A system for preparing recycled asphalt pavement materials
By acquiring on-site construction data and analyzing the aging degree of waste asphalt milling material, and adjusting the preparation process parameters in conjunction with high-temperature characteristic distribution, the problem of poor rutting resistance of recycled asphalt pavement materials was solved, achieving efficient performance matching and environmental adaptability.
Patent Information
- Application Number
- CN202611629095.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-21
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies do not fully consider the differences in aging degree of waste asphalt milling material and the requirements of construction environment when preparing recycled asphalt pavement materials, resulting in poor rutting resistance.
By collecting and analyzing data, historical temperature data and multidimensional physical indicators of RAP material at the construction site are obtained, the aging degree of asphalt phase and aggregate phase is determined, and the anti-rutting requirement coefficient is determined by combining the high temperature characteristic distribution. The preparation process parameters are then adjusted to achieve adaptive matching of material properties.
It improves the rutting resistance of recycled asphalt pavement materials, ensures that the material performance design meets the actual environmental requirements, and overcomes the performance deficiencies caused by fixed conventional processes.
Smart Images

Figure CN123120161A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of asphalt pavement material preparation technology, and more specifically to a recycled asphalt pavement material preparation system. Background Technology
[0002] Asphalt pavements are prone to rutting and deformation under the combined effects of long-term repeated vehicle loads and high-temperature environments. In order to save resources and repair pavement defects, recycled asphalt technology is widely used in engineering to recycle and reuse waste asphalt milling materials to pave recycled pavements.
[0003] Existing technologies typically involve directly mixing recycled asphalt pavement materials (RAP material), new aggregates, and base asphalt according to fixed empirical proportions and conventional mixing parameters. However, these technologies fail to adequately consider the differences in the overall aging degree of the asphalt and aggregate phases of different recycled asphalt materials during their historical service. They also fail to accurately quantify the actual rutting resistance requirements based on the specific high-temperature climate distribution characteristics of the construction site. Furthermore, they neglect the performance matching and gradation adaptation resistance during the mixing process of new and old materials. Consequently, they cannot adaptively and finely adjust the preparation process parameters according to the actual performance degradation state of the materials and the requirements of the construction environment. This results in poor rutting resistance of recycled asphalt pavement materials prepared using fixed conventional processes. Summary of the Invention
[0004] To address the problem of poor rutting resistance in existing recycled asphalt pavement materials prepared using fixed conventional processes, the present invention aims to provide a recycled asphalt pavement material preparation system, the specific technical solution of which is as follows: The first aspect of this invention provides a system for preparing recycled asphalt pavement materials, comprising: The data acquisition and preprocessing module is used to acquire all historical temperature data of the construction site, the matrix penetration of the base asphalt to be added and the RAP asphalt penetration of the current RAP material, asphalt softening temperature, moisture content and sand content; and to determine the gradation compatibility coefficient between the aggregate to be added and the current RAP material. The first determining module is used to determine the corresponding degree of asphalt phase aging based on the benchmark deviation between the RAP asphalt penetration and the asphalt softening temperature of the current RAP material; and to determine the corresponding overall aging degree based on the benchmark deviation between the moisture content and sand content of the current RAP material and the degree of asphalt phase aging. The second determining module is used to determine the rutting resistance requirement coefficient of the foundation based on the high temperature characteristic distribution of historical temperature data at the construction site; to determine the rutting resistance requirement correction coefficient by weighting the foundation rutting resistance requirement coefficient with the overall aging degree; and to determine the fusion resistance coefficient by coupling the matrix penetration, the overall aging degree and the gradation adaptation coefficient. The asphalt pavement material preparation module is used to adjust the preparation process parameters of the new recycled asphalt pavement material based on the rutting resistance requirement correction coefficient and the fusion resistance coefficient to obtain all the final preparation process parameters; and to prepare the asphalt pavement material according to all the final preparation process parameters.
[0005] Furthermore, the process of obtaining the degree of aging of the asphalt phase includes: The RAP asphalt penetration of the current RAP material is standardized by setting a preset standard asphalt penetration to determine the degree of adhesion aging of the current RAP material; the asphalt softening temperature of the current RAP material is standardized by setting a preset standard asphalt softening temperature to determine the rate of increase of softening point of the current RAP material. The degree of asphalt phase aging of the current RAP material is determined based on the average between the degree of adhesive aging and the growth rate of the softening point.
[0006] Furthermore, the process of obtaining the overall aging degree includes: Calculate the difference between the preset standard moisture content and the current moisture content of the RAP material to determine a reference moisture content difference; determine the moisture content excess rate of the current RAP material based on the ratio between the reference moisture content difference and the preset standard moisture content; determine the sand content excess rate of the current RAP material based on the calculation principle of the moisture content excess rate and the sand content of the current RAP material; determine the aggregate phase aging degree based on the average of the moisture content excess rate and the sand content excess rate. The overall aging degree is determined based on the average value between the aging degree of the aggregate phase and the aging degree of the asphalt phase.
[0007] Furthermore, the process of obtaining the basic rutting resistance demand coefficient includes: In all historical temperature data at the construction site, the cumulative value of all historical temperature data exceeding the preset high temperature threshold is positively correlated to determine the high temperature sensitivity coefficient. The rutting resistance requirement coefficient of the foundation is determined by multiplying the high temperature sensitivity coefficient with the preset dynamic stability benchmark value corresponding to the structural layer at the construction site.
[0008] Furthermore, the process of obtaining the anti-rutting demand correction coefficient includes: The corresponding actual rutting resistance requirement coefficient is determined by multiplying the positive correlation mapping value of the overall aging degree with the basic rutting resistance requirement coefficient. The rutting resistance requirement correction coefficient is determined based on the ratio between the actual rutting resistance requirement coefficient and the preset requirement benchmark value.
[0009] Furthermore, the process of obtaining the fusion resistance coefficient includes: The difference between the matrix penetration of the base asphalt to be added and the preset standard asphalt penetration is used as the reference matrix difference; the absolute value of the ratio between the reference matrix difference and the preset standard asphalt penetration is negatively correlated to determine the benchmark asphalt matching degree; the performance matching coefficient of the base asphalt to be added is determined based on the maximum value between the benchmark asphalt matching degree and the preset matching degree lower limit. The weighted matching coefficient is determined by multiplying the preset first weight with the performance matching coefficient; the weighted adaptation coefficient is determined by multiplying the preset second weight with the gradation adaptation coefficient; and the weighted aging coefficient is determined by multiplying the negative correlation mapping value of the overall aging degree with the preset third weight. The fusion resistance coefficient is determined by negatively mapping the sum of the weighted matching coefficient, the weighted adaptation coefficient, and the weighted aging coefficient.
[0010] Furthermore, the process of obtaining the final preparation process parameters includes: A preliminary fusion adjustment value is determined based on the maximum value between the fusion resistance coefficient and the preset lower limit protection parameter; a fusion adjustment coefficient is determined based on the minimum value between the preliminary fusion adjustment value and the preset upper limit protection parameter. The theoretical dosage multiple is determined by multiplying the rutting resistance correction coefficient and the fusion resistance coefficient; the preliminary dosage adjustment value is determined by the maximum value between the theoretical dosage multiple and the preset lower limit protection parameter; and the composite modifier dosage adjustment coefficient is determined by the minimum value between the preliminary dosage adjustment value and the preset upper limit protection parameter. The preliminary demand adjustment value is determined based on the maximum value between the anti-rutting demand correction coefficient and the preset lower limit protection parameter; the actual anti-rutting demand adjustment coefficient is determined based on the minimum value between the preliminary demand adjustment value and the preset upper limit protection parameter. The final preparation process parameters are determined based on the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the actual rutting resistance requirement adjustment coefficient.
[0011] Furthermore, the process for obtaining the degree of adhesive aging includes: A reference penetration difference is determined based on the difference between the preset standard asphalt penetration and the current RAP material's RAP asphalt penetration; the degree of adhesion aging of the current RAP material is determined based on the ratio between the reference penetration difference and the preset standard asphalt penetration.
[0012] Furthermore, the process of obtaining the softening point growth rate includes: A reference softening temperature difference is determined based on the difference between the current RAP material's asphalt softening temperature and the preset standard asphalt softening temperature; the softening point growth rate of the current RAP material is determined based on the ratio between the reference softening temperature difference and the preset standard asphalt softening temperature.
[0013] Furthermore, the process of determining the final preparation process parameters based on the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the actual rutting resistance requirement adjustment coefficient includes: The final mixing time parameter is determined by multiplying the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the preset mixing time. The product of the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the preset mixing base temperature is rounded down to determine the final mixing base temperature parameter. The final number of compaction passes is determined by rounding down the product of the positive correlation mapping value of the composite modifier dosage adjustment coefficient, the fusion adjustment coefficient, the actual rutting resistance requirement adjustment coefficient, and the preset number of compaction passes.
[0014] In a second aspect, the present invention provides a computer device including a memory and a processor. The memory is used to store computer program code, and the processor is used to call and run the computer program code from the memory to execute a system as described in the first aspect or any embodiment of the first aspect of the present invention.
[0015] Thirdly, the present invention provides a computer program product comprising computer program code, which, when executed, performs a system as described in the first aspect or any embodiment of the first aspect of the present invention.
[0016] Fourthly, the present invention provides a computer-readable storage medium storing computer program code that, when executed, performs a system as described in the first aspect or any embodiment of the first aspect of the present invention.
[0017] The present invention has the following beneficial effects: This invention acquires historical temperature data from the construction site, the matrix penetration of the asphalt to be added, and the multidimensional physical indicators of the current RAP material. Based on the benchmark deviation of each indicator, it determines the aging degree of the asphalt phase and the overall aging degree layer by layer to comprehensively and objectively quantify the true performance degradation state of the waste material. Simultaneously, it determines the basic rutting resistance requirement coefficient by combining the high-temperature characteristic distribution of historical temperature data from the construction site, and obtains a rutting resistance requirement correction coefficient by weighting it with the overall aging degree, ensuring that the material's performance design standards fully match the severity of the actual environment. Furthermore, it couples the matrix penetration, overall aging degree, and gradation compatibility coefficient to determine the fusion resistance coefficient, comprehensively evaluating the matching difficulty in the mixing process of new and old materials. Finally, based on the rutting resistance requirement correction coefficient and the fusion resistance coefficient, it adaptively adjusts and prepares the new recycled asphalt pavement material, effectively overcoming the shortcomings of existing technologies that neglect the differences in aging of old materials and actual environmental requirements due to the use of fixed conventional preparation processes, resulting in poor rutting resistance. This makes the preparation of new recycled asphalt pavement materials with high rutting resistance performance for different service environments and waste material states more accurate. Attached Figure Description
[0018] To more clearly illustrate the technical solutions and advantages in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0019] Figure 1 This is a structural diagram of a recycled asphalt pavement material preparation system provided in one embodiment of the present invention; Figure 2 This is a schematic diagram of a computer device structure provided in one embodiment of the present invention. Detailed Implementation
[0020] To further illustrate the technical means and effects adopted by the present invention to achieve its intended purpose, the following, in conjunction with the accompanying drawings and preferred embodiments, details the specific implementation, structure, features, and effects of a recycled asphalt pavement material preparation system proposed according to the present invention. In the following description, different "one embodiment" or "another embodiment" do not necessarily refer to the same embodiment, and specific features, structures, or characteristics in one or more embodiments can be combined in any suitable form. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as implying or suggesting relative importance or implicitly indicating the number of indicated technical features. Thus, a feature defined with "first" or "second" may explicitly or implicitly include one or more of that feature.
[0021] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains.
[0022] The following description, in conjunction with the accompanying drawings, details the specific scheme of the recycled asphalt pavement material preparation system provided by the present invention.
[0023] This invention provides a system for preparing recycled asphalt pavement materials. Please refer to [link / reference]. Figure 1 The diagram shows a structural diagram of a recycled asphalt pavement material preparation system according to an embodiment of the present invention. The system includes: a data acquisition and preprocessing module 101, a first determination module 102, a second determination module 103, and an asphalt pavement material preparation module 104.
[0024] The data acquisition and preprocessing module 101 is used to acquire all historical temperature data of the construction site, the matrix penetration of the base asphalt to be added and the RAP asphalt penetration of the current RAP material, asphalt softening temperature, moisture content and sand content; and to determine the gradation compatibility coefficient between the aggregate to be added and the current RAP material.
[0025] In one specific implementation of this invention, to accurately assess the aging state of materials and construction environment requirements, it is first necessary to collect accurate and multi-dimensional data on the environmental meteorological records of the construction site and related road raw materials. Specifically, by retrieving the daily meteorological monitoring records of the meteorological bureau or meteorological monitoring platform in the construction site location for the past five years, the temperature values or daily maximum temperature values within a preset time interval are extracted and recorded to form a time series of temperature data within a preset historical time period. This data is then used to subsequently filter out extreme high-temperature data exceeding a preset high-temperature threshold, thereby objectively reflecting the severity of high temperatures experienced by the road section during actual service.
[0026] For the waste pavement materials on site, a road milling machine was used to perform cold milling operations on the original asphalt pavement to a certain depth, and the resulting waste asphalt milled material was collected as the current RAP material. The sampled current RAP material was sent to the laboratory. First, the sample was reduced to two independent parallel samples using the quartering method. For the first group of samples, the samples were baked to constant weight using a constant temperature oven drying method (or low temperature vacuum drying method). The moisture content of the current RAP material was calculated and determined based on the mass difference before and after baking. Subsequently, the asphalt coating layer on the sample surface was washed away using a combination of solvent extraction and water washing sieving. The mass percentage of free dust and mud in the total aggregate was determined by passing the sample through a fine sieve of a specific specification (such as a 0.075mm standard sieve), thereby accurately obtaining the sand content of the current RAP material.
[0027] For the second group of parallel samples that were not baked at high temperatures, the aged asphalt in the current RAP material was completely dissolved and washed out using a centrifugal extractor and organic solvents such as trichloroethylene. The solvent was then completely evaporated using a rotary evaporator, recovering pure aged RAP asphalt. Based on this, the penetration of the recovered RAP asphalt was measured using an asphalt standard penetration tester at a standard test temperature of 25°C to obtain the RAP asphalt penetration value. Simultaneously, an asphalt softening point tester was used, placing the asphalt ring in glycerol or a water bath and heating it at a uniform rate. The instantaneous temperature at which the steel ball penetrated the asphalt layer and touched the substrate was recorded as the asphalt softening temperature of the current RAP material. Concurrently, samples of the base asphalt to be added were extracted from new asphalt tanks purchased during the construction preparation stage, and penetration tests were also conducted using a penetration tester under standard conditions of 25°C to determine and record the base asphalt penetration value.
[0028] In addition, to assess the skeleton stability of the mixed old and new aggregates, the old aggregate stripped after asphalt extraction was physically mixed with the new aggregate to be added at the construction site according to the pre-set mixing ratio. The mixed aggregate was then poured into a standard sieve set for shaking sieving tests, and the actual mass passing rate on each standard sieve aperture (e.g., 19mm, 13.2mm, 4.75mm, etc.) was recorded. The recorded actual passing rates for each aperture were compared one by one with the target passing rates for each aperture on the standard gradation curve specified in the target road design specification. The sum of the absolute values of the differences in passing rates for each corresponding sieve aperture was calculated and negatively normalized to the nearest whole number. Within the interval (i.e., the smaller the sum of the absolute values of the differences, the closer the mapping value is to 1, and the better the gradation complementarity is), the gradation compatibility coefficient between the aggregate to be added and the current RAP material is determined and quantified, thus completing the closed loop of data collection for the entire front-end raw materials and environmental conditions.
[0029] In one specific implementation of this invention, the normalization method employs minimum-maximum normalization. The normalization object covers all historical data. Specifically, after normalizing the sum of the absolute values of the differences in the passing rates of corresponding sieve apertures, the corresponding normalized value is subtracted from the real number 1 to obtain the gradation matching coefficient, which can be adjusted according to the specific implementation environment and specification requirements. It should be noted that, unless otherwise specified, the normalization function or method mentioned in this invention employs minimum-maximum normalization to normalize the normalization result to... The range. The maximum and minimum values used in the min-max normalization can be obtained according to the actual situation. For example, when multiple values can be obtained in the implementation process and it is necessary to compare the size relationship between different values, multiple values can be counted to obtain the maximum and minimum values. However, when only a single value can be obtained in the implementation process or it is not necessary to compare the size relationship between different values, the maximum and minimum values can be obtained by counting based on a large amount of historical experimental data or prior data obtained in the early stage.
[0030] The first determining module 102 is used to determine the corresponding degree of asphalt phase aging based on the benchmark deviation between the RAP asphalt penetration and asphalt softening temperature of the current RAP material; and to determine the corresponding overall aging degree based on the benchmark deviation between the moisture content and sand content of the current RAP material and the degree of asphalt phase aging. After completing the closed-loop multi-dimensional data collection of raw materials and environmental conditions, the chemical composition of the asphalt binder in the recycled waste asphalt pavement material (RAP material) has undergone significant changes due to the coupling effects of heat, oxygen, and ultraviolet radiation during long-term service. This manifests as a decline in bonding performance and hardening embrittlement, and this aging state is the core boundary condition determining the rutting resistance of the recycled pavement. Therefore, following the data collection stage, this embodiment of the invention establishes a quantitative system for the benchmark deviation between RAP asphalt penetration and softening temperature. This allows for precise identification of the extreme values of asphalt phase attenuation from two dimensions: consistency change and temperature-sensitive performance fluctuation. This scientifically determines the corresponding degree of asphalt phase aging. This step lays a high-precision physical characterization foundation for the subsequent comprehensive evaluation of the overall aging state, helps eliminate the blind addition of modifiers caused by the ambiguity of the old material's properties, ensures the recovery effect of the interfacial bonding force of the recycled mixture from the source, and provides a reliable decision-making basis for improving the high-temperature stability of the pavement.
[0031] Furthermore, considering that the interfacial bonding strength and gradation stability of recycled materials are highly susceptible to physical interference from moisture erosion and the accumulation of muddy dust during actual storage and production cycles, this aggregate phase deterioration will superimpose with the asphalt hardening effect, becoming a significant factor inducing early shoving and rutting deformation in recycled pavements. Therefore, by synergistically analyzing the benchmark deviations of moisture content and sand content and coupling them with the aging degree of the asphalt phase, the overall aging degree characterizing the degradation state of all material components is determined. This process achieves a logical leap from single-component evaluation to multi-phase composite assessment, enabling a more comprehensive examination of the true deterioration degree of waste materials under complex environments. This helps to accurately compensate for performance losses in subsequent processes, thereby significantly enhancing the skeleton density and high-temperature shear resistance of recycled mixtures, and constructing an efficient anti-rutting defense system from the material source.
[0032] The second determining module 103 is used to determine the rutting resistance requirement coefficient of the foundation based on the high temperature characteristic distribution of historical temperature data of the construction site; to determine the rutting resistance requirement correction coefficient by weighting the foundation rutting resistance requirement coefficient through the overall aging degree; and to determine the fusion resistance coefficient by coupling the matrix penetration, the overall aging degree and the gradation adaptation coefficient. After completing the physical characterization of the aging state of waste pavement materials and quantifying the degree of decay of all components, considering that the high-temperature shear resistance and structural stability of pavement materials during actual service are closely coupled with the high-temperature extreme climate environment of the construction site, this historical heat accumulation and load will significantly amplify the viscoelastic fluidity inside the material, becoming an external driving force for rutting. Therefore, by statistically analyzing the preset high-temperature characteristic distribution of historical temperature data at the construction site and combining it with the actual high-temperature severity for positive mapping, the basic rutting resistance requirement coefficient is determined. This step establishes a baseline defense line for pavement design from the perspective of environmental adaptability, ensuring that the initial performance settings of recycled materials fully match the local climate characteristics, and providing an objective benchmark reference system for subsequent correction of rutting resistance level based on the material's own decay characteristics.
[0033] Furthermore, considering that the severe aging and component deterioration of waste materials weaken their interfacial integration with new materials, designing solely based on environmental benchmarks could easily lead to insufficient high-temperature stability of the final mixture due to neglecting the performance limitations of the recycled materials. Therefore, this invention incorporates a pre-determined overall aging level to weighted correct the basic rutting resistance requirement coefficient, accurately determining the rutting resistance requirement correction coefficient that characterizes the severity of actual working conditions. This process achieves dual verification of "environmental requirements" and "material status," dynamically compensating for the rutting resistance gap caused by the performance degradation of recycled materials. This ensures that the final performance target not only meets the challenges of high-temperature environments but also fully covers the risks of recycling waste materials, significantly improving the relevance and reliability of recycled pavement design.
[0034] After clarifying the final target for rutting resistance, whether the recycled mixture can achieve the expected strength and stability depends crucially on the penetration and fusion efficiency of the new and old asphalt and aggregates at the microscopic interface and the degree of macroscopic skeleton interlocking. This fusion process is constrained by multiple factors, including the properties of the base asphalt, the aging and hardening of the waste material, and the gradation complementarity. Therefore, by performing multi-parameter coupled calculations on the penetration index of the base asphalt to be added, the overall aging degree of the waste material, and the gradation compatibility coefficient of the new and old aggregates, a fusion resistance coefficient that quantifies the difficulty of mixing the new and old components is determined. This process reveals the inherent bottleneck of material compatibility during the recycling process, providing a quantitative basis for subsequent targeted adjustments to the modifier dosage and mixing process.
[0035] The asphalt pavement material preparation module 104 is used to adjust the preparation process parameters of the new recycled asphalt pavement material based on the rutting resistance requirement correction coefficient and the fusion resistance coefficient to obtain all the final preparation process parameters; and to prepare the asphalt pavement material according to all the final preparation process parameters.
[0036] After a comprehensive analysis of the rutting resistance modification target and the material fusion resistance characteristics, in order to overcome the limitations of traditional fixed process parameters that cannot adapt to the complex and ever-changing characteristics of waste materials and the demanding environmental requirements, it is necessary to establish an adaptive control mechanism that can dynamically respond to material characteristics. Therefore, based on the coupling relationship between the rutting resistance requirement modification coefficient and the fusion resistance coefficient, the key preparation process parameters of the new recycled asphalt pavement material (including modifier dosage, mixing time, mixing temperature, and number of compaction passes) are adjusted in real time and with precision to determine all the final preparation process parameters. This process achieves a technological leap from "qualitative experience design" to "quantitative precise control," ensuring that the production of each batch of recycled material is within the optimal process window, which not only fully stimulates the effectiveness of the modifier but also avoids the aging risk caused by over-mixing, significantly improving the flexibility of the preparation process and the performance consistency of the finished product.
[0037] Finally, asphalt pavement materials are prepared based on all adaptively determined final preparation process parameters. This effectively overcomes the shortcomings of existing technologies, which suffer from poor rutting resistance due to the neglect of differences in the aging of old materials and actual environmental requirements caused by the use of fixed conventional preparation processes. This makes it more accurate to prepare new recycled asphalt pavement materials with high rutting resistance for different service environments and waste material conditions.
[0038] Preferably, in some possible implementations of the embodiments of the present invention, the process of obtaining the degree of aging of the asphalt phase includes: The RAP asphalt penetration of the current RAP material is standardized by pre-setting a standard asphalt penetration to determine the degree of adhesion aging of the current RAP material; the asphalt softening temperature of the current RAP material is standardized by pre-setting a standard asphalt softening temperature to determine the softening point growth rate of the current RAP material; and the asphalt phase aging degree of the current RAP material is determined based on the average between the degree of adhesion aging and the softening point growth rate.
[0039] In one specific implementation of this invention, the process of obtaining the degree of aging of the asphalt phase is expressed by the following formula: ;in, The current aging degree of the asphalt phase in the RAP material; Preset standard asphalt penetration; The RAP bitumen penetration of the current RAP material; This refers to the current asphalt softening temperature of the RAP material. The preset standard asphalt softening temperature; This represents the current adhesion aging level of the RAP material; This represents the softening point growth rate of the current RAP material. In one specific implementation of this invention, the preset standard asphalt penetration is set to 7 mm, and the preset standard asphalt softening temperature is set to 50 degrees Celsius. These settings are made by consulting the initial asphalt grade recorded in the original pavement design and construction archives, or by referring to the technical indicators of the corresponding base asphalt in the current highway asphalt pavement construction technical specifications, to ensure that the reference system for aging assessment conforms to the original design standards of the road section. This can be adjusted according to the specific implementation environment.
[0040] The initial design of this quantitative system aims to comprehensively characterize the evolution of the colloidal structure of waste asphalt during long-term service due to the loss of lightweight components and the increase in the proportion of asphaltite, through complementary evaluation of two dimensions: consistency and high-temperature stability. The standardized treatment of the penetration index aims to quantify the degree of attenuation of asphalt adhesive strength, reflecting the loss of its resistance to fatigue cracking; while the introduction of the softening point growth rate focuses on characterizing the hardening drift of asphalt's temperature-sensitive properties, revealing the negative impact of increased material brittleness on the impact resistance of recycled pavements. Coupled calculation of the two values effectively eliminates evaluation biases caused by local contamination or random experimental errors in a single index, thus forming a "stiffness index" that can stably characterize the true aging depth of the asphalt phase. This comprehensive evaluation result not only provides core input for the subsequent accurate determination of the overall aging degree but also serves as key logical support for the adaptive control of composite modifier dosage and mixing process parameters. This enables deep fusion of the new and old asphalt interfaces through precise performance compensation during the recycling process, improving the high-temperature stability of the recycled mixture from the perspective of molecular chain segment recovery, and laying a solid foundation for the physical property analysis of new pavement materials with long-term rutting resistance.
[0041] Preferably, in some possible implementations of the embodiments of the present invention, the process of obtaining the overall aging degree includes: Calculate the difference between the preset standard moisture content and the current moisture content of the RAP material to determine the reference moisture content difference; determine the current RAP material's moisture content exceedance rate based on the ratio between the reference moisture content difference and the preset standard moisture content; determine the current RAP material's sand content exceedance rate based on the calculation principle of moisture content exceedance rate, using the preset standard sand content and the current RAP material's sand content as the basis; determine the aggregate phase aging degree based on the average of the moisture content exceedance rate and the sand content exceedance rate; determine the overall aging degree based on the average of the aggregate phase aging degree and the asphalt phase aging degree.
[0042] In the actual production process, the underlying technological motivation for establishing an assessment system for the aging degree of aggregate phases lies in the fact that the rutting resistance of recycled asphalt mixtures depends not only on the rheological recovery of the asphalt phase, but also on the stringent constraints of the physical state and cleanliness of the aggregate surface. Fluctuations in the moisture content index directly reflect the degree to which the old aggregate has captured moisture during storage or service. High moisture content will generate a large amount of water vapor during mixing, which not only consumes heat energy and leads to uncontrolled mixing temperature, but also forms a "water film" on the aggregate surface that hinders asphalt wetting, inducing the risk of interfacial delamination. On the other hand, an excessive sand content (specifically referring to the content of muddy dust) reflects the degree of pollution and deterioration of the aggregate surface. Excessive fine particles will devour the effective components in the matrix asphalt and form a weak interlayer between the old and new interfaces, seriously weakening the skeleton density and high-temperature stability of the mixture.
[0043] By quantifying the benchmark deviations of moisture content and sand content, these complex physical disturbances can be transformed into standardized exceedance rate factors. The aggregate phase aging degree determined by this factor accurately characterizes the health status of the "physical skeleton" of waste materials. In a specific implementation of this embodiment, to ensure the rigor of the calculation logic and the rationality of the physical meaning, when calculating the difference between the reference moisture content and the reference sand content, if the measured value of the current RAP material is less than or equal to the preset standard value (i.e., not exceeding the standard), the corresponding difference is recorded as 0, and the corresponding exceedance rate is also recorded as 0. This ensures that the aging assessment model focuses on capturing the risk of performance degradation and avoids excellent indicators masking potential defects. Finally, the aggregate phase aging degree is coupled with the previously determined asphalt phase aging degree using the mean value. The resulting overall aging degree achieves closed-loop coverage of the "full component, full phase" attenuation trajectory of recycled pavement materials. This comprehensive evaluation index not only eliminates the limitations of single-index evaluation but also provides a crucial basis for performance defect compensation for subsequent adaptive control of composite modifier dosage and mixing process parameters.
[0044] In some possible implementations of this invention, the process of obtaining the degree of aggregate phase aging is expressed by the following formula: ;in, The degree of aging of the aggregate phase in the current RAP material; The preset standard moisture content; This represents the current moisture content of the RAP material. This is the reference moisture content difference for the current RAP material; The current rate of moisture content exceeding the standard in RAP material; The preset standard sand content; This represents the current sand content of the RAP material; This represents the current rate of sand content exceeding the standard in RAP material. In one specific implementation of this invention, the preset standard moisture content is set to 2%, and the preset standard sand content is set to 0.7%. These settings are made according to the technical specifications for highway asphalt pavement construction or determined based on the results of indoor calibration tests of raw materials from different construction batches. The aim is to establish an ideal physical performance reference system for the aging assessment of aggregate phases, which can be adjusted according to the specific implementation environment.
[0045] Preferably, in some possible implementations of the embodiments of the present invention, the process of obtaining the basic rutting resistance demand coefficient includes: In all historical temperature data at the construction site, the cumulative value of all historical temperature data exceeding the preset high temperature threshold is positively correlated to determine the high temperature sensitivity coefficient; the foundation anti-rutting requirement coefficient is determined based on the product between the high temperature sensitivity coefficient and the preset dynamic stability benchmark value corresponding to the structural layer at the construction site.
[0046] By statistically analyzing the cumulative temperature values exceeding a preset high-temperature threshold, the total extreme thermal effects experienced by the construction site over a historical period can be scientifically characterized. Its physical significance lies in quantifying the cumulative driving force of ambient temperature on the softening and flow deformation of asphalt binder. This cumulative value is converted into a high-temperature sensitivity coefficient through a positive correlation mapping and multiplied with a preset dynamic stability benchmark value. Its core function is to transform "qualitative climatic conditions" into "quantitative design standards." This step ensures that the performance targets of recycled materials can be dynamically locked to a lower limit based on the severity of the construction site's climate, effectively solving the problem of insufficient rutting resistance reserves caused by neglecting regional high-temperature differences in traditional processes. Through this differentiated design based on environmental characteristics, a precise performance foundation is established for the adaptive adjustment of subsequent preparation parameters, significantly improving the reliability of recycled pavement against high-temperature plastic deformation from the perspective of environmental adaptability.
[0047] In one specific implementation of this invention, the process of obtaining the basic rutting resistance requirement coefficient is expressed by the formula: ;in, The basic rutting resistance demand coefficient; The preset dynamic stability reference value; This is the cumulative value of all historical temperature data that are greater than the preset high temperature threshold; This is a normalization function. The normalization object here is selected from the historical temperature data of all construction sites stored in the historical database. The high temperature sensitivity coefficient is used. In this embodiment of the invention, the preset high temperature threshold is set to 30 degrees Celsius, which can be adjusted automatically according to the climate zone level in the pavement design specifications and the critical temperature of historical pavement high temperature defects in the specific implementation environment. The preset dynamic stability benchmark value is set to a range of 800-3000 times / mm, and is preferably set to 1500 times / mm in this embodiment of the invention. It is set with reference to the highway engineering quality inspection and evaluation standards. The purpose of setting this benchmark value is to provide a basic reference for the pavement's resistance to deformation under standard temperature and humidity conditions. It can be adjusted automatically according to the specific implementation environment, which will not be elaborated further here.
[0048] Preferably, in some possible implementations of the embodiments of the present invention, the process of obtaining the rutting resistance requirement correction coefficient includes: The actual rutting resistance requirement coefficient is determined by multiplying the positive correlation mapping value of the overall aging degree with the basic rutting resistance requirement coefficient; the rutting resistance requirement correction coefficient is determined by the ratio between the actual rutting resistance requirement coefficient and the preset requirement benchmark value. In a specific implementation of this invention, the preset requirement benchmark value is set to a range of 3000-5000 times / mm, and is preferably set to 3000 times / mm in this embodiment. It is set by referring to the upper limit index of dynamic stability of high-performance modified asphalt pavement under extremely harsh high-temperature conditions or the deformation limit performance requirements within the design life of the target pavement, and can be adjusted according to the specific implementation environment. In one specific implementation of this invention, the process of obtaining the positive correlation mapping value of the overall aging degree includes: taking the sum between twice the overall aging degree and the real number 1 as the overall aging degree, using it to establish a linear compensation benchmark for performance degradation, and converting the loss of adhesive force caused by micro-aging of the material into a safety redundancy of macro-design strength, so that when the RAP material is under extreme aging, the dynamic stability assessment standard can be significantly improved, and the high dosage of modifier can be forcibly guided to compensate for interfacial bonding defects, ensuring that the skeleton stability coefficient of the recycled mixture meets the design requirements.
[0049] The core logic behind introducing this correction system lies in establishing a synergistic compensation mechanism between "material aging defects" and "external environmental loads." By applying a secondary weighting to the basic rutting resistance requirement coefficient through the positive correlation mapping value of the overall aging degree, the physical meaning lies in quantifying the negative contribution of waste materials due to embrittlement and loss of adhesion to the stability of the pavement structure, and transforming it into an additional performance requirement increment. The function of this step is to deeply couple external environmental threats with the internal shortcomings of the old material, forming a standard that can realistically characterize the true rutting resistance capability required for recycled pavements under complex service conditions. The final rutting resistance requirement correction coefficient, derived through ratio calculation, is essentially a dimensionless "performance gap coefficient," precisely identifying the performance gap that current recycling processes need to compensate for through modifiers and mixing and compaction. This dual correction, from environmental benchmarks to material properties, ensures highly targeted adaptive adjustments to subsequent preparation process parameters, significantly improving the rutting resistance accuracy and service durability of new recycled asphalt pavement materials under high-proportion RAP addition conditions.
[0050] Preferably, in some possible implementations of the embodiments of the present invention, the process of obtaining the fusion drag coefficient includes: The difference between the penetration of the base asphalt to be added and the penetration of the preset standard asphalt is used as the reference base difference. The absolute value of the ratio between the reference base difference and the preset standard asphalt penetration is negatively correlated to determine the benchmark asphalt matching degree. The performance matching coefficient of the base asphalt to be added is determined based on the maximum value between the benchmark asphalt matching degree and the lower limit of the preset matching degree.
[0051] The core physical significance of introducing the performance matching coefficient lies in quantifying the compatibility base of the penetration and fusion of new and old asphalt at the microscopic level. The reference matrix difference can objectively characterize the degree to which the new asphalt deviates from the standard performance. The smaller the difference, the stronger the wetting and diffusion ability of the new asphalt to the aged components, which is more conducive to the deep repair of the interface. The purpose of introducing the benchmark asphalt matching degree here is to standardize and make the relevant relationships correspond. The function of setting the preset matching degree lower limit (set to 0.1 in this embodiment of the invention, which can be adjusted according to the target dynamic modulus requirements of the recycled asphalt mixture, the shear strength standard of the fusion interface between new and old asphalt, and the precision control limit of the production equipment in the specific implementation environment) is to establish a physical safety boundary for the calculation logic, avoid calculation crashes caused by abnormal parameter fluctuations under extreme working conditions, and ensure that the system always outputs stable adjustment commands.
[0052] In one specific implementation of this invention, the process of obtaining the benchmark asphalt matching degree is expressed by the following formula: ;in, The baseline asphalt matching degree is used to determine the base asphalt to be added; The matrix penetration of the base bitumen to be added; Preset standard asphalt penetration; This is the reference matrix difference value for the base asphalt to be added.
[0053] The weighted matching coefficient is determined by multiplying the preset first weight and the performance matching coefficient; the weighted adaptation coefficient is determined by multiplying the preset second weight and the gradation adaptation coefficient; and the weighted aging coefficient is determined by multiplying the negative correlation mapping value of the overall aging degree and the preset third weight.
[0054] The preset weights are designed to quantify the different contributions of new asphalt activity, aggregate gradation skeleton, and old material aging depth to the fusion efficiency of the new and old interfaces. The first and third preset weights are typically set relatively high (in this embodiment, the first preset weight is set to 0.3, and the third preset weight is set to 0.5). This is because the chemical compatibility of the asphalt components and the hardening degree of the old material are the core dominant factors determining the strength of the recycled mixture. The second preset weight (in this embodiment, the second preset weight is set to 0.2) focuses on providing auxiliary support from the gradation adaptation dimension of the physical skeleton and can be adjusted according to the emphasis on different dimensions in the specific implementation environment. Through multi-dimensional weighted calculations, key bottlenecks affecting the recovery of material properties during the preparation process can be comprehensively identified.
[0055] The fusion resistance coefficient is determined by negatively mapping the sum of the weighted matching coefficient, weighted adaptation coefficient, and weighted aging coefficient. The fusion resistance coefficient is essentially a "difficulty index" characterizing the achievement of an ideal fusion state between new and old components during the regeneration process. A larger coefficient indicates stronger interfacial fusion resistance, requiring subsequent steps to increase the dosage of reinforcing modifiers or improve mixing energy to overcome this bottleneck. This step transforms the chemical compatibility and physical complementarity between materials into a quantified resistance signal, providing precise decision feedback for the final adaptive and refined control of the preparation process parameters.
[0056] In one specific implementation of this invention, the method for negatively mapping the sum of the weighted matching coefficient, weighted adaptation coefficient, and weighted aging coefficient uses the reciprocal. That is, the reciprocal of the sum of the weighted matching coefficient, weighted adaptation coefficient, and weighted aging coefficient is used as the fusion resistance coefficient. If the sum of the weighted matching coefficient, weighted adaptation coefficient, and weighted aging coefficient is 0, then 0.01 is used instead of the sum for reciprocal processing to avoid the problem of the denominator being 0. Implementers can adjust the negative correlation mapping method according to the specific implementation environment, for example, using the reciprocal of the exponential function with the natural constant as the base for negative correlation mapping, which will not be further elaborated here.
[0057] Preferably, in a specific implementation of this invention, the process of obtaining the final preparation process parameters includes: The initial fusion adjustment value is determined based on the maximum value between the fusion resistance coefficient and the preset lower limit protection parameter; the fusion adjustment coefficient is determined based on the minimum value between the initial fusion adjustment value and the preset upper limit protection parameter. In a specific implementation of this invention, the preset lower limit protection parameter is set to 0.8, and the preset upper limit protection parameter is set to 1.2. By setting the preset lower limit protection parameter and the preset upper limit protection parameter, the initial fusion adjustment value is truncated in both directions. The purpose is to establish a physical safety boundary for the production process, which can be adjusted automatically according to the specific implementation environment. This process can effectively avoid drastic fluctuations in process parameters caused by abnormal front-end sensor data or extreme proportions, ensuring that the fusion adjustment coefficient is always within a safe range that is controllable by the equipment and where the asphalt properties are stable, and preventing instability in the quality of recycled materials due to over-correction.
[0058] The theoretical dosage multiple is determined by multiplying the rutting resistance correction coefficient and the fusion resistance coefficient. The initial dosage adjustment value is determined by the maximum value between the theoretical dosage multiple and the preset lower limit protection parameter. The composite modifier dosage adjustment coefficient is determined by the minimum value between the initial dosage adjustment value and the preset upper limit protection parameter. In determining the composite modifier dosage adjustment coefficient, the product of the rutting resistance correction coefficient and the fusion resistance coefficient is used to achieve dual compensation for both "performance gaps" and "fusion obstacles." Higher requirements and greater resistance necessitate a higher theoretical dosage multiple, thus guiding the modifier towards targeted enhancement. Through upper and lower limit protection, it is ensured that the modifier dosage meets the requirements for improved high-temperature stability without causing a surge in mixture costs or a decrease in low-temperature crack resistance due to excessive addition.
[0059] The preliminary demand adjustment value is determined based on the maximum value between the rutting resistance demand correction coefficient and the preset lower limit protection parameter; the actual rutting resistance demand adjustment coefficient is determined based on the minimum value between the preliminary demand adjustment value and the preset upper limit protection parameter. The calculation logic for the actual rutting resistance demand adjustment coefficient is introduced to directly translate the correction pressure determined by environmental load and aging degree into control commands at the process end. The adjustment coefficient determined through the limit protection mechanism ensures that the final process is both sensitive and robust to high-temperature risks. This step serves to provide a quantitative "demand benchmark" for subsequent parameter adjustments, ensuring that the strength design margin of the recycled pavement remains within the reasonable range required by specifications.
[0060] Based on the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the actual rutting resistance requirement adjustment coefficient, the final preparation process parameters are determined. Specifically, the final mixing time parameter is determined by multiplying the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the preset mixing time. When determining the final mixing time parameter, the fusion adjustment coefficient and the dosage adjustment coefficient are introduced into the product calculation. The purpose is to address the time requirement for uniform dispersion of the modifier and deep exchange at the interface between new and old asphalt. The greater the resistance or the higher the dosage, the longer the mixing time is automatically applied. The physical meaning of this is to forcibly overcome the compatibility barrier through continuous input of mechanical energy, ensuring macroscopic uniformity and thorough microscopic fusion of the mixture, thereby eliminating the risk of loosening and peeling.
[0061] In one specific implementation of this invention, the preset mixing time ranges from 45 seconds to 60 seconds. In this embodiment, it is preferably set to 50 seconds. The preparation of recycled asphalt involves heat exchange between new and old aggregates, softening of old asphalt, and diffusion between new and old asphalt. 50 seconds can ensure that the heat of the new aggregate is fully transferred to the cold RAP material, so that the aged asphalt reaches the softening point and undergoes micro-diffusion with the new asphalt. It can be adjusted according to the technical specifications for highway asphalt pavement construction, and will not be elaborated further here.
[0062] The final mixing base temperature parameter is determined by rounding down the product of the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the preset mixing base temperature. The core logic for obtaining the final mixing base temperature parameter is to reduce the viscosity of the mixture under high resistance or high modifier dosage conditions through thermal energy compensation. Appropriately increasing the mixing temperature can significantly improve the melting and dispersion efficiency of the modifier and the activity of the old asphalt. However, in this embodiment, a preset upper limit value for the mixing temperature (set to 185℃ in this embodiment, but adjustable according to the specific implementation environment) will be used as a constraint. That is, if the calculated final mixing base temperature parameter is greater than the preset upper limit value, the preset upper limit value will be used as the final mixing base temperature parameter to prevent excessively high temperatures from inducing secondary aging of the asphalt and to ensure thermodynamic balance during the recycling process. In one specific implementation of this invention, the preset mixing base temperature ranges from 150°C to 170°C. In this embodiment, it is preferably set to 160°C. The preset mixing base temperature is set by consulting the standard construction technical specifications corresponding to the type and grade of the base asphalt used, ensuring that the preset mixing base temperature meets the fluidity requirements of the new asphalt under standard working conditions. It can be adjusted according to the technical specifications for highway asphalt pavement construction, and will not be elaborated further here.
[0063] The final number of compaction passes is determined by rounding down the product of the positive correlation mapping value of the composite modifier dosage adjustment coefficient, the fusion adjustment coefficient, the actual rutting resistance requirement adjustment coefficient, and the preset number of compaction passes.
[0064] In one specific implementation of this invention, the process of obtaining the final number of compaction passes parameter is expressed by the following formula: ;in, This is the parameter for the final number of compaction passes; The preset number of compaction passes; This is a fusion adjustment factor; This is the adjustment coefficient for the dosage of the composite modifier; Adjust the coefficient to reflect the actual rutting resistance requirements; This is a floor function; when determining the final number of compaction passes, the coupling of three adjustment coefficients aims to establish the optimal energy input value to achieve the design compaction degree. Since high modifier content increases the construction viscosity of the mixture, the compaction strength needs to be adjusted through positive correlation mapping. The physical significance of this is to ensure that the recycled mixture forms a stable skeleton interlocking structure before cooling. This step directly determines the final density and rutting stiffness of the recycled pavement, and is a key engineering guarantee for achieving the design goals.
[0065] In one specific implementation of this invention, the preset number of compaction passes ranges from 8 to 12. In this embodiment, it is preferably set to 10, which includes the complete cycle of initial compaction (2 passes), intermediate compaction (6 passes), and final compaction (2 passes). This value can ensure that the mixture reaches more than 95% of the Marshall standard compaction degree under standard conditions, forming a stable skeleton dense structure. It can be adjusted by the highway asphalt pavement construction technical specifications, which will not be elaborated further here.
[0066] In summary, a recycled asphalt pavement material preparation system acquires historical temperature data from the construction site, the matrix penetration of the base asphalt to be added, and the multidimensional physical indicators of the current RAP material. Based on the benchmark deviations of each indicator, it determines the aging degree of the asphalt phase and the overall aging degree layer by layer, thus comprehensively and objectively quantifying the true performance degradation state of the waste material. Simultaneously, it determines the base rutting resistance requirement coefficient by combining the high-temperature characteristic distribution of historical temperature data from the construction site, and obtains a rutting resistance requirement correction coefficient by weighting it with the overall aging degree. This ensures that the material's performance design standards fully meet the stringent requirements of the actual environment. Furthermore, the fusion resistance coefficient, determined by coupling the matrix penetration, overall aging degree, and gradation compatibility coefficient, is used to comprehensively evaluate the matching difficulty during the mixing process of new and old materials. Finally, based on the rutting resistance correction coefficient and the fusion resistance coefficient, the preparation process parameters of the new recycled asphalt pavement material are adaptively adjusted and prepared. This effectively overcomes the shortcomings of the existing technology, which ignores the aging differences of old materials and actual environmental requirements due to the use of fixed conventional preparation processes, resulting in poor rutting resistance. This makes the preparation of new recycled asphalt pavement materials with high rutting resistance performance for different service environments and waste material states more accurate.
[0067] This invention also provides a computer device; please refer to [link / reference]. Figure 2 The diagram illustrates a computer device structure according to an embodiment of the present invention. The computer device includes a memory 201, a processor 202, and a computer program 203 stored in the memory 201 and running on the processor 202. When the processor 202 executes the computer program 203, the computer device can execute any of the aforementioned recycled asphalt pavement material preparation systems.
[0068] This invention also provides a computer program product that, when run on a computer device, enables the computer device to execute any of the aforementioned recycled asphalt pavement material preparation systems.
[0069] This invention also provides a computer-readable storage medium storing computer program code, which, when run on a computer device, enables the computer device to execute any of the aforementioned recycled asphalt pavement material preparation systems.
[0070] In the embodiments provided by the present invention, it should be understood that the computer device, computer program product and computer-readable storage medium provided are all used to execute the corresponding system provided above, and therefore the beneficial effects they can achieve can be referred to the beneficial effects of the system provided above, which will not be repeated here.
[0071] It should be noted that the order of the above embodiments of the present invention is merely for descriptive purposes and does not represent the superiority or inferiority of the embodiments. The processes depicted in the accompanying drawings do not necessarily require a specific or sequential order to achieve the desired result. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.
[0072] The various embodiments in this specification are described in a progressive manner. The same or similar parts between the various embodiments can be referred to each other. Each embodiment focuses on describing the differences from other embodiments.
Claims
1. A system for preparing recycled asphalt pavement materials, characterized in that, The system includes: The data acquisition and preprocessing module is used to acquire all historical temperature data of the construction site, the matrix penetration of the base asphalt to be added and the RAP asphalt penetration of the current RAP material, asphalt softening temperature, moisture content and sand content; and to determine the gradation compatibility coefficient between the aggregate to be added and the current RAP material. The first determining module is used to determine the corresponding degree of asphalt phase aging based on the benchmark deviation between the RAP asphalt penetration and asphalt softening temperature of the current RAP material; and to determine the corresponding overall aging degree based on the benchmark deviation between the moisture content and sand content of the current RAP material and the degree of asphalt phase aging. The second determining module is used to determine the rutting resistance requirement coefficient of the foundation based on the high temperature characteristic distribution of historical temperature data at the construction site; to determine the rutting resistance requirement correction coefficient by weighting the foundation rutting resistance requirement coefficient with the overall aging degree; and to determine the fusion resistance coefficient by coupling the matrix penetration, the overall aging degree and the gradation adaptation coefficient. The asphalt pavement material preparation module is used to adjust the preparation process parameters of the new recycled asphalt pavement material based on the rutting resistance requirement correction coefficient and the fusion resistance coefficient to obtain all the final preparation process parameters; and to prepare the asphalt pavement material according to all the final preparation process parameters.
2. The recycled asphalt pavement material preparation system according to claim 1, characterized in that, The process of obtaining the degree of aging of the asphalt phase includes: The RAP asphalt penetration of the current RAP material is standardized by setting a preset standard asphalt penetration to determine the degree of adhesion aging of the current RAP material; the asphalt softening temperature of the current RAP material is standardized by setting a preset standard asphalt softening temperature to determine the rate of increase of softening point of the current RAP material. The degree of asphalt phase aging of the current RAP material is determined based on the average between the degree of adhesive aging and the growth rate of the softening point.
3. The recycled asphalt pavement material preparation system according to claim 1, characterized in that, The process of obtaining the overall aging degree includes: Calculate the difference between the preset standard moisture content and the current moisture content of the RAP material to determine a reference moisture content difference; determine the moisture content excess rate of the current RAP material based on the ratio between the reference moisture content difference and the preset standard moisture content; determine the sand content excess rate of the current RAP material based on the calculation principle of the moisture content excess rate and the sand content of the current RAP material; determine the aggregate phase aging degree based on the average of the moisture content excess rate and the sand content excess rate. The overall aging degree is determined based on the average value between the aging degree of the aggregate phase and the aging degree of the asphalt phase.
4. The recycled asphalt pavement material preparation system according to claim 1, characterized in that, The process of obtaining the basic rutting resistance requirement coefficient includes: In all historical temperature data at the construction site, the cumulative value of all historical temperature data exceeding the preset high temperature threshold is positively correlated to determine the high temperature sensitivity coefficient. The rutting resistance requirement coefficient of the foundation is determined by multiplying the high temperature sensitivity coefficient with the preset dynamic stability benchmark value corresponding to the structural layer at the construction site.
5. The recycled asphalt pavement material preparation system according to claim 1, characterized in that, The process of obtaining the anti-rutting requirement correction coefficient includes: The corresponding actual rutting resistance requirement coefficient is determined by multiplying the positive correlation mapping value of the overall aging degree with the basic rutting resistance requirement coefficient. The rutting resistance requirement correction coefficient is determined based on the ratio between the actual rutting resistance requirement coefficient and the preset requirement benchmark value.
6. The recycled asphalt pavement material preparation system according to claim 1, characterized in that, The process of obtaining the fusion resistance coefficient includes: The difference between the penetration of the base asphalt to be added and the penetration of the preset standard asphalt is used as the reference base difference; the absolute value of the ratio between the reference base difference and the preset standard asphalt penetration is negatively correlated to determine the benchmark asphalt matching degree; the performance matching coefficient of the base asphalt to be added is determined based on the maximum value between the benchmark asphalt matching degree and the preset matching degree lower limit. The weighted matching coefficient is determined by multiplying the preset first weight with the performance matching coefficient; the weighted adaptation coefficient is determined by multiplying the preset second weight with the gradation adaptation coefficient; and the weighted aging coefficient is determined by multiplying the negative correlation mapping value of the overall aging degree with the preset third weight. The fusion resistance coefficient is determined by negatively mapping the sum of the weighted matching coefficient, the weighted adaptation coefficient, and the weighted aging coefficient.
7. The recycled asphalt pavement material preparation system according to claim 1, characterized in that, The process of obtaining the final preparation process parameters includes: A preliminary fusion adjustment value is determined based on the maximum value between the fusion resistance coefficient and the preset lower limit protection parameter; a fusion adjustment coefficient is determined based on the minimum value between the preliminary fusion adjustment value and the preset upper limit protection parameter. The theoretical dosage multiple is determined by multiplying the rutting resistance correction coefficient and the fusion resistance coefficient; the preliminary dosage adjustment value is determined by the maximum value between the theoretical dosage multiple and the preset lower limit protection parameter; and the composite modifier dosage adjustment coefficient is determined by the minimum value between the preliminary dosage adjustment value and the preset upper limit protection parameter. The preliminary demand adjustment value is determined based on the maximum value between the anti-rutting demand correction coefficient and the preset lower limit protection parameter; the actual anti-rutting demand adjustment coefficient is determined based on the minimum value between the preliminary demand adjustment value and the preset upper limit protection parameter. The final preparation process parameters are determined based on the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the actual rutting resistance requirement adjustment coefficient.
8. The recycled asphalt pavement material preparation system according to claim 2, characterized in that, The process of obtaining the degree of adhesive aging includes: A reference penetration difference is determined based on the difference between the preset standard asphalt penetration and the current RAP material's RAP asphalt penetration; the degree of adhesion aging of the current RAP material is determined based on the ratio between the reference penetration difference and the preset standard asphalt penetration.
9. The recycled asphalt pavement material preparation system according to claim 2, characterized in that, The process of obtaining the softening point growth rate includes: A reference softening temperature difference is determined based on the difference between the current RAP material's asphalt softening temperature and the preset standard asphalt softening temperature; the softening point growth rate of the current RAP material is determined based on the ratio between the reference softening temperature difference and the preset standard asphalt softening temperature.
10. A system for preparing recycled asphalt pavement material according to claim 7, characterized in that, The process of determining the final preparation process parameters based on the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the actual rutting resistance requirement adjustment coefficient includes: The final mixing time parameter is determined by multiplying the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the preset mixing time. The product of the fusion adjustment coefficient, the composite modifier dosage adjustment coefficient, and the preset mixing base temperature is rounded down to determine the final mixing base temperature parameter. The final number of compaction passes is determined by rounding down the product of the positive correlation mapping value of the composite modifier dosage adjustment coefficient, the fusion adjustment coefficient, the actual rutting resistance requirement adjustment coefficient, and the preset number of compaction passes.