Manufacturing method of terminal structural components, terminal structural components and terminal equipment
Patent Information
- Application Number
- CN202580024687.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-05-15
- Filing Date
- 2025-05-09
- Publication Date
- 2026-11-17
AI Technical Summary
When antenna vias are machined on terminal structural components, hole marks appear on the surface, affecting aesthetics and also impacting the performance of GPS, Bluetooth, and LTE signals.
Antenna vias are fabricated on a substrate and conductive paste is injected to form via antennas protruding from the outer surface. Then, a grindable masking layer is set on the outer surface. The markings are improved by grinding the masking layer, and other film layers are set on the masking layer to avoid affecting the appearance.
Without affecting the appearance, the performance of GPS, Bluetooth and LTE signals has been improved, and the problem of the through-hole antenna affecting the appearance has been solved.
Smart Images

Figure CN123126028A_ABST
Abstract
Description
Manufacturing method of terminal structural member, terminal structural member and terminal device
[0001] The present application claims priority from the Chinese patent application No. 202410605839.1 filed on May 15, 2024, and entitled "Manufacturing method of terminal structural member, terminal structural member and terminal device", the whole content of which is incorporated herein by reference. TECHNICAL FIELD
[0002] The present application relates to the technical field of terminal device, and particularly relates to a manufacturing method of terminal structural member, a terminal structural member and a terminal device. BACKGROUND
[0003] The first-level surface of a product refers to the main appearance surface of the product, which is the surface directly contacting with a user or directly presented to the user, and affects the visual experience of the user and the overall aesthetics of the product.
[0004] The outer surface of a terminal structural member (such as the outer frame of a watch, a tablet, etc.) is the first-level appearance surface. If a through-hole antenna is processed on the plastic material of the terminal structural member, and then a plurality of paint layers are covered on the plastic material, although the GPS, Bluetooth and LTE signals can be improved, the hole marks exist on the appearance surface, which affects the appearance surface of the terminal structural member. Therefore, how to process a through-hole antenna on the terminal structural member without affecting the appearance surface of the terminal structural member has been a difficult problem in the industry. SUMMARY
[0005] The present application provides a manufacturing method of terminal structural member, a terminal structural member and a terminal device to solve the technical problem in the prior art that processing an antenna through-hole on a terminal structural member affects the appearance surface of the terminal structural member.
[0006] The technical solution is as follows:
[0007] The first aspect of the present application provides a manufacturing method of terminal structural member, comprising the following contents:
[0008] Processing an antenna through-hole on a substrate of the terminal structural member, injecting a conductive slurry into the antenna through-hole and solidifying the conductive slurry to form a through-hole antenna, wherein the solidified conductive slurry protrudes from the outer surface of the substrate;
[0009] Processing an antenna on the surface of the substrate;
[0010] Processing a film layer on the outer surface of the substrate, the film layer comprising at least one polishable cover layer, and the cover layer is polished to improve the marks of the antenna through-hole.
[0011] In the process of making a via antenna, the outer surface of the substrate protrudes out of the via antenna, that is, the conductive paste solidified in the via antenna protrudes out of the outer surface of the substrate. When processing the film layer on the outer surface of the substrate, a polishable cover layer is arranged. The conductive paste protruding out of the via antenna will form a protruding mark on the cover layer. By polishing the cover layer, the mark can be improved. When subsequently arranging other coating layers on the cover layer, the influence of the via antenna on the other coating layers can be avoided, thereby realizing that the via antenna arranged can improve the GPS, Bluetooth and LTE signals without affecting the appearance of the terminal structure.
[0012] In some implementations, the solidified conductive paste is polished before printing the antenna on the surface of the substrate.
[0013] After the operation of the solidified conductive paste, the conductive paste protruding out of the outer surface of the substrate can be polished first. At this time, the polishing can reduce the polishing amount on the cover layer.
[0014] In some implementations, the conductive paste injected into the antenna via is a via paste, and the paste used to prepare the antenna on the surface of the substrate is a surface paste. The viscosity of the via paste is less than the viscosity of the surface paste, and / or the solvent proportion of the via paste is less than the solvent proportion of the surface paste.
[0015] The high viscosity of the via paste is beneficial to the liquid via paste protruding out of the outer surface of the substrate without overflowing to the surrounding, so as to facilitate the via antenna protruding out of the upper surface of the substrate.
[0016] When the via paste is heated and solidified, the organic solvent in the conductive paste will volatilize, which is not conducive to the conductive paste protruding out of the outer surface of the substrate after solidification. Therefore, it is preferred to reduce the proportion of the solvent in the via paste.
[0017] In some implementations, the conductive paste injected into the antenna via is a via paste, and the viscosity of the via paste ranges from 15,000 to 25,000 cps.
[0018] The liquid via paste is beneficial to protruding out of the outer surface of the substrate without overflowing to the surrounding, so as to facilitate the via antenna protruding out of the upper surface of the substrate.
[0019] In some implementations, the conductive paste injected into the antenna via is a via paste, and the solvent proportion of the via paste ranges from 0 to 15%.
[0020] When pouring the silver paste into the antenna via, the liquid silver paste protrudes out of the substrate surface, while the solidified silver paste is below the substrate surface. Therefore, it is preferred to set the solvent proportion of the via paste to range from 0 to 15%.
[0021] In some implementations, the conductive paste injected into the antenna via is a via paste, and the solidification shrinkage rate of the via paste is less than 1%.
[0022] The via paste has low solidification shrinkage, so that the situation that the liquid silver paste protrudes from the surface of the substrate while the solidified silver paste is lower than the surface of the substrate does not occur when the silver paste is filled into the antenna via, and therefore the via paste is preferably a paste with low solidification shrinkage.
[0023] In some implementations, the conductive paste filled into the antenna via is a via paste, and the via paste has a thermal expansion coefficient less than 30x10 -6 / K.
[0024] In the preparation of the terminal structure, baking and solidification are required in the process of manufacturing the antenna and the film layer, and the substrate and the paste will expand thermally. The via paste is a paste with low thermal expansion coefficient, so as to ensure that the shrinkage ratio of the via paste and some substrates is close, and to avoid the situation that the difference between the thermal expansion coefficients of the via paste and the substrate is too large, which is not conducive to improving the printing mark.
[0025] In some implementations, the diameter of the antenna via is not greater than 0.15 mm.
[0026] If the diameter of the antenna via is too large, when the silver paste is filled into the antenna via, the top surface of the silver paste is concave without the silver paste overflowing onto the outer surface of the substrate, and the solid conductive paste is concave when the silver paste in the antenna via is solidified, so that the printing mark cannot be eliminated by polishing the cover layer.
[0027] In some implementations, the area on the substrate where the antenna via is to be processed is referred to as a via area, and the inner side surface of the via area is injection molded with a recess.
[0028] The thickness of the via area is less than the thickness of other areas on the substrate except the via area, so that the inner side surface of the via area is recessed to reduce the height value of the antenna via in the thickness direction of the substrate, facilitate one-time filling operation of the antenna via, and facilitate laser processing of the antenna via.
[0029] In some implementations, the height value of the via area in the thickness direction is 0.1-0.5 mm.
[0030] The height value of the via area in the thickness direction is 0.1-0.5 mm, i.e., the height value of the antenna via in the thickness direction is 0.1-0.5 mm, which facilitates one-time filling operation of the antenna via and facilitates laser processing of the antenna via.
[0031] In some implementations, there is more than one antenna via; the antenna via is processed on the planar area of the substrate; and / or the antenna via is processed on the curved surface area of the substrate; and / or the substrate has a raised area formed thereon, and the antenna via is processed on the side surface of the raised area in the circumferential direction.
[0032] The position of the antenna via hole on the substrate is not limited, as long as it can be processed on the substrate.
[0033] For the via hole antenna arranged on the plane and the arc surface, the corresponding area of the covering layer needs to be polished; for the via hole antenna arranged on the waist surface, the corresponding area of the covering layer does not need to be polished, because the waist surface has little effect on the appearance surface of the terminal structural member. In addition, according to the reflection of light, the waist surface has high diffuse reflectivity, the arc surface has lower diffuse reflectivity, the plane mirror has the lowest diffuse reflectivity, the diffuse reflected light is relatively dispersed, and the light is relatively weak. The mirror reflected light is relatively concentrated, and the light is relatively strong. Because the waist surface has high diffuse reflectivity, it appears relatively dark, and it is not easy to observe the mark on the waist surface. Therefore, when the via hole antenna is arranged on the waist surface, the corresponding area of the covering layer does not need to be polished. In the case of not affecting the appearance surface of the terminal structural member, the efficiency of preparing the terminal structural member is improved.
[0034] In some implementations, the thickness of the antenna printed on the outer surface of the substrate is not greater than 16 μm.
[0035] The planar antenna has a certain thickness, and the planar antenna arranged on the outer surface of the substrate also causes the appearance surface of the terminal structural member to form a certain drop mark. By constraining the drop height, the mark formed by the printed antenna on the terminal structural member is improved.
[0036] In some implementations, the antenna printed on the outer surface of the substrate is referred to as a planar outer antenna, and the angle between any two adjacent sides of the planar outer antenna is a rounded angle.
[0037] By making the angle between any two adjacent sides of the planar outer antenna a rounded angle, the ink accumulation at the free end of the antenna is effectively improved.
[0038] In some implementations, the material of the covering layer includes polyurethane resin material or the material of the covering layer includes UV resin material.
[0039] Polyurethane resin material and UV resin material are common coating materials, and selecting appropriate polyurethane resin material and appropriate UV resin material can polish the covering layer.
[0040] In some implementations, the color base ratio of the covering layer is 1:1 to 1:2.
[0041] The covering layer uses a higher color base ratio, so that the covering layer has better polishing properties.
[0042] In some implementations, the hydroxyl content of the resin in the covering layer is ≥1.0.
[0043] By setting the hydroxyl content of the resin in the covering layer to be ≥1.0, the covering layer has better polishing properties.
[0044] In some implementations, the cover layer includes a 2-n resin and a 6-n resin.
[0045] The 6-n resin is a high-n resin, and the 2-n resin is a low-n resin. The high-n resin and the low-n resin are matched with each other to improve the performance of the resin material, so that the cover layer has better polishing performance.
[0046] In some implementations, the thickness of the cover layer ranges from 5 to 40 μm.
[0047] The thickness of the cover layer is reasonably set so that the cover layer can be polished without affecting the thickness of the film on the terminal structural member.
[0048] In some implementations, the number of cover layers is two or more, one cover layer is coated on another cover layer, or a transition layer is first coated on one cover layer, and then another cover layer is coated on the transition layer.
[0049] Since the cover layer is designed to be polishable and the hardness of the cover layer is relatively large, the adhesion performance of the cover layer is relatively poor. In order to stabilize the film layer structure on the terminal structural member, a transition layer is arranged between the two cover layers. The arrangement of the transition layer can improve the stability of the connection between the two cover layers.
[0050] Of course, the transition layer can not be arranged between the two cover layers to improve the efficiency of preparing the terminal structural member.
[0051] In some implementations, when the number of cover layers is one, a transition layer is coated on the side of the cover layer away from the substrate; when the number of cover layers is two or more, the cover layer farthest away from the substrate along the thickness direction of the substrate is referred to as an upper cover layer, and a transition layer is coated on the side of the upper cover layer away from the substrate.
[0052] The transition layer is arranged to facilitate the stability of the film layer structure on the terminal structural member.
[0053] In some implementations, a bonding primer layer is first coated on the outer surface of the substrate, and then the cover layer is coated; a surface treatment agent is coated on the outer surface of the substrate as the bonding primer layer; or a primer is coated on the outer surface of the substrate as the bonding primer layer; or a surface treatment agent layer and a primer layer are coated on the outer surface of the substrate as the bonding primer layer.
[0054] Since the cover layer is designed to be polishable and the hardness of the cover layer is relatively large, the adhesion performance of the cover layer is relatively poor. In order to stabilize the film layer structure on the terminal device, a bonding primer layer is first coated on the outer surface of the substrate, and then the cover layer is coated.
[0055] In some implementations, the substrate is a two-color injection molding and a transparent material region is formed on the substrate; the film layer includes an adhesive bottom layer, a topcoat layer and a transparent treatment layer, the adhesive bottom layer is the innermost layer of the film layer, the topcoat layer is the outermost layer of the film layer, the inner side of the topcoat layer is connected with the transparent treatment layer, the transparent treatment layer is laser-engraved on the coating layer between the transparent treatment layer and the adhesive bottom layer, and the laser-engraved region corresponds to the transparent material region.
[0056] The second aspect of the present application provides a terminal structural member, which is prepared by the manufacturing method provided in any of the technical solutions, wherein the terminal structural member comprises a substrate, a planar antenna and a film layer, more than one via antenna is arranged on the substrate, the inner and outer surfaces of the substrate are printed with the planar antenna, the film layer is arranged on the outer surface side of the substrate, and the film layer comprises more than one polishable cover layer.
[0057] Through the above technical solution, since the terminal structural member is prepared by the above method, it at least has all the beneficial effects of the manufacturing method, which will not be repeated here.
[0058] In some implementations, the film layer includes an indium plating layer.
[0059] By arranging the indium plating layer, the corrosion resistance and appearance texture are improved.
[0060] In some implementations, the appearance surface of the terminal structural member is a matte surface or a high-gloss surface.
[0061] The outermost layer of the terminal structural member is a UV topcoat layer, and by arranging the appearance surface as a matte surface or a high-gloss surface, the appearance of the terminal structural member is improved.
[0062] The third aspect of the present application provides a terminal device comprising the terminal structural member provided in any of the above technical solutions.
[0063] Through the above technical solution, since the terminal device comprises the above terminal structural member, it at least has all the beneficial effects of the terminal structural member, which will not be repeated here. BRIEF DESCRIPTION OF DRAWINGS
[0064] FIG. 1 is a front view schematic diagram of a watch;
[0065] FIG. 2 is a rear view schematic diagram of the watch;
[0066] FIG. 3 is a cross-sectional view schematic diagram of the watch case in FIG. 1 along A-A direction;
[0067] FIG. 4 is a rear view schematic diagram of another existing watch;
[0068] FIG. 5 is a cross-sectional view schematic diagram of an existing terminal structural member;
[0069] FIG. 6 is a cross-sectional view schematic diagram of another existing terminal structural member;
[0070] Figure 7 is a cross-sectional view of a prior art terminal structure;
[0071] Figure 8 is a cross-sectional view of a prior art terminal structure;
[0072] Figure 9 is a cross-sectional view of a prior art terminal structure;
[0073] Figure 10 is a cross-sectional view of a prior art terminal structure;
[0074] Figure 11 is a cross-sectional view of a substrate with a via antenna according to an embodiment of the present application;
[0075] Figure 12 is a cross-sectional view of a substrate with a cover layer according to an embodiment of the present application (the cover layer is not polished);
[0076] Figure 13 is a cross-sectional view of a substrate with a cover layer according to an embodiment of the present application (the cover layer is polished);
[0077] Figure 14 is a cross-sectional view of a substrate according to an embodiment of the present application;
[0078] Figure 15 is a front view of a circular substrate according to an embodiment of the present application;
[0079] Figure 16 is a cross-sectional view of the circular substrate of Figure 15 at B-B;
[0080] Figure 17 is a front view of a square substrate according to an embodiment of the present application;
[0081] Figure 18 is a front view of a circular substrate with a printed PDS antenna according to an embodiment of the present application;
[0082] Figure 19 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0083] Figure 20 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0084] Figure 21 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0085] Figure 22 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0086] Figure 23 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0087] Figure 24 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0088] Figure 25 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0089] Figure 26 is a cross-sectional view of a terminal structure according to an embodiment of the present application;
[0090] Fig. 27 is a cross-sectional view of a terminal structural member according to an embodiment of the present application;
[0091] Fig. 28 is a cross-sectional view of a terminal structural member according to an embodiment of the present application;
[0092] Fig. 29 is a cross-sectional view of a terminal structural member according to an embodiment of the present application;
[0093] Fig. 30 is a cross-sectional view of a terminal structural member according to an embodiment of the present application;
[0094] Fig. 31 is a cross-sectional view of a terminal structural member according to an embodiment of the present application.
[0095] In the drawings: 1, watch; 11, housing; 12, display assembly; 13, light-transmitting portion; 111, front housing; 112, rear housing; 113, transparent region; 2, terminal structural member; 21, base material; 22, substrate; 23, film layer; 24, PDS antenna; 25, via antenna; 211, PC transparent material region; 221, antenna via; 222, via region; 223, arc surface; 224, flat surface; 225, waist-shaped surface; 226, transparent material region; 231, treatment agent layer; 232, PU color paint layer; 233, UV topcoat layer; 234, PU primer layer; 235, UV primer layer; 236, indium plating layer; 237, UV midcoat layer; 238, PU cover layer; 239, masking layer; 2310, adhesive primer layer; 2311, transition layer; 2312, transparent treatment layer; 2313, laser-engraved region; 241, flat-surface outside antenna; 2411, rounded corner; 2412, hollowed-out region; 2391, PU masking layer; 2392, UV masking layer. DETAILED DESCRIPTION
[0096] In order to make the objectives, technical solutions and advantages of the present application clearer, the embodiments of the present application will be further described in detail below with reference to the drawings. The embodiments described by reference to the drawings are exemplary and are intended to explain the present application, and cannot be understood as a limitation of the present application.
[0097] In the description of the present application, it should be understood that the terms "length", "width", "thickness", "top", "bottom", "inner", "outer", "upper", "lower", "left", "right", and the like indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, and are only for the purpose of facilitating the description of the present application and simplifying the description, and therefore cannot be understood as indicating or implying that the device or element referred to must have a particular orientation, be constructed and operated in a particular orientation, and therefore cannot be understood as a limitation of the present application.
[0098] In order to clearly describe the technical solutions of the present application, the terms "first", "second", etc. are used to distinguish the same or similar items or functions and roles. Those skilled in the art can understand that the terms "first", "second", etc. do not limit the quantity and execution order, and the terms "first", "second", etc. also do not necessarily mean different.
[0099] In the present application, unless otherwise explicitly specified and limited, the terms "connected", "connected", etc. should be understood broadly, for example, it can be fixedly connected, or it can be detachably connected, or it can be integrated; it can be mechanically connected, or it can be electrically connected; it can be directly connected, or it can be indirectly connected through an intermediate medium; it can be the internal communication of two elements or the interaction relationship between two elements. Those skilled in the art can understand the specific meaning of the above terms in the present application according to the specific circumstances.
[0100] In the present application, "and / or" is only a description of the association relationship between the associated objects, which means that there can be three relationships; for example, A and / or B can mean that there are three cases of A alone, A and B together, and B alone. In addition, the character " / " in this paper generally represents that the front and rear associated objects are in an "or" relationship.
[0101] It should be noted that in the present application, the words "in an embodiment", "exemplarily", "for example" and the like are used to represent as an example, illustration or explanation. Any embodiment or design scheme described as "in an embodiment", "exemplarily", "for example" in the present application should not be interpreted as more preferred or more advantageous than other embodiments or design schemes. Rather, the use of "in an embodiment", "exemplarily", "for example" and the like is intended to present the relevant concept in a specific way.
[0102] Referring to FIGS. 1-4, FIG. 1 is a front view schematic diagram of a prior art watch, FIG. 2 is a rear view schematic diagram of the prior art watch, FIG. 3 is a A-A cross-sectional view schematic diagram of the watch shell in FIG. 1, and FIG. 4 is a rear view schematic diagram of another prior art watch.
[0103] The outer surface of the terminal structural member is an appearance primary surface. For example, when the terminal device is a watch, the terminal structural member is the shell of the watch; when the terminal device is a mobile phone, the terminal structural member can be the middle frame or the back cover of the mobile phone; when the terminal device is an electronic device such as a personal computer (PC) or a tablet computer, the terminal structural member can be the shell of the computer or the tablet computer.
[0104] Referring to FIGS. 1-4, taking a watch 1 as an example, the watch 1 includes a housing 11, a circuit board, a display module 12, a battery, a mainboard and the like. The housing 11 includes a front shell 111 and a rear shell 112. The display module 12 is arranged on the front shell 111. The battery and the mainboard are arranged in a receiving cavity surrounded by the front shell 111 and the rear shell 112. The front shell 111 and the rear shell 112 of the watch 1 are terminal structural members.
[0105] Referring to FIGS. 1-3, the rear shell 112 is provided with a hollow hole. A light-transmitting portion 13 is assembled at the hollow hole of the rear shell 112. The material of the light-transmitting portion 13 can be light-transmitting glass.
[0106] The watch 1 includes a vital sign sensor arranged in the housing 11. The vital sign sensor includes a light-emitting element and a light-receiving element. The light-emitting element can emit light to the skin of a user through the light-transmitting portion 13. Part of the light is absorbed by the skin of the user, and another part of the light is reflected by the skin of the user. The part of the light that is reflected is received by the light-receiving element. The vital sign sensor can be a PPG (PhotoPlethysmoGraph) sensor.
[0107] The terminal structural member generally includes a base material and a film layer sprayed on the base material. In addition, in order to improve the radio frequency signal of the terminal device, a PDS antenna is printed on the base material. The PDS antenna is connected with a PCB circuit board of the terminal device. The basic function of the antenna is to radiate and receive radio waves. When transmitting, the antenna converts high-frequency current into electromagnetic waves. When receiving, the antenna converts electromagnetic waves into high-frequency current. The antenna is an indispensable part of wireless communication.
[0108] The base material includes resin and reinforcing material. The reinforcing material is used to enhance the strength of the base material. Any material added to the resin to enhance the strength of the base material can be used as the reinforcing material. The resin can be PA (Polyamide, nylon). The reinforcing material can be glass fiber (GF). For example, the material of the base material 21 can be PA+55% GF material. PA+55% GF is a polyamide and glass fiber composite material. The content of the glass fiber is 55%.
[0109] Referring to FIG. 4, the rear shell 112 is not provided with a hollow hole. Instead, the rear shell 112 is formed with a transparent area 113 for light transmission. Specifically, the base material 21 of the rear shell 112 is double-injection molded. For example, the base material 21 is double-injection molded by using PA+55% GF material and polycarbonate (PC) material. The PC material is a transparent material and is used for the transparent area 113.
[0110] Referring to FIGS. 5-8, FIG. 5 is a cross-sectional view of a first existing terminal structure, FIG. 6 is a cross-sectional view of a second existing terminal structure, FIG. 7 is a cross-sectional view of a third existing terminal structure, and FIG. 8 is a cross-sectional view of a fourth existing terminal structure.
[0111] PU paint is a polyurethane coating, and UV paint is a coating that can be rapidly cured into a film in a few seconds under the irradiation of ultraviolet light. A treatment agent is used as a substance for treating the surfaces of plastics, fillers, pigments, and adhesive carriers, etc. in order to improve adhesion.
[0112] The following describes the film layer structure and manufacturing method of four existing terminal structures, which can be applied to the case that the light-transmitting portion 13 is provided on the rear case 112 of the watch 1. However, the following four film layer structures are not limited to being applied only to the watch 1.
[0113] (1) PA + 55% GF material + UV high-gloss paint, mainly applied to the rear case of a watch
[0114] Referring to FIG. 5, the film layer 23 on the material 21 is illustrated. In FIG. 5, the material 21 of PA + 55% GF material, the treatment agent layer 231, the PU color paint layer 232, and the UV topcoat layer 233 are sequentially arranged from bottom to top.
[0115] Color paint is paint in which various pigments and fillers are added to paint in order to impart color to a coating film, block light transmission, or enhance the mechanical and chemical properties of the coating film. Topcoat is the outermost film layer in a metal member coating system, and its main role is to shield the damaging effects of sunlight and polluted air on the surface of the metal member coating system, resist wind, snow, and rain, and have good aesthetic appearance. UV topcoat gloss is classified as matte, semi-matte, and bright.
[0116] The specific manufacturing method is as follows: PA + 55% GF material 21 is wiped with alcohol and electrostatically cleaned; a treatment agent is sprayed to a film thickness of 4-8 μm, baked at a temperature of 70-80°C for 10-30 min to form the treatment agent layer 231; PU color paint is sprayed to a film thickness of 8-15 μm, baked at a temperature of 70-80°C for 10-30 min to form the PU color paint layer 232; UV topcoat is sprayed to a film thickness of 20-30 μm, baked at a temperature of 50-60°C for 3-8 min, and irradiated with ultraviolet light having an energy of 800-1000 mJ / cm 2 to form the UV topcoat layer 233; numerical control (CNC) punching and laser engraving are performed.
[0117] (2) PA + 55% GF material + indium plating layer + UV topcoat, mainly applied to a mobile phone middle frame
[0118] Referring to FIG. 6, the film layer 23 on the substrate 21 is shown. In FIG. 6, from bottom to top, there are the substrate 21 of PA+55% GF material, the treatment agent layer 231, the PU primer layer 234, the UV primer layer 235, the indium plating layer 236, the UV intermediate coating layer 237, and the UV topcoat layer 233.
[0119] The primer is used to improve the adhesion of the topcoat, increase the fullness of the topcoat, provide alkali resistance, provide corrosion protection, etc., while ensuring uniform absorption of the topcoat, so that the paint system can achieve the best effect. The NCVM (Non conductive vacuum metallization) process is used to plate indium on the surface of the UV primer layer 235 to form the indium plating layer 236, so as to improve the corrosion resistance and appearance quality. The intermediate coating is an intermediate layer coating, which is commonly referred to as "intermediate paint".
[0120] The specific processing method is as follows: the substrate 21 of PA+55% GF material is wiped with alcohol and electrostatically cleaned; the treatment agent is sprayed to form the treatment agent layer 231, with a film thickness of 4-8 μm, an oven temperature of 70-80°C, and an oven time of 10-30 min; the black PU primer is sprayed to form the PU primer layer 234, with a film thickness of 6-10 μm, an oven temperature of 70-80°C, and an oven time of 10-20 min; the UV primer is sprayed to form the UV primer layer 235, with a film thickness of 22-25 μm, an oven temperature of 50-60°C, and an oven time of 3-8 min; the indium is plated to form the indium plating layer 236; the UV intermediate coating (mixed with color paste) is sprayed to form the UV intermediate coating layer 237, with a film thickness of 6-8 μm, an oven temperature of 50-60°C, and an oven time of 3-8 min; the UV topcoat is sprayed to form the UV topcoat layer 233, with a film thickness of 20-25 μm, an oven temperature of 50-60°C, and an oven time of 3-8 min, and then irradiated with ultraviolet light with an energy of 800-1000 mJ / cm 2
[0121] (3) PA+55% GF material substrate + PDS + UV topcoat, mainly applied to watch back
[0122] Referring to FIG. 7, the film layer 23 on the substrate 21 is shown. In the figure, from bottom to top, there are the substrate 21 of PA+55% GF material, the PDS antenna 24, the treatment agent layer 231, the PU cover layer 238, the UV primer layer 235, the PU color paint layer 232, and the UV topcoat layer 233.
[0123] The process of printing PDS antenna on the substrate is as follows: according to the antenna drawing, the surface of the steel plate is subjected to film and etching process to complete the production of different depth grooves of the steel plate. The conductive silver paste is poured into the pad printing equipment, the silver paste is scraped into the groove of the steel plate, under the action of a certain pressure, the pad printing rubber head dips the silver paste in the groove according to the groove pattern, and after air drying, the pad printing rubber head transfers the silver paste to the two sides of the substrate under a certain pressure, and is placed in an oven, and the curing temperature is 90-140℃, and the curing time is 2-4 hours.
[0124] The specific processing method is as follows: the substrate 21 made of PA+55% GF material is wiped with alcohol and electrostatically cleaned; PDS silver paste is pad printed to form a PDS antenna 24; a treatment agent 231 is sprayed with a film thickness of 3-12 μm, a baking temperature of 70-80℃, a baking time of 10-20 min, a PU cover layer 238 is sprayed with a film thickness of 20-35 μm, a baking temperature of 70-80℃, a baking time of 10-20 min, a UV primer is sprayed with a film thickness of 5-12 μm, a baking temperature of 50-60℃, a baking time of 3-8 min, then ultraviolet light with an energy of 800-1000 mJ / cm 2 is used for irradiation to form a UV primer layer 235; a PU covering color paint is sprayed with a film thickness of 5-15 μm, a baking temperature of 70-80℃, a baking time of 10-15 min to form a PU color paint layer 232; a UV topcoat is sprayed with a film thickness of 15-30 μm, a baking temperature of 50-60℃, a baking time of 3-8 min, then ultraviolet light with an energy of 800-1000 mJ / cm 2 is used for irradiation to form a UV topcoat layer 233; numerical control CNC punching and laser carving characters are performed.
[0125] (4) Substrate made of PA+55% GF material+PDS+indium plating layer+UV topcoat, mainly applied to watch back
[0126] Referring to FIG. 8, the film layer 23 on the substrate 21 is shown. In FIG. 8, from bottom to top, there are the substrate 21 made of PA+55% GF material, the PDS antenna 24, the treatment agent layer 231, the PU cover layer 238, the UV primer layer 235, the indium plating layer 236, the PU intermediate paint layer 237, and the UV topcoat layer 233.
[0127] The specific processing method is as follows: the PA+55% GF material 21 is wiped with alcohol and electrostatically cleaned; the PDS silver paste is pad printed to form the PDS antenna 24; the processing agent is sprayed to form a processing agent layer 231 with a film thickness of 3-12 μm, a baking temperature of 70-80°C, and a baking time of 10-20 min; the PU covering layer 238 is sprayed with a film thickness of 8-20 μm, a baking temperature of 70-80°C, and a baking time of 10-20 min; the UV primer is sprayed with a film thickness of 20-35 μm, a baking temperature of 50-60°C, a baking time of 3-8 min, and an energy of 800-1000 mJ / cm 2 to form a UV primer layer 235; the indium is electroplated to form an indium plating layer 236; the UV intermediate coating (mixed with color paste) is sprayed with a film thickness of 5-8 μm, a baking temperature of 50-60°C, a baking time of 3-8 min, and then irradiated with ultraviolet light with an energy of 800-1000 mJ / cm 2 to form a PU intermediate coating layer 237; the UV topcoat is sprayed with a film thickness of 15-30 μm, a baking temperature of 50-60°C, a baking time of 3-8 min, and then irradiated with ultraviolet light with an energy of 800-1000 mJ / cm 2 to form a UV topcoat layer 233; the numerical control CNC punching and laser-engraved characters are performed.
[0128] In the above first two terminal structural members 2, the PDS antenna 24 is not provided, resulting in poor radio frequency signals; in the latter two terminal structural members 2, the PDS antenna 24 is printed on the surface of the material 21, but the via antenna is not provided, which also affects the radio frequency signals.
[0129] Referring to FIG. 9, FIG. 9 is a cross-sectional view of a prior art terminal structural member.
[0130] The following is an example of a film layer structure and a manufacturing method of a prior art terminal structural member, which can be applied to the transparent area 113 formed on the back cover 112 of the watch 1. Of course, the following film layer structure is not limited to only being applied to the watch 1:
[0131] In FIG. 9, from bottom to top, there are the material 21 made of PA+55% GF and PA double-injection materials, the processing agent layer 231, the PU color coating layer 232, the transparent treatment layer 2312, and the UV topcoat layer 233.
[0132] The area corresponding to the PA material on the material 21 is the PC transparent material area 211, which corresponds to the transparent area 113 on the back cover 112; the transparent treatment layer 2312 is a transparent treatment agent.
[0133] The specific processing method is as follows: the PA+55% GF and PA double-injection material 21 is wiped with alcohol, electrostatic dust removal; a treatment agent is sprayed, the film thickness is 4-8 μm, the baking temperature is 70-80°C, and the baking time is 10-30 min, so as to form a treatment agent layer 231; PU color paint is sprayed, the film thickness is 8-15 μm, the baking temperature is 70-80°C, and the baking time is 10-30 min, so as to form a PU color paint layer 232; the PU color paint layer 232 is laser engraved, and the laser engraved area 2313 on the PU color paint layer 232 corresponds to the PC transparent material area 211 on the material 21; a transparent treatment agent is sprayed to form a transparent treatment layer 2312; a UV topcoat is sprayed, the film thickness is 20-30 μm, the baking temperature is 50-60°C, the baking time is 3-8 min, and the ultraviolet light with an energy of 800-1000 mJ / cm 2 is used for irradiation, so as to form a UV topcoat layer 233; numerical control CNC punching and laser engraved characters are performed.
[0134] Referring to FIG. 10, it is a sectional view of a schematic diagram of a material of a terminal structural member.
[0135] If the radio frequency signal is improved, a via hole antenna 25 can be arranged on the material 21, but a hole mark is formed on the appearance surface of the terminal structural member 2.
[0136] The PDS antenna is printed on the inner surface and the outer surface of the material 21 of the terminal structural member, a through hole is arranged on the material 21 in the thickness direction, the through hole is filled with a conductive paste, and the conductive paste is solidified to form the via hole antenna 25. The via hole antenna 25 can facilitate the PDS antenna on the upper surface of the material 21 to extend to the PDS antenna on the lower surface of the material.
[0137] Regarding the hole mark, after the conductive silver paste is poured into the antenna hole from the inner side of the material 21, the upper surface of the conductive silver paste is generally a concave arc surface. In the process of baking the conductive silver paste, the solidification of the conductive silver paste and the volatilization of the solvent inside the conductive silver paste will cause the via hole antenna 25 to shrink. Referring to FIG. 10, the top surface of the via hole antenna 25 is concave downward to form a concave arc surface 251, and thus the hole mark is formed on the appearance surface of the terminal structural member.
[0138] Therefore, how to process the via hole antenna on the terminal structural member without affecting the appearance surface of the terminal structural member has been a difficult problem in the industry.
[0139] Based on the above problems, the application provides a manufacturing method of a terminal structural member. When a via hole antenna is manufactured, the via hole antenna protrudes from the outer surface of a substrate. When a film layer on the outer surface of the substrate is processed, a polishable cover layer is arranged. The protruding part of the via hole antenna forms a protruding mark on the cover layer. The mark can be improved by polishing the cover layer. When other film layers are arranged on the cover layer subsequently, the influence of the via hole antenna on the other film layers can be avoided, so as to solve the mark of the via hole antenna, and improve the GPS, Bluetooth and LTE signals without affecting the appearance level of the terminal structural member.
[0140] The terminal structural member provided by the application is applied to scenarios including but not limited to tablets, mobile phones and watches.
[0141] The manufacturing method of the terminal structural member will be described in detail below with reference to the drawings.
[0142] Referring to FIGS. 11-13, FIG. 11 is a sectional view of a substrate provided with a via hole antenna; FIG. 12 is a sectional view of the substrate provided with a cover layer (the cover layer is not polished); and FIG. 13 is a sectional view of the substrate provided with a cover layer (the cover layer is polished).
[0143] A manufacturing method of a terminal structural member includes the following contents.
[0144] An antenna via hole 221 is processed on a substrate 22 of the terminal structural member 2. A conductive paste is injected into the antenna via hole 221, and the conductive paste is solidified to form a via hole antenna 25. The solidified conductive paste protrudes from the outer surface of the substrate 22.
[0145] An antenna is arranged on the substrate 22.
[0146] A film layer 23 is processed on the outer surface of the substrate 22. The film layer 23 includes at least one polishable cover layer 239. The cover layer 239 can be polished to improve the mark of the via hole antenna 25.
[0147] An antenna via hole 221 is arranged on the substrate 22. The antenna via hole 221 is a through hole on the substrate 22. The antenna via hole 221 communicates the inner surface and the outer surface of the substrate 22. A conductive paste is injected into the antenna via hole 221. The conductive paste is solidified in the antenna via hole 221 to form the via hole antenna 25. The inner surface and the outer surface of the substrate 22 are printed with an antenna. The outer surface of the substrate 22 is provided with the film layer 23 to form an appearance surface.
[0148] The conductive paste injected into the antenna via hole 221 includes metal silver. Of course, the conductive paste includes but is not limited to only silver. The material of the conductive paste can also be a conductive material such as copper or aluminum. When the conductive paste includes metal silver, it is called conductive silver paste.
[0149] The conductive paste is injected into the antenna via hole 221 and solidified to form the via antenna 25. The antenna is arranged on the inner side and the outer surface of the substrate 22. The antenna arranged on the side of the substrate 22 is referred to as a planar antenna, the antenna arranged on the inner side of the substrate 22 is referred to as a planar inner antenna, and the antenna arranged on the outer surface of the substrate 22 is referred to as a planar outer antenna 241. The planar outer antenna 241 is connected to the planar inner antenna through the via antenna 25, and the planar inner antenna is connected to the PCB of the terminal device.
[0150] In this embodiment, when the via antenna 25 is manufactured, the conductive paste in the antenna via hole 221 protrudes from the outer surface of the substrate 22. Referring to FIG. 11, the conductive paste in the antenna via hole 221 protruding from the outer surface of the substrate 22 is schematically shown. When the film layer 23 on the outer surface of the substrate 22 is processed, the polishable covering layer 239 is processed. The conductive paste protruding from the antenna via hole 221 forms a protruding mark on the covering layer 239. Referring to FIG. 12, the area of the covering layer 239 protruding upward under the influence of the via antenna 25 is schematically shown. The mark can be improved by polishing the covering layer 239. Referring to FIG. 13, the polished covering layer 239 is schematically shown. When other coating layers are subsequently arranged on the covering layer 239, the influence of the via antenna 25 on the other coating layers can be avoided, thereby realizing that the appearance of the terminal structural member 2 is not affected when the via antenna 25 is arranged to improve the GPS, Bluetooth, and LTE signals.
[0151] The covering layer 239 is a polishable coating layer. The covering layer 239 needs to meet certain hardness and thickness to realize that the covering layer 239 can be polished. In the prior art, the coating layers on the terminal structural member 2 cannot be polished, and the coating layers are easily punctured and have polishing marks when polished.
[0152] Preferably, the covering layer 239 comprises a high-crosslinking-degree resin.
[0153] The crosslinking degree of the resin refers to the number and density of chemical bonds formed by crosslinking groups in the resin molecules. The resin with a high crosslinking degree has better thermal stability, wear resistance, and mechanical properties.
[0154] The covering layer 239 comprises a high-crosslinking-degree resin, so that the covering layer 239 has better polishability.
[0155] Preferably, the covering layer 239 has a relatively high pigment-to-resin ratio.
[0156] The pigment-to-resin ratio is the ratio of pigments to resins in the coating.
[0157] The covering layer 239 has a relatively high pigment-to-resin ratio, so that the covering layer 239 has better polishability.
[0158] Specifically, the film layer 23 further comprises a bonding primer layer 2310 (surface treatment agent or primer) and a paint layer (topcoat or the like), and the covering layer 239 provided in the embodiment is arranged between the bonding primer layer 2310 and the paint layer.
[0159] Preferably, the number of the covering layer 239 is more than one. The more the number of the covering layer 239, the better the hiding of the mark. However, the more the number of the covering layer 239, the greater the thickness of the film layer 23 on the outer surface of the substrate 22, and the more complicated the operation. Therefore, a reasonable number of the covering layer 239 needs to be designed.
[0160] Preferably, the antenna on the surface of the substrate 22 is prepared by PDS process. In this case, the planar antenna is a PDS antenna 24. The PDS process is a technology for printing an antenna, specifically a pad printing process, which forms a conductive three-dimensional circuit by coating a conductive paste on the surface of a workpiece and printing multiple layers.
[0161] Preferably, the thickness of the antenna (planar outer antenna 241) printed on the outer surface of the substrate 22 is reduced to improve the mark formed by the difference between the planar outer antenna 241 and the substrate 22.
[0162] Preferably, more than one antenna via hole 221 is processed on the substrate 22 of the terminal structural part 2, and a conductive paste is filled in each antenna via hole 221 to form more than one via antenna 25 on the terminal structural part 2.
[0163] Specifically, the position of the antenna via hole 221 on the substrate 22 is not particularly limited as long as it can be processed on the substrate 22.
[0164] Preferably, the outer surface of the terminal structural part 2 is a matte surface or a high-gloss surface.
[0165] Preferably, the film layer 23 comprises an indium plating layer to increase the metallic texture of the outer surface of the terminal structural part 2.
[0166] The conductive paste filled in the antenna via hole 221 is a via paste, and the silver paste used to prepare the antenna on the surface of the substrate 22 is a surface paste. Preferably, the via paste is a conductive paste with relatively high viscosity.
[0167] The via paste has relatively high viscosity, which is beneficial to the liquid via paste protruding from the outer surface of the substrate 22 without overflowing to the surrounding, so as to facilitate the via paste protruding from the upper surface of the substrate 22 after solidification.
[0168] Preferably, the via paste is a conductive paste with relatively low solvent ratio.
[0169] When the via paste is heated and solidified, the organic solvent in the conductive paste will volatilize, which is not conducive to the conductive paste protruding from the outer surface of the substrate 22 after solidification. Therefore, it is preferred to reduce the ratio of the solvent in the via paste.
[0170] Preferably, the via paste is a conductive paste with low solidification shrinkage.
[0171] The via paste has low solidification shrinkage, so that when the conductive paste is filled into the antenna via 221, the liquid paste does not protrude from the surface of the substrate 22 and solidify below the surface of the substrate 22. Therefore, the via paste is preferably a paste with low solidification shrinkage.
[0172] In addition, the surface paste is preferably a conductive paste with low solidification shrinkage.
[0173] Preferably, the via paste is a conductive paste with low thermal expansion coefficient.
[0174] During the preparation of the terminal structure 2, the substrate 22 and the paste will expand due to the baking and solidification during the preparation of the antenna and the film layer 23. The via paste is a conductive paste with low thermal expansion coefficient, so that the shrinkage ratio of the via paste and the substrate 22 is close, and the difference in thermal expansion coefficient between the via paste and the substrate 22 does not adversely affect the printing.
[0175] In addition, the surface paste is preferably a paste with low thermal expansion coefficient.
[0176] Preferably, the parameters of the antenna via 221 are set reasonably, so that when the via antenna 25 is prepared, the conductive paste of the antenna via 221 protrudes from the surface of the substrate 22.
[0177] Specifically, the substrate 22 is made of plastic material, and different materials can be selected according to different application scenarios of the terminal structure 2.
[0178] The material of the substrate 22 includes resin and reinforcing material. The resin can be exemplified by PA (Polyamide, Nylon), PBT (Polybutylene Terephthalate, Polybutylene Terephthalate), PPS (Polyphenylene Sulfide, Polyphenylene Sulfide), PEEK (Poly(Ether-Ether-Ketone), Poly(Ether-Ether-Ketone)), PC (Polycarbonate, Polycarbonate) and the like. The reinforcing material can be exemplified by glass fiber (Glass Fiber, GF), carbon fiber (Carbon Fiber, CF) and the like. The reinforcing material serves to reinforce the strength of the substrate, and any material that can reinforce the strength of the substrate when added to the resin can be used as the reinforcing material.
[0179] The substrate 22 can be manufactured by double-color injection molding. In this case, the material of the substrate 22 includes the resin added with the reinforcing material and a transparent plastic material, which can be PC (Polycarbonate) or PMMA (Polymethyl Methacrylate).
[0180] The conductive paste injected into the antenna via hole 221 is a via hole paste, and the paste used to manufacture the surface antenna of the substrate 22 is a surface paste. In an embodiment, the viscosity of the via hole paste is less than that of the surface paste.
[0181] Viscosity refers to the resistance of a fluid to flow.
[0182] Because the conductive paste of the via hole antenna 25 needs to protrude out of the outer surface of the substrate 22, the via hole paste needs to be in a liquid state to protrude out of the outer surface of the substrate 22 when the via hole antenna 25 is manufactured.
[0183] Suppose the viscosity of the silver paste is very small. When the conductive paste is injected into the antenna via hole 221, if the conductive paste protrudes out of the outer surface of the substrate 22, because the resistance between the fluids is small, the conductive paste is prone to overflow out of the outer surface of the substrate 22, which is not conducive to the conductive paste of the via hole antenna 25 protruding out of the outer surface of the substrate 22. Therefore, the viscosity of the via hole paste should be relatively large.
[0184] The surface paste needs to be printed on the surface of the substrate 22 to form a planar antenna. If the surface paste is relatively large, it is not conducive to the printing of the surface paste. Therefore, the viscosity of the via hole paste should be relatively small.
[0185] In this embodiment, the viscosity of the via hole paste is set to be less than that of the surface paste, which is conducive to the conductive paste of the via hole antenna 25 protruding out of the outer surface of the substrate 22, and also facilitates the printing of the surface paste on the surface of the substrate 22.
[0186] In an embodiment, the viscosity of the via hole paste ranges from 15,000 cps to 25,000 cps.
[0187] The viscosity of the paste used to manufacture the surface antenna of the substrate 22 is generally about 5,000 pcs. In this embodiment, the viscosity of the via hole paste is designed to range from 15,000 cps to 25,000 cps, which is conducive to the conductive paste of the antenna via hole 221 protruding out of the outer surface of the substrate 22 after curing.
[0188] In this embodiment, the viscosity of the via hole paste ranges from 15,000 cps to 25,000 cps. For example, the viscosity of the via hole paste can be 15,000 cps, 20,000 cps, 25,000 cps, etc.
[0189] In an embodiment, the solvent ratio of the via paste is less than the solvent ratio of the surface paste.
[0190] The solvent ratio refers to the proportion of the solvent in the solution, which is usually expressed by mass ratio or volume ratio.
[0191] The composition of the conductive paste is complex. For example, the conductive silver paste includes high-purity silver powder, conductive medium, binder, other additives, organic solvent, polymer, glass oxide, organic raw material, and various additives, which jointly act to realize the conductivity and printing processability of the silver paste.
[0192] When the conductive paste is heated and cured, the organic solvent in the conductive paste volatilizes, which is not conducive to the protrusion of the cured conductive paste from the outer surface of the substrate 22. Therefore, it is better to reduce the solvent ratio in the via paste.
[0193] The addition of the solvent in the conductive paste can improve the performance of the silver paste and facilitate the coating and printing of the silver paste. Therefore, the solvent ratio of the silver paste is relatively large compared with the surface paste.
[0194] In the embodiment, the solvent ratio of the via paste is less than the solvent ratio of the surface paste, which is conducive to the protrusion of the cured conductive paste of the antenna via hole 221 from the outer surface of the substrate 22 and facilitates the printing and manufacturing of the planar antenna.
[0195] In an embodiment, the solvent ratio of the via paste ranges from 0 to 15%.
[0196] The conductive paste is usually a conductive silver paste. The solvent ratio of the silver paste for preparing the planar antenna usually ranges from 15 to 25%. In the embodiment, the solvent ratio of the via paste ranges from 0 to 15%, which is conducive to the protrusion of the cured conductive paste of the antenna via hole 221 from the outer surface of the substrate 22.
[0197] In the embodiment, the solvent ratio of the via paste ranges from 0 to 15%, for example, the solvent ratio of the via paste can be 5%, 8%, 10%, 15%, etc.
[0198] In an embodiment, the curing shrinkage of the via paste is less than 1%.
[0199] The curing shrinkage refers to the proportion of the volume reduction of the resin during the curing process.
[0200] In the embodiment, the curing shrinkage of the via paste is less than 1%. The low curing shrinkage of the via paste avoids the situation that the liquid silver paste protrudes from the surface of the substrate 22 while the cured silver paste is lower than the surface of the substrate 22 when the silver paste is poured into the antenna via hole 221.
[0201] Preferably, the surface paste has a curing shrinkage of less than 1%, which is conducive to the preparation of the planar antenna on the substrate 22.
[0202] In this embodiment, the via paste has a curing shrinkage of less than 1%, such as 0.7%, 0.9%, etc.
[0203] In one embodiment, the via paste has a thermal expansion coefficient of less than 30x10 -6 / K.
[0204] The thermal expansion coefficient is a physical quantity representing the thermal expansion property of an object, i.e., a measure of the expansion and contraction of the object due to temperature changes. The shrinkage ratio refers to the thermal expansion related to the dimensional change of the object.
[0205] When the material of the substrate 22 is a polyamide and glass fiber composite material, the via paste is provided with a thermal expansion coefficient of less than 30x10 -6 / K, so as to facilitate the shrinkage ratio of the via paste and the substrate 22 to be close, and avoid the difference between the thermal expansion coefficients of the via paste and the substrate 22 from being too large, which is not conducive to improving the hole mark.
[0206] Preferably, the surface paste has a thermal expansion coefficient of less than 30x10 -6 / K.
[0207] In this embodiment, the via paste has a thermal expansion coefficient of less than 30x10 -6 / K, such as a thermal expansion coefficient of 20x10 -6 / K, 10x10 -6 / K, etc.
[0208] Referring to FIG. 14, a cross-sectional view of a substrate is shown, which illustrates an antenna via 221.
[0209] In one embodiment, the diameter of the antenna via 221 is not greater than 0.15 mm.
[0210] Taking conductive paste as an example, if the diameter of the antenna via 221 is too large, when the silver paste is poured into the antenna via 221, the top surface of the silver paste is concave without silver paste overflowing onto the outer surface of the substrate 22, and when the silver paste in the antenna via 221 is cured, the solid conductive paste is concave, at which time the hole mark cannot be eliminated by polishing the cover layer 239.
[0211] In this embodiment, the diameter d of the antenna via 221 is not greater than 0.15 mm, and the small diameter of the antenna via 221 is conducive to the silver paste protruding from the outer surface of the substrate 22 without silver paste overflowing onto the outer surface of the substrate 22.
[0212] In the embodiment, the diameter of the antenna via hole 221 is not greater than 0.15 mm. For example, the diameter of the antenna via hole 221 can be set to 0.5 mm, 0.1 mm or 0.15 mm.
[0213] When the silver paste is filled into the antenna via hole 221, the conductive silver paste is filled into the antenna via hole 221 from the inner side of the substrate 22 by using a filling device. The diameter of the antenna via hole 221 is set to be not greater than 0.15 mm, and it is also easy to realize one-time filling operation, that is, when the conductive paste is filled into the antenna via hole 221 by using the filling device, the antenna via hole 221 can be filled by one-time filling operation. However, if the diameter of the antenna via hole 221 is large, the antenna via hole 221 can not be filled by one-time filling operation, so that two-time filling is required, which can affect the quality of filling the conductive paste into the antenna via hole 221.
[0214] In addition, the antenna via hole 221 can be processed on the substrate 22 of the terminal structure 2 by using the following method: the antenna via hole 221 is processed from the inner side to the outer side of the substrate 22 by using a laser, and then the burrs in the antenna via hole 221 are removed.
[0215] In the embodiment, when the number of the antenna via holes 221 is two, the diameters of the two antenna via holes 221 are the same or different.
[0216] In the embodiment, when the number of the antenna via holes 221 is more than three, the diameters of the antenna via holes 221 are the same, different or partially the same.
[0217] In one embodiment, the area of the substrate 22 where the antenna via hole 221 needs to be processed is referred to as a via hole area 222, and the inner side of the via hole area 222 is injection molded with a recess.
[0218] When the substrate 22 is injection molded, the thickness of the via hole area 222 is less than the thickness of other areas of the substrate 22 except the via hole area 222, and the inner side of the via hole area 222 is formed with a recess to reduce the height value of the antenna via hole 221 in the thickness direction of the substrate 22, so as to facilitate the one-time filling operation of the antenna via hole 221. Referring to FIG. 14, the via hole area 222 is shown.
[0219] When the conductive paste is filled into the antenna via hole 221 by using the filling device, the antenna via hole 221 can be filled by one-time filling operation. However, if the thickness of the via hole area 222 is large, the antenna via hole 221 can not be filled by one-time filling operation, so that two-time filling is required, which can affect the quality of filling the conductive paste into the antenna via hole 221.
[0220] Therefore, in order to facilitate the one-time grouting operation of the antenna via hole 221, the height of the antenna via hole 221 along the thickness direction of the substrate 22 should be as small as possible. However, a small height will affect the strength of the terminal structural part 2, so the height of the antenna via hole 221 (via hole area 222) along the thickness direction of the substrate 22 should be reasonably set.
[0221] For example, when the strength of the substrate 22 is relatively high, that is, the strength of the material used by the substrate 22 is relatively high, at this time, the height of the via hole area 222 along the thickness direction of the substrate 22 can be set to be small. When the strength of the substrate 22 is relatively small, that is, the strength of the material used by the substrate 22 is relatively low, at this time, the height of the via hole area 222 along the thickness direction of the substrate 22 can be set to be large.
[0222] In the embodiment, for the diameter of the via hole area 222, the diameter of the via hole area 222 should be as small as possible to improve the strength of the terminal structural part 2 under the condition that injection molding can be realized. Specifically, the diameter of the via hole area 222 (the diameter of the recess) is greater than the diameter of the antenna via hole 221, one via hole area 222 can process one antenna via hole 221, of course, one via hole area 222 can also process more than two antenna via holes 221.
[0223] In the embodiment, by setting the recessed via hole area 222, not only can the one-time grouting operation be facilitated, but also when the antenna via hole 221 is processed in the via hole area 222 by laser, the antenna via hole 221 can be processed by one round of laser, avoiding the need for multiple rounds of laser processing to affect the precision of the antenna via hole 221.
[0224] In the embodiment, the number of via hole areas 222 is more than one, for example, one or two via hole areas 222 are formed on the substrate 22.
[0225] In one embodiment, the height of the via hole area 222 along the thickness direction is 0.1-0.5 mm.
[0226] In the embodiment, the height of the via hole area 222 along the thickness direction is set to 0.1-0.5 mm, that is, the height of the antenna via hole 221 along the thickness direction is limited to 0.1-0.5 mm, in order to facilitate the one-time grouting operation of the antenna via hole 221.
[0227] In the embodiment, the height of the via hole area 222 along the thickness direction is 0.1-0.5 mm, for example, the height of the via hole area 222 along the thickness direction can be 0.1 mm, 0.3 mm or 0.5 mm, etc.
[0228] In one embodiment, before the antenna is set on the surface of the substrate 22, the conductive paste protruding from the outer surface side of the substrate 22 is polished.
[0229] After the conductive paste is injected into the antenna via hole and solidified, the conductive paste protruding from the outer surface side of the substrate 22 can be polished first. At this time, the polishing can reduce the polishing amount on the covering layer 239.
[0230] The polishing of the conductive paste protruding from the outer surface side of the substrate 22 can be referred to as rough polishing. Preferably, the rough polishing is performed first before the polishing of the covering layer 239 when the terminal structure 2 is prepared. Of course, the rough polishing can also be cancelled, that is, the conductive paste protruding from the outer surface side of the substrate 22 is not polished.
[0231] Regarding the polishing operation, 1500 mesh and 3000 mesh sandpaper can be used to polish alternately and evenly. When the conductive paste protruding from the outer surface side of the substrate 22 is polished, no polishing depression can occur. The polishing operation of the conductive paste protruding from the outer surface side of the substrate 22 includes but is not limited to the use of 1500 mesh and 3000 mesh sandpaper to polish alternately and evenly.
[0232] Referring to FIGS. 15-17, FIG. 15 is a schematic front view of a circular substrate; FIG. 16 is a schematic cross-sectional view at B-B in FIG. 15; and FIG. 17 is a schematic front view of a square substrate.
[0233] In an embodiment, the antenna via hole 221 is one or more; the antenna via hole 221 is processed on the planar region of the substrate 22; and / or the antenna via hole 221 is processed on the arc surface region of the substrate 22; and / or the raised region is formed on the substrate 22, and the antenna via hole 221 is processed on the side of the raised region in the circumferential direction.
[0234] The appearance surface of the terminal structure 2 generally includes a planar surface and an arc surface. If the raised region protruding outward is formed on the terminal structure 2, the circumferential side of the raised region can be referred to as a waist surface. Referring to FIGS. 15 and 17, the planar surface 224, the arc surface 223 and the waist surface 225 of the substrate 22 are shown. Regarding the arc surface 223, the regions on the appearance surface other than the waist surface 225 and the planar surface 224 can all be referred to as the arc surface 223.
[0235] The number of antenna via holes 221 can be one, and in this case, the antenna via hole 221 can be arranged on the planar surface 224 or the arc surface 223 or the waist surface 225.
[0236] The number of antenna via holes 221 can also be two, and in this case, the two antenna via holes 221 can be arranged on the planar surface 224 or the arc surface 223 or the waist surface 225; or the two antenna via holes 221 can be arranged on different surfaces, such as one on the planar surface 224 and one on the arc surface 223.
[0237] The number of antenna vias 221 can also be more than three, in which case the antenna vias 221 can all be arranged on the plane 224 or all be arranged on the arc surface 223 or all be arranged on the waist surface 225; or the antenna vias 221 can be arranged on the plane 224, the arc surface 223 and the waist surface 225.
[0238] For the via antenna 25 arranged on the plane 224 and the arc surface 223, polishing needs to be performed on the corresponding area of the cover layer 239; for the via antenna 25 arranged on the waist surface 225, polishing does not need to be performed on the corresponding area of the cover layer 239 because the waist surface 225 has little effect on the appearance surface of the terminal structural member 2. In addition, according to the reflection of light, the waist surface of the terminal structural member 2 has the highest diffuse reflectivity, the arc surface has the second highest diffuse reflectivity, the plane mirror has the lowest diffuse reflectivity, the diffuse reflected light is relatively dispersed, the light is relatively weak, the mirror reflected light is relatively concentrated, and the light is relatively strong. Because the waist surface has high diffuse reflectivity, it appears relatively dark, and thus the mark on the waist surface of the terminal structural member 2 is not easy to observe. Therefore, when the via antenna 25 is arranged on the waist surface 225 of the substrate 22, polishing does not need to be performed on the corresponding area of the cover layer 239. In this way, the efficiency of manufacturing the terminal structural member 2 is improved without affecting the appearance surface of the terminal structural member 2.
[0239] In this embodiment, when the antenna via 221 is arranged on the waist surface, the diameter of the antenna via 221 is not limited to less than 0.2 mm.
[0240] For example, the terminal structural member 2 is the back cover 112 of the watch 1, as shown in FIGS. 15 and 16, and the middle of the substrate 22 is formed with a hollow hole for mounting the light-transmitting part 13 of the terminal structural member 2.
[0241] For example, the terminal structural member 2 is the back cover 112 of the watch 1, as shown in FIG. 17, and the substrate 22 is formed by two-color injection molding, and the substrate 22 is formed with a transparent material area 226.
[0242] In one embodiment, the thickness of the antenna printed on the outer surface of the substrate 22 is not greater than 16 μm.
[0243] The antenna arranged on the side surface of the substrate 22 is referred to as a plane antenna, and the antenna arranged on the outer surface of the substrate 22 is referred to as a plane outer antenna 241. The plane outer antenna 241 has a certain thickness, and the plane outer antenna 241 also causes the appearance surface of the terminal structural member 2 to form a certain uneven mark. By restricting the thickness of the plane outer antenna 241, the mark formed on the terminal structural member 2 by the plane outer antenna 241 is improved.
[0244] In this embodiment, the thickness of the planar outer antenna 241 is not greater than 16 μm, for example, the thickness of the planar outer antenna 241 can be 10 μm, 12 μm, 14 μm, 16 μm, etc.
[0245] Preferably, since the planar outer antenna 241 needs to be connected with each via antenna, the number of the via antennas and the respective distribution on the substrate 22 will affect the area of the planar outer antenna 241 printed on the substrate 22. For example, when the number of the via antennas is relatively large and the distribution on the substrate 22 is relatively dispersed, a large area is used to print the PDS antenna on the substrate 22.
[0246] For example, the area of the planar outer antenna 241 printed on the substrate 22 is greater than 50%.
[0247] Referring to FIG. 18, FIG. 18 is a schematic front view of a circular substrate 22 on which a PDS antenna is printed. The planar outer antenna 241 is shown to be printed in a large area on the substrate 22.
[0248] When the planar outer antenna 241 is printed, the printing can be completed at one time, or according to the shape of the substrate 22, the planar outer antenna 241 can be printed twice.
[0249] In one embodiment, the angle between any two adjacent sides of the planar outer antenna 241 is a rounded corner 2411.
[0250] The PDS process is used to print the antenna, and the specific operation is as follows: silver paste is poured into a pad printing device, a pad printing rubber head dips the silver paste in the groove according to the groove pattern of the steel plate, and the pad printing rubber head silver paste is transferred to the surface of the substrate 22 provided with the antenna via 221 under a certain pressure after air drying.
[0251] The principle of the silver paste pad printing process is to use silicone deformation to take silver paste, and then use silicone deformation to remove silver paste. The silicone deformation is deformed from the middle to the periphery, so that the end receives extrusion of the silicone deformation to generate ink accumulation. The position of the ink accumulation has a thick thickness, so that the free end of the PDS antenna increases the difference in the appearance of the terminal structure 2.
[0252] In this embodiment, by setting the angle between any two adjacent sides of the planar outer antenna 241 as a rounded corner 2411, the ink accumulation condition of the free end of the PDS antenna is effectively improved, and the mark formed by the PDS antenna on the terminal structure 2 is improved. Referring to FIG. 18, the top angle of the free end of the planar outer antenna 241 is shown to be a rounded corner 2411.
[0253] In the embodiment, the two adjacent sides include any two adjacent outer sides or any two adjacent inner sides. The area of the unprinted planar outer antenna 241 is referred to as the hollow area 2412. As shown in FIG. 18, the hollow area 2412 is in a strip shape, and the angle between any two sides of the hollow area 2412 is the rounded corner 2411.
[0254] In the embodiment, the radius of the rounded corner between any two adjacent sides of the planar outer antenna 241 is preferably the same.
[0255] In the embodiment, the radius of the rounded corner between any two adjacent sides of the planar outer antenna 241 is preferably in the range of 0.2-1.0 mm. For example, the radius of the rounded corner between any two adjacent sides of the planar outer antenna 241 is 0.2 mm, 0.6 mm or 1.0 mm.
[0256] In the embodiment, the antenna arranged on the inner side of the substrate 22 is referred to as a planar inner antenna, and the angle between any two adjacent sides of the planar inner antenna is preferably a rounded corner.
[0257] In the embodiment, the radius of the rounded corner between any two adjacent sides of the planar inner antenna is preferably in the range of 0.2-1.0 mm.
[0258] In one embodiment, the material of the covering layer 239 includes a polyurethane resin material or the material of the covering layer 239 includes a UV resin material.
[0259] Polyurethane (PU), also known as polyurethane, is a high polymer material formed by polycondensation of polyol and polyisocyanate and has excellent mechanical properties. UV is a material that can be rapidly cured into a film in a few seconds under the irradiation of ultraviolet light, and is usually composed of resin, photoinitiator, auxiliary agent, etc.
[0260] In the embodiment, the covering layer 239 includes a polyurethane resin material or a UV resin material. Both the polyurethane resin material and the UV resin material are commonly used coating materials, and selecting appropriate polyurethane resin material and appropriate UV resin material can polish the covering layer 239.
[0261] Specifically, when the number of the covering layer 239 is one, the covering layer 239 includes a polyurethane resin material or a UV resin material.
[0262] When the number of the covering layer 239 is two, both of the covering layers 239 are polyurethane resin materials or both of the covering layers 239 are UV resin materials, or one of the covering layers 239 is a polyurethane resin material and the other is a UV resin material.
[0263] When the number of covering layers 239 is two, and one of them is made of polyurethane resin and the other is made of UV resin, the covering layer 239 made of polyurethane resin is arranged on the side close to the substrate 22, or the covering layer 239 made of UV resin is arranged on the side close to the substrate 22.
[0264] When the number of covering layers 239 is more than three, each of the covering layers 239 is made of polyurethane resin or UV resin, or both polyurethane resin and UV resin are included in the covering layers 239.
[0265] When the number of covering layers 239 is more than three, and both polyurethane resin and UV resin are included in the covering layers 239, the covering layers 239 made of polyurethane resin and the covering layers 239 made of UV resin are preferably arranged alternately.
[0266] In an embodiment, the pigment-to-binder ratio of the covering layer 239 is 1:1-1:2.
[0267] The pigment-to-binder ratio is the weight ratio of pigment to binder in the coating. By limiting the pigment-to-binder ratio of the covering layer 239 to 1:1-1:2, the covering layer 239 has better polishing performance.
[0268] In an embodiment, the resin hydroxyl content of the covering layer 239 is ≥1.0, based on the covering layer 239 being made of polyurethane resin.
[0269] The resin hydroxyl value is a parameter for evaluating the amount of hydroxyl groups in the resin molecules. The higher the hydroxyl value, the more hydroxyl groups there are in the resin molecules, and vice versa.
[0270] In this embodiment, by setting the resin hydroxyl content of the covering layer 239 to ≥1.0, the covering layer 239 has better polishing performance.
[0271] In an embodiment, the resin of the covering layer 239 includes 2-functional resin and 6-functional resin, based on the covering layer 239 being made of UV resin.
[0272] High-functional resin and low-functional resin refer to the number of functional groups in the polymer.
[0273] In this embodiment, the 6-functional resin is high-functional resin, and the 2-functional resin is low-functional resin. The high-functional resin and the low-functional resin are matched with each other to improve the performance of the resin material, so that the covering layer 239 has better polishing performance.
[0274] In an embodiment, the thickness of the covering layer 239 is 5-40 μm.
[0275] The thickness of the covering layer 239 is set reasonably so that the covering layer 239 can be polished without affecting the film thickness on the terminal structural member 2.
[0276] In this embodiment, the thickness of the covering layer 239 ranges from 5 to 40 μm, for example, the thickness of the covering layer 239 is 10 μm, 20 μm, 30 μm or 40 μm, etc.
[0277] In this embodiment, when the number of the covering layer 239 is two, the thickness of each covering layer 239 is the same or different.
[0278] In this embodiment, when the number of the covering layer 239 is more than three, the thickness of each covering layer 239 is the same, or the number of each covering layer 239 is not completely the same (i.e., there are some same), or the thickness of each covering layer 239 is different.
[0279] In this embodiment, when the number of the covering layer 239 is more than three, the thickness of the covering layer 239 of the same material is the same, and the thickness of the covering layer 239 of different materials is different.
[0280] In one embodiment, the substrate 22 of the terminal structural member 2 is made of plastic material. According to different application scenarios of the terminal structural member 2, the substrate 22 can be made of different materials.
[0281] Referring to Table 1 below, the following is a specific example:
[0282] The material of the terminal structural member 2 can be PA+20-75% GF, which is a polyamide and glass fiber composite material, wherein the content of glass fiber is 20-75%, and at this time, the terminal structural member 2 can be the shell of a watch.
[0283] The material of the terminal structural member 2 can be PA+20-75% GF and PC material, that is, the terminal structural member 2 is double-injection molded by using a polyamide and glass fiber composite material and a polycarbonate material, wherein the content of glass fiber in the polyamide material is 20-75%, and at this time, the terminal structural member 2 can be the shell of a notebook computer (Personal Computer, PC).
[0284] The material of the terminal structural member 2 can be PA+20-75% GF and PMMA material, that is, the terminal structural member 2 is double-injection molded by using a polyamide and glass fiber composite material and a polymethyl methacrylate material, wherein the content of glass fiber in the polyamide material is 20-75%, and at this time, the terminal structural member 2 can be the shell of a notebook computer (Personal Computer, PC).
[0285] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0286] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0287] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0288] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0289] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0290] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0291] The material of the terminal structure 2 can be PBT+10-50% GF and PC material, that is, the terminal structure 2 is double-color injection molded by using polybutylene terephthalate and glass fiber composite material and polycarbonate material, wherein the content of glass fiber in the polybutylene terephthalate is 10-50%, at this time, the terminal structure 2 can be a flat plate shell.
[0292] The material of the terminal structure 2 can be PC+20-30% GF and PMMA, i.e., the terminal structure 2 is formed by double-color injection molding of a polycarbonate and glass fiber composite material and a polymethyl methacrylate material, wherein the content of glass fiber in the polycarbonate is 20-30%, and at this time, the terminal structure 2 is a housing of a watch, a tablet, or the like.
[0293] Table 1
[0294] Referring to FIGS. 19-26, FIG. 19 is a cross-sectional view of a terminal structure, FIG. 20 is a cross-sectional view of a terminal structure, FIG. 21 is a cross-sectional view of a terminal structure, FIG. 22 is a cross-sectional view of a terminal structure, FIG. 23 is a cross-sectional view of a terminal structure, FIG. 24 is a cross-sectional view of a terminal structure, FIG. 25 is a cross-sectional view of a terminal structure, and FIG. 26 is a cross-sectional view of a terminal structure.
[0295] In an embodiment, the number of covering layers 239 is two or more, wherein one covering layer 239 is coated on another covering layer 239, or a transition layer 2311 is coated on one covering layer 239, and another covering layer 239 is coated on the transition layer 2311, and the transition layer 2311 is used to improve the bonding between the two covering layers 239.
[0296] In this embodiment, the number of covering layers 239 can be two, and the two covering layers 239 can improve the hole mark without making the thickness of the film layer 23 on the terminal structure 2 too thick. Of course, the number of covering layers 239 is preferably two, but the number of covering layers 239 is not limited to only two, and can be three or more.
[0297] When the number of covering layers 239 is two, referring to FIG. 22, one covering layer 239 is coated on another covering layer 239. At this time, the materials of the two covering layers 239 can be the same or different, and both of the two covering layers 239 need to be polished.
[0298] When the number of covering layers 239 is two, referring to FIG. 23, a transition layer 2311 is coated on one covering layer 239, and another covering layer 239 is coated on the transition layer 2311. At this time, the materials of the two covering layers 239 can be the same or different, and both of the two covering layers 239 need to be polished.
[0299] Since the covering layer 239 can be polished and the hardness of the covering layer 239 is relatively large, the adhesion of the covering layer 239 is relatively poor. In order to improve the stability of the film layer structure on the terminal structure 2, a transition layer 2311 is arranged between the two covering layers 239. The arrangement of the transition layer 2311 can improve the stability of the connection between the two covering layers 239.
[0300] Preferably, the transition layer 2311 comprises polyurethane and a hiding filler dispersed in the polyurethane, and in this case, the transition layer 2311 is also referred to as a PU transition layer.
[0301] When the number of the hiding layers 239 is more than three, the hiding layers 239 are arranged in sequence along the thickness direction and the two adjacent hiding layers 239 are connected; or, the hiding layers 239 are arranged in sequence along the thickness direction and the transition layer 2311 is arranged between any two adjacent hiding layers 239; or, the hiding layers 239 are arranged in sequence along the thickness direction, and there are two directly connected hiding layers 239 and two hiding layers 239 connected through the transition layer 2311.
[0302] In one embodiment, when the number of the hiding layers 239 is one, the transition layer 2311 is coated on the side of the hiding layer 239 away from the substrate 22; and when the number of the hiding layers 239 is more than one, the hiding layer 239 farthest from the substrate 22 is referred to as the upper hiding layer, and the transition layer 2311 is coated on the side of the upper hiding layer away from the substrate 22.
[0303] In the present embodiment, when the number of the hiding layers 239 is one, the transition layer 2311 is coated on the side of the hiding layer 239 away from the substrate 22, and then a color paint layer or the like is coated on the transition layer 2311, so as to facilitate the stability of the film layer structure on the terminal structural member 2. Of course, the transition layer 2311 is preferably coated on the side of the hiding layer 239 away from the substrate 22, and the transition layer 2311 can also not be coated on the side of the hiding layer 239 away from the substrate 22, but a color paint layer or the like is directly coated on the hiding layer 239.
[0304] In the present embodiment, when the number of the hiding layers 239 is more than one, the transition layer 2311 is coated on the side of the upper hiding layer (the hiding layer 239 farthest from the substrate 22 is referred to as the upper hiding layer) away from the substrate 22, and then a color paint layer or the like is coated on the transition layer 2311, so as to facilitate the stability of the film layer structure on the terminal structural member 2. Of course, the transition layer 2311 is preferably coated on the side of the upper hiding layer away from the substrate 22, and the transition layer 2311 can also not be coated on the side of the upper hiding layer away from the substrate 22, but a color paint layer or the like is directly coated on the upper hiding layer.
[0305] Preferably, the transition layer 2311 comprises polyurethane and a hiding filler dispersed in the polyurethane, and in this case, the transition layer 2311 is also referred to as a PU transition layer.
[0306] In one embodiment, the adhesive primer layer 2310 is first coated on the outer surface of the substrate 22, and then the hiding layer 239 is coated.
[0307] Since the design of the cover layer 239 can be polished, the hardness of the cover layer 239 is relatively large, and thus the adhesion of the cover layer 239 is relatively poor. In order to stabilize the film layer on the terminal device, the outer surface of the substrate 22 is coated with an adhesive primer 2310, and then the cover layer 239 is coated.
[0308] In this embodiment, after the adhesive primer 2310 is coated, the cover layer 239 is coated, and the cover layer 239 is polished to improve the hole marks.
[0309] In one embodiment, a surface treatment agent is coated on the outer surface of the substrate 22 as the adhesive primer 2310; or a primer is coated on the outer surface of the substrate 22 as the adhesive primer 2310; or a layer of surface treatment agent and a layer of primer are coated on the outer surface of the substrate 22 as the adhesive primer 2310.
[0310] Both the surface treatment agent and the primer have the effect of improving adhesion.
[0311] When the antenna is printed on the surface of the substrate 22, a surface treatment agent can be coated on the outer surface of the substrate 22, and the thickness of the surface treatment agent is preferably in the range of 1-5 μm.
[0312] When the antenna is printed on the surface of the substrate 22, a primer can also be coated on the outer surface of the substrate 22, and the thickness of the primer is preferably in the range of 3-15 μm.
[0313] When the antenna is printed on the surface of the substrate 22, a surface treatment agent can be coated on the outer surface of the substrate 22, and the thickness of the surface treatment agent is preferably in the range of 1-5 μm. A primer can also be coated on the outer surface of the substrate 22, and the thickness of the primer is preferably in the range of 3-15 μm.
[0314] Based on the above, referring to FIGS. 19-26, the following eight specific embodiments of the terminal structural member 2 are provided in this embodiment:
[0315] The substrate 22 of the terminal structural member 2 is made of PA+65% GF material, and PA+65% GF is a polyamide and glass fiber composite material, in which the glass fiber content is 65%. PA+65% GF is a crystalline material, with a bending modulus of 19-29 Gpa and a bending strength of 380 Mpa, which is stronger than PC+20% GF (non-crystalline material). Therefore, PA+65% GF is selected for the terminal structural member to meet the high modulus and high strength thinning requirements of the terminal structural member.
[0316] The through-hole antenna 25 is arranged on the PA+65% GF substrate 22. The substrate 22 is provided with an adhesive primer layer 2310, which is a surface treatment agent or a primer, or a surface treatment agent layer and a primer layer as the adhesive primer layer 2310. The UV topcoat layer 233 is a UV matte paint topcoat layer or a UV glossy paint topcoat layer. The PU covering layer 2391 refers to a covering layer 239 comprising a PU resin material, and the UV covering layer 2392 refers to a covering layer 239 comprising a UV resin material. The UV intermediate paint is mixed with color paste.
[0317] (1) PA+65% GF substrate 22 + PDS + UV covering layer 2392 + UV topcoat layer 233
[0318] Referring to FIG. 19, the film layers 23 on the substrate 22 are shown. In FIG. 19, from bottom to top, there are a PA+65% GF substrate 22, an adhesive primer layer 2310, a UV covering layer 2392, a PU color paint layer 232, and a UV topcoat layer 233.
[0319] The specific processing method is as follows: the PA+65% GF substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS through-hole antenna 25 is prepared; the PDS antenna 24 is prepared by pad printing PDS silver paste; the PDS appearance and performance are detected; the surface treatment agent or / and primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, and baking and curing are performed to form the adhesive primer layer 2310; the UV covering layer 2392 is sprayed, the film thickness is 5-40 μm, and baking and curing are performed; the UV covering layer 2392 is polished; the PU color paint is sprayed, the film thickness is 8-25 μm, and baking and curing are performed to form the PU color paint layer 232; the UV matte / glossy paint topcoat is sprayed, the film thickness is 15-35 μm, and baking and curing are performed to form the UV topcoat layer 233; CNC punching is performed; and the antenna performance is detected.
[0320] (2) PA+65% GF substrate 22 + PDS + PU covering layer 2391 + UV topcoat layer 233
[0321] Referring to FIG. 20, the film layers 23 on the substrate 22 are shown. In FIG. 20, from bottom to top, there are a PA+65% GF substrate 22, an adhesive primer layer 2310, a PU covering layer 2391, a PU color paint layer 232, and a UV topcoat layer 233.
[0322] The specific processing method is as follows: the PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and the primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, baking and curing are performed to form the adhesive primer layer 2310; the PU covering layer 2391 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the PU covering layer 2391 is polished; the PU color paint is sprayed, the film thickness is 5-20 μm, baking and curing are performed, and the PU color paint layer 232 is formed; the UV matte / high gloss paint surface is sprayed, the film thickness is 15-35 μm, baking and curing are performed, and the UV topcoat layer 233 is formed; CNC punching is performed; and the antenna performance is detected.
[0323] (3) PA+65% GF material substrate 22+PDS+UV covering layer 2392+PU covering layer 2391+UV topcoat layer 233
[0324] Referring to FIG. 21, the film layer 23 on the substrate 22 is shown. In FIG. 21, from bottom to top, there are the PA+65% GF material substrate 22, the adhesive primer layer 2310, the UV covering layer 2392, the PU covering layer 2391, the PU color paint layer 232, and the UV topcoat layer 233.
[0325] The specific processing method is as follows: the PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and the primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, baking and curing are performed to form the adhesive primer layer 2310; the PU covering layer 2391 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the PU covering layer 2391 is polished; the PU color paint is sprayed, the film thickness is 5-20 μm, baking and curing are performed, and the PU color paint layer 232 is formed; the UV matte / high gloss paint surface is sprayed, the film thickness is 15-35 μm, baking and curing are performed, and the UV topcoat layer 233 is formed; CNC punching is performed; and the antenna performance is detected.
[0326] (4) PA+65% GF material substrate 22+PDS+PU covering layer 2391+UV covering layer 2392+UV topcoat layer 233
[0327] Referring to FIG. 22, the film layer 23 on the substrate 22 is shown. In FIG. 22, from bottom to top, there are the PA+65% GF material substrate 22, the adhesive primer layer 2310, the PU covering layer 2391, the UV covering layer 2392, the PU color paint layer 232, and the UV topcoat layer 233.
[0328] The specific processing method is as follows: the PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via hole antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and the primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, baking and curing are performed to form the adhesive primer layer 2310; the PU covering layer 2391 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the PU covering layer 2391 is polished; the UV covering layer 2392 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the UV covering layer 2392 is polished; the PU color paint is sprayed, the film thickness is 5-20 μm, baking and curing are performed to form the PU color paint layer 232; the UV matte / high gloss paint surface is sprayed, the film thickness is 15-35 μm, baking and curing are performed to form the UV topcoat layer 233; CNC punching is performed; and the antenna performance is detected.
[0329] (5) PA+65% GF material substrate 22+PDS+PU covering layer 2391+PU transition layer 2311+UV covering layer 2392+UV topcoat layer 233
[0330] Referring to FIG. 23, the film layer 23 on the substrate 22 is shown. In FIG. 23, from bottom to top, there are the PA+65% GF material substrate 22, the adhesive primer layer 2310, the PU covering layer 2391, the PU transition layer 2311, the UV covering layer 2392, the PU color paint layer 232, and the UV topcoat layer 233.
[0331] The specific processing method is as follows: the PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via hole antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and the primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, baking and curing are performed to form the adhesive primer layer 2310; the PU covering layer 2391 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the PU covering layer 2391 is polished; the PU transition layer 2311 is sprayed, the film thickness is 5-15 μm, baking and curing are performed; the UV covering layer 2392 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the UV covering layer 2392 is polished; the PU color paint is sprayed, the film thickness is 5-20 μm, baking and curing are performed to form the PU color paint layer 232; the UV matte / high gloss paint surface is sprayed, the film thickness is 15-35 μm, baking and curing are performed to form the UV topcoat layer 233; CNC punching is performed; and the antenna performance is detected.
[0332] (6) PA+65% GF material substrate 22+PDS+PU covering layer 2391+indium plating layer 236+UV topcoat layer 233
[0333] Referring to FIG. 24, the film layer 23 on the substrate 22 is shown. In FIG. 24, from bottom to top, there are the substrate 22 of PA+65% GF material, the adhesive primer layer 2310, the PU cover layer 2391, the UV primer layer 235, the indium plating layer 236, the UV mid-coat layer 237, and the UV top-coat layer 233.
[0334] The specific processing method is as follows: PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, and baking and curing are performed to form the adhesive primer layer 2310; the PU cover layer 2391 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the PU cover layer 2391 is polished; the UV primer is sprayed, the film thickness is 15-40 μm, baking and curing are performed to form the UV primer layer 235; the indium is electroplated to form the indium plating layer 236; the UV mid-coat paint is sprayed, the film thickness is 5-12 μm, baking and curing are performed to form the UV mid-coat layer 237; the UV matte / high gloss paint top-coat is sprayed, the film thickness is 15-35 μm, baking and curing are performed to form the UV top-coat layer 233; CNC punching is performed; and the antenna performance is detected.
[0335] (7) PA+65% GF material substrate 22+PDS+PU cover layer 2391+PU transition layer 2311+indium plating layer 236+UV top-coat layer 233
[0336] Referring to FIG. 25, the film layer 23 on the substrate 22 is shown. In FIG. 25, from bottom to top, there are the substrate 22 of PA+65% GF material, the adhesive primer layer 2310, the PU cover layer 2391, the PU transition layer 2311, the UV primer layer 235, the indium plating layer 236, the UV mid-coat layer 237, and the UV top-coat layer 233.
[0337] The specific processing method is as follows: the PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, baking and curing are performed to form the adhesive primer layer 2310; the PU covering layer 2391 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the PU covering layer 2391 is polished; the PU transition layer 2311 is sprayed, the film thickness is 5-20 μm, baking and curing are performed; the UV primer is sprayed, the film thickness is 15-40 μm, baking and curing are performed, and the UV primer layer 235 is formed; the indium is electroplated to form the indium plating layer 236; the UV mid-coat paint is sprayed, the film thickness is 5-12 μm, baking and curing are performed to form the UV mid-coat paint layer 237; the UV matte / high gloss paint surface is sprayed, the film thickness is 15-35 μm, baking and curing are performed to form the UV topcoat layer 233; CNC punching is performed; and the antenna performance is detected.
[0338] (8) PA+65% GF material substrate 22+PDS+UV covering layer 2392+PU transition layer 2311+indium plating layer 236+UV topcoat layer 233
[0339] Referring to FIG. 26, the film layer 23 on the substrate 22 is shown. In FIG. 26, from bottom to top, there are the PA+65% GF material substrate 22, the adhesive primer layer 2310, the UV covering layer 2392, the PU transition layer 2311, the UV primer layer 235, the indium plating layer 236, the UV mid-coat paint layer 237, and the UV topcoat layer 233.
[0340] The specific processing method is as follows: the PA+65% GF material substrate 22 is wiped with alcohol and electrostatically cleaned; the PDS via antenna 25 is prepared; the PDS silver paste is pad printed to prepare the PDS antenna 24; the PDS appearance and performance are detected; the surface treatment agent or / and primer is sprayed, the film thickness of the treatment agent is 1-5 μm, the film thickness of the primer is 3-15 μm, baking and curing are performed to form the adhesive primer layer 2310; the UV covering layer 2392 is sprayed, the film thickness is 5-40 μm, baking and curing are performed, and the UV covering layer 2392 is polished; the PU transition layer 2311 is sprayed, the film thickness is 5-20 μm, baking and curing are performed; the UV primer is sprayed, the film thickness is 15-40 μm, baking and curing are performed, and the UV primer layer 235 is formed; the indium is electroplated to form the indium plating layer 236; the UV mid-coat paint is sprayed, the film thickness is 5-12 μm, baking and curing are performed to form the UV mid-coat paint layer 237; the UV matte / high gloss paint surface is sprayed, the film thickness is 15-35 μm, baking and curing are performed to form the UV topcoat layer 233; CNC punching is performed; and the antenna performance is detected.
[0341] In combination with the above content, a specific embodiment of a terminal structural member 2 manufacturing method is provided, including the following content:
[0342] Step 1: PDS via + polishing process
[0343] At the position of the antenna via hole 221, a reserved thickness of 0.3-0.35mm is injected, a laser is used to pass through the hole from the inside to the outside of the substrate 22, the aperture is 0.1-0.15mm; a steel needle is used to remove the filaments in the hole (microscope observation of the through hole without filaments and impurities), conductive paste is slowly filled into the antenna via hole 221, and bubbling is prevented during the filling process. Place the oven at a temperature of 90-120℃, and bake for 1-2 hours for curing. Then, the protruding silver paste on the outer surface of the substrate 22 is polished with 3000 mesh sandpaper.
[0344] Step 2: Steel plate manufacturing
[0345] According to the antenna drawing, the surface of the steel plate is subjected to a film and etching process to complete the manufacturing of different depth grooves on the steel plate, and the groove depth tolerance is ±1.0-2.5.
[0346] Step 3: PDS silver paste pad printing process
[0347] The conductive silver paste is added to 2-3% diluent, stirred for 15-25 minutes to mix evenly, then poured into the pad printing equipment, the silver paste is scraped into the groove of the steel plate, under the action of a certain pressure, the pad printing rubber head (35+ / -5HA) is used to dip the silver paste in the groove according to the groove pattern, after air drying for 1-2 seconds, the silver paste on the pad printing rubber head is transferred to the outer surface and the inner side of the substrate 22 with the via hole, and the substrate is placed in an oven at a baking temperature of 90-140℃ for 2-4 hours for curing.
[0348] Step 4: PDS antenna 24 film thickness analysis and resistance test
[0349] The PDS film thickness analysis and resistance measurement are performed by using a glue injection section, and at the same time, the PDS environmental test is performed.
[0350] Step 5: Spraying process + polishing process
[0351] Each film layer 23 is sprayed, wherein the film layer 23 includes several of the adhesive primer layer 2310, PU color paint layer 232, PU covering layer 2391, UV covering layer 2392, UV mid-coat layer 237, UV topcoat layer 233, UV primer layer 235, etc. For example, the PU color paint layer 232 is baked at a temperature of 75-85℃ for 10-20 minutes; the PU covering layer 2391 is baked at a temperature of 75-85℃ for 30-60 minutes; the UV covering layer 2392, the UV mid-coat layer 237, and the UV topcoat layer 233 are baked at a temperature of 55-65℃ for 5 minutes.
[0352] The PU covering layer 2391 and the UV covering layer 2392 are alternately polished flat with 1500 mesh / 3000 mesh sandpaper.
[0353] Step 6: Film layer 23 film thickness analysis and testing (adhesion, boiling, etc.).
[0354] Referring to FIGS. 27-31, FIG. 27 is a cross-sectional diagram of the terminal structure member 9, FIG. 28 is a cross-sectional diagram of the terminal structure member 10, FIG. 29 is a cross-sectional diagram of the terminal structure member 11, FIG. 30 is a cross-sectional diagram of the terminal structure member 12, and FIG. 31 is a cross-sectional diagram of the terminal structure member 13.
[0355] In one embodiment, the substrate 22 is two-color injection molded and the transparent material region 226 is formed on the substrate 22; the film layer includes an adhesive primer layer 2310, a topcoat layer, and a transparent treatment layer 2312, the adhesive primer layer 2310 is the innermost layer of the film layer, the topcoat layer is the outermost layer of the film layer, the inner side of the topcoat layer is connected with the transparent treatment layer 2312, the transparent treatment layer 2312 is laser-engraved on the coating layer between the transparent treatment layer 2312 and the adhesive primer layer 2310, and the laser-engraved region corresponds to the transparent material region 226.
[0356] The watch 1 includes a vital sign sensor disposed in the housing 11. The vital sign sensor includes a light emitting element and a light receiving element. The light emitting element can emit light to the user's skin through the transparent material region 226. Part of the light is absorbed by the user's skin, and another part of the light is reflected by the user's skin. The part of the light that is reflected is received by the light receiving element.
[0357] The substrate 22 is two-color injection molded, for example, the substrate 22 is two-color injection molded with PA+20-75% GF and PC, and the PC material forms the transparent material region 226 on the substrate 22.
[0358] For example, the transparent treatment layer 2312 is a transparent treatment agent, or a transparent treatment agent and a transparent UV coating form the transparent treatment layer 2312.
[0359] Preferably, when the transparent treatment layer 2312 is a transparent treatment agent, the thickness of the transparent treatment layer 2312 ranges from 2 to 12 μm.
[0360] Preferably, the transparent treatment layer 2312 is formed by a transparent treatment agent and a transparent UV coating, the thickness of the transparent treatment layer 2312 ranges from 2 to 12 μm, and the thickness of the transparent UV coating ranges from 15 to 30 μm.
[0361] In this embodiment, the film layer generally does not include an indium plating layer 236.
[0362] For example, referring to FIG. 27, the film layer 23 on the substrate 22 is shown. In FIG. 27, from bottom to top, there are the substrate 22, the adhesive bottom layer 2310, the UV cover layer 2392, the PU color paint layer 232, the transparent treatment layer 2312, and the UV topcoat layer 233, wherein the transparent material region 226 is formed on the substrate 22, and the UV cover layer 2392 and the PU color paint layer 232 are laser-engraved in the region corresponding to the transparent material region 226.
[0363] For example, referring to FIG. 28, the film layer 23 on the substrate 22 is shown. In FIG. 28, from bottom to top, there are the substrate 22, the adhesive bottom layer 2310, the PU cover layer 2391, the PU color paint layer 232, the transparent treatment layer 2312, and the UV topcoat layer 233, wherein the transparent material region 226 is formed on the substrate 22, and the PU cover layer 2391 and the PU color paint layer 232 are laser-engraved in the region corresponding to the transparent material region 226.
[0364] For example, referring to FIG. 29, the film layer 23 on the substrate 22 is shown. In FIG. 29, from bottom to top, there are the substrate 22, the adhesive bottom layer 2310, the UV cover layer 2392, the PU cover layer 2391, the PU color paint layer 232, the transparent treatment layer 2312, and the UV topcoat layer 233, wherein the transparent material region 226 is formed on the substrate 22, and the UV cover layer 2392, the PU cover layer 2391, and the PU color paint layer 232 are laser-engraved in the region corresponding to the transparent material region 226.
[0365] For example, referring to FIG. 30, the film layer 23 on the substrate 22 is shown. In FIG. 30, from bottom to top, there are the substrate 22, the adhesive bottom layer 2310, the PU cover layer 2391, the UV cover layer 2392, the PU color paint layer 232, the transparent treatment layer 2312, and the UV topcoat layer 233, wherein the transparent material region 226 is formed on the substrate 22, and the PU cover layer 2391, the UV cover layer 2392, and the PU color paint layer 232 are laser-engraved in the region corresponding to the transparent material region 226.
[0366] For example, referring to FIG. 31, the film layer 23 on the substrate 22 is shown. In FIG. 31, from bottom to top, there are the substrate 22, the adhesive bottom layer 2310, the PU cover layer 2391, the PU transition layer 2311, the UV cover layer 2392, the PU color paint layer 232, the transparent treatment layer 2312, and the UV topcoat layer 233, wherein the transparent material region 226 is formed on the substrate 22, and the PU cover layer 2391, the PU transition layer 2311, the UV cover layer 2392, and the PU color paint layer 232 are laser-engraved in the region corresponding to the transparent material region 226.
[0367] The terminal structure 2 will be described in detail below with reference to the accompanying drawings.
[0368] Referring to FIGS. 19-31, FIG. 19 is a cross-sectional view of a terminal structural member, FIG. 20 is a cross-sectional view of a terminal structural member, FIG. 21 is a cross-sectional view of a terminal structural member, FIG. 22 is a cross-sectional view of a terminal structural member, FIG. 23 is a cross-sectional view of a terminal structural member, FIG. 24 is a cross-sectional view of a terminal structural member, FIG. 25 is a cross-sectional view of a terminal structural member, FIG. 26 is a cross-sectional view of a terminal structural member, FIG. 27 is a cross-sectional view of a terminal structural member, FIG. 28 is a cross-sectional view of a terminal structural member, FIG. 29 is a cross-sectional view of a terminal structural member, FIG. 30 is a cross-sectional view of a terminal structural member, and FIG. 31 is a cross-sectional view of a terminal structural member.
[0369] The present embodiment provides a terminal structural member 2 prepared by the manufacturing method provided by any of the above embodiments. The terminal structural member 2 comprises a substrate 22, a planar antenna in a film layer 23, one or more than one via antenna 25 disposed on the substrate 22, and a planar antenna printed on the inner and outer surfaces of the substrate 22. A plurality of film layers 23 are disposed on the outer surface side of the substrate 22, and the film layer 23 comprises one or more than one polishable cover layer 239.
[0370] When the via antenna 25 is manufactured, the via antenna 25 needs to protrude from the outer surface of the substrate 22. When the film layer 23 on the outer surface of the substrate 22 is processed, the polishable cover layer 239 is disposed. The protruding conductive paste of the antenna via 221 will form a protruding mark on the cover layer 239. By polishing the cover layer 239, the mark can be improved. When other coating layers are subsequently disposed on the cover layer 239, the influence of the via antenna 25 on the other coating layers can be avoided, and thus the appearance of the terminal structural member 2 is not affected when the GPS, Bluetooth, and LTE signals are improved by disposing the via antenna 25.
[0371] In an embodiment, an adhesive primer 2310 is first coated on the outer surface of the substrate 22, and then the cover layer 239 is coated.
[0372] Since the cover layer 239 is designed to be polishable and has a relatively large hardness, the adhesion of the cover layer 239 is relatively poor. In order to ensure the stability of the film layer 23 structure on the terminal device, an adhesive primer 2310 is first coated on the outer surface of the substrate 22, and then the cover layer 239 is coated.
[0373] Preferably, a surface treatment agent is coated on the outer surface of the substrate 22 as the adhesive primer 2310; or a primer is coated on the outer surface of the substrate 22 as the adhesive primer 2310; or a layer of surface treatment agent and a layer of primer are coated on the outer surface of the substrate 22 as the adhesive primer 2310.
[0374] In one embodiment, the number of covering layers 239 is two or more, wherein one covering layer 239 is coated on another covering layer 239, or, a transition layer 2311 is coated on one covering layer 239, and then another covering layer 239 is coated on the transition layer 2311, and the transition layer 2311 is used to improve the bonding between the two covering layers 239.
[0375] In this embodiment, the number of covering layers 239 can be two, and the two covering layers 239 can improve the hole mark without making the thickness of the film layer 23 on the terminal structural member 2 too thick. Of course, the number of covering layers 239 is preferably two, but the number of covering layers 239 is not limited to only two, and can be three or more.
[0376] Referring to FIG. 22, one covering layer 239 is coated on another covering layer 239.
[0377] Referring to FIG. 23, a transition layer 2311 is coated on one covering layer 239, and then another covering layer 239 is coated on the transition layer 2311. Since the covering layer 239 can be designed to be polished, the hardness of the covering layer 239 is relatively large, and the adhesion of the covering layer 239 is relatively poor. In order to improve the stability of the film layer structure on the terminal structural member 2, the transition layer 2311 is arranged between the two covering layers 239. The arrangement of the transition layer 2311 can improve the stability of the connection between the two covering layers 239.
[0378] Preferably, the transition layer 2311 includes polyurethane and covering fillers, and the covering fillers are dispersed in the polyurethane, and in this case, the transition layer 2311 is also called a PU transition layer.
[0379] In one embodiment, when the number of covering layers 239 is one, a transition layer 2311 is coated on the side of the covering layer 239 away from the substrate 22; and when the number of covering layers 239 is two or more, the covering layer 239 farthest away from the substrate 22 along the thickness direction of the substrate 22 is called an upper covering layer, and a transition layer 2311 is coated on the side of the upper covering layer away from the substrate 22.
[0380] In this embodiment, referring to FIG. 25, when the number of covering layers 239 is one, a transition layer 2311 is coated on the side of the covering layer 239 away from the substrate 22, and then a color paint layer or the like is coated on the transition layer 2311, so as to improve the stability of the film layer structure on the terminal structural member 2.
[0381] In this embodiment, when the number of covering layers 239 is two, a transition layer 2311 is coated on the side of the upper covering layer away from the substrate 22, and then a color paint layer or the like is coated on the transition layer 2311, so as to improve the stability of the film layer structure on the terminal structural member 2.
[0382] In an embodiment, the film layer 23 comprises an indium plating layer 236.
[0383] The indium plating is generally to deposit indium on the surface by electrolysis to form an indium film, so as to improve the corrosion resistance and appearance quality.
[0384] Referring to FIGS. 24-26, the indium plating layer 236 is shown. When the indium plating layer 236 is arranged, the UV primer layer 235 is arranged below the indium plating layer 236, the UV mid-coat layer 237 is arranged above the indium plating layer 236, and the UV top-coat layer 238 is arranged above the UV mid-coat layer 237.
[0385] In an embodiment, the appearance surface of the terminal structural member 2 is a matte surface or a high-gloss surface.
[0386] In the embodiment, referring to FIGS. 19-31, the outermost layer of the terminal structural member 2 is the UV top-coat layer 238, which is divided into a matte surface, a semi-matte surface, and a bright surface according to the gloss of the UV top-coat layer 238. Preferably, the appearance surface of the terminal structural member 2 is a matte surface or a high-gloss surface.
[0387] In an embodiment, referring to FIGS. 27-31, the substrate 22 is provided with a transparent material area 226, the film layer 23 comprises a top-coat layer and a transparent treatment layer 2312, the top-coat layer is the outermost layer of the film layer 23, the inner side of the top-coat layer is connected to the transparent treatment layer 2312, the transparent treatment layer 2312 and the adhesive primer layer 2310 are provided with laser engraving on the coating layer therebetween, and the laser-engraved area corresponds to the transparent material area 226.
[0388] In an embodiment, the thickness of the antenna printed on the outer surface of the substrate 22 is not greater than 16 μm.
[0389] In an embodiment, referring to FIG. 18, the angle between any two adjacent sides of the planar outer antenna 241 is a rounded corner 2411.
[0390] A terminal device comprises the terminal structural member 2 provided in any of the above embodiments.
[0391] The terminal device includes but is not limited to a handheld device, a vehicle-mounted device, a wearable device, a computing device, or other processing devices connected to a wireless modem. For example, the terminal device can include a smart watch, a smart wristband, a smart phone, a personal digital assistant (PDA) computer, a tablet computer, a laptop computer, a vehicle-mounted computer, smart glasses, and other terminal devices that need to be provided with a via antenna 25 on the terminal structural member 2.
[0392] The above-described embodiments are only used to illustrate the technical solutions of the present application, but not limit them; although the present application is described in detail with reference to the foregoing embodiments, those skilled in the art should understand that: it can still modify the technical solutions recorded in the foregoing embodiments, or make equivalent replacement to part of the technical features; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present application, and should be included in the protection scope of the present application.
Claims
1. A method of making a terminal structure member, characterized by, The application relates to a terminal structure and a manufacturing method thereof. The application comprises the following contents: An antenna via hole is processed on a substrate of a terminal structure, a conductive paste is injected into the antenna via hole, and the conductive paste is solidified to form a via hole antenna, wherein the solidified conductive paste protrudes from the outer surface of the substrate; An antenna is arranged on the surface of the substrate; 2. The method for manufacturing the terminal structural component as described in claim 1, characterized in that, A film layer is processed on the outer surface of the substrate, the film layer comprises at least one polishable cover layer, and the antenna via hole can be improved by polishing the cover layer.
3. The method for manufacturing the terminal structural component as described in claim 1, characterized in that, The solidified conductive paste is polished before the antenna is arranged on the surface of the substrate. The conductive paste injected into the antenna via hole is a via hole paste, and a paste for preparing a surface antenna of the substrate is a surface paste; 4. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The viscosity of the via hole paste is less than that of the surface paste, and / or the solvent proportion of the via hole paste is less than that of the surface paste.
5. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The conductive paste injected into the antenna via hole is a via hole paste, and the viscosity of the via hole paste ranges from 15000 to 25000 cps.
6. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The conductive paste injected into the antenna via hole is a via hole paste, and the solvent proportion of the via hole paste ranges from 0 to 15%.
7. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The conductive paste injected into the antenna via hole is a via hole paste, and a coefficient of thermal expansion of the via hole paste is less than 30x10 -6 / K.
8. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The conductive paste injected into the antenna via hole is a via hole paste, and the solidification shrinkage of the via hole paste is less than 1%.
9. The method of claim 1, wherein The diameter of the antenna via hole is not greater than 0.15 mm.
10. The method for manufacturing the terminal structural component as described in claim 9, characterized in that, The area of the substrate where the antenna via hole needs to be processed is referred to as a via hole area, the substrate is injection molded, and the inner side of the via hole area is injection molded with a recess.
11. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The height value of the via hole area along the thickness direction of the substrate ranges from 0.1 to 0.5 mm. The antenna via hole is more than one; The antenna via hole is processed on the planar area of the substrate; And / or the antenna via hole is processed on the curved surface area of the substrate; 12. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. And / or the antenna via hole is processed on the side surface of the convex area along the circumferential direction.
13. The method of claim 1, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The thickness of the antenna printed on the outer surface of the substrate is not greater than 16 mu m.
14. The method of claim 1-13, wherein The antenna printed on the outer surface of the substrate is referred to as a planar outer side antenna, and the angle between any two adjacent sides of the planar outer side antenna is a rounded angle.
15. The method for manufacturing the terminal structural component as described in claim 14, characterized in that, The material of the cover layer comprises a polyurethane resin material, or the material of the cover layer comprises a UV resin material.
16. The method of claim 14, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The color base ratio of the cover layer is 1:1 to 1:
2.
17. The method of claim 14, wherein the terminal structure is a terminal structure of a terminal of a mobile communication terminal. The hydroxyl content of the resin in the cover layer is greater than or equal to 1.
0.
18. The method of claim 1-13, wherein The cover layer comprises a 2-off resin and a 6-off resin.
19. The method of claim 1-13, wherein The thickness of the cover layer ranges from 5 to 40 mu m.
20. The method of claim 1-13, wherein The number of the cover layer is more than two, one cover layer is coated on another cover layer, or a transition layer is coated on one cover layer, and then another cover layer is coated on the transition layer.
21. The method of claim 1-13, wherein When the number of the cover layer is one, a transition layer is coated on the side of the cover layer away from the substrate; when the number of the cover layer is more than two, the cover layer farthest away from the substrate along the thickness direction of the substrate is referred to as an upper cover layer, and a transition layer is coated on the side of the upper cover layer away from the substrate. An adhesive primer is first coated on the outer surface of the substrate, and then the cover layer is coated; A surface treatment agent is coated on the outer surface of the substrate as the adhesive primer; Or, a primer is coated on the outer surface of the substrate as the adhesive primer layer; Or, a surface treatment agent layer and a primer layer are coated on the outer surface of the substrate as the adhesive primer layer.
22. The method of claim 1-13, wherein The substrate is a two-color injection molding and a transparent material region is formed on the substrate; the film layer comprises an adhesive primer layer, a topcoat layer and a transparent treatment layer, the adhesive primer layer is the innermost layer of the film layer, the topcoat layer is the outermost layer of the film layer, the inner side of the topcoat layer is connected with the transparent treatment layer, the transparent treatment layer and the adhesive primer layer are laser engraved on the coating layer therebetween, and the laser engraved region corresponds to the transparent material region.
23. A terminal construction element, characterized by The terminal structural member is prepared by the method for manufacturing the terminal structural member according to any one of claims 1-22, wherein the terminal structural member comprises a substrate, a planar antenna and a film layer, the substrate is provided with one or more than one via antenna, the inner and outer surfaces of the substrate are printed with the planar antenna, and the film layer is arranged on the outer surface side of the substrate, the film layer comprises one or more than one polishable cover layer.
24. The end termination of claim 23, wherein, The film layer comprises an indium plating layer.
25. The end termination of claim 23, wherein the outer surface of the outer sleeve is substantially cylindrical. The appearance surface of the terminal structural member is a matte surface or a high-gloss surface.
26. A terminal device, comprising: The terminal structural member comprises the terminal structural member according to any one of claims 23-25.