetrated by a plurality of side anode guide rods, the plurality of side anode guide rods extend out of the anode carbon block, the plurality of side anode guide rods include an anode bus bar, the anode carbon block also includes a top anode guide rod, the top anode guide rod extends out of the anode carbon block; a fixing device includes an anode clamp and a metal claw; the anode carbon block is fixed to the first sling and the second sling by the anode clamp fixed; the anode carbon block is connected to the intermediate sling by the metal claw; the electrolytic cell, the electrolytic cell can be filled with electrolyte; the cathode structure, located on the other side of the electrolytic cell, includes a cathode carbon block and a cathode lining, which together with the electrolytic cell constitute the cathode part of the electrolytic reaction, effectively solving the problem of high replacement frequency of anodes and uneven current distribution of carbon blocks in the prior art, which leads to the inability to continue the electrolytic aluminum production process. The use of a built-in conductor structure saves the operation of pulling out and inserting nail rods, improves the sealing effect of the electrolytic cell, reduces the replacement frequency of anodes, and improves the efficiency of electrolytic aluminum production.
[0010] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, which can be implemented in accordance with the contents of the description, and to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are specifically listed below. It should be understood that the content described in this section is not intended to identify the key or important features of the embodiments of the present application, nor is it intended to limit the scope of the present application. Other features of the present application will become easy to understand through the following description. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] In order to more clearly illustrate the technical solutions in this application or the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are merely exemplary, and a person of ordinary skill in the art can obtain other drawings based on the provided drawings without creative work.
[0012] Figure 1 This is a schematic structural diagram of a continuous anode aluminum electrolytic cell for this application.
[0013] Description of reference numerals:
[0014] Steel beam 1, middle hanger 2, top anode guide rod 3, metal claw 4, metal thorn 15, anode carbon block 5, anode clamp 14, side anode guide rod 6, anode busbar 7, alumina 8, electrolyte 9, aluminum liquid 10, cathode carbon block 11, cathode liner 12. DETAILED DESCRIPTION
[0015] The present application provides a continuous anode aluminum electrolytic cell, which solves the problem in the prior art that the electrolytic aluminum production process cannot be continuous due to the high frequency of anode replacement and uneven current distribution of carbon blocks. The application adopts a built-in conductor structure, which saves the operation of pulling out and inserting nail rods, improves the sealing effect of the electrolytic cell, reduces the frequency of anode replacement, and improves the efficiency of electrolytic aluminum production.
[0016] Below, the technical solutions in this application will be clearly and completely described with reference to the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of this application, rather than all the embodiments of this application. It should be understood that this application is not limited to the example embodiments described herein. Based on the embodiments of this application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application. It should also be noted that, for the convenience of description, only the parts related to this application, rather than all of them, are shown in the accompanying drawings.
[0017] Please see the attached Figure 1 , the present application provides a continuous anode aluminum electrolysis cell, comprising:
[0018] The top structure includes a steel beam 1 , on which a first sling, a second sling, and an intermediate sling 2 are installed.
[0019] Specifically, in the aluminum electrolytic cell top structure of this embodiment, the steel beam 1 serves as a load-bearing component, and the slings installed on it include a first sling, a second sling, and an intermediate sling 2. The first sling and the second sling are located at both ends of the steel beam 1 and are used to lift the anode carbon blocks 5. The intermediate sling 2 is located in the middle of the steel beam 1 and is used to assist in lifting the top anode guide rod 3. The steel beam 1 meets the weight requirements of the electrolytic cell superstructure to ensure that it will not break or deform during the lifting process. The structure of the sling should be easy to inspect and repair to reduce maintenance costs and downtime.
[0020] The anode structure includes an anode carbon block 5, which is penetrated by multiple side anode guide rods 6. The multiple side anode guide rods 6 extend out of the anode carbon block 5. The multiple side anode guide rods 6 include an anode busbar. The anode carbon block 5 also includes a top anode guide rod 3, and the top anode guide rod 3 extends out of the anode carbon block 5.
[0021] Specifically, the anode structure is the part connected to the positive electrode of the power supply during electrolysis, responsible for conducting current and participating in the electrochemical reaction. The anode structure includes components such as the anode carbon block 5, side anode guide rods 6, an anode busbar, and a top anode guide rod 3. The anode carbon block 5 is a key component in an aluminum electrolysis cell. It not only serves as a medium for conducting current but also plays a vital role in the electrolysis reaction. During the electrolysis process, the anode carbon block 5 gradually consumes. Made of a carbonaceous material with high electrical conductivity and corrosion resistance, the side anode guide rods 6 extend through the anode carbon block 5, ensuring smooth flow of current. The side anode guide rods 6 are evenly distributed along the sides of the anode carbon block 5. They extend outside the anode carbon block 5 to facilitate connection to the anode busbar 7 or other conductive components. The anode busbar 7 connects the side anode guide rods 6 to the positive electrode of the power supply. The anode busbar 7 is made of highly conductive aluminum. Its design and layout must take into account the uniformity of current distribution and the overall stability of the electrolysis cell. The top anode guide rod 3 is another important component of the anode structure. It extends outside the anode carbon block 5 to further ensure stable current transmission. The presence of the top anode guide rod 3 enhances the overall stability of the anode structure and helps optimize current distribution.
[0022] The fixing device includes an anode clamp 14 and a metal claw 4.
[0023] Specifically, the fixing device ensures that the anode carbon block 5 and its related components maintain a stable position during the electrolysis process. The anode clamp 14 is a specially designed fastener for fixing the anode carbon block 5 and its guide rod. By tightly clamping the anode carbon block 5 and the guide rod together, loosening or displacement caused by factors such as current, thermal stress or mechanical vibration during the electrolysis process is prevented. Since the anode carbon block 5 and the guide rod are subjected to greater stress during the electrolysis process, the anode clamp 14 needs to have a higher strength to withstand these stresses. Considering the harsh environment in the electrolytic cell, the anode clamp 14 is made of corrosion-resistant material to extend its service life. The metal claw 4 may fasten the anode carbon block 5 to the top anode guide rod 3 to ensure the stability of the electrolysis process.
[0024] The anode carbon block 5 is fixed to the first sling and the second sling via the anode clamp 14 .
[0025] Specifically, the anode clamp 14 is primarily used to secure the anode carbon block 5 and its associated components, such as the anode guide rod. The anode clamp 14 cooperates with the first and second slings to secure the anode carbon block 5. The anode carbon block 5 is lifted using the slings and temporarily secured in a predetermined position using the anode clamp 14 for subsequent securing.
[0026] The anode carbon block 5 is connected to the intermediate sling 2 via the metal claws 4 .
[0027] Specifically, the anode carbon block 5 is connected to the intermediate hanger 2 via metal claws 4, which also securely connect the anode carbon block 5 to the guide rod. The metal claws 4 possess sufficient strength and adaptability to securely grasp the anode carbon block 5 and connect it to the intermediate hanger 2. The matching connection points or interfaces between the intermediate hanger 2 and the metal claws 4 ensure stable support and fixation of the anode carbon block 5.
[0028] An electrolytic cell, wherein the electrolytic cell can be filled with an electrolyte 9 .
[0029] Specifically, an electrolytic cell typically consists of a cell body, an anode, a cathode, a diaphragm, an electrolyte 9 circulation system, a cooling system, and an electrical control system. The cell body is a container for the electrolyte 9. The anode and cathode are connected to the positive and negative terminals of a power source, respectively. Through electrolysis, the ions in the electrolyte 9 are converted into the desired products. Ensure the electrolytic cell is clean and dry, and inspect the integrity of the cell body, anode, cathode, and other components. Prepare the required electrolyte 9 and adjust its concentration and temperature according to process requirements. Open the inlet or filling port of the electrolytic cell and slowly pour the prepared electrolyte 9 into the cell body. During the filling process, it is important to carefully control the flow rate and volume of the electrolyte 9 to avoid excessive pressure shock to the electrolytic cell. During the filling process, gas may be generated in the electrolytic cell, which needs to be promptly discharged through the exhaust port. After filling is complete, close the inlet and exhaust ports and conduct a thorough inspection of the electrolytic cell to ensure there are no leaks.
[0030] The cathode structure, located on the other side of the electrolytic cell, includes a cathode carbon block 11 and a cathode liner 12, and together with the electrolytic cell constitutes the cathode part of the electrolysis reaction.
[0031] Specifically, the cathode structure is located on the other side of the electrolytic cell, opposite to the anode structure, and together constitutes the cathode part of the electrolytic reaction. The cathode structure mainly includes a cathode carbon block 11 and a cathode lining 12. The cathode carbon block 11 is the main part of the cathode of the aluminum electrolytic cell and directly participates in the electrolytic reaction. The cathode carbon block 11 is made of high-quality anthracite, coke, graphite, etc. These raw materials are processed through specific processes such as calcination, crushing, screening, kneading, molding and roasting, and finally form a carbon block with the required physical and chemical properties. The cathode carbon block 11 has good electrical conductivity. As the lining material of the electrolytic cell, the cathode carbon block 11 can resist the erosion of high-temperature molten salt and aluminum liquid 10, and protect the electrolytic cell shell from damage. The cathode lining 12 is the cathode structure of the electrolytic cell, including the bottom carbon material in direct contact with the melt, as well as the side lining material, conductive rods, etc. The cathode lining 12 has good sealing properties. The cathode lining 12 material can resist the erosion of high-temperature molten salt and aluminum liquid 10, protect the electrolytic cell shell from damage, extend the service life of the electrolytic cell, and generate aluminum by decomposing aluminum oxide 7.
[0032] Furthermore, the carbon raw material is placed in a forming machine and formed into a preliminary anode carbon block through high-pressure pressing.
[0033] Specifically, the raw materials of the anode carbon block 5 mainly include aggregates such as petroleum coke and asphalt coke, and binders such as coal tar. These raw materials need to undergo pretreatment processes such as calcination, crushing, and screening to achieve the particle size and purity requirements required for molding. In the production of the anode carbon block 5, the molding equipment includes a carbon molding machine, a chain-type carbon molding machine, a prebaked anode molding machine, etc. After the raw materials are reasonably mixed, they are metered into the mold according to the required amount of different specifications and sizes. The molding machine meters the pretreated carbon raw materials according to a certain proportion and adds them to the mold. After the mold is closed, the molding machine applies high pressure to the mold through the hydraulic system and starts the vibration system at the same time. Vibration helps to reduce the friction between the materials inside, so that the materials are rearranged in the mold and more tightly combined. After a certain period of high-pressure pressing and vibration, the raw materials form a preliminary anode carbon block with a certain strength and density in the mold. Subsequently, the molding machine opens the mold and pushes out the preliminary anode carbon block.
[0034] Furthermore, internal pores are preset in the preliminary anode carbon block.
[0035] Specifically, a corresponding pore structure is designed into the mold of the forming machine so that during the high-pressure pressing process, the raw material can follow the shape of the mold to form a preliminary anode carbon block with internal pores. After the preliminary anode carbon block is formed, pores are preset inside the carbon block through methods such as mechanical drilling, laser drilling, or chemical etching.
[0036] Furthermore, the preliminary anode carbon block is preheated and sent to a roasting furnace for high-temperature roasting. Aluminum liquid is poured into the preset internal pores. After the aluminum liquid cools, metal thorns 15 are generated to form the anode carbon block 5.
[0037] Specifically, the primary purpose of preheating is to remove moisture and volatiles from the preliminary anode carbon blocks, reduce stress and cracking caused by the rapid temperature increase during the roasting process, and improve roasting efficiency. The preliminary anode carbon blocks are placed in a preheating furnace and heated at a relatively low temperature. The preheating temperature and time need to be adjusted according to the carbon block material, size, and preheating furnace performance. Roasting is a core step in anode carbon block production. The high-temperature treatment causes physical and chemical changes in the carbon blocks, improving their mechanical strength, chemical stability, and electrical conductivity. Furthermore, the roasting process changes the porosity of the carbon blocks, preparing them for subsequent aluminum molten filling. The preheated preliminary anode carbon blocks are then placed in a roasting furnace and roasted at high temperatures. The roasting temperature typically reaches over 1000°C, even around 1400°C, depending on the carbon block material and the desired properties. The roasting time is generally several dozen hours to ensure the carbon blocks are fully sintered and stabilized. Liquid aluminum is poured into the pre-set internal pores of the anode carbon block 5. Upon cooling, the molten aluminum solidifies and bonds tightly to the carbon block, forming metal spikes 15. These metal spikes 15 help increase the contact area between the anode and the electrolyte 9, promoting the electrolytic reaction. After calcination, the anode carbon block 5 is removed from the calciner and cooled to a temperature above the melting point of aluminum but below the damage temperature of the carbon block. Molten aluminum is then injected into the pores within the carbon block using specialized aluminum-filling equipment. The aluminum-filling process requires precise control of the aluminum flow rate, temperature, and filling speed to ensure that the aluminum evenly fills the pores and forms a good bond. After aluminum-filling is complete, the anode carbon block 5 is allowed to cool naturally or forced cooling is used to solidify the aluminum. During the cooling process, excessively fast or excessively slow cooling rates should be avoided to prevent cracking of the carbon block or the detachment of the aluminum spikes. Finally, the anode carbon block 5 undergoes necessary post-processing, such as trimming, cleaning, and inspection, to ensure that its quality meets requirements.
[0038] Furthermore, the height of the anode carbon block 5 is greater than 1200 mm.
[0039] Specifically, the anode carbon block 5 with a height greater than 1200 mm is used in the process of continuously manufacturing aluminum in the electrolytic cell. The anode carbon block 5 with a height greater than 1200 mm may have the characteristics of a larger electrolysis area, a higher current density and a longer service life.
[0040] Furthermore, the side surface of the anode carbon block 5 includes a plurality of holes, and the holes are internally threaded, and the plurality of side anode guide rods 6 are connected to the anode carbon block 5 through the holes.
[0041] Specifically, a plurality of holes are designed on the side of the anode carbon block 5, and these holes have an internal thread structure in order to realize a detachable connection between the anode carbon block 5 and the anode guide rod. The internal thread holes allow the anode guide rod to be fixed to the anode carbon block 5 by means of a threaded connection, thereby facilitating installation, disassembly and maintenance. The threaded connection can provide a relatively stable connection effect, ensuring that the anode guide rod is not easy to loosen or fall off during the electrolysis process. Due to the threaded connection, the anode guide rod can be easily disassembled and reinstalled from the anode carbon block 5, which facilitates the replacement and maintenance of the anode carbon block 5. By adjusting the number and position of the anode guide rods, the requirements of electrolytic cells of different specifications and models can be met.
[0042] Furthermore, the metal claws 4 are aluminum claws, and the aluminum claws are connected to the intermediate hanger 2 and the anode carbon block 5 by means of molten iron phosphorus water cooling welding.
[0043] Specifically, the aluminum claws serve as connectors to firmly connect the anode carbon block 5 and the intermediate hanger 2. They are able to withstand the high temperature, current and mechanical stress generated during the electrolysis process, ensure the stable suspension of the anode carbon block 5, and maintain good electrical conductivity. Phosphorus-iron water-cooled welding utilizes molten phosphorus-iron alloy as solder. When the phosphorus-iron alloy melts and flows into the weld joint, it undergoes metallurgical bonding with the materials of the anode carbon block 5 and the intermediate hanger 2 to form a strong connection. Subsequently, through the cooling process, the solder solidifies, thereby firmly connecting the anode carbon block 5 and the intermediate hanger 2 together. First, the welding area of the anode carbon block 5 and the intermediate hanger 2 needs to be cleaned to remove oxides, oil stains and other impurities on the surface to ensure welding quality. The phosphorus-iron alloy is melted at high temperature to form a molten solder. The molten phosphorus-iron alloy solder is poured into the pre-designed weld joint so that the solder is in full contact with the materials of the anode carbon block 5 and the intermediate hanger 2 and undergoes metallurgical bonding. After welding is completed, the welded joint is allowed to cool naturally or forcedly cool to solidify the solder, thereby firmly connecting the anode carbon block 5 and the intermediate hanger 2 together.
[0044] Furthermore, the anode clamp 14 is an adjustable fastening structure.
[0045] Specifically, the two parts of the clamp are connected by bolts, and the degree of tightening is adjusted by rotating the nut. The adjustable anode clamp 14 can accommodate anodes of different sizes and shapes, as well as slight changes in the protected structure, such as dimensional changes caused by thermal expansion and contraction.
[0046] The above description of the disclosed embodiments is intended to enable one skilled in the art to implement or use the present application. Various modifications to these embodiments will be readily apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application is not limited to the embodiments shown herein, but is intended to conform to the widest scope consistent with the principles and novel features disclosed herein.
[0047] Obviously, those skilled in the art may make various changes and modifications to the present application without departing from the spirit and scope of the present application. Thus, if these modifications and variations of the present application fall within the scope of the present application and its equivalents, the present application is intended to include these modifications and variations.
Claims
1. A continuous anode aluminum electrolysis cell, characterized in that: include: The top structure includes a steel beam, on which a first sling, a second sling, and an intermediate sling are installed; An anode structure, comprising an anode carbon block, wherein the anode carbon block is penetrated by a plurality of side anode guide rods, the plurality of side anode guide rods extend out of the anode carbon block, the plurality of side anode guide rods include an anode bus bar, the anode carbon block further comprises a top anode guide rod, the top anode guide rod extends out of the anode carbon block; Fixing devices, including anode clamps and metal claws; Fixing the anode carbon block to the first hanger and the second hanger through the anode clamp; Connecting the anode carbon block to the intermediate hanger via the metal claws; An electrolytic cell, wherein the electrolytic cell can be filled with an electrolyte; The cathode structure, located at the other side of the electrolytic cell, comprises a cathode carbon block and a cathode liner, and together with the electrolytic cell constitutes the cathode part of the electrolytic reaction.
2. A continuous anode aluminum electrolysis cell according to claim 1, characterized in that: The carbon raw material is placed in a molding machine and formed into a preliminary anode carbon block through high-pressure pressing.
3. A continuous anode aluminum electrolysis cell according to claim 2, characterized in that: Internal pores are preset in the preliminary anode carbon block.
4. A continuous anode aluminum electrolysis cell according to claim 3, characterized in that: The preliminary anode carbon block is preheated, and the preheated preliminary anode carbon block is sent to a roasting furnace for high-temperature roasting, and aluminum liquid is poured into the preset internal pores. After the aluminum liquid is cooled, metal thorns will be generated to form the anode carbon block.
5. A continuous anode aluminum electrolysis cell according to claim 4, characterized in that: The height of the anode carbon block is greater than 1200 mm.
6. A continuous anode aluminum electrolysis cell according to claim 4, characterized in that: The side surface of the anode carbon block includes a plurality of holes, the holes are internal threads, and the plurality of side anode guide rods are connected to the anode carbon block through the holes.
7. A continuous anode aluminum electrolysis cell according to claim 1, characterized in that: The metal claws are aluminum claws, and the aluminum claws are connected to the intermediate hanger and the anode carbon block by means of molten iron phosphorus water cooling welding.
8. A continuous anode aluminum electrolysis cell according to claim 1, characterized in that: The anode clamp is an adjustable fastening structure.