A method for preparing iridescent silk textured fabric
By using a blending and dyeing process of fine denier extra-long vinylon fiber and ordinary fine cotton fiber, the problem of monotonous colors in batik fabrics has been solved, resulting in rich textures and color effects, improving the quality and aesthetics of the fabric, and simplifying the production process.
Patent Information
- Application Number
- CN202410574141.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-10
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-05-10
AI Technical Summary
Existing batik fabrics have monotonous yarn colors, a rough style, and poor fineness, making it difficult to achieve the effect of hair-like ice wax texture.
It uses a blend of fine denier extra-long vinylon fiber and ordinary fine cotton fiber. Through combing, spinning, weaving and dyeing processes, the difference in dye absorption and dyeing efficiency of the fibers is controlled to form a texture effect with varying shades of similar colors, simulating the randomness, imperfection and disorder of hair wax texture.
It achieves rich textures and colors in fabrics, improves yarn strength and elasticity, simplifies the printing and dyeing process, reduces energy consumption, and produces iridescent silk texture fabrics with rich visual appeal.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of fabric technology, and in particular relates to a method for preparing iridescent silk texture fabric. Background Technology
[0002] Wax patterns are the soul of batik (wax printing) fabrics. Hair-like ice wax patterns have characteristics such as randomness, beauty of imperfection, beauty of disorder and texture, and are colorful.
[0003] Most existing batik fabric yarns are ordinary white greige fabric yarns, which are processed by spinning first and then printing and dyeing. The colors are monotonous, the style is rough, and the fineness is poor. The hairline wax texture has always been a technical pain point that has been difficult to solve in the existing batik (wax printing) production. Summary of the Invention
[0004] The purpose of this invention is to provide a method for preparing iridescent silk textured fabric, aiming to solve the problems mentioned in the background art.
[0005] The present invention is implemented as follows: a method for preparing iridescent silk textured fabric includes the following steps:
[0006] (1) Fine denier extra-long vinylon fiber and untreated ordinary fine cotton raw cotton fiber are mixed and combed to obtain yarn;
[0007] (2) The yarn is woven into fabric to obtain greige fabric;
[0008] (3) The raw fabric is dyed and printed to obtain iridescent silk texture fabric.
[0009] Preferably, in step (1), the length of the fine denier extra-long vinylon fiber is 51 mm, and the length of the fine cotton fiber is 23-33 mm.
[0010] Preferably, in step (1), the fine denier extra-long vinylon fiber accounts for 1-2% of the fine denier extra-long vinylon fiber and the untreated ordinary lint cotton raw cotton fiber.
[0011] Preferably, in step (1), the combed spinning specifically includes: first, mixing the two raw materials into cotton, then opening and cleaning the cotton, then combing the cotton, then preparing for combing, combing, drawing roving, spinning, winding, and finally packaging.
[0012] Preferably, the pre-combing preparation includes pre-drawing sliver, sliver winding, sliver winding, sliver winding, and sliver winding.
[0013] Preferably, in step (2), the weaving process specifically includes: warping the yarn according to the fabric specifications, then sizing, threading the reed, weaving, finishing, inspection and repair, and finally packaging.
[0014] Preferably, in step (3), the dyeing and printing production specifically includes: first, turning the greige fabric over and sewing it, then performing singeing, descaling and bleaching, mercerizing, semi-bleaching, stretching and rolling, then dyeing or ordinary printing or wax-resistant printing or real wax printing, then steaming, soaping, stretching and sizing finishing, calendering or not calendering, and finally finished product inspection and packaging.
[0015] This invention provides a method for preparing iridescent textured fabric, utilizing vinylon fiber, whose properties are similar to cotton and is known as "synthetic cotton." It is the most absorbent of the existing synthetic fibers. The vinylon fiber specifications used are 1.56 Dtex × 51 mm. During printing and dyeing, it simulates the texture of hair wax. Hair wax texture is formed after dyeing through the fine cracks in the resist agent (rosin or paraffin). This invention simulates the characteristics of hair wax texture, such as randomness, beauty of imperfection, beauty of disorder, and beauty of texture. The principle is that during printing and dyeing, the different dye absorption and dyeing efficiencies of fibers with different properties produce the effect of different shades and light colors of similar colors, revealing different textures. The collision of fibers of different shades creates a subtle iridescent effect.
[0016] This invention innovates the traditional method of achieving a uniform color on cotton textiles through dyeing and printing processes after spinning and weaving. Instead, it involves incorporating vinylon fibers into the textile, which, after spinning and weaving, undergoes dyeing and printing processes to achieve similar colors and textures with varying shades. During printing, different patterns and colors bond with the vinylon fibers to form a new vinylon fiber color, resulting in richer color layers on the fabric.
[0017] In the spinning process, extra-long fine denier vinylon fibers are blended with regular fine cotton. The fine cotton is 23-33mm long, while the vinylon fiber is 51mm. Vinylon fibers are significantly longer than regular fine cotton fibers, making them easier to spin and weave during processing. This improves yarn strength, elasticity, pilling resistance, and durability. Regular fine cotton is blended with 1-2% vinylon fibers for a thorough and precise mix. After weaving, this blend is applied to dyeing and printing, resulting in a natural, irregular texture with similar colors but varying shades. The waxy finish is finer, showcasing the dynamic beauty of the extra-long fibers. The colors are rich, exhibiting a random yet stable quality, creating a unique, unpredictable effect. The wax texture is characterized by its uncertainty and its ability to mimic the natural texture of hair wax. It has an abstract quality and its formation process has a unique and accidental beauty. The resulting texture is more uniform and free-flowing. The texture is generated during dyeing and printing. The amount of wax texture produced can be controlled by the depth of dyeing, the printing and dyeing process, the coverage area, and the size of the pattern. This results in a richer and more dynamic texture. Compared to traditional production and dyeing processes, it is simpler and can achieve textures of varying depths and multiple color layers with accurate and disordered control. Different layers create a richer visual aesthetic. The direction of the wax texture can be controlled more accurately, both horizontally and vertically, and the density and shape of the texture can be controlled.
[0018] The spinning process controls the thickness of the fibers by combing them out of their disorder. During the dyeing process, the occasional disorder that creates fine lines and cloud-like patterns adds to the aesthetic appeal. Through dyeing and printing, the different depths of the wax patterns are accurately controlled, creating a distinctive style of batik (wax printing) and mechanically produced batik (wax printing), with clearer and more delicate lines. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention.
[0020] The specific implementation of the present invention will be described in detail below with reference to specific embodiments.
[0021] Example 1
[0022] A method for preparing an iridescent silk textured fabric includes the following steps:
[0023] (1) Mix fine denier extra-long vinylon fiber and untreated ordinary fine cotton raw cotton fiber, and comb and spin yarn to obtain yarn. The process sequence is: blending two raw materials → opening and cleaning cotton (multi-component intelligent fine blending and opening cotton unit) → carding → pre-combing preparation (pre-drawing, sliver lap, sliver lap, drawing lap, sliver drawing lap) → combing → drawing (2-3 times) roving → spinning → winding → packaging completed;
[0024] Among them, two raw materials are used to blend cotton: vinylon fiber is mixed with untreated fine cotton fiber at a ratio of 1-2%;
[0025] Opening and cleaning: In the cotton opening and cleaning stage, the cotton is opened to reduce impurities, breakage, and fiber damage, and to prevent cotton knots as much as possible. A multi-component intelligent fine blending and opening unit is used. This production unit mainly includes a weighing feeder, a fine opening machine, and a weighing device. The multi-component intelligent fine blending and opening unit ensures thorough and precise mixing in multiple compartments, producing a uniform cotton lap for the next carding process. Carding: Using a flat or roller type, the small cotton bundles and clumps are further broken down into single fibers by the movement of the needle surface. Impurities and non-spinnable short fibers are further removed, and the fibers are straightened parallel to form a sliver, which is then coiled into a sliver can. Pre-drawing: The pre-drawing process determines the straightness of the fibers, and the yarn sliver is fed into the pre-drawn sliver. Front hook fibers are numerous, accounting for about 50% of the total fiber count. If these front hooks are not effectively straightened in the pre-drawing process, it will not only increase the damage to the front hooks by the combing cylinder, but may even cause a small number of front hook fibers to be directly caught by the combing cylinder. Mixing with waste cotton will affect the quality indicators of yarn, such as evenness, strength, and hairiness; Sliver lap: arranging carded slivers or pre-drawn slivers in parallel to form a sliver lap; Bundling: combining several sliver laps into one sliver lap; Combing: removing impurities and short, coarse fibers from the fiber by using a machine with carding needles on its surface to alternately comb the two ends of the fiber bundle, removing unacceptable short fibers, improving fiber length uniformity, separating tangled fibers into single strands, and removing impurities and fiber granules mixed in the raw material. The spinning process greatly improves the spinnability of raw materials, resulting in yarns that are even, smooth, and significantly stronger. The woven fabrics have clear textures, fewer streaks, and a clean surface. Roving: The sliver is evenly stretched and thinned to further straighten and parallel the fibers and twist them, producing rovings of different counts and twists, which is beneficial for the next spinning process. Spinning: The final step in the spinning process, spinning the roving into fine yarn with a certain count and meeting quality standards, for use in twisted, woven, or knitted yarns.
[0026] Spinning and winding: On a winding machine, fine yarn from bobbins is processed into larger-capacity, well-formed packaged yarns that meet certain requirements, facilitating subsequent processes. The winding process also checks the yarn diameter (thickness and thinness), removes foreign fibers, trifilaments, defects, and impurities to ensure yarn quality. Impurities and larger defects are removed and sheared, followed by quality inspection using a tension device and an electronic yarn clearer. During the yarn inspection stage, the electronic clearer can be partially switched off or adjusted, and photoelectric electronic yarn clearers can be used. When producing on an automatic winding machine, the yarn clearing parameters should be set according to the yarn defect situation or distribution to ensure normal air splicing and knotting, and to eliminate harmful defects such as coarse and fine foreign fibers to the greatest extent. Adjust the foreign fiber function to ensure that the fabric surface is uniform and free of obvious yarn defects. Turn off or adjust the automatic foreign fiber removal device to prevent accidental removal of vinylon fibers, thereby reducing yarn loss, increasing yarn yield, reducing losses, reducing production energy consumption, improving production efficiency, and obtaining iridescent silk texture creative yarn, which is indistinguishable from other ordinary yarns in appearance.
[0027] (2) Weaving and fabric making: the process sequence is as follows: warping the yarn according to the fabric specifications → sizing the yarn → threading the reed → weaving the process → finishing, inspecting and repairing → packaging the greige fabric to obtain the iridescent silk pattern creative batik (wax printing) greige fabric.
[0028] Among them, yarn warping: the obtained batik (wax printing) iridescent silk texture yarn is wound into several warp beams according to the fabric specification head number of the total number of warp yarns required for the whole fabric. The yarn is grouped and warped and wound on the warp beams to prepare for the next process of sizing.
[0029] Sizing: In order to improve the weavability of the yarn, enhance its smoothness and abrasion resistance, and at the same time increase the abrasion resistance of the warp yarn, the warp beams are placed on the sizing machine, the yarn is sizing, and then dried in an oven and separated to complete the sizing process.
[0030] Threading the reed: On the warp beam after sizing, each warp yarn is threaded into the heddle and reed in a certain order according to the fabric specifications and process requirements. Stop warp pieces are inserted on the warp yarns to form a shed during weaving, which facilitates the introduction of weft yarns to weave the required fabric.
[0031] Weaving: The warp beams, with the reeds already threaded, are placed on the loom. The weft yarns (selected from wax-dyed (wax-printed) hairline textured yarns, iridescent textured yarns, or regular grey yarns) are guided in the weft direction to interweave two different styles of grey fabric according to process requirements. The fabric is then wound up in the fabric draw-out area of the loom to the specified length before being laid out.
[0032] Finishing and Inspection: Inspect the warp and weft density of the greige fabric, and repair weaving and yarn defects according to standards;
[0033] Fabric packaging completed: Fold neatly according to the folding requirements (measured in yards or meters), and piece together each piece of fabric into a bundle according to the standard length of each piece.
[0034] (3) The printing and dyeing production process is as follows: fabric turning → singeing → descaling and bleaching (combined machine) → mercerizing → semi-bleaching (natural white) stretching and rolling → dyeing or ordinary printing or wax resist printing or real wax printing → steaming → soaping → stretching and sizing → calendering / non-calendering → finished product inspection → packaging completed.
[0035] Among them, the fabric turning and sewing: the edges of the fabric seam are aligned, and the flat sewing machine sews the fabric flat, straight and strong to ensure continuous production in subsequent processes;
[0036] Singeing: Singeing with two positive and two negative flames at a speed of 100-120m / min, extinguishing the fire with alkali and dropping the fabric, alkali concentration of 15-20 g / L, and stacking for 8-10 hours. The singeing quality reaches grade 4-5, burning off the fuzz on the surface of the fabric, making the fabric surface smooth and beautiful, and preventing uneven dyeing and printing and printing defects caused by the presence of fuzz during dyeing and printing. It also improves the gloss of the fabric surface, increases the smoothness, and improves the anti-pilling and anti-fuzzing properties.
[0037] Desizing, scouring, and bleaching: This includes desizing, scouring, and bleaching processes. During weaving, the warp yarns are sizingd, and the raw cotton fibers themselves contain a lot of natural impurities such as oils, waxes, and pectin. Natural fibers tend to be yellowish, and there are also stains and impurities from the production process. Desizing improves the fabric's penetration ability, allowing for better dye absorption during bleaching, dyeing, and printing, increasing whiteness for brighter colors, a smoother surface, uniform color, and good colorfastness. The desizing process (caustic soda: 15-20 g / L, penetrant: 2 g / L, detergent: 2 g / L) 0.5 g / L, steaming time: 65 minutes, temperature: 98-100℃), boiling process (caustic soda: 30 g / L, penetrant: 1.5 g / L, boiling agent: 3-5 g / L, steaming time: 65 minutes, temperature: 98-100℃, rolling mill pressure average pressure: 0.2 MPa, speed: 80-90 m / min), bleaching process (hydrogen peroxide: 5 g / L, stabilizer PAM-3: 6 g / L, steaming time: 70 minutes, temperature: 98-100℃);
[0038] Mercerizing: During the processing, cotton products are treated with a concentrated caustic soda solution under tension, and then the caustic soda is washed away under tension. After mercerizing, the surface of the cotton products has a silk-like luster, which enhances the penetration and adsorption capacity and ensures the dimensional stability of the fabric. The caustic soda concentration in the front trough heavy calender is 220-230 g / L, and the caustic soda concentration in the back trough heavy calender is 240-250 g / L. The caustic soda is washed under tension using fabric clamps or straight rollers, and multiple suction sprays of diluted caustic soda are used to ensure sufficient mercerizing. The products are then thoroughly washed with hot and cold water in multiple steamers, and finally washed with room temperature water in the last compartment. Glacial acetic acid is added to adjust the pH value to 5-8.
[0039] Semi-bleached (natural white) stretching and rolling: Automatic weft straightening machine before entering the drying room to straighten weft skew and weft bend; width: expand the width according to requirements; drying room temperature: 150-160℃; machine speed: 60-70 m / min; press with water or penetrating agent; press pressure: 0.2MPa; strictly control temperature, machine speed and moisture content to ensure stable and neat width; automatic width expansion and edge trimming equipment rolls up and drops the fabric.
[0040] Dyeing, regular printing, wax resist printing, or wax printing:
[0041] Dyeing: Through dyeing with medium and sensitive colors, the dyed fabric surface exhibits different effects due to the different absorption and dyeing rates of fibers with different properties under the same one-bath dyeing process. This results in similar but different colors. The color depth and lightness of vinylon fibers show different effects, highlighting the texture of vinylon fibers. The collision of different shades of fibers creates a subtle and iridescent effect. Through the fine and long color layers of vinylon fibers, a colorful fabric surface effect is achieved.
[0042] Ordinary printing, anti-wax printing, or real wax printing: Patterns are randomly printed onto the fabric surface. The patterns partially cover the vinylon fibers, resulting in varying dye uptake rates. This creates different effects due to the different absorption rates of the fibers, producing similar colors across the fibers. The subtle differences in color depth and hue between the vinylon fibers highlight their texture. The interplay of different shades creates a subtle, iridescent effect, enriching the color layers of the print. It simulates the waxy texture of hair, with fine cracks formed after dyeing, mimicking the randomness, imperfections, disorder, and texture of hair wax. This results in unique, disordered dyeing of fibers, producing more vibrant and colorful hues. It particularly showcases the natural, irregular texture, finer wax patterns, and the dynamic beauty of ultra-long fibers. The colors are rich, random, and of stable quality, with a unique randomness and uncertainty, creating a three-dimensional effect and mimicking the texture of hair wax. The natural texture of wax patterns has an abstract quality, and the formation process has a unique aesthetic appeal due to its accidental nature. The texture displayed on yarn and fabric is more uniform. The effect of wax patterns can be controlled by adjusting the coverage area and the size of the pattern during printing. The depth of color can reveal a richer and more dynamic texture, which is richer in color than traditional production. It is possible to produce textures of varying depths in a single print. Multiple color layers can be accurately and randomly controlled, creating a richer and more unique visual aesthetic. The direction of the wax pattern can be more accurately controlled, and the density and shape of the horizontal and vertical (radial and weft) textures can be controlled. By imitating the cracked wax pattern, the density and shape of the texture can be controlled through the printing pattern. The fineness of the mixed fibers can be controlled by combing them out during the spinning process. The fine lines and cloud-like patterns of varying depths caused by the accidental randomness of printing and dyeing further enhance the aesthetic appeal. By dyeing and printing different color positions, the depth of the wax pattern can be accurately controlled, with unique color combinations and arrangements.
[0043] Steaming: After printing or secondary printing, to ensure better bonding between the dye and cotton fibers, improve color fastness under certain temperature, pressure and humidity conditions. Temperature: 100-105℃, time: 8-10 minutes.
[0044] Soap washing: to improve its color fastness and brightness, remove the unfixed and floating dyes on its surface with detergent, anti-staining solution, etc., and clean it in a multi-stage high-efficiency steam washing box;
[0045] Stirring and sizing finishing: Using a rolling mill, water, sizing or functional additives are added to the padding tank for finishing. In the drying room, a heat source is provided for drying. Mechanical tension is applied to the fabric clamp to complete the finishing. The fabric dimensions are stable and it has certain fabric functions through padding.
[0046] Calendering / Non-calendering: Conventional calendering mills are vertical three-roll calendering mills. By changing the steel rolls, calendering (flat surface), embossing, and production of different patterns and varieties can be achieved. Different varieties and styles can be produced by adjusting the machine pressure, temperature, etc.
[0047] Finished product inspection: Inspection is conducted on fabric weaving defects, dyeing defects, and printing defects;
[0048] Packaging complete: The inspected finished fabrics are rolled up or folded neatly according to the folding requirements (measured in yards or meters), and pieced together into fabric bags according to the standard length of each piece of fabric.
[0049] The dyeing process in this embodiment of the invention eliminates four production steps in the traditional production process: waxing → wax washing → wax drying → wax dyeing and waxing again → wax washing → wax drying → wax re-dyeing. This greatly reduces energy consumption and improves production efficiency. The process in this embodiment of the invention is energy-saving and reduces consumption of steam, water resources and electricity, promoting green and sustainable development and obtaining iridescent silk pattern batik (wax printing) fabric.
[0050] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A method of making a iridescent silk fabric, characterized in that, Includes the following steps: (1) Fine denier extra-long vinylon fiber and untreated ordinary fine cotton raw cotton fiber are mixed and combed to obtain yarn; (2) The yarn is woven into fabric to obtain greige fabric; (3) The greige fabric is printed and dyed to obtain iridescent silk texture fabric; In step (1), the length of the fine denier extra-long vinylon fiber is 51mm, and the length of the fine cotton fiber is 23-33mm; In step (1), the fine denier extra-long vinylon fiber accounts for 1-2% of both the fine denier extra-long vinylon fiber and the untreated ordinary lint cotton fiber; In step (3), the dyeing and printing production specifically includes: first, turning the greige fabric over and sewing it, then performing singeing, descaling and bleaching, mercerizing, semi-bleaching, stretching and rolling, then dyeing or ordinary printing or wax-resistant printing or real wax printing, then steaming, soaping, stretching and sizing finishing, calendering or not calendering, and finally finished product inspection and packaging. Dyeing: Through dyeing with medium and sensitive colors, the dyed fabric surface exhibits the same dyeing process in a one-bath dyeing process. However, due to the different dye absorption and dyeing rates of fibers with different properties, the colors are similar but not identical, simulating the natural texture of hair ice wax pattern. Regular printing, anti-wax printing, or real wax printing: The pattern is randomly printed on the fabric surface, covering some of the fine denier extra-long vinylon fibers. Due to the different dyeing rates of the fibers, the covered areas of the printed pattern are formed. The different dyeing rates of the fibers with different properties produce different effects, resulting in similar but different colors, simulating the natural texture of hair ice wax.
2. The method of making an iridescent silk fabric according to claim 1, wherein, In step (1), the combed spinning specifically includes: first, mixing the two raw materials into cotton, then opening and cleaning the cotton, then combing the cotton, then preparing for combing, combing, drawing roving, spinning, winding, and finally packaging.
3. The method of claim 2, wherein the iridescent silk fabric is prepared by the steps of: The preparations before combing include pre-combing, sliver winding, sliver winding and winding, and sliver winding and winding.
4. The method of claim 1, wherein the iridescent silk fabric is prepared by the steps of: In step (2), the weaving process specifically includes: warping the yarn according to the fabric specifications, then sizing, threading the reed, weaving, finishing, inspection and repair, and finally packaging.
Citation Information
Patent Citations
Method for dyeing cotton-polyester blended weft-knitted fabric heather grey
CN109235080A