Molten steel anti-penetration tray in powder high-temperature alloy field

During the high-temperature alloy melting process, the anti-penetration tray for molten steel with an egg-tray structure and a threaded groove is used to solve the problem of poor anti-penetration effect of existing trays, achieve uniform distribution of molten steel and the formation of eddy currents, and significantly The risk of leaks and clogging is reduced and equipment safety is improved.

CN221795301UActive Publication Date: 2024-10-01HANGFA YOUCAI (ZHENJIANG) SUPERALLOY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420207936.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-29
Publication Date
2024-10-01
Estimated Expiration
2034-01-29

AI Technical Summary

Technical Problem

The existing molten steel tray has poor anti-penetration effect during the high-temperature alloy smelting process, resulting in leakage of molten steel and breakdown of the furnace body. It is also difficult to clean, affecting the purity of the alloy and the safety of the equipment.

Method used

An anti-penetration tray for molten steel in the field of powdered high-temperature alloys is designed. It adopts an egg-tray structure and a threaded groove combination to achieve rapid assembly and fixation through transverse and longitudinal snap-in structures. The egg-tray structure allows the molten steel to be evenly distributed and form eddy currents. , reducing the risk of leaks and clogging.

Benefits of technology

It effectively prevents uneven flow and blockage of liquid steel, improves the anti-penetration effect, reduces the probability of liquid steel accumulation and breakdown of the furnace body, and improves the practicality and safety of the pallet.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221795301U_ABST
    Figure CN221795301U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of metal smelting, and discloses a molten steel anti-penetration tray in the field of powder superalloy, which comprises anti-penetration tray bodies, grooves are formed in the anti-penetration tray bodies, transverse clamping structures are arranged on the side walls of the two transversely adjacent anti-penetration tray bodies, and the transverse clamping structures are arranged on the side walls of the two transversely adjacent anti-penetration tray bodies. The anti-penetration tray bodies are used for transversely fixing the two adjacent anti-penetration tray bodies, and longitudinal clamping structures are arranged on the side walls of the two longitudinally adjacent anti-penetration tray bodies. According to the molten steel anti-penetration tray in the powder high-temperature alloy field, through the design of the egg support type steel receiving disc, molten steel leaked from a crucible can be evenly distributed on the surface of the whole steel receiving disc, and the effect that the molten steel leaked from the crucible is prevented from flowing unevenly and blocking the steel receiving disc is achieved through the tray; and meanwhile, molten steel leaked from the crucible can generate vortexes through the curve grooves, the flow speed of the molten steel leaked from the crucible is further increased, the molten steel leaked from the crucible is prevented from being accumulated at one position to break down a furnace body, and the egg support structure can uniformly distribute loads.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of metal smelting, in particular to a molten steel anti-penetration tray in the field of powder high-temperature alloys. Background Art

[0002] During the smelting process of high-temperature alloys, cracks will form and expand in the melting crucible as the number of smelting times increases. Larger gaps will cause the molten steel to penetrate from the cracks to the outside of the smelting coil, causing a large amount of penetrated molten steel to leak from the melting crucible into the melting chamber, causing the furnace body to break down. The molten steel tray is a key protective device used to receive the leaked molten steel from the crucible, preventing the molten steel leaking from the leaking crucible from breaking down and exploding the melting chamber. It has become an indispensable on-site item in the high-temperature alloy smelting process. It is usually located at the bottom of the furnace to collect leaked molten metal steel and ensure equipment safety.

[0003] At present, most of the methods used are to lay a layer of fused magnesia on the steel receiving tray to suppress the flow of leaked molten steel in the steel receiving tray. However, during the vacuuming process, the fused magnesia collides with each other for a long time and adsorbs metal oxide dust on the surface, which is difficult to clean. These dusts are brought into the furnace body with the vacuum airflow, causing pollution of the purity of the molten steel and inclusion of alloy powder. At the same time, the molten steel flows into the melting chamber, which will cause the furnace body to break down and damage the melting chamber. Therefore, a molten steel anti-penetration tray in the field of powder high-temperature alloys is proposed. Utility Model Content

[0004] 1. Technical issues to be solved

[0005] In view of the deficiencies in the prior art, the utility model provides a steel liquid anti-penetration tray in the field of powder high-temperature alloys, which has the advantages of good anti-penetration effect of the tray and solves the problem of poor anti-penetration effect of the tray.

[0006] (II) Technical solution

[0007] In order to achieve the purpose of good anti-penetration effect of the above-mentioned pallet, the utility model provides the following technical solutions:

[0008] A steel liquid anti-penetration tray in the field of powder high-temperature alloys, comprising an anti-penetration tray body, the anti-penetration tray body being provided with a groove, a transverse clamping structure being provided on the side walls of two transversely adjacent anti-penetration tray bodies for transversely fixing the two adjacent anti-penetration tray bodies, and a longitudinal clamping structure being provided on the side walls of two longitudinally adjacent anti-penetration tray bodies for longitudinally fixing the two adjacent anti-penetration tray bodies.

[0009] As a preferred technical solution of the utility model, the groove is eggshell-shaped, and no less than three grooves are provided on the anti-penetration tray body, and a threaded groove is provided inside each groove.

[0010] As a preferred technical solution of the utility model, the transverse clamping structure includes a longitudinal clamping strip and a longitudinal clamping groove opened on the opposite side walls of the anti-penetration tray body, wherein the longitudinal clamping strip on the side wall of one anti-penetration tray body is clamped with the longitudinal clamping groove on the adjacent anti-penetration tray body.

[0011] As a preferred technical solution of the utility model, the longitudinal clamping structure includes a transverse clamping strip and a transverse clamping groove opened on the opposite side walls of the anti-penetration tray body, wherein the transverse clamping strip on the side wall of one anti-penetration tray body is clamped with the transverse clamping groove on the adjacent anti-penetration tray body.

[0012] As a preferred technical solution of the utility model, the upper surface of the anti-penetration tray body is provided with an inclined surface.

[0013] As a preferred technical solution of the utility model, the lowest point of the inclined surface is close to the top of the groove.

[0014] (III) Beneficial effects

[0015] Compared with the prior art, the utility model provides a steel liquid anti-penetration tray in the field of powder high-temperature alloys, which has the following beneficial effects:

[0016] The steel liquid anti-penetration tray in the field of powder high-temperature alloy can evenly distribute the steel liquid leaked from the crucible on the entire surface of the steel receiving tray through the design of the egg-tray type steel receiving tray, so that the tray can prevent the steel liquid leaked from the crucible from flowing unevenly and clogging the steel receiving tray. At the same time, the steel liquid leaked from the crucible can generate eddy currents through these curved grooves, further increasing the flow rate of the steel liquid leaked from the crucible, preventing the steel liquid leaked from the crucible from accumulating in one place and penetrating the furnace body. The egg-tray structure can evenly distribute the load. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a three-dimensional structural schematic diagram of the utility model;

[0018] Figure 2 This is a schematic diagram of a three-dimensional side view of a single anti-penetration tray body of the utility model;

[0019] Figure 3 This is a schematic diagram of the three-dimensional structure of a single anti-penetration tray body of the utility model;

[0020] Figure 4 This is a schematic diagram of the three-dimensional structure of a single anti-penetration tray body of the utility model;

[0021] Figure 5 It is a schematic diagram of the three-dimensional structure of a single groove of the utility model.

[0022] In the figure: 1. Anti-penetration tray body; 2. Groove; 3. Horizontal slot; 4. Longitudinal strip; 5. Inclined surface; 6. Horizontal strip; 7. Longitudinal slot; 8. Threaded groove. DETAILED DESCRIPTION

[0023] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0024] In the description of the present invention, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.

[0025] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0026] See also Figure 1-5, a steel liquid anti-penetration tray in the field of powder high-temperature alloys, comprising an anti-penetration tray body 1, a groove 2 is provided on the anti-penetration tray body 1, a threaded groove 8 is provided on the inner wall of the groove 2, wherein the groove 2 is an eggshell-shaped shape, and the anti-penetration tray body 1 is provided with not less than three grooves 2, each groove 2 is provided with a threaded groove 8 inside, wherein the threaded groove 8 is annularly provided inside the groove 2 from top to bottom, and a plurality of equidistant egg-tray-shaped grooves 2 are adjacently provided to form a continuous whole, a plurality of equidistantly arranged threaded grooves 8 accelerate the fluidity of the steel liquid leaked from the crucible, and can make the steel liquid leaked from the crucible evenly distributed on the inner wall of the entire groove, at the same time, a plurality of small pieces are spliced ​​and placed to provide a large span of space coverage, reducing the probability of the steel liquid flowing to the smelting chamber and causing the furnace body to break through, a transverse clamping structure is provided on the side walls of two transversely adjacent anti-penetration tray bodies 1, for transversely fixing the two adjacent anti-penetration tray bodies 1, wherein the transverse clamping structure includes a longitudinal clamping strip 4 and a longitudinal clamping groove 7 provided on the opposite side walls of the anti-penetration tray body 1 , a longitudinal clamping strip 4 on the side wall of one anti-penetration tray body 1 is clamped with a longitudinal clamping groove 7 on an adjacent anti-penetration tray body 1, so that the two transversely adjacent anti-penetration tray bodies 1 can be quickly assembled together by clamping the longitudinal clamping strip 4 and the longitudinal clamping groove 7, thereby improving the operating efficiency, and at the same time reducing the gap between the two adjacent anti-penetration tray bodies 1, making the connection more complete, and reducing the probability of molten steel leaking from the crucible falling into the smelting chamber. A longitudinal clamping structure is provided on the side walls of the two longitudinally adjacent anti-penetration tray bodies 1 for longitudinally fixing the two adjacent anti-penetration tray bodies 1, and the longitudinal clamping structure includes a transverse clamping strip 6 and a transverse clamping groove 3 provided on the opposite side walls of the anti-penetration tray body 1, and a transverse clamping strip 6 on the side wall of one anti-penetration tray body 1 is clamped with a transverse clamping groove 3 on an adjacent anti-penetration tray body 1, so that the two longitudinally adjacent anti-penetration tray bodies 1 can be quickly assembled together by clamping the transverse clamping strip 6 and the transverse clamping groove 3, thereby achieving a quick assembly effect.

[0027] In the present embodiment, the egg-tray structure of the anti-penetration tray body is a plurality of eggshell-shaped grooves 2 with threaded grooves 8 therein, so that the molten steel drops into the threaded grooves 8 inside the grooves 2, and can flow down quickly while forming eddies in each groove 2, which is not easy to cause the grooves 2 to be blocked. At the same time, it can be quickly replaced and assembled. When one of the pieces is damaged, only the damaged part needs to be replaced without replacing the entire anti-penetration tray body, thereby improving the practicality and flexibility of the tray.

[0028] In this embodiment, the anti-penetration tray body 1 is made of an aluminum oxide material, which has the advantages of heat resistance and a small thermal expansion coefficient.

[0029] In this embodiment, a slope 5 is provided on the upper surface of the anti-penetration tray body 1, wherein the lowest point of the slope 5 is close to the top of the groove 2, so that the molten steel falling to the edge of the anti-penetration tray body 1 can flow back into the groove 2 through the slope 5.

[0030] Working principle: by sliding up and down, the longitudinal card strip 4 and the longitudinal card slot 7 are engaged with each other, so that the two transversely adjacent anti-penetration tray bodies 1 can be assembled together by sliding up and down, and by sliding left and right, the transverse card strip 6 and the transverse card slot 3 are engaged with each other, so that the two longitudinally adjacent anti-penetration tray bodies 1 can be assembled together by sliding left and right, so as to achieve the effect of facilitating bottle loading. Through the eggshell-shaped groove 2 and the threaded groove 8 opened inside the groove 2, the molten steel can flow down quickly and form eddies in each groove 2, which is not easy to cause the groove 2 to be blocked. Multiple equidistant curved grooves 2 accelerate the fluidity of the molten steel and can make the molten steel evenly distributed on the entire tray body. At the same time, multiple small pieces are spliced ​​and placed to provide a large span of space coverage, which reduces the probability of the molten steel flowing into the melting chamber and causing the furnace body to be pierced.

[0031] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A steel liquid anti-penetration tray in the field of powder high temperature alloy, comprising an anti-penetration tray body (1), characterized in that: A groove (2) is provided on the anti-penetration tray body (1); a transverse clamping structure is provided on the side walls of two transversely adjacent anti-penetration tray bodies (1) for transversely fixing the two adjacent anti-penetration tray bodies (1); and a longitudinal clamping structure is provided on the side walls of two longitudinally adjacent anti-penetration tray bodies (1) for longitudinally fixing the two adjacent anti-penetration tray bodies (1).

2. The anti-penetration tray for liquid steel in the field of powder high-temperature alloy according to claim 1, characterized in that: The groove (2) is eggshell-shaped, and the anti-penetration tray body (1) is provided with no less than three grooves (2), each groove (2) having a thread groove (8) formed inside.

3. The anti-penetration tray for liquid steel in the field of powder high-temperature alloy according to claim 1, characterized in that: The transverse clamping structure comprises a longitudinal clamping strip (4) and a longitudinal clamping groove (7) provided on opposite side walls of the anti-penetration tray body (1), wherein the longitudinal clamping strip (4) on the side wall of one anti-penetration tray body (1) is clamped with the longitudinal clamping groove (7) on the adjacent anti-penetration tray body (1).

4. The anti-penetration tray for molten steel in the field of powder high-temperature alloy according to claim 1, characterized in that: The longitudinal clamping structure comprises a transverse clamping strip (6) and a transverse clamping groove (3) provided on opposite side walls of the anti-penetration tray body (1), wherein the transverse clamping strip (6) on the side wall of one anti-penetration tray body (1) is clamped with the transverse clamping groove (3) on the adjacent anti-penetration tray body (1).

5. The anti-penetration tray for liquid steel in the field of powder high-temperature alloy according to claim 1, characterized in that: The upper surface of the anti-penetration tray body (1) is provided with an inclined surface (5).

6. The anti-penetration tray for molten steel in the field of powder high-temperature alloy according to claim 5, characterized in that: The lowest point of the inclined surface (5) is close to the top of the groove (2).