A method for immobilizing xylanase and its application

By combining amino functionalization and directional adsorption of nano-zinc oxide/ethyl cellulose composite fiber carriers with the use of low-concentration cross-linking agents, the problems of enzyme activity loss and stability in xylanase immobilization methods were solved, achieving efficient enzyme immobilization and continuous catalytic effect.

CN123107982APending Publication Date: 2026-11-17ZHEJIANG FORESTRY UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611502003.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-24
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing xylanase immobilization methods suffer from problems such as significant enzyme activity loss, poor stability, low mass transfer efficiency, poor reusability, use of toxic cross-linking agents, and difficulty in continuous large-scale application.

Method used

Nano-zinc oxide/ethyl cellulose composite fiber was used as the immobilization carrier. The surface of the carrier was functionalized with 3-aminopropyltriethoxysilane. Xylanase with hexahistine tag was used for synergistic directional adsorption between coordination-hydrogen bonds between zinc ions and amino groups on the surface of nano-zinc oxide. Combined with low-concentration genipin and cross-linking, the carrier was lyophilized and preserved using a protective agent system of polyethylene glycol 2000, glycine, calcium chloride and phosphate buffer.

Benefits of technology

It improves enzyme activity recovery, thermal stability, and reusability, enhances enzyme-substrate mass transfer efficiency, reduces enzyme activity loss, and achieves stable and efficient continuous catalytic preparation of xylooligosaccharides.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123107982A_ABST
    Figure CN123107982A_ABST
Patent Text Reader

Abstract

This invention relates to the field of enzyme immobilization technology and discloses a method for preparing and applying immobilized xylanase. The method uses nano-zinc oxide / ethyl cellulose composite fibers as the immobilization carrier and introduces amino functionalized sites on the fiber surface, which increases the specific surface area of ​​the carrier and improves the mass transfer efficiency between the enzyme and substrate. Simultaneously, it utilizes the coordination of zinc ions with histidine tags to achieve directional immobilization, reducing steric hindrance at the enzyme's active site. The use of a low-concentration genipin temperature, cross-linking, and a polyethylene glycol 2000 / glycine / calcium chloride protective agent system helps maintain the enzyme's native conformation, thereby improving enzyme activity recovery, thermal stability, and reusability. The resulting immobilized xylanase can be applied in the fields of xylooligosaccharide preparation, feed additives, papermaking auxiliaries, food processing, brewing, and biomass degradation, exhibiting advantages such as high enzyme activity recovery, good stability, and continuous operation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of enzyme immobilization technology, specifically to a method for the immobilization and preparation of xylanase and its application. Background Technology

[0002] Xylanases are enzymes that hydrolyze the β-1,4-xylosidic bonds in xylan molecules, and they have wide applications in xylooligosaccharide preparation, feed additives, papermaking auxiliaries, food processing, brewing, and biomass degradation. However, free xylanases suffer from poor thermal stability, limited pH adaptability, easy inactivation, difficulty in recovery, and inability to be reused, which restricts their industrial applications. Immobilization technology is an important means to improve the stability and reusability of xylanases, but existing immobilization methods still have many shortcomings.

[0003] Existing immobilization methods, such as sodium alginate encapsulation, covalent bonding, adsorption, cross-linking, and carrier immobilization, often suffer from significant reductions in enzyme activity due to chemical modifications, steric hindrance, or carrier mass transfer limitations. Some methods exhibit low immobilization rates, increased Km values, and decreased enzyme-substrate binding capacity. Certain carriers, such as mesoporous molecular sieves, magnetic nanoparticles, and Eupergit C, present challenges due to complex preparation, high cost, poor dispersibility, or the need for toxic cross-linking agents like glutaraldehyde, impacting environmental friendliness and large-scale application. Furthermore, traditionally immobilized enzymes exhibit rapid activity decline during repeated use and continuous operation, are prone to conformational changes and enzyme activity loss during freeze-drying, and the stability of continuous catalysis in packed beds remains to be improved.

[0004] Therefore, it is of great significance to develop a xylanase immobilization method with high enzyme activity recovery rate, good mass transfer efficiency, abundant immobilization sites, mild cross-linking, stable preservation and continuous use. Summary of the Invention

[0005] (a) Technical problems to be solved To address the shortcomings of existing technologies, this invention provides an immobilized preparation method and application of xylanase, which has the advantages of high enzyme activity recovery rate, good thermal stability and reusability, high mass transfer efficiency, stable freeze-drying preservation, mild and environmentally friendly cross-linking, and continuous catalysis. It solves the problems of large enzyme activity loss, poor stability, low mass transfer efficiency, poor reusability, use of toxic cross-linking agents, and difficulty in continuous large-scale application of existing immobilization methods.

[0006] (II) Technical Solution To achieve the above objectives, the present invention provides the following technical solution: a method for immobilizing xylanase, comprising the following steps: Step 1: Preparation of carrier precursor: Prepare ethyl cellulose, nano zinc oxide, anhydrous ethanol and N,N-dimethylformamide in the specified proportions. Disperse nano zinc oxide in anhydrous ethanol in the specified proportion to obtain zinc oxide suspension. Add ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent to form ethyl cellulose solution. Slowly add zinc oxide suspension to ethyl cellulose solution and stir evenly to obtain nano zinc oxide / ethyl cellulose mixed spinning precursor solution. Step 2, preparation of composite fiber carrier: The precursor solution obtained in Step 2 is injected into an electrospinning device to obtain nascent nano zinc oxide / ethyl cellulose composite fiber mat deposited on an aluminum foil receiving plate under set conditions. Step 3, Vacuum Drying: After spinning, the nascent nano zinc oxide / ethyl cellulose composite fiber felt deposited on the aluminum foil is dried under vacuum conditions at room temperature to obtain nano zinc oxide / ethyl cellulose composite fiber felt, and its weight is recorded as m; Step 4: Amine functionalization of the carrier surface: Prepare a functionalization solution consisting of 3-aminopropyltriethoxysilane, anhydrous ethanol and ultrapure water. Immerse the composite fiber felt obtained in Step 3 into the functionalization solution and keep it at 55-65℃ for 2-3 hours. After the reaction is complete, wash it 3-5 times with anhydrous ethanol and vacuum dry it at 55-60℃ and a vacuum degree of -0.08 to -0.10 MPa for 6-12 hours until constant weight is reached. After naturally cooling to room temperature, remove it to obtain the amino-functionalized nano zinc oxide / ethyl cellulose composite fiber carrier. Step 5, Immobilization of xylanase: Dissolve xylanase in a protective agent solution to prepare an enzyme solution. Immerse the amino-functionalized composite fiber carrier obtained in Step 4 into the enzyme solution and shake to adsorb under set conditions. Then add genipin and continue gentle shaking crosslinking. After crosslinking, wash with phosphate buffer until no free protein can be detected in the washing solution to obtain immobilized xylanase. Step 6, Freeze-drying and preservation: The immobilized xylanase obtained in step 5 is placed in a diluted protective agent solution, pre-frozen at low temperature, and then transferred to a vacuum freeze dryer. It is dried under the set cold trap conditions to finally obtain immobilized xylanase dry powder.

[0007] Preferably, the raw materials and their mass ratios for the carrier precursor in step one are: 10-14 parts ethyl cellulose; 2-4 parts nano zinc oxide; 55-60 parts anhydrous ethanol; and 28-30 parts N,N-dimethylformamide.

[0008] Preferably, the viscosity of the ethyl cellulose is controlled between 45 and 55 mPa·s; and the average particle size of the nano zinc oxide is between 20 and 40 nm.

[0009] Preferably, the carrier precursor preparation process in step one is as follows: S1.1 First, add nano zinc oxide to 1 / 3 to 1 / 2 anhydrous ethanol and sonicate for 30 to 45 minutes to form a zinc oxide suspension; S1.2 Add the ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent, and stir magnetically in a water bath at 40-50℃ and 200-300r / min for 2-3 hours until completely dissolved to obtain an ethyl cellulose solution; S1.3 Add zinc oxide suspension dropwise to ethyl cellulose solution at a rate of 0.5-1.0 mL / min, and continue to stir magnetically at 300-400 r / min for 1-2 h to obtain nano zinc oxide / ethyl cellulose mixed spinning precursor solution.

[0010] Preferably, the preparation conditions for the composite fiber carrier in step two are as follows: the electrospinning device uses a stainless steel needle with an inner diameter of 0.5-0.8 mm; the spinning voltage is set to 15-22 kV when preparing the composite fiber carrier; the distance between the needle and the aluminum foil receiving plate is 12-18 cm; the solution flow rate is 0.5-1.0 mL / h; the ambient temperature is 25-30℃; and the relative humidity is 35%-50%.

[0011] Preferably, in step three, vacuum drying is performed at room temperature for 12–24 hours, resulting in nano-zinc oxide / ethyl cellulose composite fiber felt with an average fiber diameter of 300–800 nm, a specific surface area of ​​0.55–0.70 m² / g, and a water contact angle of 105°–120°.

[0012] Preferably, in step four: (1) Composition of the functionalized liquid: The volume ratio of anhydrous ethanol to ultrapure water is 95:5, and the volume fraction of 3-aminopropyltriethoxysilane is 1% to 3%; (2) Based on the mass m of the fiber felt: the ratio of composite fiber felt to functional liquid is 1g: 20-50mL.

[0013] Preferably, the immobilization process of xylanase in step five is as follows: S2.1 Dissolve xylanase in a protective agent solution to prepare an enzyme solution with an enzyme protein concentration of 1.5–3.0 mg / mL; S2.2. The amino-functionalized composite fiber carrier obtained in step four is immersed in the enzyme solution at a ratio of 1g:15-25mL, and the adsorption is carried out under mild conditions of 4-8℃ and 60-80rpm for 4-6h to obtain a carrier-enzyme solution mixed system. S2.3 Add genipin to the carrier-enzyme solution mixture obtained in S2.2, so that the final concentration of genipin is 0.1% to 0.3%, and continue to gently shake and crosslink at 20 to 25°C for 30 to 60 minutes. S2.4 After cross-linking, wash the immobilized xylanase after cross-linking 3 to 5 times with pH 6.0 to 7.0 phosphate buffer until no free protein can be detected in the washing solution, and the immobilized xylanase is obtained.

[0014] Preferably, in step six, the freeze-drying and preservation are performed as follows: S3.1 Prepare a protective agent solution consisting of polyethylene glycol 2000, glycine, calcium chloride, and phosphate buffer solution with pH 6.0-7.0 and 20-50 mmol / L. Place the immobilized xylanase obtained in step five into the protective agent solution diluted 5-10 times at a ratio of 1g:3-5mL, and pre-freeze at a temperature of -25 to -45℃ for 4-5 hours. S3.2 Then transfer to a vacuum freeze dryer and dry for 12 to 24 hours at a cold trap temperature of -50 to -55°C and a vacuum degree of 10 to 30 Pa to obtain immobilized xylanase dry powder. S3.3 The freeze-dried immobilized xylanase powder was stored in a sealed container at 4°C.

[0015] An application of a xylanase: the xylanase prepared according to the above process is applied in the field of xylooligosaccharide preparation.

[0016] Compared with the prior art, the present invention provides a method for immobilizing xylanase and its application, which has the following beneficial effects: 1. This invention uses nano-zinc oxide / ethyl cellulose composite fiber as an immobilization carrier and performs amino functionalization on the fiber surface with 3-aminopropyltriethoxysilane, which achieves the beneficial effects of increasing the specific surface area and porosity of the carrier, improving enzyme-substrate mass transfer, increasing enzyme immobilization sites, and improving xylanase loading and enzyme activity recovery rate.

[0017] 2. This invention achieves beneficial effects such as directional immobilization of xylanase with a hexahistidine tag, synergistic adsorption between coordination-hydrogen bonds between zinc ions and amino groups on the surface of nano-zinc oxide, and the use of low-concentration geniemin temperature and cross-linking, thereby realizing the beneficial effects of directional immobilization of xylanase, reducing steric hindrance of active centers, avoiding enzyme inactivation caused by strong cross-linking agents such as glutaraldehyde, and improving thermal stability and reusability.

[0018] 3. This invention uses a protective agent system composed of polyethylene glycol 2000, glycine, calcium chloride and phosphate buffer for pre-freezing and vacuum freeze-drying, and uses immobilized xylanase for continuous catalysis in a packed bed reactor. This achieves the beneficial effects of improving freeze-drying stability, reducing enzyme activity loss during storage and operation, improving continuous catalytic efficiency and xylooligosaccharide preparation efficiency. Attached Figure Description

[0019] Figure 1This is a flowchart of the xylanase immobilization process of the present invention. Detailed Implementation

[0020] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0021] Please see Figure 1 A method for immobilizing xylanase, comprising the following steps: Step 1: Preparation of carrier precursor: Prepare ethyl cellulose (EC), nano zinc oxide (ZnO), anhydrous ethanol and N,N-dimethylformamide (DMF) in the specified proportions. Disperse nano zinc oxide in anhydrous ethanol to obtain a zinc oxide suspension. Add ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent to form an ethyl cellulose solution. Slowly add the zinc oxide suspension to the ethyl cellulose solution and stir until homogeneous to obtain a nano zinc oxide / ethyl cellulose mixed spinning precursor solution. Step 2, preparation of composite fiber carrier: The precursor solution obtained in Step 2 is injected into an electrospinning device to obtain nascent nano zinc oxide / ethyl cellulose composite fiber mat deposited on an aluminum foil receiving plate under set conditions. Step 3, Vacuum Drying: After spinning, the nascent nano zinc oxide / ethyl cellulose composite fiber felt deposited on the aluminum foil is dried under vacuum conditions at room temperature to obtain nano zinc oxide / ethyl cellulose composite fiber felt, and its weight is recorded as m; Step 4: Amine functionalization of the carrier surface: Prepare a functionalization solution consisting of 3-aminopropyltriethoxysilane (APTES), anhydrous ethanol, and ultrapure water. Immerse the composite fiber felt obtained in Step 3 into the functionalization solution and keep it at 55-65℃ for 2-3 hours to allow 3-aminopropyltriethoxysilane to condense with the hydroxyl groups on the fiber surface and the nano zinc oxide surface, introducing amino groups. After the reaction is complete, wash with anhydrous ethanol 3-5 times and vacuum dry at 55-60℃ and a vacuum degree of -0.08 to -0.10 MPa for 6-12 hours until constant weight is achieved. After naturally cooling to room temperature, remove the fiber to obtain the amino-functionalized nano zinc oxide / ethyl cellulose composite fiber carrier. Step 5, Immobilization of xylanase: Dissolve xylanase in a protective agent solution to prepare an enzyme solution. Immerse the amino-functionalized composite fiber carrier obtained in Step 4 into the enzyme solution and shake to adsorb under set conditions. Then add genipin and continue gentle shaking crosslinking. After crosslinking, wash with phosphate buffer until no free protein can be detected in the washing solution to obtain immobilized xylanase. Step 6, Freeze-drying and preservation: The immobilized xylanase obtained in step 5 is placed in a diluted protective agent solution, pre-frozen at low temperature, and then transferred to a vacuum freeze dryer. It is dried under the set cold trap conditions to finally obtain immobilized xylanase dry powder.

[0022] The advantages are: by using nano-zinc oxide / ethyl cellulose composite fibers as the immobilization carrier and introducing amino functionalized sites on the fiber surface, it is beneficial to increase the specific surface area of ​​the carrier and improve the mass transfer efficiency between the enzyme and the substrate. At the same time, the coordination between zinc ions and histidine tags is used to achieve directional immobilization and reduce the steric hindrance of the enzyme active site. The low-concentration genipin mild cross-linking and polyethylene glycol 2000 / glycine / calcium chloride protective agent system are beneficial to maintain the native conformation of the enzyme and improve the enzyme activity recovery rate, thermal stability and reusability stability.

[0023] Specifically, the raw materials and their mass ratios for the carrier precursor in step one are as follows: 10-14 parts ethyl cellulose; 2-4 parts nano zinc oxide; 55-60 parts anhydrous ethanol; and 28-30 parts N,N-dimethylformamide.

[0024] The advantages are: by limiting the mass ratio of ethyl cellulose, nano zinc oxide, anhydrous ethanol and N,N-dimethylformamide, it is beneficial to obtain a spinning precursor solution with suitable viscosity and uniform zinc oxide dispersion, thereby ensuring the stability of the electrospinning process, forming continuous and uniform nanocomposite fibers, and ultimately improving the carrier's loading capacity for xylanase.

[0025] Specifically, the viscosity of ethyl cellulose is controlled between 45 and 55 mPa·s; the average particle size of nano zinc oxide is between 20 and 40 nm.

[0026] The advantages are: by selecting ethyl cellulose with a viscosity of 45-55 mPa·s and nano zinc oxide with an average particle size of 20-40 nm, it is beneficial to balance the spinnability of the spinning solution and the dispersion stability of nano zinc oxide, so that nano zinc oxide is uniformly exposed on the fiber surface, providing sufficient coordination sites for subsequent amino functionalization and directional immobilization.

[0027] Specifically, the process for preparing the carrier precursor in step one is as follows: S1.1 First, add nano zinc oxide to 1 / 3 to 1 / 2 anhydrous ethanol and sonicate for 30 to 45 minutes to form a uniform zinc oxide suspension. S1.2 Add the ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent, and stir magnetically in a water bath at 40-50℃ and 200-300r / min for 2-3 hours until completely dissolved to obtain an ethyl cellulose solution; S1.3. The zinc oxide suspension is slowly added dropwise to the ethyl cellulose solution at a rate of 0.5-1.0 mL / min, and the mixture is magnetically stirred at a speed of 300-400 r / min for 1-2 h to obtain a nano zinc oxide / ethyl cellulose mixed spinning precursor solution.

[0028] The advantages are: by first ultrasonically dispersing the nano zinc oxide in a portion of anhydrous ethanol and then slowly mixing it with the ethyl cellulose solution, it is beneficial to avoid the agglomeration of the nano zinc oxide; by controlling the dissolution temperature, stirring speed and dropping rate, it is beneficial to obtain a uniformly dispersed and viscosity-stable spinning precursor solution, which ultimately provides good conditions for subsequent electrospinning.

[0029] Specifically, the preparation conditions for the composite fiber carrier in step two are as follows: the electrospinning device uses a stainless steel needle with an inner diameter of 0.5–0.8 mm; the spinning voltage is set to 15–22 kV when preparing the composite fiber carrier; the distance between the needle and the aluminum foil receiving plate is 12–18 cm; the solution flow rate is 0.5–1.0 mL / h; the ambient temperature is 25–30 °C; and the relative humidity is 35%–50%.

[0030] The advantages are: by controlling the needle inner diameter, spinning voltage, receiving distance, solution flow rate, ambient temperature and relative humidity, it is beneficial to form nanocomposite fibers with uniform diameter, no bead strands, and no adhesion, thereby increasing the specific surface area and porosity of the fiber mat, which is conducive to the immobilization of xylanase and substrate mass transfer.

[0031] Specifically, in step three, vacuum drying is performed: vacuum drying is carried out at room temperature for 12 to 24 hours. The average fiber diameter in the obtained nano zinc oxide / ethyl cellulose composite fiber felt is 300 to 800 nm, the specific surface area of ​​the fiber felt is 0.55 to 0.70 m² / g, and the water contact angle is 105° to 120°. The carrier is nano zinc oxide / ethyl cellulose composite fiber.

[0032] The advantages are: room temperature vacuum drying helps to maintain the fiber morphology and pore structure while removing residual solvents, avoiding fiber shrinkage or nano zinc oxide aggregation caused by high temperature drying; the resulting fibers have an average diameter of 300-800 nm and a specific surface area of ​​0.55-0.70 m² / g, which helps to improve enzyme loading and catalytic efficiency.

[0033] Specifically, in step four: (1) Composition of the functionalized liquid: The volume ratio of anhydrous ethanol to ultrapure water is 95:5, and the volume fraction of 3-aminopropyltriethoxysilane is 1% to 3%; (2) Based on the mass m of the fiber felt: the ratio of composite fiber felt to functional liquid is 1g: 20-50mL.

[0034] The advantages are: by using an ethanol-water system and controlling the volume fraction of 3-aminopropyltriethoxysilane, it is beneficial for 3-aminopropyltriethoxysilane to undergo uniform hydrolysis and condensation on the fiber surface, thereby introducing an appropriate amount of amino groups; by controlling the ratio of composite fiber felt to functionalizing liquid, it is beneficial to avoid excessive functionalizing liquid leading to pore blockage or excessive amino density, thereby increasing the number of immobilization sites while maintaining enzyme activity.

[0035] Specifically, the immobilization process of xylanase in step five: S2.1 Dissolve xylanase in a protective agent solution to prepare an enzyme solution with an enzyme protein concentration of 1.5–3.0 mg / mL; S2.2. The amino-functionalized composite fiber carrier obtained in step four is immersed in the enzyme solution at a ratio of 1g:15-25mL, and the adsorption is carried out under mild conditions of 4-8℃ and 60-80rpm for 4-6h to obtain a carrier-enzyme solution mixed system. S2.3 Add genipin to the carrier-enzyme solution mixture obtained after adsorption in S2.2, and add the amount to make the final concentration of genipin 0.1% to 0.3% (w / v), that is, 15 to 75 mg of genipin per g of carrier. Continue to gently shake and crosslink at 20 to 25°C for 30 to 60 min. S2.4 After cross-linking, wash the immobilized xylanase after cross-linking 3 to 5 times with phosphate buffer at pH 6.0 to 7.0, each time using 5 to 10 mL / g of carrier, until no free protein can be detected in the washing solution, thus obtaining immobilized xylanase.

[0036] The advantages are: maintaining the xylanase conformation through a protective agent system, and utilizing the coordination-hydrogen bond synergy between the hexahistidine-tagged xylanase and the amino-functionalized nano-zinc oxide / ethyl cellulose composite fiber carrier, which facilitates directional adsorption, oriented the enzyme active site toward the substrate; and the mild cross-linking of low-concentration genipin at 20-25℃ helps stabilize the enzyme adsorption conformation, avoiding activity loss caused by strong cross-linking agents such as glutaraldehyde, thereby improving enzyme activity recovery rate and reusability stability.

[0037] Specifically, in step six, freeze-drying and preservation: S3.1 Prepare a protective agent solution consisting of polyethylene glycol 2000, glycine, calcium chloride, and phosphate buffer solution with pH 6.0-7.0 and 20-50 mmol / L. Place the immobilized xylanase obtained in step five into the protective agent solution diluted 5-10 times at a ratio of 1g:3-5mL, and pre-freeze at a temperature of -25 to -45℃ for 4-5 hours. S3.2 Then transfer to a vacuum freeze dryer and dry for 12 to 24 hours at a cold trap temperature of -50 to -55°C and a vacuum degree of 10 to 30 Pa until the sample is loose dry powder with a moisture content of <5%, thus obtaining immobilized xylanase dry powder. S3.3 The freeze-dried immobilized xylanase powder should be sealed, protected from light, and dried at 4°C to avoid repeated moisture absorption and freeze-thaw cycles. During storage, the enzyme activity loss should not exceed 10% of the initial activity.

[0038] The advantages are: the protective agent system composed of polyethylene glycol 2000, glycine, calcium chloride and phosphate buffer helps stabilize the molecular conformation of xylanase during pre-freezing and freeze-drying, thereby reducing ice crystal damage and dehydration denaturation; by controlling the pre-freezing temperature, cold trap temperature, vacuum degree and drying time, it is beneficial to obtain loose immobilized xylanase dry powder with low water content, ultimately improving storage stability and ease of use.

[0039] An application of xylanase: The xylanase prepared according to the above process is applied in the field of xylooligosaccharide preparation. When used to catalyze the hydrolysis of corn cob xylan to prepare xylooligosaccharides, the obtained immobilized xylanase dry powder is filled into a packed bed reactor by wet packing, with the ratio of filling height to column inner diameter being 8:1 to 15:1. It can also be applied in the fields of feed additives, papermaking auxiliaries, food processing, brewing, or biomass degradation.

[0040] The preparation process of the present invention is applied to the examples as follows: Example 1

[0041] This embodiment provides a method for the immobilization and preparation of xylanase, the specific steps of which are as follows: Step 1: Preparation of carrier precursor: Weigh 12 parts by weight of ethyl cellulose, 3 parts by weight of nano zinc oxide, 57 parts by weight of anhydrous ethanol, and 28 parts by weight of N,N-dimethylformamide; the viscosity of ethyl cellulose is 45-55 mPa·s, and the average particle size of nano zinc oxide is 20-40 nm; add nano zinc oxide to 1 / 2 anhydrous ethanol and sonicate for 40 min to form a uniform zinc oxide suspension; add ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent, and stir magnetically in a water bath at 45℃ and 250 r / min for 2.5 h until completely dissolved to obtain an ethyl cellulose solution; slowly add the zinc oxide suspension dropwise to the ethyl cellulose solution at a rate of 0.8 mL / min, and continue to stir magnetically at 350 r / min for 1.5 h to obtain a nano zinc oxide / ethyl cellulose mixed spinning precursor solution.

[0042] Step 2, Preparation of composite fiber carrier: The precursor solution is injected into an electrospinning device using a stainless steel needle with an inner diameter of 0.6 mm. The spinning voltage is set to 18 kV, the distance between the needle and the aluminum foil receiving plate is 15 cm, the solution flow rate is 0.8 mL / h, the ambient temperature is 28 ℃, and the relative humidity is 45%. This yields nascent nano-zinc oxide / ethyl cellulose composite fiber mat deposited on the aluminum foil receiving plate.

[0043] Step 3, Vacuum drying: The nascent composite fiber felt was vacuum dried at room temperature for 18 hours to obtain nano zinc oxide / ethyl cellulose composite fiber felt. 1.0 g of the fiber was weighed and used for subsequent immobilization. The obtained fiber had an average diameter of 520 nm, a specific surface area of ​​0.62 m² / g, and a water contact angle of 112°.

[0044] Step 4: Amine functionalization of the carrier surface: Prepare a functionalization solution with anhydrous ethanol and ultrapure water in a volume ratio of 95:5 and 3-aminopropyltriethoxysilane in a volume fraction of 2%; based on a fiber felt mass of 1.0 g, the volume of functionalization solution is 30 mL; immerse the fiber felt in the functionalization solution and keep it at 60 °C for 2.5 h to allow 3-aminopropyltriethoxysilane to condense with the hydroxyl groups on the fiber surface and the nano zinc oxide surface, introducing amino groups; after the reaction is complete, wash with anhydrous ethanol 4 times, 10 mL each time, and vacuum dry at 58 °C and a vacuum degree of -0.09 MPa for 8 h until constant weight, and naturally cool to room temperature to obtain an amino-functionalized nano zinc oxide / ethyl cellulose composite fiber carrier.

[0045] Step 5: Immobilization of xylanase: Prepare a protective agent solution containing 4.5% (w / v) polyethylene glycol 2000, 3.5% (w / v) glycine, 2 mmol / L calcium chloride, with the remainder being pH 6.5, 30 mmol / L phosphate buffer. Recombinant GH11 family xylanase with a hexahistidine tag was dissolved in a protective agent solution to prepare an enzyme solution with a protein concentration of 2.0 mg / mL. An amino-functionalized composite fiber carrier was immersed in the enzyme solution at a ratio of 1.0 g carrier to 20 mL enzyme solution, and the mixture was gently shaken at 4 °C and 70 rpm for 5 h to obtain a carrier-enzyme solution mixture. Genipin was added to this mixture to a final concentration of 0.2% (w / v), i.e., 40 mg genipin per g carrier. The mixture was then gently shaken at 22 °C for 45 min for cross-linking. After cross-linking, the mixture was washed four times with pH 6.5 phosphate buffer, 8 mL / g carrier each time, until no free protein was detected in the washings, thus obtaining immobilized xylanase.

[0046] Step 6, Freeze-drying and Preservation: Prepare a protective agent solution consisting of polyethylene glycol 2000, glycine, calcium chloride, and pH 6.5, 30 mmol / L phosphate buffer, and dilute it 5 times; place the immobilized xylanase in the diluted protective agent solution at a ratio of 1 g: 4 mL, and pre-freeze at -35℃ for 4.5 h; then transfer it to a vacuum freeze dryer and dry it for 18 h at a cold trap temperature of -52℃ and a vacuum degree of 20 Pa until the sample is in a loose dry powder state with a water content of <5%, thus obtaining immobilized xylanase dry powder; the freeze-dried immobilized xylanase dry powder is sealed, protected from light, and dried at 4℃.

[0047] Application: Immobilized xylanase dry powder was packed into a packed bed reactor using a wet packing method, with a packing height to column inner diameter ratio of 10:1. Corn cob xylan was used as the substrate at a concentration of 10 g / L, dissolved in a pH 5.8 citrate-disodium hydrogen phosphate buffer solution. The reaction temperature was 52℃, the feed flow rate was 0.5 mL / min, and the effluent was collected to obtain the xylooligosaccharide product. Example 2

[0048] Immobilized xylanase dry powder was prepared using the same process as in Example 1.

[0049] Applications: packed bed height to column inner diameter ratio 8:1, substrate concentration 8 g / L, pH 5.5, temperature 48℃, flow rate 0.3 mL / min. Example 3

[0050] Immobilized xylanase dry powder was prepared using the same process as in Example 1.

[0051] Applications: Packed bed height to column inner diameter ratio 15:1, substrate concentration 15 g / L, pH 6.0, temperature 55℃, flow rate 0.8 mL / min.

[0052] Comparative Example 1 This comparative example is basically the same as Example 1, except that: in step four, 3-aminopropyltriethoxysilane amino functionalization is not performed; instead, the fiber felt is simply soaked in a mixture of anhydrous ethanol and ultrapure water. The remaining steps are the same as in Example 1. That is, xylanase is directly immobilized using unamino-functionalized nano-zinc oxide / ethyl cellulose composite fibers. The results show that due to the lack of amino functionalization sites on the carrier surface, the enzyme adsorption capacity and directional immobilization effect decrease, and the enzyme activity recovery rate, reusability stability, and continuous operation stability of the packed bed are all significantly lower than in Example 1.

[0053] Comparative Example 2 This comparative example is basically the same as Example 1, except that genipin is not used in step five; instead, 2% glutaraldehyde (w / v) is used as the cross-linking agent, and cross-linking is performed at 25°C for 2 hours. The remaining steps are the same as in Example 1. The results show that strong cross-linking with glutaraldehyde easily leads to modification of the xylanase active site and conformational rigidity, resulting in a decrease in enzyme activity recovery. After repeated use, the enzyme activity decreases rapidly, indicating that low-concentration genipin and gentle cross-linking are more conducive to maintaining enzyme activity.

[0054] Comparative Example 3 This comparative example is basically the same as Example 1, except that in step five, a common GH11 family xylanase without a hexahistidine tag was used, and random adsorption immobilization was employed. The remaining steps were the same as in Example 1. The results showed that without the histidine tag, the directional coordination-hydrogen bond synergy between the enzyme and zinc ions and amino groups on the carrier surface was weakened, the enzyme molecule orientation was random, and the active center was easily affected by steric hindrance. The enzyme activity recovery rate, Km value, and reusability stability were all inferior to those of Example 1, indicating that the histidine tag-surface coordination / hydrogen bond synergistic directional adsorption strategy has significant advantages.

[0055] The following table 1 is obtained from the test results of Examples 1-3 and Comparative Examples 1-3:

[0056] Note: The enzyme activity recovery rate in the table is calculated as the ratio of the total activity of the immobilized enzyme to the total activity of the added enzyme; the stability for repeated use is determined by recovering the immobilized enzyme after each catalytic reaction and using it continuously for 10 times; the thermal stability is calculated by the half-life of the residual enzyme activity after incubation at 50℃ for different times; the Km value is determined using corn cob xylan of different concentrations as substrates; the stability for continuous operation of the packed bed is calculated by the enzymatic hydrolysis efficiency of the effluent after 20 batches of continuous operation.

[0057] In summary, a comparison of Examples 1-3 with Comparative Examples 1-3 shows that this process, through the use of nano-zinc oxide / ethyl cellulose composite fiber carrier, 3-aminopropyltriethoxysilane amino functionalization, histidine tag-zinc ion / amino coordination-hydrogen bond synergistic directional adsorption, low-concentration genipin gentle cross-linking, polyethylene glycol 2000 / glycine / calcium chloride protective agent freeze-drying, and packed bed continuous catalysis, significantly improves the enzyme activity recovery rate, thermal stability, reusability stability, and continuous operation stability of xylanase. Among these, Example 1 exhibits the best overall effect, achieving an enzyme activity recovery rate of 88.2%, a relative enzyme activity of 92.5% after 10 reuses, a half-life of 8.6 h at 50°C, a Km value of 3.2 mg / mL, and a relative enzyme activity of 90.1% after 20 batches of continuous packed bed operation. Comparative Examples 1-3 verified the key roles of amino-functionalized carrier, low-concentration genipin, cross-linking, and histidine tag directional immobilization, respectively, indicating that this process has good application prospects in the fields of xylooligosaccharide preparation, feed additives, papermaking auxiliaries, food processing, brewing, or biomass degradation.

[0058] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A method for immobilizing and preparing xylanase, characterized in that, Includes the following steps: Step 1: Preparation of carrier precursor: Prepare ethyl cellulose, nano zinc oxide, anhydrous ethanol and N,N-dimethylformamide in the specified proportions. Disperse nano zinc oxide in anhydrous ethanol in the specified proportion to obtain zinc oxide suspension. Add ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent to form ethyl cellulose solution. Slowly add zinc oxide suspension to ethyl cellulose solution and stir evenly to obtain nano zinc oxide / ethyl cellulose mixed spinning precursor solution. Step 2, preparation of composite fiber carrier: The precursor solution obtained in Step 2 is injected into an electrospinning device to obtain nascent nano zinc oxide / ethyl cellulose composite fiber mat deposited on an aluminum foil receiving plate under set conditions. Step 3, Vacuum Drying: After spinning, the nascent nano zinc oxide / ethyl cellulose composite fiber felt deposited on the aluminum foil is dried under vacuum conditions at room temperature to obtain nano zinc oxide / ethyl cellulose composite fiber felt, and its weight is recorded as m; Step 4: Amine functionalization of the carrier surface: Prepare a functionalization solution consisting of 3-aminopropyltriethoxysilane, anhydrous ethanol and ultrapure water. Immerse the composite fiber felt obtained in Step 3 into the functionalization solution and keep it at 55-65℃ for 2-3 hours. After the reaction is complete, wash it 3-5 times with anhydrous ethanol and vacuum dry it at 55-60℃ and a vacuum degree of -0.08 to -0.10 MPa for 6-12 hours until constant weight is reached. After naturally cooling to room temperature, remove it to obtain the amino-functionalized nano zinc oxide / ethyl cellulose composite fiber carrier. Step 5, Immobilization of xylanase: Dissolve xylanase in a protective agent solution to prepare an enzyme solution. Immerse the amino-functionalized composite fiber carrier obtained in Step 4 into the enzyme solution and shake to adsorb under set conditions. Then add genipin and continue gentle shaking crosslinking. After crosslinking, wash with phosphate buffer until no free protein can be detected in the washing solution to obtain immobilized xylanase. Step 6, Freeze-drying and preservation: The immobilized xylanase obtained in step 5 is placed in a diluted protective agent solution, pre-frozen at low temperature, and then transferred to a vacuum freeze dryer. It is dried under the set cold trap conditions to finally obtain immobilized xylanase dry powder.

2. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, The raw materials and their mass ratios for the carrier precursor in step one are: 10-14 parts ethyl cellulose; 2-4 parts nano zinc oxide; 55-60 parts of anhydrous ethanol; 28-30 parts of N,N-dimethylformamide.

3. The method for immobilizing and preparing xylanase according to claim 2, characterized in that, The viscosity of the ethyl cellulose is controlled between 45 and 55 mPa·s; the average particle size of the nano zinc oxide is between 20 and 40 nm.

4. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, The carrier precursor preparation process in step one is as follows: S1.1 First, add nano zinc oxide to 1 / 3 to 1 / 2 anhydrous ethanol and sonicate for 30 to 45 minutes to form a zinc oxide suspension; S1.2 Add the ethyl cellulose to the remaining anhydrous ethanol and N,N-dimethylformamide mixed solvent, and stir magnetically in a water bath at 40-50℃ and 200-300r / min for 2-3 hours until completely dissolved to obtain an ethyl cellulose solution; S1.3 Add zinc oxide suspension dropwise to ethyl cellulose solution at a rate of 0.5-1.0 mL / min, and continue to stir magnetically at 300-400 r / min for 1-2 h to obtain nano zinc oxide / ethyl cellulose mixed spinning precursor solution.

5. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, The preparation conditions for the composite fiber carrier in step two are as follows: the electrospinning device uses a stainless steel needle with an inner diameter of 0.5-0.8 mm; the spinning voltage is set to 15-22 kV when preparing the composite fiber carrier; the distance between the needle and the aluminum foil receiving plate is 12-18 cm; the solution flow rate is 0.5-1.0 mL / h; the ambient temperature is 25-30℃; and the relative humidity is 35%-50%.

6. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, In step three, vacuum drying is performed at room temperature for 12–24 hours. The resulting nano-zinc oxide / ethyl cellulose composite fiber felt has an average fiber diameter of 300–800 nm, a specific surface area of ​​0.55–0.70 m² / g, and a water contact angle of 105°–120°.

7. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, In step four: (1) Composition of the functionalized liquid: The volume ratio of anhydrous ethanol to ultrapure water is 95:5, and the volume fraction of 3-aminopropyltriethoxysilane is 1% to 3%; (2) Based on the mass m of the fiber felt: the ratio of composite fiber felt to functional liquid is 1g: 20-50mL.

8. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, The immobilization process of xylanase in step five: S2.1 Dissolve xylanase in a protective agent solution to prepare an enzyme solution with an enzyme protein concentration of 1.5–3.0 mg / mL; S2.

2. The amino-functionalized composite fiber carrier obtained in step four is immersed in the enzyme solution at a ratio of 1g:15-25mL, and the adsorption is carried out under mild conditions of 4-8℃ and 60-80rpm for 4-6h to obtain a carrier-enzyme solution mixed system. S2.3 Add genipin to the carrier-enzyme solution mixture obtained in S2.2, so that the final concentration of genipin is 0.1% to 0.3%, and continue to gently shake and crosslink at 20 to 25°C for 30 to 60 minutes. S2.4 After cross-linking, wash the immobilized xylanase after cross-linking 3 to 5 times with pH 6.0 to 7.0 phosphate buffer until no free protein can be detected in the washing solution, and the immobilized xylanase is obtained.

9. The method for immobilizing and preparing xylanase according to claim 1, characterized in that, Freeze-drying and preservation in step six: S3.1 Prepare a protective agent solution consisting of polyethylene glycol 2000, glycine, calcium chloride, and phosphate buffer solution with pH 6.0-7.0 and 20-50 mmol / L. Place the immobilized xylanase obtained in step five into the protective agent solution diluted 5-10 times at a ratio of 1g:3-5mL, and pre-freeze at a temperature of -25 to -45℃ for 4-5 hours. S3.2 Then transfer to a vacuum freeze dryer and dry for 12 to 24 hours at a cold trap temperature of -50 to -55°C and a vacuum degree of 10 to 30 Pa to obtain immobilized xylanase dry powder. S3.3 The freeze-dried immobilized xylanase powder was stored in a sealed container at 4°C.

10. An application of a xylanase, characterized in that, The xylanase prepared according to claim 1 is applied in the field of xylooligosaccharide preparation.