Processing methods for composite metal frames, composite metal frames and electronic devices
By depositing molten filler metal into the deposition holes of the composite metal frame and solidifying it to form a filler, the problem of uneven connection during the hot melt drilling process is solved, thus improving the quality of the composite metal frame.
Patent Information
- Application Number
- CN202411393201.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-09-30
AI Technical Summary
During the hot melt drilling process, uneven release of processing stress in the outer metal material leads to poor uniformity at the joint of the composite metal frame, resulting in lower quality.
During the processing of the composite metal frame, a deposition hole is formed and molten filler metal is deposited in it to form a filler body that fits tightly against the inner wall of the main hole segment. Part of the filler body and the corresponding second metal layer are removed to form a mounting hole, so that the filler body and the second metal layer are exposed from the inner wall of the mounting hole.
It improves the uniformity of the connection of the composite metal frame, reduces the defects of sidewall cracking in CNC machining, and improves the quality of the composite metal frame.
Smart Images

Figure CN119426784B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of metal processing technology, specifically to a processing method for a composite metal frame, a composite metal frame, and an electronic device. Background Technology
[0002] When two metal materials are stacked together by a hot melt drill, a deposition hole is usually first machined on the inner metal material. Then, a tool with a sharp angle is used to rotate at high speed on the surface of the outer metal material and squeeze it from the outer metal material to the inner metal material. The outer metal material is melted at high temperature and high frequency to form a hot melt hole that connects to the deposition hole. The sidewall of the hot melt hole is formed by the melted metal material and adheres to at least part of the sidewall of the deposition hole.
[0003] However, due to the uneven release of processing stress on the outer metal material during the hot melt drilling process, problems such as cracking or missing parts of the sidewall of the formed hot melt hole occur, resulting in poor uniformity of the two metal materials at the joint and low quality of the composite metal frame. Summary of the Invention
[0004] In view of the above, it is necessary to provide a processing method for composite metal frames, composite metal frames, and electronic devices to improve the quality of composite metal frames.
[0005] To achieve the above objectives, in a first aspect, this application discloses a method for processing a composite metal frame, comprising:
[0006] A metal composite substrate is provided, the metal composite substrate comprising a first metal layer and a second metal layer stacked together;
[0007] Deposition holes are formed from the surface of the first metal layer into the interior of the metal composite substrate. Each deposition hole includes a main hole segment and a receiving hole segment connected to each other. The main hole segment is located on one side of the first metal layer, and the receiving hole segment is at least partially received into the second metal layer. The diameter of at least a portion of the receiving hole segment is larger than the diameter of the main hole segment.
[0008] Molten filler metal is deposited and solidified in the deposition hole to form a filler body, such that the filler body fits tightly against the inner wall of the main hole segment;
[0009] A portion of the filler and the second metal layer corresponding to the filler are removed to form a mounting hole, wherein the second metal layer and the filler are exposed from the inner wall of the mounting hole.
[0010] As an optional implementation, in an embodiment of the first aspect of this application, the step of forming a deposition hole from the surface of the first metal layer into the interior of the metal composite substrate includes:
[0011] The first tool is used to drill a hole in the first metal layer into the second metal layer to form the main hole segment;
[0012] A second tool is used to drill a hole from the bottom of the main body hole section toward the second metal layer to form the receiving hole section, which extends into the second metal layer.
[0013] As an optional implementation, in an embodiment of the first aspect of this application, the diameter of the receiving hole segment increases from the end connected to the main hole segment to the end away from the main hole segment.
[0014] As an optional implementation, in an embodiment of the first aspect of this application, the step of depositing molten filler metal within the deposition hole and solidifying it to form a filler includes:
[0015] A filler wire is inserted into the deposition hole and is arranged coaxially with the deposition hole.
[0016] The filler wire is irradiated with a laser whose spot coincides with the center of the deposition hole, so that the filler wire melts and fills the deposition hole to form the filler.
[0017] As an optional implementation, in an embodiment of the first aspect of this application, the processing method of the composite metal frame further includes:
[0018] Images of the deposition pores were captured.
[0019] Determine the position of the light spot on the image and the position of the center of the deposition hole;
[0020] Based on the fact that the position of the light spot and the position of the center of the deposition hole are within a preset error range, it is determined that the center of the light spot coincides with the center of the deposition hole.
[0021] As an optional implementation, in an embodiment of the first aspect of this application, prior to the step of inserting the filling wire into the deposition hole, the method further includes:
[0022] The straightness of the filler wire is adjusted using a wire straightening device;
[0023] The straightness of the adjusted filler wire is tested using a testing device.
[0024] As an optional implementation, in an embodiment of the first aspect of this application, the wire straightening device includes a rotating wheel assembly and an adjusting assembly arranged side by side. The rotating wheel assembly includes n rotating wheels spaced apart, and the adjusting assembly includes (n-1) adjusting members spaced apart. The n rotating wheels and (n-1) adjusting members are arranged alternately. The step of adjusting the straightness of the filler wire using the wire straightening device includes:
[0025] The filler wire is brought into contact with n of the moving wheels, wherein the filler wire includes a first end and a second end opposite to each other;
[0026] The adjusting member corresponding to the first end among (n-1) adjusting members is moved toward the driving wheel assembly and abuts against the first end, so that the second end moves a first distance in a first direction;
[0027] One of the (n-1) adjustment members is moved toward the drive wheel assembly and abuts against the filler wire, so that the second end moves the first distance in a second direction opposite to the first direction;
[0028] The remaining adjustment member of the (n-1) adjustment members is moved toward the drive wheel assembly and abuts against the filler wire to adjust the straightness of the filler wire.
[0029] As an optional implementation, in an embodiment of the first aspect of this application, the detection device includes a detection block with a detection hole, and the step of using the detection device to detect the straightness of the adjusted filler wire includes:
[0030] The filling metal wire is passed through the detection hole of the detection block multiple times;
[0031] Based on the fact that the filler wire does not contact the wall of the detection hole, it is confirmed that the straightness of the filler wire meets the standard.
[0032] As an optional implementation, in an embodiment of the first aspect of this application, the laser is connected to the filler wire, and after confirming that the straightness of the filler wire meets the standard, the method further includes:
[0033] Place the test block in the first position;
[0034] The laser is directed to emit a laser beam toward the center of the test block;
[0035] Based on the fact that the laser spot emitted by the laser is located at the center of the test block, the test block is moved a second distance toward the laser to a second position;
[0036] Determine whether the laser spot emitted by the laser is located at the center of the test block;
[0037] Based on the fact that the laser spot emitted by the laser is located at the center of the test block, the test block is moved away from the laser by the second distance to the first position, and it is determined again whether the laser spot emitted by the laser is located at the center of the test block;
[0038] Based on the fact that the laser spot emitted by the laser is once again located at the center of the test block, the filler wire is moved toward the center of the test block, and it is determined whether the projection of the filler wire on the test block coincides with the center of the test block;
[0039] Based on the fact that the projection of the filler wire on the test block coincides with the center of the test block, it is determined that the laser spot emitted by the laser is concentric with the filler wire.
[0040] As an optional implementation, in an embodiment of the first aspect of this application, the method further includes:
[0041] Based on the fact that the laser spot emitted by the laser is concentric with the filling metal wire, the laser is directed towards the test metal plate, wherein the distance between the test metal plate and the laser is equal to the distance between the bottom of the deposition hole and the laser.
[0042] The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
[0043] As an optional implementation, in an embodiment of the first aspect of this application, the step of determining the position of the laser to be qualified based on the laser spot emitted by the laser towards the test metal plate conforming to a standard includes:
[0044] Detect the color of the laser spot emitted by the laser towards the test metal plate;
[0045] Based on the color of the laser spot emitted by the laser towards the test metal plate, determine whether the laser spot emitted by the laser towards the test metal plate meets the standard;
[0046] The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
[0047] As an optional implementation, in an embodiment of the first aspect of this application, the step of determining the position of the laser to be qualified based on the laser spot emitted by the laser towards the test metal plate conforming to a standard includes:
[0048] Detect the shape of the laser spot emitted by the laser towards the test metal plate;
[0049] Based on the shape of the laser spot emitted by the laser towards the test metal plate, determine whether the laser spot emitted by the laser towards the test metal plate meets the standard;
[0050] The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
[0051] As an optional implementation, in an embodiment of the first aspect of this application, the step of determining the position of the laser to be qualified based on the compliance criteria of the laser emitted by the laser toward the test metal plate includes:
[0052] The size of the laser spot emitted by the laser towards the test metal plate is detected;
[0053] Based on the size of the laser spot emitted by the laser towards the test metal plate, determine whether the laser spot emitted by the laser towards the test metal plate meets the standard;
[0054] The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
[0055] Secondly, this application discloses a composite metal frame, including a first metal layer and a second metal layer stacked together. The composite metal frame also includes deposition holes, which are formed from the surface of the first metal layer into the interior of the metal composite substrate. Each deposition hole includes a main hole segment and a receiving hole segment connected to each other. The main hole segment is located on one side of the first metal layer, and the receiving hole segment is at least partially received into the second metal layer. The diameter of at least a portion of the receiving hole segment is larger than the diameter of the main hole segment. A filler is tightly attached to the inner wall of the deposition hole. The filler and the second metal layer corresponding to the filler are provided with mounting holes, and the second metal layer and the filler are exposed on the inner wall of the mounting holes.
[0056] As an optional implementation, in an embodiment of the second aspect of this application, the material of the first metal layer includes an aluminum alloy, the material of the second metal layer includes titanium or a titanium alloy, and the material of the filler includes titanium.
[0057] Thirdly, this application discloses an electronic device including a composite metal frame as described in the second aspect above.
[0058] In the aforementioned processing method of the composite metal frame, the composite metal frame, and the electronic device, a deposition hole is first formed from the surface of the first metal layer into the interior of the metal composite substrate. The deposition hole includes a main hole segment and a receiving hole segment connected to each other. The main hole segment is located on one side of the first metal layer, and the receiving hole segment is at least partially received into the second metal layer. The diameter of the at least partially receiving hole segment is larger than the diameter of the main hole segment. Then, molten filler metal is deposited in the deposition hole and solidified to form a filler body, so that the filler body is tightly attached to the inner wall of the main hole segment. Finally, part of the filler body and the second metal layer corresponding to the filler body are removed to form a mounting hole. The second metal layer and the filler body are exposed from the inner wall of the mounting hole. Since the diameter of at least partially receiving hole segment is larger than the diameter of the main hole segment, the molten filler metal can fill the deposition hole to form a filler body, reducing the CNC machining sidewall cracking caused by incomplete filling. Furthermore, since the second metal layer and the filler body are exposed from the inner wall of the mounting hole, the filler body can tightly attach to the connection between the first metal layer and the second metal layer, resulting in better uniformity at the connection between the first metal layer and the second metal layer, thereby improving the quality of the composite metal frame. Attached Figure Description
[0059] Figure 1 This is a flowchart illustrating a processing method for a composite metal frame according to an embodiment of this application.
[0060] Figure 2 This is a schematic diagram of the structure of a metal composite substrate proposed in an embodiment of this application.
[0061] Figure 3 for Figure 2 The diagram shows a cross-sectional view of the metal composite substrate along the AA direction.
[0062] Figure 4 for Figure 2 The diagram shows the structure of the metal composite substrate after the filling material has been formed in the deposition pores.
[0063] Figure 5 for Figure 4 The diagram shows a composite metal frame structure obtained by removing part of the filler and the second metal layer corresponding to the filler from the metal composite substrate to form mounting holes.
[0064] Figure 6 A flowchart illustrating the steps involved in forming deposition pores from the surface of the first metal layer into the interior of the metal composite substrate.
[0065] Figure 7 A flowchart illustrating the steps involved in depositing molten filler metal within a deposition well and solidifying it to form a filler.
[0066] Figure 8 This is a schematic diagram of the structure of the metal wire filling the deposition hole under laser irradiation.
[0067] Figure 9 A flowchart illustrating the steps to ensure the center of the light spot coincides with the center of the deposition hole.
[0068] Figure 10 This is a flowchart of the steps preceding the insertion of the filler wire into the deposition hole.
[0069] Figure 11 This is a schematic diagram of the wire straightening device.
[0070] Figure 12 for Figure 11 The diagram shows the process of adjusting the straightness of the metal wire using the wire straightening device.
[0071] Figure 13 This is a schematic diagram of the detection device.
[0072] Figure 14 A flowchart illustrating the steps involved in adjusting the straightness of the filler wire in the wire straightening device.
[0073] Figure 15 A flowchart illustrating the steps involved in using a testing device to detect the straightness of the adjusted filler wire.
[0074] Figure 16 The flowchart shows the steps to confirm that the straightness of the filler wire meets the standard.
[0075] Figure 17 A schematic diagram illustrating the structure used to determine whether the projection of the filler wire onto the test block coincides with the center of the test block.
[0076] Figure 18 This is a top view of the test block.
[0077] Figure 19 A flowchart illustrating the steps for determining the qualified position of the laser in one embodiment of this application.
[0078] Figure 20 A flowchart illustrating the steps for determining the qualified position of the laser in another embodiment of this application.
[0079] Figure 21 This is a schematic diagram of the structure of the laser spot emitted by the laser device of this application.
[0080] Figure 22 A flowchart illustrating the steps for determining the position of the laser to be qualified according to another embodiment of this application.
[0081] Figure 23 A flowchart illustrating the steps for determining the position of the laser in another embodiment of this application.
[0082] Explanation of main component symbols
[0083] Metal composite substrate 100
[0084] First metal layer 10
[0085] Second metal layer 20
[0086] Deposition pore 30
[0087] Main hole section 31
[0088] Accommodation section 32
[0089] Filler 40
[0090] Mounting hole 41
[0091] 200 filler wires
[0092] First end 210
[0093] Second end 220
[0094] Laser 300
[0095] Spot size 310
[0096] 400 yarn straightening device
[0097] Drive wheel assembly 410
[0098] Drive wheel 411
[0099] Adjustment component 420
[0100] Adjustment part 421
[0101] Detection device 500
[0102] Detection Block 510
[0103] Detection well 511
[0104] Laser 601
[0105] Test Block 600
[0106] Scale circle 610
[0107] Composite metal frame 700 Detailed Implementation
[0108] The embodiments of this application are described in detail below. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain this application, and should not be construed as limiting this application.
[0109] In the description of this application, it should be noted that, unless otherwise explicitly specified and limited, the term "connection" should be interpreted broadly. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a connection that allows communication between the components; it can be a direct connection or an indirect connection through an intermediate medium; it can be the internal communication between two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.
[0110] The embodiments of this case will be described in detail below with reference to the accompanying drawings.
[0111] Firstly, please see Figure 1 This application discloses a composite metal frame 700 (e.g., Figure 5 The processing method shown includes:
[0112] S10, please refer to Figure 2 A metal composite substrate 100 is provided, the metal composite substrate 100 including a first metal layer 10 and a second metal layer 20 laminated together.
[0113] The first metal layer 10 is made of aluminum alloy, and the second metal layer 20 is made of titanium or titanium alloy. It is understood that in other embodiments, the first metal layer 10 and the second metal layer 20 may also be made of other metals; no specific limitations are made here. The metal forming the first metal layer 10 has a lower hardness than the metal forming the second metal layer 20, and the second metal layer 20 has stronger chemical stability than the first metal layer 10.
[0114] S20, please refer to Figure 3 A deposition hole 30 is formed from the surface of the first metal layer 10 into the interior of the metal composite substrate 100. The deposition hole 30 includes a main hole segment 31 and a receiving hole segment 32 connected to each other. The main hole segment 31 is located on one side of the first metal layer 10, and the receiving hole segment 32 is at least partially received into the second metal layer 20. The diameter of the at least partially receiving hole segment 32 is larger than the diameter of the main hole segment 31.
[0115] Among them, the deposition pore 30 is roughly T-shaped.
[0116] S30, please refer to Figure 4 Molten filler metal is deposited and solidified in the deposition hole 30 to form filler 40, so that filler 40 fits tightly against the inner wall of the main hole segment 31.
[0117] The filler metal can be made of the same material as the second metal layer 20, i.e., the filler metal is made of titanium or titanium alloy.
[0118] S40, please refer to Figure 5Part of the filler 40 and the second metal layer 20 corresponding to the filler 40 are removed to form a mounting hole 41, and the second metal layer 20 and the filler 40 are exposed from the inner wall of the mounting hole 41.
[0119] In the above-mentioned processing method of composite metal frame 700, since the diameter of at least part of the receiving hole segment 32 is larger than the diameter of the main hole segment 31, the molten filler metal can fill the main hole segment 31 of the deposition hole 30 to form a filler 40, reducing the CNC machining sidewall cracking caused by incomplete filling. Furthermore, the second metal layer 20 and the filler 40 are exposed from the inner wall of the mounting hole 41, and the filler 40 can closely fit the connection between the first metal layer 10 and the second metal layer 20. The uniformity of the connection between the first metal layer 10 and the second metal layer 20 is better, thereby improving the quality of the composite metal frame 700.
[0120] As an optional implementation, please refer to Figure 6 The step of forming deposition holes 30 from the surface of the first metal layer 10 into the interior of the metal composite substrate includes:
[0121] S21, a first tool is used to make a hole in the first metal layer 10 into the second metal layer 20 to form the main hole segment 31.
[0122] S22, using a second tool, drill a hole from the bottom of the main body hole section 31 toward the second metal layer 20 to form a receiving hole section 32, which extends into the second metal layer 20.
[0123] Both the first and second cutting tools are milling cutters. The first and second cutting tools work together to process the deposition holes 30 of the required size.
[0124] In some embodiments, after forming the receiving hole segment 32, a third tool can be used to finish mill the inner wall of the main hole segment 31 so that the filler 40 fits tightly against the inner wall of the main hole segment 31.
[0125] As an optional implementation, the diameter of the receiving hole section 32 increases from the end connected to the main hole section 31 to the end away from the main hole section 31. This ensures that the bottom corner of the main hole section 31 is properly cleared, preventing residue from the bottom of the machining process, which could affect the flow of molten filler metal or cause uneven filling.
[0126] The diameter of the receiving hole section 32 can gradually increase from the end connected to the main hole section 31 to the end away from the main hole section 31, or it can increase first and then decrease. The diameter of the receiving hole section 32 after the diameter decreases is larger than the diameter of the main hole section 31.
[0127] The aperture of the main hole segment 31 is in the range of 2mm-4mm. If the aperture of the main hole segment 31 is less than 2mm, the laser will be misaligned and may burn the hole wall of the main hole segment 31. If the aperture of the main hole segment 31 is greater than 4mm, the filler metal wire will be wasted and more energy will be needed to melt the filler metal wire. In addition, due to the large volume, the molten filler metal is difficult to solidify evenly, which may easily lead to quality problems.
[0128] As an optional implementation, please refer to Figure 7 The step of depositing molten filler metal within the deposition well 30 and solidifying it to form the filler 40 includes:
[0129] S31, please refer to Figure 8 The filler wire 200 is inserted into the deposition hole 30 and is arranged coaxially with the deposition hole 30.
[0130] S32, a laser 300 with a spot 310 coinciding with the center of the deposition hole 30 is used to irradiate the filling metal wire 200, so that the filling metal wire 200 melts and fills the deposition hole 30 to form a filler 40.
[0131] The filler wire 200 can be ejected through a wire ejector (not shown). The coaxiality of the filler wire 200 with the deposition hole 30 ensures the precise positioning of the filler wire 200 within the deposition hole 30, allowing the laser energy 300 to be concentrated on the tip of the filler wire 200, thereby achieving precise control over the filling of molten metal. Laser irradiation can rapidly melt the filler wire 200, reducing the heat-affected zone and thus improving the quality and structural integrity of the filler 40. Furthermore, laser melting and filling can optimize the microstructure of the filler 40, thereby improving its mechanical properties and corrosion resistance.
[0132] As an optional implementation, please refer to Figure 9 The processing method of the composite metal frame 700 also includes:
[0133] S421, capture an image of the deposition well 30.
[0134] The deposition holes 30 can be imaged using a CCD camera to analyze their size, shape, and location, ensuring the accuracy of subsequent laser processing 300.
[0135] S422, determine the position of the light spot 310 on the image and the position of the center of the deposition hole 30.
[0136] Image processing technology can be used to determine the exact position of the laser spot 310 on the image. At the same time, it is also necessary to determine the position of the center of the deposition hole 30 so that the laser spot 310 can be accurately aligned with the center of the deposition hole 30.
[0137] S423, based on the fact that the positions of the light spot 310 and the center of the deposition hole 30 are within a preset error range, determine that the center of the light spot 310 coincides with the center of the deposition hole 30.
[0138] To ensure precise alignment of the laser 300 irradiation, the position of the laser 300 is adjusted by comparing the position of the laser spot 310 with the center position of the deposition hole 30, so that it coincides with the center of the deposition hole 30 or is within an acceptable error range. It can be understood that the preset error range defines the maximum allowable deviation when the laser spot 310 and the center of the deposition hole 30 are aligned. This deviation range needs to be set according to specific processing requirements and material properties. The preset error range can be ±0.05mm.
[0139] The above steps improve the precision and quality of the filling process, ensuring that the filler wire 200 melts accurately within the deposition hole 30 to form a uniform and dense filler body 40. By precisely controlling the position of the laser 300 irradiation, defects such as bubbles, incomplete filling, or over-melting during processing can be reduced, thereby improving the performance and reliability of the final product. Furthermore, this precise alignment technology can also improve production efficiency, reduce material waste, and potentially extend the service life of processing equipment.
[0140] As an optional implementation, please refer to Figure 10 Prior to the step of inserting the filling wire 200 into the deposition hole 30, the method further includes:
[0141] S411, please refer to Figure 11 The straightness of the filler wire 200 is adjusted using the wire straightening device 400.
[0142] S412, using detection device 500 (e.g.) Figure 13 (As shown) The straightness of the adjusted filler wire 200 was checked.
[0143] The function of the detection device 500 is to verify whether the filler wire 200 has reached the required straightness standard after adjustment. Through detection, it can be ensured that the quality of the filler wire 200 meets the processing requirements and avoid problems such as uneven filling, poor contact of hole walls or inaccurate laser irradiation caused by bending or twisting of the filler wire 200.
[0144] The above steps improve the precision and quality of the filling process, ensuring that the filler wire 200 melts accurately and fills the deposition holes 30. Ensuring the straightness of the filler wire 200 reduces potential defects during the filling process, such as bubbles, incomplete filling, or over-melting, thereby improving the performance and reliability of the final product. Furthermore, this control over the straightness of the filler wire 200 can improve production efficiency, reduce material waste, and potentially extend the lifespan of processing equipment. Precise control of the quality of the filler wire 200 ensures stability and consistency during laser processing, resulting in better filling effects.
[0145] As an optional implementation, please refer to Figure 11 and Figure 14 The wire straightening device 400 includes a rotating wheel assembly 410 and an adjusting assembly 420 arranged side by side. The rotating wheel assembly 410 includes n rotating wheels 411 spaced apart, and the adjusting assembly 420 includes (n-1) adjusting members 421 spaced apart. The n rotating wheels 411 and (n-1) adjusting members 421 are arranged alternately. The steps for adjusting the straightness of the filler metal wire 200 using the wire straightening device 400 specifically include:
[0146] S411A, causing the filler wire 200 to abut against n moving wheels 411, wherein the filler wire 200 includes a first end 210 and a second end 220 opposite to each other.
[0147] S411B, please refer to Figure 12 In the case of A, the adjustment member 421 corresponding to the first end 210 among the (n-1) adjustment members 421 moves toward the driving wheel assembly 410 and abuts against the first end 210, so that the second end 220 moves a first distance in the first direction (e.g., Figure 12 (As shown in B in the diagram).
[0148] S411C, causing another adjusting member 421 of the (n-1) adjusting members 421 to move toward the driving wheel assembly 410 and abut against the filler wire 200, so that the second end 220 moves a first distance in a second direction opposite to the first direction (e.g., ...). Figure 12 (As shown in C). The first direction is to the right, and the second direction is to the left.
[0149] S411D, please refer to Figure 12 D in the middle causes the remaining adjustment member 421 of the (n-1) adjustment members 421 to move toward the drive wheel assembly 410 and abut against the filler wire 200 to adjust the straightness of the filler wire 200.
[0150] Specifically, n is 4. There are two yarn-forming devices 400, which are spaced apart vertically. Please refer to [link to relevant documentation]. Figure 12The two wire straightening devices 400 can operate sequentially, and each wire straightening device 400 operates sequentially according to steps S411A-S411D to adjust the straightness of the filler metal wire 200.
[0151] In the above steps, by moving and slightly abutting the first adjusting member 421, force can be applied to the first end 210 of the filler wire 200, causing a slight displacement of its second end 220 in the first direction; by moving and slightly abutting the second adjusting member 421, the second end 220 of the filler wire 200 can be displaced in the second direction opposite to the first direction, to further adjust and correct the straightness of the filler wire 200; by moving and slightly abutting the remaining adjusting member 421, the filler wire 200 can be finely adjusted to ensure that the straightness of the entire filler wire 200 meets the requirements. Through the coordinated work of the moving wheel assembly 410 and the adjusting assembly 420, the filler wire 200 can be precisely adjusted to ensure its smooth delivery and accurate filling within the deposition hole 30. It is understood that during the operation of the second wire straightening device 400, the force on the filler wire 200 can be applied by the movement and slight resistance of the first adjusting member 421, causing its second end 220 to slightly shift in a third direction, which is perpendicular to the first direction; the movement and slight resistance of the second adjusting member 421 can cause the second end 220 of the filler wire 200 to shift in a fourth direction opposite to the third direction, so as to further adjust and correct the straightness of the filler wire 200; the movement and slight resistance of the remaining adjusting member 421 can be used to make fine adjustments to the filler wire 200.
[0152] As an optional implementation, please refer to Figure 13 and Figure 15 The detection device 500 includes a detection block 510, on which a detection hole 511 is provided. The step of using the detection device 500 to detect the straightness of the adjusted filler wire 200 includes:
[0153] S412A causes the filler wire to pass through the detection hole 511 of the detection block 510 more than 200 times.
[0154] S412B, based on the fact that the filler wire 200 does not contact the hole wall of the detection hole 511, confirms that the straightness of the filler wire 200 meets the standard.
[0155] Specifically, the filler wire 200 can pass through the detection hole 511 of the detection block 510 three times consecutively. The diameter of the detection hole 511 is 1.5mm-2mm. The length of the filler wire 200 can be 200mm.
[0156] In the above steps, the straightness is checked by passing the filler wire 200 through a test hole 511 with a specific size and shape. The design of the test hole 511 is usually to simulate certain characteristics of the actual deposition hole 30 or to provide a standardized test environment. If the filler wire 200 does not contact the hole wall when passing through the test hole 511, it indicates that the straightness of the filler wire 200 meets the requirements. That is, the filler wire 200 maintains good alignment during the passage without deviation or bending. This can be used to make a final confirmation of the straightness of the filler wire 200 and ensure that it can be accurately guided and positioned in the subsequent deposition process.
[0157] As an optional implementation, please refer to Figure 16 The laser is connected to the filler wire 200, meaning the laser and the filler wire 200 are bound together. After confirming that the straightness of the filler wire 200 meets the standard, the method further includes:
[0158] S401, please refer to Figure 17 Place test block 600 in the first position.
[0159] S402, please refer to the above as well. Figure 18 This causes the laser 601 to emit laser 300 toward the center of the test block 600.
[0160] The test block 600 has multiple concentric graduated circles 610 on its surface, with diameters of 1mm, 2mm, 3mm, 4mm, and 5mm respectively. By emitting a laser 300 toward the center of the test block 600, the alignment of the laser 601 with the deposition hole 30 during actual operation can be simulated.
[0161] S403, based on the fact that the laser spot 310 emitted by the laser 300 from the laser 601 is located at the center of the test block 600, the test block 600 is moved a second distance toward the laser 601 to a second position.
[0162] The second distance is 5mm.
[0163] S404, determine whether the spot 310 of the laser 300 emitted by the laser 601 is located at the center of the test block 600.
[0164] By reconfirming the position of the light spot 310, it can be ensured that the light spot 310 remains aligned with the center after the test block 600 is moved.
[0165] S405, based on the fact that the laser spot 310 emitted by the laser 300 is located at the center of the test block 600, the test block 600 is moved a second distance away from the laser 601 to the first position, and it is determined again whether the laser spot 310 emitted by the laser 300 is located at the center of the test block 600.
[0166] The stability and alignment accuracy of the laser 601 can be verified by repeating the alignment process.
[0167] S406, based on the fact that the laser spot 310 emitted by the laser 300 is once again located at the center of the test block 600, the filler wire 200 is moved toward the center of the test block 600, and it is determined whether the projection of the filler wire 200 on the test block 600 coincides with the center of the test block 600.
[0168] By checking the concentricity of the filler wire 200 and the light spot 310 through the projection of the filler wire 200, it can be ensured that the filler wire 200 is located at the center of the laser irradiation.
[0169] S407, based on the fact that the projection of the filler wire 200 on the test block 600 coincides with the center of the test block 600, it is determined that the spot 310 of the laser 300 emitted by the laser 601 is concentric with the filler wire 200.
[0170] By confirming the concentricity of the filler wire 200 and the light spot 310, it can be ensured that the laser energy 300 is effectively transferred to the filler wire 200.
[0171] As an optional implementation, please refer to Figure 19 The method further includes:
[0172] S408, based on the fact that the laser spot 310 of the laser 300 emitted by the laser 601 is concentric with the filling metal wire 200, the laser 601 emits the laser 300 toward the test metal plate (not shown), wherein the distance between the test metal plate and the laser 601 is equal to the distance between the bottom of the deposition hole 30 and the laser 601.
[0173] By using a test metal plate at the same distance from the deposition hole 30 to simulate actual processing conditions, it can be ensured that the positioning of the laser 601 and the quality of the spot 310 in actual operation are consistent with those under test conditions.
[0174] S409, the position of the laser 601 is deemed qualified based on the fact that the laser spot 310 emitted by the laser 300 towards the test metal plate by the laser 601 meets the standard.
[0175] If the position and quality of the laser spot 310 on the test metal plate meet the predetermined standards, it indicates that the position of the laser 601 is correct, which can ensure that the laser 601 can accurately irradiate the filler wire 200 and the deposition hole 30 during the actual deposition process. This step is the final confirmation of the laser 601 positioning, ensuring the accuracy and repeatability of the laser 300 processing process.
[0176] As an optional implementation, please refer to Figure 20 Based on the fact that the laser spot 310 emitted by laser 300 from laser 601 towards the test metal plate conforms to the standard, the steps to determine that the position of laser 601 is qualified include:
[0177] S4091A, please refer to Figure 21 The color of the laser spot 310 emitted by the laser 300 emitted by the laser 601 towards the test metal plate is detected.
[0178] S4092A, based on the color of the laser spot 310 emitted by the laser 300 emitted by the laser 601 towards the test metal plate, determine whether the laser spot 310 of the laser 300 emitted by the laser 601 towards the test metal plate meets the standard.
[0179] S4093A, the position of laser 601 is deemed qualified based on the fact that the laser spot 310 emitted by laser 300 towards the test metal plate by laser 601 meets the standard.
[0180] Among them, the color of the standard-compliant light spot 310 is in the orange-yellow range.
[0181] In the above steps, color detection is part of quality control to ensure the accuracy and consistency of the laser 300 processing and avoid processing defects; by detecting the color of the spot 310, it can be ensured that the laser 601 is accurately aligned with the filler metal wire 200.
[0182] As an optional implementation, please refer to Figure 22 Based on the fact that the laser spot 310 emitted by laser 300 from laser 601 towards the test metal plate conforms to the standard, the steps to determine that the position of laser 601 is qualified include:
[0183] S4091B, detects the shape of the spot 310 of the laser 300 emitted by the laser 601 towards the test metal plate.
[0184] S4092B, based on the shape of the laser spot 310 emitted by the laser 300 from the laser 601 toward the test metal plate, determines whether the laser spot 310 of the laser 300 emitted by the laser 601 toward the test metal plate conforms to the standard.
[0185] S4093B, the position of laser 601 is deemed qualified based on the fact that the laser spot 310 emitted by laser 300 towards the test metal plate by laser 601 meets the standard.
[0186] Among them, the standard light spot 310 has a ring-shaped structure and is evenly distributed.
[0187] In the above steps, shape detection is part of quality control to ensure the accuracy and consistency of the laser 300 processing process and avoid processing defects; by detecting the shape of the spot 310, it can be ensured that the laser 601 is accurately aligned with the filler wire 200.
[0188] As an optional implementation, please refer to Figure 23 The steps for determining the positional qualification of laser 601 based on the compliance of laser 300 emitted by laser 601 towards the test metal plate include:
[0189] S4091C, detects the size of the spot 310 of the laser 300 emitted by the laser 601 towards the test metal plate.
[0190] S4092C, based on the size of the laser spot 310 emitted by the laser 300 from the laser 601 toward the test metal plate, determines whether the laser spot 310 of the laser 300 emitted by the laser 601 toward the test metal plate conforms to the standard.
[0191] S4093C, the laser spot 310 of the laser 300 emitted by the laser 601 toward the test metal plate conforms to the standard, confirming that the position of the laser 601 is qualified.
[0192] The diameter of the standard light spot 310 is between 1 mm and 2 mm. During measurement, the inner and outer rings of the light spot 310 are measured and the average value is taken, and the measurement is performed at least three times.
[0193] In the above steps, dimensional inspection is part of quality control to ensure the accuracy and consistency of the laser 300 processing and avoid processing defects; by inspecting the size of the spot 310, it can be ensured that the laser 601 is accurately aligned with the filler wire 200.
[0194] Secondly, please see Figures 3 to 5This application discloses a composite metal frame 700, including a first metal layer 10 and a second metal layer 20 stacked together. The composite metal frame 700 also includes a deposition hole 30, which is formed from the surface of the first metal layer 10 toward the second metal layer 20. The deposition hole 30 includes a main hole segment 31 and a receiving hole segment 32 connected to each other. The main hole segment 31 is located on one side of the first metal layer 10, and the receiving hole segment 32 is at least partially received in the second metal layer 20. The diameter of the at least partially receiving hole segment 32 is larger than the diameter of the main hole segment 31. A filler 40 is tightly attached to the inner wall of the deposition hole 30. The filler 40 and the second metal layer 20 corresponding to the filler 40 are provided with a mounting hole 41, and the second metal layer 20 and the filler 40 are exposed on the inner wall of the mounting hole 41.
[0195] The material of the first metal layer 10 includes an aluminum alloy, the material of the second metal layer 20 includes titanium or a titanium alloy, and the material of the filler 40 includes titanium.
[0196] Thirdly, this application discloses an electronic device including the aforementioned composite metal frame 700. The electronic device may be, but is not limited to, a mobile phone, tablet computer, laptop computer, smartwatch, monitor, etc.
[0197] It will be apparent to those skilled in the art that this application is not limited to the details of the exemplary embodiments described above, and that this application can be implemented in other specific forms without departing from the spirit or essential characteristics of this application. Therefore, the embodiments should be regarded as exemplary and non-limiting in all respects, and the scope of this application is defined by the appended claims rather than the foregoing description. Thus, all variations falling within the meaning and scope of equivalents of the claims are intended to be embraced within this application.
[0198] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application and are not intended to limit it. Although this application has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of this application without departing from the spirit and scope of the technical solutions of this application.
Claims
1. A method of processing a composite metal frame, characterized by, include: A metal composite substrate is provided, the metal composite substrate comprising a first metal layer and a second metal layer stacked together; A deposition hole is formed from the surface of the first metal layer into the interior of the metal composite substrate. The deposition hole includes a main hole segment and a receiving hole segment connected to each other. The main hole segment is located on one side of the first metal layer, and the receiving hole segment is at least partially received into the second metal layer. The diameter of at least a portion of the receiving hole segment is larger than the diameter of the main hole segment. The step of forming the deposition hole from the surface of the first metal layer into the interior of the metal composite substrate includes: using a first tool to drill a hole in the first metal layer into the second metal layer to form the main hole segment; using a second tool to drill a hole from the bottom of the main hole segment into the second metal layer to form the receiving hole segment, the receiving hole segment extending into the second metal layer; and the diameter of the receiving hole segment increases from the end connected to the main hole segment towards the end away from the main hole segment. The process involves depositing molten filler metal within the deposition hole and solidifying it to form a filler body. The step of depositing molten filler metal within the deposition hole and solidifying it to form a filler body includes: inserting a filler metal wire into the deposition hole and coaxially aligning the filler metal wire with the deposition hole; irradiating the filler metal wire with a laser beam whose spot coincides with the center of the deposition hole, causing the filler metal wire to melt and fill the deposition hole to form the filler body; the processing method further includes: capturing an image of the deposition hole; determining the position of the laser spot on the image and the position of the center of the deposition hole; and, based on the fact that the position of the laser spot and the position of the center of the deposition hole are within a preset error range, determining that the laser spot coincides with the center of the deposition hole; so that the filler body fits tightly against the inner wall of the main hole segment. A portion of the filler and the second metal layer corresponding to the filler are removed to form a mounting hole, wherein the second metal layer and the filler are exposed from the inner wall of the mounting hole.
2. The method of claim 1, wherein the composite metal bezel is made of a material selected from the group consisting of aluminum, stainless steel, and titanium. Prior to the step of inserting the filling wire into the deposition hole, the method further includes: The straightness of the filler wire is adjusted using a wire straightening device; The straightness of the adjusted filler wire is tested using a testing device.
3. The method of claim 2, wherein the composite metal bezel is formed by a process comprising: The wire straightening device includes a rotating wheel assembly and an adjusting assembly arranged side by side. The rotating wheel assembly includes n rotating wheels spaced apart, and the adjusting assembly includes n-1 adjusting members spaced apart. The n rotating wheels and n-1 adjusting members are arranged alternately. The step of adjusting the straightness of the filler wire using the wire straightening device includes: The filler wire is brought into contact with n of the moving wheels, wherein the filler wire includes opposing first and second ends; The adjustment member corresponding to the first end among the n-1 adjustment members is moved toward the driving wheel assembly and abuts against the first end, so that the second end moves a first distance in a first direction; One of the n-1 adjusting members is moved toward the drive wheel assembly and abuts against the filler wire, so that the second end moves the first distance in a second direction opposite to the first direction; The remaining adjustment member out of the n-1 adjustment members is moved toward the drive wheel assembly and abuts against the filler wire to adjust the straightness of the filler wire.
4. The method of claim 2, wherein the composite metal bezel is formed by a process comprising: The detection device includes a detection block with a detection hole. The step of using the detection device to detect the straightness of the adjusted filler wire includes: The filling metal wire is passed through the detection hole of the detection block multiple times; Based on the fact that the filler wire does not contact the wall of the detection hole, it is confirmed that the straightness of the filler wire meets the standard.
5. The method of claim 4, wherein the composite metal bezel is formed by a process comprising: The laser is connected to the filler wire, and after confirming that the straightness of the filler wire meets the standard, the method further includes: Place the test block in the first position; The laser is directed to emit a laser beam toward the center of the test block; Based on the fact that the laser spot emitted by the laser is located at the center of the test block, the test block is moved a second distance toward the laser to a second position; Determine whether the laser spot emitted by the laser is located at the center of the test block; Based on the fact that the laser spot emitted by the laser is located at the center of the test block, the test block is moved away from the laser by the second distance to the first position, and it is determined again whether the laser spot emitted by the laser is located at the center of the test block; Based on the fact that the laser spot emitted by the laser is once again located at the center of the test block, the filler wire is moved toward the center of the test block, and it is determined whether the projection of the filler wire on the test block coincides with the center of the test block; Based on the fact that the projection of the filler wire on the test block coincides with the center of the test block, it is determined that the laser spot emitted by the laser is concentric with the filler wire.
6. The processing method of the composite metal frame as described in claim 5, characterized in that, The method further includes: Based on the fact that the laser spot emitted by the laser is concentric with the filling metal wire, the laser is directed towards the test metal plate, wherein the distance between the test metal plate and the laser is equal to the distance between the bottom of the deposition hole and the laser. The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
7. The processing method of the composite metal frame as described in claim 6, characterized in that, The step of determining that the laser's position is qualified based on the laser spot emitted by the laser towards the test metal plate conforming to the standard includes: Detect the color of the laser spot emitted by the laser towards the test metal plate; Based on the color of the laser spot emitted by the laser towards the test metal plate, determine whether the laser spot emitted by the laser towards the test metal plate meets the standard; The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
8. The processing method of the composite metal frame as described in claim 6, characterized in that, The step of determining that the laser's position is qualified based on the laser spot emitted by the laser towards the test metal plate conforming to the standard includes: Detect the shape of the laser spot emitted by the laser towards the test metal plate; Based on the shape of the laser spot emitted by the laser towards the test metal plate, determine whether the laser spot emitted by the laser towards the test metal plate meets the standard; The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
9. The processing method of the composite metal frame as described in claim 6, characterized in that, The step of determining the position of the laser to be qualified based on the compliance criteria of the laser emitted by the laser toward the test metal plate includes: The size of the laser spot emitted by the laser towards the test metal plate is detected; Based on the size of the laser spot emitted by the laser towards the test metal plate, determine whether the laser spot emitted by the laser towards the test metal plate meets the standard; The laser beam emitted by the laser towards the test metal plate conforms to the standard, thus confirming that the laser's position is qualified.
10. A composite metal frame, characterized in that, The composite metal frame includes a first metal layer and a second metal layer stacked together. The composite metal frame also includes deposition holes formed from the surface of the first metal layer into the interior of the metal composite substrate. Each deposition hole includes a main hole segment and a receiving hole segment connected to each other. The main hole segment is located on one side of the first metal layer, and the receiving hole segment is at least partially received within the second metal layer. The diameter of at least a portion of the receiving hole segment is larger than the diameter of the main hole segment. A filler is tightly fitted to the inner wall of the deposition hole. An installation hole is formed by removing a portion of the filler and the second metal layer corresponding to the filler. The second metal layer and the filler are exposed on the inner wall of the installation hole.
11. The composite metal frame as described in claim 10, characterized in that, The material of the first metal layer includes an aluminum alloy, the material of the second metal layer includes titanium or a titanium alloy, and the material of the filler includes titanium.
12. An electronic device, characterized in that, Includes the composite metal frame as described in claim 10.
Citation Information
Patent Citations
Bonding structure and bonding method
CN114269505A
Aluminium alloy laser welding wire-feeding mechanism
CN1775450A
Soldering joint comprising a plurality of overlapping metal sheets, with a spacer located between an upper metal sheet and a lower metal sheet