A method for producing hemp-nylon blended colored yarn
By using a method of dyeing without pretreatment and blending with nylon staple fibers, the problems of long pretreatment process and uneven mixing of hemp fibers were solved, realizing the production of efficient and energy-saving hemp-nylon blended yarn, improving the abrasion resistance and strength of the yarn, and obtaining unique color effects.
Patent Information
- Application Number
- CN202611403531.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-10
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, the pretreatment process for hemp fibers is lengthy, energy-intensive, and consumes a lot of auxiliaries. Furthermore, the uneven mixing of nylon and hemp fibers results in a loose yarn structure, limited improvement in abrasion resistance and strength, and a lack of mature technical solutions for blended hemp/nylon staple fiber yarn spinning.
A dyeing method without pretreatment is adopted, in which a penetrant is used to treat the hemp fibers in the dyeing bath, and then the hemp fibers are fully mixed with nylon short fibers in the opening, cleaning and carding processes to form hemp-nylon blended colored yarn.
It significantly shortens the process, saves resources, improves fiber mixing uniformity, enhances yarn structure density, improves abrasion resistance and breaking strength, and achieves unique three-dimensional color effects and good color fastness.
Abstract
Description
Technical Field
[0001] This invention relates to a method for producing hemp-nylon blended colored yarn, belonging to the field of textile industry technology. Background Technology
[0002] Colored yarn, produced using a "dye-then-spin" process, creates a unique hazy, three-dimensional effect while shortening subsequent processing steps, reducing production costs, and resulting in higher added value. In recent years, hemp fiber has gained attention due to its excellent moisture absorption, breathability, and natural antibacterial properties. However, its rough feel, poor elasticity, and insufficient abrasion resistance limit its application in high-end apparel fabrics. Nylon fiber possesses excellent abrasion resistance and elastic recovery rate; blending hemp and nylon allows for complementary advantages, yielding high-performance blended yarns.
[0003] In existing technologies, the dyeing of loose hemp fibers typically requires pretreatment processes such as oxygen bleaching or enzyme treatment to remove impurities and improve whiteness and permeability. However, for loose hemp fibers used in colored yarn production, which are mostly processed into medium-dark colors with less stringent whiteness requirements, conventional pretreatment processes are not only lengthy, energy-intensive, and consume large amounts of auxiliaries, but also significantly reduce the strength of the hemp fibers. Furthermore, in existing technologies involving hemp / nylon blends, nylon is often plied with hemp staple yarn in filament form rather than being fully blended with hemp fibers in staple form, resulting in uneven fiber mixing, insufficient yarn density, and limited improvement in properties such as abrasion resistance and strength. Currently, there is no mature technology that integrates untreated dyeing of loose hemp fibers with colored yarn produced from hemp / nylon staple fiber blends. Summary of the Invention
[0004] To achieve the above objectives, the present invention provides the following technical solution: A method for producing a hemp-nylon blended colored yarn includes the following steps: (1) No pretreatment dyeing process for hemp fiber: Hemp fiber is placed in a special cage for dyeing hemp fiber, water is added, the bath ratio is 1:6~16, penetrant JFC:1-3g / L is added to the dyeing vat, and the vat is kept at 60℃ for 10min without draining the liquid; reactive dye is added directly to the dyeing vat and kept at 10-20min; sodium sulfate is added to the dyeing vat at a concentration of 10-80g / L and kept at 60-90℃ for 15-30min; soda ash is added to the dyeing vat at a concentration of 10-30g / L, and the vat is kept at 60min before draining the liquid to obtain dyed hemp fiber; (2) Post-processing steps: The dyed hemp fibers obtained in step 1 are placed in hot water at a liquor ratio of 1:6~16. Soap washing agent NCF: 1-2g / L is added to the dyeing vat, the temperature is raised to 98℃ and kept at 15min, and then the liquid is drained. Soap washing is performed 1-3 times according to the concentration of reactive dye. Then, warm water is added to the dyeing vat in sequence, and acetic acid: 0.5-0.6g / L, softener KOKE GLN: 2.5-3.5% and color fixing agent KOKE FFC: 3-5% are added. The temperature is kept at 50℃ for 20min, the liquid is drained, the fibers are taken out and dried. (3) Blended spinning process: The dyed hemp fibers dried in step 2 are mixed with nylon staple fibers in a set ratio, and then spun into hemp-nylon blended colored yarn through the processes of opening machine mixing, carding, pre-combining, drawing, roving and spinning.
[0005] Preferably, the loose fiber mentioned in step 1 is one or more of flax, ramie, and industrial hemp, and the fiber morphology is a hemp web or hemp strip state after carding. The density of the fiber in the special cage for loose fiber dyeing is 0.2-0.3 g / cm³, the density of the fiber in the cage is uniform, and the surface is not obviously uneven.
[0006] Preferably, the reactive dye in step 1 is one or more of vinyl sulfone dyes, triazine dyes, or dual reactive dyes.
[0007] Preferably, the penetrant JFC described in step 1 has salt and alkali resistance.
[0008] Preferably, the nylon staple fiber in step 3 is nylon 6 or nylon 66 staple fiber with a fiber length of 38mm*1.2 denier.
[0009] Preferably, the ratio of dyed hemp fiber to nylon staple fiber in step 3 is as follows by weight: hemp fiber 50%~80% and nylon staple fiber 20%~50%.
[0010] Preferably, the specific process parameters for the blended spinning process in step 3 are as follows: Mixing: Mix twice with an opening machine, and beat at a speed of 300-400 r / min by hand; Carding: machine speed 35-45m / min, cylinder-flat spacing 8-7-7-8 / 1000 inches, sliver weight 20.0-22.0g / 5m; Pre-combining: Combine 6-8 strips after the machine, machine speed 300-350 r / min, output quantity 21.0-23.0 g / 5m; Sliver combining: 6-8 slivers are combined after the machine, machine speed 300-350 r / min, output sliver weight 20.0-22.0 g / 5m; Roving: basis weight 6.0-7.0g / 10m, spindle speed 800-900r / min, twist coefficient 70-80; Fine yarn: The yarn count is 20S~40S English count, and the twist is adjusted according to the yarn count.
[0011] Preferably, after the spinning process described in step 3, a winding process may also be included.
[0012] The beneficial effects of this invention are: Eliminates the need for pretreatment before dyeing hemp fibers: The high-efficiency penetrant is used to treat the fibers in the same dyeing bath, eliminating the need for separate oxygen bleaching or enzyme treatment steps. This significantly shortens the process, saves water, electricity, and steam consumption, reduces the use of auxiliaries, and minimizes damage to the strength of hemp fibers.
[0013] Nylon is blended in the form of short fibers: Unlike the existing technology of plying nylon filaments with linen yarn, this invention uses nylon short fibers and dyed linen fibers to be fully mixed in processes such as opening and cleaning, carding, and drawing. The fibers are evenly distributed, the yarn structure is dense, and the abrasion resistance and breaking strength are superior.
[0014] The dyed yarn has a unique style: after dyeing, hemp fibers are blended with natural or dyed nylon to obtain a unique three-dimensional pattern effect with contrasting or blended hemp and nylon colors, and the color fastness is excellent.
[0015] Highly integrated process: It organically combines pretreatment-free dyeing with short-fiber blended spinning to form a complete, efficient, and energy-saving production solution for linen-nylon blended colored yarn, filling a gap in this technical field. Detailed Implementation
[0016] Example 1: 70% hemp / 30% nylon, medium to dark color dyeing Step (1) Dyeing of hemp fibers without pretreatment: Fiber type: Loose flax fiber (after combing, in strip form) Cage density: 0.25 g / cm³ Bath ratio: 1:6 Add penetrant JFC: 1g / L, incubate at 60℃ for 10min, do not drain. Reactive dye: Reactive Black SRFD 8% (by weight of fiber), heat treatment for 10 min Sodium sulfate: 10g / L, keep warm at 60℃ for 15min Soda ash: 30g / L, keep warm for 60 minutes and then drain. Post-processing of step (2): Use a liquor ratio of 1:6, add hot water (85℃), soap detergent NCF: 2g / L, heat at 98℃ for 15min, drain, and repeat the soaping process once.
[0017] Add warm water (50℃), acetic acid 0.5g / L, softener KOKE GLN: 3.5%, fixative KOKE FFC: 3%, incubate at 50℃ for 20 minutes, then drain. Remove the fibers and dry them until the moisture regain is 8%. Step (3) Blended spinning (linen: nylon = 80:20): Nylon staple fiber: Nylon 6, length 38mm, fineness 1.5D Mixing: Mix twice with an opening machine, and beat at a speed of 300 rpm. Carding: machine speed 45m / min, cylinder-flat spacing 8-7-7-8 / 1000 inches, sliver weight 21.0g / 5m Pre-combination: 8 strips are combined after the machine, machine speed 350 r / min, output quantity 23.0 g / 5m Drawing: 8 slivers are drawn together after the machine, machine speed 300 r / min, output weight 22g / 5m Roving: basis weight 6g / 10m, spindle speed 800r / min, twist coefficient 70 Fine yarn: 40 count.
[0018] Example 2: 60% hemp / 40% nylon, color dyed Step (1) Dyeing of hemp fibers without pretreatment: Fiber type: Ramie loose fiber Cage density: 0.28 g / cm³ Bath ratio: 1:16 Add penetrant JFC: 3g / L, incubate at 60℃ for 10 minutes, do not drain. Reactive dyes: Yageerz Blue GN: 3%, Yageerz Red 6BN: 0.8%, Yageerz Yellow 4RN: 0.3% (by fiber weight), heat treatment for 20 min. Sodium sulfate: 80g / L, keep warm at 90℃ for 30 minutes Soda ash: 10g / L, incubate at 90℃ for 60 minutes, then drain. Post-processing of step (2): The dyed hemp fibers obtained in step (1) are placed in hot water at 85°C with a liquor ratio of 1:16. Soaping agent NCF:1g / L is added to the dyeing vat, the temperature is raised to 98°C and kept for 15 minutes, and then the liquid is drained. Soaping is performed 3 times according to the concentration of reactive dye. Then, the dyeing vat is placed in warm water at 50°C, and acetic acid:0.6g / L, softener KOKE GLN:2.5% and fixing agent KOKE FFC:3% are added in sequence. The vat is kept at 50°C for 20 minutes, the liquid is drained, the fibers are taken out and dried. Step (3) Blended spinning (ramie:nylon = 50:50): Nylon staple fiber: Nylon 66, length 38mm Mixing: Mix twice with an opening machine and beat at a speed of 400 rpm; Carding: machine speed 35m / min, cylinder-flat spacing 8-7-7-8 / 1000 inches, sliver weight 20.0-22.0g / 5m; Pre-combination: The last 6 strands are combined at a speed of 300 r / min, and the output quantity is 21.0 g / 5m; Sliver combining: 6 slivers are combined after the machine, machine speed is 350 r / min, and the output sliver quantity is 20.0 g / 5m; Roving: basis weight 7.0g / 10m, spindle speed 900r / min, twist coefficient 80; Fine yarn: spun with a count of 20S (English count). Comparative Example 1: Existing Technology: Natural Linen / Nylon Filament Ply Yarn The yarn is made from natural flax staple fiber spun into 30-count linen yarn, which is then twisted together with 70D nylon filament.
[0019] Yarn quality test results: As can be seen from the comparison, the fracture strength of Embodiments 1 and 2 of the present invention is increased by about 10%, the wear resistance is increased by 20%, and the strips are more uniform compared with Comparative Example 1.
Claims
1. A method for producing a hemp-nylon blended colored yarn, characterized in that, Includes the following steps: (1) No pretreatment dyeing process for hemp fiber: Hemp fiber is placed in a special cage for dyeing hemp fiber, water is added, the bath ratio is 1:6~16, penetrant JFC:1-3g / L is added to the dyeing vat, and the vat is kept at 60℃ for 10min without draining the liquid; reactive dye is added directly to the dyeing vat and kept at 10-20min; sodium sulfate is added to the dyeing vat at a concentration of 10-80g / L and kept at 60-90℃ for 15-30min; soda ash is added to the dyeing vat at a concentration of 10-30g / L, and the vat is kept at 60min before draining the liquid to obtain dyed hemp fiber; (2) Post-processing steps: The dyed hemp fibers obtained in step (1) are placed in hot water at a liquor ratio of 1:6~16. Soap washing agent NCF:1-2g / L is added to the dyeing vat, the temperature is raised to 98℃ and kept warm for 15min, and then the liquid is drained. Soap washing is performed 1-3 times according to the concentration of reactive dye. Then, warm water is added to the dyeing vat in sequence, and acetic acid:0.5-0.6g / L, softener KOKE GLN:2.5-3.5% and color fixing agent KOKE FFC:3-5% are added. The vat is kept warm at 50℃ for 20min, the liquid is drained, the fibers are taken out and dried. (3) Blended spinning process: The dyed hemp fibers dried in step (2) are mixed with nylon staple fibers in a set ratio, and then spun into hemp-nylon blended colored yarn through the processes of opening machine mixing, carding, pre-combining, drawing, roving and spinning.
2. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, The loose fiber mentioned in step (1) is one or more of flax, ramie, and industrial hemp. The fiber morphology is a hemp web or hemp strip after carding. The density of the fiber in the special cage for loose fiber dyeing is 0.2-0.3 g / cm³. The density of the fiber in the cage is uniform and consistent, and the surface is not obviously uneven.
3. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, The reactive dye mentioned in step (1) is one or more of vinyl sulfone type dyes, triazine type dyes, or dual reactive group type dyes.
4. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, The penetrant JFC mentioned in step (1) has salt and alkali resistance.
5. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, The nylon staple fiber mentioned in step (3) is nylon 6 or nylon 66 staple fiber with a fiber length of 38mm*1.2 denier.
6. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, The ratio of dyed hemp fiber to nylon staple fiber in step (3) is as follows by weight: hemp fiber 50%~80%, nylon staple fiber 20%~50%.
7. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, The specific process parameters for the blended spinning process in step (3) are as follows: Mixing: Mix twice with an opening machine, and beat at a speed of 300-400 r / min by hand; Carding: machine speed 35-45m / min, cylinder-flat spacing 8-7-7-8 / 1000 inches, sliver weight 20.0-22.0g / 5m; Pre-combining: Combine 6-8 strips after the machine, machine speed 300-350 r / min, output quantity 21.0-23.0 g / 5m; Sliver combining: 6-8 slivers are combined after the machine, machine speed 300-350 r / min, output sliver weight 20.0-22.0 g / 5m; Roving: basis weight 6.0-7.0g / 10m, spindle speed 800-900r / min, twist coefficient 70-80; Fine yarn: The yarn count is 20S~40S English count, and the twist is adjusted according to the yarn count.
8. The method for producing a hemp-nylon blended colored yarn according to claim 1, characterized in that, After the spinning process described in step (3), a winding process may also be included.