A green synthesis process for high-purity hexadecyl isooctanoate and its application in cosmetics

By using molecular sieve-supported composite catalysts and segmented temperature-controlled vacuum esterification reactions, the problems of equipment corrosion and environmental pollution in the synthesis of hexadecyl isooctanoate have been solved, realizing the green synthesis of high-purity hexadecyl isooctanoate and its multifunctional cosmetic applications.

CN123106424APending Publication Date: 2026-11-17YICHANG MINGYA NEW MATERIAL TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611425582.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

The existing synthesis process for hexadecyl isooctanoate has problems such as highly corrosive equipment, numerous side reactions, and serious environmental pollution, making it difficult to meet the purity and environmental protection requirements of high-end cosmetics.

Method used

High-purity hexadecyl isooctanoate was prepared by using a boron trifluoride and zinc chloride composite Lewis acid catalyst supported on HZSM-5 molecular sieve and combining it with a segmented temperature-controlled vacuum esterification reaction. The catalyst can be recycled, reducing wastewater discharge.

Benefits of technology

The production of high-purity, low-impurity, and light-colored isooctanoic acid hexadecyl ester has been achieved, with high catalytic selectivity, few side reactions, and compliance with high-end cosmetic standards, thus improving the skin-moisturizing, penetrating, and stability effects of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
Patent Text Reader

Abstract

This invention discloses a green synthesis process for high-purity hexadecyl isooctanoate and its application in cosmetics, relating to the field of fine chemical technology. Addressing the technical shortcomings of existing hexadecyl isooctanoate synthesis processes, such as strong catalyst corrosivity, numerous byproducts, low product purity, and poor color, this invention employs a solid composite Lewis acid-molecular sieve supported catalyst to replace the traditional strong acid catalyst. A green process of segmented temperature-controlled and reduced-pressure esterification is used to prepare hexadecyl isooctanoate, effectively improving product purity, with parameters compatible with cosmetic-grade raw material standards. The hexadecyl isooctanoate prepared by this invention features high purity, light color, no odor, good biocompatibility, and excellent breathability and skin-moisturizing properties. It can be widely used in cosmetics such as face creams, lotions, and foundations, offering multiple benefits including moisturizing, softening, penetration enhancement, and stabilizing active ingredients. The preparation process of this invention is green and environmentally friendly, requires minimal equipment, and is suitable for large-scale industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of fine chemical technology, specifically to a method for preparing hexadecyl isooctanoate. Background Technology

[0002] Hexadecyl isooctanoate, known as "seabird feather oil," is a high-end fatty acid ester compound. It is a non-ionic oily raw material with excellent oil compatibility, skin permeability, spreadability, and low irritation. It also possesses good antioxidant, anti-discoloration, and anti-odor stability. It can be used as a thickener, emulsifier, emulsifier, lubricant, and surfactant, making it an indispensable functional raw material in the cosmetics industry. Compared to traditional cosmetic ester raw materials such as isooctyl palmitate and stearate, hexadecyl isooctanoate has a moderate degree of molecular branching, lower oil viscosity, and stronger spreadability. It can form a thin, breathable protective film on the skin surface without clogging pores, providing moisturizing, softening, and brightening effects. It can also act as a carrier for active ingredients, enhancing the skin penetration efficiency of skincare ingredients.

[0003] Currently, the industrial synthesis of hexadecyl isooctanoate mostly employs the traditional homogeneous strong acid catalytic esterification process, which involves the direct esterification reaction of isooctanoic acid and hexadecyl alcohol under the catalysis of a mixed system of concentrated sulfuric acid and sulfurous acid. This process has several inherent drawbacks: First, the strong acid catalyst is highly corrosive, requiring sophisticated production equipment, resulting in significant equipment wear and tear and high production costs. Second, side reactions such as carbonization and alcohol dehydration easily occur during the reaction, generating impurities such as pigments, ethers, and oligomers, leading to a yellowish color and high impurity content in the finished product. This necessitates complex decolorization and impurity removal processes, and the acid value and residual alcohol content of the finished product often fail to meet the standards for high-end cosmetic raw materials. Third, the strong acid catalyst cannot be recovered after the reaction, and the neutralization and washing process generates a large amount of saline wastewater, causing severe environmental pollution and failing to meet the requirements of green chemical production.

[0004] Existing technology CN 101486646 A discloses a method for synthesizing hexadecyl isooctanoate. This method uses an acidic catalyst and a color-protecting agent to esterify isooctanoic acid with hexadecyl alcohol. However, after the reaction, this method requires steps such as vacuum deacidification, neutralization, water washing, and vacuum dehydration, making the preparation process complex and posing environmental pollution problems. Summary of the Invention

[0005] Therefore, this invention provides a green synthesis process for preparing high-purity hexadecanoate isooctanoate using a novel composite catalyst system and segmented temperature-controlled vacuum esterification. This process yields high-purity, low-impurity, light-colored cosmetic-grade hexadecanoate isooctanoate.

[0006] A green synthesis process for high-purity hexadecanoic acid ester includes the following steps:

[0007] (1) Catalyst preparation: HZSM-5 molecular sieve was used as a support to support boron trifluoride and zinc chloride composite Lewis acid. The loading amount was 8%~12% of the support mass. After drying at 120℃ for 2~3h and calcining at 400℃ for 2~4h, a solid composite catalyst was obtained. The catalyst particle size was 20~40 mesh and the specific surface area was ≥320m² / g.

[0008] (2) Esterification reaction: The reaction raw materials, isooctanoic acid and hexadecyl alcohol, are precisely mixed in a molar ratio of 1:1.1 to 1:1.3 into the reaction vessel and stirred evenly. 0.2% to 0.5% of the total mass of the raw materials is added to the composite catalyst and stirred evenly. First stage low temperature reaction: The temperature is raised to 110 to 125℃, the vacuum degree is -0.08 to -0.09 MPa, and the reaction is kept at the temperature for 2 to 3 hours to complete most of the esterification reaction. By-product water is generated and removed by vacuum. Second stage high temperature refining reaction: The temperature is raised to 145 to 160℃, the vacuum degree is increased to -0.095 to -0.10 MPa, and the reaction is kept at the temperature for 1.5 to 2.5 hours to completely complete the esterification reaction and remove residual water and unreacted small molecule raw materials.

[0009] (3) Post-processing and product purification: After the reaction is completed, the temperature is reduced to 60~70℃ and the solid catalyst is recovered by filtration. The filtrate is subjected to vacuum distillation, activated carbon decolorization and sterile filtration to remove trace impurities and pigments, and finally a colorless, transparent and odorless high-purity isooctanoic acid hexadecyl ester product is obtained.

[0010] This invention also provides the application of the above-mentioned high-purity hexadecyl isooctanoate in cosmetics. The hexadecyl isooctanoate can be used as a multifunctional raw material in skincare and makeup cosmetics. Specific applications are as follows:

[0011] 1. As a lightweight moisturizer: Add 2%~8% to face creams, lotions, and hand creams to form a breathable moisturizing protective film, improve moisturizing duration by more than 40%, leave the skin feeling refreshed and non-sticky, and prevent acne and oiliness.

[0012] 2. As a penetration enhancer: Add 1%~5%, combined with active ingredients such as vitamin C, niacinamide, and plant peptides, to increase the skin penetration efficiency of active ingredients by 30%~50% and enhance skin care effects.

[0013] 3. As an active stabilizer: Add 3%~6% to encapsulate and isolate heat-sensitive and easily oxidized active ingredients, delay ingredient deactivation, and extend the shelf life of cosmetics by 6~12 months.

[0014] 4. As a makeup texture modifier: Add 4%~10% to foundation, concealer, and blush to improve the spreadability and adherence of makeup, reduce caking and powdering, and increase makeup duration by more than 25%.

[0015] Compared with the prior art, the beneficial effects of the present invention are:

[0016] 1. Catalyst system innovation: Abandoning traditional highly corrosive homogeneous acid catalysts, we adopt molecular sieve supported composite Lewis acid solid catalysts. The catalysts are recyclable and reusable, produce no wastewater pollution, have high catalytic selectivity, significantly suppress side reactions, reduce impurity generation from the source, and improve product purity.

[0017] 2. Innovative process parameters: The esterification reaction mode adopts segmented temperature control and gradient decompression, which matches the esterification reaction kinetics. The reaction is carried out at low temperature and fast in the early stage, and at high temperature and decompression in the later stage to remove by-product water and residual raw materials. The reaction conversion rate is ≥99.5%, the product purity is ≥99.9%, and the acid value is ≤0.1mgKOH / g, which fully meets the standards for high-end cosmetic raw materials.

[0018] 3. Innovative Application Functions: Breaking through the traditional single moisturizing function, high-purity hexadecyl isooctanoate is used as a four-functional raw material in cosmetics, serving as a moisturizer, penetration enhancer, active stabilizer, and texture modifier, thus solving the problems of poor skin feel, low stability of active ingredients, and insufficient spreadability of makeup in traditional products. Attached Figure Description

[0020] Figure 1 This is a concealer formulated with hexadecyl isooctanoate as the raw material. Before and after comparison photos show the effect of its application. Detailed Implementation

[0022] To better understand the technical content of this invention, specific embodiments are provided below to further illustrate the invention. The following descriptions are merely preferred embodiments of the invention and do not represent the scope of protection of this invention. Any modifications, equivalent substitutions, variations, etc., made within the spirit and principles of this invention are still within the scope of protection of this invention.

[0023] Example 1

[0024] (1) Catalyst preparation: HZSM-5 molecular sieve was selected, and boron trifluoride-zinc chloride composite Lewis acid with a mass ratio of 10% was loaded. The mixture was dried at 120℃ for 2h and calcined at 400℃ for 3h to activate it, thus obtaining a solid composite catalyst.

[0025] (2) Esterification reaction: The reaction raw materials, isooctanoic acid and hexadecyl alcohol, are added to the reactor at a molar ratio of 1:1.2. 0.3% of the total mass of the raw materials is added to the composite catalyst and stirred evenly. The reaction is carried out at 120℃ and -0.085MPa for 2.5h to remove most of the by-product water. The temperature is raised to 155℃ and -0.098MPa for 2h to complete the esterification.

[0026] (3) Post-processing and product purification: The catalyst was recovered by filtration at 65°C, the filtrate was distilled at 100°C and -0.10MPa, 0.25% activated carbon was added for decolorization, and the product was obtained by precision sterile filtration to obtain the finished product hexadecyl isooctanoate.

[0027] According to the test results, the product of this embodiment has a purity of 99.92%, an acid value of 0.032 mg KOH / g, a moisture content of 0.018%, an APHA of ≤5, no odor or irritation, and fully meets the standards for high-end cosmetic raw materials. The reaction conversion rate is 99.55%.

[0028] Example 2 (Skincare Product Application Example)

[0029] This highly moisturizing and refreshing lotion contains the following ingredients by weight percentage: 5% high-purity hexadecyl isooctanoate, 4% squalane, 3% glycerin, 0.2% sodium hyaluronate, 2% niacinamide, 1.5% plant extracts, 2.5% emulsifier, balance deionized water, and 0.1% preservative. Prepared using conventional emulsification processes, the lotion has a light texture, absorbs quickly after application, and leaves no sticky residue. It maintains 78% skin hydration within 24 hours. Compared to lotions made from common ester-based ingredients, its moisturizing effect is 42% longer-lasting, retains over 90% of niacinamide activity, and extends shelf life by 8 months.

[0030] Example 3 (Makeup Application Example)

[0031] This concealer, by weight percentage, contains the following ingredients: 8.0% high-purity isooctanoic acid hexadecyl ester, 8.0% squalane, 18.0% titanium dioxide, 6.0% talc (ultra-fine lipophilic), 4.0% mica powder, 8.0% plant oil, 3.0% emulsifier, 2.0% moisturizer, 0.5% vitamin E tocopherol, 2.0% sodium hyaluronate (small molecule), 1.0% allantoin, 10.0% polydimethylsiloxane (5cs), balance deionized water, and 0.5% additives. The resulting foundation exhibits excellent spreadability, adheres naturally to the skin without caking or creasing, and lasts up to 10 hours. Compared to traditional ingredients, it significantly improves the fineness and staying power of the makeup. See the comparison of usage effects. Figure 1 As shown.

[0032] Comparative example (traditional process)

[0033] Using a traditional concentrated sulfuric acid-sulfurous acid composite catalytic process, with the same raw material ratio, reaction temperature and time, isooctanoic acid hexadecyl ester was prepared. The finished product had a purity of 95.2%, an acid value of 0.35 mg KOH / g, and an APHA of ≥30. However, it contained trace amounts of irritating impurities, and when applied to cosmetics, it left a sticky feeling on the skin. The active ingredients had poor stability and a short shelf life. Furthermore, the production process generated a large amount of saline wastewater, resulting in poor environmental performance.

Claims

1. A green synthesis process for high-purity hexadecyl isooctanoate, characterized in that, The preparation steps include: mixing the reaction raw materials isooctanoic acid and hexadecyl alcohol with a solid composite catalyst to carry out an esterification reaction, and then refining the product by post-treatment such as filtration, vacuum distillation and decolorization to obtain high-purity isooctanoic acid hexadecyl ester.

2. The synthesis process according to claim 1, characterized in that, The catalyst uses HZSM-5 molecular sieve as a support, loaded with 8%~12% boron trifluoride-zinc chloride composite Lewis acid by mass ratio. After drying at 120℃ for 2~3 h and calcining at 400℃ for 2~4 h, a solid composite catalyst is obtained. The catalyst particle size is 20~40 mesh, and the specific surface area is ≥320 m² / g.

3. The synthesis process according to claim 1, characterized in that, The molar ratio of isooctanoic acid to cetyl alcohol is 1:1.1 to 1:1.

3. The mass of catalyst added is 0.2% to 0.5% of the total mass of the raw materials. The segmented temperature-controlled vacuum esterification range is: reacting at 110 to 125℃ and -0.08 to -0.09 MPa for 2 to 3 hours, and then reacting at 145 to 160℃ and -0.095 to -0.10 MPa for 1.5 to 2.5 hours.

4. The synthesis process according to claim 1, characterized in that, During post-treatment, the reduced pressure distillation temperature is 100℃ and the vacuum degree is -0.10MPa. The amount of activated carbon used for decolorization is 0.2%~0.3% of the filtrate mass.

5. The high-purity hexadecyl isooctanoate prepared by the process according to any one of claims 1-4, characterized in that, The product has a purity of ≥99.9%, an acid value of ≤0.1mgKOH / g, an APHA color of ≤5, and is odorless and non-irritating to the skin.

6. The application of the high-purity hexadecyl isooctanoate as described in claim 5 in cosmetics, characterized in that, The hexadecyl isooctanoate is used as a multifunctional raw material in skin care and makeup cosmetics, and has the functions of moisturizing, penetrating and enhancing efficacy, stabilizing activity and regulating texture.

7. The application according to claim 6, characterized in that, As a moisturizer, it can be added to lotions and creams at a rate of 2% to 8% to improve the product's breathability and hydration, and prevent stickiness and breakouts.

8. The application according to claim 6, characterized in that, As a penetration enhancer and active stabilizer, it is added to serums and skin lotions at a rate of 1% to 5% to improve the penetration efficiency of active ingredients and extend the product's shelf life.

9. The application according to claim 6, characterized in that, As a texture modifier, it is added to makeup products at a rate of 4% to 10% to improve the spreadability, adherence, and staying power of makeup.

Citation Information

Patent Citations

  • Method for synthesizing isooctanoic acid hexadecyl ester