A VCM flexible printed coil structure and its manufacturing method

By integrally printing planar spiral conductive lines on a flexible insulating substrate and adopting a segmented gradient sintering process, the problems of large thickness and process defects of VCM actuation coils were solved, achieving ultra-thin camera module adaptation and high-precision driving effect.

CN123120460APending Publication Date: 2026-11-17FUTURE FIREFLY TECHNOLOGY (SHENZHEN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611304163.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-26
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

The existing VCM actuator coils are thick and cannot be adapted to ultra-thin camera modules of less than 5mm. In addition, there are defects such as pinholes and cracks in the printing process, and the inductance consistency and thrust linearity are insufficient, making it difficult to meet the high-precision drive requirements of high-end OIS modules.

Method used

A planar spiral conductive circuit is integrally printed on a flexible insulating substrate. Combined with segmented gradient sintering process and roll-to-roll continuous printing, single-layer, double-layer and multi-layer stacked VCM flexible printed coils are prepared. The conductive phase is formed by low-temperature pre-baking, medium-temperature glue removal and high-temperature metallization sintering, which simplifies the production process and improves the quality of the circuit.

Benefits of technology

It achieves controllable overall coil thickness, controllable inductance dispersion, significantly improved thrust linearity, and significantly improved mass production yield, meeting the high-precision drive requirements of high-end OIS modules and reducing production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention discloses a VCM flexible printed coil structure and its manufacturing method, belonging to the technical field of miniature camera actuators. The coil structure includes a flexible insulating substrate and a planar spiral conductive line integrally printed on it. The conductive line width is 20μm to 100μm, continuously formed without segmented splicing breaks, and arranged in single-layer, double-layer, and multi-layer stacked configurations. The manufacturing method includes substrate plasma activation pretreatment, one-time printing of conductive paste using a screen, segmented gradient sintering and curing, insulation encapsulation, and slitting. The segmented gradient sintering involves three temperature-controlled processes: low-temperature pre-baking, medium-temperature adhesive removal, and high-temperature metallization sintering. The coil of this invention has controllable overall thickness, low inductance dispersion, and high mass production yield, making it suitable for ultra-thin camera modules below 5mm and high-end OIS optical image stabilization drive requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of miniature camera actuator technology, specifically relating to a VCM flexible printed coil structure and its manufacturing method. Background Technology

[0002] The mainstream solution for VCM actuation coils in the built-in camera modules of current consumer electronics mobile phones and tablets is to use enameled copper wire wound coils. This solution requires a plastic or metal winding frame, and the total thickness of the coil body and the frame is relatively large, which cannot be adapted to thinner and lighter terminal devices. The winding process involves a lot of manual intervention, resulting in poor consistency between coil inductance and thrust, and low batch yield.

[0003] Alternative solutions such as flexible etched circuit coils and printed conductive coils are gradually emerging in the industry. Flexible etched copper foil coils are limited by the minimum thickness of the copper foil substrate and the lateral etching effect, resulting in bottlenecks in miniaturization of linewidth and spacing. Multi-layer stacking requires laminating dry film, leading to significant thickness increases between layers. Furthermore, the etching process suffers from high copper foil loss, a long process chain, and high equipment and environmental treatment costs. While existing printed conductive coils offer improvements in thickness and process, the uniformity of circuit conductivity and the linearity of push force still need further enhancement.

[0004] In addition, the sintering step of the existing printed coil manufacturing process uses a single constant temperature treatment, and the slurry solvent and organic carrier evaporate rapidly and simultaneously. This makes the circuit prone to pinholes and cracks, resulting in large coil resistance deviations and insufficient thrust linearity, which makes it difficult to meet the high-precision drive requirements of high-end image stabilization OIS modules. Summary of the Invention

[0005] The purpose of this invention is to provide a VCM flexible printed coil structure and its manufacturing method to solve the problem that the existing VCM actuation coil has a large overall thickness and cannot be adapted to ultra-thin camera modules below 5mm. At the same time, the printing and sintering process is optimized to reduce pinholes and cracks in the circuit, improve inductance consistency and thrust linearity, and meet the high-precision driving requirements of high-end OIS optical image stabilization modules.

[0006] The present invention adopts the following technical solution:

[0007] This solution provides a VCM flexible printed coil structure, including a flexible insulating substrate and a planar spiral conductive line integrally printed on the flexible insulating substrate; the line width of the conductive line is 20μm to 100μm, the conductive line is continuously formed and has no segmented splicing breaks; the planar spiral conductive line adopts a single-layer, double-layer and multi-layer stacked arrangement.

[0008] Furthermore, the flexible insulating substrate is a polyimide film with a thickness of 5 μm to 25 μm; the spacing between adjacent conductive lines is 10 μm to 50 μm; and the outer side of the conductive lines is covered with an insulating protective coating.

[0009] Furthermore, in the multi-layer stacked arrangement, an insulating isolation layer is provided between two adjacent layers of conductive lines, and the two adjacent layers of conductive lines achieve circuit conduction through conductive lap posts.

[0010] Furthermore, the conductive circuit is formed by printing and sintering a conductive paste, wherein the conductive paste comprises, by mass fraction: 60% to 85% conductive metal powder, 12% to 35% organic carrier, 0.5% to 3% insulating rheology modifier, and 0.1% to 2% sintering accelerator; the conductive metal powder is selected from silver powder and silver-palladium alloy powder.

[0011] This invention also provides a method for manufacturing a VCM flexible printed coil structure, comprising the following steps:

[0012] S1 Substrate Pretreatment: Plasma activation cleaning is performed on the surface of the roll-shaped flexible insulating substrate to remove the mold release agent on the substrate surface and improve the adhesion of the slurry.

[0013] S2 circuit printing: Conductive paste is used to form a planar spiral conductive circuit pattern in one go through screen printing, thus completing the circuit formation.

[0014] S3 segmented gradient sintering: The conductive circuit is cured by sequentially undergoing three temperature-controlled processes: low-temperature pre-baking, medium-temperature adhesive removal, and high-temperature metallization sintering. The low-temperature pre-baking temperature is 80℃, the medium-temperature adhesive removal temperature is 180℃, and the high-temperature metallization sintering temperature is 280℃; the low-temperature pre-baking time is 10 min, the medium-temperature adhesive removal time is 20 min, and the high-temperature metallization sintering time is 30 min, with the three temperature-controlled processes being carried out by continuous temperature increases.

[0015] S4 Insulating Encapsulation: An insulating protective coating is applied to the surface of the conductive lines and then dried and cured.

[0016] S5 slitting and forming: Cutting according to module size to obtain single finished coils.

[0017] Furthermore, the screen printing described in step S2 is a roll-to-roll continuous printing process.

[0018] Furthermore, when manufacturing coils in a multi-layer stacked arrangement, after the first layer of conductive lines is sintered and cured, an insulating layer is coated and conductive lap posts are prepared, and then the next layer of conductive lines is printed. The above process is repeated until the target number of stacked layers is reached, and finally the whole is insulated, encapsulated, and slit into shape.

[0019] The beneficial effects achieved by the present invention using the above solution are as follows:

[0020] 1. It adopts a planar spiral conductive circuit with integrated printing, covering single-layer, double-layer and multi-layer stacked arrangement. The coil has no winding skeleton, the overall thickness is controllable, and it can be adapted to ultra-thin mobile phone camera modules below 5mm. The integrated printed circuit has no segmented splicing breaks, the inductance dispersion is controllable, and the thrust linearity is greatly improved, meeting the high-precision drive requirements of optical image stabilization.

[0021] 2. A segmented gradient sintering process is adopted, which removes the slurry solvent by low-temperature pre-baking, decomposes the organic carrier by medium-temperature debinding, and forms a conductive phase by high-temperature metallization sintering. This avoids the problems of pinholes, cracks and uneven resistance caused by single constant temperature sintering. The DC resistance deviation of the coil can be controlled, which improves the mass production yield.

[0022] 3. The roll-to-roll continuous printing process replaces the winding and etching processes, simplifying the production process, significantly reducing the cost per unit, and greatly improving the mass production yield. Attached Figure Description

[0023] Figure 1 This is a schematic diagram of the overall structure of the VCM flexible printed coil of the present invention;

[0024] Figure 2 This is a schematic diagram of the manufacturing process of the VCM flexible printed coil of the present invention. Detailed Implementation

[0025] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0026] like Figure 1 As shown, the VCM flexible printed coil structure of the present invention includes a flexible insulating substrate and a planar spiral conductive line integrally printed on the flexible insulating substrate, with lead-out terminals at both ends of the planar spiral conductive line.

[0027] like Figure 2 As shown, the manufacturing method of the VCM flexible printed coil of the present invention includes five steps in sequence: S1 substrate pretreatment, S2 circuit printing, S3 segmented gradient sintering, S4 insulation encapsulation and S5 slitting and forming. The S3 and segmented gradient sintering steps further include three stages of continuous temperature control treatment: low temperature pre-baking, medium temperature glue removal and high temperature metallization sintering. Example 1: Single-layer printed VCM coil

[0028] This embodiment provides a single-layer printed VCM coil, and the specific preparation process is as follows.

[0029] A 10μm thick polyimide film was selected as the flexible insulating substrate. The surface of the roll substrate was subjected to plasma activation cleaning to remove the mold release agent on the substrate surface and improve the adhesion of the slurry.

[0030] A planar spiral conductive circuit pattern with a line width of 50μm is formed on the surface of a substrate in one step by using conductive paste through screen printing. The spacing between adjacent conductive lines is 30μm.

[0031] The printed circuit is subjected to segmented gradient sintering: first, it is pre-baked at a low temperature of 80℃ for 10 minutes to remove the slurry solvent, then it is decomposed by removing the adhesive at a medium temperature of 180℃ for 20 minutes, and finally it is metallized and sintered at a high temperature of 280℃ for 30 minutes to form a conductive phase. The three-stage temperature control is carried out by continuous temperature increase.

[0032] An insulating protective coating is applied to the surface of the conductive circuit and dried and cured. The coil is then cut to the module size to obtain a single-piece finished single-layer printed VCM coil.

[0033] The single-layer printed VCM coil prepared in this embodiment has an overall thickness of 22μm, which is compatible with AF autofocus VCM modules. Example 2: Double-layer stacked printed VCM coil

[0034] This embodiment provides a double-layer stacked printed VCM coil, and the specific fabrication process is as follows.

[0035] A 15μm thick polyimide film was selected as the flexible insulating substrate. After plasma activation and cleaning, the first layer of planar spiral conductive circuit was formed by screen printing with conductive paste, and then cured by segmented gradient sintering.

[0036] An insulating layer is coated on the surface of the first layer of conductive circuits. Conductive lap posts are prepared at corresponding positions between the layers. Then, a second layer of reverse spiral conductive circuits is formed by screen printing with conductive paste. The second layer of circuits is connected to the first layer of circuits through the conductive lap posts.

[0037] The double-layer circuit is subjected to segmented gradient sintering and curing, coated with an insulating protective coating and dried, and then cut according to the module size to obtain the double-layer stacked printed VCM coil.

[0038] The inductance of the double-layer stacked printed VCM coil obtained in this embodiment is twice that of the single-layer structure, which is compatible with the OIS optical image stabilization VCM module, and the overall thickness of the module is controlled within 4.2mm.

[0039] Comparative example: Traditional enameled copper wire wound coil

[0040] This comparative example uses traditional enameled copper wire to wind the coil. Enameled copper wire of the same driving thrust specification is selected to wind a planar spiral coil on a plastic frame. The finished coil is obtained through spot welding, glue coating and shaping processes.

[0041] The coil produced in this comparative example has an overall thickness of 7.5 mm, an inductance dispersion of more than 10%, and a mass production yield of less than 85%. Compared with the printed coil of this invention, it has significant differences in terms of thinness, consistency, and mass production yield.

[0042] Comparative experimental data:

[0043] To verify the technical effect of the segmented gradient sintering process of the present invention, a control experiment was conducted under the same experimental standard: using the same 10μm polyimide substrate, 50μm linewidth single-layer spiral coil, the same batch of conductive paste and the same printing thickness, two sets of processes were adopted, namely conventional single isothermal sintering and the three-segment gradient sintering process of the present invention. 1000 samples were tested in each group, and the core test data are shown in the table below.

[0044]

[0045] As shown in the table above, after adopting the three-stage gradient sintering process of this invention, appearance defects such as pinholes, edge cracks and bubble protrusions in the circuit are significantly reduced, and the overall defect rate is reduced by 93.89%; the deviation of the coil DC resistance and the inductance dispersion are significantly reduced, the heat generation uniformity under full power drive is greatly improved, and the thrust linearity meets the high-precision drive requirements of high-end OIS modules.

[0046] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to the embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

[0047] The present invention and its embodiments have been described above. This description is not restrictive, and the accompanying drawings are only one embodiment of the present invention; the actual structure is not limited thereto. In conclusion, if those skilled in the art are inspired by this description and design similar structures and embodiments without departing from the spirit of the invention, such designs should fall within the protection scope of the present invention.

Claims

1. A VCM flexible printed coil structure, characterized by: It includes a flexible insulating substrate and a planar spiral conductive line integrally printed on the flexible insulating substrate; the line width of the conductive line is 20μm to 100μm, the conductive line is continuously formed and has no segmented splicing breaks; the planar spiral conductive line is arranged in single-layer, double-layer and multi-layer stacked form.

2. The VCM flexible printed coil structure according to claim 1, characterized in that: The flexible insulating substrate is a polyimide film with a thickness of 5 μm to 25 μm; the spacing between adjacent conductive lines is 10 μm to 50 μm; and the outer side of the conductive lines is covered with an insulating protective coating.

3. The VCM flexible printed coil structure of claim 1, wherein: In the multi-layer stacked arrangement, an insulating isolation layer is provided between two adjacent conductive lines, and the two adjacent conductive lines are connected by conductive bonding posts.

4. The VCM flexible printed coil structure of claim 1, wherein: The conductive circuit is formed by printing and sintering a conductive paste. The conductive paste comprises, by mass fraction: 60% to 85% conductive metal powder, 12% to 35% organic carrier, 0.5% to 3% insulating rheology modifier, and 0.1% to 2% sintering accelerator. The conductive metal powder is selected from silver powder and silver-palladium alloy powder.

5. A method of manufacturing a VCM flexible printed coil structure as claimed in any one of claims 1 to 4, characterized by: Includes the following steps; S1 Substrate Pretreatment: Plasma activation cleaning is performed on the surface of the roll-shaped flexible insulating substrate; S2 circuit printing: A planar spiral conductive circuit pattern is formed in one step by using conductive paste and screen printing. S3 segmented gradient sintering: The conductive circuit is solidified by three temperature-controlled processes: low-temperature pre-baking, medium-temperature debinding, and high-temperature metallization sintering. S4 Insulating Encapsulation: An insulating protective coating is applied to the surface of the conductive lines and then dried and cured. S5 slitting and forming: Cutting according to module size to obtain single finished coils.

6. The method of manufacturing a VCM flexible printed coil structure according to claim 5, wherein: The low-temperature pre-baking temperature in step S3 is 80°C, the medium-temperature debinding temperature is 180°C, and the high-temperature metallization sintering temperature is 280°C.

7. The method of manufacturing a VCM flexible printed coil structure of claim 5, wherein: The plasma activation cleaning described in step S1 is used to remove the release agent from the surface of the flexible insulating substrate and improve the adhesion of the conductive paste to the flexible insulating substrate.

8. The method for manufacturing the VCM flexible printed coil structure according to claim 5, characterized in that: The screen printing described in step S2 is a roll-to-roll continuous printing process.

9. The method of manufacturing a VCM flexible printed coil structure of claim 5, wherein: When manufacturing coils in a multi-layer stacked arrangement, after the first layer of conductive lines is sintered and cured, an insulating layer is coated and conductive lap posts are prepared, and then the next layer of conductive lines is printed.

10. The method of manufacturing a VCM flexible printed coil structure of claim 6, wherein: In step S3, the low-temperature pre-baking time is 10 minutes, the medium-temperature debinding time is 20 minutes, and the high-temperature metallization sintering time is 30 minutes. The three-stage temperature control process is carried out with continuous temperature increases.