Antioxidant emulsion preparation device

By designing an antioxidant emulsion preparation device that includes an AOE oil tank, an AOE emulsification tank, a KOH storage tank and a vacuum feeder, the problems of insufficient antioxidant properties and easy decomposition at high temperatures in the existing technology have been solved, and the application of HRG resin has been achieved. Highly efficient antioxidant performance and stability guarantee to meet the needs of industrial production.

CN221832160UActive Publication Date: 2024-10-15TIANJIN DAGU CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420228354.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-31
Publication Date
2024-10-15
Estimated Expiration
2034-01-31

AI Technical Summary

Technical Problem

The existing antioxidant emulsion device is not effective in improving the antioxidant properties of ABS resin, and it is easy to decompose at high temperatures, so it cannot meet the antioxidant performance requirements of HRG resin in industrial production.

Method used

An antioxidant emulsion preparation device is designed. Through the combination of AOE oil tank, AOE emulsification tank, KOH storage tank, ion-free water tank, vacuum feeder and AOE pump, low-pressure steam heating and stirring technology are used to synthesize higher Antioxidant emulsion for antioxidant effect, including the addition of thiodipropionic acid in the AOE carburetor tank Didodecanol ester, polymerized hindered phenol antioxidant and tallow fatty acid are heated and stirred with steam to form an oily liquid. KOH solution and deionized water are then added to the AOE emulsification tank for saponification reaction to form an emulsifier, and defoaming is added agent and xanthan gum, and finally complete the phase transformation through an emulsifier to form a highly efficient antioxidant emulsion.

Benefits of technology

It has achieved a significant improvement in the oxidation resistance of HRG resin, can maintain stability under high temperature conditions, meet the requirements for antioxidant performance in industrial production, avoid fire risks, and improve the sensitivity and accuracy of monitoring process parameters.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221832160U_ABST
    Figure CN221832160U_ABST
Patent Text Reader

Abstract

The utility model discloses an anti-oxidation emulsion preparation device, and belongs to the technical field of anti-oxidation emulsion preparation. The device is composed of an AOE oil melting tank, an AOE emulsifying tank, a KOH storage tank, an ion-free water tank, a vacuum charging machine and an AOE pump, the AOE oil melting tank is provided with an AOE oil melting tank jacket, an AOE oil melting tank stirrer and the like, the AOE oil melting tank jacket is provided with a steam inlet and a steam outlet, and raw materials are melted into oily liquid under the action of low-pressure steam; the AOE emulsifying tank is provided with an AOE emulsifying tank jacket, an AOE emulsifying tank stirrer, an emulsifier and the like; the AOE emulsifying tank jacket 8 is provided with a steam inlet and a steam outlet; under the action of low-pressure steam, the oily liquid, KOH, deionized water, a defoaming agent and xanthan gum are subjected to phase conversion in the AOE emulsification tank to form AOE emulsion, and then the AOE emulsion is conveyed to an ABS device from an outlet of the AOE emulsification tank through an AOE pump. The anti-oxidation emulsion prepared by the device is suitable for improving the oxidation resistance of ABS (Acrylonitrile Butadiene Styrene) resin.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of antioxidant emulsion (AOE) preparation, and specifically relates to an antioxidant emulsion (AOE) preparation device. The antioxidant emulsion (AOE) prepared by the device is suitable for improving the antioxidant property of ABS (butadiene-styrene-acrylonitrile polymer) resin. Background Art

[0002] With the increasing quality requirements for ABS resin in industrial production, it is necessary to reduce the water content of the raw material HRG (high rubber grafted powder) resin to improve the mechanical properties of ABS resin; and reducing the water content of HRG resin requires increasing the drying temperature, but increasing the drying temperature may cause HRG resin to be oxidized, thereby causing serious problems such as fire in the production process, so it is necessary to improve the antioxidant properties of HRG resin by improving the auxiliary antioxidant emulsion (AOE). However, the antioxidant effect of AOE produced by the commonly used equipment is general, resulting in insufficient antioxidant properties of HRG resin, easy decomposition at high temperature, and unable to meet production requirements. Therefore, it is necessary to design a set of antioxidant emulsion (AOE) preparation equipment on the ABS production equipment to prepare an AOE with better antioxidant effect to meet the requirements of HRG resin for antioxidant properties. Utility Model Content

[0003] The utility model aims to provide an antioxidant emulsion (AOE) preparation device.

[0004] As attached Figure 1As shown, an antioxidant emulsion preparation device is composed of an AOE oil tank 1, an AOE emulsification tank 2, a KOH storage tank 3, an ion-free water tank 4, a vacuum feeder 5 and an AOE pump 6. The AOE oil tank 1 is provided with an AOE oil tank jacket 7, an AOE oil tank stirrer 9 and an AOE oil tank thermometer 12. The top of the AOE oil tank 1 is provided with three inlets and the bottom is provided with an outlet; one inlet is added with 595-605 kg of didodecanol thiodipropionate (DLTDP), one inlet is added with 595-605 kg of polymerized hindered phenol antioxidant (CPL) through the vacuum feeder 5, and one inlet is added with a TFA flowmeter 14. 63-67 kg of tallow fatty acid (TFA) is added; the AOE oil tank jacket 7 is provided with a steam inlet and a steam outlet. Under the continuous heating of low-pressure steam (0.38-0.42 MPa, 180-220°C), the AOE oil tank thermometer 12 reads 74-78°C and then the AOE oil tank stirrer 9 is started to melt the solid raw material into an oily liquid. After stirring and reacting for 2-3 hours, the raw material is transported from the outlet to the AOE emulsification tank 2 through a pipeline; the AOE emulsification tank 2 is provided with an AOE emulsification tank jacket 8, an AOE emulsification tank stirrer 10, an emulsifier 11 and an AOE emulsification tank thermometer 13. The AOE emulsification tank jacket 8 is provided with A steam inlet and a steam outlet are provided; under the continuous heating of low-pressure steam (0.38-0.42MPa, 180-220°C), the reading of the AOE emulsification tank thermometer 13 rises to 63-67°C to complete the preheating of the AOE emulsification tank; the top of the AOE emulsification tank 2 is provided with four inlets and the bottom is provided with an outlet. The preheated AOE emulsification tank first receives the oily liquid from the AOE oil tank 1, and then starts the AOE emulsification tank stirring 10 to fully mix the liquid in the tank, and then adds 67-77kg of KOH solution with a mass concentration of 19-23%, and reacts with TFA to form an emulsifier, and stirs for 0 .4 to 0.6 hours later, start the emulsifier 11 and add 1000 to 1100 kg of ion-free water at 63 to 67° C. in the ion-free water tank 4 into the AOE emulsification tank 2, and complete the phase transition of the material from the oil phase to the water phase under the high-speed rotation of the emulsifier (the AOE emulsification tank stirring 10 and the emulsifier 11 can operate independently to ensure the smooth completion of the phase transition); finally, add 24 to 26 kg of defoaming agent (the main component is a mixture of dimethylsiloxane and other organic matter) and 1.5 to 2.5 kg of xanthan gum, stir for 0.5 to 1.5 hours to form an AOE emulsion, and then transport it to the ABS device from the outlet of the AOE emulsification tank 2 through the AOE pump 6.

[0005] The AOE oil tank 1 adopts an enamel inner wall and an enamel stirrer, which can effectively prevent materials from adhering to the inner wall and the stirrer of the AOE oil tank, reducing the cleaning frequency on the one hand and ensuring the heat exchange efficiency of the jacket steam on the other hand.

[0006] The AOE emulsification tank 2 has a stainless steel inner wall, is connected to the AOE oil tank 1, the KOH storage tank 3 and the deionized water tank 4 via pipelines at the top, and is connected to the AOE pump 6 via pipelines at the bottom.

[0007] The KOH solution is stored in a KOH storage tank 3, which has a stainless steel inner wall and is provided with two inlets and one outlet. One inlet is used to add 28-32 kg of a KOH solution with a mass concentration of 50% through a KOH flowmeter 15, and one inlet is used to add 39-45 kg of deionized water through a deionized water flowmeter 16 to form a 67-77 kg KOH solution with a mass concentration of 19-23%, which is then transported to the AOE emulsification tank 2 through the outlet under the action of gravity.

[0008] Deionized water is stored in a deionized water tank 4, which has a stainless steel inner wall and is provided with an inlet and an outlet. 1000-1100 kg of deionized water at 63-67° C. is added from the inlet through a deionized water flowmeter 16, and then transported to the AOE emulsification tank under the action of gravity.

[0009] The vacuum feeder 5 is of model ZKS-4, which is connected to the AOE oil tank 1 via a pipeline to transport the polymerized hindered phenol antioxidant (CPL) to the AOE oil tank 1.

[0010] The AOE pump 6 is a diaphragm pump, which is connected to the AOE emulsification tank 2 via a pipeline to transport the prepared antioxidant emulsion (AOE) to the ABS device.

[0011] The utility model has the beneficial effects of: being able to quickly realize the preparation of antioxidant emulsion AOE, and improving the monitoring sensitivity and accuracy of process parameters through the setting and control of digital instruments (thermal resistance thermometer, orifice plate flowmeter, etc.). BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Schematic diagram of the antioxidant emulsion preparation device.

[0013] In the figure: AOE oil tank 1, AOE emulsification tank 2, KOH storage tank 3, deionized water tank 4, vacuum feeder 5, AOE pump 6, AOE oil tank jacket 7, AOE emulsification tank jacket 8, AOE oil tank stirring 9 (rotation speed 85rpm), AOE emulsification tank stirring 10 (rotation speed 45rpm), emulsifier 11 (rotation speed 1470rpm), AOE oil tank thermometer 12, AOE emulsification tank thermometer 13, TFA flowmeter 14, KOH flowmeter 15, deionized water flowmeter 16. DETAILED DESCRIPTION

[0014] Example 1

[0015] See attached Figure 1 , an antioxidant emulsion preparation device, comprising an AOE oil tank 1, an AOE emulsification tank 2, a KOH storage tank 3, an ion-free water tank 4, a vacuum feeder 5 and an AOE pump 6. The AOE oil tank 1 is provided with an AOE oil tank jacket 7, an AOE oil tank stirrer 9 and an AOE oil tank thermometer 12. The top of the AOE oil tank 1 is provided with three inlets and the bottom is provided with an outlet; one inlet is used to add 600 kg of DLTDP, one inlet is used to add 600 kg of CPL through the vacuum feeder 5, and one inlet is used to add 65 kg of TFA through the TFA flowmeter 14; the AOE oil tank jacket 7 is provided with a steam inlet and a steam outlet. outlet, under the continuous heating of low-pressure steam (0.4MPa, 200℃), the reading of AOE oil tank thermometer 12 rises to 76℃, then the AOE oil tank stirring 9 is started to melt the raw materials to obtain oily liquid, which is sent to AOE emulsification tank 2 from the outlet after stirring for 2.5h; AOE emulsification tank 2 is equipped with AOE emulsification tank jacket 8, AOE emulsification tank stirring 10, emulsifier 11 and AOE emulsification tank thermometer 13, and AOE emulsification tank jacket 8 is provided with a steam inlet and a steam outlet; under the continuous heating of low-pressure steam (0.4MPa, 200℃), the reading of AOE emulsification tank thermometer 13 rises to 65℃ to complete the AOE emulsification tank preheating; the top of the AOE emulsification tank 2 is provided with four inlets and the bottom is provided with an outlet. The preheated AOE emulsification tank 2 first receives the oily liquid from the AOE oil tank 1, and then starts the AOE emulsification tank stirring 10, and then adds 72kg of KOH solution with a mass concentration of 21%. After 0.5h, the emulsifier 11 is started and 1050kg of 65℃ deionized water in the deionized water tank 4 is added to the AOE emulsification tank 2 to complete the phase transition of the material from the oil phase to the water phase; finally, 25kg of defoaming agent (the main component is a mixture of dimethylsiloxane and other organic substances) and 2kg of xanthan gum are added, and after stirring for 1h, the reaction product AOE is removed from the AOE emulsification tank 1. The outlet of E emulsification tank 2 is transported to the ABS device through AOE pump 6; the KOH storage tank is provided with two inlets and one outlet, one inlet is used to add 30kg of KOH solution with a mass concentration of 50% through KOH flowmeter 15, and one inlet is used to add 42kg of deionized water through deionized water flowmeter 16 to form 72kg of KOH solution with a mass concentration of 21%; the deionized water tank 4 is made of stainless steel, and is provided with one inlet and one outlet, and 1050kg of 65℃ deionized water is added from the inlet through deionized water flowmeter 16; the AOE pump 6 is a diaphragm pump, which transports the prepared antioxidant emulsion to the ABS device.

[0016] Example 2: Antioxidant Test

[0017] 1. Purpose: To test the isothermal antioxidant property of HRG resin prepared by using the antioxidant emulsion (AOE) of the present invention by DSC analyzer.

[0018] 2. Principle: Under isothermal conditions, the stability of the resin can be tested as a function of time at a fixed temperature. The test results of high temperature / short time isothermal DSC can be used to predict low temperature stability.

[0019] 3. Testing process:

[0020] 1) One hour before the test, turn on the heating unit and set the air flow rate of the DSC cell to 50±2mL / min;

[0021] 2) HRG latex and two AOE emulsions (one is the AOE prepared in this application, and the other is the AOE purchased from Hengnuo Technology) were mixed at a mass ratio of 170:1, and HRG resin samples were obtained after flocculation. After the samples passed through a 0.85 mm sieve, 10±1 mg of the sieve was weighed and placed in sample trays respectively;

[0022] 3) Take another empty reference pan and place it on the rear thermocouple of the DSC sensor;

[0023] 4) Set the temperature according to the specified value. When the temperature reaches the set value, place the sample plate on the front thermocouple of the DSC sensor for quick inspection;

[0024] 5) During the DSC test, closely monitor the real-time curve on the computer screen. When the exothermic peak exceeds its highest point, it will automatically stop, or if there is no exothermic phenomenon within 120 minutes, the instrument will stop running;

[0025] 6) Use data analysis software to find the approximate time when the exothermic reaction starts, and express the result in minutes;

[0026] 7) The above process was repeated 5 times. The results are shown in Table 1.

[0027] Table 1: 200℃ isothermal DSC oxidation resistance test data

[0028] Number of tests 1 2 3 4 5 Hengnuo Technology AOE emulsion antioxidant performance / min 20 22 19 24 22 The oxidation resistance of AOE emulsion prepared in this application / min 44 42 46 45 45

[0029] 4. Test results:

[0030] It can be seen that when the AOE emulsion and the HRG emulsion are mixed in equal proportions, the oxidation resistance of the HRG resin prepared using the AOE emulsion of the present application is greatly improved.

Claims

1. An antioxidant emulsion preparation device, characterized in that: The invention comprises an AOE oil tank (1), an AOE emulsification tank (2), a KOH storage tank (3), an ion-free water tank (4), a vacuum feeder (5) and an AOE pump (6). The AOE oil tank (1) is provided with an AOE oil tank jacket (7), an AOE oil tank stirrer (9) and an AOE oil tank thermometer (12). The top of the AOE oil tank (1) is provided with three inlets and the bottom is provided with an outlet. One inlet is used to add dilauryl thiodipropionate, one inlet is used to add a polymerization hindered phenol antioxidant through the vacuum feeder (5), and one inlet is used to add tallow fatty acid through a TFA flowmeter (14). The AOE oil tank jacket (7) is provided with a steam inlet and a steam outlet. The raw materials are The AOE oil tank (1) is melted into an oily liquid; the AOE emulsification tank (2) is provided with an AOE emulsification tank jacket (8), an AOE emulsification tank stirrer (10), an emulsifier (11) and an AOE emulsification tank thermometer (13); the AOE emulsification tank jacket (8) is provided with a steam inlet and a steam outlet; the top of the AOE emulsification tank (2) is provided with four inlets, and the bottom is provided with an outlet; the oily liquid from the AOE oil tank (1), a KOH solution with a mass concentration of 19 to 23%, deionized water, a defoaming agent and xanthan gum are respectively added to the four inlets; the raw materials undergo phase transformation in the AOE emulsification tank (2) to form an AOE emulsion, and then are transported from the outlet to the ABS device through an AOE pump (6).

2. The device for preparing an antioxidant emulsion according to claim 1, characterized in that: The AOE oil tank (1) has an enamel inner wall and an enamel stirring device.

3. The device for preparing an antioxidant emulsion according to claim 1, characterized in that: The AOE emulsification tank (2) has a stainless steel inner wall.

4. The device for preparing an antioxidant emulsion according to claim 1, characterized in that: The KOH solution is stored in a KOH storage tank (3). The KOH storage tank (3) has a stainless steel inner wall and is provided with two inlets and one outlet. A KOH solution with a mass concentration of 50% is added to the inlet through a KOH flowmeter (15), and deionized water is added to the other inlet through a deionized water flowmeter (16). The formed KOH solution with a mass concentration of 19-23% is transported to the AOE emulsification tank (2) through the outlet under the action of gravity.

5. The device for preparing an antioxidant emulsion according to claim 1, characterized in that: Deionized water is stored in a deionized water tank (4). The deionized water tank (4) has a stainless steel inner wall and is provided with an inlet and an outlet. Deionized water at 63-67° C. is added from the inlet through a deionized water flow meter (16) and then transported to the AOE emulsification tank (2) under the action of gravity.

6. The device for preparing an antioxidant emulsion according to claim 1, characterized in that: The vacuum feeder (5) is of model ZKS-4, and the AOE pump (6) is a diaphragm pump.