Optical composite film and preparation method thereof, backlight module and display panel

By adopting integrated bonding in the optical composite film, multiple layer structures are stacked in sequence to form an integrated polarized composite film, the existing optical film is solved by low assembly efficiency, scratching and luminance in the backlight module. The problem of decreasing has achieved a reduction in thickness and an increase in shade, and improved the brightness and quality of the backlight module.

CN119087709APending Publication Date: 2024-12-06JIANGSU HONOPTICAL MATERIAL TECH CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411492089.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-24
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The use of multiple architectures in the existing optical films in the backlight module leads to low assembly efficiency, easy scratching, and reduced brightness. The upper diffusion and lower polarizer stack have GAP gaps, resulting in thicker backlight modules and high production costs. If multiple prisms are combined with diffusion, rainbow patterns will appear, and the picture tastes poorly.

Method used

An optical composite film is adopted, including a first substrate layer, a first prism layer, a second substrate layer, a polarizer, a PSA layer and an atomized back coating, and a plurality of layers are stacked in sequence through integrated bonding. The body structure reduces the thickness and improves the shielding degree to form an integrated polarized composite film.

Benefits of technology

The thickness of the optical composite film is reduced, the production cost is reduced and the shielding degree is improved, the assembly efficiency and scratching problems are solved, and the rainbow pattern is avoided, and the brightness and quality of the backlight module are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119087709A_ABST
    Figure CN119087709A_ABST
Patent Text Reader

Abstract

The invention discloses an optical composite film and a preparation method thereof, a backlight module and a display panel, and relates to the technical field of display. The optical composite film comprises a first base material layer and a second base material layer, the first prism layer is arranged on the first substrate layer; the second base material layer is arranged on the first prism layer far away from one side of the first base material layer; the polaroid is arranged on one side, far away from the first prism layer, of the second substrate layer; and the PSA layer is arranged on one side, far away from the second base material layer, of the polaroid. According to the invention, the problems that the assembly efficiency is low, the brightness is reduced due to the easy generation of scratches, and the backlight module is thicker and the production cost is relatively higher due to the GAP gap formed between the upper diffusion sheet and the lower polaroid when the existing optical film generally uses the matching of a plurality of frameworks to meet the brightness requirement are solved; meanwhile, if a plurality of prism combinations are not matched with diffusion, rainbow lines can appear, the picture taste is poor, and the brightness is reduced due to the fact that the prism combinations are easy to scratch during assembly.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of display technology, and in particular to an optical composite film and a preparation method thereof, a backlight module, and a display panel. Background Art

[0002] With the progress of the times, the LCD industry has developed rapidly, and products with higher brightness and relatively lower prices are favored by people. Therefore, the LCD industry is also facing challenges in product cost control. The backlight materials used in the current backlight modules generally use a combination of multiple films (3Film structure, 4film structure) or a composite film (POP, MOP, DOP) with a diffusion film.

[0003] Application No. CN200810127579.2 proposes an optical film, comprising a substrate and a microstructure layer located on the surface of the substrate, wherein the microstructure layer comprises a plurality of columnar structures and the columnar structures comprise at least two columnar structures selected from the group consisting of a linear columnar structure whose peak height varies along the extension direction, a linear columnar structure whose peak height does not vary along the extension direction, a curved columnar structure whose peak height varies along the extension direction, and a curved columnar structure whose peak height does not vary along the extension direction. The optical film of the present invention has a light-gathering effect and can effectively reduce optical interference.

[0004] The existing optical films generally use multiple structures to meet the brightness requirements, resulting in low assembly efficiency, easy scratches, resulting in reduced brightness, and a gap between the upper diffuser and the lower polarizer, resulting in a thicker backlight module and relatively high production costs; at the same time, if multiple prisms are not combined with an upper diffuser, rainbow patterns will appear, the picture quality is poor, and the assembly is easy to scratch, resulting in reduced brightness; and the direct backlight is generally used with a lower diffuser, resulting in a thicker backlight module. No effective solution has been proposed for the above problems. Summary of the invention

[0005] Purpose of the invention: To provide an optical composite film and a preparation method thereof, a backlight module, and a display panel, so as to solve at least one of the problems existing in the above-mentioned prior art.

[0006] Technical solution: An optical composite film, comprising: a first substrate layer; A first prism layer, disposed on the first substrate layer; A second substrate layer is disposed on the first prism layer at a side away from the first substrate layer; a polarizer, disposed on the second substrate layer at a side away from the first prism layer; A PSA layer is disposed on the polarizer at a side away from the second substrate layer; and A hazed back coating layer is disposed on the first substrate layer at a side away from the first prism layer; Wherein, a plurality of layer structures are stacked in sequence according to a preset order so as to reduce the thickness of the optical composite film and improve the shielding degree.

[0007] Preferably, a first bonding adhesive layer is provided between the first prism layer and the second substrate layer.

[0008] Preferably, a second bonding adhesive layer is provided between the second substrate layer and the polarizer; Wherein, particles are arranged in the second bonding adhesive layer.

[0009] Preferably, a release film is provided on the side of the PSA layer away from the polarizer to form an integrated polarizing composite film.

[0010] Preferably, a second prism layer and a third substrate layer are stacked in sequence from top to bottom between the first substrate layer and the atomized back coating layer; The first prism portion of the first prism layer and the second prism portion of the second prism layer are two groups of orthogonal prisms.

[0011] Preferably, the first prism layer adopts a shaking appearance, and / or the second prism layer adopts a shaking appearance.

[0012] Preferably, a first bonding adhesive layer is provided between the first prism layer and the second substrate layer, and a second bonding adhesive layer is provided between the second substrate layer and the polarizer; Wherein, particles are arranged in the first bonding adhesive layer, or particles are arranged in the second bonding adhesive layer.

[0013] Preferably, the cross-sections of the first prism layer and the second prism layer are both isosceles triangles, and the width of the bases thereof is 10 um-80 um.

[0014] Preferably, the top angle between the first prism layer and the second prism layer is 60-95°.

[0015] Preferably, the refractive index range of the first prism layer and the second prism structure layer is 1.5-1.7.

[0016] Preferably, the thickness of the first substrate layer, the second substrate layer and the third substrate layer is 20um-300um.

[0017] In order to achieve the above objective, according to another aspect of the present application, a backlight module is also provided.

[0018] The backlight module according to the present application includes the optical composite film as described above.

[0019] In order to achieve the above objective, according to another aspect of the present application, a display panel is also provided.

[0020] The display panel according to the present application includes the backlight module as described above.

[0021] In order to achieve the above objective, according to another aspect of the present application, a method for preparing an optical composite film is also provided.

[0022] The method for preparing an optical composite film according to the present application is applied to prepare the optical composite film as described above; and comprises the following steps: Step 1: preparing a first substrate layer; Step 2: coating a first light-curing coating on the first substrate layer; Step 3: Imprinting and molding the mold using a light-curing transfer process to obtain a first prism layer; Step 4: preparing a second substrate layer; Step 5, applying adhesive on both sides of the second substrate layer respectively; Step 6: Paste the second substrate layer onto the first prism layer on the side away from the first substrate layer by heat pressing or gluing; Step 7: attaching a polarizer to the side of the second substrate layer away from the first prism layer by means of an adhesive, and fixing the polarizer by means of a pressure-sensitive adhesive or heat pressing; Step 8, uniformly coating the PSA layer on the side of the polarizer away from the second substrate layer; Step nine, attaching a release film to the PSA layer; Step 10: coating a hazed back coating layer on the side of the first substrate layer away from the first prism layer.

[0023] Beneficial effect: In the embodiment of the present application, an integrated bonding method is adopted, and multiple layer structures are stacked in sequence according to a preset order to reduce the thickness of the optical composite film and increase the shielding degree, thereby achieving the purpose of forming an integrated polarizing composite film, thereby achieving the technical effects of reducing the thickness of the optical composite film, reducing production costs and increasing the shielding degree, thereby solving the problem that the existing optical film generally uses multiple structures to meet the brightness requirements, resulting in low assembly efficiency, easy scratches resulting in reduced brightness, and a GAP gap between the upper diffuser and the lower polarizer stacked, resulting in a thicker backlight module and relatively high production costs; at the same time, if the combination of multiple prisms is not matched with an upper diffuser, rainbow patterns will appear, the picture quality is poor, and the assembly is easy to be scratched, resulting in a decrease in brightness; and the direct backlight is generally used with a lower diffuser, resulting in a thicker backlight module. Technical problems. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic diagram of the planar structure of the optical composite film of the present invention; Figure 2is a schematic flow chart of another method for preparing an optical composite film of the present invention; and Figure 3 It is a schematic diagram of the process of preparing another optical composite film of the present invention.

[0025] The accompanying drawings are marked as follows: 10. a first substrate layer; 20. First prism layer; 30. a second substrate layer; 40. Polarizer; 50. PSA layer; 60. Atomized back coating; 70. First bonding adhesive layer; 80, second bonding adhesive layer; 90. Release film; 100, second prism layer; 110. A third substrate layer. DETAILED DESCRIPTION

[0026] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present application.

[0027] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0028] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0029] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0030] like Figure 1-3 As shown, the present application relates to an optical composite film and a preparation method thereof, a backlight module, and a display panel. Figure 1 As shown, the optical composite film includes: a first substrate layer 10; the first substrate layer 10 refers to a basic material layer, which can achieve a good supporting effect; at the same time, it can also cooperate with other components to achieve multiple functional effects.

[0031] It should be noted that the first substrate layer 10 includes two end surfaces, one end surface being a light emitting surface and the other end surface being a light incident surface.

[0032] Preferably, the first substrate layer 10 includes, but is not limited to, any one of polyethylene terephthalate (PET), polycarbonate (PC) or polymethyl methacrylate (PMMA), which has excellent mechanical properties, transparency and heat resistance, and serves as the main first substrate layer 10 in the optical composite film, providing strength and stability while maintaining the transparency of the material; it can also achieve the effect of having a variety of materials to choose from, thereby achieving the effect of flexible use.

[0033] The first prism layer 20 is disposed on the first substrate layer 10, and can achieve good prism molding, thereby ensuring good optical performance. The optical film brightening functional layer, the prism structure is formed by UV glue by mold embossing and curing.

[0034] The second substrate layer 30 is disposed on the first prism layer 20 at a side away from the first substrate layer 10 ; it can achieve good bearing and fixing effects, thereby ensuring a stable interlayer structure.

[0035] The polarizer 40 is disposed on the second substrate layer 30 on the side away from the first prism layer 20; the first prism layer 20 and the second substrate layer 30 may respectively refract light, control the direction of light propagation or provide structural support, while the polarizer 40 is responsible for allowing light in a specific direction to pass through and blocking light in other directions, thereby enhancing the contrast of the display or improving the efficiency of light utilization.

[0036] The PSA layer 50 is disposed on the polarizer 40 on the side away from the second substrate layer 30; the PSA layer 50 is used to firmly adhere the polarizer 40 to another substrate or optical component, for example, in a display or touch panel, the polarizer 40 is fixed to a protective glass or other substrate. The PSA layer 50 needs to have high transparency and low refractive index to ensure that it does not interfere with the transmission of light, thereby maintaining the overall optical performance of the polarizer 40 and the optical component. The PSA layer 50 is a pressure-sensitive adhesive material and will eventually be attached to the panel glass.

[0037] The atomized back coating layer 60 is disposed on the first substrate layer 10 on the side away from the first prism layer 20; the atomized back coating layer 60 has high shielding properties and is obtained by stamping with a machined microstructure mold or coating with a particle-containing glue. Due to its high shielding properties, it can replace the lower diffuser plate, saving a layer of plate and reducing the thickness of the backlight module.

[0038] Among them, multiple layer structures are stacked in sequence according to a preset order to reduce the thickness of the optical composite film and improve the shielding degree, so as to achieve a good integrated polarizing composite film forming effect.

[0039] The present application can realize direct bonding between the substrate layer 30 and the lower polarizer 40 to reduce the air layer gap by about 1 mm, greatly reducing the thickness of the backlight module; The atomized layer is on top of the prism and the two can be directly attached, which can solve the problem of rainbow lines appearing when the prisms are crossed and improve the shielding performance; The back-coated atomized layer can replace the lower diffuser plate, reducing material usage costs, improving assembly efficiency, and making the backlight module thinner and lighter.

[0040] From the above description, it can be seen that the present application achieves the following technical effects: In the embodiment of the present application, an integrated bonding method is adopted, and multiple layer structures are stacked in sequence according to a preset order to reduce the thickness of the optical composite film and increase the shielding degree, so as to achieve the purpose of forming an integrated polarized composite film, thereby achieving the technical effects of reducing the thickness of the optical composite film, reducing the production cost and improving the shielding degree, thereby solving the problem that the existing optical film generally uses multiple structures to meet the brightness requirements, resulting in low assembly efficiency, easy scratches and reduced brightness, and there is a GAP gap between the upper diffuser and the lower polarizer 40, resulting in a thicker backlight module and relatively high production cost; at the same time, if the combination of multiple prisms is not matched with an upper diffuser, rainbow patterns will appear, the picture quality is poor, and the assembly is easy to be scratched, resulting in a decrease in brightness; and the direct backlight is generally used with a lower diffuser, resulting in a thicker backlight module. Technical problems.

[0041] Furthermore, a first bonding adhesive layer 70 is provided between the first prism layer 20 and the second substrate layer 30. It is understood that a good interlayer connection effect can be ensured, thereby ensuring the stability of the structure. The first bonding adhesive layer 70 plays an adhesive role, bonding the first prism layer 20 and the second substrate layer 30 together.

[0042] Furthermore, a second bonding adhesive layer 80 is provided between the second substrate layer 30 and the polarizer 40; Wherein, particles are arranged in the second bonding adhesive layer 80. It can be understood that a good interlayer connection effect can be ensured, thereby ensuring the stability of the structure; at the same time, by adding particles, a certain haze can be provided to play a shielding role.

[0043] Specifically, the particle-containing bonding adhesive layer is obtained by mixing diffused particles into bonding adhesive, which can provide a certain haze to play a shielding role, and can also bond the second substrate layer 30 and the polarizer 40 together, thereby eliminating the gap between the polarizer 40 and the composite film in the traditional structure, greatly reducing the total thickness.

[0044] Furthermore, a release film 90 is provided on the side of the PSA layer 50 away from the polarizer 40 to form an integrated polarizing composite film. It can be understood that a good protective effect on the film can be achieved. Preferably, the release film 90 is made of PE or PET and is a consumable material on the product.

[0045] like Figure 2 As shown, a second prism layer 100 and a third substrate layer 110 are sequentially stacked between the first substrate layer 10 and the atomized back coating layer 60 from top to bottom; The first prism portion of the first prism layer 20 and the second prism portion of the second prism layer 100 are two groups of orthogonal prisms. It can be understood that good optical performance can be achieved.

[0046] Furthermore, the first prism layer 20 and the second prism layer 100 are of equal height or unequal height.

[0047] Further, the first prism layer 20 has a shaking shape, and / or the second prism layer 100 has a shaking shape. It is understandable that in order to improve the anti-interference ability of the product, in the above two states, one group of prisms has a shaking shape, or both groups of prisms have a shaking shape.

[0048] like Figure 3 As shown, a first bonding adhesive layer 70 is disposed between the first prism layer 20 and the second substrate layer 30 , and a second bonding adhesive layer 80 is disposed between the second substrate layer 30 and the polarizer 40 ; Wherein, particles are provided in the first bonding adhesive layer 70, or particles are provided in the second bonding adhesive layer 80. It can be understood that a good interlayer connection effect can be achieved; at the same time, particles can be added to the corresponding bonding adhesive layer according to actual use requirements, so as to achieve a shielding effect.

[0049] Furthermore, the cross-sections of the first prism layer 20 and the second prism layer 100 are both isosceles triangles, and the width of the bases thereof is 10um-80um. It is understandable that good optical performance can be achieved, and a variety of widths can be flexibly selected.

[0050] Furthermore, the vertex angles of the first prism layer 20 and the second prism layer 100 are 60-95°. It is understandable that a variety of vertex angles can be selected, thereby achieving a flexible use effect.

[0051] Furthermore, the refractive index of the first prism layer 20 and the second prism structure layer is in the range of 1.5-1.7. It can be understood that a good refractive index can be ensured.

[0052] Furthermore, the thickness of the first substrate layer 10, the second substrate layer 30 and the third substrate layer 110 is 20um-300um. It can be understood that a good supporting effect can be achieved, and at the same time, a variety of sizes can be selected.

[0053] The specific examples are further described below: Example 1 Adopt liquid crystal glass paste integrated polarized DOP composite film.

[0054] At this time, after testing, the results of the optical composite film are: excellent shielding effect, excellent film scratch resistance, module thickness is 8mm, assembly efficiency is excellent, there is no rainbow pattern phenomenon, and the brightness ratio is 138%.

[0055] Example 2 The difference between Example 2 and Example 1 is that a liquid crystal glass-attached integrated polarizing POP composite film is used.

[0056] At this time, after testing, the results of the optical composite film are: excellent shielding effect, excellent film scratch resistance, module thickness is 8mm, assembly efficiency is excellent, there is no rainbow pattern phenomenon, and the brightness ratio is 162%.

[0057] Comparative Example 1 The difference between Comparative Example 1 and Example 1 is that a general lower polarizer 40+DOP composite film+diffuser plate is used to attach the liquid crystal glass.

[0058] At this time, after testing, the results of the optical composite film are: excellent shielding effect, excellent scratch resistance of the film, module thickness is 11mm, assembly efficiency is low, there is no rainbow pattern phenomenon, and the brightness ratio is 130%.

[0059] Comparative Example 2 The difference between Comparative Example 2 and Example 1 is that a liquid crystal glass is attached with a general lower polarizer 40 + an upper diffusion film + a POP composite film + a diffusion plate.

[0060] At this time, after testing, the results of the optical composite film are: good shielding effect, poor scratch resistance of the film, module thickness is 11mm, assembly efficiency is low, rainbow pattern phenomenon is slight, and brightness ratio is 153%.

[0061] It should be noted that the comparative example is a combination of optical films in a backlight module commonly used in the market, and a direct-type liquid crystal display is used as a comparison object.

[0062] The results of various embodiments and comparative examples are shown in Table 1: Table 1 From the above test results we can see that: Through Examples 1-2 and Comparison 1-2, it can be seen that both DOP and POP are integrated lamination solutions that can replace the diffuser plate, saving a layer of material cost and making the product thinner. The lamination layer contains particles to form haze, which can effectively replace the upper diffuser film. And it is integrated with the lower polarizer, and the assembly efficiency is increased by more than 50%.

[0063] The present invention also has the following beneficial effects: 1. This application provides a single film solution with high brightness, high shielding, good scratch resistance, and anti-interference comprehensive effects. It can also improve assembly efficiency and make display products thinner and lighter.

[0064] 2. High-shielding atomized back coating can replace the diffuser plate, making the product lighter and thinner.

[0065] 3. Directly bond with the lower polarizer to reduce the gap between the film materials.

[0066] The present application also relates to a backlight module, comprising the optical composite film as described above, which can be used in a liquid crystal display device to improve the display quality of the display device.

[0067] The present application also relates to a display panel, comprising the backlight module as described above.

[0068] The display panel of this embodiment may be: a liquid crystal panel, electronic paper, a liquid crystal television, a liquid crystal display, or any other product or component having a display function.

[0069] The present application also relates to a method for preparing an optical composite film, which is applied to prepare the optical composite film as described above; the method comprises the following steps: Step 1: preparing a first substrate layer 10; Step 2: coating a first photocurable coating on the first substrate layer 10; Step 3: Using a mold to obtain the first prism layer 20 by embossing using a light-curing transfer process; Step 4: preparing a second substrate layer 30; Step 5, coating adhesive on both sides of the second substrate layer 30 respectively; Step 6: Paste the second substrate layer 30 onto the first prism layer 20 on the side away from the first substrate layer 10 by heat pressing or gluing; Step 7: attaching the polarizer 40 to the side of the second substrate layer 30 away from the first prism layer 20 by adhesive, and fixing the polarizer 40 by pressure-sensitive adhesive or heat pressing; Step 8: uniformly coating the PSA layer 50 on the side of the polarizer 40 away from the second substrate layer 30; Step nine, attaching a release film 90 to the PSA layer 50; Step 10: coating a hazed back coating layer 60 on the side of the first substrate layer 10 away from the first prism layer 20 .

[0070] Specifically, step 1: preparing a first substrate layer 10; Providing the basic structural layer of the optical film, a transparent substrate with good optical properties and mechanical strength is usually selected.

[0071] The first substrate layer 10 is generally made of PET (polyester) or PC (polycarbonate) material, which has good light transmittance, heat resistance and mechanical strength, and is suitable for optical film applications.

[0072] The thickness of the substrate layer ranges from 50 to 200 microns, and is selected based on the final use of the film.

[0073] Step 2: coating a first photocurable coating on the first substrate layer 10; Provides a base coating for the subsequent formation of the prism layer, and hardens the coating through a photocuring process.

[0074] Light-curing coatings are usually ultraviolet light-curing resins (UV resins) with good optical transparency and hardening properties.

[0075] The coating is evenly applied using a precision coater, and the coating thickness is generally between 10-50 microns, ensuring the uniformity and flatness of the coating.

[0076] During the photocuring process, an ultraviolet light source with a wavelength of 365nm is used for irradiation. The irradiation time is determined according to the type and thickness of the coating, generally ranging from a few seconds to tens of seconds.

[0077] Step 3: Obtain the first prism layer 20 by embossing the mold using a light-curing transfer process; The prism layer is formed by embossing the light-curing coating using a mold structure.

[0078] The mold surface has a microstructured prism shape, usually a metal mold or a specially processed polymer mold.

[0079] The photocuring transfer process is to press the mold onto the surface of the photocuring coating that has not been fully cured, and cure the coating in the mold through ultraviolet light irradiation, thereby forming a layer with a microscopic prismatic structure.

[0080] During the embossing process, the mold applies a certain pressure (usually 0.1-0.5MPa) for a few seconds to tens of seconds to ensure that the coating is formed without bubbles or defects.

[0081] The structural parameters of the prism layer include height, angle, spacing, etc., which are usually adjusted according to the optical design requirements. For example, the prism height is generally in the range of 5-50 microns.

[0082] Step 4: preparing the second substrate layer 30; As the second layer of the composite membrane, it provides support and stability.

[0083] The second substrate layer 30 is generally similar to the first substrate layer 10 and can be made of PET or PC.

[0084] Step 5: Coating adhesive on both sides of the second substrate layer 30; Adhesive is coated on both sides of the second substrate layer 30 for subsequent interlayer bonding.

[0085] The adhesive can be acrylic or epoxy based, with high clarity and good adhesion.

[0086] The adhesive is uniformly coated on both sides of the second substrate layer 30 using a coating device, and the coating thickness is generally 5-20 microns.

[0087] Step 6: Paste the second substrate layer 30 onto the first prism layer 20 on the side away from the first substrate layer 10 by heat pressing or gluing; The second substrate layer 30 is bonded to the first prism layer 20 to form a composite structure.

[0088] It is heated by a heat press at a temperature of 100-150°C and a certain pressure (about 0.2-0.6 MPa) is applied, and the bonding time is about 5-30 seconds.

[0089] If gluing is adopted, UV curing glue or hot melt glue can be used, and the bonding is completed by irradiating ultraviolet light or heating.

[0090] Step 7: attaching the polarizer 40 to the side of the second substrate layer 30 away from the first prism layer 20 by adhesive; A polarizer 40 is bonded to the other side of the second substrate layer 30 to impart a polarizing optical function to the composite film.

[0091] The polarizer 40 can be fixed by pressure sensitive adhesive (PSA) or heat pressing. If pressure sensitive adhesive is used, ensure that the adhesive layer is uniform and free of bubbles; if heat pressing is used, it is usually heated and bonded at 60-100°C.

[0092] The thickness of the polarizer 40 is generally 50-200 microns, which is selected according to specific requirements.

[0093] Step 8: uniformly coating the PSA layer 50 on the side of the polarizer 40 away from the second substrate layer 30; A pressure sensitive adhesive (PSA layer 50 ) is coated on the surface of the polarizer 40 to facilitate subsequent film material adhesion.

[0094] Use a coater to evenly coat PSA, the coating thickness is usually 10-30 microns. Ensure that the adhesive layer is uniform and has good transparency.

[0095] Step nine: attaching a release film 90 to the PSA layer 50; The PSA layer 50 is protected from contamination and damage during transportation and storage.

[0096] Usually, materials with low adhesion and easy peeling are selected, such as PET film coated with silicone oil.

[0097] The release film 90 is evenly attached to the surface of the PSA layer 50 by a laminating device to ensure that there are no bubbles or wrinkles.

[0098] Step 10: coating a hazed back coating layer 60 on the side of the first substrate layer 10 away from the first prism layer 20; The composite film is given specific scattering optical properties and its optical performance is enhanced.

[0099] Commonly used polyurethane or acrylic coatings have good atomization effect.

[0100] The coating thickness is generally 5-20 microns by spraying or roller coating.

[0101] After the coating is formed, it needs to be dried and cured. The drying temperature is usually 50-80°C and the time is about 5-10 minutes.

[0102] The preferred embodiments of the present invention are described in detail above in conjunction with the accompanying drawings. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, various equivalent transformations can be made to the technical scheme of the present invention, and these equivalent transformations all belong to the protection scope of the present invention.

Claims

1. An optical composite film, characterized in that: include: A first substrate layer (10); A first prism layer (20) is disposed on the first substrate layer (10); A second substrate layer (30) is disposed on the first prism layer (20) at a side away from the first substrate layer (10); A polarizing film (40) is arranged on the second substrate layer (30) at a side away from the first prism layer (20); A PSA layer (50) is disposed on the polarizer (40) at a side away from the second substrate layer (30); and A hazed back coating layer (60) is disposed on the first substrate layer (10) at a side away from the first prism layer (20); Wherein, a plurality of layer structures are stacked in sequence according to a preset order so as to reduce the thickness of the optical composite film and improve the shielding degree.

2. The optical composite film according to claim 1, characterized in that: A first bonding adhesive layer (70) is provided between the first prism layer (20) and the second substrate layer (30).

3. The optical composite film according to claim 1, characterized in that: A second bonding adhesive layer (80) is provided between the second substrate layer (30) and the polarizer (40); Wherein, particles are arranged in the second bonding adhesive layer (80).

4. The optical composite film according to claim 1, characterized in that: A release film (90) is provided on the side of the PSA layer (50) away from the polarizer (40) to form an integrated polarizing composite film.

5. The optical composite film according to claim 1, characterized in that: A second prism layer (100) and a third substrate layer (110) are stacked in sequence from top to bottom between the first substrate layer (10) and the atomized back coating layer (60); The first prism portion of the first prism layer (20) and the second prism portion of the second prism layer (100) are two groups of orthogonal prisms.

6. The optical composite film according to claim 5, characterized in that: The first prism layer (20) adopts a shaking appearance, and / or the second prism layer (100) adopts a shaking appearance.

7. The optical composite film according to claim 6, characterized in that: A first bonding adhesive layer (70) is provided between the first prism layer (20) and the second substrate layer (30), and a second bonding adhesive layer (80) is provided between the second substrate layer (30) and the polarizer (40); Wherein, particles are arranged in the first bonding adhesive layer (70), or particles are arranged in the second bonding adhesive layer (80).

8. The optical composite film according to claim 5, characterized in that: The cross-sections of the first prism layer (20) and the second prism layer (100) are both isosceles triangles, and the width of their bases is 10 um-80 um.

9. The optical composite film according to claim 5, characterized in that: The vertex angles of the first prism layer (20) and the second prism layer (100) are 60-95°.

10. The optical composite film according to claim 5, characterized in that: The refractive index range of the first prism layer (20) and the second prism structure layer is 1.5-1.

7.

11. The optical composite film according to claim 5, characterized in that: The thickness of the first substrate layer (10), the second substrate layer (30) and the third substrate layer (110) is 20 um-300 um.

12. A backlight module, characterized in that: The optical composite film comprises the optical composite film as claimed in any one of claims 1 to 11.

13. A display panel, characterized in that Comprising the backlight module as claimed in claim 12.

14. A method for preparing an optical composite film, characterized in that: The method is used for preparing an optical composite film according to any one of claims 1 to 11; comprising the following steps: Step 1: preparing a first substrate layer (10); Step 2: coating a first photocurable coating on the first substrate layer (10); Step 3: Using a mold to obtain a first prism layer (20) by embossing using a light-curing transfer process; Step 4: preparing a second substrate layer (30); Step 5: coating adhesive on both sides of the second substrate layer (30); Step 6: Paste the second substrate layer (30) onto the first prism layer (20) on the side away from the first substrate layer (10) by heat pressing or gluing; Step 7: A polarizer (40) is bonded to the side of the second substrate layer (30) away from the first prism layer (20) by means of an adhesive, and the polarizer (40) is fixed by means of a pressure-sensitive adhesive or heat pressing; Step 8: uniformly coating the PSA layer (50) on the side of the polarizer (40) away from the second substrate layer (30); Step nine, attaching a release film (90) to the PSA layer (50); Step 10: coating a haze back coating layer (60) on the side of the first substrate layer (10) away from the first prism layer (20).

Citation Information

Patent Citations

  • Optical film

    CN101295047A

  • Optical film, polarizing sheet, backlight module and display device

    CN107238976A

  • Optical composite film and preparation method thereof

    CN111443516A

  • COP multilayer composite film and preparation method thereof

    CN117170139A

  • Multilayer polarization brightening optical laminating film

    CN215986824U