Liquid nitrogen cooling die cushion of extrusion die
Through the design of liquid nitrogen cooling die pad, liquid nitrogen evaporation and nitrogen encirclement are used to prevent oxidation reaction, solve the oxidation problem in aluminum profile extrusion and achieve die cooling, improving profile quality and die life.
Patent Information
- Application Number
- CN202323645171.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-09-24
- Estimated Expiration
- 2033-12-29
AI Technical Summary
During the extrusion process of aluminum profiles, the oxidation of aluminum and oxygen at high temperatures results in the production of aluminum oxide particles, which affects the quality of the profiles. Excessive extrusion speed may cause distortion, deformation or cracks of the profiles, and overheating of the mold will shorten the service life. A kind of Technology that avoids oxidation and cools molds.
A liquid nitrogen cooling mold pad is designed. By setting annular air guide grooves and ventilation grooves on the mold pad, liquid nitrogen evaporates and absorbs heat. Nitrogen enters the mold cavity through the air guide channel to form an inert gas surrounding circle, preventing oxidation reactions and cooling the mold at the same time.
It effectively avoids the generation of aluminum oxide particles, reduces the defect rate on the surface of the profile, extends the service life of the mold, and achieves an efficient cooling effect.
Smart Images

Figure CN221754350U
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of die pads of aluminum profile extrusion dies, in particular to a liquid nitrogen cooling die pad of the extrusion die. Background Art
[0002] At present, the extrusion die of aluminum profiles usually consists of two parts: a die surface and a die pad. The die pad of the extrusion die is usually a disc with a rectangular cross-section at the center. The die surface and the die pad are usually assembled and fastened in a surface-fitting manner to form a complete set of extrusion dies for aluminum profiles. The extrusion die is widely used in the production of various aluminum alloy profiles.
[0003] Among them, aluminum alloy extrusion is pressure-formed in a high-temperature and high-pressure environment, and the extrusion die is the core of aluminum alloy extrusion forming, that is, the extrusion die directly affects the size and surface quality of the profile. Specifically, the extrusion die needs to be heated to about 480°C before extrusion begins, and the aluminum alloy is formed at high temperature through the die working zone (the extrusion die working zone is a section in the aluminum extrusion die that is perpendicular to the die working end face and is used to ensure the shape, size and surface quality of the extruded product). However, in this process, metal aluminum will oxidize with oxygen at high temperatures, resulting in granular oxides on the surface of the profile, which affects the quality of the profile. For profile products with high surface requirements, this type of profile cannot be used because of the presence of aluminum oxide particles; at the same time, the metal friction between the profile surface and the die surface during extrusion and the ingot generate a lot of heat during thermoplastic deformation, resulting in an increase in the temperature of the mold, profile and ingot. If the extrusion speed is too high, the profile surface will be distorted, deformed, or even cracked. Defects such as; at the same time, the mold is overheated and its service life is shortened. In order to remove this extra heat, a strong cooling medium must be used.
[0004] Therefore, how to provide a mold pad that can avoid the generation of aluminum oxide particles and cool the mold to produce aluminum profiles is an urgent problem to be solved. Utility Model Content
[0005] One of the main purposes of the utility model is to provide a liquid nitrogen cooling die pad for an extrusion die, which can prevent aluminum profiles from generating aluminum oxide particles during extrusion molding and simultaneously achieve the effect of cooling the die.
[0006] In order to achieve the above-mentioned purpose of the utility model, the utility model provides a liquid nitrogen cooling die pad of an extrusion mold, including a die pad body, a die cavity penetrating its opposite surface is opened at the center position of the die pad body, a surface on the die pad body is set as a working surface, an annular air guide groove is opened on the working surface, the annular air guide groove surrounds the die cavity, a plurality of ventilation grooves communicating with the die cavity are opened between the annular air guide groove and the die cavity, a liquid nitrogen channel is also opened on the working surface, one end of the liquid nitrogen channel passes through the outer edge of the working surface, and the other end of the liquid nitrogen channel is communicated with the annular air guide groove.
[0007] Furthermore, the cross-section of the mold cavity is rectangular, and the four sides of the mold cavity on the working surface are respectively the first side, the second side, the third side and the fourth side, the first side is parallel to and opposite to the third side, the second side and the fourth side are parallel to and opposite to each other, a plurality of the ventilation grooves are arranged between the first side and the annular air guide groove, a plurality of the ventilation grooves are also arranged between the third side and the annular air guide groove, a plurality of the ventilation grooves are also arranged between the second side and the annular air guide groove, and a plurality of the ventilation grooves are also arranged between the fourth side and the annular air guide groove.
[0008] Furthermore, the number of ventilation grooves between the first side and the annular air guiding groove is equal to the number of ventilation grooves between the third side and the annular air guiding groove.
[0009] Furthermore, the number of ventilation grooves between the second side and the annular air guiding groove is equal to the number of ventilation grooves between the fourth side and the annular air guiding groove.
[0010] Furthermore, the number of ventilation grooves between the first side and the annular air guiding groove is greater than the number of ventilation grooves between the second side and the annular air guiding groove.
[0011] Furthermore, there are at least two ventilation grooves between the second side or the fourth side and the annular air guide groove.
[0012] Furthermore, at least three ventilation grooves are provided between the first side or the third side and the annular air guide groove.
[0013] Furthermore, a groove width of the ventilation groove between the first side and the annular air guiding groove is the same as a groove width of the ventilation groove between the second side and the annular air guiding groove.
[0014] Further, a groove width of the ventilation groove between the first side and the annular air guiding groove is smaller than a groove width of the ventilation groove between the second side and the annular air guiding groove.
[0015] Compared with the prior art, the liquid nitrogen cooling die pad of the extrusion die of the utility model has the following beneficial effects:
[0016] When the liquid nitrogen cooling die pad of the extrusion die of the utility model is in use, the working surface of the die pad is fitted and fastened together with the die surface, and then the aluminum ingot is placed in the die working belt of the die surface for extrusion into an aluminum profile. During the extrusion molding process, liquid nitrogen is injected into the liquid nitrogen channel. When the aluminum profile extends from the die working belt of the die surface and enters the die cavity of the die pad, the liquid nitrogen evaporates on the surface of the mold and the profile, and absorbs the heat of the mold during evaporation. Since the die surface and the die pad surface are fitted, the air guide groove forms an air guide channel inside the extrusion die. After the liquid nitrogen evaporates, nitrogen (inert gas) will enter the ventilation groove through the air guide channel and then enter the die cavity, thereby forming an inert gas encirclement around the discharge port of the aluminum profile, preventing the profile from contacting with oxygen, and blocking the high-temperature profile from oxidizing with oxygen, thereby avoiding the generation of aluminum oxide particles on the surface of the profile, and at the same time, achieving the effect of cooling the mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the structure of the liquid nitrogen cooling die pad of the extrusion die of the utility model;
[0018] Figure 2 It is a top view of the liquid nitrogen cooling die pad of the extrusion die of the utility model;
[0019] Figure 3 It is a schematic structural diagram of another angle of the liquid nitrogen cooling die pad of the extrusion die of the utility model;
[0020] Figure 4 This is a schematic diagram of the structure of an embodiment of the utility model involving setting a liquid nitrogen access nozzle in a liquid nitrogen channel;
[0021] Figure 5 It is a schematic diagram of an extrusion die according to an embodiment of the utility model.
[0022] Numbers in the attached drawings:
[0023] 10. Mold surface; 101. Mold working belt; 20. Mold pad; 201. Mold pad body; 2010. Working surface; 2011. Mold cavity; 20111. First side; 20112. Second side; 20113. Third side; 20114. Fourth side; 202. Annular air guide groove; 203. Ventilation groove; 204. Liquid nitrogen channel; 205. Liquid nitrogen access nozzle. DETAILED DESCRIPTION
[0024] It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0025] In the description of the present invention, it should be understood that the terms "length", "up", "down", "front", "back", "top", "bottom", etc. indicating the orientation or position relationship are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0026] In the description of the present utility model, it should be noted that, unless otherwise clearly specified and limited, the terms "install", "connect", "connect", and "set" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present utility model can be understood according to specific circumstances.
[0027] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0028] Embodiment 1
[0029] Please refer to Figure 1-Figure 5The utility model proposes a liquid nitrogen cooling die pad 20 of an extrusion die, comprising a die pad body 201, a die cavity 2011 penetrating the opposite surface of the die pad body 201 is provided at the center position thereof, a surface on the die pad body 201 is set as a working surface 2010, an annular air guide groove 202 is provided on the working surface, the annular air guide groove 202 surrounds the die cavity 2011, a plurality of ventilation grooves 203 communicating with the die cavity 2011 are provided between the annular air guide groove 202 and the die cavity 2011, a liquid nitrogen channel 204 is further provided on the working surface 2010, one end of the liquid nitrogen channel 204 penetrates the outer edge of the working surface 2010, and the other end of the liquid nitrogen channel 204 communicates with the annular air guide groove 202. When the liquid nitrogen cooling die pad 20 of the extrusion die of the utility model is used, the working surface 2010 of the die pad 20 is fastened to the die surface 10, and then the aluminum ingot is placed in the die working belt 101 of the die surface 10 for extrusion into an aluminum profile. During the extrusion molding process, liquid nitrogen is injected into the liquid nitrogen channel 204. When the aluminum profile extends from the die working belt 101 of the die surface 10 and enters the die cavity 2011 of the die pad 20, the liquid nitrogen evaporates on the surface of the mold and the profile, absorbing the heat of the mold during evaporation. Since the mold surface 10 and the mold pad 20 are in contact with each other, the air guide groove forms an air guide channel inside the extrusion mold. After the liquid nitrogen evaporates, the nitrogen (inert gas) will enter the air guide groove 203 through the air guide channel and then enter the mold cavity 2011, thereby forming an inert gas encirclement around the discharge port of the aluminum profile, preventing the profile from contacting with oxygen, and blocking the high-temperature profile from undergoing oxidation reaction with oxygen, thereby avoiding the generation of aluminum oxide particles on the surface of the profile and having the effect of cooling the mold.
[0030] In one embodiment, the cross-section of the mold cavity 2011 is rectangular, and the four sides of the mold cavity 2011 on the working surface 2010 are respectively a first side 20111, a second side 20112, a third side 20113 and a fourth side 20114. The first side 20111 and the third side 20113 are arranged parallel to each other, and the second side 20112 and the fourth side 20114 are arranged parallel to each other. A plurality of ventilation grooves 203 are arranged between the first side 20111 and the annular air guide groove 202, and a plurality of ventilation grooves 203 are also arranged between the third side 20113 and the annular air guide groove 202; a plurality of ventilation grooves 203 are also arranged between the second side 20112 and the annular air guide groove 202, and a plurality of ventilation grooves 203 are also arranged between the fourth side 20114 and the annular air guide groove 202. In this way, an inert gas surround can be quickly formed around the discharge port of the aluminum profile, further avoiding the generation of aluminum oxide particles on the surface of the profile.
[0031] In one embodiment, a liquid nitrogen access nozzle 205 is fixed at one end of the liquid nitrogen channel 204 facing away from the annular gas guide groove 202, and the liquid nitrogen access nozzle 205 can facilitate the liquid nitrogen to flow into the liquid nitrogen channel 204. The liquid nitrogen access nozzle 205 can be fixed to the mold pad body 201 by gluing.
[0032] In one embodiment, the number of ventilation grooves 203 between the first side 20111 of the mold cavity 2011 on the working surface 2010 and the annular air guide groove 202 is equal to the number of ventilation grooves 203 between the third side 20113 of the mold cavity 2011 on the working surface 2010 and the annular air guide groove 202, so that the speed at which nitrogen enters the mold cavity 2011 from the first side 20111 and the speed at which nitrogen enters the mold cavity 2011 from the third side 20113 are equal. Similarly, the number of ventilation grooves 203 between the second side 20112 of the mold cavity 2011 on the working surface 2010 and the annular air guide groove 202 is equal to the number of ventilation grooves 203 between the fourth side 20114 of the mold cavity 2011 on the working surface 2010 and the annular air guide groove 202, so that the rate at which nitrogen enters the mold cavity 2011 from the second side 20112 is the same as the rate at which nitrogen enters the mold cavity 2011 from the fourth side 20114.
[0033] In one embodiment, the number of ventilation grooves 203 between the first side 20111 of the mold cavity 2011 on the working surface 2010 and the annular air guide groove 202 is greater than the number of ventilation grooves 203 between the second side 20112 of the mold cavity 2011 on the working surface 2010 and the annular air guide groove 202. Since the cross section of the mold cavity 2011 is a rectangle, it can be understood that the first side 20111 and the third side 20113 of the mold cavity 2011 on the working surface 2010 are equal, the second side 20112 and the fourth side 20114 are equal, and the length of the first side 20111 is greater than the length of the second side 20112. Therefore, the number of ventilation grooves 203 between the first side 20111 and the annular air guide groove 202 is greater than the number of ventilation grooves 203 between the second side 20112 and the annular air guide groove 202, which can increase the flow rate of nitrogen entering the mold cavity 2011 from the first side 20111 or the third side 20113.
[0034] In one embodiment, at least two ventilation grooves 203 are provided between the second side 20112 or the fourth side 20114 and the annular air guide groove 202; at least three ventilation grooves 203 are provided between the first side 20111 or the third side 20113 and the annular air guide groove 202. Exemplarily, two ventilation grooves 203 are provided between the second side 20112 or the fourth side 20114 and the annular air guide groove 202, but not limited to two, and three ventilation grooves 203 are provided between the first side 20111 or the third side 20113 and the annular air guide groove 202, but not limited to three. Since the length of the first side 20111 is greater than that of the second side 20112, the length of the first side 20111 is equal to the length of the third side 20113, and the length of the second side 20112 is equal to the length of the fourth side 20114, three ventilation grooves 203 are arranged between the first side 20111 and the third side 20113 and the annular air guide groove 202, and two ventilation grooves 203 are arranged between the second side 20112 or the fourth side 20114 and the annular air guide groove 202 to ensure that nitrogen quickly forms an inert gas encirclement at the discharge port of the mold cavity 2011.
[0035] In one embodiment, the groove width of the ventilation groove 203 between the first side 20111 and the annular air guide groove 202 is the same as the groove width of the ventilation groove 203 between the second side 20112 and the annular air guide groove 202. This can avoid large differences in nitrogen entering the mold cavity 2011 through each ventilation groove 203, thereby avoiding affecting the rapid formation of an inert gas encirclement at the outlet of the mold cavity 2011.
[0036] Embodiment 2
[0037] The difference between this embodiment and the first embodiment is that the groove width of the ventilation groove 203 between the first side 20111 and the annular air guiding groove 202 is different from the groove width of the ventilation groove 203 between the second side 20112 and the annular air guiding groove 202 .
[0038] In this embodiment, the groove width of the vent groove 203 between the first side 20111 and the annular air guide groove 202 is smaller than the groove width of the vent groove 203 between the second side 20112 and the annular air guide groove 202, so that nitrogen can quickly form an inert gas encirclement at the discharge port of the mold cavity 2011, and at the same time, the rate of formation of the inert gas encirclement can be controlled. Therefore, for those skilled in the art, by reasonably changing the groove width and structure of each vent groove 203, it should also fall within the protection scope of the utility model.
[0039] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made by using the contents of the specification and drawings of the present invention, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A liquid nitrogen cooling die pad for an extrusion die, comprising a die pad body, wherein a die cavity penetrating through opposite surfaces of the die pad body is provided at the center thereof, wherein: A surface on the mold pad body is set as a working surface, an annular air guide groove is opened on the working surface, the annular air guide groove surrounds the mold cavity, a plurality of ventilation grooves communicating with the mold cavity are opened between the annular air guide groove and the mold cavity, and a liquid nitrogen channel is also opened on the working surface, one end of the liquid nitrogen channel passes through the outer edge of the working surface, and the other end of the liquid nitrogen channel is communicated with the annular air guide groove.
2. The liquid nitrogen cooling die pad of an extrusion die according to claim 1, characterized in that: The cross-section of the mold cavity is rectangular, and the four sides of the mold cavity on the working surface are respectively the first side, the second side, the third side and the fourth side, the first side is parallel to and opposite to the third side, the second side and the fourth side are parallel to and opposite to each other, a plurality of ventilation grooves are arranged between the first side and the annular air guide groove, a plurality of ventilation grooves are also arranged between the third side and the annular air guide groove, a plurality of ventilation grooves are also arranged between the second side and the annular air guide groove, and a plurality of ventilation grooves are also arranged between the fourth side and the annular air guide groove.
3. The liquid nitrogen cooling die pad of an extrusion die according to claim 2, characterized in that: The number of ventilation grooves between the first side and the annular air guiding groove is equal to the number of ventilation grooves between the third side and the annular air guiding groove.
4. The liquid nitrogen cooling die pad of an extrusion die according to claim 2, characterized in that: The number of ventilation grooves between the second side and the annular air guiding groove is equal to the number of ventilation grooves between the fourth side and the annular air guiding groove.
5. The liquid nitrogen cooling die pad of an extrusion die according to claim 2, characterized in that: The number of ventilation grooves between the first side and the annular air guiding groove is greater than the number of ventilation grooves between the second side and the annular air guiding groove.
6. The liquid nitrogen cooling die pad of an extrusion die according to claim 5, characterized in that: There are at least two ventilation grooves between the second side or the fourth side and the annular air guide groove.
7. The liquid nitrogen cooling die pad of an extrusion die according to claim 6, characterized in that: There are at least three ventilation grooves between the first side or the third side and the annular air guide groove.
8. The liquid nitrogen cooling die pad of an extrusion die according to claim 7, characterized in that: The groove width of the ventilation groove between the first side and the annular air guiding groove is the same as the groove width of the ventilation groove between the second side and the annular air guiding groove.
9. The liquid nitrogen cooling die pad of an extrusion die according to claim 7, characterized in that: The groove width of the ventilation groove between the first side and the annular air guiding groove is smaller than the groove width of the ventilation groove between the second side and the annular air guiding groove.