A type of mold for machining crossbeams of Al-Zn-Mg-Cu aluminum profile seats.

By designing a machining mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams, and utilizing a sliding and extrusion structure to achieve multi-process machining, the problems of machining accuracy and adaptability of aluminum profile seat crossbeams were solved, and machining efficiency and accuracy were improved.

CN123102838APending Publication Date: 2026-11-17ANHUI XINBO ALUMINUM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611328341.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-31
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies struggle to efficiently process the mounting holes and side extensions of Al-Zn-Mg-Cu aluminum profile seat beams, especially when ensuring processing accuracy and adapting to the raised structure of the base plate.

Method used

A crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams was designed, comprising an upper mold base, a lower mold base, an upper contact part, a side forming part, and an extrusion column. Multi-process processing is achieved through sliding and extrusion, and support blocks and guide components are combined to enhance positioning and accuracy.

Benefits of technology

This technology enables multi-stage one-time processing of aluminum profiles, improving processing accuracy and efficiency, ensuring the adaptability of mounting holes and side extensions in forming, and enhancing processing adaptability and accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102838A_ABST
    Figure CN123102838A_ABST
Patent Text Reader

Abstract

This invention relates to the field of automotive parts processing equipment technology, and discloses a crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams, including an upper mold base and a lower mold base. The lower mold base has a lower die for placing the aluminum profile, and the upper mold base has an upper abutment mounted on it via a first elastic element. The upper mold base also has a punching element. A side forming element for extending the side of the aluminum profile is mounted on the upper mold base via a second elastic element, and an extrusion column is mounted on the side forming element. The lower die, upper abutment, and side forming element form a structure for limiting the aluminum profile. During the punching process, as the upper mold base moves downward, the side forming element and the lower die perform initial extrusion of the side extension of the aluminum profile. Then, by applying a downward force to the extrusion column, the side forming element and the lower die complete the shaping of the side extension of the aluminum profile. This invention can realize the processing of holes and side extensions in aluminum profiles, increasing processing efficiency and accuracy.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of automotive parts processing equipment technology, and in particular to a crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams. Background Technology

[0002] 7-series super-hard aluminum alloys (Al-Zn-Mg-Cu) are renowned for their exceptional strength, especially 7075 aluminum alloy. After extrusion and T6 treatment, its tensile strength can reach 572 MPa, and its yield strength 503 MPa. These figures even surpass many ordinary structural steels, while its density is only 2.8 g / cm³, achieving true lightness and strength. 7-series aluminum alloys are mainly used in aerospace vehicle frames, high-performance bicycle frames, tennis rackets, and other fields with extreme requirements for strength-to-weight ratio.

[0003] The seat crossbeam is mounted on the car floor, and the seat crossbeam often has mounting holes machined on it, which are usually made by stamping. In order to ensure that the extension of the aluminum profile of the seat crossbeam has a large contact area with the floor, additional technology is often required to shape the extensions on both sides of the crossbeam to adapt to the structure of the base with protrusions. Summary of the Invention

[0004] To address the technical problems existing in the background art, the present invention proposes a crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams.

[0005] The present invention proposes a crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam, including an upper mold base and a lower mold base. The lower mold base has a lower mold for placing aluminum profiles. An upper abutment is installed on the upper mold base through a first elastic element. The upper mold base is provided with a punched part, which can slide relative to the upper abutment in the vertical direction.

[0006] The upper die base is provided with a side forming part for extending and forming the side of the aluminum profile via a second elastic element. An extrusion column is also installed on the side forming part, and the extrusion column extends out of the upper die base. The lower die, the upper abutment, and the side forming part form a forming for extending the side of the aluminum profile.

[0007] During the process of the upper die moving downward to complete the punching process of the punched part, the side forming part and the lower die complete the initial extrusion of the side extension of the aluminum profile; then, by applying a downward force to the extrusion column, the side forming part and the lower die complete the forming of the side extension of the aluminum profile.

[0008] As a further optimization of the present invention, the lower die base is also provided with a support block, which is disposed in the through hole of the aluminum profile for support. The support block has a limit hole, and the punching part can slide in the limit hole.

[0009] As a further optimization of the present invention, there is a gap between the support block and the aluminum profile during the punching process of the punched part, and when the side forming part moves to the bottom, the support block contacts the top surface inside the aluminum profile.

[0010] To facilitate waste removal, as a further optimization of the present invention, the support block is provided with a material guiding channel, which is connected to the limiting hole.

[0011] As a further optimization of the present invention, the inner wall of the through hole of the aluminum profile has a side support, the support block has a portion that contacts the bottom surface of the side support, the side support is provided with an auxiliary support, and there is a positioning structure between the auxiliary support and the support block. The positioning structure consists of a groove formed on the support block and a positioning strip provided on the auxiliary support that cooperates with the groove.

[0012] As a further optimization of the present invention, the first elastic element is provided in at least two sets, and the at least two sets of the first elastic elements are distributed on the upper surface of the upper contact element.

[0013] To further increase processing accuracy, as a further optimization of the present invention, the side forming part contacts the side of the aluminum profile.

[0014] As a further optimization of the present invention, at least two sets of extrusion columns are provided, and at least two sets of extrusion columns are distributed along the length direction of the side forming part.

[0015] As a further optimization of the present invention, an extrusion block is also provided, and at least two sets of extrusion columns are connected to the extrusion block. A sliding groove is opened on the upper mold base, and the extrusion block is vertically slidably installed on the extrusion block.

[0016] To further increase machining accuracy, as a further optimization of the present invention, at least two sets of guide components are provided between the upper mold base and the lower mold base. Each guide component includes a guide post and a guide cylinder. The guide cylinder is mounted on the lower mold base, and the guide post is mounted on the upper mold base. During mold closing or opening, the guide post slides vertically within the guide cylinder.

[0017] In this invention, the proposed Al-Zn-Mg-Cu aluminum profile seat crossbeam processing mold achieves the limitation of the aluminum profile during the punching process through the setting of the upper contact part and the side forming part. After punching is completed by the setting of the side forming part and the extrusion column, the extrusion column drives the side forming part downward to form the protruding part of the side extension of the aluminum profile. Multiple processing steps can be achieved by placing the material once. The side forming part completes the limitation of the aluminum profile during the stamping process. Furthermore, the setting of the support block facilitates punching and the re-shaping of the punched part during the side forming process of the aluminum profile, further increasing the processing accuracy.

[0018] Additional aspects and advantages of the invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description

[0019] Figure 1 This is a schematic diagram of the structure of the present invention;

[0020] Figure 2 This is a cross-sectional view of the present invention;

[0021] Figure 3 This is a cross-sectional view of the present invention from another angle;

[0022] Figure 4 This is a schematic diagram of the filling component structure of the present invention;

[0023] Figure 5 This is a schematic diagram of the seat crossbeam structure processed according to the present invention;

[0024] In the diagram: 1. Upper die base; 2. Lower die base; 3. Lower die; 4. Aluminum profile; 40. Through hole; 41. Side extension; 42. Side support; 5. Upper contact part; 6. First elastic element; 7. Second elastic element; 8. Side forming part; 9. Punched part; 10. Support block; 100. Limiting hole; 101. Material guide channel; 11. Guide assembly; 12. Auxiliary support; 13. Extrusion column; 14. Extrusion block. Detailed Implementation

[0025] Embodiments of the present invention are described in detail below. Examples of these embodiments are illustrated in the accompanying drawings, wherein the same or similar symbols denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and should not be construed as limiting the present invention.

[0026] like Figure 1-4The above describes a crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam, which includes an upper mold base 1 and a lower mold base 2. The upper mold base 1 has a lower mold 3 for placing aluminum profile 4. The lower mold 3 is fixed to the lower mold base 2 by a fixing member. An upper abutment 5 is installed on the upper mold base 1 by a first elastic member 6. The upper mold base 1 is provided with a punch 9, which can slide relative to the upper abutment 5 in the vertical direction.

[0027] The upper mold base 1 is provided with a side forming part 8 for forming the side extension 41 of the aluminum profile 4 via a second elastic member 7. An extrusion column 13 is also installed on the side forming part 8, extending out of the upper mold base 1. The lower mold 3, the upper abutment 5, and the side forming part 8 form a structure for limiting the aluminum profile 4. There are two sets of the side forming part 8 and the second elastic member 7. One set of the side forming part 8 cooperates with one set of the second elastic member 7. The two sets of side forming parts 8 are located on both sides of the upper abutment 5 and are used to process the side extension 41 on both sides of the aluminum profile 4. It should be noted that the first elastic member 6 and the second elastic member 7 can be mold springs. There are at least two sets of both the first elastic member 6 and the second elastic member 7. At least two sets of the first elastic member 6 are distributed on the upper surface of the upper abutment 5, and at least two sets of the second elastic member 7 are distributed on the upper surface of the side forming part 8. It should also be noted that, in order to limit its displacement, the upper mold base 1 has holes for accommodating part of the first elastic member 6 and the second elastic member 7.

[0028] During the punching process, the upper die holder 1 moves downward to make the punched part complete the punching process. The side forming part 8 and the lower die 3 complete the initial extrusion of the side extension 41 of the aluminum profile 4. Then, by applying a downward force to the extrusion column 13, the side forming part 8 and the lower die 3 complete the forming of the side extension 41 of the aluminum profile 4.

[0029] During processing, the aluminum profile 4 is first placed in the lower receiving groove on the lower die 3 to initially limit the lower part of the aluminum profile 4. Then, the external stamping equipment drives the upper die base 1 to move downward. During the downward movement of the upper die base 1, the upper contact member 5 contacts the uppermost surface of the aluminum profile 4, and the side forming member 8 contacts the side extension 41 of the aluminum profile 4. Then, the first elastic member 6 and the second elastic member 7 are pressed to limit the aluminum profile 4. Then, the punching member 9 completes the punching. After punching, the external stamping equipment drives the extrusion column 13 to move the side forming member 8 downward to complete the forming of the side of the aluminum profile 4 so that it adapts to the raised structure of the base plate. It should be noted that the lower die 3 has a structure that cooperates with the side forming to form the protrusion and groove on the side extension 41. After processing, the part is as follows: Figure 5 As shown.

[0030] To further increase processing accuracy, preferably, the side forming part 8 contacts the side surface of the aluminum profile 4. During the punching and side extension 41 processing of the aluminum profile 4, the side surface of the side forming part 8 contacts the outer surface of the aluminum profile 4 to limit the movement of the aluminum profile 4.

[0031] To further improve processing accuracy, preferably, a support block 10 is also provided on the lower die base 2. The support block 10 is slidably installed on the lower die base 2 and is located in the through hole 40 of the aluminum profile 4 for support. A limit hole 100 is opened on the support block 10, and the punching part 9 can slide within the limit hole 100. This completes the support of the aluminum profile 4 during the processing. During the punching process of the punching part 9, there is a gap between the support block 10 and the aluminum profile 4. When the side forming part 8 moves to the bottom, the support block 10 contacts the top surface inside the aluminum profile 4.

[0032] The support block 10 is used to support the through hole 40 inside the aluminum profile 4. During the punching process, there is a gap between the support block 10 and the inner top surface of the through hole 40. As the side forming part 8 moves downward, the upper abutment 5 and the upper mold base 1 move downward accordingly. After the side forming part 8 is formed, the upper abutment 5 and the support block 10 abut against the aluminum profile 4. During the forming process of the side extension 41, the punching part 9 is located inside the hole, which facilitates the punching process and shapes the punched part, increasing processing accuracy and efficiency.

[0033] To facilitate the removal of waste, preferably, the support block 10 has a guide channel 101, which is connected to the limiting hole 100. The guide channel 101 is set along the length of the support block 10. The support block 10 provides support for the side of the through hole 40 and prevents the punching waste from contacting the aluminum profile 4 and the lower die base 2.

[0034] To further increase processing accuracy, preferably, some aluminum profiles 4 have side supports 42 on the inner wall of the through holes 40. The support block 10 has a portion that contacts the bottom surface of the side support 42. The side support 42 is provided with an auxiliary support 12. There is a positioning structure between the auxiliary support 12 and the support block 10. This positioning structure consists of a groove formed on the support block 10 and a positioning strip provided on the auxiliary support 12 that cooperates with the groove. During the installation process, the aluminum profile 4 is first placed on the lower mold 3, and at this time, the inner wall of the through hole 40 of the aluminum profile 4 is in contact with the side wall of the support block 10.

[0035] Preferably, at least two sets of extrusion columns 13 are provided, and at least two sets of extrusion columns 13 are distributed along the length direction of the side forming part 8.

[0036] Preferably, an extrusion block 14 is also provided, and at least two sets of extrusion columns 13 are connected to the extrusion block 14. A sliding groove is opened on the upper mold base 1, and the extrusion block 14 is vertically slidably installed on the extrusion block 14.

[0037] To further increase machining accuracy, preferably, at least two sets of guide components 11 are provided between the upper mold base 1 and the lower mold base 2. Each guide component 11 includes a guide post and a guide cylinder. The guide cylinder is mounted on the lower mold base 2, and the guide post is mounted on the upper mold base 1. During mold closing or opening, the guide post slides vertically within the guide cylinder. It should be noted that those skilled in the art can also use other existing guide components 11 with different structures.

[0038] It should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," and "circumferential" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the present invention.

[0039] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.

[0040] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection, an electrical connection, or a connection that allows communication between the components; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components, unless otherwise explicitly limited. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.

[0041] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can mean that the first feature is in direct contact with the second feature, or that the first feature is in indirect contact with the second feature through an intermediate medium. Furthermore, "above," "over," and "on top" of the second feature can mean that the first feature is directly above or diagonally above the second feature, or simply that the first feature is at a higher horizontal level than the second feature.

[0042] The above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any equivalent substitutions or modifications made by those skilled in the art within the scope of the technology disclosed in the present invention, based on the technical solution and inventive concept of the present invention, should be covered within the scope of protection of the present invention.

Claims

1. A crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam, comprising an upper mold base (1) and a lower mold base (2), wherein the lower mold base (2) has a lower mold (3) for placing aluminum profile (4), characterized in that, An upper abutment (5) is mounted on the upper mold base (1) via a first elastic element (6), and a punch (9) is provided on the upper mold base (1). The punch (9) can slide relative to the upper abutment (5) in the vertical direction. The upper die base (1) is provided with a side forming part (8) for forming the side extension (41) of the aluminum profile (4) via a second elastic member (7). An extrusion column (13) is also installed on the side forming part (8), and the extrusion column (13) extends out of the upper die base (1). The lower die (3), the upper abutment (5), and the side forming part (8) together form a side extension (41) for forming the aluminum profile (4). During the process of the upper die holder (1) moving downward to make the punched part (9) complete the punching process, the side forming part (8) and the lower die (3) complete the initial extrusion of the side extension (41) of the aluminum profile (4); then, by applying a downward force to the extrusion column (13), the side forming part (8) and the lower die (3) complete the forming of the side extension (41) of the aluminum profile (4).

2. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams according to claim 1, characterized in that, The lower die base (2) is also provided with a support block (10), which is provided in the through hole (40) of the aluminum profile (4) for support. The support block (10) has a limit hole (100) and the punching part (9) can slide in the limit hole (100).

3. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams according to claim 2, characterized in that, During the punching process of the punched part (9), there is a gap between the support block (10) and the aluminum profile (4). When the side forming part (8) moves to the bottom, the support block (10) contacts the top surface inside the aluminum profile (4).

4. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam according to claim 2, characterized in that, The support block (10) has a material guiding channel (101) which is connected to the limiting hole (100).

5. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams according to claim 2, characterized in that, The inner wall of the through hole (40) of the aluminum profile (4) has a side support (42). The support block (10) has a part that contacts the bottom surface of the side support (42). An auxiliary support (12) is provided on the side support (42). There is a positioning structure between the auxiliary support (12) and the support block (10). The positioning structure is a groove opened on the support block (10) and a positioning strip provided on the auxiliary support (12) that cooperates with the groove.

6. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeams according to claim 1, characterized in that, The first elastic element (6) is provided in at least two sets, and at least two sets of the first elastic element (6) are distributed on the upper surface of the upper contact element (5).

7. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam according to claim 1, characterized in that, The side molding (8) is in contact with the side of the aluminum profile (4).

8. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam according to claim 1, characterized in that, At least two sets of the extrusion columns (13) are provided, and at least two sets of the extrusion columns (13) are distributed along the length direction of the side forming part (8).

9. The crossbeam processing mold for Al-Zn-Mg-Cu aluminum profile seat crossbeam according to claim 1, characterized in that, An extrusion block (14) is also provided, and at least two sets of extrusion columns (13) are connected to the extrusion block (14). A sliding groove is opened on the upper mold base (1), and the extrusion block (14) is vertically slidably installed on the extrusion block (14).