Power semiconductor modules and their packaging methods
By using flip-chip design and bonding wire-free packaging methods, the problem of bonding wire breakage and detachment in traditional power semiconductor modules has been solved, achieving high reliability and high yield power semiconductor module packaging, and improving heat dissipation and electrical performance.
Patent Information
- Application Number
- CN202611359829.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-03
- Publication Date
- 2026-11-10
AI Technical Summary
In traditional power semiconductor modules, bonding wires are prone to breakage or detachment at high temperatures, leading to module failure. Existing technical solutions suffer from problems such as insufficient connection strength, poor layout flexibility, complex processes, or high costs.
By adopting a flip-chip design, the bonding wire connection is eliminated. The electrical connection between the semiconductor chip and the substrate is achieved through a sintered connection layer or a solder connection layer. The electrodes on the back side are connected by metal connectors, and the connection between the tin-antimony solder and the heat dissipation substrate is combined to optimize electrical and heat dissipation performance.
It significantly improves the reliability and aging performance of the module, reduces manufacturing costs, simplifies the process, increases production yield, avoids the risk of bond wire failure, and optimizes electrical and heat dissipation performance.
Smart Images

Figure CN123076288A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor technology. Specifically, this invention relates to a power semiconductor module and its packaging method. Background Technology
[0002] In traditional power semiconductor module packaging processes, electrical connections are typically achieved on the chip surface using bonding wires (such as aluminum wires), such as... Figure 6 As shown. However, due to limitations in the material of the bonding wires themselves, the ultrasonic bonding principle, and equipment stability, the bonding wires become a critical failure point during the high-temperature operation of the module. According to statistics, in long-term aging tests of power semiconductor modules, the failure rate caused by bonding wire breakage or detachment exceeds 50%.
[0003] With advancements in silicon carbide chip technology, its operating junction temperature has increased from 150℃ to 175℃, leading to a dramatic increase in heat generation. The inconsistency in the thermal expansion coefficients of the chip and bonding wire materials causes enormous thermal stress at the junction under high temperatures. When this stress exceeds the connection strength, it triggers the bonding wire to break or detach, ultimately causing module failure.
[0004] To address this issue, existing technologies have proposed several solutions. For example, Chinese patent application number 202223066475.X discloses a copper strip bonding structure, which improves connection strength, but the chip is subjected to significant stress during the copper strip bonding process, posing a risk of internal dark cracks. Furthermore, it lacks layout flexibility and requires additional DTS (Distributed Trace Module) processes, increasing costs. Chinese patent application number 202211496029.4 discloses a clip copper strip connection scheme, which avoids DTS processes, but its drive signal terminals still use bonding wires, failing to completely eliminate the risk of bonding wire failure. Chinese patent application number 202210037750.0 discloses a double-sided flip-chip packaging structure, which eliminates bonding wires, but the process is complex, yield is low, and double-sided heat dissipation complicates the cooling system, making it unsuitable for mainstream automotive single-sided water-cooling systems.
[0005] This invention provides a power semiconductor module and its packaging method, particularly concerning how to eliminate bonding wire connections, prevent bonding wire failure risks, and improve heat dissipation performance and production yield. Summary of the Invention
[0006] This invention aims to at least solve one of the technical problems existing in the prior art. To this end, this invention provides a power semiconductor module that, through a flip-chip design, completely eliminates bonding wire connections, eliminates the risk of bonding wire failure, and improves heat dissipation performance and production yield.
[0007] To achieve the above objectives, the technical solution adopted by the present invention is: a power semiconductor module, comprising: Liner; A semiconductor chip has a first main surface and a second main surface opposite to each other. The first main surface is provided with a first electrode and a second electrode, and the second main surface is provided with a third electrode. The metal connector is electrically connected to the third electrode on the second main surface of the semiconductor chip through the second connection layer; The semiconductor chip is disposed with its first main surface facing the substrate and is electrically connected to the substrate through a first connecting layer, which is located between the first main surface of the semiconductor chip and the substrate.
[0008] The first electrode is the source, the second electrode is the gate, the third electrode is the drain, and the semiconductor chip is a silicon carbide chip.
[0009] The first connecting layer is a sintered connecting layer or a welded connecting layer; the material of the sintered connecting layer contains silver; the material of the welded connecting layer contains high-lead solder.
[0010] The material of the second bonding layer includes solder or sintering material.
[0011] The metal connector has a plate-like structure, and the orthographic projection of the metal connector on the semiconductor chip covers the third electrode.
[0012] The power semiconductor module further includes a heat dissipation substrate, the liner is disposed on the heat dissipation substrate and connected to the heat dissipation substrate through a third connection layer; The material of the third connecting layer includes tin-antimony solder.
[0013] The present invention also provides a packaging method for a power semiconductor module, comprising the following steps: A substrate and a semiconductor chip are provided, the semiconductor chip having a first main surface and a second main surface opposite to each other, the first main surface being provided with a first electrode and a second electrode, and the second main surface being provided with a third electrode; The semiconductor chip is arranged with its first main surface facing the substrate, and a first connection layer is formed between the first main surface and the substrate to achieve electrical connection between the semiconductor chip and the substrate. A metal connector is provided, which is aligned with the third electrode on the second main surface of the semiconductor chip, and a second connection layer is formed between the metal connector and the third electrode to achieve electrical connection between the metal connector and the semiconductor chip.
[0014] The step of forming the first connection layer includes: A sintered material is provided on the liner; The first main surface of the semiconductor chip is attached to the sintering material; The sintering material is sintered to form the first connecting layer.
[0015] The step of forming the second connection layer includes: Solder is applied to the second main surface of the semiconductor chip and / or the metal connector; The metal connector is attached to the second main surface; Reflow soldering is performed to form the second bonding layer; After the step of forming the second connecting layer, the method further includes: providing a heat dissipation substrate; disposing the liner on the heat dissipation substrate and forming a third connecting layer to connect the liner and the heat dissipation substrate; wherein the temperature during the formation of the third connecting layer is lower than the melting point of the second connecting layer.
[0016] After the step of forming the first connection layer and before the step of forming the second connection layer, the method further includes: Provide heat dissipation substrate; The liner is disposed on the heat dissipation substrate, and a third connecting layer is formed to connect the liner and the heat dissipation substrate; The temperature during the formation of the second connecting layer is lower than the melting point of the third connecting layer.
[0017] The power semiconductor module of this invention, by flip-chip bonding of the semiconductor chip, allows the first and second electrodes to be directly connected to the substrate via a first interconnect layer. Simultaneously, a metal connector connects the third electrode on the back side, completely eliminating the bonding wires required in traditional processes. This eliminates the risk of failure due to broken or detached bonding wires, significantly improving module reliability and aging performance, as well as heat dissipation and production yield. Furthermore, the design of the metal connectors is more flexible, no longer limited by the bonding wire layout, which facilitates optimized electrical performance.
[0018] The power semiconductor module packaging method of the present invention simplifies the process flow, eliminates the bonding process, reduces manufacturing costs, and improves yield. Attached Figure Description
[0019] This manual includes the following figures, which illustrate the following: Figure 1 A top view of a power semiconductor module provided in an embodiment of the present invention; Figure 2 A perspective view of a power semiconductor module provided in an embodiment of the present invention; Figure 3 This is a schematic diagram of the surface layout of a semiconductor chip provided in an embodiment of the present invention; Figure 4 A schematic flowchart of the power semiconductor module packaging route 1 provided in an embodiment of the present invention; Figure 5 A schematic flowchart of the power semiconductor module packaging route 2 provided in an embodiment of the present invention; Figure 6 This is a schematic diagram of the bonding structure of a traditional power semiconductor module; Figure 7 This is a schematic diagram of bond wire breakage failure; Figure 8 This is a schematic diagram illustrating bond wire detachment failure. The markings in the diagram are as follows: 101-First metal lead-out terminal; 102-Second metal lead-out terminal; 103-Third metal lead-out terminal; 104-Fourth metal lead-out terminal; 105-Fifth metal lead-out terminal; 106-Sixth metal lead-out terminal; 107-Seventh metal lead-out terminal; 108-Eighth metal lead-out terminal; 109-Ninth metal lead-out terminal; 110-Tenth metal lead-out terminal; 201-Heat dissipation substrate; 202-Backing plate; 301-Semiconductor chip; 302-First electrode; 303-Second electrode; 401-First metal connector; 402-Second metal connector. Detailed Implementation
[0020] The specific embodiments of the present invention will be further described in detail below with reference to the accompanying drawings, in order to help those skilled in the art to have a more complete, accurate and in-depth understanding of the concept and technical solutions of the present invention, and to facilitate its implementation.
[0021] It should be noted that in the following embodiments, the terms "first," "second," and "third" do not represent an absolute distinction in structure and / or function, nor do they represent the order of execution; they are merely for the convenience of description.
[0022] Firstly, such as Figures 1 to 3 As shown, an embodiment of the present invention provides a power semiconductor module, including: Liner 202; Semiconductor chip 301 has a first main surface and a second main surface opposite to each other. The first main surface is provided with a first electrode 302 and a second electrode 303, and the second main surface is provided with a third electrode. The metal connector is electrically connected to the third electrode on the second main surface of the semiconductor chip 301 through the second connection layer; The semiconductor chip 301 is disposed with its first main surface facing the substrate 202 and is electrically connected to the substrate 202 through a first connecting layer, which is located between the first main surface of the semiconductor chip 301 and the substrate 202.
[0023] Specifically, in this embodiment of the invention, in response to the problem that bonding wires in traditional power semiconductor modules are prone to breakage or detachment during high-temperature operation, leading to module failure, this embodiment of the invention provides a power semiconductor module that completely eliminates bonding wires from the structure through a flip-chip design, thereby fundamentally eliminating the risk of bonding wire failure.
[0024] In this embodiment of the invention, the semiconductor chip 301 has two surfaces, namely a first main surface (front) and a second main surface (back). The first and second main surfaces are the two end surfaces of the semiconductor chip 301 in the thickness direction, and are parallel to each other. The semiconductor chip 301 is flip-chip mounted with the first main surface facing the substrate 202. A first electrode 302 and a second electrode 303 are disposed on the first main surface, and a third electrode is disposed on the second main surface. The first electrode 302 is specifically the source electrode, the second electrode 303 is specifically the gate electrode, and the third electrode is specifically the drain electrode. The semiconductor chip 301 is a silicon carbide chip. Since the operating junction temperature of silicon carbide chips is typically as high as 175°C or even higher, the heat generation is extremely large, and traditional bonding wire connection methods are prone to failure under such severe thermal stress conditions. In this invention, a flip-chip design is adopted, with the first main surface of the chip directly facing the substrate 202, laying the structural foundation for subsequent electrical connection through a large-area interconnect layer.
[0025] The SiC chip is fixed to the upper surface of the substrate 202 with its front side (S and G poles) facing down and its back side (D pole) facing up via a metal connector, thus eliminating the need for bonding wires. Compared to traditional bonding processes, this effectively improves the aging performance of the module, avoids the common aging failure mode of bonding wire detachment, and also improves the overall process yield of the module by eliminating the bonding process.
[0026] The silicon carbide chip is flip-chip mounted onto the surface of the substrate 202, thereby achieving electrical connection between the chip's gate (G) and source (S) terminals and the substrate 202. The drain (D) terminal on the back of the silicon carbide chip is connected to the power terminal via a metal connector. The silicon carbide chip and substrate 202 can be fixed by silver sintering or by high-temperature soldering, while the chip and metal connectors are soldered by low-temperature soldering. Both sides of the entire silicon carbide chip are fixed to other components by large-area solder / sintering layers, further avoiding stress concentration and thus achieving high reliability and aging performance.
[0027] A first connection layer is disposed between the semiconductor chip 301 and the substrate 202. Since the semiconductor chip 301 is flip-chip mounted, the first connection layer is located between the first main surface of the semiconductor chip 301 and the substrate 202. The first connection layer not only serves a mechanical fixing function, but more importantly, it enables electrical conduction between the first electrode 302 and the second electrode 303 of the semiconductor chip 301 and the corresponding circuits on the substrate 202. In this embodiment of the invention, the first connection layer is a sintered connection layer or a soldered connection layer; the material of the sintered connection layer includes silver. The silver sintering process has extremely high connection reliability, and the thermal resistance of silver material is extremely low, approximately 20% of that of traditional brazing solder, which is crucial for improving the heat dissipation efficiency of high-power modules.
[0028] Of course, depending on different cost and process requirements, the first connecting layer can also be a welded connecting layer. The material can be high-temperature solder such as high-lead solder, with a liquidus temperature close to 300°C, good wettability, and low void rate after welding.
[0029] In this embodiment of the invention, the metal connector has a plate-like structure, and the orthographic projection of the metal connector on the semiconductor chip 301 covers the third electrode. Two metal connectors are provided, namely a first metal connector 401 and a second metal connector 402, and multiple first metal connectors 401 and second metal connectors 402 are provided. The first metal connectors 401 and 402 are electrically connected to the third electrode on the second main surface of the semiconductor chip 301 through a second connection layer. The first metal connectors 401 and 402 serve as power terminal leads and current busbars. The first metal connectors 401 and 402 are single straight-line structures, specifically clip copper busbars, which are simple to prepare and allow for precise mounting and positioning. Compared with traditional thin bonding wires, the plate-like metal connector can carry a larger current. The orthographic projection of the first metal connectors 401 and 402 on the semiconductor chip 301 covers the third electrode, which can improve the module's current carrying capacity and heat dissipation performance. The material of the second connection layer includes solder or sintering material.
[0030] like Figure 1 and Figure 2 As shown, the power semiconductor module of this embodiment further includes a heat dissipation substrate 201, and a substrate 202 is disposed on the heat dissipation substrate 201 and connected to the heat dissipation substrate 201 through a third connection layer. The substrate 202 is typically a ceramic substrate with a specific circuit pattern on its surface. The heat dissipation substrate 201 provides support and heat dissipation channels for the module.
[0031] In this embodiment of the invention, the material of the third connecting layer includes tin-antimony solder. Tin-antimony solder has excellent creep resistance and a relatively moderate melting point, making it suitable for large-area welding of the backing plate 202 and the substrate. To further reduce the void ratio of the solder layer, the welding process can employ a formic acid vacuum welding process. By controlling key parameters such as welding temperature, time, vacuum value, and formic acid injection amount, it can be ensured that heat can be efficiently conducted to the heat dissipation substrate 201.
[0032] The power semiconductor module of this embodiment further includes a molding compound that encapsulates at least a portion of the semiconductor chip 301, the substrate 202, and the metal connectors. The molding compound is made of epoxy resin and formed using a transfer molding process, providing insulation, moisture protection, and mechanical protection for the internal components.
[0033] The power semiconductor module of this invention, through the above-described structural design, achieves bond-free connections between the semiconductor chip 301 and the substrate 202, and between the semiconductor chip 301 and the metal connector. This structure not only eliminates the main failure mode of bond wire breakage, significantly improving the power cycle life of the module, but also optimizes electrical performance through the design of the plate-shaped metal connector.
[0034] Secondly, embodiments of the present invention also provide a packaging method for a power semiconductor module, comprising the following steps: S1: A substrate 202 and a semiconductor chip 301 are provided. The semiconductor chip 301 has a first main surface and a second main surface opposite to each other. A first electrode 302 and a second electrode 303 are provided on the first main surface, and a third electrode is provided on the second main surface. S2: The semiconductor chip 301 is arranged with its first main surface facing the substrate 202, and a first connection layer is formed between the first main surface and the substrate 202 to realize the electrical connection between the semiconductor chip 301 and the substrate 202. S3: Provide a metal connector, align the metal connector with the third electrode on the second main surface of the semiconductor chip 301, and form a second connection layer between the metal connector and the third electrode to achieve electrical connection between the metal connector and the semiconductor chip 301.
[0035] In step S2 above, forming the first connection layer specifically includes the following steps: S201: Set sintering material, such as silver paste or silver film, on the liner 202; S202: Mount the first main surface of the semiconductor chip 301 onto the sintering material; S203: The sintering material is sintered to form the first bonding layer.
[0036] Because the area of the second electrode 303 (gate) of the semiconductor chip 301 is small, for example only 0.8mm × 0.8mm, the sintering temperature, pressure, and time must be strictly controlled during the sintering process to prevent sintered material from overflowing to the surrounding area and avoiding the risk of short circuit breakdown of the chip. The silver sintering process is a solid-state diffusion process; the silver material does not melt and flow like solder, so the risk of overflow is relatively low. However, strict control of mounting accuracy and pressure uniformity is still necessary. Sintering is usually carried out in a sintering furnace, requiring control of the protective atmosphere (such as nitrogen or syngas) and application of pressure at peak temperature to ensure densification.
[0037] In step S3 above, a first metal connector 401 and a second metal connector 402 are provided, the first metal connector 401 and the second metal connector 402 are aligned with the third electrode on the second main surface of the semiconductor chip 301, and a second connection layer is formed between the first metal connector 401 and the second metal connector 402 and the third electrode to realize the electrical connection between the first metal connector 401 and the second metal connector 402 and the semiconductor chip 301.
[0038] In step S3 above, forming the second connection layer specifically includes the following steps: S301: Apply solder to the second main surface of the semiconductor chip 301 and / or the metal connector; S302: Attach the metal connector to the second main surface; S303: Perform reflow soldering to form a second bonding layer.
[0039] Specifically, solder, such as solder paste, is first applied to the second main surface of the semiconductor chip 301, or to the first metal connector 401 and the second metal connector 402. Then, the first metal connector 401 and the second metal connector 402 are mounted onto the second main surface; finally, reflow soldering is performed to form the second bonding layer. The reflow soldering process requires precise control of the temperature profile to ensure that the solder completely melts and wets the solder interface, while simultaneously reducing the void ratio of the solder layer through methods such as vacuum pressure holding.
[0040] like Figure 4 As shown, in a specific embodiment of the present invention, the packaging method of the power semiconductor module further includes the following steps: S4: Provide a heat dissipation substrate 201; place a liner 202 on the heat dissipation substrate 201 and form a third connecting layer to connect the liner 202 and the heat dissipation substrate 201; wherein the temperature during the formation of the third connecting layer is lower than the melting point of the second connecting layer.
[0041] like Figure 4As shown, the first process route provided by this embodiment of the invention is as follows: after the step of forming the second connecting layer, the backing plate 202 is then connected to the heat dissipation substrate 201. In this process route, since the formation of the third connecting layer is after the formation of the second connecting layer, the temperature during the formation of the third connecting layer must be lower than the melting point of the second connecting layer. For example, if the second connecting layer uses high-lead solder, the third connecting layer can use tin-antimony solder or SAC305 solder with a lower melting point. This can prevent the already formed Clip solder layer from remelting during the substrate soldering process, thereby ensuring structural stability.
[0042] like Figure 5 As shown, in another specific embodiment of the present invention, after the step of forming the first interconnect layer and before the step of forming the second interconnect layer, the packaging method of the power semiconductor module further includes the following steps: S21: Provides a heat dissipation substrate 201; A liner 202 is disposed on a heat dissipation substrate 201, and a third connecting layer is formed to connect the liner 202 and the heat dissipation substrate 201.
[0043] The temperature during the formation of the second connecting layer is lower than the melting point of the third connecting layer.
[0044] like Figure 5 As shown, the second process route provided in this embodiment of the invention is as follows: After providing the heat dissipation substrate 201, a substrate 202 with a semiconductor chip 301 sintered on it is disposed on the heat dissipation substrate 201, and a third connection layer is formed to connect the substrate 202 and the heat dissipation substrate 201. A tin-antimony solder with a high melting point can be used in this process. Finally, a metal connector welding process is performed, i.e., a second connection layer is formed, connecting the first metal connector 401 and the second metal connector 402 to the back of the chip.
[0045] In this process flow, since the substrate is soldered first and the metal connectors are soldered later, the temperature during the formation of the second interconnect layer must be lower than the melting point of the third interconnect layer. For example, if tin-antimony solder is used for the third interconnect layer, then a solder with a lower melting point, such as SAC305 solder, must be used for the second interconnect layer. This sequential arrangement effectively avoids the use of lead-containing solder, meets the industry's lead-free requirements, and also prevents the substrate solder from remelting in subsequent processes.
[0046] In conjunction with yield control in actual manufacturing processes, substrate 202 testing is performed after soldering. The packaging method of this embodiment also includes a substrate 202 testing step. After chip sintering, electrical testing can be performed to check the condition of the front-end electrical connections. Since the bonding wires are eliminated, failure modes such as dark cracks, cracking, and chipping that may occur during the bonding process in traditional technologies are avoided, which helps improve yield. Simultaneously, the substrate 202 testing here serves as a preventative check, preventing the failure of the entire full-bridge module due to the failure of one half-bridge.
[0047] The present invention has been described above by way of example with reference to the accompanying drawings. Obviously, the specific implementation of the present invention is not limited to the above-described manner. Any non-substantial improvements made using the inventive concept and technical solution; or the direct application of the inventive concept and technical solution to other situations without modification, are all within the protection scope of the present invention.
Claims
1. A power semiconductor module, characterized in that, include: Liner plate (202); A semiconductor chip (301) has a first main surface and a second main surface opposite to each other. The first main surface is provided with a first electrode and a second electrode, and the second main surface is provided with a third electrode. The metal connector is electrically connected to the third electrode on the second main surface of the semiconductor chip (301) through the second connection layer; The semiconductor chip (301) is disposed with its first main surface facing the substrate (202) and is electrically connected to the substrate (202) through a first connecting layer, which is located between the first main surface of the semiconductor chip (301) and the substrate (202).
2. The power semiconductor module according to claim 1, characterized in that, The first electrode is the source, the second electrode is the gate, the third electrode is the drain, and the semiconductor chip (301) is a silicon carbide chip.
3. The power semiconductor module according to claim 1, characterized in that, The first connecting layer is a sintered connecting layer or a welded connecting layer; the material of the sintered connecting layer contains silver; the material of the welded connecting layer contains high-lead solder.
4. The power semiconductor module according to claim 1, characterized in that, The material of the second bonding layer includes solder or sintering material.
5. The power semiconductor module according to claim 1, characterized in that, The metal connector has a plate-like structure, and the orthographic projection of the metal connector on the semiconductor chip (301) covers the third electrode.
6. The power semiconductor module according to claim 1, characterized in that, It also includes a heat dissipation substrate (201), wherein the liner (202) is disposed on the heat dissipation substrate (201) and connected to the heat dissipation substrate (201) through a third connecting layer; The material of the third connecting layer includes tin-antimony solder.
7. A packaging method for a power semiconductor module, characterized in that, Includes the following steps: A substrate (202) and a semiconductor chip (301) are provided. The semiconductor chip (301) has a first main surface and a second main surface opposite to each other. The first main surface is provided with a first electrode and a second electrode, and the second main surface is provided with a third electrode. The semiconductor chip (301) is arranged with its first main surface facing the substrate (202), and a first connection layer is formed between the first main surface and the substrate (202) to achieve electrical connection between the semiconductor chip (301) and the substrate (202); A metal connector is provided, which is aligned with the third electrode on the second main surface of the semiconductor chip (301), and a second connection layer is formed between the metal connector and the third electrode to achieve electrical connection between the metal connector and the semiconductor chip (301).
8. The packaging method according to claim 7, characterized in that, The step of forming the first connection layer includes: Sintered material is provided on the liner (202); The first main surface of the semiconductor chip (301) is attached to the sintering material; The sintering material is sintered to form the first connecting layer.
9. The packaging method according to claim 7, characterized in that, The step of forming the second connection layer includes: Solder is applied to the second main surface of the semiconductor chip (301) and / or the metal connector; The metal connector is attached to the second main surface; Reflow soldering is performed to form the second bonding layer; After the step of forming the second connecting layer, the method further includes: providing a heat dissipation substrate (201); disposing the liner (202) on the heat dissipation substrate (201) and forming a third connecting layer to connect the liner (202) and the heat dissipation substrate (201); wherein the temperature during the formation of the third connecting layer is lower than the melting point of the second connecting layer.
10. The packaging method according to claim 7, characterized in that, After the step of forming the first connection layer and before the step of forming the second connection layer, the method further includes: A heat dissipation substrate (201) is provided. The liner (202) is disposed on the heat dissipation substrate (201) and a third connecting layer is formed to connect the liner (202) and the heat dissipation substrate (201). The temperature during the formation of the second connecting layer is lower than the melting point of the third connecting layer.
Citation Information
Patent Citations
Double-sided flip packaging structure of wide bandgap power module suitable for high-temperature environment
CN114400220A
Power module packaging structure with stacked wiring
CN116913910B