Scanning ion beam deposition and etch

By adopting asymmetric scanning speed and path adjustment in ion beam etching, the internal and external side asymmetry problems caused by beam divergence are solved, and the effect of high uniform etching on the wafer is achieved.

CN119096002APending Publication Date: 2024-12-06PLASMA NES GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380024374.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-03
Filing Date
2023-02-08
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

During ion beam etching, due to the divergence of the small beam, asymmetry occurs between the inner and outer sides of the device on the wafer, affecting the uniformity of the etching.

Method used

Using asymmetric scanning speed technology, the etch asymmetry on the inner and outer sides is corrected by adjusting the scanning path and beam flux of the wafer to ensure etch uniformity on the entire wafer.

Benefits of technology

The problem of internal and external side asymmetry caused by beam divergence is effectively solved, and a high uniform etching effect on the entire wafer is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119096002A_ABST
    Figure CN119096002A_ABST
Patent Text Reader

Abstract

A method is provided to adjust the asymmetric speed of scanning in a scanning ion beam deposition or etch process to correct for the asymmetry of deposition or etch between the inner and outer sides of device structures on a wafer while maintaining the overall uniformity of the respective deposition or etch throughout the wafer.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application is a continuation-in-part of U.S. patent application No. 17 / 536,025, entitled “Scanning Ion Beam Etch,” filed on November 27, 2021, which is a divisional of U.S. patent application No. 16 / 398,487, entitled “Scanning Ion Beam Etch,” filed on April 30, 2019, which claims the benefit of U.S. patent application No. 62 / 666,324, filed on May 3, 2018, the contents of which are incorporated herein by reference in their entirety. Technical Field

[0003] The present invention relates to the field of charged particle sources, including plasma sources for direct etching and deposition, broad beam ion sources for ion beam deposition and etching, and electron sources for surface modification. Background Art

[0004] Figure 1 An ion beam etching (IBE) system is shown. In an IBE process, a wafer 180 is placed in front of an ion source 105. At least one surface of the wafer 180 can be exposed to a beam 130. The ion source 105 can include a plasma chamber 110 and an ion extraction grid system 150. The ion extraction grid system 150 includes a plurality of conductive plates having a plurality of holes aligned from plate to plate. The grid system 150 extracts and helps collimate the ion beamlets that come out of each hole of the plate and forms a substantially collimated ion beam 130. The plasma in the plasma source can be generated by methods known in the art, including direct current (DC) and radio frequency (RF) inductively coupled plasma (ICP) coils 160. The energy of the ions extracted from the ion source 105 is defined by the voltage applied to the grid system 150.

[0005] The electron source 230 can be placed between the ion extraction grid system 150 and the wafer stage to prevent charge damage on the wafer from the impact ions. The wafer 180 is placed on the wafer stage 140. The stage 140 can rotate the wafer about the central axis 220. During at least a portion of the etching process, the stage 140 can tilt the wafer 180 relative to the ion beam 130. By tilting the wafer 180, the ions from the beam 130 can be directed at any angle relative to the wafer surface. Any solid material can be etched with the IBE process. Provision can be made on the wafer stage 140 to cool the wafer 180 during the etching process to prevent thermal damage to the devices on the wafer 180. The wafer 180 can also be heated to a specific temperature to enhance the ion beam etching process.

[0006] A typical wafer 180 may include many devices and may be covered with a photoresist mask or other types of masks. The devices may be processed using ion beam exposure to etch the desired shape of the device on the wafer 180. The desired shape of the device may be achieved by adjusting process parameters such as: wafer tilt angle during etching, etching duration, beam energy, beam current, photoresist mask sidewall angle, wafer temperature, etc. When the device is made of multiple layers of material and a precise etching endpoint at a predetermined layer is generally required, the endpoint detector 240 may be placed in the line of sight of the wafer 180.

[0007] It is contemplated that devices on the etched wafer 180 show similar shapes (eg, sidewall profiles, etc.). However, the devices may show different shapes depending on their location on the wafer 180. One example of a particular type of shape difference is referred to as internal asymmetry and external asymmetry. Figure 2a to Figure 2c A schematic representation of the asymmetry of the inside (IB) side 191 of the device and the outside (OB) side 192 of the device after ion beam etching is shown. The asymmetry can be quantified as the difference in sidewall angles on one side a and the opposite side β. Figure 2a A symmetric etch is shown. Figure 2b and Figure 2c An asymmetric etch is shown.

[0008] The asymmetry of the IB side 191 and the OB side 192 of the device in ion beam etching generally has a specific relationship with the tilt of the wafer 180. This relationship is Figure 3a to Figure 3b Shown in. Figure 3a is a top view of the etched wafer 180. The tilt axis extends along the diagonal of the wafer, as shown with respect to the top view of the wafer. Figure 3a , the wafer 180 is etched by an ion beam impinging on the wafer 180 from a direction perpendicular to the paper surface. Figure 3b yes Figure 3a A cross-sectional view of a wafer along a diagonal line perpendicular to the tilt axis. Figure 3b 180, the cross-section of the wafer, the direction of the tilt axis extends along the middle of the wafer and is perpendicular to the plane of the paper. The asymmetry between the IB side 191 of the device and the OB side 192 of the device can be seen on devices positioned toward the top and bottom of the wafer 180. The asymmetry becomes more pronounced the further the device is from the tilt axis, and as the tilt angle increases, for example, the further the wafer 180 is tilted away from the normal incidence angle of the incident beam.

[0009] In an ideal ion source and grid system, all beamlets would be perfectly collimated and the ions would not diverge from the intended direction. In such a system, all features etched on the wafer 180 would be perfectly symmetrical. Practical ion beam etching systems have non-zero beam divergence.

[0010] In practice, an ion source produces an ion beam which is a collection of beamlets with finite non-zero beam divergence, such as Figure 4 180 . The beamlet divergence 131 is shown in the figure. As a result of this beamlet divergence, there will be more intense etching on the side of the wafer 180 near the ion source and less intense etching on the side of the wafer 180 away from the ion source as the wafer is tilted away from the normal beam incidence. By rotating the wafer 180 about the axis 220, the etch depth in the featureless area of ​​the wafer 180 can be made more uniform. However, the devices on the wafer 180 are typically made of three-dimensional features rather than flat surfaces. On the three-dimensional features on the wafer 180, the effect of the tilt of the wafer 180 away from the normal beam incidence combined with the beam divergence is that the inner side 191 of the device on the wafer 180 will experience a different beam exposure than the outer side 192 of the device. This inner side asymmetry and outer side asymmetry become more significant when the device is located away from the tilt axis of the wafer 180, and as the tilt angle increases away from the normal beam incidence.

[0011] Translating (eg, scanning) the wafer 180 across the beam can account for asymmetries between the interior side 191 of the device and the exterior side 192 of the device. Figure 5 In FIG. 5 , the area marked by the double-ended arrow 550 is the area of ​​the wafer where ion beam exposure occurs. A single instance of wafer translation is when all regions of the wafer begin translation at any point outside the region indicated by 550, and the translation path of the wafer through the region indicated by 550 is considered one scan. Figure 7 In FIG. 5 , the region 550 where ion beam exposure occurs is defined by introducing physical beam blocks 171 and 172 .

[0012] In some embodiments, the path of the wafer 180 during translation is defined as a scan path. For at least one scan, the scan path may be in a plane parallel (or nearly parallel) to the plane of the tilted wafer surface. For at least one scan, the scan path of the wafer translation may be linear. For at least one scan, the path of the wafer translation may be non-linear (e.g., curved). For at least one scan, the scan path may be parallel to the tilted wafer 180. For at least one scan, the wafer tilt may be constant during the scan path. For at least one scan, the wafer tilt may vary along the path of the scan. For at least one scan, the scan path may be parallel to the wafer 180 during at least one point in the scan. For at least one scan, the scan path may be parallel to the wafer 180 at all points during the scan. For at least one scan, the scan path may be in a different plane from the wafer 180. For all scans, the scan path may be in a plane parallel (or nearly parallel) to the plane of the tilted wafer surface. For all scans, the scan path of the wafer translation may be linear. For all scans, the path of the wafer translation may be non-linear (e.g., curved). For all scans, the scan path may be parallel to the tilted wafer 180. For all scans, the wafer tilt may be constant during the scan path. For all scans, the wafer tilt may vary along the scan path. For all scans, the scan path may be parallel to the wafer 180 during at least one point in the scan. For all scans, the scan path may be parallel to the wafer 180 at all points during the scan. For all scans, the scan path may be in a different plane than the wafer 180. Summary of the invention

[0013] According to an embodiment, the present disclosure is directed to using an asymmetric scan speed in an ion beam etching process to correct for asymmetry in etching between inner and outer sides of a device structure on a wafer while maintaining overall uniformity of etching across the wafer.

[0014] According to another embodiment, the invention is directed to using asymmetric scan speeds in an ion beam etching process to produce exaggerated asymmetry in etching between inner and outer sides of devices on a wafer while maintaining overall uniformity of etching across the wafer.

[0015] According to another embodiment, the present disclosure is directed to using symmetric velocity scanning to control the asymmetry of the inner and outer sides even when the ion beam system is configured with a small ion source and a small grid. Without asymmetric velocity scanning, the lateral dimensions of the ion source and the grid would need to be larger than the sum of the wafer diameters, i.e., twice the divergence of the beamlet projected on the scan plane, and the ion beam density would need to be highly uniform in the lateral dimensions.

[0016] According to another embodiment, the present disclosure is directed to using asymmetric velocity scanning in combination with symmetric velocity scanning to address inner and outer side asymmetry and wafer etching uniformity, wherein the number of scans required to complete the etching process may be a single scan or multiple scans.

[0017] According to another embodiment, the present disclosure is directed to a process in which the scanning motion may be a straight linear motion of the wafer center across the ion beam, or may include slight deviations from a straight line, such as a curved motion path of the wafer center across the ion beam.

[0018] According to another embodiment, the present invention is directed to an alternative to asymmetric velocity scanning motion of a wafer in which the ion beam current or ion beam voltage is modulated as the wafer moves across the ion beam. The wafer may be exposed to larger beam currents or higher beam voltages as the center of the wafer scans beyond the mid-plane of the ion source on the far side of the scan.

[0019] According to another embodiment, the present disclosure is directed to an alternative to asymmetric velocity profile scanning achieved by modulating the scan path so that the wafer spends more time exposed to the ion beam on the far side of the scan after the wafer has passed through the mid-plane of the ion source.

[0020] According to another embodiment, the present disclosure is directed to an alternative scheme for asymmetric velocity scanning of a wafer across an ion beam by placing the beam block in an asymmetric manner relative to a mid-plane of the ion source and the grid, so that even with a symmetric velocity profile of the scan, the wafer spends more time exposed to the ion beam on the far side of the scan.

[0021] According to one aspect of an embodiment of the present invention, a method for correcting asymmetry during a wafer etching process is provided, wherein the method includes: generating plasma from a plasma source, the plasma source including a plasma chamber and an ion extraction grid system, the ion extraction grid system being configured to generate an ion beam from the plasma, the ion beam having a central axis; supporting a wafer on a stage; scanning the wafer relative to the ion beam along a scanning path; and modifying an applied beam flux based on a position of the wafer.

[0022] According to another aspect of an embodiment of the present invention, a method for correcting asymmetry during a wafer etching process is provided, wherein the method includes: generating plasma from a plasma source, the plasma source including a plasma chamber and an ion extraction grid system, the ion extraction grid system being configured to generate an ion beam from the plasma, the ion beam having a central axis; supporting a wafer on a stage, including at least one of the following: rotating the stage about the central axis and tilting the stage relative to the ion beam during at least a portion of the etching process; scanning the wafer relative to the ion beam along a scanning path according to a scanning speed function; and modifying an applied beam flux according to a position of the wafer by changing the scanning speed function as the wafer travels along the scanning path.

[0023] According to another aspect of an embodiment of the present invention, a method for correcting asymmetry during a wafer etching process is provided, wherein the method includes: generating plasma from a plasma source, the plasma source including a plasma chamber and an ion extraction grid system, the ion extraction grid system being configured to generate an ion beam from the plasma, the ion beam having a central axis; supporting a wafer on a stage; scanning the wafer relative to the ion beam along a scanning path, the scanning path including a sweeping path from a first end of the ion beam to a second end of the ion beam according to a sweeping speed function and a retracement path from the second end of the ion beam to the first end of the ion beam according to a retracement speed function, wherein one of the sweeping speed function and the retracement speed function varies with time, and the applied beam flux is modified according to the position of the wafer.

[0024] According to another aspect of an embodiment of the present invention, a method for correcting asymmetry during a wafer deposition process is provided, wherein the method includes: generating plasma from a plasma source, the plasma source including a plasma chamber and an ion extraction grid system, the ion extraction grid system being configured to generate an ion beam from the plasma, the ion beam having a central axis; supporting a wafer on a stage; scanning the wafer relative to the ion beam along a scanning path; and modifying an applied beam flux based on a position of the wafer.

[0025] According to another aspect of an embodiment of the present invention, in an ion beam sputtering system having a vacuum chamber, a wafer on a stage, a target material, and an ion beam source, a method for depositing a uniform sputtered material layer on the wafer in the ion beam sputtering system includes the following steps: generating ions from an ion beam source; directing the generated ions onto the target material, whereby a portion of the target material is sputtered toward the wafer as part of a deposition plume; exposing the wafer to the deposition plume in a deposition area; and scanning the wafer across the deposition area along a scanning path relative to the deposition plume, wherein a scanning speed of the wafer changes as the wafer moves along the scanning path, wherein the scanning speed decreases as the area of ​​the wafer exposed to the deposition plume decreases.

[0026] According to another aspect of an embodiment of the present invention, in an ion beam sputtering system having a vacuum chamber, a wafer on a stage, a target material, and an ion beam source, a method for depositing a uniform material layer on the wafer in the ion beam sputtering system includes the following steps: generating ions from an ion beam source; directing the generated ions onto the target material, whereby a portion of the target material is sputtered toward the wafer as part of a deposition plume; exposing the wafer to the deposition plume in a deposition area; and scanning the wafer across the deposition area along a scanning path relative to the deposition plume according to a scanning speed function, wherein the scanning speed of the wafer changes as the wafer moves along the scanning path, and wherein the scanning speed decreases as the area of ​​the wafer exposed to the deposition plume decreases.

[0027] Additional features and advantages of the present disclosure will be set forth in the following description, and in part will be apparent from the description, or can be learned by practicing the principles disclosed herein. The features and advantages of the present disclosure can be realized and obtained by the instruments and combinations particularly pointed out in the appended claims. These and other features of the present disclosure will become more apparent from the following description and the appended claims, or can be learned by practicing the principles set forth herein. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] In order to describe the manner in which the above and other advantages and features of the present disclosure can be obtained, a more particular description of the principles briefly described above will be presented by reference to specific embodiments thereof shown in the accompanying drawings. It should be understood that these drawings depict only exemplary embodiments of the present disclosure and are not therefore to be considered limiting of its scope. The principles of the present invention are described and explained with additional specificity and detail through the use of the accompanying drawings, in which:

[0029] Figure 1 An ion beam etching system is shown;

[0030] Figure 2a Symmetric etching is shown;

[0031] Figure 2b An asymmetric etch is shown;

[0032] Figure 2c An asymmetric etch is shown;

[0033] Figure 3a is a top view of the etched wafer 180;

[0034] Figure 3b yes Figure 3a A cross-sectional view along a diagonal line of the wafer perpendicular to the tilt axis;

[0035] Figure 4 Ion beam divergence is shown;

[0036] Figure 5 An improved scanning ion beam etching system according to an embodiment of the present disclosure is shown;

[0037] Figure 6 An improved scanning ion beam etching system according to an embodiment of the present disclosure is shown;

[0038] Figure 7 An improved scanning ion beam etching system according to an embodiment of the present disclosure is shown;

[0039] Figure 8 shows a variable scan speed according to an embodiment of the present disclosure;

[0040] Fig. 9 shows relative etching from the center of a wafer at a constant scan speed and a variable scan speed according to an embodiment of the present disclosure;

[0041] Fig.10a shows beamlet divergence and divergence effects on the inner side of a wafer relative to the outer side of a wafer as the beam is scanned across the wafer in accordance with an embodiment of the present disclosure;

[0042] Fig.10b shows beamlet divergence and divergence effects on the inner side of a wafer relative to the outer side of a wafer as the beam is scanned across the wafer in accordance with an embodiment of the present disclosure;

[0043] Fig.11a A beam with higher flux at the beam center is shown;

[0044] Fig.11b A uniform beam is shown, where the flux is independent of the position in the beam;

[0045] Fig.12 The mid-plane of the source and the far side of the scan are shown, where preferential etching of the outer side of the device occurs;

[0046] Fig.13One type of asymmetric velocity profile (solid line) is shown that preferentially etches the outer side on the far side of the scan compared to a symmetric velocity (dashed line) scan;

[0047] Fig.14 The mid-plane of the source and the near side of the scan are shown, where preferential etching of the interior side of the device occurs;

[0048] Fig.15 One type of asymmetric velocity profile is shown, which is a step type (solid line) that preferentially etches the outer side on the far side of the scan compared to an asymmetric velocity profile of a smoothly changing type (dashed line) scan;

[0049] Fig.16 An ion beam deposition system is shown;

[0050] Fig.17 An improved scanning ion beam deposition system according to an embodiment of the present disclosure is shown; and

[0051] Fig.18 An ion beam deposition system with a pre-clean assist source is shown.

[0052] Like reference numerals refer to like parts throughout the several views of the drawings. DETAILED DESCRIPTION

[0053] Figure 5 A diagram of an improved scanning ion beam etching (IBE) system of the present disclosure is shown.The wafer 180 may be tilted away from normal incidence relative to the ion beam and scanned across the beam starting from the outside of the beam on one end to the outside of the beam on the opposite end.

[0054] In some embodiments, to compensate for non-uniform beam flux, the wafer scan speed may be varied during the wafer scan. Figure 5 As shown, the wafer 180 is typically scanned back and forth in and / or through the beam 130. A typical wafer scan may begin with the wafer 180 in position 500. The wafer 180 is scanned (e.g., translated) through the beam to position 510. The wafer 180 may then be scanned (e.g., translated) from position 510 back to position 500. The wafer 180 may stop (e.g., zero velocity) between scans (at either or both of position 500 and position 510). The path from position 500 to position 510 and back again to position 500 may be a continuous path. The path followed by the wafer 180 to scan from position 500 to position 510 may be the same as the path followed by the wafer 180 to scan from position 510 to position 500. The path followed by the wafer 180 to scan from position 510 to position 500 may be different from the path followed by the wafer 180 to scan from position 500 to position 510.

[0055] The wafer 180 in position 500 and / or position 510 may be at least partially exposed to the beam. The wafer 180 in position 500 and / or position 510 may be fully exposed to the beam. The wafer 180 in position 500 and / or position 510 may be at least partially outside the beam (e.g., not exposed to the beam). The wafer 180 in position 500 and / or position 510 may be completely outside the beam (e.g., not exposed to the beam). The position 500 and / or position 510 may be constant between at least two scans. The position 500 and / or position 510 may be constant for more than two scans. The position 500 and / or position 510 may be constant for all scans. The position 500 and / or position 510 may change between at least two scans. The position 500 and / or position 510 may change between more than two scans. The position 500 and / or position 510 may change between each scan. The length of the wafer scan (e.g., the distance between point 500 and point 510) may be constant in at least two scans. The length of the wafer scan may be constant for all scans. The length of the wafer scan may be different between at least two scans. The length of the wafer scan may be different in more than two scans. The length of the wafer scan may be different for all wafer scans.

[0056] In some embodiments, at least a portion of the wafer 180 may begin scanning outside the ion beam. All wafers 180 may begin scanning outside the ion beam. A portion of the wafer 180 may be exposed to the beam during scanning. During scanning, all wafers 180 may be exposed to the beam. At the end of the scan, a portion of the wafer 180 may be outside the beam (e.g., not exposed to the beam). At the end of the scan, all wafers 180 may be outside the beam (e.g., not exposed to the beam). In one embodiment, the wafer 180 is not exposed to the beam at the beginning of the scan, a portion of the wafer 180 is exposed to the beam during the scan, and the wafer 180 is not exposed to the beam at the end of the scan. The wafer 180 may scan back and forth at a desired tilt angle relative to the ion beam. When the wafer 180 is scanned across the beam, the wafer 180 may rotate around the axis 220. During scanning, the rotation speed may be constant. During scanning, the rotation speed may vary. The process of scanning at a fixed scanning speed may be repeated until the desired etching depth is achieved. The scan path may be centered in the beam (eg, the midpoint of the scan approximately coincides with the center of the beam). The scan path may be offset in the ion beam (eg, the midpoint of the scan does not coincide with the center of the beam).

[0057] The scanning method solves the problems of inner and outer asymmetry caused by the tilt of the wafer 180 and the divergence of the beamlets, which cause the near side of the wafer 180 to be etched at a higher rate than the far side of the wafer 180 in conventional ion beam etching (IBE) machines.

[0058] Many ion beam operations, such as ion beam smoothing, sidewall etching, and sidewall cleaning, require a large tilt angle relative to the ion beam. The wafer 180 can be tilted greater than about 10 degrees relative to the normal incidence of the ion beam. The wafer 180 can be tilted greater than 30 degrees relative to the normal incidence of the ion beam. Figure 6 As shown in , scanning at a large tilt angle causes the midpoint of the scan to move further away from the ion source and the scan length to increase in order to be able to scan the wafer 180 across the ion beam. In a high vacuum / ultra-high vacuum chamber, it may be difficult to accommodate the increased scan length and the larger distance between the wafer 180 and the source.

[0059] like Figure 7 As shown, by inserting physical blocks 171 and 172 toward the end of the scan, the required scan length can be reduced. Blocks 171 and 172 form an aperture that narrows beam 130, thereby creating a portion or "slit" of the ion beam through which wafer 180 is scanned. Blocks 171 and 172 can be inserted symmetrically with respect to midplane 310 of ion source 105 and ion extraction grid system 150, as shown in FIG. Figure 7 As shown. Blocks 171 and 172 may be inserted asymmetrically with respect to mid-plane 310. By adjusting the position of upper block 171 or lower block 172 or both, the slit width may be adjusted. However, in the case where it is desired to scan wafer 180 across the slit at a large tilt angle, the distance from ion extraction grid system 150 to wafer 180 at the midpoint of its scan may be much greater than in a conventional ion beam etching (IBE) system.

[0060] In a practical IBE system, the beam density of beam 130 may be spatially non-uniform. This non-uniformity may be due to beamlet divergence. This effect generally increases with increasing source-to-wafer distance and may be amplified by larger distances between midpoints of the wafer scan. Scanning wafer 180 with beam 130 at a constant scan speed may result in highly non-uniform etching, where the center of the wafer etches much faster than the edge of the wafer. Figure 8 As shown in the schematic diagram in , deploying a variable scan speed can significantly improve etching uniformity across the wafer 180. As the wafer 180 moves away from the midpoint of the scan, slowing the scan speed can enhance etching at points of the wafer 180 that are away from its center.

[0061] In some embodiments, the wafer speed may be varied during a wafer scan. The wafer scan speed may be varied continuously during a scan. The wafer scan speed may be constant during certain portions of a scan. The wafer speed profile may be the same for at least two scans. The wafer scan speed profile may be the same for all scans. The wafer scan speed may be varied between at least two scans. The wafer scan speed profile may be varied for each scan. The wafer scan speed may be zero during at least one point during a scan. The wafer speed profile may be symmetrical (e.g., see Figure 8 ). The scanning speed distribution may be monotonic. The scanning speed distribution may be discontinuous.

[0062] exist Figure 8 An example of a symmetrical variable speed for achieving highly uniform etching across the wafer 180 is shown in FIG. The midpoint of the scan is represented by X=0. The direction of the scan is along the X-axis. Negative X-axis positions are closer to the ion source 105 than positive X-axis positions. Figure 8 The example of FIG. 1 shows a variable speed that is symmetrical about the midpoint of the scan. The symmetrical variable speed of the scan can be used to obtain uniform etching across the wafer 180. The symmetrical variable speed profile can be a step function or a smooth function, such as in FIG. Figure 8 As shown in the example of . The symmetrical variable speed as shown in the example is used to obtain uniform etching across the entire wafer 180, such as Fig. 9 shown.

[0063] Scanning the wafer 180 across the beam 130 does not address the second cause of asymmetry between the inside and outside of the device. This second cause of asymmetry is due to the large distance required to enable scanning of the tilted wafer 180 across the beam 130, the limited size of the ion source 105 and the ion extraction grid system 150, and the small beam divergence. This effect is Figure 10a to Figure 10b At large distances, the limited lateral dimensions and small beam divergence of the ion source 105 result in the interior side 191 of the device being exposed to a greater number of ions than the exterior side of the device. This asymmetry exists at all tilt angles. Figures 10a to 10b When the rotating wafer 180 is scanned on the beam 130, the amount of etching on the outer side 192 of the device at the outer edge of the wafer 180 is much less than the amount of etching on the inner side 191 of the device, as shown in FIG. Figure 10a to Figure 10b The solid angles projected from the inner side 191 of the device and the outer side 192 of the device to the plane of the ion extraction grid system 150 represent the beam exposure on the inner side 191 and the outer side 192, respectively, when the wafer 180 is scanned on the beam 130. Fig.10a and Fig.10b In FIG. 1 , the imbalance in beam exposure of the inner side 191 and the outer side 192 of the device can be clearly seen.

[0064] The inner and outer etching asymmetries associated with the limited size and small beam divergence of the ion source 105 can be addressed by making the ion source 105 and the grids of the ion extraction grid system 150 significantly larger in the Y-axis direction, as shown in FIG. Figure 11a to Figure 11b shown. Fig.11a A beam 130 is shown having a higher flux at the center of the beam 130. It is possible to have a beam 130 with higher energy at the edge of the beam 130 than at the center of the beam 130 (not shown). Fig.11b A uniform beam 130 is shown, where the flux is independent of the position in the beam 130. The Y-axis direction is the scanning direction. Fig.11b As shown, increasing the lateral dimension of the grids of the ion source 105 and the ion extraction grid system 150 to at least equal to the sum of the chip diameter and twice the beamlet divergence and making the ion flux uniform in the lateral dimension can allow the inner side 191 and the outer side 192 of the device to be exposed to the same ion beam exposure and eliminate the asymmetry between the inner side 191 and the outer side 192 of the device.

[0065] Fig.11a The non-ideal ion beam shown in shows an example when the flux of the ion beam 130 is higher at the center of the beam 130 than at the edge of the beam 130. It is possible to have an ion beam 130 where the flux of the ion beam 130 is higher at the edge of the beam 130 than at the center of the beam 130 (e.g., by magnetic confinement of the beam, a non-uniform grid system, etc.). In this case, it may be desirable to increase the dose in the center of the wafer 180 compared to the edge of the wafer 180 during the scan. The scan speed at the end of the scan can be greater than the scan speed in the center of the scan (e.g., the scan speed toward at least one point at the end of the scan is higher than the scan speed toward a point in the center of the scan).

[0066] Establishing and maintaining a uniform plasma distribution across a large ion source 105 may be difficult in practice. Large variations in plasma density across the lateral dimensions of the plasma source may be difficult to resolve. The large lateral dimensions of the grid may lead to failures caused by mechanical instabilities associated with thermal expansion and contraction cycles of ion source operation. Due to the particularly large challenges associated with larger sized ion sources and larger sized grids, it is desirable to address the asymmetry problem with smaller ion sources and smaller grids.

[0067] refer to Fig.12 When the center of the wafer is located at the far side of the scan 301 (eg, the wafer scan position is far from the ion beam source 105), slowing down the scan speed may also improve uniformity. Fig.12As shown, the scan speed can be reduced for at least a portion of the points below the mid-plane 310 of the ion source 105 and the ion extraction grid system 150. The reduced scan speed enhances etching on the outer side 192 of the device. By slowing the scan speed when the center of the wafer is on the far side of the scan, the inner side and outer side asymmetry (which may exist in scanning at a symmetric speed) can be improved.

[0068] Fig.13 An example of a scanning speed distribution described by the system of the present disclosure is shown. Fig.13 In the schematic diagram shown, the positive x position is a position 301 far from the center of the wafer where the scan speed is reduced to increase etching on the outer side 192 of the device. By increasing the scan speed on the negative x side of the scan (e.g., as the wafer 180 is closer to the ion source 105), rather than those requirements for good uniformity in the symmetrical variable scan profile 303, overall excellent uniformity of etching across the wafer 180 can be maintained.

[0069] The scanning speed can be a function of the distance of the ion beam 105 from the wafer during scanning. During scanning, as the distance between the wafer 180 and the ion beam 130 increases, the scanning speed can decrease. As the area of ​​the wafer 180 exposed to the beam 130 increases, the scanning speed can increase. As the area of ​​the wafer 180 exposed to the beam 130 decreases, the scanning speed can decrease.

[0070] In some embodiments, the scan acceleration may vary during a scan. The scan acceleration profile may be asymmetric. The scan acceleration may be the same between at least two scans. The scan acceleration curve is a graph of wafer acceleration relative to the position of the wafer 180 along the scan path. The scan acceleration curve may be the same for more than two scans. The scan acceleration curve may be the same for all scans. The scan acceleration curve may be different between at least two scans. The scan acceleration curve may be different for more than two scans. The scan acceleration curve may be different for all scans. The scan acceleration may be constant during at least a portion of the scan. The scan speed may be selected to maintain a constant dose of ions across at least one region of the wafer 180 during the scan. The scan speed may be selected to maintain a constant dose of ions across all exposed regions of the wafer 180 during the scan.

[0071] When the wafer center is at the near side of scan 302, i.e., a point above the mid-plane 310 of the ion source 105 and the grid system 150, as shown in FIG. Fig.14 As shown, increasing the scan speed reduces etching on the inner side 191 of the device. Figure 8 , Fig.13 , Fig.14 and Fig.15 In the schematic diagram shown, the negative X position is on the near side 302 of the scan. When the center of the wafer is on the near side 302, increasing the scan speed reduces etching on the inner side 191 of the device. By reducing the scan speed on the positive X side of the scan, an overall excellent uniformity of etching across the wafer 180 is maintained. Fig.13 , the relationship of such a velocity profile relative to the symmetrical velocity profile 303 required for good film uniformity across the wafer 180 is shown.

[0072] In some embodiments, the shape of the speed versus position can be a stepped speed configuration or a smoothly varying configuration. Fig.15 denoted by 304. The asymmetric velocity profile causes the wafer 180 to spend more time on the positive x-side (e.g., further away from the ion source 105) than on the negative x-side, thereby ensuring more etching on the outer side 192 of the device compared to the inner side 191 of the device. This process with asymmetric scanning velocities enables inner and outer side asymmetry control even when the etching system is configured with an ion source 105 having a lateral dimension less than the sum of the wafer diameter and twice the projection of the beamlet divergence onto the wafer scan plane.

[0073] The interior side 191 of the device can be preferentially etched by slowing the scan speed on the near side to correct for asymmetries that occur in systems with sources that have a lesser beam density at the center of the source than away from the center of the source.

[0074] Exemplary ion beam etching process parameters are as follows.

[0075] - The power of the plasma source is in the range of about 100W-5kW.

[0076] - The process chamber pressure is in the range of 1E-3 Torr to 1E-5 Torr.

[0077] - The gas composition may contain an inert gas (e.g., Ar, Kr, Xe, He, etc. or a mixture of these gases).

[0078] - The gas composition may contain reactive gases (e.g., halogen-containing gases, C x H y F z , Cl 2 , oxygen-containing gas, O 2 , nitrogen-containing gas, N 2 NF 3 , carbon-containing gases, CH 4 ,CO,CO 2 , sulfur-containing gases, SF 6 , hydrogen-containing gas, H 2 , H 2O or a mixture of these).

[0079] - The gas composition may contain a mixture of inert and reactive gases.

[0080] - The wafer temperature can be in the range of about -40°C to 400°C.

[0081] - The wafer scanning speed may be in the range of about 0.01 mm / sec to 1 cm / sec. In one embodiment, the wafer scanning speed ranges from 1 mm / sec to 100 mm / sec.

[0082] - Wafer rotation speeds range from about 0.5 RPM to 1000 RPM.

[0083] - The ion beam voltage is typically less than about 500 eV.

[0084] - The wafer tilt angle is in a range from about 1 degree (eg, 1 degree off perpendicular to the ion beam 105 ) to about 85 degrees (eg, a glancing angle to the ion beam 105 ).

[0085] Any of the steps and procedures described above, although referred to herein as being included in an etching process, may also be applied to a deposition process.

[0086] Fig.16 An ion beam deposition (IBD) system is shown. In an IBD process, a target 145 is placed in front of an ion source 105. The ion source 105 may include a plasma chamber 110 and an ion extraction grid system 150. The ion extraction grid system 150 includes a plurality of conductive plates having a plurality of holes therein that are aligned from plate to plate. The grid system 150 extracts and helps collimate the ion beamlets that come out of each hole of the plate and forms a substantially collimated ion beam 130. The plasma in the plasma chamber 110 may be generated by methods known in the art, including direct current (DC) and radio frequency (RF) inductively coupled plasma (ICP) coils 160. The energy of the ions extracted from the ion source 105 is defined by the voltage applied to the grid system 150. The extracted ions in the collimated ion beam 130 impact on the target 145, causing the target material to sputter toward the wafer on the wafer stage 140 in the deposition plume.

[0087] The stage 140 can rotate the wafer about a central axis. The stage 140 can tilt the wafer relative to the sputtered material for at least a portion of the deposition process. By tilting the wafer stage 140, the deposition plume of sputtered material from the target 145 can be directed at any angle relative to the wafer surface. Provision can be made on the wafer stage 140 to cool the wafer during the deposition process to prevent thermal damage to devices on the wafer. The wafer can also be heated to a specific temperature to enhance the ion beam deposition process.

[0088] In an ideal ion beam deposition system, all beamlets and sputtered material in the deposition plume would be perfectly collimated, with no divergence of ions and / or sputtered material from the intended direction. In such a system, all features deposited on the wafer would be perfectly symmetrical. However, practical ion beam deposition systems have non-zero beam divergence and non-zero deposition plume divergence.

[0089] In practice, an ion source produces an ion beam that is a collection of small beams with a finite non-zero beam divergence. In addition, the sputtered material in the deposition plume has a finite non-zero divergence. As a result of the divergence of the sputtered material within the deposition plume, as the wafer is tilted away from the normal sputtered material incidence, there will be a more intense deposition on the side of the wafer close to the target, while there will be a less intense deposition on the side of the wafer away from the target. By rotating the wafer about an axis, the deposition depth can be formed more uniformly in the featureless area of ​​the wafer. However, the devices on the wafer are typically made of three-dimensional features rather than flat surfaces. On the three-dimensional features on the wafer, the effect of the wafer tilting away from the normal sputtered material incidence of the deposition plume and combining the beam divergence is that the inner side of the device on the wafer will experience a different amount of sputtered material exposure from the deposition plume than the outer side of the device. The asymmetry of the inner and outer sides becomes more pronounced as the position of the device moves away from the tilt axis of the wafer and as the tilt angle increases away from the normal sputtered material incidence of the deposition plume.

[0090] Translating (e.g., scanning) the wafer over the deposition plume of sputtered material can account for asymmetries between the interior side of the device and the exterior side of the device. Fig.17 In the embodiment of the present invention, the location where the deposition plume exposure occurs is defined by the introduction of physical beam blocks 171 and 172. As shown in FIG17, by inserting physical blocks 171 and 172 toward the end of the scan, the required scan length can be reduced. Blocks 171 and 172 form an orifice that narrows the deposition plume of sputtered material, thereby creating a portion or "slit" of the deposition plume through which the wafer is scanned. Fig.17As shown, blocks 171 and 172 can be inserted symmetrically with respect to the mid-plane of the deposition plume. Blocks 171 and 172 can be inserted asymmetrically with respect to the mid-plane of the deposition plume. By adjusting the position of the upper block 171 or the lower block 172 or both, the slit width can be adjusted. However, in the case where it is necessary to scan the wafer across the slit of the deposition plume at a large tilt angle, the distance from the target to the wafer at the midpoint of the scan of the wafer can be much larger than in a conventional ion beam deposition (IBD) system.

[0091] In a practical IBD system, the beam density of the deposition plume of sputtered material can be spatially non-uniform. This non-uniformity may be due to divergence of the deposition plume. This effect generally increases with increasing target-to-wafer distance and can be amplified by larger distances between midpoints of the wafer scan. Scanning a wafer through the deposition plume at a constant scan speed results in highly non-uniform deposition, where deposition at the center of the wafer is much faster than at the edges of the wafer. Deploying a variable scan speed can significantly improve deposition uniformity across the wafer. Slowing the scan speed as the wafer moves away from the midpoint of the scan can enhance the deposition process at points of the wafer away from its center.

[0092] In some embodiments, the wafer speed may be varied during a wafer scan. The wafer scan speed may be varied continuously during a scan. The wafer scan speed may be constant during certain portions of a scan. The wafer speed profile may be the same for at least two scans. The wafer scan speed profile may be the same for all scans. The wafer scan speed may be varied between at least two scans. The wafer scan speed profile may vary for each scan. The wafer scan speed may be zero during at least one point during a scan. The wafer speed profile may be symmetrical. The scan speed profile may be monotonic. The scan speed profile may be discontinuous.

[0093] Fig.18An ion beam deposition system with a pre-cleaning auxiliary source is shown. In this embodiment of the present invention, an additional ion source 106 is provided in the ion beam deposition system. At least one surface of a wafer on a wafer stage 140 can be exposed to a beam 135 from the ion source 106. The ion source 106 can include a plasma chamber 111 and an ion extraction grid system 151. The ion extraction grid system 151 includes a plurality of conductive plates with a plurality of holes aligned from plate to plate in the plurality of conductive plates. The grid system 151 extracts and helps collimate the ion beamlets coming out of each hole of the plate and forms an ion beam 135. The plasma in the plasma chamber 111 can be generated by methods known in the art, including direct current (DC) and radio frequency (RF) inductively coupled plasma (ICP) coils 161. The energy of the ions extracted from the ion source 106 is defined by the voltage applied to the grid system 151. The ion beam 135 from the ion source 106 can be used to improve the film properties of the deposited material, such as the stoichiometric ratio of the compound, internal stress, optical properties, etc. The ion beam 135 from the ion source 106 can also be used to pre-clean the wafer prior to the deposition process to enhance film adhesion to the wafer. However, integration of the ion source 106 within the IBD does not change the inherent inside / outside asymmetry of sidewall deposition thickness on 3-D features.

[0094] Although various examples and other information are used to explain various aspects within the scope of the appended claims, limitations on the claims should not be implied based on specific features or arrangements in such examples, because a person of ordinary skill will be able to use these examples to derive a variety of implementations. In addition, although some subjects have been described in language specific to examples of structural features and / or method steps, it should be understood that the subject matter defined in the appended claims is not necessarily limited to the features or actions described. For example, such functions may be distributed differently or performed in components other than those identified herein. On the contrary, the described features and steps are disclosed as examples of components of systems and methods within the scope of the appended claims. In addition, the claim language stating "at least one" set indicates that one member of the set or multiple members of the set satisfy the claim.

Claims

1. A method for depositing a uniform layer of sputtered material onto the wafer in an ion beam sputtering system having a vacuum chamber, a wafer on a stage, a target material, and an ion beam source, the method comprising the following steps: generating ions from said ion beam source; directing the generated ions onto the target material whereby a portion of the target material is sputtered toward the wafer as part of a deposition plume; exposing the wafer to the deposition plume within a deposition zone; as well as The wafer is scanned across the deposition zone along a scan path relative to the deposition plume, wherein a scan speed of the wafer varies as the wafer travels along the scan path, wherein the scan speed decreases as an area of ​​the wafer exposed to the deposition plume decreases. 2 . The method of claim 1 , further comprising rotating the stage during at least a portion of the scanning step.

3. The method of claim 1, further comprising tilting the stage relative to the deposition plume during at least a portion of the scanning step.

4. The method according to claim 1, wherein: The scan path is linear.

5. The method according to claim 1, wherein: The scan path is non-linear. The method of claim 1 , further comprising inserting a plurality of physical blocks along the scan path.

7. The method of claim 1, further comprising adjusting an amount of time the wafer is exposed to the deposition plume.

8. The method according to claim 1, wherein: The scanning speed of the wafer is slowed as the center of the wafer travels along a distal side of the scanning path.

9. The method according to claim 1, wherein: During the scanning step, the scanning speed decreases as the distance between the wafer and the target material increases.

10. A method for depositing a uniform material layer onto a wafer in an ion beam sputtering system having a vacuum chamber, a wafer on a stage, a target material, and an ion beam source, the method comprising the following steps: generating ions from said ion beam source; directing the generated ions onto the target material whereby a portion of the target material is sputtered toward the wafer as part of a deposition plume; exposing the wafer to the deposition plume within a deposition zone; as well as The wafer is scanned across the deposition zone along a scan path relative to the deposition plume according to a scan speed function, wherein a scan speed of the wafer varies as the wafer travels along the scan path, wherein the scan speed decreases as an area of ​​the wafer exposed to the deposition plume decreases.

11. The method of claim 10, further comprising rotating the stage during at least a portion of the scanning step.

12. The method of claim 10, further comprising tilting the stage relative to the deposition plume during at least a portion of the scanning step.

13. The method according to claim 10, wherein: The scan path is linear.

14. The method according to claim 10, wherein: The scan path is non-linear.

15. The method of claim 10, further comprising inserting a plurality of physical blocks along the scan path.

16. The method of claim 10, further comprising adjusting an amount of time the wafer is exposed to the deposition plume.

17. The method according to claim 10, wherein: The scanning path further includes a sweep-out path and a retrace path, wherein the sweep-out path is from a first end of the deposition plume to a second end of the deposition plume, and the retrace path is from the second end of the deposition plume to the first end of the deposition plume, wherein the sweep-out path is the same as the retrace path.

18. The method according to claim 10, wherein: The scanning path further includes a sweep-out path and a retrace path, wherein the sweep-out path is from a first end of the deposition plume to a second end of the deposition plume, and the retrace path is from the second end of the deposition plume to the first end of the deposition plume, wherein the sweep-out path is different from the retrace path.

19. The method according to claim 10, wherein: The scanning path further includes a sweep-out path and a sweep-back path, wherein the sweep-out path is from a first end of the deposition plume to a second end of the deposition plume, and the sweep-back path is from the second end of the deposition plume to the first end of the deposition plume, wherein an endpoint of the sweep-out path is different from an endpoint of the sweep-back path.

20. The method according to claim 10, wherein: The scanning path further includes a sweep path and a retrace path, wherein the sweep path is from a first end of the deposition plume to a second end of the deposition plume according to a sweep velocity function, and the retrace path is from the second end of the deposition plume to the first end of the deposition plume according to a retrace velocity function, wherein the sweep velocity function is different from the retrace velocity function.

21. The method according to claim 10, wherein: The scanning path further includes a sweep path and a retrace path, wherein the sweep path is from a first end of the deposition plume to a second end of the deposition plume according to a sweep velocity function, and the retrace path is from the second end of the deposition plume to the first end of the deposition plume according to a retrace velocity function, wherein the sweep velocity function or the retrace velocity function varies with time.