A processing technology for high resilience linen core-spun yarn
By using intermittent spraying and heating vaporization processes with compound carrier adhesive in flax core-spun yarn, the problems of low production efficiency and structural instability in existing technologies have been solved, enabling the rapid preparation and improved stability of high-resilience flax core-spun yarn.
Patent Information
- Application Number
- CN202611562129.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-10
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, the dissolution process of coating soluble polyester fibers with flax fibers is time-consuming, resulting in low production efficiency. Furthermore, vinylon fibers are prone to swelling or deformation during washing, affecting the stability of the fiber structure.
A carrier adhesive is formed by compounding p-dichlorobenzene, dispersion emulsion and hydrogel in the form of fine particles. This adhesive is sprayed onto the elastic inner core fiber in an alternating manner and then vaporized after heating to form an intermittent pore structure with built-in composite fibers. Combined with alkali boiling, acid washing, bleaching and water washing steps, high resilience flax core-spun yarn is finally prepared.
It improves elastic recovery, shortens processing time, increases production efficiency, maintains the stability and uniformity of fiber structure, reduces the amount of dichlorobenzene used, and enhances the uniform distribution of elastic fibers.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of processing and preparation technology of flax core-spun yarn, and particularly relates to a processing technology for high resilience flax core-spun yarn. Background Technology
[0002] Flax is a pure natural fiber, and its excellent properties such as sweat absorption and moisture wicking, breathability, antibacterial properties, and cooling effect have led to its increasingly widespread development and application. Flax yarn is the only natural fiber spun from processed fibers, a characteristic inherent to flax itself. While flax fiber possesses many excellent properties, its poor wrinkle resistance limits its applications. Therefore, it is now generally used in core-spun yarn structures, where flax fibers are wrapped around elastic fibers to form composite core-spun yarns. This enhances the elasticity and wrinkle resistance of flax fibers. However, to achieve even better elastic recovery, elastic fibers are often combined with soluble fibers such as soluble polyester fibers. After twisting, the polyester fibers are coated with flax fibers, and then dissolved in a subsequent process to create a porous structure that greatly improves elasticity and resilience. However, this process results in a long dissolution cycle, as the dissolution of soluble polyester with strong alkali through flax fiber coating takes a considerable amount of time, leading to low production efficiency. Another method involves washing vinylon fibers, but this causes swelling and damages the fiber structure. Furthermore, the washing process requires strict control of conditions, which carries the risk of deformation and hardening. Therefore, existing processing methods need to be improved to increase the dissolution rate while ensuring structural stability. Summary of the Invention
[0003] To address the shortcomings of the prior art, the present invention solves the following problem: because coating with flax fibers and dissolving soluble polyester with strong alkali requires a long time, production efficiency is low. Alternatively, vinylon fibers can be prepared by washing them with water, but vinylon fibers swell during washing, which can damage the fiber structure. At the same time, the conditions for washing vinylon fibers are strictly controlled, which may lead to deformation and hardening.
[0004] To solve the above problems, the technical solution adopted by the present invention is as follows: A processing technique for high resilience linen core-spun yarn, comprising the following steps: S1. Prepare the carrier gel; pulverize p-dichlorobenzene to make it into fine particles; combine the fine particles of p-dichlorobenzene, dispersion emulsion, and hydrogel, and stir slowly to form the carrier gel. S2. Intermittent spraying: Select elastic core fibers and spray carrier adhesive on the elastic core fibers in an intermittent manner, while distributing it vertically and horizontally, so that the carrier adhesive on the elastic core fibers is distributed vertically and horizontally; after heating and curing, the built-in composite fiber is obtained. S3, Linen Covering: Linen yarn and inner fibers are spun on a spinning machine to obtain pre-core-spun yarn with linen yarn covering inner composite fibers; S4. Heating and vaporization: The pre-core-spun yarn is fed into the heating chamber for heating, which causes the dichlorobenzene particles on the built-in composite fiber to vaporize and be discharged, resulting in an intermittent, staggered pore structure on the built-in composite fiber. S5. Post-washing: The pre-core-spun yarn from step S4 is subjected to alkaline boiling, acid washing, bleaching, dechlorination, water washing, and drying to obtain the flax core-spun yarn.
[0005] Furthermore, in step S1, the diameter of the p-dichlorobenzene particles pulverized into fine particles is 0.1 to 0.4 mm.
[0006] Furthermore, in step S1, the weight parts of each component are: 3 to 8% p-dichlorobenzene, 25 to 35% dispersion emulsion, and 20 to 30% hydrogel.
[0007] Furthermore, in step S1, the dispersion emulsion is an aqueous polyurethane solution.
[0008] Furthermore, in step S2, the elastic core fiber is spandex fiber or polyester elastic fiber.
[0009] Furthermore, in step S2, the heating and curing temperature is 30 to 35°C, and the heating and curing time is 5 to 8 minutes.
[0010] Furthermore, in step S3, the flax yarn is processed from raw flax with a splitting index of 250 or higher.
[0011] Furthermore, in step S4, the heating temperature is 45 to 50°C, and the heating time is 30 to 40 minutes.
[0012] The beneficial effects of this invention are as follows: 1. This invention involves compounding fine-particle p-dichlorobenzene, a dispersion emulsion, and a hydrogel, and slowly stirring to form a carrier adhesive. The carrier adhesive is then sprayed onto elastic core fibers in an alternating pattern, with the layers distributed vertically and horizontally. After being wrapped in flax, the fibers are heated and vaporized. The pre-spun yarn is then fed into a heating chamber for heating, causing the p-dichlorobenzene particles on the inner composite fibers to vaporize and be discharged. This results in an intermittent, alternating porous structure on the inner composite fibers, thereby improving elastic recovery. This invention achieves porosity through heating and vaporization, resulting in fast forming speed and high processing efficiency.
[0013] 2. The carrier adhesive of the present invention is distributed alternately and vertically on the elastic core fiber. It can be understood as first spraying the carrier adhesive from top to bottom, then spraying the carrier adhesive from bottom to top at intervals, and then spraying the carrier adhesive from top to bottom at intervals again, and so on, so as to achieve the carrier adhesive being distributed alternately on both the upper and lower sides, and the carrier adhesive on the upper side and the carrier adhesive on the lower side are distributed alternately in the upper and lower positions. In this way, the pores are uniformly distributed in an intermittent manner along the entire axial direction of the elastic fiber, so as to achieve a uniform distribution of the elastic structure and more stable performance. At the same time, the amount of carrier adhesive used is reduced by the intermittent distribution, thereby reducing the amount of dichlorobenzene used. This results in faster heating and vaporization in the later stage because the amount of dichlorobenzene used for vaporization is reduced.
[0014] 3. This invention combines fine-particle p-dichlorobenzene, a dispersion emulsion, and a hydrogel. The dispersion emulsion is an aqueous polyurethane solution. The aqueous polyurethane solution can improve the internal flexible and stable strong bonding points, improve structural stability, and will not affect the yarn manufacturing. The hydrogel provides a uniformly dispersed aqueous colloidal environment, allowing the p-dichlorobenzene and the aqueous polyurethane solution to be fully and evenly mixed and distributed. Thus, during spraying, the p-dichlorobenzene is more evenly distributed, and the elasticity enhancement performance is more evenly distributed. Detailed Implementation
[0015] The present invention will now be described in further detail.
[0016] A processing technique for high resilience linen core-spun yarn, comprising the following steps: S1. Prepare the carrier adhesive solution; pulverize p-dichlorobenzene to produce fine particles; combine the finely pulverized p-dichlorobenzene, dispersion emulsion, and hydrogel, and stir slowly to form the carrier adhesive solution; the p-dichlorobenzene particles are pulverized to a diameter of 0.2 mm. The weight parts of each component are: p-dichlorobenzene 6%, dispersion emulsion 25%, and hydrogel 25%. The dispersion emulsion is an aqueous polyurethane solution.
[0017] S2. Intermittent Spraying: Elastic core fibers are selected, and carrier adhesive is sprayed onto the fibers in an intermittent, staggered pattern. This results in a staggered and alternating distribution of the carrier adhesive on the elastic core fibers. After heat curing, an embedded composite fiber is obtained. The elastic core fibers are spandex or polyester elastic fibers. The heat curing temperature is 30℃, and the curing time is 6 minutes.
[0018] S3. Flax-coated yarn: Flax yarn and inner fibers are spun on a spinning machine to obtain a pre-core-spun yarn in which flax yarn coats the inner composite fibers; the flax yarn is made from raw flax with a splitting index of greater than or equal to 250 count.
[0019] S4. Heating and Gasification: The pre-spun yarn is fed into a heating chamber for heating, causing the dichlorobenzene particles on the built-in composite fibers to vaporize and be discharged, resulting in an intermittent, staggered pore structure on the built-in composite fibers; the heating temperature is 47℃, and the heating time is 30 minutes. The vaporized airflow can be recovered by a fan and discharged after environmental purification through purification materials.
[0020] S5. Post-washing: The pre-spun yarn from step S4 is subjected to alkaline boiling, acid washing, bleaching, dechlorination, water washing, and drying to obtain flax core-spun yarn.
[0021] This invention involves compounding fine-particle p-dichlorobenzene, a dispersion emulsion, and a hydrogel, and slowly stirring them to form a carrier adhesive. This carrier adhesive is then sprayed onto elastic core fibers in an alternating pattern, creating a staggered distribution. After being wrapped in flax, the pre-spun yarn is heated and vaporized. The pre-spun yarn is then fed into a heating chamber, causing the p-dichlorobenzene particles on the inner composite fibers to vaporize and dissipate. This results in a discontinuous, staggered porous structure on the inner composite fibers, thus improving elastic recovery. This invention achieves porosity through heating and vaporization, resulting in fast forming speed and high processing efficiency.
[0022] The carrier adhesive of this invention is distributed alternately and vertically on the elastic core fiber. This can be understood as first spraying the carrier adhesive from top to bottom, then spraying it upwards from bottom to top at intervals, and then spraying it downwards from top to bottom at intervals again, repeating this process. This achieves an alternating distribution of the carrier adhesive on both the upper and lower sides, with the upper and lower sides exhibiting an alternating vertical distribution. This results in a uniform, discontinuous distribution of pores along the entire axial direction of the elastic fiber, achieving a uniform distribution of the elastic structure and more stable performance. Simultaneously, the discontinuous vertical distribution reduces the amount of carrier adhesive used, thereby reducing the amount of dichlorobenzene used. This allows for faster gasification during subsequent heating because the amount of dichlorobenzene used for gasification is reduced.
[0023] This invention combines fine-particle p-dichlorobenzene, a dispersion emulsion, and a hydrogel. The dispersion emulsion is an aqueous polyurethane solution, which improves the internal flexible and stable strong bonding points, enhancing structural stability without affecting yarn manufacturing. The hydrogel provides a uniformly dispersed aqueous colloidal environment, allowing the p-dichlorobenzene and the aqueous polyurethane solution to be fully and evenly mixed and distributed. This results in a more uniform distribution of p-dichlorobenzene and a more uniform distribution of elasticity enhancement properties during spraying.
[0024] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A processing technology for high-resilience flax core-spun yarn, characterized in that, The steps are as follows: S1. Prepare the carrier gel; pulverize p-dichlorobenzene to make it into fine particles; combine the fine particles of p-dichlorobenzene, dispersion emulsion, and hydrogel, and stir slowly to form the carrier gel. S2. Intermittent spraying: Select elastic core fibers and spray carrier adhesive on the elastic core fibers in an intermittent manner, while distributing it vertically and horizontally, so that the carrier adhesive on the elastic core fibers is distributed vertically and horizontally; after heating and curing, the built-in composite fiber is obtained. S3, Linen Covering: Linen yarn and inner fibers are spun on a spinning machine to obtain pre-core-spun yarn with linen yarn covering inner composite fibers; S4. Heating and vaporization: The pre-core-spun yarn is fed into the heating chamber for heating, which causes the dichlorobenzene particles on the built-in composite fiber to vaporize and be discharged, resulting in an intermittent, staggered pore structure on the built-in composite fiber. S5. Post-washing: The pre-core-spun yarn from step S4 is subjected to alkaline boiling, acid washing, bleaching, dechlorination, water washing, and drying to obtain the flax core-spun yarn.
2. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S1, the p-dichlorobenzene is pulverized into fine particles with a diameter of 0.1 to 0.4 mm.
3. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S1, the weight parts of each component are: 3 to 8% p-dichlorobenzene, 25 to 35% dispersion emulsion, and 20 to 30% hydrogel.
4. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S1, the dispersion emulsion is an aqueous polyurethane solution.
5. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S2, the elastic core fiber is spandex fiber or polyester elastic fiber.
6. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S2, the heating and curing temperature is 30 to 35°C, and the heating and curing time is 5 to 8 minutes.
7. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S3, the flax yarn is processed from raw flax with a splitting index of 250 or higher.
8. The processing technology of high resilience flax core-spun yarn according to claim 1, characterized in that, In step S4, the heating temperature is 45 to 50°C and the heating time is 30 to 40 minutes.