Photoelectric detector

By designing structures of different types of doped regions and highly doped regions in the photodetector, the electric field in the absorption layer and the carrier transmission distance are shortened, and the problem of taking into account both the response and bandwidth of the silicon-based photodetector is achieved with high efficiency photoelectric detection effect and low power consumption.

CN119092569APending Publication Date: 2024-12-06WUHAN OPTICAL VALLEY INFORMATION OPTOELECTRONICS INNOVATION CENT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411108938.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Existing silicon-based photodetectors are difficult to balance between responsiveness and bandwidth, high responsiveness is usually accompanied by lower bandwidth, and the introduction of new materials or structural complexity increases manufacturing costs and process difficulty.

Method used

Design a photodetector, including different types of doped regions arranged sequentially on the substrate layer, the absorption layer is provided with a highly doped region close to the upper surface, and is connected to the electrode through an interconnected structure, using P-type and N-type doped regions. The concentration, position and width are reasonably designed to enhance the electric field in the absorption layer and shorten the transmission distance of photogenerated carriers.

Benefits of technology

It significantly improves the bandwidth and responsiveness of the photodetector and operates at lower voltages to achieve low power consumption, avoiding increasing manufacturing process complexity and cost while improving device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119092569A_ABST
    Figure CN119092569A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a photoelectric detector. The photoelectric detector comprises a substrate layer; the insulating layer is positioned on the substrate layer; the optical waveguide is positioned on the insulating layer; wherein the optical waveguide comprises a first type heavily doped region, a first type highly doped region, a first type doped region, a first intrinsic region, a first second type doped region, a second intrinsic region, a second second type doped region, a second type highly doped region and a second type heavily doped region which are sequentially arranged in a first direction; the first type is different from the second type; the first direction is parallel to the top surface of the substrate layer; the absorption layer is positioned on the optical waveguide; wherein the absorption layer close to the upper surface comprises a second first type highly doped region; the material of the absorption layer is different from that of the optical waveguide; and the interconnection structure is arranged to connect the first type heavily doped region and the second first type heavily doped region to the first electrode and connect the second type heavily doped region to the second electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the technical field of optical communication devices, and more specifically, relates to a photodetector. Background Art

[0002] With the development of 5G networks, optical interconnection in data centers, and high-performance computing systems, the demand for data transmission rate and processing power has increased dramatically, and high-bandwidth photodetectors are one of the key components to achieve high-speed data transmission. In order to achieve more compact and lower-cost optoelectronic devices, integrated optoelectronic technology has developed rapidly, among which silicon-based optoelectronic platforms have attracted much attention due to their high compatibility with mature CMOS processes. Summary of the invention

[0003] In view of this, an embodiment of the present application provides a photodetector to solve at least one problem existing in the background technology.

[0004] An embodiment of the present application provides a photodetector, which includes: a substrate layer; an insulating layer, located on the substrate layer; an optical waveguide, located on the insulating layer; wherein the optical waveguide includes a first type heavily doped region, a first first type high doped region, a first type doped region, a first intrinsic region, a first second type doped region, a second intrinsic region, a second second type doped region, a second type high doped region, and a second type heavily doped region arranged in sequence in a first direction; the first type is different from the second type; the first direction is a direction parallel to the top surface of the substrate layer; an absorption layer, located on the optical waveguide; wherein the absorption layer includes a second first type high doped region near the upper surface; the material of the absorption layer is different from that of the optical waveguide; an interconnection structure, configured to connect the first type heavily doped region and the second first type high doped region to the first electrode, and to connect the second type heavily doped region to the second electrode.

[0005] In some embodiments, the center of the first second type doped region and the center of the absorption layer have an offset in the first direction, and the offset value is greater than or equal to zero; and / or the second first type highly doped region is located directly above the first second type doped region.

[0006] In some embodiments, the material of the optical waveguide includes silicon, and the material of the absorption layer includes germanium or germanium-silicon alloy.

[0007] In some embodiments, the absorption layer has a size range of 400nm to 3000nm in the first direction, a size range of 200nm to 700nm in the second direction, and a size range of 5μm to 100μm in the third direction; wherein the second direction is a direction perpendicular to the top surface of the substrate layer, and the second direction is perpendicular to the third direction.

[0008] In some embodiments, the absorption layer covers at least the first intrinsic region, the first second type doping region, and the second intrinsic region.

[0009] In some embodiments, the doping concentration range of the first type heavily doped region and the second type heavily doped region is 8×10 19 cm -3 ~1×10 21 cm -3 , and the doping concentration range of the first type high doping region, the second type high doping region and the second type high doping region is 8×10 17 cm -3 ~5×10 18 cm -3 , and the doping concentration range of the first type doping region, the first second type doping region and the second second type doping region is 1×10 17 cm -3 ~4×10 17 cm -3 .

[0010] In some embodiments, the optical waveguide type includes a strip waveguide or a ridge waveguide.

[0011] In some embodiments, the photodetector further includes: a tapered waveguide connected to the optical waveguide in a direction parallel to the top surface of the substrate layer and perpendicular to the first direction; the dimension of the tapered waveguide connected to the optical waveguide in the first direction is equal to or smaller than the dimension of the absorption layer in the first direction.

[0012] In some embodiments, the interconnect structure includes: a first via layer, including a plurality of conductive vias respectively contacting a first type heavily doped region, a second first type highly doped region, and a second type heavily doped region; a first metal layer, located on the first via layer and connected to the first via layer; a second via layer, located on the first metal layer and connected to the first metal layer; a second metal layer, located on the second via layer and connected to the second via layer; wherein the second metal layer includes a first electrode and a second electrode; wherein the plurality of conductive vias are distributed in an array or spliced ​​together to form a whole.

[0013] In some embodiments, the first electrode and the second electrode materials include copper / copper alloy or aluminum / aluminum alloy, which are used to connect to an external voltage source, a transimpedance amplifier or a signal source of the photodetector.

[0014] Each embodiment provided in this application has at least one of the following beneficial effects:

[0015] The photodetector provided in the present application has a first type (e.g., P-type) highly doped region placed near the upper surface of the absorption layer (e.g., the material of the absorption layer is germanium), and the highly doped region is connected to the first electrode through an interconnection structure. Such a design can significantly shorten the transmission distance of photogenerated carriers in the device, thereby improving the bandwidth of the detector;

[0016] The photodetector provided by the present application uses the first type (e.g., P-type) doping in the absorption layer, so that the device conducts photocurrent through photogenerated electrons. Compared with hole conduction, the mobility of electrons is higher, which further improves the bandwidth of the photodetector.

[0017] The photodetector provided in the present application has a first type (e.g., P-type) and a second type (e.g., N-type) doped regions respectively arranged on the upper and lower sides of an absorption layer (e.g., the material of the absorption layer is germanium), and the concentration, position, and width of the two doped regions are reasonably designed (e.g., can be achieved through a photolithography process, an ion implantation process, etc.) to ensure that they can effectively enhance the electric field in the absorption layer; when a voltage is applied, the enhanced electric field can excite the Franz-Keldysh effect of the absorption layer material, thereby improving the responsivity of the photodetector;

[0018] The photodetector provided in the present application has a unique doping structure (eg, an optical waveguide includes a plurality of different doping regions) design, which enables the photodetector to operate at a lower voltage, thereby achieving a low power consumption effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In the accompanying drawings (which are not necessarily drawn to scale), like reference numerals may describe similar components in different views. Like reference numerals with different letter suffixes may represent different examples of similar components. The accompanying drawings generally illustrate various embodiments discussed herein by way of example and not limitation.

[0020] Figure 1A A top view of the structure of a photoelectric detector provided in an embodiment of the present application;

[0021] Figure 1B A cross-sectional view of a photodetector provided in an embodiment of the present application;

[0022] Figure 1C A cross-sectional view of another photodetector provided in an embodiment of the present application;

[0023] Figure 2 A schematic diagram of a process for manufacturing a photoelectric detector provided in an embodiment of the present application;

[0024] 3A to 3HA schematic cross-sectional view of the device structure of the photodetector provided in an embodiment of the present application during the manufacturing process;

[0025] Figure 4 A cross-sectional view of another photodetector provided in an embodiment of the present application;

[0026] Figure 5A A comparison diagram of electric fields between a photodetector and another photodetector provided according to an embodiment of the present application;

[0027] Figure 5B The figure is a comparison diagram of bandwidth response curves of a photodetector and another photodetector provided according to an embodiment of the present application. DETAILED DESCRIPTION

[0028] In order to make the technical solutions and advantages of the embodiments of the present application clearer, the technical solutions of the present application are further elaborated in detail below in conjunction with the accompanying drawings and specific embodiments of the specification.

[0029] In the embodiments of the present application, the terms "first", "second", etc. are used to distinguish similar objects, but are not used to describe a specific order or sequence.

[0030] In the embodiments of the present application, unless otherwise clearly specified and limited, the “upper” or “lower” relationship between two layers in a semiconductor structure may be direct contact between the two layers, or indirect contact between the two layers through an intermediate layer.

[0031] In the embodiments of the present application, the term "layer" refers to a material portion including an area with a thickness. The layer may extend over the entirety of the lower or upper structure, or may have a range that is smaller than the range of the lower or upper structure. In addition, a layer may be a region of a homogeneous or inhomogeneous continuous structure having a thickness that is less than the thickness of the continuous structure. For example, a layer may be located between the top and bottom surfaces of a continuous structure, or a layer may be between any horizontal pairs at the top and bottom surfaces of a continuous structure. A layer may extend horizontally, vertically and / or along an inclined surface. Furthermore, a layer may include multiple sublayers.

[0032] In the embodiments of the present application, spatially relative terms, such as "below", "below", "downward", "above", "above", "up", "upward", etc., can describe the relationship of one element or feature to another (multiple) elements or (multiple) features for ease of description in this article, as shown in the figures. Spatially relative terms are intended to cover different orientations of the device in use or operation other than the orientation depicted in the figure. The device can be oriented in other ways (rotated 90 degrees or in other orientations), and the spatially relative descriptors used in this article can also be interpreted accordingly.

[0033] The silicon itself of silicon photodetectors has a weak absorption of light in the telecommunication band, so it is necessary to enhance the detection performance of photodetectors by introducing other materials such as germanium. However, germanium-silicon photodetectors often face a trade-off between responsivity and bandwidth, that is, high responsivity is usually accompanied by lower bandwidth, and vice versa. New structures and designs can be developed on mature silicon-based optoelectronic platforms to break this limitation, for example, introducing group III, group V materials or graphene to enhance the absorption performance of photodetectors, and directly introducing strained layers and quantum dots on the germanium-silicon structure of photodetectors to optimize absorption performance. However, although these methods have potential, they inevitably introduce additional complexity, resulting in increased manufacturing process costs and possible reductions in device yield. Therefore, it is very meaningful to achieve integrated photodetectors with both high responsivity and high bandwidth without increasing too much process difficulty or cost.

[0034] An embodiment of the present application provides a photodetector, which includes: a substrate layer; an insulating layer, located on the substrate layer; an optical waveguide, located on the insulating layer; wherein the optical waveguide includes a first type heavily doped region, a first first type high doped region, a first type doped region, a first intrinsic region, a first second type doped region, a second intrinsic region, a second second type doped region, a second type high doped region, and a second type heavily doped region arranged in sequence in a first direction; the first type is different from the second type; the first direction is a direction parallel to the top surface of the substrate layer; an absorption layer, located on the optical waveguide; wherein the absorption layer includes a second first type high doped region near the upper surface; the material of the absorption layer is different from that of the optical waveguide; an interconnection structure, configured to connect the first type heavily doped region and the second first type high doped region to the first electrode, and to connect the second type heavily doped region to the second electrode.

[0035] It should be noted that the first type and the second type are different, which can be understood as: the first type is P-type, and the second type is N-type; or, the first type is N-type, and the second type is P-type.

[0036] Figure 1A A top view of the structure of a photodetector provided in an embodiment of the present application. Figure 1B A cross-sectional view of a photodetector provided in an embodiment of the present application. Figure 1C A cross-sectional view of yet another photodetector provided in an embodiment of the present application.

[0037] refer to Figure 1A and Figure 1B, the first type is P type, and the second type is N type. The embodiment of the present application provides a photodetector, which includes: a substrate layer 100; an insulating layer 200, located on the substrate layer 100; an optical waveguide 300, located on the insulating layer 200; wherein the optical waveguide 300 includes a P-type heavily doped region 301, a first P-type highly doped region 302, a P-type doped region 303, a first intrinsic region 304, a first N-type doped region 305, a second intrinsic region 306, a second N-type doped region 307, an N-type highly doped region 308, and a first intrinsic region 309. doped region 308, N-type heavily doped region 309; the first direction is a direction parallel to the top surface of the substrate layer; an absorption layer 400, located on the optical waveguide 300; wherein the absorption layer 400 includes a second P-type highly doped region 401 near the upper surface; the material of the absorption layer 400 is different from that of the optical waveguide 300; an interconnection structure, configured to connect the P-type heavily doped region 301 and the second P-type highly doped region 401 to the first electrode 801, and to connect the N-type heavily doped region 309 to the second electrode 802.

[0038] refer to Figure 1C , the first type is N type, and the second type is P type. The embodiment of the present application provides a photodetector, which includes: a substrate layer 100; an insulating layer 200, located on the substrate layer 100; an optical waveguide 300, located on the insulating layer 200; wherein the optical waveguide 300 includes an N-type heavily doped region 301, a first N-type highly doped region 302, an N-type doped region 303, a first intrinsic region 304, a first P-type doped region 305, a second intrinsic region 306, a second P-type doped region 307, and a P-type highly doped region 308 arranged in sequence in a first direction. doped region 308, P-type heavily doped region 309; the first direction is a direction parallel to the top surface of the substrate layer; an absorption layer 400, located on the optical waveguide 300; wherein the absorption layer 400 includes a second N-type highly doped region 401 near the upper surface; the material of the absorption layer 400 is different from that of the optical waveguide 300; an interconnection structure, configured to connect the N-type heavily doped region 301 and the second N-type highly doped region 401 to the first electrode 801, and to connect the P-type heavily doped region 309 to the second electrode 802.

[0039] Below, reference Figure 1A and Figure 1B , a photodetector of the first type being P type and a photodetector of the second type being N type is taken as an example for detailed description.

[0040] Figure 1B The photodetector shown is Figure 1C The photodetectors shown differ mainly in the interchange of doping types, e.g. Figure 1B The first type heavily doped region 301 of the photodetector shown is a P-type heavily doped region, and the second type heavily doped region 309 is an N-type heavily doped region. Figure 1CThe first type heavily doped region 301 of the photodetector shown is an N-type heavily doped region, and the second type heavily doped region 309 is a P-type heavily doped region. Figure 1C Other features of the photodetector and its manufacturing method shown in the figure can be similarly referred to below. Figure 1B Details of the photodetector and its manufacturing method are shown.

[0041] Here and below, the first direction may be the direction of electron flow of the photodetector, the second direction may be the direction of stacking of the various layers of the photodetector, and the third direction may be the propagation direction of the incident light (or optical signal) of the photodetector. The substrate (or substrate layer) may include a top surface (or top surface) on the front side and a bottom surface (or bottom surface) on the back side opposite to the front side: ignoring the flatness of the top surface and the bottom surface, the direction perpendicular to the top surface and the bottom surface of the substrate is defined as the second direction. The second direction is also the stacking direction of the various layers of the structure subsequently deposited on the substrate, or the height direction of the device. The surface where the top and bottom surfaces of the substrate are located, or strictly speaking, the center plane in the thickness direction of the substrate, is determined as the substrate plane. Two mutually intersecting (for example, perpendicular to each other) first directions and third directions are defined in the direction of the substrate plane. For the convenience of describing the embodiments of the present application, the first direction may be represented as the x direction in the accompanying drawings; the second direction may be represented as the y direction in the accompanying drawings; and the third direction may be represented as the z direction in the accompanying drawings.

[0042] Here and below, the terms "heavily doped region", "highly doped region", "doped region" and "intrinsic region" may be understood as regions with different doping concentrations; the doping concentration of the term "heavily doped region" is greater than the doping concentration of the "highly doped region", the doping concentration of the "highly doped region" is greater than the doping concentration of the "doped region"; the doping concentration of the term "intrinsic region" or the concentration of impurity elements it has should be less than the doping concentration of the "doped region". For example, the doping concentration of the P-type heavily doped region 301 is greater than the doping concentration of the first P-type highly doped region 302. Concentration, the doping concentration of the first P-type high doping region 302 is greater than the doping concentration of the P-type doping region 303; for another example, the doping concentrations of the first N-type doping region 305 and the second N-type doping region 307 are both lower than the doping concentration of the N-type high doping region 308, and the doping concentration of the N-type high doping region 308 is lower than the doping concentration of the N-type heavily doped region 309; the doping concentrations of the first intrinsic region 304 and the second intrinsic region 306 are both lower than the doping concentrations of the P-type doping region 303, the first N-type doping region 305 or the second N-type doping region 307.

[0043] In some embodiments, the material of the substrate layer 100 may include a single semiconductor material (e.g., silicon (Si), germanium (Ge), etc.), a compound semiconductor material (e.g., silicon germanium (SiGe), etc.). In some embodiments, the material of the insulating layer 200 may include silicon oxide, such as silicon dioxide. The material of the optical waveguide 300 may be any semiconductor material, and the material of the optical waveguide 300 is not strictly limited here. In some embodiments, the semiconductor material includes silicon. In the following description, the semiconductor material may be silicon as an example for description.

[0044] Different regions formed by the optical waveguide 300 of the photodetector have different doping regions, including regions doped with P-type dopants and N-type dopants of different concentrations, and undoped regions (intrinsic regions).

[0045] The structure of the photodetector provided according to the embodiments of the present application will be described in detail below.

[0046] In some embodiments, the center of the first N-type doping region 305 and the center of the absorption layer 400 have an offset Δx in the first direction, and the value of the offset Δx is greater than or equal to zero; and / or, the second P-type highly doped region 401 is located directly above the first N-type doping region 305 .

[0047] In some embodiments, the center of the second P-type highly doped region 401 and the center of the first N-type doped region 305 have an offset Δx in the first direction, and the value of the offset is greater than or equal to zero.

[0048] Here and below, the term "center" may be understood as a center line extending along the y direction in a cross section (e.g., a plane formed by the x direction and the y direction). Figure 1B As shown, the center of the absorption layer 400 can refer to a first center line L1 in a plane formed by the x-direction and the y-direction, and the center of the second P-type highly doped region 401 can refer to a second center line L2 in a plane formed by the x-direction and the y-direction.

[0049] In some embodiments, the center of the optical waveguide 300 is located in the region where the first N-type doping region 305 is located in the first direction. Figure 1B As shown, the center of the optical waveguide 300 refers to the first center line L1, and the first center line L1 extends through the area where the first N-type doping region 305 is located, which can indicate that the center of the optical waveguide 300 is located in the area where the first N-type doping region 305 is located in the first direction. In some embodiments, the center of the absorption layer 400 and the center of the optical waveguide 300 coincide with each other in the first direction. For example, as Figure 1BAs shown, the centers of the absorption layer 400 and the optical waveguide 300 can refer to the first center line L1, which indicates that the centers of the absorption layer 400 and the optical waveguide 300 coincide with each other in the first direction.

[0050] Here and below, the term "coincidence" can be understood as coincidence within the range allowed by process errors. For example, the centers of the absorption layer 400 and the optical waveguide 300 are offset within a certain range in the first direction, and the offset within the certain range is within the range allowed by process errors. It can be considered that the centers of the absorption layer 400 and the optical waveguide 300 coincide with each other in the first direction.

[0051] In some embodiments, there is an offset Δx between the center of the first N-type doping region 305 and the center of the absorption layer 400 in the first direction, and the value of the offset Δx may be greater than or equal to zero. In practical applications, the offset direction of the offset Δx may be a direction from the first N-type doping region 305 to or away from the N-type heavily doped region 309 in the first direction. For example, Figure 1B As shown, in the first direction from the first N-type doping region 305 to the N-type heavily doped region 309 , the center of the first N-type doping region 305 deviates from the center of the absorption layer 400 , that is, the second center line L2 has an offset Δx with the first center line L1 .

[0052] In some embodiments, the second P-type highly doped region 401 is located directly above the first N-type doped region 305. In some embodiments, the second P-type highly doped region 401 covers the first N-type doped region 305. In some embodiments, the center of the second P-type highly doped region 401 and the center of the first N-type doped region 305 overlap in the first direction. Figure 1B As shown, the centers of the second P-type highly doped region 401 and the first N-type doped region 305 can refer to the second center line L2, and the centers of the second P-type highly doped region 401 and the first N-type doped region 305 overlap in the first direction.

[0053] In some embodiments, the material of the optical waveguide 300 is different from the material of the absorption layer 400. In some embodiments, the material of the optical waveguide 300 includes silicon, and the material of the absorption layer 400 includes germanium or germanium-silicon alloy. Exemplarily, the material of the optical waveguide 300 is silicon and its doping elements, and the material of the absorption layer 400 is germanium and its doping elements.

[0054] In some embodiments, the absorption layer 400 has a size range of 400nm to 3000nm in the first direction, a size range of 200nm to 700nm in the second direction, and a size range of 5μm to 100μm in the third direction; wherein the second direction is a direction perpendicular to the top surface of the substrate layer, and the second direction is perpendicular to the third direction.

[0055] In some embodiments, the doping depth of the second P-type highly doped region 401 ranges from 100 nm to 200 nm.

[0056] Here and below, the term “doping depth” may be understood as the junction depth. For example, the doping depth of the second P-type highly doped region 401 may be understood as the junction depth of the second P-type highly doped region 401 .

[0057] In some embodiments, the ratio of the size of the absorption layer 400 in the second direction to the doping depth of the second P-type highly doped region 401 is in the range of 2 to 10. In practical applications, the ratio of the size of the absorption layer 400 in the second direction to the doping depth of the second P-type highly doped region 401 is 3 or 4. In practical applications, the size of the absorption layer 400 in the second direction ranges from 200nm to 700nm, preferably, the size of the absorption layer 400 in the second direction is 240nm, 360nm or 600nm; the doping depth of the second P-type highly doped region 401 ranges from 100nm to 200nm, preferably, the doping depth of the second P-type highly doped region 401 is 120nm, 150nm or 180nm. For example, the size of the absorption layer 400 in the second direction is 360nm, and the doping depth of the second P-type highly doped region 401 is 120nm.

[0058] In some embodiments, the absorption layer 400 covers at least the first intrinsic region 304 , the first N-type doping region 305 , and the second intrinsic region 306 .

[0059] refer to Figure 1B In some embodiments, the first type is P-type and the second type is N-type photodetector, the absorption layer 400 covers the first intrinsic region 304, the first N-type doped region 305 and the second intrinsic region 306, and covers part of the P-type doped region 303 and part of the second N-type doped region 307; wherein the size of the first intrinsic region 304 in the first direction is greater than or equal to the size of the second intrinsic region 306 in the first direction.

[0060] refer to Figure 1C In some embodiments, the first type is N-type and the second type is P-type photodetector, and the absorption layer 400 covers the first intrinsic region 304, the first P-type doped region 305 and the second intrinsic region 306, and covers part of the N-type doped region 303 and part of the second P-type doped region 307; wherein the size of the first intrinsic region 304 in the first direction is less than or equal to the size of the second intrinsic region 306 in the first direction.

[0061] In some embodiments, the doping concentration range of the P-type heavily doped region 301 and the N-type heavily doped region 309 is 8×10 19 cm -3 ~1×10 21 cm-3 The doping concentration range of the first P-type high doping region 302, the N-type high doping region 308 and the second P-type high doping region 401 is 8×10 17 cm -3 ~5×10 18 cm -3 The doping concentration range of the P-type doping region 303, the first N-type doping region 305 and the second N-type doping region 307 is 1×10 17 cm -3 ~4×10 17 cm -3 .

[0062] In some embodiments, the doping concentration of the first intrinsic region 304 and the second intrinsic region 306 is less than a predetermined value, for example, less than 1×10 16 cm -3 .

[0063] In some embodiments, the doping concentration of the absorption layer 400 is less than a predetermined value. For example, the doping concentration of the absorption layer 400 is less than 1×10 16 cm -3 .

[0064] In some embodiments, the optical waveguide 300 type includes a strip waveguide or a ridge waveguide.

[0065] In some embodiments, the photodetector further includes: a tapered waveguide 10 connected to the optical waveguide 300 in a direction parallel to the top surface of the substrate layer and perpendicular to the first direction; the dimension of the tapered waveguide 10 connected to the optical waveguide 300 in the first direction is equal to or smaller than the dimension of the absorption layer 400 in the first direction. In practical applications, the dimension of the tapered waveguide 10 connected to the optical waveguide 300 in the first direction is equal to the dimension of the absorption layer 400 in the first direction.

[0066] In some embodiments, the incident light of the photodetector is adiabatically coupled into the optical waveguide 300 through a section of tapered waveguide 10. The tapered waveguide 10 and the optical waveguide 300 together form an optical waveguide structure, which limits the incident light to be transmitted along the length direction of the detector. This transmission structure makes the transit direction of the photogenerated carriers of the detector perpendicular to the light absorption direction, avoiding the restriction between the detector's responsivity and the carrier transit time. In addition, the width of the side where the tapered waveguide 10 is connected to the optical waveguide 300 is equal to the width of the absorption layer 400, which allows the incident light to be absorbed by the absorption layer 400 more instead of being dissipated in the silicon waveguide, effectively reducing the device loss.

[0067] In some embodiments, the interconnect structure includes: a first via layer, including multiple conductive vias 501, 502 and 503 respectively contacting the P-type heavily doped region 301, the second P-type highly doped region 401, and the N-type heavily doped region 309; a first metal layer, located on the first via layer and connected to the first via layer; a second via layer, located on the first metal layer and connected to the first metal layer; a second metal layer, located on the second via layer and connected to the second via layer; wherein the second metal layer includes a first electrode 801 and a second electrode 802; wherein the multiple conductive vias are distributed in an array or spliced ​​together to form a whole.

[0068] In some embodiments, the plurality of conductive vias 501 on the P-type heavily doped region 301, the plurality of conductive vias 503 on the N-type heavily doped region 309, or the plurality of conductive vias 502 on the second P-type highly doped region 401 are distributed in an array or are spliced ​​together to form a whole. For example, the plurality of conductive vias 501 on the P-type heavily doped region 301, the plurality of conductive vias 503 on the N-type heavily doped region 309, and the plurality of conductive vias 502 on the second P-type highly doped region 401 are distributed in an array.

[0069] In some embodiments, the first metal layer includes a first electrode layer 601 and a second electrode layer 602, and the plurality of conductive vias 701 on the first electrode layer 601 or the plurality of conductive vias 702 on the second electrode layer 602 are distributed in an array or spliced ​​together to form a whole. For example, the plurality of conductive vias 701 on the first electrode layer 601 and the plurality of conductive vias 702 on the second electrode layer 602 are distributed in an array.

[0070] In some embodiments, the first electrode 801 and the second electrode 802 are made of copper / copper alloy or aluminum / aluminum alloy, and are used to connect to an external voltage source, a transimpedance amplifier (TIA) or a signal source of the photodetector.

[0071] In some embodiments, the first electrode 801 and the second electrode 802 are used to connect to a transimpedance amplifier, and the electrical signal generated by the photodetector is provided to the transimpedance amplifier, which can convert the current signal received from the photodetector into a voltage signal. In some embodiments, the transimpedance amplifier converts the current signal received from the photodetector into a voltage signal as an output signal, and the output signal of the transimpedance amplifier is provided to a digital signal processor (DSP).

[0072] In some embodiments, the photodetector includes, in sequence along the second direction: a substrate layer 100; an insulating layer 200 located on the substrate layer 100; an optical waveguide 300 located on the insulating layer 200; and the optical waveguide 300 includes a P-type heavily doped region 301, a first P-type highly doped region 302, a P-type doped region 303, a first intrinsic region 304, a first N-type doped region 305, a second intrinsic region 306, a second N-type doped region 307, an N-type highly doped region 308, and an N-type heavily doped region 309 arranged in sequence in the horizontal direction. ; The absorption layer 400 of the device is located above the optical waveguide 300, and the light absorption layer 400 includes a second P-type highly doped region 401 near the upper surface; the first via layer includes a conductive via 501 in contact with the P-type heavily doped region 301, a conductive via 502 in contact with the second P-type highly doped region 401, and a conductive via 503 in contact with the N-type heavily doped region 309; the first metal layer includes a first electrode layer 601 connecting the conductive vias 501 and 502, and a second electrode layer 602 connecting the conductive via 503. The second via layer includes a conductive via 701 in contact with the first electrode layer 601, and a conductive via 702 in contact with the second electrode layer 602; the second metal layer includes a first electrode 801 connecting the conductive via 701, and a second electrode 802 connecting the conductive via 702; the cladding layer 900 is formed between the second metal layer and the insulating layer 200.

[0073] It should be noted that, in order to clearly show the relative positions of the insulating layer 200, the optical waveguide 300, the absorption layer 400, and the second metal layer (including the first electrode 801 and the second electrode 802) of the photodetector, Figure 1A The covering layer 900 between the second metal layer and the insulating layer 200 is omitted.

[0074] In practical applications, the material of the coating layer 900 may include but is not limited to silicon oxide or silicon nitride.

[0075] Figure 4 This is a cross-sectional view of another photodetector provided in an embodiment of the present application. It should be noted that: Figure 4 Another type of photodetector (hereinafter referred to as the second type of device) shown can be used as Figure 1B A control group of a photodetector (hereinafter referred to as the first type of device) is shown. Figure 4 The second type of device shown is similar to Figure 1B The first type of devices shown are mainly different in that: Figure 1B The first type of device shown, Figure 4 The second type of device shown lacks the second P-type highly doped region 401, the first N-type doped region 305, the conductive via 501, and the second intrinsic region 306 of the first type of device; Figure 4 The size of the first intrinsic region 304 in the second type of device shown is Figure 1B The first intrinsic region 304 , the first N-type doping region 305 , and the second intrinsic region 306 in the first type of device shown have the same size as a whole.

[0076] It should be noted that Figure 4 The various components / layers / structures / regions in the second type of device shown can refer to Figure 1B The same identified components / layers / structures / regions in the first type of devices shown are understood.

[0077] Figure 5A A comparison diagram of the electric fields of a photodetector and another photodetector provided according to an embodiment of the present application. Figure 5A It can be seen that the absorption layers of the two types of devices compared (exemplary material is germanium) have the same width size. It can be clearly seen that under the same operating voltage, the absorption layer of the first type of device has a higher electric field strength than that of the second type of device. This enhanced electric field can excite the Franz-Caldisi effect of the absorption layer material, thereby improving the responsivity of the photodetector. This unique doping structure design also enables the photodetector to operate at a lower voltage, thereby achieving a low power consumption effect.

[0078] Figure 5B The figure is a comparison diagram of bandwidth response curves of a photodetector and another photodetector provided according to an embodiment of the present application. Figure 5B It can be seen that the first type of device has a significant improvement in bandwidth. Compared with the second type of device, the first type of device can process high-speed signals more effectively, thus showing better performance in the field of data transmission and communication.

[0079] Each embodiment provided in this application has at least one of the following beneficial effects:

[0080] The photodetector provided in the present application has a P-type highly doped region placed near the upper surface of the absorption layer (for example, the material of the absorption layer is germanium), and the highly doped region is connected to the first electrode through an interconnection structure. Such a design can significantly shorten the transmission distance of photogenerated carriers in the device, thereby improving the bandwidth of the detector;

[0081] The photodetector provided by the present application uses P-type doping in the absorption layer, so that the device conducts photocurrent through photogenerated electrons. Compared with hole conduction, the mobility of electrons is higher, which further improves the bandwidth of the photodetector.

[0082] The photodetector provided in the present application has P-type and N-type doping regions respectively arranged on the upper and lower sides of the absorption layer (for example, the material of the absorption layer is germanium), and the concentration, position and width of the two doping regions are reasonably designed (for example, they can be realized by photolithography process, ion implantation process, etc.) to ensure that they can effectively enhance the electric field in the absorption layer; when voltage is applied, this enhanced electric field can excite the Franz-Caldisi effect of the absorption layer material, thereby improving the responsiveness of the photodetector;

[0083] The photodetector provided in the present application has a unique doping structure (eg, an optical waveguide includes a plurality of different doping regions) design, which enables the photodetector to operate at a lower voltage, thereby achieving a low power consumption effect.

[0084] The present application also provides a method for manufacturing a photoelectric detector, which is specifically referred to as Figure 2 As shown, the method comprises the following steps:

[0085] Step S201, providing a substrate, wherein the surface of the substrate includes a first semiconductor layer;

[0086] Step S202, performing an etching process to etch the first semiconductor layer to form a waveguide region;

[0087] Step S203, performing a selective doping process to form a P-type heavily doped region, a first P-type highly doped region, a P-type doped region, a first intrinsic region, a first N-type doped region, a second intrinsic region, a second N-type doped region, an N-type highly doped region, and an N-type heavily doped region arranged in sequence in a first direction in the waveguide region; the first direction is a direction parallel to the top surface of the substrate layer;

[0088] Step S204, forming a second semiconductor layer on the optical waveguide; performing a selective doping process to form a second P-type highly doped region at the surface of the second semiconductor layer, thereby obtaining an absorption layer having the second P-type highly doped region at the surface; wherein the material of the absorption layer is different from the material of the optical waveguide;

[0089] Step S205, forming an interconnection structure on the P-type heavily doped region, the second P-type highly doped region and the N-type heavily doped region; wherein the interconnection structure connects the P-type heavily doped region and the second P-type highly doped region to the first electrode, and connects the N-type heavily doped region to the second electrode.

[0090] Combination Figure 2 Schematic diagram of the manufacturing method of the photoelectric detector, 3A to 3H The device structure cross-sectional view during the manufacturing process of the photoelectric detector is further described in detail the manufacturing method of the photoelectric detector provided in the embodiment of the present application.

[0091] Step S201 is executed to provide a substrate.

[0092] refer to Figure 3A , providing a substrate 123, the substrate 123 may include a multi-layer structure, and a functional layer is further grown on the multi-layer structure. The substrate 123 of the present application may include a multi-layer structure, wherein the surface of the substrate 123 includes a first semiconductor layer 300', and the layer below the surface may include a single semiconductor material (for example, an insulating layer composed of silicon (Si) and its oxide, germanium (Ge), etc.) and its oxide The insulating layer or a compound semiconductor material (for example, silicon germanium (SiGe), etc.) and its oxide The insulating layer. The substrate 123 can be a silicon-on-insulator (Silicon-On-Insulator, SOI) or a germanium-on-insulator (Germanium-On-Insulator, GeOI), etc.

[0093] The embodiment of the present application is described by taking the substrate 123 as an SOI substrate as an example. The SOI substrate is formed by stacking a substrate layer 100, an insulating layer 200 and a first semiconductor layer 300' in sequence in the thickness direction. The substrate layer 100 is used to provide structural support for the photodetector. The insulating layer 200 is used to achieve electrical isolation between the active layer and the substrate silicon, block the leakage current between the active layer (such as the first semiconductor layer 300') and the substrate silicon, and reduce the parasitic capacitance of the device. The first semiconductor layer 300' is used to form an optical waveguide and an active region of the photodetector.

[0094] In some embodiments, the material of the substrate layer 100 may include a single semiconductor material (for example, silicon (Si), germanium (Ge), etc.) or a compound semiconductor material (for example, silicon germanium (SiGe), etc.). In practical applications, the substrate layer 100 may be a silicon wafer or a wafer formed of other materials. Therefore, the material of the substrate layer 100 may be silicon, germanium, sapphire, etc. In some embodiments, the material of the insulating layer 200 may include silicon oxide, such as silicon dioxide. In practical applications, the insulating layer 200 may be directly obtained by thermally oxidizing the substrate layer 100. In some embodiments, the material of the first semiconductor layer 300' may include silicon. For example, the material of the substrate layer 100 is silicon, and the insulating layer 200 is obtained by thermally oxidizing the substrate layer 100. The material of the insulating layer 200 is silicon dioxide. Further, silicon is deposited on the insulating layer 200 to obtain the first semiconductor layer 300'.

[0095] In some embodiments, the substrate layer 100 may have a thicker thickness than the thickness of the first semiconductor layer 300'. In practical applications, the thickness of the substrate layer 100 ranges from 600 μm to 800 μm, for example, the thickness of the substrate layer 100 may be 700 μm. The thickness of the insulating layer 200 ranges from 1 μm to 4 μm, for example, the thickness of the insulating layer 200 may be 2 μm or 3 μm. The thickness of the first semiconductor layer 300' ranges from 100 nm to 300 nm, for example, the thickness of the first semiconductor layer 300' may be 120 nm, 150 nm, 180 nm, 200 nm, 220 nm, 230 nm, 260 nm or 280 nm.

[0096] Execute step S202 to form a waveguide region.

[0097] refer to Figure 3B , using a standard photolithography process, the first semiconductor layer 300' is etched on the SOI substrate to form a waveguide region 300".

[0098] In some embodiments, the waveguide region may include a precursor morphology for forming a stripe waveguide or a ridge waveguide. That is, a selective doping process is performed on the waveguide region having the precursor morphology to obtain the stripe waveguide or the ridge waveguide.

[0099] In some embodiments, the waveguide region may include a first portion for forming an optical waveguide and a second portion for forming a tapered waveguide; the second portion is connected to the first portion along the third direction. In some embodiments, the second portion has the same size as the first portion along the second direction.

[0100] Step S203 is executed to form an optical waveguide.

[0101] refer to Figure 3C , a selective ion implantation process is performed to form an optical waveguide 300 in the waveguide area, wherein the optical waveguide 300 includes a P-type heavily doped region 301, a first P-type highly doped region 302, a P-type doped region 303, a first intrinsic region 304, a first N-type doped region 305, a second intrinsic region 306, a second N-type doped region 307, an N-type highly doped region 308, and an N-type heavily doped region 309 arranged in sequence in a first direction.

[0102] In the actual process, the mask lithography process can be used to sequentially open windows in the areas to be doped. Then, ion implantation is performed in the windows to form the above-mentioned different doping areas. In the actual process, the position and size of the windows can be controlled and the ion implantation process can be controlled so that the position and width of each doping area reach the set value. In the actual process, the ion concentration of each doping area can be controlled by controlling the implantation dose and energy of the ion implantation process.

[0103] In some embodiments, the size of the first intrinsic region 304 in the first direction is greater than or equal to the size of the second intrinsic region 306 in the first direction. In practical applications, the size of the first intrinsic region 304 in the first direction ranges from 200 nm to 700 nm, and the size of the second intrinsic region 306 in the first direction ranges from 100 nm to 300 nm. For example, the size of the first intrinsic region 304 in the first direction is 240 nm, and the size of the second intrinsic region 306 in the first direction is 120 nm.

[0104] In some embodiments, the doping concentration range of the P-type heavily doped region 301 and the N-type heavily doped region 309 is 8×10 19 cm -3 ~1×10 21 cm -3 The doping concentration range of the first P-type high-doping region 302 and the N-type high-doping region 308 is 8×10 17 cm -3 ~5×10 18 cm -3 The doping concentration range of the P-type doping region 303, the first N-type doping region 305 and the second N-type doping region 307 is 1×10 17 cm -3 ~4×10 17 cm -3 In some embodiments, the specific doping concentrations of different doping regions with the same doping concentration range may be the same or different. For example, in a doping concentration of 8×10 19 cm -3 ~1×10 21 cm -3 In the range of , the doping concentrations of the P-type heavily doped region 301 and the N-type heavily doped region 309 may be the same or different; for example, in the range of 1×10 17 cm -3 ~4×10 17 cm -3 Within the range of , the doping concentrations of the P-type doping region 303, the first N-type doping region 305, and the second N-type doping region 307 may be the same or partially the same, or may be different.

[0105] In some embodiments, the doping concentration of the first intrinsic region 304 and the second intrinsic region 306 is less than a predetermined value, for example, less than 1×10 16 cm -3 .

[0106] In some embodiments, the dopant in the P-type heavily doped region 301, the first P-type highly doped region 302, and the P-type doped region 303 is boron (B) element; the dopant in the first N-type doped region 305, the second N-type doped region 307, the N-type highly doped region 308, and the N-type heavily doped region 309 is phosphorus (P) element or asium (As) element.

[0107] Step S204 is executed to form an absorption layer.

[0108] refer to Figure 3D , a cladding layer 900, an absorption layer 400 and a second P-type highly doped region 401 are formed on the optical waveguide 300. The specific process steps to be performed are: first, a cladding layer 900 is deposited on the optical waveguide 300; then, a window is opened on the cladding layer 900, and a second semiconductor layer is formed at this window by an epitaxial process. Finally, a selective ion implantation process is performed to form a second P-type highly doped region 401 at the surface position of the second semiconductor layer, and an absorption layer 400 having a second P-type highly doped region 401 at the surface position is obtained. In practical applications, the material of the cladding layer 900 may include but is not limited to silicon oxide or silicon nitride. In practical applications, the material of the second semiconductor layer may include but is not limited to germanium.

[0109] In the actual process, the position and width of the second semiconductor layer can be made to reach the set value by controlling the position and size of the opening window and performing an epitaxial process.

[0110] In some embodiments, the second semiconductor layer at least covers the first intrinsic region 304, the first N-type doping region 305, and the second intrinsic region 306. In some embodiments, the second semiconductor layer covers the first intrinsic region 304, the first N-type doping region 305, and the second intrinsic region 306, and covers a portion of the P-type doping region 303 and the second N-type doping region 307.

[0111] In some embodiments, the second semiconductor layer has a size ranging from 400 nm to 3000 nm in the first direction, a size ranging from 200 nm to 700 nm in the second direction, and a size ranging from 5 μm to 100 μm in the third direction.

[0112] In some embodiments, the material of the first semiconductor layer 300' is different from the material of the second semiconductor layer. In practical applications, the material of the first semiconductor layer 300' may include silicon, and the material of the second semiconductor layer may include germanium or germanium-silicon alloy.

[0113] In the actual process, the position and size of the opening window and the ion implantation process can be controlled to make the position and width of the second P-type highly doped region 401 reach the set value. In the actual process, the ion concentration and ion implantation depth of the second P-type highly doped region 401 can be controlled to reach the set value by controlling the implantation dose and energy of the ion implantation process.

[0114] In some embodiments, the center of the optical waveguide 300 is located in the region where the first N-type doping region 305 is located in the first direction. In some embodiments, the center of the absorption layer 400 and the optical waveguide 300 are coincident in the first direction.

[0115] In some embodiments, there is an offset Δx between the center of the first N-type doping region 305 and the center of the absorption layer 400 in the first direction, and the value of the offset Δx may be greater than or equal to 0. In practical applications, the offset direction of the offset Δx may be a direction from the first N-type doping region 305 to or away from the N-type heavily doped region 309 in the first direction.

[0116] In some embodiments, the second P-type highly doped region 401 is located directly above the first N-type doped region 305. In some embodiments, the second P-type highly doped region 401 covers the first N-type doped region 305. In some embodiments, the centers of the second P-type highly doped region 401 and the first N-type doped region 305 coincide with each other in the first direction.

[0117] In some embodiments, the doping concentration of the second P-type high-doping region 401 is in the range of 8×10 17 cm -3 ~5×10 18 cm -3 In some embodiments, the dopant in the second P-type highly doped region 401 is boron (B).

[0118] In some embodiments, the doping concentration of the portion of the absorption layer 400 excluding the second P-type high-doping region 401 is less than a predetermined value, for example, less than 1×10 16 cm -3 .

[0119] In some embodiments, the doping depth of the second P-type highly doped region 401 ranges from 100 nm to 200 nm. The doping depth of the second P-type highly doped region 401 can be understood as the junction depth of the second P-type highly doped region 401 .

[0120] In some embodiments, the ratio of the size of the absorption layer 400 in the second direction to the doping depth of the second P-type highly doped region 401 is in the range of 2 to 10. In practical applications, the ratio of the size of the absorption layer 400 in the second direction to the doping depth of the second P-type highly doped region 401 is 3 or 4. In practical applications, the size of the absorption layer 400 in the second direction ranges from 200nm to 700nm, preferably, the size of the absorption layer 400 in the second direction is 240nm, 360nm or 600nm; the doping depth of the second P-type highly doped region 401 ranges from 100nm to 200nm, preferably, the doping depth of the second P-type highly doped region 401 is 120nm, 150nm or 180nm. For example, the size of the absorption layer 400 in the second direction is 360nm, and the doping depth of the second P-type highly doped region 401 is 120nm.

[0121] Execute step S205 to form an interconnection structure.

[0122] refer to Figure 3E A plurality of first contact holes are opened on the P-type heavily doped region 301, the N-type heavily doped region 309 and the second P-type highly doped region 401, and metal (such as tungsten) is injected into the plurality of first contact holes to form a first through-hole layer, and the first through-hole layer includes a plurality of conductive through-holes 501, 502 and 503.

[0123] In some embodiments, the plurality of conductive vias 501 on the P-type heavily doped region 301, the plurality of conductive vias 503 on the N-type heavily doped region 309, or the plurality of conductive vias 502 on the second P-type highly doped region 401 are distributed in an array or are spliced ​​together to form a whole. For example, the plurality of conductive vias 501 on the P-type heavily doped region 301, the plurality of conductive vias 503 on the N-type heavily doped region 309, and the plurality of conductive vias 502 on the second P-type highly doped region 401 are distributed in an array.

[0124] refer to Figure 3F A first metal layer is formed in a designated area by a deposition process, the first metal layer comprising a first electrode layer 601 connecting the conductive via 501 and the conductive via 502, and a second electrode layer 602 connecting the conductive via 503. The material of the first metal layer can be metal (such as tungsten or copper / copper alloy).

[0125] refer to Figure 3G A second contact hole is opened on the first electrode layer 601 and the second electrode layer 602 , and metal (such as tungsten) is injected into the second contact hole to form a second through-hole layer. The second through-hole layer includes a plurality of conductive through-holes 701 and 702 .

[0126] In some embodiments, the plurality of conductive vias 701 on the first electrode layer 601 or the plurality of conductive vias 702 on the second electrode layer 602 are distributed in an array or are spliced ​​together to form a whole. For example, the plurality of conductive vias 701 on the first electrode layer 601 and the plurality of conductive vias 702 on the second electrode layer 602 are distributed in an array.

[0127] refer to Figure 3H A second metal layer is formed in a designated area by a deposition process, the second metal layer comprising a first electrode 801 connected to the conductive via 701 and a second electrode 802 connected to the conductive via 702. The material of the second metal layer can be metal (copper / copper alloy or aluminum / aluminum alloy).

[0128] In some embodiments, the materials of the first electrode 801 and the second electrode 802 include copper / copper alloy or aluminum / aluminum alloy, which are used to connect to an external voltage source, a transimpedance amplifier or a signal source of the photodetector.

[0129] The manufacturing method of the photodetector provided in each embodiment of the present application has a manufacturing process that is compatible with the Multi Project Wafer (MPW) process provided by the mainstream foundry. When manufacturing such a photodetector, there is no need to introduce any additional manufacturing steps, such as the growth of quantum dots or the application of a stress layer. This design not only reduces production costs, but also avoids the problem of low device production yield caused by complex additional processes. The detector of the present application provides a cost-effective, efficient and reliable solution suitable for practical on-chip optoelectronic applications.

[0130] The photodetector manufactured using the photodetector manufacturing method provided in each embodiment of the present application is the same as or similar to the photodetector provided in the above-mentioned embodiments. For the technical features not fully disclosed in the embodiments of the photodetector manufacturing method of the present application, please refer to the technical features disclosed in the above-mentioned embodiments of the photodetector of the present application for understanding, and no further details will be given here.

[0131] It should be noted that the photoelectric detector embodiment provided in the present application and the photoelectric detector manufacturing method embodiment belong to the same concept: the technical features in the technical solutions recorded in the embodiments can be arbitrarily combined without conflict. However, it should be further noted that the photoelectric detector provided in the embodiment of the present application, the combination of its various technical features can already solve the technical problem to be solved by the present application: therefore, the photoelectric detector provided in the embodiment of the present application may not be limited by the photoelectric detector manufacturing method provided in the embodiment of the present application, and any photoelectric detector manufactured by the manufacturing method that can form the photoelectric detector structure provided in the embodiment of the present application is within the scope of protection of the present application.

[0132] The above description is only a preferred embodiment of the present application and is not intended to limit the scope of protection of the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the scope of protection of the present application.

Claims

1. A photodetector, It is characterized in that The photodetector comprises: A substrate layer (100); An insulating layer (200) located on the substrate layer (100); An optical waveguide (300) is located on the insulating layer (200); wherein the optical waveguide (300) comprises a first type heavily doped region (301), a first first type highly doped region (302), a first type doped region (303), a first intrinsic region (304), a first second type doped region (305), a second intrinsic region (306), a second second type doped region (307), a second type highly doped region (308), and a second type heavily doped region (309) arranged in sequence in a first direction; the first direction is a direction parallel to the top surface of the substrate layer; the first type is different from the second type; An absorption layer (400) is located on the optical waveguide (300); wherein the absorption layer (400) comprises a second first-type highly doped region (401) near the upper surface; and the material of the absorption layer (400) is different from that of the optical waveguide (300); An interconnect structure is configured to connect the first type heavily doped region (301) and the second first type highly doped region (401) to a first electrode (801), and to connect the second type heavily doped region (309) to a second electrode (802).

2. The photodetector according to claim 1, It is characterized in that The center of the first second type doped region (305) and the center of the absorption layer (400) have an offset (Δx) in the first direction, and the value of the offset (Δx) is greater than or equal to zero; and / or the second first type highly doped region (401) is located directly above the first second type doped region (305).

3. The photodetector according to claim 1, It is characterized in that The material of the optical waveguide (300) includes silicon, and the material of the absorption layer (400) includes germanium or germanium-silicon alloy.

4. The photodetector according to claim 1, It is characterized in that The absorption layer (400) has a size range of 400nm to 3000nm in the first direction, a size range of 200nm to 700nm in the second direction, and a size range of 5μm to 100μm in the third direction; wherein the second direction is a direction perpendicular to the top surface of the substrate layer, and the second direction is perpendicular to the third direction.

5. The photodetector according to any one of claims 1 to 4, It is characterized in that The absorption layer (400) at least covers the first intrinsic region (304), the first second type doping region (305) and the second intrinsic region (306).

6. The photodetector according to claim 1, It is characterized in that The doping concentration range of the first type heavily doped region (301) and the second type heavily doped region (309) is 8×10 19 cm -3 ~1×10 21 cm -3 The doping concentration range of the first first type highly doped region (302), the second type highly doped region (308) and the second first type highly doped region (401) is 8×10 17 cm -3 ~5×10 18 cm -3 The doping concentration of the first type doping region (303), the first second type doping region (305) and the second second type doping region (307) is in the range of 1×10 17 cm -3 ~4×10 17 cm -3 .

7. The photodetector according to claim 1, It is characterized in that The optical waveguide (300) type includes a strip waveguide or a ridge waveguide.

8. The photodetector according to claim 1, It is characterized in that The photodetector further comprises: A tapered waveguide (10) is connected to the optical waveguide (300) in a direction parallel to the top surface of the substrate layer and perpendicular to the first direction; the dimension of the tapered waveguide (10) connected to the optical waveguide (300) in the first direction is equal to or smaller than the dimension of the absorption layer (400) in the first direction.

9. The photodetector according to claim 1, It is characterized in that The interconnect structure comprises: A first through-hole layer, comprising a plurality of conductive through-holes respectively contacting the first type heavily doped region (301), the second first type highly doped region (401), and the second type heavily doped region (309); a first metal layer, located on the first via layer and connected to the first via layer; a second via layer, located on the first metal layer and connected to the first metal layer; A second metal layer is located on the second through-hole layer and connected to the second through-hole layer; wherein the second metal layer includes the first electrode (801) and the second electrode (802); Wherein, the plurality of conductive through holes are distributed in an array form or are spliced ​​together to form a whole.

10. The photodetector according to claim 1, It is characterized in that The first electrode (801) and the second electrode (802) are made of copper / copper alloy or aluminum / aluminum alloy, and are used to connect to an external voltage source, a transimpedance amplifier or a signal source of the photodetector.