Electronic components and methods for manufacturing electronic components

By introducing voids and a multi-layered external electrode design into the electronic components, the peeling problem caused by the difference in thermal expansion coefficients between the substrate layer and the magnetic resin is solved, thereby improving the stability and temperature resistance of the electrical connection.

CN123125672APending Publication Date: 2026-11-17MURATA MFG CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202580027464.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-05-15
Filing Date
2025-05-01
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing coil components, the difference in thermal expansion coefficients between the base layer and the resin of the magnet causes a peeling problem, affecting the stability of the electrical connection.

Method used

Multiple gaps are introduced into the electronic components. The gaps are formed between the external electrode and the blank through a photo-firing process. Combined with the multi-layer external electrode design, including Cu, Ni and Sn layer plating, the bonding strength between the electrode and the blank is enhanced.

Benefits of technology

It effectively prevents the external electrodes from peeling off from the billet, improves the stability and temperature resistance of the electrical connection, and ensures the reliability of electrical conduction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123125672A_ABST
    Figure CN123125672A_ABST
Patent Text Reader

Abstract

An inductor component has a blank (11), an internal wiring, and a first external electrode. The blank (11) contains metal magnetic particles (12) and synthetic resin (13). The internal wiring extends inside the blank (11). In addition, a part of the internal wiring is exposed outside the blank (11). The first external electrode is layered on the surface of the blank (11). In addition, the first external electrode is in contact with the internal wiring. The first external electrode has a first layer (31A) located on the blank (11) side in the first external electrode. The first layer (31A) contains Cu. Furthermore, a plurality of voids P exist between the first layer (31A) and the synthetic resin (13) in the blank (11).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to electronic components and methods for manufacturing electronic components. Background Technology

[0002] Patent Document 1 discloses a coil component comprising a magnetic body, a coil, and terminal electrodes. The magnetic body comprises resin and metallic magnetic particles. The coil extends inside the magnetic body. Furthermore, the ends of the coil are exposed outside the magnetic body. The terminal electrodes comprise a base layer and a capping layer. The base layer is laminated onto the surface of the magnetic body. The base layer is in contact with the ends of the coil. The base layer is made of a conductive metal such as silver, copper, gold, or aluminum. The capping layer covers the base layer from the outside. The capping layer is made of silver or a conductive resin containing silver.

[0003] Patent Document 1: Japanese Patent Application Publication No. 2016-32050

[0004] In the coil component of Patent Document 1, the base layer is also in partial contact with the resin in the magnetic material. If we compare the coefficients of thermal expansion of the conductive metal used as the base layer material and the resin of the magnetic material, there is a significant difference between the two values. Therefore, the coil component of Patent Document 1 may experience delamination between the base layer and the resin of the magnetic material due to temperature changes, etc. Summary of the Invention

[0005] To address the aforementioned issues, the electronic component disclosed herein comprises: a blank containing metallic magnetic particles and a synthetic resin; internal wiring extending inside the blank, with a portion exposed outside the blank; and an external electrode stacked on the surface of the blank and in contact with the internal wiring, the external electrode having a first layer located at the position closest to the blank and containing Cu, and a plurality of voids existing between the first layer and the synthetic resin in the blank.

[0006] Furthermore, the method for manufacturing the electronic component disclosed herein includes: a blank preparation step, preparing a blank having internal wiring extensions and containing metallic magnetic particles and synthetic resin; a coating step, coating a conductive paste across the surface of the blank and the ends of the internal wiring; and a photo-firing step, photo-firing the conductive paste by irradiating it with light of a wavelength absorbed by the conductive paste to form a first layer, and forming a plurality of voids between the first layer and the synthetic resin in the blank.

[0007] In electronic components, it is possible to prevent the first layer of the external electrode from peeling off from the blank. Attached Figure Description

[0008] Figure 1 This is a 3D view of an inductor component.

[0009] Figure 2 This is a 3D view of an inductor component.

[0010] Figure 3 This is a partial cross-sectional view of the inductor component.

[0011] Figure 4 It is an enlarged sectional view of the area near the surface of the billet.

[0012] Figure 5 It is a diagram showing the distribution of elements in the first layer of the external electrode.

[0013] Figure 6 This is a flowchart illustrating the manufacturing method of an inductor component. Detailed Implementation

[0014] <An Implementation of the Electronic Component>

[0015] The following describes one embodiment in which this disclosure is applied to an inductor component. Furthermore, the accompanying drawings are schematic diagrams for ease of understanding, and may include enlarged or omitted components. Therefore, there may be instances where the size ratios of the components differ from the actual size ratios.

[0016] <Overall Composition>

[0017] First, the overall structure of the inductor component 10 will be explained.

[0018] like Figure 1 As shown, the inductor component 10 includes a blank 11. The blank 11 is rectangular parallelepiped in shape. Figure 4 As shown, the blank 11 contains metallic magnetic particles 12 and synthetic resin 13. Furthermore, the metallic magnetic particles 12 have a particle body 12A composed of a magnetic material and an insulating coating 12B covering the surface of the particle body 12A. An example of the material of the particle body 12A is Fe or an alloy containing Fe. An example of the material of the insulating coating 12B is inorganic glass. Specifically, the insulating coating 12B is made of zinc phosphate glass. The synthetic resin 13 is made of one or more resins selected from epoxy resin, phenolic resin, polyester resin, polyimide resin, polyolefin resin, and silicone resin.

[0019] The following, such as Figure 1As shown, one of the surfaces with the largest area in the cuboid blank 11 is designated as the mounting surface 11A. Furthermore, an axis orthogonal to the mounting surface 11A is designated as the first axis X. Moreover, the direction along the first axis X towards which the mounting surface 11A faces is designated as the first positive direction X1, and its opposite direction is designated as the first negative direction X2. Furthermore, an axis orthogonal to the first axis X and parallel to one side of the mounting surface 11A is designated as the second axis Y. Moreover, a specific direction along the second axis Y is designated as the second positive direction Y1, and its opposite direction is designated as the second negative direction Y2.

[0020] like Figure 1 As shown, the inductor component 10 has internal wiring 21. Furthermore, in Figure 1 as well as Figure 2 The diagram is shown with the blank 11 in perspective. The internal wiring 21 extends inside the blank 11. More specifically, the internal wiring 21 is wound around an imaginary line that is parallel to the first axis X and passes through the center of the mounting surface 11A.

[0021] like Figure 1 As shown, the internal wiring 21 includes a first end 22, a first winding portion 23, a transition portion 24, a second winding portion 25, and a second end 26.

[0022] like Figure 2 As shown, the first end portion 22 is located near the edge of the blank body 11 in the second positive direction Y1. The end face 22A of the first end portion 22 is approximately the same as the mounting surface 11A of the blank body 11. The end face 22A of the first end portion 22 is exposed on the outside of the blank body 11. Moreover, the first end portion 22 extends from the end face 22A toward the first negative direction X2.

[0023] like Figure 1 As shown, the first winding portion 23 is connected to the end of the first end portion 22 opposite to the end face 22A. The first winding portion 23 extends in an imaginary plane orthogonal to the first axis X. If the first winding portion 23 is traced back from the side connected to the first end portion 22, it is wound approximately 2.5 turns from the outer peripheral side toward the inner peripheral side. The transition portion 24 extends in a straight line at an incline from the inner peripheral side end of the first winding portion 23 toward the first negative direction X2 and the second positive direction Y1.

[0024] The second winding portion 25 is connected to the end of the transition portion 24 opposite to the first winding portion 23. The second winding portion 25 extends in an imaginary plane orthogonal to the first axis X. If the first winding portion 23 is traced back from the side connected to the transition portion 24, it is wound approximately 2.5 turns from the inner circumferential side to the outer circumferential side. Moreover, the outer circumferential end of the second winding portion 25 is located near the edge of the second negative direction Y2 side inside the blank 11.

[0025] The second end 26 is connected to the outer peripheral end of the second winding portion 25. Therefore, the second end 26 is located near the edge of the interior of the blank 11 on the second negative direction Y2 side. The second end 26 extends from the outer peripheral end of the second winding portion 25 toward the first positive direction X1 side. Furthermore, as... Figure 2 As shown, the end face 26A of the second end 26 is approximately the same as the mounting surface 11A of the blank 11. In addition, the end face 26A of the second end 26 is exposed on the outside of the blank 11.

[0026] like Figure 2 As shown, the inductor component 10 includes a first external electrode 31 and a second external electrode 32.

[0027] The first external electrode 31 is stacked on the mounting surface 11A of the blank 11. The first external electrode 31 is rectangular when viewed from above along the first axis X. The first external electrode 31 covers a portion of the mounting surface 11A in the second positive direction Y1. In addition, the first external electrode 31 contacts the end face 22A of the first end 22 in the internal wiring 21. That is, the first external electrode 31 has a portion covering the mounting surface 11A and a portion covering the end face 22A.

[0028] like Figure 3 As shown, the first external electrode 31 has a three-layer structure consisting of a first layer 31A, a second layer 31B, and a third layer 31C. Furthermore, in Figure 3 In this illustration, the distinction between the metallic magnetic particles 12 and the synthetic resin 13 in the blank 11 is omitted; instead, they are shown as a single, integrated component. Additionally, Figure 3 The thicknesses of the first layer 31A, the second layer 31B, and the third layer 31C, and the relationship between the thicknesses of each layer, are illustrative and not limited to this example. Figure 3 The content of the illustration.

[0029] The first layer 31A is located on the side closest to the blank 11 among the layers constituting the first external electrode 31. That is, the first layer 31A is in contact with the blank 11. The first layer 31A contains Cu as the main component and contains trace amounts of Zn, Si and P. Furthermore, the details of the first layer 31A and its related structure will be described later.

[0030] The second layer 31B is stacked on the outer surface of the first layer 31A on the side opposite to the blank 11, that is, on the outer surface on the side of the first positive direction X1. The second layer 31B contains Ni as the main component. The second layer 31B is a so-called Ni-plated layer.

[0031] The third layer 31C is laminated on the outer surface of the second layer 31B on the side opposite to the blank 11, that is, the outer surface on the side of the first positive direction X1. The third layer 31C contains Sn as the main component. The third layer 31C is a so-called Sn-plated layer.

[0032] like Figure 2 As shown, the second external electrode 32 is stacked on the mounting surface 11A of the blank 11. The second external electrode 32 is rectangular when viewed from above along the first axis X. In this embodiment, the second external electrode 32 has the same shape and size as the first external electrode 31. The second external electrode 32 covers a portion of the mounting surface 11A on the second negative direction Y2 side. Furthermore, the second external electrode 32 is separate from the first external electrode 31. The second external electrode 32 contacts the end face 26A of the second end 26 in the internal wiring 21. That is, the second external electrode 32 has a portion covering the mounting surface 11A and a portion covering the end face 26A. The second external electrode 32, like the first external electrode 31, has a three-layer structure. The structure of each layer of the second external electrode 32 is the same as that of each layer of the first external electrode 31, therefore, description is omitted.

[0033] <Details of the external electrodes>

[0034] The first external electrode 31, and particularly the first layer 31A, will be described in detail below. Furthermore, the second external electrode 32 is identical to the first external electrode 31, and therefore its description is omitted.

[0035] like Figure 4 As shown, multiple voids P exist between the first layer 31A of the first external electrode 31 and the synthetic resin 13 in the blank 11. In this embodiment, not only the synthetic resin 13, but also the metallic magnetic particles 12 are exposed towards the outside of the blank 11. Furthermore, multiple voids P also exist between the first layer 31A of the first external electrode 31 and the metallic magnetic particles 12 in the blank 11. Thus, voids P are distributed throughout the entire space between the first layer 31A of the first external electrode 31 and the mounting surface 11A of the blank 11. Furthermore, the voids P referred to here are portions without solid components at room temperature and pressure, not so-called vacuum spaces. Therefore, the presence of gaseous components within the voids P is permissible.

[0036] like Figure 4As shown, assuming a cross-section orthogonal to the mounting surface 11A of the blank 11, the boundary portion of the blank 11 and the first layer 31A of the inductor component 10 is observed. At this time, the average circular equivalent diameter of the voids P at each location is 100 nm or less. The circular equivalent diameter refers to the diameter of a circle with an area equal to the area measured in the cross-sectional observation described above. Furthermore, the average circular equivalent diameter is calculated as follows: The interface between the first layer 31A and the synthetic resin 13 of the blank 11 is observed over a length of 500 μm, and the area of ​​the voids P present within this observation range is measured. The same void P area measurement and circular equivalent diameter calculation are repeated at least five times at different locations. Furthermore, the average circular equivalent diameter of all voids P is set as the aforementioned average circular equivalent diameter.

[0037] like Figure 4 As shown, the blank 11 has a recess 11B that is recessed into the interior of the blank 11 relative to the mounting surface 11A. The width of the opening edge of the recess 11B is smaller than the maximum width inside the recess 11B. That is, the recess 11B has a shape that narrows on the opening side. Furthermore, this recess 11B is formed during the manufacturing process of the inductor component 10, described later, by removing metal magnetic particles 12 exposed from the mounting surface 11A of the blank 11. Moreover, the first layer 31A of the first external electrode 31 is also present inside the recess 11B. In this embodiment, the first layer 31A of the first external electrode 31 fills the entire recess 11B.

[0038] like Figure 4 As shown, the thickness of the first layer 31A of the first external electrode 31 differs in the portion on the metallic magnetic particles 12 in the blank 11 and in the portion on the synthetic resin 13. Specifically, the average thickness T1 of the first layer 31A on the synthetic resin 13 is greater than the average thickness T2 of the first layer 31A on the metallic magnetic particles 12. Furthermore, in Figure 4 In the diagram, the boundary between the portion on the metallic magnetic particles 12 and the portion on the synthetic resin 13 in the first layer 31A is hypothetically illustrated with a double-dotted line.

[0039] The average thickness T1 of the first layer 31A on the synthetic resin 13 is calculated as follows. First, a cross-section of the boundary between the synthetic resin 13, including the preform 11, and the first layer 31A is photographed using an electron microscope. This cross-section is orthogonal to the mounting surface 11A of the preform 11. Next, in the photographed image, a measurement range along the direction of the outer surface of the synthetic resin 13 is determined. This measurement range is 10 μm or more. The measurement range can also be continuously 10 μm or more, or the sum of the ranges at multiple different locations can also be 10 μm or more. Furthermore, the cross-sectional area of ​​the first layer 31A within the measurement range is calculated by image processing. Details will be explained later, but the second layer 31B partially penetrates the interior of the first layer 31A. However, when calculating the cross-sectional area of ​​the first layer 31A, the entire region from the mounting surface 11A of the preform 11 to the outer surface of the first layer 31A is considered to be composed of the first layer 31A. Next, the value obtained by dividing the calculated cross-sectional area of ​​the first layer 31A within the measurement range by the length of the measurement range is set as the average value of the thickness T1 of the first layer 31A on the synthetic resin 13. The average value of the thickness T2 of the first layer 31A on the metallic magnetic particles 12 can also be calculated similarly by taking the cross-section containing the boundary between the metallic magnetic particles 12 and the first layer 31A as the object of the photograph.

[0040] like Figure 3 As shown, the average thickness Tb of the first layer 31A on the blank 11 is less than 3 μm. In addition, the average thickness Tb of the first layer 31A on the blank 11 is greater than the average thickness Tc of the first layer 31A on the end face 22A of the first end 22 in the internal wiring 21.

[0041] The average thickness Tb of the first layer 31A on the blank 11 is calculated as follows. First, a cross-section containing the boundary between the blank 11 and the first layer 31A is taken using an electron microscope, and this cross-section is orthogonal to the mounting surface 11A of the blank 11. Next, in the captured image, the observation range along the direction of the mounting surface 11A of the blank 11 is determined. This observation range is 100 μm or more. The observation range can also be continuously 100 μm or more, or the sum of the ranges at multiple different locations can also be 100 μm or more. Furthermore, the proportion A of the length of the length of the observation range in which the synthetic resin 13 contacts the first layer 31A is calculated as a percentage. The value derived using the following formula is then set as the average thickness Tb of the first layer 31A on the blank 11.

[0042] Formula: Average value of thickness T1 × (A / 100) + Average value of thickness T2 ((100-A) / 100)

[0043] That is, the average thickness Tb of the first layer 31A on the blank 11 is obtained by taking into account the presence ratio of the synthetic resin 13 and the metal magnetic particles 12 on the mounting surface 11A, based on the average thickness T1 of the first layer 31A on the synthetic resin 13 and the average thickness T2 of the first layer 31A on the metal magnetic particles 12.

[0044] In addition, the cross-section containing the boundary between the end face 22A and the first layer 31A can be used as the subject of the photograph, and the average thickness Tc of the first layer 31A on the end face 22A of the first end 22 can be calculated in the same way as the average thickness T1 and the average thickness T2.

[0045] like Figure 5 As shown, the first layer 31A has multiple continuous pores ST. Specifically, the first layer 31A has a copper portion P1 mainly composed of Cu. Moreover, the copper portion P1 has a structure in which Cu is distributed in a sponge-like manner. However, in Figure 5 In the diagram, the portion where the Cu concentration is above a specified value is designated as copper portion P1. Therefore, copper portion P1 is depicted as a localized distribution. In reality, copper portion P1 is distributed throughout the entire structure between the billet 11 and the second layer 31B. Furthermore, in... Figure 3 as well as Figure 4 In the diagram, the first layer 31A is schematically illustrated as a uniform layer composed of copper portion P1.

[0046] The continuous vent ST opens on the outer surface of the second layer 31B side in the first layer 31A. Furthermore, the second layer 31B also exists inside the continuous vent ST. In this embodiment, the second layer 31B fills approximately the entire area of ​​the continuous vent ST. Moreover, the second layer 31B extends via the continuous vent ST to the end face 22A of the first end 22 in the internal wiring 21.

[0047] Here, the portion of the first external electrode 31 extending from the mounting surface 11A of the billet 11 or the end face 22A of the first end 22 to the outer surface of the first layer 31A is designated as a specific portion SP. Furthermore, this specific portion SP is divided into an inner layer L1 on the side of the billet 11 and an outer layer L2 on the side opposite to the billet 11 in a direction orthogonal to the mounting surface 11A. In this case, the proportion of copper portion P1 of the first layer 31A in the outer layer L2 is larger than the proportion of copper portion P1 of the first layer 31A in the inner layer L1. That is, in the portion extending from the mounting surface 11A of the billet 11 or the end face 22A of the first end 22 to the outer surface of the first layer 31A, the concentration of Cu is higher in the region farther from the billet 11. Thus, it is possible to observe, using TEM-EDX (energy-dispersive X-ray spectroscopy), what elements are present in the specific portion SP and at what concentrations.

[0048] Furthermore, in a cross-section orthogonal to the mounting surface 11A of the blank 11, the midpoint of the line segment connecting any point on the mounting surface 11A of the blank 11 or the end face 22A of the first end 22 to the outer surface of the first layer 31A with the shortest distance is defined as the midpoint from the mounting surface 11A of the blank 11 or the end face 22A of the first end 22 to the outer surface of the first layer 31A. Therefore, when the midpoint is similarly determined at an infinite number of points, the line connecting these midpoints becomes an imaginary boundary line with the inner layer L1 and the outer layer L2.

[0049] like Figure 5 As shown, the first layer 31A, in addition to the copper portion P1, also has multiple metal-containing portions P2, which contain Si, Zn, and P. As described above, in this embodiment, the insulating coating 12B in the metallic magnetic particles 12 is made of zinc phosphate glass. Therefore, the metal-containing portions P2 contain Si and Zn, which are metallic elements other than Cu among the elements contained in the insulating coating 12B. Furthermore, in Figure 5 In the illustration, the metal-containing portion P2 is shown as an independent entity from the copper portion P1, with an origin. However, there are also cases where the metal-containing portion P2 contains Cu, just like the copper portion P1. When the first external electrode 31 is observed in cross-section orthogonal to the mounting surface 11A of the blank 11, the average circular equivalent diameter of the metal-containing portion P2 at each location is 0.01 μm or more and 10 μm or less. Furthermore, the average circular equivalent diameter of the metal-containing portion P2 can be calculated using images obtained by TEM-EDX, similar to the case of void P.

[0050] <Manufacturing Method of Inductor Components>

[0051] Next, the manufacturing method of the inductor component 10 will be described.

[0052] like Figure 6 As shown, the manufacturing method of the inductor component 10 includes a blank preparation process S11, an R-beveling process S12, a coating process S13, a light firing process S14, and a plating process S15.

[0053] In the blank preparation step S11, a blank 11 with internal wiring 21 disposed inside is prepared. The blank 11 in this stage is in a state before the R-beveling is performed and before the first external electrode 31 and the second external electrode 32 are formed. The blank 11 in this stage can be formed, for example, as follows: First, the internal wiring 21 is pre-wound into a predetermined shape. Then, the formed internal wiring 21, together with a mixture of metal magnetic particles 12, synthetic resin 13, and other adhesive components, is disposed in a mold having a cuboid cavity. By stamping and heating in this state, a blank 11 with the internal wiring 21 disposed inside and the synthetic resin 13 cured is obtained. Furthermore, the blank preparation step S11 is independent of the blank 11 manufacturing process; the blank 11 can be obtained in any way.

[0054] Next, the radius (R) chamfering process S12 is performed. In the radius chamfering process S12, the blank 11 prepared in the blank preparation process S11 is radius chamfered. As a method of radius chamfering, tumbling grinding is an example. Through this radius chamfering process S12, a blank 11 with radius chamfered corners is obtained. In addition, by accompanying the radius chamfering process S12, a portion of the exposed metal magnetic particles 12 on the surface of the blank 11 is removed, thereby forming a recess 11B that is recessed relative to the mounting surface 11A of the blank 11.

[0055] Next, a coating process S13 is performed. In coating process S13, conductive paste is applied to two portions of the mounting surface 11A of the blank 11. Specifically, conductive paste is applied to the portions of the mounting surface 11A corresponding to the first end 22 of the internal wiring 21 and the portions corresponding to the second end 26 of the internal wiring 21. At this time, the conductive paste is applied across the mounting surface 11A of the blank 11 and the first end 22 of the internal wiring 21. Similarly, conductive paste is applied across the mounting surface 11A of the blank 11 and the second end 26 of the internal wiring 21.

[0056] Furthermore, the conductive paste is a complex ink. The conductive paste for the complex ink is prepared as follows: First, an amine compound such as 2-ethylhexylamine is mixed with an alkanolamine such as 2-amino-2-methylpropanol. Then, 10-300 wt% of a silicon component, such as an organosilicon resin, is added relative to the weight of Cu alone. Finally, copper formate is added and dissolved to prepare the conductive paste. In this embodiment, the conductive paste does not exhibit conductivity. That is, the conductive paste itself is an insulator.

[0057] Next, a photo-firing process S14 is performed. Specifically, in the photo-firing process S14, light of a wavelength that the conductive paste can absorb is irradiated onto the conductive paste coated on the blank 11. In this photo-firing process S14, the light is irradiated multiple times, each time for about a few milliseconds. In addition, the number of irradiations and the intensity of the light are adjusted so that the total energy imparted to the conductive paste through multiple irradiations is a few joules to tens of joules per square centimeter. The conductive paste is fired through this photo-firing process S14 to form a first layer 31A of a solid and conductive first external electrode 31. In addition, the copper portion P1 of the first layer 31A is in close contact with the blank 11, and multiple gaps P are formed between the first layer 31A and the mounting surface 11A of the blank 11. Similarly, a first layer of the second external electrode 32 is also formed.

[0058] Next, a plating process S15 is performed. In this plating process S15, nickel is electroplated onto the first layer 31A of the first external electrode 31 and the first layer of the second external electrode 32. This forms the second layer 31B of the first external electrode 31 and the second layer of the second external electrode 32. Then, tin is electroplated onto the second layer 31B of the first external electrode 31 and the second layer of the second external electrode 32. This forms the third layer 31C of the first external electrode 31 and the third layer of the second external electrode 32. Thus, the inductor component 10 is formed.

[0059] <Effects of the Implementation Method>

[0060] The effects shared by both the first external electrode 31 and the second external electrode 32 in the following description will be explained using the first external electrode 31 as an example.

[0061] (1) In the above embodiment, there are multiple voids P between the first layer 31A of the first external electrode 31 and the synthetic resin 13 of the blank 11. Assume that the inductor component 10 is exposed to temperature changes. At this time, since there is a difference in the thermal expansion coefficient between Cu contained in the first layer 31A and the synthetic resin 13, stress is generated at the interface between the two. Even in such a case, the stress generated at the interface can be released by changing the shape of the voids P, etc. That is, the voids P can function as spaces for easing stress. Therefore, even if the inductor component 10 is exposed to temperature changes, the peeling of the first layer 31A from the synthetic resin 13 of the blank 11 can be suppressed.

[0062] (2) In the above embodiment, the average circular equivalent diameter of the void P in each part is less than 100 nm. If the void P is of this size, the presence of void P is less likely to have a negative impact on the bonding strength of the first layer 31A with respect to the synthetic resin 13 of the preform 11.

[0063] (3) In the above embodiment, from the viewpoint of ensuring the bonding strength between the first external electrode 31 and the blank 11, the first layer 31A only needs to be in contact with the synthetic resin 13. In this regard, in the above embodiment, the average thickness T1 of the first layer 31A on the synthetic resin 13 is greater than the average thickness T2 of the first layer 31A on the metal magnetic particles 12. With such a thickness setting, even if the overall thickness of the first layer 31A is reduced, it is possible to suppress the insufficient thickness T1 of the first layer 31A on the synthetic resin 13, which is prone to affecting the bonding strength.

[0064] (4) In the above embodiment, the average thickness Tb of the first layer 31A on the blank 11 is greater than the average thickness Tc of the first layer 31A on the end face 22A of the first end 22 in the internal wiring 21. As described above, in order to ensure the bonding strength between the first external electrode 31 and the blank 11, it is preferable to make the thickness Tb of the first layer 31A on the blank 11 relatively large.

[0065] (5) In the above embodiment, the average thickness Tb of the first layer 31A on the blank 11 is 3 μm or less. As described above, in this embodiment, the presence of voids P can suppress peeling of the first layer 31A. Therefore, even a relatively thin first layer 31A with an average thickness Tb of 3 μm or less on the blank 11 can be obtained, resulting in a highly reliable first layer 31A that is less prone to peeling. That is, the effect of the above-mentioned void P configuration is particularly well achieved in a relatively thin first layer 31A with an average thickness of 3 μm or less on the blank 11.

[0066] (6) In the above embodiment, the first layer 31A of the first external electrode 31 fills the entire recess 11B. According to this configuration, the first layer 31A is not easily peeled off from the blank 11 through the so-called anchoring effect.

[0067] (7) In the above embodiment, a second layer 31B exists inside the continuous pores ST of the first layer 31A. According to this configuration, the second layer 31B is not easily peeled off from the first layer 31A through the so-called anchoring effect.

[0068] (8) In the above embodiment, the second layer 31B reaches the end face 22A of the first end 22 in the internal wiring 21 via continuous vents ST. With this configuration, an electrical path from the second layer 31B to the internal wiring 21 is ensured without passing through the boundary between the first layer 31A and the second layer 31B. Therefore, even if a stripping occurs between the first layer 31A and the second layer 31B, electrical continuity between the first external electrode 31 and the internal wiring 21 can be ensured.

[0069] (9) In the above embodiment, in a specific portion SP, the proportion of the copper portion P1 of the first layer 31A in the outer layer L2 is larger than the proportion of the copper portion P1 of the first layer 31A in the inner layer L1. By making the proportion of the copper portion P1 in the outer layer L2 larger in this way, the bonding strength of the first layer 31A with respect to the Ni contained in the second layer 31B that is in contact with the outer surface of the outer layer L2 can be improved.

[0070] (10) In the above embodiment, the first layer 31A has a copper portion P1 and a plurality of metal-containing portions P2 containing Zn and Si. The Zn and Si contained in the metal-containing portions P2 are likely to originate from the insulating coating 12B in the metal magnetic particles 12. Moreover, if the components of the insulating coating 12B enter the first layer 31A of the first external electrode 31, the Cu component of the first layer 31A is also likely to reach the metal magnetic particles 12. Thus, if the components of the first layer 31A and the metal magnetic particles 12 are mixed, a high bonding strength can be expected. In addition, the average circumferential equivalent diameter of the metal-containing portions P2 is 0.01 μm or more and 10 μm or less. If it is of this size, the presence of the metal-containing portions P2 is unlikely to have a negative impact on the electrical conductivity and other properties of the first layer 31A.

[0071] (11) In the above embodiment, the second layer 31B of the first external electrode 31 contains Ni and the third layer 31C contains Sn. If this is the configuration, the second layer 31B and the third layer 31C can be formed by electrolytic plating.

[0072] (12) In the above embodiment, the internal wiring 21 is a wound inductor wiring. In other words, the configuration related to the gap P is applied to the inductor component 10. When current flows through the internal wiring 21 of the inductor component 10, the internal wiring 21 heats up. As a result, the temperature of the inductor component 10 as a whole also rises. It is particularly preferable to apply the configuration related to the gap P to the inductor component 10, which is subject to such temperature changes, to suppress the peeling of the first layer 31A.

[0073] (13) In the above embodiment, the conductive paste is solidified by photo-firing to form the first layer 31A of the first external electrode 31. By performing photo-firing, the adhesion between the first layer 31A and the blank 11 can be improved. In addition, the components of the conductive paste that undergo volume change or volatilize during the photo-firing process S14 are sealed, thereby forming voids P.

[0074] <Example of Change>

[0075] Unless otherwise specified, the following variations can be applied to both the first external electrode 31 and the second external electrode 32. The first external electrode 31 will be used as the representative example, and the description of the second external electrode 32 will be omitted.

[0076] • The shape and material of the blank 11 in the inductor component 10 can be appropriately changed. If the blank 11 has metallic magnetic particles 12 and synthetic resin 13, it is suitable to apply the configuration related to the aforementioned gap P. Furthermore, if the blank 11 has metallic magnetic particles 12 and synthetic resin 13, it is not limited to the inductor component 10, and the configuration related to the gap P can also be applied to electronic components such as capacitors and thermistors.

[0077] • The shape of the internal wiring 21 in the inductor component 10 is not limited. As long as the shape functions as inductor wiring, the shape of the internal wiring 21 can be any shape.

[0078] • The shape of the first external electrode 31 in the inductor component 10 is not limited. For example, the first external electrode 31 may also be a so-called L-shaped electrode that spans one of the outer surfaces of the blank 11 and the other outer surfaces adjacent to that outer surface. Furthermore, the first external electrode 31 may also be a so-called five-sided electrode that spans one of the outer surfaces of the blank 11 and the other four outer surfaces adjacent to that outer surface.

[0079] • The blank 11 may also not have the recess 11B. For example, when the proportion of metallic magnetic particles 12 in the blank 11 is small, or when the entire surface area of ​​the blank 11 is composed of synthetic resin 13, the blank 11 may not have the recess 11B.

[0080] • The second layer 31B of the first external electrode 31 may not reach the internal wiring 21. For example, when the first layer 31A is thicker, there may be a case where the second layer 31B does not reach the internal wiring 21. In addition, although the continuous pore ST opens on the side of the second layer 31B, if it does not reach the side of the blank 11, the second layer 31B does not directly contact the internal wiring 21.

[0081] • The first layer 31A of the first external electrode 31 may also not have continuous pores ST. In this case, the second layer 31B is indirectly electrically connected to the internal wiring 21 via the first layer 31A.

[0082] • The first layer 31A of the first external electrode 31 may contain other metallic elements besides Cu. Specifically, the first layer 31A may also contain Ni, an element other than Cu among the elements constituting the second layer 31B. Furthermore, in this variation, Ni may be contained in the first layer 31A in any manner. For example, Cu and Ni may be alloyed within the first layer 31A, or monomeric Cu and monomeric Ni may be mixed together. In this variation, the Ni composition of the first layer 31A is mixed with the Ni composition of the second layer 31B, and a clear boundary is not easily established between them. Therefore, an improved bonding strength between the first layer 31A and the second layer 31B is desirable. Additionally, for example, if the conductive paste contains nickel formate in addition to copper formate, then the first layer 31A contains Ni as in this variation.

[0083] • The second layer 31B of the first external electrode 31 may not be filled in the entire continuous pore ST. In other words, a portion of the continuous pore ST may exist as a space not filled with the second layer 31B.

[0084] • The materials of the second layer 31B and the third layer 31C in the first external electrode 31 are not limited. They can be appropriately changed according to the type of substrate on which the inductor component 10 is mounted and the purpose of the inductor component 10.

[0085] Furthermore, the first external electrode 31 only needs to have a first layer 31A as the layer located closest to the blank 11. For example, either or both of the second layer 31B and the third layer 31C can be omitted. In addition, the first external electrode 31 may have other layers besides the first layer 31A, the second layer 31B, and the third layer 31C.

[0086] • The void P only needs to exist between the first layer 31A and the synthetic resin 13 of the blank 11. That is, the void P between the first layer 31A and the metallic magnetic particles 12 of the blank 11 is not necessary.

[0087] • The average circular equivalent diameter of the void P at each location is not limited to 100 nm or less as illustrated in the above embodiment. Even if the average circular equivalent diameter of the void P exceeds 100 nm, it is sufficient to ensure the bonding strength of the first layer 31A with respect to the blank 11.

[0088] • The average thickness T1 of the first layer 31A on the synthetic resin 13 can be the same as or smaller than the average thickness T2 of the first layer 31A on the metallic magnetic particles 12.

[0089] Similarly, the average thickness Tb of the first layer 31A on the blank 11 can be the same as or smaller than the average thickness Tc of the first layer 31A on the internal wiring 21.

[0090] • The average thickness Tb of the first layer 31A on the blank 11 can also exceed 3 μm.

[0091] • The metallic magnetic particles 12 may not be located on the surface of the blank 11. In other words, the entire surface area of ​​the blank 11 may be composed of synthetic resin 13.

[0092] • The first layer 31A of the first external electrode 31 may not fill the entire recess 11B of the blank 11. That is, the first layer 31A may exist only in a part of the interior of the recess 11B.

[0093] • The proportion of the copper portion P1 of the first layer 31A in the specific portion SP is not limited to the example of the above embodiment. For example, the proportion of the copper portion P1 of the first layer 31A in the outer layer L2 may be smaller than the proportion of the copper portion P1 of the first layer 31A in the inner layer L1. In addition, the copper portion P1 may be evenly distributed in the specific portion SP.

[0094] • The average circular equivalent diameter of the metal containing the P2 portion is not limited to 0.01 μm or more and 10 μm or less as illustrated in the above embodiments. That is, the average circular equivalent diameter of the metal containing the P2 portion may be less than 0.01 μm or more than 10 μm.

[0095] • The material of the particle body 12A of the metallic magnetic particle 12 can be any metal that has magnetic properties.

[0096] • The insulating coating 12B of the metallic magnetic particles 12 can be made of any material that is insulating. For example, the insulating coating 12B can also be a glass film formed by the so-called sol-gel method. In addition, the metallic elements other than Cu in the insulating coating 12B of the metallic magnetic particles 12 are not limited to Si and Zn. Furthermore, the metallic elements mentioned here also include so-called half-metallic elements such as B, Si, Ge, As, Sb, and Te.

[0097] • The metallic magnetic particles 12 may also not have an insulating coating 12B.

[0098] • Alternatively, the R-beveling process S12 in the manufacturing method of inductor component 10 can be replaced by other grinding or etching processes. Alternatively, the grinding process, such as the R-beveling process S12, can be omitted.

[0099] • As a process for curing the conductive paste, other processes can be used instead of the photofiring process S14. For example, the entire blank 11 coated with the conductive paste can be fired in a nitrogen atmosphere. Even with a firing method different from the photofiring process S14, voids P can be formed by adjusting the temperature conditions, firing time, etc.

[0100] • The conductive paste described in the above embodiments is not limited to a fluid semi-solid object, but also includes gel-like and liquid-like objects. That is, the conductive paste only needs to have a viscosity that allows it to remain on the coated area when coated on the surface of the blank 11.

[0101] • In the above embodiments, the materials used when the conductive paste is a complex ink are not limited to the examples described in the above embodiments. For example, the amine compound can be any of the primary, secondary, and tertiary amines, and the number of N atoms is not limited. For example, it can be a primary amine such as octylamine or hexylamine, a secondary amine such as di-n-butylamine, or a tertiary amine such as N,N-dimethylhexylamine. In addition, the amine compound can be an alkanolamine, a diamine, etc., and the positional relationship between the N atom and the OH group is not limited to α, β, γ positions, etc. Furthermore, the number of N and O atoms in one molecule is not particularly limited. For example, it can be an α-hydroxyamine such as 2-dimethylaminoethanol or 2-ethylaminoethanol, a β-hydroxyamine such as 3-amino-1-propanol or 4-amino-2-butanol. Furthermore, it can be a diamine such as ethylenediamine, or a cyclic diamine such as piperazine. In addition, the silicon component can be, for example, various silicone-modified resins such as epoxy resin, polyester resin, and phenolic resin, as well as sol-gel materials, etc. Alternatively, metal salts composed of formic acid, acetic acid, oxalic acid, and other organic acids can also be used as metal salts.

[0102] • In the above embodiments, the conductive paste can also be a so-called nano-ink. In the case of nano-ink, the conductive paste is prepared as follows: First, nano-metal powder composed of Cu is dispersed in a solvent containing solvents such as cellosol, carbidol, hydrocarbons, and aromatic compounds. Furthermore, 10-300 wt% of various silicone-modified resins, silicone resins, or sol-gel materials are added relative to the weight of Cu alone. This method of preparing nano-ink is merely an example; other methods can also be used to prepare nano-ink.

[0103] <Postscript>

[0104] This document records the technical concepts that can be grasped based on the above-described implementation methods and variations.

[0105] [Postscript 1]

[0106] An electronic component, wherein:

[0107] The blank contains metallic magnetic particles and synthetic resin;

[0108] Internal wiring extends inside the aforementioned blank, with a portion exposed outside the aforementioned blank; and

[0109] External electrodes, stacked on the surface of the aforementioned blank, are in contact with the aforementioned internal wiring.

[0110] The aforementioned external electrode has a first layer, which is located closest to the blank in the external electrode and contains Cu.

[0111] There are multiple voids between the first layer and the synthetic resin in the preform.

[0112] [Postscript 2]

[0113] According to the electronic components described in Appendix 1, among which,

[0114] When a cross-sectional view is taken in a section orthogonal to the surface of the blank, the average circular equivalent diameter of the above-mentioned voids in each part is less than 100 nm.

[0115] [Postscript 3]

[0116] According to the electronic components described in Appendix 1 or Appendix 2, wherein,

[0117] The aforementioned metallic magnetic particles and the aforementioned synthetic resin are both located on the surface of the blank.

[0118] The average thickness of the first layer on the synthetic resin is greater than the average thickness of the first layer on the metallic magnetic particles.

[0119] [Postscript 4]

[0120] According to any one of the electronic components described in Appendix 1 to 3, among which,

[0121] The average thickness of the first layer on the blank is greater than the average thickness of the first layer on the internal wiring.

[0122] [Postscript 5]

[0123] According to any one of the electronic components described in Appendix 1 to 4, among which,

[0124] The average thickness of the first layer on the aforementioned blank is less than 3 μm.

[0125] [Postscript 6]

[0126] According to any one of the electronic components described in Appendix 1 to 5, among which,

[0127] The aforementioned blank has a recess that extends from the surface of the blank toward the interior.

[0128] The first layer mentioned above exists inside the aforementioned recess.

[0129] [Postscript 7]

[0130] According to any one of the electronic components described in Appendix 1 to 6, among which,

[0131] The aforementioned external electrode also has a second layer, which is stacked on the outer surface of the first layer on the side opposite to the blank, and contains Ni.

[0132] The first layer described above has continuous pores opening on the outer surface of the second layer.

[0133] The aforementioned second layer exists within at least a portion of the aforementioned continuous pores.

[0134] [Postscript 8]

[0135] According to the electronic components described in Appendix 7, among which,

[0136] The second layer reaches the internal wiring via the continuous pores.

[0137] [Postscript 9]

[0138] According to the electronic components described in Appendix 7 or 8, among which,

[0139] When the portion extending from the surface of the blank to the outer surface of the first layer is divided into two equal parts in a direction orthogonal to the surface of the blank—an inner layer on the blank side and an outer layer on the opposite side of the blank—

[0140] The proportion of the first layer in the outer layer is greater than the proportion of the first layer in the inner layer.

[0141] [Postscript 10]

[0142] According to any one of the electronic components described in Appendix 1 to 9, among which,

[0143] The aforementioned metallic magnetic particles have a particle body composed of a magnetic material and an insulating coating covering the surface of the particle body.

[0144] The first layer described above has multiple metal-containing portions, which contain metal elements other than Cu among the elements contained in the insulating coating described above.

[0145] When the external electrode is viewed in a cross-section orthogonal to the surface of the blank, the average circular equivalent diameter of the metal-containing portion in each location is 0.01 μm or more and 10 μm or less.

[0146] [Postscript 11]

[0147] According to any one of the electronic components described in Appendix 1 to 10, among which,

[0148] The aforementioned external electrodes also have:

[0149] The second layer, stacked on the outer surface of the first layer opposite to the blank, contains Ni; and

[0150] The third layer is stacked on the outer surface of the second layer on the side opposite to the first layer, and contains Sn.

[0151] [Postscript 12]

[0152] According to any one of the electronic components described in Appendix 1 to 11, among which,

[0153] The aforementioned internal wiring refers to the inductor wiring wound inside the aforementioned blank.

[0154] [Postscript 13]

[0155] According to any one of the electronic components described in Appendix 1 to 12, among which,

[0156] The aforementioned external electrode also has a second layer, which is stacked on the outer surface of the first layer on the side opposite to the blank, and contains metallic elements other than Cu.

[0157] The first layer mentioned above contains elements other than Cu that constitute the second layer mentioned above.

[0158] [Postscript 14]

[0159] A method for manufacturing an electronic component, comprising:

[0160] The billet preparation process involves preparing a billet that contains internal wiring extensions and includes metallic magnetic particles and synthetic resin.

[0161] The coating process involves coating a conductive paste across the surface of the preform and the ends of the internal wiring; and

[0162] In the photofiring process, the conductive slurry is irradiated with light of a wavelength absorbed by the conductive slurry to form a first layer, and multiple voids are formed between the first layer and the synthetic resin in the preform.

[0163] Explanation of reference numerals in the attached figures

[0164] 10…Inductor component; 11…Bulkhead; 11A…Mounting surface of the bulkhead; 12…Metallic magnetic particles; 13…Synthetic resin; 21…Internal wiring; 31…First external electrode; 31A…First layer; P…Gap.

Claims

1. An electronic component, wherein, have: The blank contains metallic magnetic particles and synthetic resin; Internal wiring extends inside the aforementioned blank, with a portion exposed outside the aforementioned blank; and External electrodes, stacked on the surface of the aforementioned blank, are in contact with the aforementioned internal wiring. The aforementioned external electrode has a first layer, which is located closest to the blank side in the external electrode and contains Cu. There are multiple voids between the first layer and the synthetic resin in the preform.

2. The electronic component according to claim 1, wherein, When viewed in cross-section with a cross-section orthogonal to the surface of the blank, the average circular equivalent diameter of the aforementioned voids at each location is less than 100 nm.

3. The electronic component according to claim 1 or 2, wherein, Both the aforementioned metallic magnetic particles and the aforementioned synthetic resin are located on the surface of the blank. The average thickness of the first layer on the synthetic resin is greater than the average thickness of the first layer on the metallic magnetic particles.

4. The electronic component according to any one of claims 1 to 3, wherein, The average thickness of the first layer on the blank is greater than the average thickness of the first layer on the internal wiring.

5. The electronic component according to any one of claims 1 to 4, wherein, The average thickness of the first layer on the above-mentioned blank is less than 3 μm.

6. The electronic component according to any one of claims 1 to 5, wherein, The aforementioned blank has a recess that extends from the surface of the blank toward the interior. The first layer mentioned above exists inside the aforementioned recess.

7. The electronic component according to any one of claims 1 to 6, wherein, The aforementioned external electrode also has a second layer, which is stacked on the outer surface of the first layer opposite to the aforementioned blank, and contains Ni. The first layer described above has continuous pores opening on the outer surface of the second layer. The aforementioned second layer exists within at least a portion of the aforementioned continuous pores.

8. The electronic component according to claim 7, wherein, The second layer reaches the internal wiring via the continuous pores.

9. The electronic component according to claim 7 or 8, wherein, When dividing the portion from the surface of the billet to the outer surface of the first layer into an inner layer on the billet side and an outer layer on the opposite side of the billet in a direction orthogonal to the surface of the billet, The proportion of the first layer in the outer layer is greater than the proportion of the first layer in the inner layer.

10. The electronic component according to any one of claims 1 to 9, wherein, The aforementioned metallic magnetic particles have a particle body composed of a magnetic material and an insulating coating covering the surface of the particle body. The first layer described above has multiple metal-containing portions, which contain metal elements other than Cu among the elements contained in the insulating coating described above. When the external electrode is observed in cross-section with a cross-section orthogonal to the surface of the blank, the average circular equivalent diameter of the metal-containing portion in each part is 0.01 μm or more and 10 μm or less.

11. The electronic component according to any one of claims 1 to 10, wherein, The aforementioned external electrodes also have: The second layer, stacked on the outer surface of the first layer opposite to the blank, contains Ni; and The third layer is the outer surface of the second layer that is opposite to the first layer, and contains Sn.

12. The electronic component according to any one of claims 1 to 11, wherein, The aforementioned internal wiring refers to the inductor wiring wound inside the aforementioned blank.

13. The electronic component according to any one of claims 1 to 12, wherein, The aforementioned external electrode also has a second layer, which is stacked on the outer surface of the first layer opposite to the aforementioned blank, and contains metallic elements other than Cu. The first layer mentioned above contains elements other than Cu that constitute the second layer mentioned above.

14. A method for manufacturing an electronic component, wherein, Include: The billet preparation process involves preparing a billet that contains internal wiring extensions and includes metallic magnetic particles and synthetic resin. The coating process involves coating a conductive paste across the surface of the blank and the ends of the internal wiring; and In the photofiring process, the conductive slurry is irradiated with light of a wavelength absorbed by the conductive slurry to form a first layer, and multiple voids are formed between the first layer and the synthetic resin in the preform.

Citation Information

Patent Citations

  • Coil component, manufacturing method thereof, and electronic apparatus