Alloy roller with high-temperature-corrosion-resistant surface

By arranging convex structures and connecting structures on the surface of the alloy roller, the molten droplets are promoted to thicken from both sides to the middle during the cladding process, forming a metallurgical bond, which solves the problem of insufficient interlayer bonding ability of the existing alloy rollers and improves its High temperature corrosion resistance and impact resistance.

CN221817014UActive Publication Date: 2024-10-11马鞍山市恒泰重工机械有限公司
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202323179534.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-11-24
Publication Date
2024-10-11
Estimated Expiration
2033-11-24

AI Technical Summary

Technical Problem

Existing alloy rollers have layered wave spreading morphology or 'cavity' characteristics during the cladding process, resulting in poor inter-layer bonding ability and affecting its high-temperature corrosion resistance and impact resistance.

Method used

The convex structure is used in conjunction with the connecting structure. By arranging the connecting structure and the convex structure on the surface of the roller body, the molten droplets gradually thicken from both sides to the middle during the cladding process, forming temperature distribution characteristics and promoting subsequent deposition of molten droplets. Metallurgically bonded with the previous layer to improve the bonding strength between layers.

Benefits of technology

It effectively increases the interlayer bonding strength of the alloy roller, improves high temperature corrosion resistance and impact resistance, and avoids the problem of insufficient bonding ability caused by the layered wave spreading morphology and 'cavity' characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221817014U_ABST
    Figure CN221817014U_ABST
Patent Text Reader

Abstract

The surface high-temperature-corrosion-resistant alloy roller comprises a roller body and a high-temperature-corrosion-resistant metal composite layer, a connecting structure is arranged on the roller body in the circumferential direction, and protruding structures are arranged on the two sides of the connecting structure. The protruding structures are matched with the connecting structures to gradually thicken the molten drops from the two sides to the middle in the cladding process, the number of the spread molten drops at the protruding positions of the edges of the connecting structures is small, the thickness is small, heat carried by the molten drops in the area is limited, and compared with a thick area in the middle, the molten drops can be rapidly cooled within a short time. The central strip-shaped area on the upper portion of the inner side of the molten drop is separated from the cold base body through the molten drop belt which is cooled in advance, the molten drop belt which is cooled in advance is equivalent to a hot base body and has a heat insulation function, and therefore the strip-shaped area is kept at the highest temperature all the time. In the cladding process, the temperature distribution characteristic is beneficial to forming metallurgical bonding of subsequently deposited molten drops and previous deposited molten drops at the local position of the surface layer, so that the interlayer bonding strength is fully improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of alloy rollers, in particular to an alloy roller with a surface resistant to high temperature corrosion. Background Art

[0002] Existing steel rolling rollers at home and abroad are all made of cast iron. Due to their frequent use, generally after more than a week of use, the roller surface will be worn out by the steel, affecting the transmission and causing scratches, pits and other quality problems on the product surface. The rollers must be replaced in time, and the steel tapping temperature is high and the rollers need to adapt to a wider temperature range, and also need to have corrosion resistance, high temperature resistance, impact resistance and other properties.

[0003] Most of the existing alloy rollers have a layer of cemented carbide clad on the surface. The traditional process is to perform sandblasting or spiral roughening on the surface before cladding, but simple sandblasting or spiral roughening cannot ensure the interlayer bonding strength. After the spiral roughening treatment, a roughening groove is formed. During the cladding, the molten droplets will allow more molten droplets to spread to the plane area outside the roughening groove. In the process of the molten droplets spreading outward, the part of the molten droplets closest to the substrate solidifies first. Under the action of the temperature gradient, some molten particles above the center area of ​​the solidified molten droplets will continue to spread outward on the solidified layer. However, as the cooling continues, the spreading speed of the upper molten droplets decreases. At the same time, due to the barrier effect of the previously solidified molten droplets, the spreading distance of the upper molten droplets decreases, thus forming a layered wave spreading morphology. The pit structure caused by sandblasting has the worst heat dissipation capacity. This is because the deeper pit structure limits the spread of the molten droplets, forming a thicker spread shape, reducing its contact area with the substrate. At the same time, as the molten droplets close to the inner wall of the pit solidify, a layer of "hot matrix" protection will be formed on the internal unsolidified area. The interaction between the two makes it more difficult for the molten droplets in the pit structure to introduce heat into the substrate in time to cool down. The core area wrapped by the first solidified layer is in an unsolidified state, and the molten droplets in the pit structure form a unique "cavity" feature in the bottom area. The existing methods have layered wavy spreading morphology or "cavity" characteristics during cladding, so its interlayer bonding ability needs to be further improved. Utility Model Content

[0004] The technical problem to be solved by the utility model is: how to improve the interlayer bonding ability of the existing alloy roller and the surface metal hard alloy composite layer.

[0005] In order to solve the above technical problems, the utility model has obtained the technical solution of the utility model through practice and summary. The utility model adopts the following technical solution:

[0006] A surface high temperature corrosion resistant alloy roller comprises a roller body and a high temperature corrosion resistant metal composite layer. A connecting structure is circumferentially arranged on the roller body, and convex structures are arranged on both sides of the connecting structure.

[0007] Through the convex structure and the connection structure, the molten droplets are gradually thickened from the two sides to the middle during the cladding process. At the convex position of the edge of the connection structure, the spread molten droplets are less and thinner, so that the heat carried by the molten droplets in this area is limited. Compared with the thicker area in the middle, it can be quickly cooled down in a short time. The central strip area on the upper inner side of the molten droplet is separated from the cold matrix by the molten droplet belt that has been cooled in advance. The molten droplet belt that has been cooled in advance is equivalent to a "hot matrix" and has a heat-insulating effect, so that the strip area always maintains the highest temperature. During the cladding process, this temperature distribution feature is conducive to the metallurgical bonding of the subsequently deposited molten droplets with the previous layer of deposited molten droplets at a local position on the surface, thereby fully improving the interlayer bonding strength.

[0008] In a preferred solution, the connection structure is a reticulated groove, both sides of the reticulated groove are provided with protrusions, and the reticulated groove and the protrusions are suitable for the combination of the roller surface and the high temperature corrosion resistant metal composite layer.

[0009] In a preferred embodiment, the anilox grooves include a plurality of annular grooves and a plurality of sinusoidal linear grooves, the plurality of sinusoidal linear grooves are uniformly distributed circumferentially on the outer peripheral surface of the roller body, and the plurality of annular grooves are uniformly distributed axially on the outer peripheral surface of the roller body.

[0010] In a preferred embodiment, the anilox grooves include two spiral grooves with opposite rotation directions, and linear grooves are circumferentially arranged in the area surrounded by the spiral grooves.

[0011] In a preferred embodiment, the anvil grooves include a plurality of equally spaced annular grooves 1 and 2, the annular grooves 1 and 2 are arranged alternately, and the annular grooves 2 are annular grooves with sinusoidal paths.

[0012] Preferably, the connection structure is a spiral groove, which is a single spiral groove or a double spiral groove. The double spiral groove is two spiral grooves with opposite spiral structures. The connection point of the two spiral grooves is located in the middle of the roller body and takes the middle of the roller body as the starting point.

[0013] In a preferred embodiment, the connection structure is a V-shaped groove evenly distributed on the surface of the roller body, and the V-shaped groove is in the middle of the roller body.

[0014] In a preferred embodiment, the high temperature corrosion resistant metal composite layer is provided with a thermal barrier alloy layer and a corrosion resistant working layer in sequence from the inside to the outside.

[0015] In a preferred solution, the outer peripheral surface of the roller body is gradually recessed from both ends to the middle, and the outer peripheral surface of the corrosion-resistant working layer is a cylindrical surface.

[0016] In a preferred embodiment, the connecting surface between the thermal barrier alloy layer and the corrosion-resistant working layer is a cylindrical surface and the thickness of the corrosion-resistant working layer is consistent.

[0017] Compared with the prior art, the utility model has the following beneficial effects:

[0018] The utility model adopts the cooperation of the protruding structure and the connecting structure. Through the cooperation of the protruding structure and the connecting structure, the molten droplets are gradually thickened from the two sides to the middle during the cladding process. At the protruding position of the edge of the connecting structure, the amount of spread molten droplets is small and the thickness is thin, so that the heat carried by the molten droplets in this area is limited. Compared with the thicker area in the middle, it can be quickly cooled in a short time. The central strip area on the upper inner side of the molten droplet is separated from the cold matrix by the molten droplet belt that has been cooled in advance. The molten droplet belt that has been cooled in advance is equivalent to a "hot matrix" and has a heat-insulating effect, so that the strip area always maintains the highest temperature. During the cladding process, this temperature distribution feature is conducive to the subsequent deposited molten droplets and the previous layer of deposited molten droplets to form a metallurgical bond at a local position on the surface, thereby fully improving the interlayer bonding strength. It effectively solves the problem that the existing means (spiral roughening or sandblasting) have a layered wave spreading morphology or "cavity" characteristics during cladding, resulting in poor interlayer bonding ability. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the overall structure of the utility model;

[0020] Figure 2 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0021] Figure 3 for Figure 2 A partial enlarged view of the middle A;

[0022] Figure 4 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0023] Figure 5 for Figure 4 A partial enlarged view of point B in the middle;

[0024] Figure 6 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0025] Figure 7 for Figure 6 A partial enlarged view of point C in the middle;

[0026] Figure 8 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0027] Fig. 9 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0028] Fig.10 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0029] Fig.11 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0030] Fig.12 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0031] Fig.13 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0032] Fig.14 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0033] Fig.15 A schematic diagram of a roller structure according to an embodiment of the present invention;

[0034] Fig.16 It is a cross-sectional view of the overall structure of the utility model.

[0035] In the figure: roller body 1; high temperature corrosion resistant metal composite layer 2; connecting structure 3; protruding structure 4; corrosion resistant working layer 21; thermal barrier alloy layer 22. DETAILED DESCRIPTION

[0036] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.

[0037] In the description of the present invention, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.

[0038] An embodiment of the present invention is a surface high temperature corrosion resistant alloy roller, comprising a roller body 1 and a high temperature corrosion resistant metal composite layer 2, wherein a connecting structure 3 is circumferentially arranged on the roller body 1, and protruding structures 4 are arranged on both sides of the connecting structure 3.

[0039] The molten droplets are gradually thickened from both sides to the middle during the cladding process through the raised structure 4 and the connecting structure 3. At the raised position on the edge of the connecting structure 3, the spread molten droplets are less and thinner, so that the heat carried by the molten droplets in this area is limited. Compared with the thicker area in the middle, it can be cooled down rapidly in a short time. The central strip area on the upper inner side of the molten droplet is separated from the cold matrix by the molten droplet belt that has been cooled down in advance. The molten droplet belt that has been cooled down in advance is equivalent to a "hot matrix" and has a heat-insulating effect, so that the strip area always maintains the highest temperature. During the cladding process, this temperature distribution feature is conducive to the subsequent deposited molten droplets to form a metallurgical bond with the previous layer of deposited molten droplets at a local position on the surface, thereby fully improving the interlayer bonding strength.

[0040] On the basis of the above embodiment, the following improvements are made: the connection structure 3 is a mesh groove, and a protrusion structure 4 is provided on both sides of the groove of the mesh groove. The mesh groove and the protrusion structure 4 are suitable for the combination of the roller body 1 surface and the high temperature corrosion resistant metal composite layer 2. The mesh groove and the protrusion structure 4 ensure the interlayer bonding ability, and also make the high temperature corrosion resistant metal composite layer 2 and the roller body 1 have a tendency to move sideways. When the alloy roller is in working condition, the high temperature corrosion resistant metal composite layer 2 on the outside exerts pressure on the steel material, resulting in the alloy layer structure having a tendency to move to both sides, that is, the pressure on both sides is converted into the structural stress inside the high temperature corrosion resistant metal composite layer 2 through the mesh groove and the protrusion structure 4. Since the high temperature corrosion resistant metal composite layer 2 is made of high strength alloy material, it can fully accommodate the structural stress inside it without structural damage, and at the same time, the separation and shedding phenomenon of the roller body and the high temperature corrosion resistant metal composite layer 2 can be eliminated.

[0041] The following are examples of different structural arrangements:

[0042] One situation: the anilox grooves include a plurality of annular grooves and a plurality of sinusoidal linear grooves, the plurality of sinusoidal linear grooves are evenly distributed circumferentially on the outer peripheral surface of the roller body 1, and the plurality of annular grooves are evenly distributed axially on the outer peripheral surface of the roller body 1. Since the sinusoidal linear grooves face the steel material to be rolled, the impact resistance of the alloy roller can be improved.

[0043] In another case, the mesh grooves include two spiral grooves with opposite rotation directions, and linear grooves are arranged circumferentially in the area surrounded by the spiral grooves. The middle linear groove structure can improve the interlayer bonding strength in several small areas separated by the mesh.

[0044] In another case, the anvil grooves include a plurality of equally spaced annular grooves 1 and 2, which are arranged alternately, and the annular grooves 2 are annular grooves with sinusoidal paths, and are arranged in a forward direction to prevent the delamination trend toward both ends and reduce the impact strength between layers.

[0045] In another case, the mesh grooves are V-shaped grooves 1 and 2 evenly distributed on the surface of the roller body 1, and the V-shaped grooves 1 and 2 are arranged in opposite directions. The two V-shaped grooves are arranged in opposite directions to form a mesh structure, so that when it is subjected to the impact of the steel, there will be an opposite resistance, which is then converted into internal stress of the structure and digested in the high temperature corrosion resistant metal composite layer 2.

[0046] Based on the above embodiment, the following improvements are made: the connection structure 3 is a spiral groove, the spiral groove is a single spiral groove or a double spiral groove, the double spiral groove is two spiral grooves with opposite spiral structures, the connection point of the two spiral grooves is located in the middle of the roller body 1, and the middle of the roller body 1 is used as the starting point. The impact resistance can also be improved.

[0047] Based on the above embodiment, the following improvement is made: the high temperature corrosion resistant metal composite layer 2 is provided with a thermal barrier alloy layer 22 and a corrosion resistant working layer 21 in sequence from the inside to the outside.

[0048] The outer circumference of the roller body 1 is gradually concave from both ends to the middle, and the outer circumference of the corrosion-resistant working layer 21 is a cylindrical surface.

[0049] The connecting surface between the thermal barrier alloy layer 22 and the corrosion-resistant working layer 21 is a cylindrical surface and the thickness of the corrosion-resistant working layer 21 is consistent.

[0050] Since the middle of the roller body 1 contacts the steel for a long time, the middle part thereof can obtain an effective thermal barrier effect, which is more conducive to the stability of the middle structure and can also enhance the interlayer separation barrier of the structure.

[0051] The above is only a preferred specific implementation of the utility model, but the protection scope of the utility model is not limited to this. The replacement can be a replacement of part of the structure, device, method step, or a complete technical solution. Equivalent replacement or change based on the technical solution of the utility model and its utility model concept should be included in the protection scope of the utility model.

Claims

1. A surface high temperature corrosion resistant alloy roller, characterized in that: It comprises a roller body (1) and a high temperature corrosion resistant metal composite layer (2), wherein a connecting structure (3) is circumferentially arranged on the roller body (1), and protruding structures (4) are arranged on both sides of the connecting structure (3).

2. The surface high temperature corrosion resistant alloy roller according to claim 1, characterized in that: The connection structure (3) is a reticulated groove, and protrusions are arranged on both sides of the groove. The reticulated groove and the protrusions are suitable for combining the surface of the roller body (1) and the high temperature corrosion resistant metal composite layer (2).

3. The surface high temperature corrosion resistant alloy roller according to claim 2, characterized in that: The anilox grooves include a plurality of annular grooves and a plurality of sinusoidal linear grooves, the plurality of sinusoidal linear grooves are evenly distributed circumferentially on the outer peripheral surface of the roller body (1), and the plurality of annular grooves are evenly distributed axially on the outer peripheral surface of the roller body (1).

4. The surface high temperature corrosion resistant alloy roller according to claim 2, characterized in that: The reticulated grooves include two spiral grooves with opposite rotation directions, and linear grooves are arranged circumferentially in the area surrounded by the spiral grooves.

5. The surface high temperature corrosion resistant alloy roller according to claim 2, characterized in that: The anvil grooves include a plurality of annular grooves 1 and 2 distributed at equal intervals, the annular grooves 1 and 2 are arranged alternately, and the annular grooves 2 are annular grooves with sinusoidal paths.

6. The surface high temperature corrosion resistant alloy roller according to claim 1, characterized in that: The connection structure (3) is a spiral groove, which is a single spiral groove or a double spiral groove. The double spiral groove is two spiral grooves with opposite spiral structures. The connection point of the two spiral grooves is located in the middle of the roller body (1), and the middle of the roller body (1) is used as the starting point.

7. The surface high temperature corrosion resistant alloy roller according to claim 1, characterized in that: The connection structure (3) is a V-shaped groove evenly distributed on the surface of the roller body (1), and the V-shaped groove is in the middle of the roller body (1).

8. The surface high temperature corrosion resistant alloy roller according to claim 1, characterized in that: The high temperature corrosion resistant metal composite layer (2) is provided with a thermal barrier alloy layer (22) and a corrosion resistant working layer (21) in sequence from the inside to the outside.

9. The surface high temperature corrosion resistant alloy roller according to claim 8, characterized in that: The outer peripheral surface of the roller body (1) is gradually concave from both ends to the middle, and the outer peripheral surface of the corrosion-resistant working layer (21) is a cylindrical surface.

10. The surface high temperature corrosion resistant alloy roller according to claim 9, characterized in that: The connecting surface between the thermal barrier alloy layer (22) and the corrosion-resistant working layer (21) is a cylindrical surface, and the thickness of the corrosion-resistant working layer (21) is consistent.

Citation Information

Cited By

  • Antioxidant and wear-resistant composite coating on surface of alloy roller and manufacturing process

    CN117926162A

  • Antioxidant and wear-resistant composite coating and manufacturing process of alloy roller surface

    CN117926162B