Substrate processing methods
By using a combination of oligomeric metal-oxygen bond precursor compounds and oxygen reactant compounds, the problem of gap filling in semiconductor devices was solved, enabling the deposition of metal oxide layers without gaps or voids, thus improving the filling effect.
Patent Information
- Application Number
- CN202610637504.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-14
- Filing Date
- 2026-05-11
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies struggle to effectively fill gap features in semiconductor devices, especially as feature sizes decrease and complexity increases, leading to difficulties in conformal gap filling and seamless or void filling.
A combination of metal-oxygen bond precursor compounds in oligomeric form and oxygen reactant compounds is used to decompose the compounds and allow them to migrate into vertical and horizontal gaps by heating the substrate and providing pulsed compounds in the reaction chamber, forming a substantially seamless metal oxide layer.
It achieves seamless filling of vertical and horizontal gaps, improves the shape retention and filling effect of gap filling, and reduces the formation of gaps or voids.
Smart Images

Figure CN123108527A_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to methods for forming semiconductor structures, and more particularly, to methods for filling gap features on a substrate. Background Technology
[0002] Semiconductor devices typically include patterned features for forming (e.g., 3D) transistors, stripes, gate-around transistors, etc. During the formation of such devices, it is generally desirable to fill the gaps within or between various features. As feature sizes on the substrate decrease and / or feature complexity increases, filling these gaps with materials possessing the desired properties can become increasingly difficult.
[0003] Various profile control methods exist in gap-filling techniques. Common gap-filling techniques include depositing materials using chemical vapor deposition (CVD) or atomic layer deposition (ALD) processes. While some techniques work well for certain applications, achieving the desired shape-preserving gap filling and / or gap-free or void-free gap filling can be challenging. Therefore, improved gap-filling methods are often needed.
[0004] Any discussion of problems and solutions is included in this disclosure for the purpose of providing context for this disclosure only, and should not be construed as an admission that any or all of the discussions were known at the time of making this disclosure. Summary of the Invention
[0005] This synopsis is provided to introduce some concepts in a simplified form. These concepts are further described in detail in the following detailed description of exemplary embodiments of this disclosure. This synopsis is not intended to identify key or essential features of the claimed subject matter, nor is it intended to limit the scope of the claimed subject matter.
[0006] According to various embodiments of the present disclosure, a method is provided, the method comprising: providing a substrate into a reaction chamber, the substrate including a vertical gap and a horizontal gap; heating the substrate within the reaction chamber; providing a first precursor compound comprising a metal-oxygen bond, the first precursor compound being in the form of an oligomer; and providing a reactant compound into the reaction chamber, the reactant compound comprising oxygen, heating the substrate causing the oligomer to decompose into a decomposed compound and causing the decomposed compound to migrate into the vertical gap and the horizontal gap, the decomposed compound comprising a metal-oxygen bond.
[0007] In some embodiments, the method further includes forming a metal oxide layer on a substrate.
[0008] In some embodiments, the metal oxide layer is substantially seamless.
[0009] In some embodiments, the metal element of the metal oxide layer includes at least one of aluminum, titanium, zirconium, or tantalum.
[0010] In some embodiments, the first precursor compound has M x R y The chemical formula of (OR')z, where M is a metal, y+z=3x, and x is the number of units in the oligomer.
[0011] In some embodiments, the first precursor compound comprises aluminum dimethylisopropoxide, and the aluminum dimethylisopropoxide is in dimer form prior to decomposition.
[0012] In some embodiments, the metal oxide layer comprises aluminum oxide.
[0013] In some embodiments, the first precursor compound further includes an alkyl group bonded to oxygen.
[0014] In some embodiments, the migration of the decomposed compounds into the horizontal gap occurs at least partially via molecular flow.
[0015] In some embodiments, the substrate is heated to a temperature greater than 250°C during the heating step.
[0016] In some embodiments, the substrate is heated to a temperature between 250°C and 400°C during the heating step.
[0017] According to various embodiments of the present disclosure, a method is provided comprising: heating a substrate in a reaction chamber, the substrate including a vertical gap and a horizontal gap; pulse a first precursor compound into the reaction chamber, the first precursor compound comprising a metal-oxygen bond and being in the form of an oligomer, the heating of the substrate comprising heating to a temperature above the decomposition temperature of the oligomer to form a decomposed compound; pulse a reactant compound into the reaction chamber, the reactant compound comprising oxygen, the decomposition of the oligomer into the decomposed compound causing the decomposed compound to migrate into the vertical gap and the horizontal gap; and forming a substantially seamless metal oxide layer on the substrate.
[0018] In some embodiments, the first precursor compound further includes an alkyl group bonded to oxygen.
[0019] In some embodiments, the metal element of the metal oxide layer includes at least one of aluminum, titanium, zirconium, or tantalum.
[0020] In some embodiments, the first precursor compound includes aluminum dimethylisopropoxide.
[0021] In some embodiments, the reactant compound includes water.
[0022] In some embodiments, heating the substrate includes heating the substrate to a temperature greater than 250°C.
[0023] According to various embodiments of the present disclosure, a method is provided comprising: heating a substrate in a reaction chamber to a temperature greater than 250°C, the substrate including a vertical gap and a horizontal gap; providing a first precursor compound into the reaction chamber, the first precursor compound comprising a metal-oxygen bond and being in the form of an oligomer; providing a reactant compound into the reaction chamber, the reactant compound comprising water; forming a flowable compound comprising a metal hydroxide and a metal-oxygen bond in response to providing the reactant compound, the flowable compound migrating into the vertical gap and the horizontal gap; and forming a substantially seamless metal oxide layer on the substrate.
[0024] In some embodiments, the oligomer decomposes into a decomposed compound in response to contact of a first precursor compound with a heated substrate.
[0025] In some embodiments, the first precursor compound includes aluminum dimethylisopropoxide.
[0026] For the purpose of outlining this disclosure and the advantages achieved relative to the prior art, certain objects and advantages of this disclosure have been described above. It should be understood, of course, that not all of these objects or advantages may necessarily be achieved according to any particular example of this disclosure. Therefore, for example, those skilled in the art will recognize that the examples disclosed herein may be implemented in a way that achieves or optimizes one or more advantages taught or suggested herein, without necessarily achieving other objects or advantages that may be taught or suggested herein.
[0027] All these examples are intended to fall within the scope of this disclosure. These and other examples will become apparent to those skilled in the art from the following detailed description of certain examples with reference to the accompanying drawings, and the content of this disclosure is not limited to any particular example discussed. Attached Figure Description
[0028] Although the specification concludes with claims, which specifically point out and explicitly claim protection for what is considered an example of this disclosure, the advantages of the embodiments of the invention can be more readily determined from the description of particular examples when read in conjunction with the accompanying drawings. In all the drawings, elements with the same element numbers are intended to be identical.
[0029] Figure 1 These are schematic diagrams of exemplary reactor systems based on various examples.
[0030] Figure 2A These are schematic diagrams of semiconductor structures based on various examples.
[0031] Figure 2B It is based on various examples Figure 2A A close-up view of a portion of a semiconductor structure.
[0032] Figure 3AThis is a schematic diagram of another semiconductor structure based on various examples.
[0033] Figure 3B It is based on various examples Figure 3A A close-up view of a portion of a semiconductor structure.
[0034] Figure 4A This is a schematic diagram of another semiconductor structure based on various examples.
[0035] Figure 4B It is based on various examples Figure 4A A close-up view of a portion of a semiconductor structure.
[0036] Figure 5 Methods for depositing materials on substrates according to various examples are described.
[0037] It should be understood that the elements in the accompanying drawings are shown for simplicity and clarity and are not necessarily drawn to scale. For example, the dimensions of some elements may be exaggerated relative to other elements to aid in understanding the embodiments shown in this disclosure. Detailed Implementation
[0038] The descriptions of the methods, structures, apparatuses, and systems provided below are merely exemplary and intended for illustrative purposes only. The following descriptions are not intended to limit the scope of this disclosure or the claims. Furthermore, the recitation of multiple examples having the described features is not intended to exclude other examples having additional features or other examples comprising different combinations of the described features. For example, various examples are set forth as embodiments and may be recited in the dependent claims. Unless otherwise stated, examples or components thereof may be combined or may be applied separately from each other. Methods may include the disclosed steps in any suitable and / or desired order or combination. The illustrations presented herein are not intended to be actual views of any particular material, apparatus, structure, or device, but are merely representations for illustrating examples of this disclosure.
[0039] As used herein, the term “and / or” includes any and all combinations of one or more of the associated listed items. Unless otherwise stated, expressions such as “at least one of…” modify the entire column of elements when following an element in the column, and not necessarily a single element in the column.
[0040] As used herein, the terms “comprising,” “including,” and variations thereof specify the presence of the stated feature, integer, step, process, component, part, and / or group thereof, and do not exclude the presence or addition of one or more other features, integers, steps, processes, components, parts, and / or groups thereof. In this disclosure, the meaning of any definition does not necessarily exclude the common and customary meanings in some examples.
[0041] As used herein, the term "substrate" can refer to any one or more underlying materials, including any one or more underlying materials that can be modified or on which devices, circuits, or films or layers can be formed. A "substrate" can be continuous or discontinuous; rigid or flexible; solid or porous; and combinations thereof. A substrate can be in any form, such as powder, plate, or workpiece. Plate-type substrates can include wafers of various shapes and sizes. Substrates can be made of semiconductor materials, including, for example, silicon, silicon germanium, silicon oxide, gallium arsenide, gallium nitride, and / or silicon carbide.
[0042] As used herein, the term "atomic layer deposition" (ALD) can refer to a vapor deposition process in which deposition cycles, preferably multiple consecutive cycles, are performed in a processing chamber. Typically, during each cycle, a precursor is chemisorbed onto the deposition surface (e.g., a substrate surface or a previously deposited lower layer surface, such as material from a previous ALD cycle), forming a monolayer or sub-monolayer that is not readily reactive with another precursor (i.e., a self-limiting reaction). Subsequently, if desired, a reactant (e.g., another precursor or reactive gas) can be introduced into the processing chamber to convert the chemisorbed precursor into the desired material on the deposition surface. Typically, the reactant is capable of further reacting with the precursor. Furthermore, a purging step can be used during each cycle to remove excess precursor from the processing chamber and / or excess reactant and / or reaction byproducts from the processing chamber after the conversion of the chemisorbed precursor. Additionally, as used herein, the term "atomic layer deposition" is also intended to include processes specified by related terms such as "chemical vapor deposition" when performed with alternating pulses of a precursor composition, a reactive gas, and a purging gas (e.g., an inert carrier gas).
[0043] As used herein, the term “chemical vapor deposition” (CVD) can refer to any process in which a substrate is exposed to one or more precursors, which react and / or decompose on the substrate surface to produce the desired deposition.
[0044] In some examples, "film" refers to a layer extending in a direction perpendicular to the thickness direction. In some examples, "layer" refers to a material of a certain thickness formed on a surface, and can be synonymous with a film or non-film structure. A film or layer can consist of discrete single films or layers or multiple films or layers with certain properties, and the boundaries between adjacent films or layers may or may not be clear, and may or may not be based on the physical, chemical and / or any other properties, formation processes or sequences and / or functions or purposes of adjacent films or layers. A layer or film can be continuous or discontinuous. Furthermore, a single film or layer can be formed using one or more deposition cycles and / or one or more deposition and processing cycles.
[0045] As used herein, "precursor" can refer to a compound that participates in a chemical reaction to form another compound or element, wherein a portion of the precursor (an element or group within the precursor) is incorporated into the compound or element produced by the chemical reaction. The compound or element produced by the chemical reaction can be a layer and / or film formed on a substrate surface.
[0046] As used in this article, "reactant" can refer to a compound that participates in a chemical reaction to form another compound or element. In some cases, reactants can be precursors.
[0047] In this disclosure, any two numbers of a variable may constitute a feasible range of the variable, and any range indicated may include or exclude endpoints, and may combine all ranges and ratio limits disclosed herein. Furthermore, any value of the indicated variable (whether or not it is indicated by “about”) may refer to an exact value or an approximate value and include equivalents, and in some examples may refer to the mean, median, representative value, multi-value, etc. (e.g., “about” may refer to ±10% of the subject value). Unless otherwise specified, references to “a,” “an,” and / or “the” may include one or more, and references to singular items may also include plural items. When referring to components of the system discussed herein, the term “connection” means a direct connection or an indirect connection with other intermediate elements, as appropriate. Unless otherwise stated, the terms “first,” “second,” etc., and / or “primary,” “secondary,” etc., are used herein merely as labels and are not intended to impose any order, position, or hierarchy requirements on the items referred to by these terms. Furthermore, references to items such as “second” do not require or exclude the existence of items such as “first” or lower numbered items and / or items such as “third” or higher numbered items. Furthermore, references to items such as "first" and "second" do not imply the absence of intermediate items, and such intermediate items may exist.
[0048] Reactor systems used for ALD, CVD, etc., can be used in a variety of applications, including depositing and etching materials on substrate surfaces. In various examples, see references... Figure 1 The reactor system 50 may include a reaction chamber 4, a base 6 for holding the substrate 30 during processing, a fluid distribution system 8 (e.g., a spray head) for dispensing one or more reactants and / or precursors to the surface of the substrate 30, and one or more reactant sources 10, 12 and / or carrier gas and / or purge gas sources 14, which are fluidly coupled to the reaction chamber 4 via lines 16-20 and / or valves or controllers 22-26. The system 50 may also include a vacuum source 28 fluidly coupled to the reaction chamber 4. A sealing member 29 may separate (e.g., at least partially fluidly separate) a portion of the volume within the reaction chamber 4.
[0049] Figure 2A and Figure 2BA schematic diagram depicting a portion of a semiconductor structure 200 is shown. The semiconductor structure 200 includes a substrate 210 and a material 220 disposed therein and thereon. The substrate 210 may include vertical pillars 212 and / or horizontal strips 214. The substrate 210 may include recesses or vertical gaps 230 (e.g., vertically located between the vertical pillars 212 and / or horizontal strips 214). The substrate 210 may include horizontal gaps 240 between the strips 214.
[0050] The vertical gap 230 and the horizontal gap 240 can have any suitable dimensions. For example, the vertical gap 230 can have a dimension (e.g., width or thickness) 233 of 10-30 nanometers (nm), 10-20 nm, or 15-20 nm. As another example, the horizontal gap 240 can have a dimension (e.g., height or thickness) 243 of 5-20 nm, 5-15 nm, or about 5 or 10 nm (e.g., the horizontal gap 240 can have a dimension 243 of about 10 nm, or a dimension 246 of about 5 or 6 nm). In this context, "about" means ±1, 2, or 3 nm. The vertical gap 230 and the horizontal gap 240 can include any suitable aspect ratio. For example, the vertical gap 230 can have an aspect ratio ranging from 7:1 to 12:1, and / or the horizontal gap 240 can have an aspect ratio ranging from 2:1 to 5:1.
[0051] In various examples, material 220 may be deposited in the vertical pillars 212 and / or strips 214 in response to a deposition process. Material 220 may include a metal oxide. The metal oxide may include any suitable material and / or compound, such as alumina, tantalum oxide, zirconium oxide, and / or titanium oxide, any of which may or may not be stoichiometric. Cracks and / or voids 229 may be formed in material 220 during deposition. For example, a substantially conformal process may result in material 220 being deposited on defects in the substrate 210 and / or accumulating at various locations, resulting in regional pinching of material 220 to form voids 229. Deposition processes performed at relatively low temperatures (e.g., below 250°C or below 200°C) may result in such deposition of material 220 and voids 229.
[0052] Cracks or voids 229 may be undesirable, and therefore a deposition process that forms a structure without cracks or voids (i.e., seamless and / or void-free) may be desirable. In various examples, Figure 5 A method 500 for depositing material on a substrate is described. See also: Figure 3A and Figure 3B The substrate 210 can be provided (step 502) to the reaction chamber (e.g. Figure 1In reaction chamber 4). As discussed herein, substrate 210 may include features (vertical pillars 212 and / or horizontal bands 214) having gap features therebetween (e.g., vertical gaps 230 and / or horizontal gaps 240). Substrate 210 may be heated (step 504). Heating of substrate 210 may occur during and / or while preparing to provide precursor / reactant and / or forming material 220. Substrate 210 may be heated to any suitable temperature, such as temperatures in the range of 100°C to 400°C, 200°C or higher and / or 250°C or higher, or temperatures in the range of 250-400°C or 250-300°C.
[0053] A first precursor compound may be supplied to the reaction chamber (step 506). The first precursor compound may be pulsed from a precursor source and contact the substrate 210. The first precursor compound may travel downwards along the vertical gap 230 and into the horizontal gap 240. In various examples, the first precursor compound may comprise a metal oxide precursor. In various examples, the first precursor compound may comprise a metal-oxygen bond. The metal in the first precursor compound may comprise metals from Groups 2 to 15 of the periodic table, such as aluminum, zirconium, titanium, and / or tantalum. In various examples, the first precursor compound may comprise an alkyl group coupled / bonded to an oxygen atom.
[0054] The first precursor compound may be present and / or provided as an oligomer (as used herein, "oligomer" includes dimers, trimers, tetramers, and any other compound containing repeating units (i.e., units that are themselves considered monomers). For example, the first precursor compound may be present as a dimer or a trimer.
[0055] In various examples, the first precursor compound can be a compound with the chemical formula M. x R y (OR') z The compound, wherein M is a metal (e.g., the example discussed herein), wherein y + z = 3x, and wherein x is the number of units in the oligomer, i.e., x = 1 is a monomer, x = 2 is a dimer, x = 3 is a trimer, x = 4 is a tetramer, etc. For example, x can be 2, y can be 4, and / or z can be 2. R can be any alkyl group containing 1-6 carbon atoms. For example, R can contain methyl, ethyl, isopropyl, isobutyl, and / or tert-butyl. R' can be any alkyl group containing 1-8 carbon atoms or any aryl group containing a benzene ring and optionally containing an alkyl group attached to the ring. For example, R' can include methyl, ethyl, isopropyl, tert-butyl, and / or phenyl.
[0056] In various examples, the first precursor compound may include aluminum dimethylisopropoxide, aluminum diethylisopropoxide, aluminum diisobutylisopropoxide, aluminum di-tert-butylisopropoxide, aluminum dimethylmethoxide, aluminum diethylmethoxide, aluminum diisobutylmethoxide, aluminum di-tert-butylmethoxide, aluminum dimethylethoxide, aluminum diethylethoxide, aluminum diisobutylethoxide, aluminum di-tert-butylethoxide, aluminum dimethyl-tert-butoxide, aluminum diethyl-tert-butoxide, aluminum diisobutyl-tert-butoxide, aluminum dimethyl-sec-butoxide, aluminum diethyl-sec-butoxide, aluminum diisobutyl-sec-butoxide, aluminum di-tert-butyl-sec-butoxide, aluminum dimethyl-tert-pentanol, aluminum diethyl-tert-pentanol, aluminum diisobutyl-tert-pentanol, and / or aluminum di-tert-butyl-tert-pentanol. Compounds corresponding to the foregoing can also be conceived that include zirconium, titanium, tantalum, hafnium, and / or gallium, for example, replacing aluminum atoms.
[0057] The first precursor compound may be provided for any suitable pulse duration. For example, the first precursor compound may be provided for any duration of pulse (each time the first precursor compound is provided) of 0.1 to 10 seconds, 1 to 10 seconds, 0.1 to 0.5 seconds, 0.5 to 1 second, 1 to 3 seconds, etc.
[0058] In various examples, a reactant compound may be provided to the reaction chamber (step 508). The reactant compound may contain oxygen. For example, the reactant compound may include water (H2O), alcohols (e.g., methanol, ethanol, isopropanol and / or tert-butanol) and / or aldehydes (e.g., formaldehyde, acetaldehyde, propionaldehyde, butyraldehyde and / or neopentaldehyde).
[0059] The reactant compound may be provided for any suitable pulse duration. For example, the reactant compound may be provided for any duration of pulse (each time the reactant compound is provided), such as 0.1 to 10 seconds, 1 to 10 seconds, 0.1 to 0.5 seconds, 0.5 to 1 second, 1 to 3 seconds, etc.
[0060] After each pulse of the first precursor compound and / or reactant compound, a purging step may be present, wherein the reaction chamber is purged with a purging gas (e.g., a non-reactive and / or inert gas, such as nitrogen, helium, argon, krypton, xenon, etc.). For example, a purging step may be present after step 506, and a purging step may be present after step 508. During the purging step, the purging gas may be supplied from purging gas source 14 to reaction chamber 4. Figure 1 (As shown). The purge gas can be provided (e.g., pulsed) for any suitable duration, such as any duration of 0.1 to 10 seconds, 1 to 10 seconds, 0.1 to 0.5 seconds, 0.5 to 1 second, 1 to 3 seconds, etc.
[0061] In various examples, a flowable compound can be formed (step 510) in response to heating the substrate 210 (step 504), providing a first precursor compound (step 506), and / or providing a reactant compound (step 508). For example, in response to heating the substrate 210 with the first precursor compound, oligomers of the first precursor compound can at least partially decompose into smaller oligomers (e.g., trimers to dimers) or decompose into monomers. Therefore, step 504 may include heating the substrate 210 to a temperature above the decomposition temperature of the corresponding first precursor compound. For example, the decomposition temperature may include temperatures in the range of 100°C to 400°C, 200°C or higher and / or 250°C or higher, or temperatures in the range of 250-400°C or 250-300°C. As another example, for a first precursor compound containing aluminum dimethylisopropoxide (which may be in dimer form), the aluminum dimethylisopropoxide dimer may decompose into monomers at temperatures of about 250°C or above, about 280°C or above, or about 300°C or above (“about” may mean ±20°C or as otherwise defined herein). In response, the decomposed compound (e.g., the monomeric aluminum dimethylisopropoxide) may selectively migrate into vertical gaps 230 and / or horizontal gaps 240. For example, the decomposed compound may selectively migrate into relatively smaller gaps (e.g., horizontal gaps 240) before filling relatively larger gaps (e.g., vertical gaps 230). Not bound by theory, this migration can occur because the decomposed compound can be smaller, thus allowing for greater mobility within smaller horizontal gaps 240, and / or because the flow of the decomposed compound can at least partially become a molecular flow (as opposed to a viscous flow). In the horizontal gap 240, the high surface area to volume ratio promotes a high probability (or guaranteed, i.e., 100%) of interaction between the decomposed compound and the surface of the substrate 210. Therefore, the interaction between the decomposed compound and the surface can be high-energy, promoting the preferential flow of the decomposed compound into the horizontal gap 240 (e.g., through capillary action).
[0062] In various examples, the first precursor compound (in its oligomeric form) can form larger oligomers (with a larger unit number) prior to the decomposition discussed herein. For example, the monomer and / or oligomer can react in the gas or liquid phase, and / or on the surface of a substrate, to produce larger oligomers (i.e., oligomer formation). Such product oligomers may contain flowable and / or gap-filling properties. As another example, a dimer of aluminum dimethylisopropoxide (formula Al2(OiPr)2Me4) can react with a monomer of aluminum dimethylisopropoxide (formula Al(OiPr)Me2) to form its trimer (formula Al3(OiPr)3Me6). The trimer can further react with other monomeric or dimer substances to form larger oligomers, some of which may have properties that enhance flowability and / or gap-filling (e.g., vapor pressure, molecular weight, ability to undergo crosslinking reactions).
[0063] As another example of forming a flowable compound (step 510), without being bound by theory, a first precursor compound and a reactant compound (e.g., water) can form a sol-gel in the vertical gap 230 and / or the horizontal gap 240. The sol-gel may comprise a metal hydroxide (e.g., aluminum hydroxide) matrix, which can be formed from water molecules remaining and / or retained in the substrate 210. The flowable compound (e.g., comprising a sol-gel) can preferentially flow into the vertical gap 230 and / or the horizontal gap 240. In various examples, the flowable compound can flow into the vertical gap 230 and then preferentially into the horizontal gap 240, thereby filling the horizontal gap 240 without gaps or voids before further deposition onto the surface and / or area / volume of the vertical gap 230. This can facilitate seamless / void-free filling of the horizontal gap (e.g., as shown in the image). Figure 3A and Figure 3B (The horizontal gap 240 in structure 300 is shown).
[0064] In response to the migration of the first precursor compound and / or any resulting compound (e.g., decomposed compound and / or sol-gel) into the vertical gap 230 and / or horizontal gap 240, a metal oxide layer can be formed (step 510). (The metal oxide layer is...) Figures 3A to 4B The material 220 in the structure. The compound within the vertical gap 230 and / or horizontal gap 240 can be further decomposed into a metal oxide layer, for example by heat provided by the heated substrate 210. For example, the decomposed compound (e.g., a monomer of the first precursor compound) can be further decomposed (e.g., cleaving metal-carbon bonds within such a compound) to form a metal oxide, and / or a sol-gel containing a matrix containing a metal hydroxide can further decompose the metal hydroxide into a metal oxide.
[0065] In various examples, it may not be necessary to provide an oxygen-containing reactant compound to form the metal oxide layer (i.e., step 508 may be appropriately omitted). According to the examples discussed herein, the first oxygen-containing precursor compound may provide sufficient oxygen (co-reactant) to promote the formation of the metal oxide layer.
[0066] The steps of method 500 can be repeated in any suitable order and / or number in any combination to achieve the desired metal oxide layer on substrate 210. For example, horizontal gaps 240 can be filled and a film can be formed in vertical gaps 230 (e.g., vertical gaps 230 can be left unfilled), for example... Figure 3A The structure is 300. To also fill the vertical gap 230, such as... Figure 4A As shown in structure 400, the steps of method 500 can be repeated to form a metal oxide layer. The metal oxide layer can be formed without gaps or voids, as shown in the seamless horizontal gap filling of structure 300 (and its close-up view 390) and the seamless vertical gap filling 425 of structure 400 (and its close-up view 490).
[0067] The examples given above in this disclosure do not limit the scope of the claimed subject matter, as they are merely examples. The invention is defined by the appended claims and their legal equivalents. Any equivalent embodiments are intended to fall within the scope of this disclosure. In fact, various modifications to this disclosure, such as alternative useful combinations of the described elements, in addition to those shown and described herein, will become apparent to those skilled in the art from the description. These modifications and embodiments are also intended to fall within the scope of the appended claims.
Claims
1. A method comprising: A substrate is provided into the reaction chamber, wherein the substrate includes a vertical gap and a horizontal gap; The substrate is heated within the reaction chamber; Provided a first precursor compound comprising a metal-oxygen bond, wherein the first precursor compound is in the form of an oligomer; and A reactant compound, containing oxygen, is supplied to the reaction chamber. In this process, heating the substrate causes the oligomer to decompose into decomposed compounds, and the decomposed compounds migrate into the vertical and horizontal gaps, wherein the decomposed compounds contain metal-oxygen bonds.
2. The method according to claim 1, further comprising forming a metal oxide layer on the substrate.
3. The method according to claim 2, wherein, The metal oxide layer is essentially seamless.
4. The method according to claim 3, wherein, The metal element in the metal oxide layer includes at least one of aluminum, titanium, zirconium, or tantalum.
5. The method according to claim 4, wherein, The first precursor compound has M x R y (OR') z The chemical formula of , where M is a metal, where y+z=3x, and where x is the number of units in the oligomer.
6. The method according to claim 5, wherein, The first precursor compound includes aluminum dimethylisopropoxide, wherein the aluminum dimethylisopropoxide is in dimer form prior to the decomposition.
7. The method according to claim 6, wherein, The metal oxide layer includes aluminum oxide.
8. The method according to claim 4, wherein, The first precursor compound further comprises an alkyl group bonded to the oxygen.
9. The method according to claim 1, wherein, The decomposed compounds migrate into the horizontal gap, at least in part, via molecular flow.
10. The method according to claim 1, wherein, The substrate is heated to a temperature greater than 250°C during the heating step.
11. The method according to claim 10, wherein, During the heating step, the substrate is heated to a temperature between 250°C and 400°C.
12. A method comprising: A substrate is heated in a reaction chamber, the substrate comprising a vertical gap and a horizontal gap; A first precursor compound is pulsed into a reaction chamber, wherein the first precursor compound contains a metal-oxygen bond, and wherein the first precursor compound is in the form of an oligomer, wherein the heating substrate comprises heating to a temperature above the decomposition temperature of the oligomer to form a decomposed compound; The reactant compound, which contains oxygen, is pulsed into the reaction chamber. Among these, the decomposition of oligomers into compounds leads to the migration of these compounds into both vertical and horizontal gaps; and A substantially seamless metal oxide layer is formed on the substrate.
13. The method according to claim 12, wherein, The first precursor compound further comprises an alkyl group bonded to the oxygen.
14. The method according to claim 13, wherein, The metal element in the metal oxide layer includes at least one of aluminum, titanium, zirconium, or tantalum.
15. The method according to claim 14, wherein, The first precursor compound includes dimethylaluminum isopropoxide.
16. The method according to claim 12, wherein, The reactant compounds include water.
17. The method according to claim 12, wherein, Heating the substrate includes heating the substrate to a temperature greater than 250°C.
18. A method comprising: The substrate in the reaction chamber is heated to a temperature greater than 250°C. The substrate includes vertical and horizontal gaps. A first precursor compound is provided into the reaction chamber, wherein the first precursor compound contains a metal-oxygen bond, and wherein the first precursor compound is in the form of an oligomer. A reactant compound is provided into a reaction chamber, wherein the reactant compound contains water; In response to the provision of reactant compounds, a flowable compound comprising metal hydroxides and metal-oxygen bonds is formed, wherein the flowable compound migrates into vertical and horizontal gaps; and A substantially seamless metal oxide layer is formed on the substrate.
19. The method according to claim 18, wherein, The oligomer decomposes into its constituent compounds in response to the first precursor compound contacting a heated substrate.
20. The method according to claim 18, wherein, The first precursor compound includes dimethylaluminum isopropoxide.