Rapid forming and pressing die for high-precision aluminum veneer

By designing a high-precision aluminum veneer rapid prototyping pressing mold and using the combined structure of a telescopic rod and a damping spring, the aluminum veneer can automatically detach from the upper and lower molds after forming, which solves the problem of the aluminum veneer getting stuck in the lower mold and being unable to demould in traditional molds. problem, improving the molding efficiency and the convenience of mold replacement.

CN221869966UActive Publication Date: 2024-10-22FUJIAN JINNUO BUILDING MATERIAL CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420364069.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-27
Publication Date
2024-10-22
Estimated Expiration
2034-02-27

AI Technical Summary

Technical Problem

Traditional aluminum veneer pressing molds tend to get stuck in the lower mold during the aluminum veneer forming process and cannot be demoulded. The existing solutions can only separate the aluminum veneer from the upper mold, but cannot solve the demoulding problem when the aluminum veneer is stuck in the lower mold. .

Method used

A high-precision aluminum veneer rapid prototyping pressing mold is designed. It adopts a structure that combines the top mold assembly and the bottom mold assembly. The upper mold is demoulded through the first telescopic rod and the second telescopic rod. The damping spring and the The second release plate realizes the demoulding of the lower mold, ensuring that the aluminum veneer can automatically detach from the molds on both sides after forming.

Benefits of technology

It realizes that the aluminum veneer can automatically detach from the top mold assembly and the bottom mold assembly after forming, solves the problem of the aluminum veneer being stuck in the lower mold and unable to be demoulded, and improves the efficiency of mold use and the convenience of replacement.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221869966U_ABST
    Figure CN221869966U_ABST
Patent Text Reader

Abstract

The utility model discloses a high-precision rapid forming and pressing die for an aluminum veneer, which relates to the technical field of aluminum veneer processing and comprises a bottom plate, a support frame is arranged on the bottom plate, a top die component for pressing the aluminum veneer and demoulding from the top is arranged on the support frame, and a bottom die component for pressing the aluminum veneer and separating from the bottom is arranged on the bottom plate. According to the utility model, through the top mold assembly, the second telescopic rod extends downwards to separate the upper mold from the first demolding plate, so that the effect that the upper end of the aluminum veneer is separated from the upper mold is achieved, and through the bottom mold assembly, the second demolding plate is separated from the lower mold through the damping spring, so that the effect that the aluminum veneer is separated from the lower mold is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of aluminum single plate processing, in particular to a high-precision aluminum single plate rapid prototyping pressing die. Background Art

[0002] With the development of the construction industry, the use of aluminum veneers is also increasing. Aluminum veneers need to be pressed and formed during the production process. The traditional aluminum veneer pressing mold is composed of an upper mold assembly and a lower mold assembly. During use, the aluminum veneer is pressed by the mutual cooperation between the upper mold assembly and the lower mold assembly. However, in the actual aluminum veneer forming process, the aluminum veneer is easily stuck in the upper mold assembly and cannot be demolded. For example, a high-precision aluminum veneer rapid prototyping pressing mold is recorded in the patent with patent announcement number CN218452551U. The recorded solution is that after the mold is pressed, the gear is driven to rotate by rotating the rotating rod, and the linkage rack is driven to move the stripping plate downward to separate the aluminum veneer from the mold. However, the pressing mold can only separate the aluminum veneer from the upper mold. When the aluminum veneer is stuck in the lower mold, the aluminum veneer in the pressing mold cannot be demolded.

[0003] Based on this, a high-precision aluminum single plate rapid prototyping pressing die is now provided, which can eliminate the disadvantages of the existing device. Utility Model Content

[0004] The utility model aims to provide a high-precision aluminum veneer rapid prototyping pressing die to solve the problem that the pressing die can only separate the aluminum veneer from the upper die, and when the aluminum veneer is stuck in the lower die, the aluminum veneer in the pressing die cannot be demoulded.

[0005] In order to achieve the above purpose, the utility model provides the following technical solutions:

[0006] A high-precision aluminum single plate rapid prototyping pressing die comprises a bottom plate, a support frame is provided on the bottom plate, a top die assembly is provided on the support frame for pressing the aluminum single plate and demoulding from the top, and a bottom die assembly is provided on the bottom plate for pressing the aluminum single plate and demoulding from the bottom.

[0007] On the basis of the above technical solutions, the present invention also provides the following optional technical solutions:

[0008] The top mold assembly includes a first telescopic rod, a second telescopic rod, a fixed plate, an upper mold, a connecting plate, a first stripping plate, a through slot and a second bolt. The first telescopic rod and the second telescopic rod are fixed to a support frame. The output end of the first telescopic rod is connected to the fixed plate. An upper mold is provided on the lower side of the fixed plate. A first stripping plate is slidably connected inside the upper mold. A connecting plate is provided at the output end of the second telescopic rod. The connecting plate is connected to the first stripping plate by a second bolt. A through slot is provided in the center of the fixed plate and the upper mold.

[0009] In an optional solution: the through groove matches the connecting plate.

[0010] In an optional scheme: the bottom mold assembly includes a lower mold, a limit seat, a first threaded hole, a second stripping plate, a support column, a damping spring and a groove, a limit seat is provided at the bottom of the lower mold, two first threaded holes are provided at the front end of the limit seat, a groove is provided in the center of the lower mold, a plurality of support columns are provided at the bottom of the groove, a damping spring is provided inside the support column, and the upper end of the damping spring is connected to the second stripping plate.

[0011] In an optional solution: the second stripping plate matches the groove.

[0012] In an optional solution: a limiting groove matching the limiting seat is provided at the center of the base plate, and a second threaded hole connected to the first threaded hole is provided at the front end of the base plate.

[0013] In an optional solution: when the bottom surface of the second stripping plate contacts the upper end surface of the support column, the upper surface of the second stripping plate is flush with the upper surface of the lower mold.

[0014] In an optional solution: the base plate is connected to the limit seat via a first bolt.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0016] 1. The utility model uses the top mold assembly to extend the second telescopic rod downward to separate the upper mold from the first stripping plate, thereby achieving the effect of separating the upper end of the aluminum veneer from the upper mold.

[0017] 2. The utility model uses a damping spring through a bottom mold assembly to separate the second stripper plate from the lower mold, thereby achieving the effect of separating the aluminum veneer from the lower mold. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a structural schematic diagram of the utility model.

[0019] Figure 2 It is a structural schematic diagram of the top mold assembly of the utility model.

[0020] Figure 3 It is a structural schematic diagram of the bottom mold assembly of the utility model.

[0021] Figure 4 It is a structural schematic diagram of the bottom plate of the utility model.

[0022] Notes on figure numbers: 100, base plate; 101, support frame; 102, first bolt; 103, second threaded hole; 104, limit groove; 200, top mold assembly; 201, first telescopic rod; 202, second telescopic rod; 203, fixing plate; 204, upper mold; 205, connecting plate; 206, first stripping plate; 207, through groove; 300, bottom mold assembly; 301, lower mold; 302, limit seat; 303, first threaded hole; 304, second stripping plate; 305, support column; 306, damping spring; 307, groove. DETAILED DESCRIPTION

[0023] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments.

[0024] Example 1

[0025] In one embodiment, Figure 1-Figure 4 As shown, a high-precision aluminum veneer rapid prototyping pressing mold includes a base plate 100, a support frame 101 is provided on the base plate 100, a top mold assembly 200 for pressing the aluminum veneer and demolding from the top is provided on the support frame 101, and a bottom mold assembly 300 for pressing the aluminum veneer and detaching from the bottom is provided on the base plate 100. When in use, the aluminum veneer is pressed by the top mold assembly 200 and the bottom mold assembly 300, and the pressed aluminum veneer can automatically fall off from the top mold assembly 200 and the bottom mold assembly 300.

[0026] In one embodiment, Figure 2 As shown, the top mold assembly 200 includes a first telescopic rod 201, a second telescopic rod 202, a fixed plate 203, an upper mold 204, a connecting plate 205, a first stripping plate 206, a through slot 207 and a second bolt 208. The first telescopic rod 201 and the second telescopic rod 202 are fixed to the support frame 101. The output end of the first telescopic rod 201 is connected to the fixed plate 203. An upper mold 204 is provided at the lower side of the fixed plate 203. A first stripping plate 206 is slidably connected inside the upper mold 204. A connecting plate 205 is provided at the output end of the second telescopic rod 202. The connecting plate 205 It is connected to the first stripping plate 206 by a second bolt 208, and a through slot 207 is provided in the center of the fixed plate 203 and the upper mold 204. When in use, the first telescopic rod 201 and the second telescopic rod 202 are extended synchronously, and the fixed plate 203 drives the upper mold 204 to move downward close to the bottom mold assembly 300 to press the aluminum veneer. After the pressing is completed, the first telescopic rod 201 and the second telescopic rod 202 are retreated synchronously, and the fixed plate 203 drives the upper mold 204 to move upward. After rising to a certain height, the first telescopic rod 201 is fixed, and the second telescopic rod 202 is extended downward to enable the first stripping plate 206 to push the aluminum veneer out.

[0027] In one embodiment, Figure 2 and Figure 3 As shown, the through slot 207 matches the connecting plate 205 , and when the upper mold is replaced, the connecting plate 205 passes through the through slot 207 and is connected to the first stripping plate 206 .

[0028] In one embodiment, Figure 3 As shown, the bottom mold assembly 300 includes a lower mold 301, a limit seat 302, a first threaded hole 303, a second stripping plate 304, a support column 305, a damping spring 306 and a groove 307. A limit seat 302 is provided at the bottom of the lower mold 301, and two first threaded holes 303 are provided at the front end of the limit seat 302. A groove 307 is provided in the center of the lower mold 301, and a plurality of support columns 305 are provided at the bottom of the groove 307. A damping spring 306 is provided inside the support column 305, and the upper end of the damping spring 306 is connected to the second stripping plate 304. After the aluminum veneer is pressed, the top mold assembly 200 moves upward, and the damping spring 306 inside the support column 305 pushes the second stripping plate 304 to separate from the lower mold 301, so that the aluminum veneer is separated from the lower mold 301.

[0029] Example 2

[0030] In one embodiment, Figure 2 and Figure 3 As shown, a limiting groove 104 matching the limiting seat 302 is provided at the center of the base plate 100, and a second threaded hole 103 connected to the first threaded hole 303 is provided at the front end of the base plate 100. The base plate 100 is connected to the limiting seat 302 through a first bolt 102. The limiting seat 302 can be separated from the limiting groove 104 by unscrewing the second bolt 102, so as to facilitate the replacement of the lower mold 301.

[0031] The above embodiment discloses a high-precision aluminum single plate rapid prototyping pressing die, wherein, when in use, the first telescopic rod 201 and the second telescopic rod 202 are extended synchronously, and the fixed plate 203 drives the upper mold 204 to move downward close to the bottom mold assembly 300 to press the aluminum single plate. After the pressing is completed, the first telescopic rod 201 and the second telescopic rod 202 are retracted synchronously, and the fixed plate 203 drives the upper mold 204 to move upward. After rising to a certain height, the first telescopic rod 201 is fixed, and the second telescopic rod 202 is extended downward to make the first stripping plate 206 and the upper mold 204, so that the aluminum single plate The plate is separated from the upper mold 204. After the aluminum veneer is pressed, the top mold assembly 200 moves upward, and the damping spring 306 inside the support column 305 pushes the second stripping plate 304 to separate from the lower mold 301, so that the aluminum veneer is separated from the lower mold 301. When replacing the mold, unscrew the second bolt 208 to separate the first stripping plate 206 from the connecting plate, and then separate the upper mold 204 from the fixed plate, so that the upper mold 204 can be replaced very conveniently. By unscrewing the second bolt 102, the limit seat 302 can be separated from the limit groove 104, so that the lower mold 301 can be replaced very conveniently.

[0032] The above is only a specific implementation of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any person skilled in the art who is familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.

Claims

1. A high-precision aluminum single plate rapid prototyping pressing die, comprising a base plate (100), wherein a support frame (101) is provided on the base plate (100), characterized in that: The support frame (101) is provided with a top mold assembly (200) for pressing the aluminum single plate and demoulding from the top, and the bottom plate (100) is provided with a bottom mold assembly (300) for pressing the aluminum single plate and demoulding from the bottom.

2. The high-precision aluminum single plate rapid prototyping pressing die according to claim 1, characterized in that: The top mold assembly (200) comprises a first telescopic rod (201), a second telescopic rod (202), a fixed plate (203), an upper mold (204), a connecting plate (205), a first stripping plate (206), a through slot (207) and a second bolt (208); the first telescopic rod (201) and the second telescopic rod (202) are fixed on a support frame (101); an output end of the first telescopic rod (201) is connected to the fixed plate (203); an upper mold (204) is provided at the lower side of the fixed plate (203); a first stripping plate (206) is slidably connected inside the upper mold (204); a connecting plate (205) is provided at the output end of the second telescopic rod (202); the connecting plate (205) is connected to the first stripping plate (206) by a second bolt (208); a through slot (207) is provided at the center of the fixed plate (203) and the upper mold (204).

3. The high-precision aluminum single plate rapid prototyping pressing die according to claim 2, characterized in that: The through slot (207) matches the connecting plate (205).

4. The high-precision aluminum single plate rapid prototyping pressing die according to claim 1, characterized in that: The bottom mold assembly (300) comprises a lower mold (301), a limiting seat (302), a first threaded hole (303), a second stripping plate (304), a support column (305), a damping spring (306) and a groove (307). A limiting seat (302) is provided at the bottom of the lower mold (301), two first threaded holes (303) are provided at the front end of the limiting seat (302), a groove (307) is provided at the center of the lower mold (301), a plurality of support columns (305) are provided at the bottom of the groove (307), a damping spring (306) is provided inside the support column (305), and the upper end of the damping spring (306) is connected to the second stripping plate (304).

5. The high-precision aluminum single plate rapid prototyping pressing die according to claim 4, characterized in that: The second stripping plate (304) matches the groove (307).

6. The high-precision aluminum single plate rapid prototyping pressing die according to claim 4, characterized in that: A limiting groove (104) matching the limiting seat (302) is provided at the center of the bottom plate (100), and a second threaded hole (103) connected to the first threaded hole (303) is provided at the front end of the bottom plate (100).

7. The high-precision aluminum single plate rapid prototyping pressing die according to claim 4, characterized in that: When the bottom surface of the second stripping plate (304) contacts the upper end surface of the support column (305), the upper surface of the second stripping plate (304) is flush with the upper surface of the limiting seat (302).

8. The high-precision aluminum single plate rapid prototyping pressing die according to claim 4, characterized in that: The bottom plate (100) is connected to the lower mold (301) via a first bolt (102).

Citation Information

Cited By

  • Double-sided pressing equipment for aluminum veneer

    CN224222440U