A closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers and its operation method.
By constructing a closed-loop recycling metallurgical system for the industrial park based on nickel-chromium-silicon-iron element carriers, the problem of resource recycling within the stainless steel industrial park has been solved. This system enables cross-process recycling of Fe, Ni, Cr, and Si elements, improving the park's resource utilization rate and economic benefits, and meeting the requirements of green manufacturing.
Patent Information
- Application Number
- CN202611234363.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-14
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, the Ni, Cr, and Fe resources in stainless steel oxide scale within stainless steel industrial parks cannot be recycled. Solid waste from the production process needs to be transported off-site for treatment. There is a lack of collaborative recycling mechanisms within the park, resulting in a broken resource utilization chain and making it difficult to form a closed-loop metallurgical system.
By using nickel-chromium-silicon-iron element carriers, a closed-loop metallurgical system is constructed in the industrial park. Through the collection of iron oxide scale, raw material analysis and batching, production of nickel-chromium-silicon-iron, utilization of stainless steel and closed-loop circulation control, the system realizes the cross-process recycling of Fe, Ni, Cr and Si elements, breaks the linear production mode and establishes a fully closed-loop element recycling network.
It achieves efficient recycling of Fe, Ni, Cr and Si elements in stainless steel iron oxide scale, reduces dependence on external nickel and chromium sources, reduces solid waste discharge, improves the resource recycling rate of the park, enhances the benefits of the circular economy, meets green manufacturing and ESG performance indicators, and realizes closed-loop operation of material flow within the park.
Smart Images

Figure CN123108231A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of metal waste recycling technology, specifically relating to a closed-loop recycling metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers and its operation method. Background Technology
[0002] The hot rolling mills, cold rolling mills, and annealing plants in stainless steel industrial parks continuously generate large amounts of stainless steel iron oxide scale during production. This type of iron oxide scale typically contains high levels of Fe, Ni, and Cr elements, and has high resource utilization value.
[0003] Currently, the industry mainly uses the following processing methods: returning to the nickel-iron submerged arc furnace to recover nickel, direct reduction and recovery in an electric arc furnace, or direct sale to third-party companies for comprehensive utilization. The electric furnace method is divided into two types: the electric arc furnace method and the submerged arc furnace method. In the electric arc furnace method, stainless steel oxide scale is directly added to the furnace along with other furnace materials during the smelting process. After melting, a reducing agent is added to reduce the oxides, thereby obtaining a ferroalloy with a high chromium and nickel content. The biggest drawback of this electric arc furnace method is that, because the pre-reduced scale is relatively light, it basically floats on the slag surface after being added to the electric arc furnace and is difficult to enter the molten steel in a short time. The reducing agent used in the electric arc furnace is generally ferrosilicon, which is costly, and this method can only partially recover Fe from the stainless steel oxide scale, not Cr and Mn. In the submerged arc furnace method, stainless steel oxide scale is added to the furnace along with other ores and reduced with carbon; the reaction mechanism is basically the same as that of the electric arc furnace. Because electric arc furnaces rely on electroslag heating, they consume a lot of electricity and produce a large amount of slag. The chromium recovery rate in the smelting of stainless steel iron oxide scale using this method is low, the cost is high, and there is a large amount of residual chromium oxide slag in the slag. Similar to the electric arc furnace method, valuable resources such as chromium and nickel cannot be reasonably recycled and utilized.
[0004] Although the above methods can achieve partial recovery of valuable metals, the following problems still exist: (1) Ni, Cr, and Fe resources cannot be recycled within the park; (2) Solid waste resources in the production process need to be transported out for treatment; (3) There is a lack of collaborative recycling mechanism within the park; (4) The resource utilization chain is interrupted; (5) The circular economy benefits are not obvious; (6) It is difficult to form a closed-loop metallurgical system. Existing technologies mainly focus on the single recovery of Ni and Cr elements in iron oxide scale, but lack a park-level closed-loop metallurgical system that uses nickel-chromium-silicon iron as an element carrier to realize the cross-process recycling of Fe, Ni, Cr, and Si elements.
[0005] Therefore, it is necessary to develop a new closed-loop metallurgical system for industrial parks to achieve efficient recycling of resources within stainless steel industrial parks. Summary of the Invention
[0006] Addressing at least one deficiency of existing technologies, this invention aims to provide a closed-loop recycling metallurgical system for industrial parks based on a nickel-chromium-silicon-iron element carrier and its operation method. This invention innovatively proposes the concept of a nickel-chromium-silicon-iron element carrier, establishing a cross-process recycling channel for key elements such as iron, nickel, chromium, and silicon throughout the stainless steel production process. Through systematic internal resource reallocation, it achieves the recycling of elements such as iron, nickel, chromium, and silicon from stainless steel oxide scale, significantly reducing reliance on externally purchased nickel and chromium sources. This reduces solid waste discharge and resource loss at the source, effectively promoting the closed-loop operation of material flow within the production park, achieving a resource recycling rate of ≥90%.
[0007] To achieve the above objectives, the present invention adopts the following technical solution: a closed-loop metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers, comprising, in sequence, an iron oxide scale collection unit, a raw material analysis and batching unit, a nickel-chromium-silicon-iron production unit, a stainless steel utilization unit, and a closed-loop control unit. The stainless steel utilization unit is: the nickel-chromium-silicon ferrosilicon product obtained from the nickel-chromium-silicon ferrosilicon production unit is added as an element carrier to the stainless steel smelting process. The closed-loop circulation control unit is configured to: input the iron oxide scale obtained from the stainless steel utilization unit into the iron oxide scale collection unit, and then control the iron oxide scale to sequentially enter the raw material analysis and batching unit, the nickel-chromium-silicon ferrosilicon production unit, and the stainless steel utilization unit, thereby realizing the circulation of Fe, Ni, Cr, and Si elements in the metallurgical system within the park.
[0008] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-rich ferrosilicon elements described in this invention, the iron oxide scale collection unit collects stainless steel iron oxide scale generated within the industrial park by the ferrosilicon plant and stores and manages it centrally.
[0009] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-rich ferrosilicon element carriers described in this invention, the ferrosilicon plant collects stainless steel oxide scale generated within the industrial park, including stainless steel oxide scale generated by the hot rolling mill, cold rolling mill, and annealing plant.
[0010] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers described in this invention, the raw material analysis and batching unit is as follows: chemical composition analysis is performed on stainless steel iron oxide scale from different sources, and a batching model is established based on the target product composition requirements, existing raw material composition, and recovery rate of each element to determine the amount of iron oxide scale added, the iron oxide scale replacement ratio, the amount of silica added, and the amount of carbonaceous reducing agent added, and the furnace charge is prepared.
[0011] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers described in this invention, the target product requirements are: Si = 65-68%; Ni ≥ 1.5%; Cr ≥ 3.5%.
[0012] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-rich ferrosilicon element carriers described in this invention, the nickel-chromium-rich ferrosilicon production unit is: adding the furnace charge prepared in the raw material analysis and batching unit into a ferrosilicon submerged arc furnace for smelting to obtain nickel-chromium-rich ferrosilicon products.
[0013] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-rich ferrosilicon elements described in this invention, the ferrosilicon submerged arc furnace has a capacity of 36MW.
[0014] The nickel-chromium-rich ferrosilicon production unit described in this invention utilizes the strong reducing environment of a ferrosilicon submerged arc furnace to reduce Fe, Ni, and Cr elements in stainless steel oxide scale.
[0015] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-ferrosilicon element carriers described in this invention, the main components of the nickel-chromium-ferrosilicon product include: Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%; Fe: balance.
[0016] The nickel-chromium-rich ferrosilicon production unit of this invention produces a nickel-chromium-rich ferrosilicon product, which is used not only as a ferrosilicon product but also as a metallurgical element carrier for the inter-process transfer of Fe, Ni, Cr, and Si elements. The nickel-chromium-rich ferrosilicon product facilitates the transfer of elements between different production units.
[0017] As one embodiment of the closed-loop circulating metallurgical system based on nickel-chromium-ferrosilicon element carrier described in this invention, the stainless steel utilization unit is as follows: the nickel-chromium-ferrosilicon product obtained from the nickel-chromium-ferrosilicon production unit is added as an element carrier to the stainless steel smelting reduction process; wherein, the Si contained in the nickel-chromium-ferrosilicon product is used for deoxidation and alloying; Ni enters the molten steel; and Cr enters the molten steel.
[0018] The nickel-chromium-ferrosilicon (Ni-Cr) product obtained from the Ni-Cr production unit is used as an element carrier in the stainless steel smelting reduction process of the closed-loop circulating metallurgical system based on Ni-Cr ferrosilicon element carrier described in this invention has the following advantages: First, by utilizing the strong reducing properties of elemental silicon (Si) contained in the Ni-Cr ferrosilicon product, silicon alloying is completed simultaneously during the deep deoxidation process of molten steel, eliminating the need for additional ferrosilicon deoxidizer. This reduces material consumption and heat loss in traditional deoxidation processes and avoids adverse interference to the purity of molten steel from external deoxidation products. Second, the nickel (Ni) and chromium (Cr) in the carrier are directly dissolved into the molten steel matrix in a pre-alloyed form during the deoxidation process. Due to their good wettability and similar melting point to molten steel, compared with the traditional addition method of cold nickel plates and ferrochrome alloys, the melting and diffusion time is significantly shortened, reducing the energy consumption and furnace lining erosion risk during the reduction period. Third, since the nickel-chromium-rich ferrosilicon products come from secondary resources within the industrial park, the Ni and Cr elements introduced have already undergone component pre-adjustment in the initial raw material analysis and batching unit, ensuring that the furnace feed ratio precisely matches the target steel composition model. This allows for narrow-window control of the molten steel composition at the end of the reduction process, reducing rework or downgrading due to compositional deviations, thereby improving the pass rate and batch stability of stainless steel products. Fourth, this addition method enables the cross-process cycle to be substantially implemented at the critical node of smelting reduction: the deoxidation reaction product of Si (SiO2) can be captured and recovered in the subsequent slag-making process, while Ni and Cr remain permanently in the product, realizing the dual functional coupling of "deoxidizer function" and "alloying element supply." This fundamentally breaks the traditional operation mode of separate feeding for deoxidation and alloying, providing a quantifiable and closed-loop technical support for the park's closed-loop cycle. Fifth, from a system perspective, this solution reduces the consumption of purchased ferrosilicon, nickel plates, and ferrochrome simultaneously, while also reducing the carbon emissions and energy consumption inherent in the corresponding raw material mining, transportation, and pretreatment processes. While reducing raw material costs, it provides a clear accounting basis for the contribution rate of recycled elements per ton of stainless steel, meeting the rigid requirements of green manufacturing and ESG performance indicators.
[0019] As one embodiment of the closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers described in this invention, the stainless steel utilization unit includes: an AOD furnace, a VOD furnace, and an LF furnace.
[0020] This invention also claims protection for a method of operating the closed-loop circulating metallurgical system in a park based on a nickel-chromium-silicon-iron element carrier, comprising the following steps: Step S1: Collect stainless steel oxide scale generated from hot rolling mill, cold rolling mill and annealing plant; Step S2: Detect the Fe, Ni and Cr content in the stainless steel oxide scale; Step S3: Establish a formulation model based on the target product composition, existing raw material composition, and the recovery rate of each element; Step S4: Complete the furnace charge preparation according to the batching model; Step S5: Add the prepared furnace charge to the ferrosilicon submerged arc furnace; Step S6: Obtain nickel-chromium-rich ferrosilicon product; Step S7: Add nickel-chromium-rich ferrosilicon as an element carrier to the stainless steel smelting system; Step S8: Allow Ni, Cr, and Si elements to enter the molten steel; Step S9: A new stainless steel product is formed, and iron oxide scale is generated again during the production process; Step S10: The iron oxide scale generated in step S9 is returned to step S1 for iron oxide scale collection through the closed-loop circulation control unit, thereby realizing the closed-loop circulation of Fe, Ni, Cr and Si elements in the metallurgical system within the park.
[0021] As one embodiment of the operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier described in this invention, the target product composition in step S3 includes Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%.
[0022] As one embodiment of the operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier described in this invention, the Fe recovery rate, Ni recovery rate, and Cr recovery rate in the stainless steel iron oxide scale are ≥95%, ≥95%, and ≥92%, respectively.
[0023] Compared with the prior art, the present invention has the following beneficial effects: (1) The present invention provides a closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers, breaking the existing linear production mode of independent operation of each process within the industrial park, and constructing a fully closed-loop element circulation network covering ironmaking, steelmaking, and processing processes. This circulating metallurgical system introduces "nickel-chromium-silicon-iron element carriers" as cross-process media for the first time. The carrier uses stainless steel oxide scale generated within the industrial park as the substrate, and after composition adjustment and physical reconstruction, it has stable element supply activity. Based on this carrier, the present invention can realize the directional migration and metered recycling of Fe, Ni, Cr, and Si elements between smelting units (Fe recovery rate ≥95%, Ni recovery rate ≥95%, Cr recovery rate ≥92%). Specifically, by establishing a dynamic coupling relationship between the carrier addition amount and the target steel composition model, the above alloying elements can complete cross-process circulation without interfering with the main process, thereby cutting off the process-level dependence on purchased nickel-chromium raw materials in the technical path and forming a closed-loop feedback regulation mechanism.
[0024] (2) The present invention provides a closed-loop recycling metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers and its operation method, which can effectively eliminate the physical loss of alloy resources from the industrial park and control the amount of solid waste discharged to within the self-consumption threshold of the treatment system. Through the tiered reuse of internal elements, the comprehensive resource utilization rate of the industrial park reaches the theoretical upper limit of the designed closed-loop recycling, while reducing the consumption of purchased nickel and chromium sources to the minimum boundary level used only for start-up compensation. Based on the dual accounting of material flow and value flow, the present invention can significantly improve the difference in the circular economic benefits per ton of steel in the industrial park, and is naturally compatible with the current green manufacturing evaluation system and ESG management indicator requirements, and has high prospects for industrial promotion.
[0025] (3) The closed-loop recycling metallurgical system of the park based on nickel-chromium-silicon-iron element carrier of the present invention can process 3,000 tons of stainless steel iron oxide scale per month. The iron oxide scale can replace 50-100% of the iron source. The park resource recycling rate is ≥90%, and the annual comprehensive economic benefit is about US$23 million. Attached Figure Description
[0026] Figure 1 This is a schematic diagram of a closed-loop circulating metallurgical system in an industrial park based on a nickel-chromium-silicon-iron element carrier, according to an embodiment of the present invention.
[0027] Figure 2 This is a schematic diagram illustrating the circulation of Fe, Ni, Cr, and Si elements in a closed-loop circulating metallurgical system based on a nickel-chromium-silicon-iron element carrier, according to an embodiment of the present invention. Detailed Implementation
[0028] The technical solutions of the present invention will be clearly and completely described below with reference to the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0029] Unless otherwise specified, the experimental methods used in the examples and comparative examples are conventional methods, and the materials and reagents used are commercially available unless otherwise specified.
[0030] Example 1: A closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers It includes, in sequence, an iron oxide scale collection unit, a raw material analysis and batching unit, a nickel-chromium-rich ferrosilicon production unit, a stainless steel utilization unit, and a closed-loop circulation control unit.
[0031] The iron oxide scale collection unit collects stainless steel iron oxide scale generated within the ferrosilicon plant's collection park and stores and manages it centrally.
[0032] The ferrosilicon plant collects stainless steel oxide scale generated within the industrial park, including stainless steel oxide scale generated by the hot rolling mill, cold rolling mill, and annealing mill.
[0033] The raw material analysis and batching unit is as follows: chemical composition analysis is performed on stainless steel iron oxide scale from different sources, and a batching model is established based on the target product composition requirements (Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%), existing raw material composition, and recovery rate of each element to determine the amount of iron oxide scale added, the iron oxide scale replacement ratio, the amount of silica added, and the amount of carbonaceous reducing agent added to prepare the furnace charge.
[0034] The nickel-chromium-rich ferrosilicon production unit is as follows: the furnace charge prepared in the raw material analysis and batching unit is added to the ferrosilicon submerged arc furnace for smelting to obtain nickel-chromium-rich ferrosilicon products.
[0035] The main components of the nickel-chromium-rich ferrosilicon product include: Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%; Fe: balance.
[0036] The specifications of the ferrosilicon submerged arc furnace are 36MW.
[0037] In this embodiment, the nickel-chromium-rich ferrosilicon production unit utilizes the strong reducing environment of a ferrosilicon submerged arc furnace to reduce Fe, Ni, and Cr elements in stainless steel oxide scale.
[0038] The nickel-chromium-rich ferrosilicon production unit described in this embodiment produces a nickel-chromium-rich ferrosilicon product, which is used not only as a ferrosilicon product but also as a metallurgical element carrier for the inter-process transfer of Fe, Ni, Cr, and Si elements. The nickel-chromium-rich ferrosilicon product facilitates the transfer of elements between different production units.
[0039] The stainless steel utilization unit is as follows: the obtained nickel-chromium-rich ferrosilicon product is added as an element carrier to the stainless steel smelting reduction process; wherein, the Si contained in the nickel-chromium-rich ferrosilicon product is used for deoxidation and alloying; Ni enters the molten steel; and Cr enters the molten steel.
[0040] The stainless steel utilization unit includes: AOD furnace, VOD furnace, and LF furnace.
[0041] The closed-loop circulation control unit works as follows: Iron oxide scale obtained from the stainless steel utilization unit is transported to the iron oxide scale collection unit. The scale then re-enters the raw material analysis and batching unit for Fe, Ni, and Cr content detection. Based on the target product composition (Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%), existing raw material composition, and the recovery rate of each element, a batching model is established to determine the amount of iron oxide scale added, the iron oxide scale replacement ratio, the amount of silica added, and the amount of carbonaceous reducing agent added for furnace charge preparation. The prepared furnace charge enters the nickel-chromium-rich ferrosilicon production unit for nickel-chromium-rich ferrosilicon product production. The resulting nickel-chromium-rich ferrosilicon product enters the stainless steel utilization unit to prepare new stainless steel products. The obtained iron oxide scale is then recycled again through the closed-loop circulation control unit, achieving a closed-loop circulation of Fe, Ni, Cr, and Si elements within the metallurgical system within the industrial park.
[0042] Example 2: An operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier. Step S1: Collect stainless steel oxide scale generated from hot rolling mill, cold rolling mill and annealing plant; Step S2: Detect the Fe, Ni and Cr content in the stainless steel oxide scale (Fe: 55-60%, Ni: 3-5%, Cr: 7-8%). Step S3: Based on the target product composition, existing raw material composition, and the recovery rate of each element, establish a formulation model; Step S4: Based on the batching model, complete the furnace charge preparation, with the following batch ratio: silica 600kg, stainless steel iron oxide scale 145-155kg, semi-coke 370-380kg. Step S5: Add the prepared furnace charge to the ferrosilicon submerged arc furnace; Step S6: Obtain nickel-chromium-rich ferrosilicon product; Step S7: Add nickel-chromium-rich ferrosilicon as an element carrier to the stainless steel smelting system; Step S8: Allow Ni, Cr, and Si elements to enter the molten steel; Step S9: A new stainless steel product is formed, and iron oxide scale is generated again during the production process; Step S10: The iron oxide scale generated in step S9 is returned to step S1 for iron oxide scale collection through the closed-loop circulation control unit, thereby realizing the closed-loop circulation of Fe, Ni, Cr and Si elements in the metallurgical system within the park.
[0043] The target product composition in step S3 includes Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%.
[0044] In the operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier, the Fe recovery rate in stainless steel iron oxide scale is ≥95%, the Ni recovery rate is ≥95%, and the Cr recovery rate is ≥92%.
[0045] The above embodiments are merely illustrative of the principles and effects of the present invention and are not intended to limit the invention. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in the present invention should still be covered by the claims of the present invention.
Claims
1. A park closed circuit metallurgical system based on a rich nickel-chromium-silicon-iron elemental carrier, characterized by, It includes, in sequence, an iron oxide scale collection unit, a raw material analysis and batching unit, a nickel-chromium-rich ferrosilicon production unit, a stainless steel utilization unit, and a closed-loop circulation control unit; The stainless steel utilization unit is: the nickel-chromium-silicon ferrosilicon product obtained from the nickel-chromium-silicon ferrosilicon production unit is added as an element carrier to the stainless steel smelting process. The closed-loop circulation control unit is configured to: input the iron oxide scale obtained from the stainless steel utilization unit into the iron oxide scale collection unit, and then control the iron oxide scale to sequentially enter the raw material analysis and batching unit, the nickel-chromium-silicon ferrosilicon production unit, and the stainless steel utilization unit, thereby realizing the circulation of Fe, Ni, Cr, and Si elements in the metallurgical system within the park.
2. The closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers as described in claim 1, characterized in that, The iron oxide scale collection unit collects stainless steel iron oxide scale generated within the ferrosilicon plant's collection park and stores and manages it centrally.
3. The closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers as described in claim 1, characterized in that, The raw material analysis and batching unit is as follows: chemical composition analysis is performed on stainless steel iron oxide scale from different sources, and a batching model is established based on the target product composition requirements, existing raw material composition, and recovery rate of each element to determine the amount of iron oxide scale added, the iron oxide scale replacement ratio, the amount of silica added, and the amount of carbonaceous reducing agent added, and to prepare the furnace charge.
4. The closed loop campus metallurgical system based on a ferronickelsilicon iron rich elemental carrier according to claim 1, wherein, The nickel-chromium-rich ferrosilicon production unit is as follows: the furnace charge prepared in the raw material analysis and batching unit is added to the ferrosilicon submerged arc furnace for smelting to obtain nickel-chromium-rich ferrosilicon products.
5. The closed-loop circulating metallurgical system for industrial parks based on nickel-chromium-silicon-iron element carriers as described in claim 4, characterized in that... The main components of the nickel-chromium-rich ferrosilicon product include: Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%; Fe: balance; The specifications of the ferrosilicon submerged arc furnace are 36MW.
6. The closed loop campus metallurgical system based on a ferronickelsilicon iron rich elemental carrier according to claim 1, wherein, The stainless steel utilization unit includes: AOD furnace, VOD furnace, and LF furnace.
7. A method of operating a closed-loop metallurgical system for a park based on a ferro-nickel-chromium-silicon element carrier according to any one of claims 1 to 6, characterized in that, Includes the following steps: Step S1: Collect stainless steel oxide scale generated from hot rolling mill, cold rolling mill and annealing plant; Step S2: Detect the Fe, Ni and Cr content in the stainless steel oxide scale; Step S3: Based on the target product composition, existing raw material composition, and the recovery rate of each element, establish a formulation model; Step S4: Complete the furnace charge preparation according to the batching model; Step S5: Add the prepared furnace charge to the ferrosilicon submerged arc furnace; Step S6: Obtain nickel-chromium-rich ferrosilicon product; Step S7: Add nickel-chromium-rich ferrosilicon as an element carrier to the stainless steel smelting system; Step S8: Allow Ni, Cr, and Si elements to enter the molten steel; Step S9: A new stainless steel product is formed, and iron oxide scale is generated again during the production process; Step S10: The iron oxide scale generated in step S9 is returned to step S1 for iron oxide scale collection through the closed-loop circulation control unit, realizing the circulation of Fe, Ni, Cr and Si elements in the metallurgical system within the park.
8. The operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier as described in claim 7, characterized in that, The target product composition mentioned in step S3 includes Si: 65-68%; Ni: ≥1.5%; Cr: ≥3.5%.
9. The operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier as described in claim 7, characterized in that, In the operation method of the closed-loop circulating metallurgical system in the industrial park based on nickel-chromium-silicon-iron element carrier, the Fe recovery rate in stainless steel iron oxide scale is ≥95%, the Ni recovery rate is ≥95%, and the Cr recovery rate is ≥92%.