High-temperature rapid annealing device for semiconductor material

By using graphite supports and magnetically coupled quartz rods in a high-temperature rapid annealing device for semiconductor materials, combined with the strict protection of InP and GaAs substrates, and using hydrogen annealing, the problem that traditional CVD cannot effectively protect the sample is solved, and the sample surface is reduced The effect of roughness and imperfections.

CN221861598UActive Publication Date: 2024-10-18GUANGXI NORMAL UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420250845.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-01
Publication Date
2024-10-18
Estimated Expiration
2034-02-01

AI Technical Summary

Technical Problem

Traditional CVD cannot effectively protect the sample during high-temperature rapid annealing, resulting in increased surface roughness and defects.

Method used

A high-temperature rapid annealing device for semiconductor materials was designed, using a graphite holder and a magnetically coupled quartz rod, combined with InP and GaAs substrates to closely protect the sample, and annealed with hydrogen to fully eliminate oxygen impurity gas before annealing.

Benefits of technology

It effectively reduces the surface roughness of the sample after annealing, avoids the appearance of surface defects on the sample, and improves the annealing effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221861598U_ABST
    Figure CN221861598U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of semiconductor materials and devices, in particular to a high-temperature rapid annealing device for semiconductor materials, which comprises an annealing cavity quartz tube, a push-pull mechanism and a protection mechanism, the push-pull mechanism comprises a first magnet, a second magnet and a quartz rod, and the protection mechanism comprises a graphite support, an InP substrate and a GaAs substrate. A polished surface of an InP substrate is upwards placed on a quartz rod, a groove in the bottom of a graphite support is aligned with the InP substrate, a polished surface of a sample is upwards placed on the InP substrate through a cavity cut by the graphite support, finally, the polished surface of a GaAs substrate is downwards covered on the sample, a first magnet is driven by a handle to move on the outer wall of a quartz tube, and the InP substrate is placed on the quartz rod. And the quartz rod in the quartz tube is moved through magnetic coupling, so that the graphite bracket is moved to a corresponding annealing position. The sample is tightly protected by InP and GaAs at the upper part and the lower part, hydrogen is used for annealing, and impurity gases such as oxygen and the like are fully eliminated before annealing, so that the surface roughness of the annealed sample is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductor materials and devices, in particular to a high-temperature rapid annealing device for semiconductor materials. Background Art

[0002] In the semiconductor industry, heat treatment of semiconductor materials is essential. Its main purpose is to release internal stress, increase the ductility of materials, reduce deformation and cracking tendencies, and also change the crystal structure of the surface or interior of semiconductor materials, eliminate defects, etc., to obtain the required specific properties. In actual production, annealing is one of the most commonly used methods in the heat treatment process of semiconductor materials.

[0003] The high temperature rapid annealing is performed by simple CVD (chemical vapor deposition), which is simple to operate and has low equipment cost. Since the sample is only protected by GaAs and nitrogen, the surface roughness of the sample will increase, and even defects will appear on the surface of the sample. Utility Model Content

[0004] The utility model aims to provide a high-temperature rapid annealing device for semiconductor materials, comprising a cut graphite support and a quartz rod moved by magnetic coupling inside a CVD, wherein the sample is tightly protected by InP and GaAs above and below, and hydrogen is used for annealing. Impurity gases such as oxygen are fully excluded before annealing, aiming to solve the problem that traditional CVD cannot provide good protection for the sample during high-temperature rapid annealing.

[0005] To achieve the above-mentioned purpose, the utility model provides a high-temperature rapid annealing device for semiconductor materials, comprising an annealing cavity quartz tube, a push-pull mechanism and a protection mechanism;

[0006] The push-pull mechanism includes a handle, a first magnet, a second magnet and a quartz rod, the quartz rod is installed in the quartz tube of the annealing chamber, the second magnet is arranged on one side of the quartz rod, the first magnet is magnetically coupled with the second magnet and is arranged outside the quartz tube of the annealing chamber, the handle is fixedly connected to the first magnet and is located on one side of the second magnet, and the protection mechanism is arranged on the other side of the quartz rod.

[0007] Wherein, the protection mechanism includes a graphite support, an InP substrate and a GaAs substrate, wherein the graphite support is arranged on one side of the quartz rod; the InP substrate is connected to the graphite support and placed on one side of the quartz rod; the GaAs substrate is connected to the graphite support and arranged on the sample above the InP substrate.

[0008] Wherein, the graphite support has a square hole and a square groove, the square hole is arranged in the middle of the graphite support; the square groove is arranged at the bottom of the graphite support.

[0009] The quartz rod has a circular hole, and the circular hole is located on one side of the quartz rod for placing the second magnet.

[0010] Wherein, the quartz rod is a semicircular quartz rod.

[0011] The utility model discloses a high-temperature rapid annealing device for semiconductor materials. The utility model provides a high-temperature rapid annealing device for InP heterojunction (or semiconductor material), which specifically comprises CVD, a quartz tube, a push-pull mechanism, and a protection mechanism. The push-pull mechanism comprises a first magnet, a second magnet and a quartz rod. The protection mechanism comprises a graphite support, an InP substrate, and a GaAs substrate. The polished surface of the InP substrate is placed on the quartz rod upwards, the groove at the bottom of the graphite support is aligned with the InP substrate and placed well, the polished surface of the sample is placed on the InP substrate through a hole cut out by the graphite support, and finally the polished surface of the GaAs substrate is covered on the sample downwards. The first magnet is driven to move on the outer wall of the quartz tube by a handle, and the quartz rod in the quartz tube is moved by magnetic coupling to move the graphite support to a corresponding annealing position. Since the sample is tightly protected by InP and GaAs above and below, hydrogen is used for annealing, and impurity gases such as oxygen are fully eliminated before annealing, so that the surface roughness of the sample after annealing is reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.

[0013] Figure 1 It is a schematic diagram of the overall structure of the high-temperature rapid annealing device for semiconductor materials of the utility model.

[0014] Figure 2 It is a structural schematic diagram of the graphite bracket of the utility model.

[0015] Figure 3 The utility model is a flow chart of a high-temperature rapid annealing device for semiconductor materials.

[0016] In the figure: 1-handle, 2-first magnet, 3-second magnet, 4-quartz rod, 5-graphite bracket, 6-GaAs substrate, 7-annealing sample, 8-InP substrate, 9-annealing cavity quartz tube, 41-circular hole, 51-square hole, 52-square groove. DETAILED DESCRIPTION

[0017] Embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, but should not be understood as limiting the present invention.

[0018] The first embodiment of the present application is:

[0019] See also Figure 1 and Figure 2 ,in Figure 1 It is a schematic diagram of the overall structure of the high-temperature rapid annealing device for semiconductor materials. Figure 2 It is a schematic diagram of the structure of the graphite support 5.

[0020] The utility model provides a high-temperature rapid annealing device for semiconductor materials: including an annealing cavity quartz tube, a push-pull mechanism and a protection mechanism, the push-pull mechanism includes a handle, a first magnet, a second magnet and a quartz rod, the protection mechanism includes a graphite bracket, an InP substrate and a GaAs substrate, the graphite bracket has a square hole and a square groove, the quartz rod has a circular hole, and the quartz rod is a semicircular quartz rod. The above scheme solves the problem of using simple CVD (chemical vapor deposition) for high-temperature rapid annealing, which is simple to operate and has low equipment cost. The problem that the sample surface roughness becomes higher and even defects appear on the sample surface when only GaAs and nitrogen are used for protection is caused.

[0021] In this embodiment, the annealing chamber quartz tube 9, a push-pull mechanism, and a protection mechanism are specifically included. The push-pull mechanism includes a handle 1, a first magnet 2, a second magnet 3, and a quartz rod 4. The protection mechanism includes a graphite support 5, an InP substrate 8, and a GaAs substrate 6. The polished surface of the InP substrate 8 is placed on the quartz rod 4 with the polished surface facing upward. The bottom groove of the graphite support 5 is aligned with the InP substrate 8 and placed well. The polished surface of the sample 7 is placed on the InP substrate 8 with the polished surface facing upward through the cavity cut by the graphite support 5. Finally, the polished surface of the GaAs substrate 6 is covered on the sample 7 with the polished surface facing downward. The handle 1 drives the first magnet 2 to move on the outer wall of the annealing chamber quartz tube 9. The quartz rod 4 in the annealing chamber quartz tube 9 is moved by magnetic coupling to move the graphite support 5 to the corresponding annealing position. Since the sample 7 is tightly protected by the InP substrate 8 and the GaAs substrate 6 from top to bottom, hydrogen annealing is used, and impurity gases such as oxygen are fully eliminated before annealing, so that the surface roughness of the sample after annealing is reduced.

[0022] Among them, a 1.3cm*1.3cm square groove 52 is cut out at the bottom of the graphite support 5 to just clamp the InP substrate 8 to prevent the InP substrate 8 from moving during the process of pushing and pulling the quartz rod 4, and a 1.1cm*1.1cm square hole 51 is cut out in the middle of the groove at the bottom of the graphite support 5 to make the GaAs substrate 6 completely cover the sample and prevent it from moving during the process of pushing and pulling the quartz rod.

[0023] See also Figure 3 The utility model provides a high-temperature rapid annealing of an InP heterojunction (or semiconductor material), and the specific operation process is as follows:

[0024] S1. Place the InP substrate 8 with the polished surface facing upward on the quartz rod 4, and align the bottom groove of the graphite support 5 with the InP substrate 8;

[0025] The S2 sample is placed on the InP substrate 8 through the hole cut out by the graphite support 5 with the polished surface facing upward, and the GaAs substrate 6 is covered on the sample with the polished surface facing downward;

[0026] S3: placing the quartz rod 4 on the right side of the double temperature zone (the utility model is applicable to different types of CVD tube furnaces, such as single temperature zone CVD, double temperature zone CVD and three temperature zone CVD);

[0027] S4: extracting the air in the annealing cavity quartz tube 9 by a mechanical pump until the pressure in the annealing cavity quartz tube 9 reaches 0.62 Pa;

[0028] S5: filling the cavity quartz tube with N2 gas until the pressure in the cavity quartz tube reaches 0.1 mPa;

[0029] S6: repeat steps S4 to S5 twice to fully remove the air or other impurity gases in the quartz tube;

[0030] S7: Start heating the left and right temperature zones of the dual-temperature zone CVD, use hydrogen annealing, and the gas flow is from right to left (flowing in from the graphite support), with a gas flow rate of 50sscm;

[0031] S8 When the left and right temperature zones of the dual-temperature zone CVD are heated to 580°C, the handle 1 is used to drive the first magnet 2 to move on the outer wall of the quartz tube 9 of the annealing chamber, so that the second magnet 3 adsorbed by the first magnet 2 moves, and the movement of the second magnet 3 drives the quartz rod 4 to move, and the movement of the quartz rod 4 drives the graphite support 5 and the annealed sample to move;

[0032] The S9 sample was moved to the middle part of the right temperature zone of CVD and annealed for 10 min;

[0033] After S10 annealing, the sample is completely pulled out of the CVD right temperature zone and quickly cooled to room temperature;

[0034] S11 cools the dual-temperature zone CVD to room temperature, and while cooling, the hydrogen gas flow does not change.

[0035] What is disclosed above is only one or more preferred embodiments of the present application, and cannot be used to limit the scope of rights of the present application. Ordinary technicians in this field can understand that all or part of the processes of implementing the above embodiments and equivalent changes made according to the claims of the present application are still within the scope covered by the present application.

Claims

1. A high temperature rapid annealing device for semiconductor materials, characterized in that: It includes an annealing cavity quartz tube, a push-pull mechanism and a protection mechanism; The push-pull mechanism includes a handle, a first magnet, a second magnet and a quartz rod, the quartz rod is installed in the quartz tube of the annealing chamber, the second magnet is arranged on one side of the quartz rod, the first magnet is magnetically coupled with the second magnet and is arranged outside the quartz tube of the annealing chamber, the handle is fixedly connected to the first magnet and is located on one side of the second magnet, and the protection mechanism is arranged on the other side of the quartz rod.

2. The high temperature rapid annealing device for semiconductor materials according to claim 1, characterized in that: The protection mechanism includes a graphite support, an InP substrate and a GaAs substrate, wherein the graphite support is arranged on one side of the quartz rod; the InP substrate is connected to the graphite support and placed on one side of the quartz rod; the GaAs substrate is connected to the graphite support and arranged on the sample above the InP substrate.

3. The high temperature rapid annealing device for semiconductor materials according to claim 2, characterized in that: The graphite support has a square hole and a square groove, wherein the square hole is arranged in the middle of the graphite support; and the square groove is arranged at the bottom of the graphite support.

4. The high temperature rapid annealing device for semiconductor materials according to claim 1, characterized in that: The quartz rod has a circular hole, and the circular hole is located on one side of the quartz rod for placing the second magnet.

5. The high temperature rapid annealing device for semiconductor materials according to claim 1, characterized in that: The quartz rod is a semicircular quartz rod.