Supercharger output pin with good wear resistance

By using a combination of alloy steel materials, chromium elements and quenching layers, the wear resistance and fatigue resistance of the supercharger output pin are enhanced, solving the problem of insufficient wear resistance in the existing technology and extending the service life of the equipment.

CN221823914UActive Publication Date: 2024-10-11JIUBANG TRANSMISSION TECH (SUZHOU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323420924.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-15
Publication Date
2024-10-11
Estimated Expiration
2033-12-15

AI Technical Summary

Technical Problem

The existing supercharger output pin has insufficient wear resistance, which limits the service life and performance of the supercharger.

Method used

A supercharger output pin including a three-section shaft body is designed. It is made of alloy steel with chromium elements added to it. It is combined with a quenching layer and a carbide coating. The width of the shaft body is gradually reduced, and keyways are set at specific positions to strengthen it. Connection stability.

Benefits of technology

It significantly improves the wear resistance, fatigue strength and corrosion resistance of the supercharger, prolongs the service life of the equipment, and ensures its wear resistance and service life by controlling the coating thickness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221823914U_ABST
    Figure CN221823914U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of automobile turbocharging, and discloses a supercharger output pin with good wear resistance, which comprises three sections of shaft bodies. According to the supercharger output pin with the good wear resistance, the interior of the three-section shaft body and the interior of the external shaft body are made of alloy steel, meanwhile, the chromium element is added into the alloy steel, and therefore the hardness and the tensile strength of the alloy steel can be improved, and the wear resistance of the alloy steel is greatly enhanced; the surface hardness and wear resistance are improved, meanwhile, the fatigue resistance and corrosion resistance can be improved, then a layer of hard alloy with the thickness of 2-4 microns covers the outer portion of the quenching layer, so that a coating is formed, and the coating of the hard alloy has high hardness and high wear resistance and can effectively resist wear and friction; and meanwhile, the thickness of the coating is controlled to be 2-4 microns, so that the wear resistance and the service life of the coating can be ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of automobile turbocharging, in particular to a turbocharger output pin with good wear resistance. Background Art

[0002] With the continuous development of industrial technology, superchargers have been widely used in many fields.

[0003] The supercharger output pin is a key component in the supercharger, and its wear resistance has an important influence on the performance and life of the supercharger. However, the existing supercharger output pins often have the problem of insufficient wear resistance, which limits the service life and performance of the supercharger. Therefore, a supercharger output pin with good wear resistance is proposed to solve the above-mentioned problem. Utility Model Content

[0004] 1. Technical issues to be solved

[0005] In view of the deficiencies in the prior art, the utility model provides a supercharger output pin with good wear resistance, which has the advantages of good wear resistance, etc., and solves the problem that the existing supercharger output pin often has insufficient wear resistance.

[0006] (II) Technical solution

[0007] In order to achieve the above purpose, the utility model provides the following technical solutions:

[0008] A supercharger output pin with good wear resistance comprises three shaft bodies, namely a first shaft body, a second shaft body and a third shaft body, one end of the first shaft body is fixedly connected to one end of the second shaft body, and the other end of the second shaft body is fixedly connected to one end of the third shaft body;

[0009] The shaft widths of the first shaft section, the second shaft section and the third shaft section decrease in sequence and the decreasing values ​​are equal.

[0010] As a preferred technical solution of the utility model, the first section shaft body is fixedly connected to an external shaft body on the outside, and a first keyway is fixedly connected to one side of the external shaft body.

[0011] As a preferred technical solution of the utility model, an inner groove is provided in the middle of the second section of the shaft body, and a second key groove is provided on the same side of the first key groove of the third section of the shaft body.

[0012] As a preferred technical solution of the present utility model, the external shaft body and the internal materials of the three-section shaft body are alloy steel, and chromium element is added to the alloy steel.

[0013] As a preferred technical solution of the utility model, the surfaces of the external shaft body and the three-section shaft body are provided with a quenching layer, and the surface of the quenching layer is provided with a coating.

[0014] As a preferred technical solution of the present invention, the coating material is cemented carbide, and the thickness of the coating is 2-4 microns.

[0015] (III) Beneficial effects

[0016] Compared with the prior art, the utility model provides a supercharger output pin with good wear resistance, which has the following beneficial effects:

[0017] The supercharger output pin with good wear resistance is prepared by setting the internal material of the three-section shaft body and the external shaft body to alloy steel and adding chromium element into the alloy steel, which not only improves the hardness and tensile strength of the alloy steel, but also greatly enhances its wear resistance. The three-section shaft body and the external shaft body are quenched in the quenching layer to improve the hardness and wear resistance of the surface, and also improve the fatigue strength and corrosion resistance. The quenching layer is then covered with a layer of cemented carbide with a thickness of 2-4 microns to form a coating. The cemented carbide coating has high hardness and high wear resistance, can effectively resist wear and friction, and thus prolong the service life of the supercharger. At the same time, the thickness of the coating is controlled at 2-4 microns, which can ensure the wear resistance and service life of the coating. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the structure of the utility model;

[0019] Figure 2 This is the appearance diagram of the utility model.

[0020] In the figure: 1, the first section of the shaft; 2, the second section of the shaft; 3, the third section of the shaft; 4, the external shaft; 5, the first keyway; 6, the second keyway; 7, the quenching layer; 8, the coating. DETAILED DESCRIPTION

[0021] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0022] In the description of the present invention, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.

[0023] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0024] See also Figure 1-2 A supercharger output pin with good wear resistance comprises three shaft bodies, namely a first shaft body 1, a second shaft body 2 and a third shaft body 3, one end of the first shaft body 1 is fixedly connected to one end of the second shaft body 2, and the other end of the second shaft body 2 is fixedly connected to one end of the third shaft body 3;

[0025] The shaft widths of the first shaft section 1, the second shaft section 2 and the third shaft section 3 decrease in sequence and the decreasing values ​​are equal.

[0026] In this embodiment, the first section shaft body 1 is fixedly connected to an external shaft body 4 , and one side of the external shaft body 4 is fixedly connected to a first key groove 5 .

[0027] It should be noted that the first keyway 5 is used to install a key and then be fixedly connected to the turbine, and the first section of the shaft body 1 is located outside at both ends of the circumscribed shaft body 4 for installing bearings.

[0028] In this embodiment, an inner groove is provided in the middle of the second section shaft body 2 , and a second key groove 6 is provided on the same side of the first key groove 5 in the third section shaft body 3 .

[0029] It should be noted that the inner groove is used to be fixedly connected to the external fixing device, and the second keyway 6 is used to be fixedly connected to the air pipe in the engine.

[0030] In this embodiment, the external shaft body 4 and the internal materials of the three-section shaft body are alloy steel, and chromium elements are added to the alloy steel.

[0031] It should be noted that adding chromium element into the alloy steel can not only improve the hardness and tensile strength of the alloy steel, but also greatly enhance the wear resistance of the external shaft body 4 and the three-section shaft body.

[0032] In this embodiment, a quenching layer 7 is provided on the surface of the circumscribed shaft body 4 and the three-section shaft body, and a coating 8 is provided on the surface of the quenching layer 7 .

[0033] It should be noted that quenching the quenching layer 7 can improve the hardness and wear resistance of the surface of the external shaft body 4 and the three-section shaft body, and can also improve their fatigue strength and corrosion resistance.

[0034] In this embodiment, the coating 8 is made of cemented carbide, and the thickness of the coating 8 is 2-4 microns.

[0035] It should be noted that the cemented carbide coating 8 has high hardness and high wear resistance, and can effectively resist wear and friction, thereby extending the service life of the supercharger. At the same time, the thickness of the coating 8 is controlled at 2-4 microns, which can ensure the wear resistance and service life of the coating.

[0036] Beneficial effects: The supercharger output pin with good wear resistance is achieved by setting the internal material of the three-section shaft body and the external shaft body 4 to alloy steel and adding chromium elements to the alloy steel, which not only improves the hardness and tensile strength of the alloy steel, but also greatly enhances its wear resistance. The quenching layer 7 of the three-section shaft body and the external shaft body 4 is quenched to improve the hardness and wear resistance of its surface, and also improves its fatigue strength and corrosion resistance. The quenching layer 7 is then covered with a layer of cemented carbide with a thickness of 2-4 microns to form a coating 8. The cemented carbide coating 8 has high hardness and high wear resistance, can effectively resist wear and friction, and thus extend the service life of the supercharger. At the same time, the thickness of the coating 8 is controlled at 2-4 microns, which can ensure the wear resistance and service life of the coating.

[0037] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A supercharger output pin with good wear resistance, comprising three shaft sections, namely a first shaft section (1), a second shaft section (2) and a third shaft section (3), wherein one end of the first shaft section (1) is fixedly connected to one end of the second shaft section (2), and the other end of the second shaft section (2) is fixedly connected to one end of the third shaft section (3); Features: The shaft widths of the first shaft section (1), the second shaft section (2) and the third shaft section (3) decrease in sequence and the decreasing values ​​are equal.

2. A supercharger output pin with good wear resistance according to claim 1, characterized in that: The first section of the shaft body (1) is fixedly connected to an external shaft body (4) on the outside, and a first keyway (5) is fixedly connected to one side of the external shaft body (4).

3. A supercharger output pin with good wear resistance according to claim 2, characterized in that: The second section of the shaft body (2) is provided with an inner groove in the middle, and the third section of the shaft body (3) is provided with a second key groove (6) on the same side as the first key groove (5).

4. A supercharger output pin with good wear resistance according to claim 2, characterized in that: The surfaces of the external shaft body (4) and the three-section shaft body are provided with a quenching layer (7), and the surface of the quenching layer (7) is provided with a coating (8).