BOPP (biaxially-oriented polypropylene) pearlized film composite gluing trademark coating device
By using tensioning components, uniform glue coating and drying mechanism in the trademark coating device, the problems of uneven glue coating, low drying efficiency and inaccurate pressure control are solved, and efficient and stable glue coating and compounding process is achieved, improving the improvement of Product quality and production efficiency.
Patent Information
- Application Number
- CN202411192459.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-27
AI Technical Summary
Traditional trademark coating devices have problems such as uneven glue coating, low drying efficiency, inaccurate pressure control, unstable membrane tension and low degree of automation, resulting in unstable product quality and low production efficiency.
A BOPP pearlescent film composite glue coating trademark coating device was designed, using tensioning components, uniform glue coating mechanism, drying mechanism and composite mechanism to achieve continuous production through coordinated operation, ensuring stable film tension, uniform glue coating and rapid drying and compound precision to reduce manual intervention.
It improves production speed and product quality, ensures firm bonding between glue and film, reduces bubble and layering defects, improves the durability and overall quality of the product, and meets the market's demand for high-quality and standardized products.
Smart Images

Figure CN119189324A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of production and packaging, in particular to a BOPP pearlescent film composite glue-coated trademark coating device. Background Art
[0002] In the field of modern commodity production and packaging, the quality and appearance of trademarks play a vital role in product identification, promotion and sales. With the continuous improvement of consumers' requirements for product quality and packaging, and the increasingly fierce market competition, the development of efficient and high-quality trademark coating equipment has become an urgent need in the industry.
[0003] There are often many problems with traditional trademark coating processes. For example, during the gluing process, due to the insufficient precision of the gluing equipment, it is easy to cause uneven gluing, which affects the bonding effect between the glue and the film and the appearance quality of the trademark. At the same time, the inefficiency of the drying process or the poor drying effect may cause incomplete curing of the glue, resulting in problems such as degumming of the trademark in subsequent use. During the composite process, previous devices may not be able to achieve precise pressure control and close fit of the two layers of film, thus affecting the firmness of the composite and the overall performance of the product. Moreover, during the entire production process, the tension control of the film is not stable enough, which easily causes deformation and wrinkles of the film, further reducing the quality and production efficiency of the product. In addition, the traditional device has a low degree of automation and requires a lot of manual intervention, which not only increases labor costs, but also makes it difficult to ensure the consistency and stability of production. At the same time, due to the poor synergy of each link, the production process is not smooth enough, affecting the overall production speed and production capacity.
[0004] Therefore, we propose a BOPP pearlescent film composite glue coating trademark coating device to solve the above problems. Summary of the invention
[0005] The purpose of the present invention is to solve the problems in the prior art and to propose a BOPP pearl film composite glue coating trademark coating device.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] A BOPP pearl film composite glue-coated trademark coating device comprises a frame, two mounting frames are symmetrically mounted on the frame, a tensioning wheel is mounted on each mounting frame through a tensioning assembly, two U-shaped card slots are symmetrically provided on the upper end of each mounting frame, a pearl film roller is commonly clamped on the two U-shaped card slots on one mounting frame, and a composite film roller is commonly clamped on the two U-shaped card slots on the other mounting frame, a driving motor is provided at one end of the composite film roller, and the driving motor is mounted on the side wall of the mounting frame;
[0008] A gluing mechanism is also installed on the mounting frame on which the pearl film roller is clamped, and a drying mechanism is installed on the frame, and the drying mechanism is located on a side of the gluing mechanism away from the pearl film roller;
[0009] An extension frame is also provided on the mounting frame on which the composite film roller is clamped, and a composite mechanism and a trademark film roller are installed on the extension frame.
[0010] In the above-mentioned BOPP pearl film composite glue-coated trademark coating device, the glue coating mechanism includes a glue cylinder and a glue barrel, and the glue barrel is installed on the frame, and the glue cylinder is fixedly installed on the mounting frame, and a liquid pump is installed in the glue barrel, and the output end of the liquid pump is connected to the glue cylinder through a connecting pipe;
[0011] The glue coating mechanism also includes a first motor, and the first motor is fixedly mounted on a mounting frame at a corresponding position. The output end of the first motor extends into the glue cylinder and is equipped with a glue spreading frame. The glue cylinder is evenly connected with a plurality of glue coating tubes.
[0012] In the above-mentioned BOPP pearlescent film composite glue-coated trademark coating device, each of the tensioning components includes two symmetrically arranged tensioning frames, and each tensioning frame is installed on the mounting frame through a connecting shaft, and a torsion spring is installed between each of the tensioning frames and the mounting frame, and the torsion spring is sleeved on the connecting shaft;
[0013] Each of the tensioning frames is provided with a movable groove, and both ends of the tensioning wheel are slidably connected in the movable grooves at corresponding positions. A tensioning spring is installed between the inner wall of each movable groove and the tensioning wheel, and the tensioning spring is located in the movable groove.
[0014] In the above-mentioned BOPP pearlescent film composite glue-coated trademark coating device, the drying mechanism includes a support frame, and the support frame is installed on the upper end surface of the frame, a hot air blower is installed on the support frame, a buffer box is installed on the upper end of the support frame, the output end of the hot air blower is connected to the buffer box through an air supply pipe, and the upper end surface of the buffer box is evenly connected with an air outlet pipe.
[0015] In the above-mentioned BOPP pearlescent film composite glue-coated trademark coating device, a scraper is installed on the upper end surface of the buffer box, and the scraper is located on the side close to the glue coating mechanism, and the length of the scraper is equal to the width of the buffer box.
[0016] In the above-mentioned BOPP pearlescent film composite glue-coated trademark coating device, the glue-distributing frame includes a central axis, and the central axis is fixedly connected to the output end of the first motor, and a plurality of glue-pushing plates are symmetrically installed on the outer wall of the central axis, and both ends of each glue-pushing plate are in contact with the inner wall of the glue cylinder, and the port of the connecting pipe is located between two adjacent glue-pushing plates.
[0017] In the above-mentioned BOPP pearlescent film composite glue-coated trademark coating device, the glue-distributing frame includes a central axis, and the central axis is fixedly connected to the output end of the first motor, and a plurality of glue-pushing plates are symmetrically installed on the outer wall of the central axis, and both ends of each glue-pushing plate are in contact with the inner wall of the glue cylinder, and the port of the connecting pipe is located between two adjacent glue-pushing plates.
[0018] Compared with the prior art, the present invention has the following beneficial effects:
[0019] 1. The coordinated operation of various mechanisms realizes the continuous production of gluing, drying and laminating, reduces the waiting time between production links, and greatly improves the overall production speed; the rapid drying process shortens the glue curing time, allowing the product to enter the next process faster, speeding up the production rhythm; the automated gluing and laminating operations reduce manual intervention, reduce production interruptions and efficiency reductions caused by human factors, and effectively improve production efficiency.
[0020] 2. The tensioning component keeps the film in a stable tension during transmission, avoiding deformation and wrinkles of the film, ensuring the flatness and accuracy of gluing and lamination, and improving the appearance quality of the product. The uniform gluing mechanism can ensure that the glue is evenly distributed on the pearlescent film, making the bond between the glue and the film stronger and enhancing the durability of the product. The effective drying mechanism ensures that the glue solidifies in time, avoiding poor bonding and quality problems caused by undried glue, and improving the performance stability of the product. The precise laminating mechanism makes the two layers of film tightly combined, reducing defects such as bubbles and stratification, and improving the overall quality of the product.
[0021] 3. The automated control and stable operating parameters of the device can ensure that each production batch of products is highly consistent in terms of glue coating amount, drying degree and composite effect, avoiding the differences caused by manual operation, making the product quality more stable and reliable, and meeting the market demand for high-quality, standardized products.
[0022] In summary, the present invention, through the synergistic effect of its various mechanisms, has significant beneficial effects in improving production efficiency, ensuring product quality, reducing costs, enhancing operational convenience and improving market competitiveness, bringing important value to the production and development of enterprises. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 This is a schematic diagram of the structure of a BOPP pearlescent film composite glue-coated trademark coating device proposed by the present invention;
[0024] Figure 2 This is an enlarged view of the structure of the pearl film roller in a BOPP pearl film composite glue-coated trademark coating device proposed by the present invention;
[0025] Figure 3This is an enlarged view of the structure of the composite film roller in a BOPP pearlescent film composite glue-coated trademark coating device proposed by the present invention;
[0026] Figure 4 This is an enlarged view of the tensioning frame structure of a BOPP pearlescent film composite glue-coated trademark coating device proposed by the present invention;
[0027] Figure 5 This is an enlarged view of the torsion spring structure in a BOPP pearlescent film composite glue-coated trademark coating device proposed by the present invention;
[0028] Figure 6 This is an enlarged view of the structure of the glue cylinder in a BOPP pearlescent film composite glue-coated trademark coating device proposed by the present invention;
[0029] Figure 7 This is an enlarged view of the structure of the glue-spreading frame in the BOPP pearlescent film composite glue-coated trademark coating device proposed by the present invention.
[0030] In the figure: 1 frame, 2 glue barrel, 3 mounting frame, 4 pearl film roller, 5 tensioning frame, 6 tensioning wheel, 7 first motor, 8 composite roller, 9 transmission gear, 10 composite film roller, 11 extension frame, 12 support frame, 13 hot air blower, 14 air pipe, 15 buffer box, 16 connecting shaft, 17 movable groove, 18 tensioning spring, 19 U-shaped card slot, 20 second motor, 21 trademark film roller, 22 connecting pipeline, 23 torsion spring, 24 glue cylinder, 25 glue coating tube, 26 glue leveling frame;
[0031] 26 glue spreading rack, 2601 center axis, 2602 glue pushing plate. DETAILED DESCRIPTION
[0032] The following examples are for illustrative purposes only and are not intended to limit the scope of the present invention.
[0033] Example
[0034] Reference Figure 1-7A BOPP pearlescent film composite glue coating trademark coating device includes a frame 1, two mounting frames 3 are symmetrically mounted on the frame 1, each mounting frame 3 is mounted with a tensioning wheel 6 through a tensioning assembly, each tensioning assembly includes two symmetrically arranged tensioning frames 5, and each tensioning frame 5 is mounted on the mounting frame 3 through a connecting shaft 16, each tensioning frame 5 and the mounting frame 3 are jointly installed with a torsion spring 23, and the torsion spring 23 is sleeved on the connecting shaft 16; each tensioning frame 5 is provided with a movable groove 17, and both ends of the tensioning wheel 6 are slidably connected to the movable groove 1 corresponding to the position 7, a tensioning spring 18 is installed between the inner wall of each movable groove 17 and the tensioning wheel 6, and the tensioning spring 18 is located in the movable groove 17; it effectively maintains the stability of the tension of the film during the transmission process, prevents the film from wrinkling, deformation or excessive stretching due to improper tension, thereby ensuring the flatness and dimensional accuracy of the film, reducing the problems of uneven glue coating and loose composite due to fluctuations in film tension, improving the consistency and quality stability of the product, adapting to films of different specifications and materials, and being able to flexibly adjust the tension according to the characteristics of the film, thereby broadening the scope of application of the device to raw materials.
[0035] Two U-shaped slots 19 are symmetrically provided at the upper end of each mounting frame 3, wherein the two U-shaped slots 19 on one mounting frame 3 are jointly provided with a pearlescent film roller 4, and the two U-shaped slots 19 on the other mounting frame 3 are jointly provided with a composite film roller 10, and a drive motor is provided at one end of the composite film roller 10, and the drive motor is installed on the side wall of the mounting frame 3.
[0036] A gluing mechanism is also installed on the mounting frame 3 on which the pearlescent film roller 4 is clamped. The gluing mechanism includes a glue cylinder 24 and a glue barrel 2, and the glue barrel 2 is installed on the frame 1, and the glue cylinder 24 is fixedly installed on the mounting frame 3, a liquid pump is installed in the glue barrel 2, and the output end of the liquid pump is connected to the glue cylinder 24 through a connecting pipe 22; the gluing mechanism also includes a first motor 7, and the first motor 7 is fixedly installed on the mounting frame 3 at a corresponding position, the output end of the first motor 7 extends into the glue cylinder 24 and is installed with a glue leveling rack 26, a plurality of glue coating tubes 25 are evenly connected to the glue cylinder 24, the glue leveling rack 26 includes a central axis 2601, and the central axis 2601 is fixedly connected to the output end of the first motor 7, and the outer wall of the central axis 2601 is symmetrically arranged A plurality of glue pushing plates 2602 are provided, and both ends of each glue pushing plate 2602 are in contact with the inner wall of the glue cylinder 24, and the port of the connecting pipe 22 is located between two adjacent glue pushing plates 2602. The cooperation between the glue barrel 1 and the glue cylinder 24, and the precise delivery of the liquid pump ensure the continuity and stability of the glue supply and avoid the glue breaking phenomenon during the gluing process. The rotating movement of the glue leveling rack 26 can make the glue fully stirred and evenly distributed in the glue cylinder 24, so that the pearlescent film can be evenly coated through the glue coating tube 25, avoiding the situation of excessive or insufficient local glue, and improving the glue coating quality. The uniform and appropriate amount of glue coating helps to enhance the bonding force between the pearlescent film and the trademark film, and improve the firmness and durability of the composite product.
[0037] A drying mechanism is installed on the frame 1, and the drying mechanism is located on the side of the glue coating mechanism away from the pearl film roller 4. The drying mechanism includes a support frame 12, and the support frame 12 is installed on the upper end surface of the frame 1. A hot air blower 13 is installed on the support frame 12, and a buffer box 15 is installed on the upper end of the support frame 12. The output end of the hot air blower 13 is connected with the buffer box 15 through an air supply pipe 14, and the upper end surface of the buffer box 15 is evenly connected with an air outlet pipe. A scraper is installed on the upper end surface of the buffer box 15, and the scraper is located on the side close to the glue coating mechanism, and the length of the scraper is equal to the width of the buffer box 15; the scraper can scrape off excess glue on the pearl film to ensure that the thickness of the glue coating layer is uniform and meets the requirements, avoid waste caused by too thick a glue layer, and prevent the glue layer from being too thin to affect the bonding effect. Through the scraping effect of the scraper, the surface of the film after glue coating is smoother and the glue distribution is more even. The quality and consistency of the product can be improved. An appropriate amount of glue layer helps to evenly transfer heat during the drying process, promotes the rapid curing of glue, and improves drying efficiency and quality. Uniform and appropriate glue coating can make the bond between glue and film stronger, improve the durability of the trademark during use, and make the surface of the film after glue coating neat and smooth, without traces of glue accumulation or flow, thereby improving the appearance quality of the final product; the combination of the hot air blower 13 and the buffer box 15 can produce uniform and stable hot air, quickly and effectively dry the pearlescent film after glue coating, greatly shortening the production cycle, and the uniform drying effect helps the glue to evenly cure, avoiding the situation of local undried or over-dried, ensuring the quality and performance of the glue coating layer, and timely drying can prevent the glue from being contaminated or damaged in the uncured state, thereby improving the product qualification rate and production efficiency.
[0038] An extension frame 11 is also provided on the mounting frame 3 on which the composite film roller 10 is clamped, and a composite mechanism and a trademark film roller 21 are installed on the extension frame 11. The composite mechanism includes two symmetrically arranged composite rollers 8, and the two composite rollers 8 are both located on the extension frame 11. Transmission gears 9 are installed at both ends of each composite roller 8, and the two transmission gears 9 are meshed. A second motor 20 is installed at the end of one of the composite rollers 8 away from the transmission gear 9; the synchronous reverse rotation of the two composite rollers 8 and the meshing of the transmission gears 9 can achieve uniform pressing of the pearlescent film and the trademark film to ensure the tightness and consistency of the composite. Appropriate pressure and speed control help to fully penetrate and bond the glue between the two layers of film, further improving the strength and stability of the composite product. Precise composite operation can reduce the occurrence of defects such as bubbles and stratification, and improve the appearance quality and performance of the product.
[0039] Working principle:
[0040] First, before compounding, the composite film roller 10, the pearl film roller 4 and the trademark film roller 21 are installed. After the installation is completed, the driving motor is started to make the composite film roller 10 start to rotate, providing power for the subsequent film winding. When the pearl film released from the pearl film roller 4 passes through the tensioning wheel 6, due to the action of the torsion spring 23 between the tensioning frame 5 and the mounting frame 3 and the tensioning spring 18 between the tensioning wheel 6 and the inner wall of the movable groove 17, it can ensure that the pearl film always maintains an appropriate and stable tension. This stable tension is conducive to the smooth progress of the subsequent gluing and compounding processes, and avoids undesirable conditions such as film relaxation, wrinkles or excessive stretching. Then, the glue in the glue barrel 2 is transported to the glue cylinder 24 through the connecting pipe 22 under the action of the liquid pump. At this time, the first motor 7 drives the glue leveling frame 26 to rotate, and the central axis 2601 of the glue leveling frame 26 drives the push The glue plate 2602 rotates, and the two ends of the glue pushing plate 2602 contact the inner wall of the glue cylinder 24, so that the glue entering the glue cylinder 24 can be evenly distributed. The evenly distributed glue is then evenly coated on the lower surface of the passing pearlescent film through a number of glue coating tubes 25 evenly connected on the glue cylinder 24. The pearlescent film after glue coating continues to move forward. When passing through the scraper, the scraper scrapes off the excess glue on the pearlescent film to make the glue coating more uniform and appropriate, thereby ensuring the subsequent drying and compounding effects. Subsequently, the hot air blower 13 works to generate hot air, and the hot air is transported to the buffer box 15 through the air supply pipe 14. The buffer box 15 plays a role in buffering and evenly distributing the hot air, so that the hot air can be more evenly blown out from the air outlet pipes evenly connected to its upper end face, and the pearlescent film after glue coating is dried. This can accelerate the curing of the glue and improve production efficiency and coating quality. At the same time, the trademark film is released from the trademark film roller 21 and enters the composite mechanism together with the dried pearl film. In the composite mechanism, one of the composite rollers 8 is driven by the second motor 20 to rotate, and the two composite rollers 8 are synchronously rotated in opposite directions through the mutually meshing transmission gears 9 installed at both ends of the two composite rollers 8, so that the pearl film and the trademark film are pressed together to achieve a firm composite. Finally, the composite film passes through the tension wheel 6 to maintain tension again to ensure the flatness of the film and the tightness of the winding, and then is wound on the composite film roller 10 to complete the entire coating and composite process.
[0041] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A BOPP pearlescent film composite glue-coated trademark coating device, comprising a frame (1), characterized in that: Two mounting frames (3) are symmetrically mounted on the frame (1), each mounting frame (3) is mounted with a tensioning wheel (6) via a tensioning assembly, and each mounting frame (3) is symmetrically provided with two U-shaped card slots (19) at the upper end, wherein the two U-shaped card slots (19) on one of the mounting frames (3) are commonly provided with a pearlescent film roller (4), and the two U-shaped card slots (19) on the other mounting frame (3) are commonly provided with a composite film roller (10), and a driving motor is provided at one end of the composite film roller (10), and the driving motor is mounted on the side wall of the mounting frame (3); A gluing mechanism is also installed on the mounting frame (3) on which the pearlescent film roller (4) is mounted, and a drying mechanism is installed on the frame (1), and the drying mechanism is located on a side of the gluing mechanism away from the pearlescent film roller (4); An extension frame (11) is also provided on the mounting frame (3) on which the composite film roller (10) is mounted, and a composite mechanism and a trademark film roller (21) are mounted on the extension frame (11).
2. The BOPP pearl film composite glue-coated trademark coating device according to claim 1 is characterized by: The glue coating mechanism comprises a glue cylinder (24) and a glue barrel (2), wherein the glue barrel (2) is mounted on a frame (1), and the glue cylinder (24) is fixedly mounted on a mounting frame (3), a liquid pump is installed in the glue barrel (2), and an output end of the liquid pump is connected to the glue cylinder (24) via a connecting pipe (22); The glue coating mechanism also includes a first motor (7), and the first motor (7) is fixedly mounted on a mounting frame (3) at a corresponding position, the output end of the first motor (7) extends into a glue cylinder (24) and is equipped with a glue spreading frame (26), and the glue cylinder (24) is evenly connected to a plurality of glue coating tubes (25).
3. The BOPP pearl film composite glue-coated trademark coating device according to claim 1 is characterized by: Each of the tensioning components comprises two tensioning frames (5) which are symmetrically arranged, and each tensioning frame (5) is mounted on the mounting frame (3) via a connecting shaft (16); a torsion spring (23) is installed between each of the tensioning frames (5) and the mounting frame (3), and the torsion spring (23) is sleeved on the connecting shaft (16); Each of the tensioning frames (5) is provided with a movable groove (17), and both ends of the tensioning wheel (6) are slidably connected in the movable grooves (17) at corresponding positions. A tensioning spring (18) is installed between the inner wall of each movable groove (17) and the tensioning wheel (6), and the tensioning spring (18) is located in the movable groove (17).
4. The BOPP pearl film composite glue-coated trademark coating device according to claim 1 is characterized by: The drying mechanism comprises a support frame (12), and the support frame (12) is mounted on the upper end surface of the frame (1), a hot air blower (13) is mounted on the support frame (12), a buffer box (15) is mounted on the upper end of the support frame (12), an output end of the hot air blower (13) is connected to the buffer box (15) through an air delivery pipe (14), and an upper end surface of the buffer box (15) is evenly connected to an air outlet pipe.
5. The BOPP pearl film composite glue-coated trademark coating device according to claim 4 is characterized by: A scraper is installed on the upper end surface of the buffer box (15), and the scraper is located on a side close to the glue coating mechanism, and the length of the scraper is equal to the width of the buffer box (15).
6. The BOPP pearl film composite glue-coated trademark coating device according to claim 2 is characterized by: The glue spreading frame (26) includes a central axis (2601), and the central axis (2601) is fixedly connected to the output end of the first motor (7), and a plurality of glue pushing plates (2602) are symmetrically installed on the outer wall of the central axis (2601), and both ends of each glue pushing plate (2602) are in contact with the inner wall of the glue cylinder (24), and the port of the connecting pipe (22) is located between two adjacent glue pushing plates (2602).
7. The BOPP pearl film composite glue-coated trademark coating device according to claim 1 is characterized by: The composite mechanism comprises two composite rollers (8) which are symmetrically arranged, and the two composite rollers (8) are both located on an extension frame (11), and transmission gears (9) are installed at both ends of each composite roller (8), and the two transmission gears (9) are meshed, and a second motor (20) is installed at one end of one of the composite rollers (8) away from the transmission gear (9).