Die for verifying anti-falling performance of surface coating of galvanized steel sheet of automobile
By designing a mold with draw beads to simulate the stamping friction state, the problem in the existing technology of being unable to identify the risk of coating peeling off of galvanized steel plates is solved, and the verification accuracy of the anti-shedding performance of the coating on the surface of galvanized steel plates is improved.
Patent Information
- Application Number
- CN202420279156.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-05
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2034-02-05
AI Technical Summary
Existing methods for verifying the anti-shedding performance of coatings on the surface of automotive galvanized steel sheets cannot effectively simulate the friction state during stamping, resulting in the inability to accurately identify and judge the risk of coating peeling.
A mold including an upper mold and a lower mold is designed. By setting two draw beads around the punch of the lower mold, combined with a balance block and a limit block, the friction state of the automobile galvanized steel plate during the stamping process is simulated, and the friction state is increased. Friction resistance, thereby verifying the anti-falling performance of the coating.
It effectively simulates the friction state of the galvanized steel plate during the stamping process, improves the accuracy of judgment of the risk of coating peeling, and solves the problem of identifying the risk of coating peeling in the manufacturing process of galvanized steel plates.
Smart Images

Figure CN221899046U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of automobile manufacturing, in particular to a mold for verifying the anti-shedding performance of the surface coating of an automobile galvanized steel plate. Background Art
[0002] During the stamping process of automotive galvanized steel sheets, the coating will fall off due to deformation and friction of the steel sheet material. The zinc powder after falling off will adhere to the surface of the mold, causing surface quality defects such as pits and embossing on the parts after stamping. The problem of coating falling off is often caused by friction. At present, the only methods for verifying the anti-falling performance are bending and ball punching experiments. The existing anti-falling performance verification methods can often only verify the dezincification under deformation, and they cannot simulate the friction state during stamping. Therefore, there is an urgent need for a mold for verifying the anti-falling performance of the coating on the surface of automotive galvanized steel sheets. Utility Model Content
[0003] In view of the deficiencies existing in the prior art, the utility model provides a mold for verifying the anti-shedding performance of the coating on the surface of a galvanized steel plate of an automobile.
[0004] The utility model discloses a mold for verifying the anti-shedding performance of the coating on the surface of a galvanized steel plate of an automobile, comprising
[0005] As a further improvement of the utility model, it includes:
[0006] An upper die, the upper die comprising a backing plate and a concave die mounted on the lower surface of the backing plate and arranged downward;
[0007] A lower die, the lower die comprising a die base body, a punch and a blank holder installed on the upper surface of the die base body, the blank holder is sleeved on the outer side of the punch, and two drawing ribs are arranged around the periphery of the punch and at the connection between the blank holder and the blank holder;
[0008] Balancing blocks, a plurality of balancing blocks are arranged on the blank holding surface of the blank holding ring, and a plurality of balancing blocks are used to cover gaskets to adjust the gap between the die and the blank holding ring;
[0009] Limit blocks, multiple limit blocks are arranged on the outside of the pressure ring and installed on the mold base body, and multiple limit blocks are used to cover gaskets to adjust the gap between the die and the punch.
[0010] As a further improvement of the utility model, guide sleeves are respectively installed at the four corners of the lower surface of the pad downward in the vertical direction, and a guide column is respectively provided on the upper surface of the mold base body corresponding to the position of the guide sleeve;
[0011] When the upper mold and the lower mold are closed, a plurality of the guide posts are inserted into the corresponding guide sleeves.
[0012] As a further improvement of the utility model, the edge of the die is chamfered to form a rounded corner of the die;
[0013] The edge of the punch is chamfered to form a rounded corner of the punch that matches the rounded corner of the die.
[0014] As a further improvement of the utility model, the die is provided with rib grooves which match the two drawing ribs.
[0015] As a further improvement of the utility model, a plurality of positioning pins are arranged around the material holding surface of the blank holding ring;
[0016] The plurality of positioning pins are used to limit the position of the automotive galvanized steel sheet test piece placed on the lower die.
[0017] As a further improvement of the utility model, the two draw beads include a first annular draw bead close to the punch and a second annular draw bead close to the blank holder;
[0018] The resistance coefficient of the first annular drawbead is 0.45-0.5, and the resistance coefficient of the second annular drawbead is 0.35-0.45.
[0019] As a further improvement of the present invention, the first annular drawbead and the second annular drawbead are both semicircular drawbeads;
[0020] The spacing between the first annular draw bead and the second annular draw bead is 20 mm-30 mm.
[0021] As a further improvement of the present invention, the material inflow of the two draw beads is 30 mm-50 mm.
[0022] As a further improvement of the utility model, the upper die is detachably mounted on the slide block of the press, and the lower die is detachably mounted on the workbench of the press.
[0023] Compared with the prior art, the beneficial effects of the utility model are:
[0024] The utility model has a simple structure and is easy to operate. By arranging an upper die with a concave die and a lower die with a punch and arranging two drawing ribs around the punch, the anti-peeling performance of the surface coating of the automobile galvanized steel plate under the stamping friction state can be effectively simulated, and the problem that the risk of surface coating peeling cannot be identified in the galvanized steel plate manufacturing process is solved. The setting of the two drawing ribs can also effectively increase the friction resistance of the automobile galvanized steel plate under stamping, and further improve the accuracy of judging the risk of surface coating peeling of the automobile galvanized steel plate. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 An exploded view of the structure of a mold for verifying the anti-shedding performance of the surface coating of a galvanized steel plate for automobiles disclosed in an embodiment of the utility model;
[0026] Figure 2 A structural assembly diagram of a mold for verifying the anti-shedding performance of the coating on the surface of a galvanized steel plate for an automobile disclosed in an embodiment of the utility model;
[0027] Figure 3 A structural side sectional view of a mold for verifying the anti-shedding performance of the coating on the surface of a galvanized steel plate for automobiles disclosed in one embodiment of the utility model;
[0028] Figure 4 A schematic diagram of the upper mold structure of a mold for verifying the anti-shedding performance of the surface coating of a galvanized steel plate for an automobile disclosed in an embodiment of the utility model;
[0029] Figure 5 The utility model discloses a schematic diagram of the lower mold structure of a mold for verifying the anti-shedding performance of the surface coating of a galvanized steel plate of an automobile according to an embodiment of the utility model.
[0030] In the figure:
[0031] 1. Upper die; 11. Pad; 12. Concave die; 13. Guide sleeve; 14. First stop block; 15. Rib groove;
[0032] 2. Lower die; 21. Die base body; 22. Punch; 23. Binder ring; 241. First annular draw rib; 242. Second annular draw rib; 25. Guide sleeve; 26. Second limit block; 27. Balance block; 28. Positioning pin. DETAILED DESCRIPTION
[0033] In order to make the purpose, technical solution and advantages of the embodiment of the utility model clearer, the technical solution in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is a part of the embodiment of the utility model, not all of the embodiments. Based on the embodiment of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0034] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0035] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0036] The utility model is further described in detail below in conjunction with the accompanying drawings:
[0037] like Figure 1-3 As shown, according to the utility model, a mold for verifying the anti-peeling performance of the surface coating of a galvanized steel plate for automobiles comprises an upper mold 1, a lower mold 2, a balancing block 27 and a limiting block 26, wherein the upper mold 1 comprises a pad 11 and a die 12 installed on the lower surface of the pad 11 and arranged downward; the lower mold 2 comprises a die base body 21 and a punch 22 and a pressure ring 23 installed on the upper surface of the die base body 21, the pressure ring 23 is sleeved on the outer side of the punch 22, and two drawing ribs are arranged around the connection between the punch 22 and the pressure ring 23; a plurality of balancing blocks 27 are arranged on the pressing surface of the pressure ring 23, and the plurality of balancing blocks 27 are used to sleeve gaskets to adjust the gap between the die 12 and the pressure ring 23; a plurality of limiting blocks 26 are arranged on the outer side of the pressure ring 23 and are installed on the die base body 21, and the plurality of limiting blocks 26 are used to sleeve gaskets to adjust the gap between the die 12 and the punch 22.
[0038] In this embodiment, the structure is simple and the operation is convenient. By setting an upper die 1 with a die 12 and a lower die 2 with a punch 22, and arranging two drawing ribs around the punch 22, the anti-peeling performance of the surface coating of the automobile galvanized steel sheet under the stamping friction state can be effectively simulated, which solves the problem that the risk of surface coating peeling cannot be identified in the galvanized steel sheet manufacturing process. The setting of two drawing ribs can also effectively increase the friction resistance of the automobile galvanized steel sheet under stamping, further improving the accuracy of judging the risk of surface coating peeling of the automobile galvanized steel sheet.
[0039] Specific:
[0040] like Figure 4 As shown, in the above embodiment, preferably, the pad 11 is of a rectangular structure, a die 12 is fixedly installed at the center of the lower surface of the pad 11, and the die 12 is arranged downward, and guide sleeves 13 are installed downward in the vertical direction at the four corners of the lower surface of the pad 11, and the die 12 is surrounded by rib grooves 15 that cooperate with the two drawing ribs.
[0041] like Figure 5 As shown, in the above embodiment, preferably, the mold base body 21 is of a rectangular structure, and a matching punch 22 is arranged at the center of the upper surface of the mold body 21 corresponding to the position of the die 12, and a pressure ring 23 is arranged around the upper surface of the mold body 21 corresponding to the punch 22, and two drawing ribs are arranged in sequence from the inside to the outside at the connection between the pressure ring 23 and the punch 22.
[0042] In the above embodiment, preferably, guide sleeves 25 are installed at the four corners of the upper surface of the mold base body 21 in the vertical direction upward. During actual mold closing, multiple guide sleeves 25 can be inserted into the corresponding guide sleeves 13 of the upper mold 1.
[0043] In the above embodiment, preferably, a plurality of second limit blocks 26 are symmetrically installed on the upper surface of the mold base body 21 corresponding to the outer side of the pressure ring 23, and a plurality of first limit blocks 14 cooperating with the second limit blocks 26 are provided on the lower surface of the pad 11 corresponding to the plurality of second limit blocks 26. In the present embodiment, the number of second limit blocks 26 is 4, and the four second limit blocks 26 are symmetrically arranged on the left and right sides of the pressure ring 23 in pairs, and are fixedly installed on the upper surface of the mold base body 21. In the present embodiment, the first limit block 14 and the second limit block 26 are both cylindrical. During the film closing process, the first limit block 14 and the second limit block 26 can adjust the gap between the die 12 and the punch 22 by setting a gasket.
[0044] In the above embodiment, preferably, the blank holder 23 has a rectangular structure, and a center hole is reserved in the center of the blank holder 23 for the punch 22 to pass through. A plurality of balancing blocks 27 are arranged around the pressing surface of the blank holder 23. In this embodiment, eight balancing blocks 27 are provided, that is, a balancing block 27 is provided at each corner of the pressing surface of the blank holder 23, and a balancing block 27 is provided in the middle of each edge. The balancing block 27 in this embodiment is a cylindrical balancing block, and a plurality of gaskets can be provided on the cylindrical balancing block to adjust the gap between the die 22 and the blank holder 23.
[0045] In the above embodiment, preferably, a plurality of positioning pins 28 are arranged around the pressing surface of the pressure ring 23. In this embodiment, the number of positioning pins 28 is 8, that is, two positioning pins 28 are arranged on each of the four sides of the pressing surface of the pressure ring 23. The arrangement of multiple positioning pins 28 can be used to limit the automotive galvanized steel plate test piece placed on the lower mold 2.
[0046] In the above embodiment, preferably, the edge of the die 12 is chamfered to form a die rounded corner; the edge of the punch 22 is chamfered to form a punch rounded corner that matches the die rounded corner. The die rounded corner and the punch rounded corner in this embodiment can be designed with reference to the drawing die of the automobile outer cover.
[0047] In the above embodiment, preferably, the two draw beads include a first annular draw bead 241 close to the punch 22 and a second annular draw bead 242 close to the blank holder 23; wherein the resistance coefficient of the first annular draw bead 241 is 0.45-0.5, and the resistance coefficient of the second annular draw bead 242 is 0.35-0.45.
[0048] In the above embodiment, preferably, both the first annular draw bead 241 and the second annular draw bead 242 are semicircular draw bead; the arrangement interval between the first annular draw bead 241 and the second annular draw bead 242 is 20 mm-30 mm.
[0049] In the above embodiment, preferably, the material inflow of the two draw beads is controlled to be 30 mm-50 mm.
[0050] In the above embodiment, preferably, the upper mold 1 is detachably mounted on the slider of the press, and the lower mold 2 is detachably mounted on the workbench of the press. The upper mold 1 and the lower mold 2 can realize the stamping, film closing and mold opening operations by moving the slider of the press up and down. The detachable connections in this embodiment are all bolt connections, and the backing plate 11 and the mold body 21 in this embodiment are both provided with bolt holes for the bolts to pass through.
[0051] The method of using this embodiment is as follows:
[0052] 1) Cut the tested automotive galvanized steel sheet into test pieces of specified size and shape, wipe them clean, weigh them, and record their weight;
[0053] 2) Place the cut test piece into the lower die 2 and place it in the multiple positioning pins 28 of the blank holder 3;
[0054] 3) By adding or removing gaskets on the balancing block 27, the working gap between the die 12 and the blank holder 23 is adjusted to the thickness of the test piece; by adding or removing gaskets on the limiting block 26, the gap between the die 12 and the punch 22 is adjusted to the thickness of the test piece;
[0055] 4) According to the type of steel of the test piece, set the main cylinder pressure and blank holding force of the press, turn on the press, and use the force of the press to punch the test piece into a part;
[0056] 5) After stamping, wipe the parts clean and weigh them, and record their weight. According to the amount of coating shedding (test piece weight - part weight), evaluate the anti-shedding performance.
[0057] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may be subject to various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A mold for verifying the anti-peeling performance of the surface coating of automobile galvanized steel plates. It is characterized in that include: An upper die, the upper die comprising a backing plate and a concave die mounted on the lower surface of the backing plate and arranged downward; A lower die, the lower die comprising a die base body, a punch and a blank holder installed on the upper surface of the die base body, the blank holder is sleeved on the outer side of the punch, and two drawing ribs are arranged around the periphery of the punch and at the connection between the blank holder and the blank holder; Balancing blocks, a plurality of balancing blocks are arranged on the blank holding surface of the blank holding ring, and a plurality of balancing blocks are used to cover gaskets to adjust the gap between the die and the blank holding ring; Limit blocks, multiple limit blocks are arranged on the outside of the pressure ring and installed on the mold base body, and multiple limit blocks are used to cover gaskets to adjust the gap between the die and the punch.
2. The mold according to claim 1, It is characterized in that Guide sleeves are respectively installed at the four corners of the lower surface of the pad downward in the vertical direction, and a guide column is respectively provided on the upper surface of the mold base body corresponding to the position of the guide sleeve; When the upper mold and the lower mold are closed, a plurality of the guide posts are inserted into the corresponding guide sleeves.
3. The mold according to claim 1, It is characterized in that The edge of the die is chamfered to form a rounded corner of the die; The edge of the punch is chamfered to form a rounded corner of the punch that matches the rounded corner of the die.
4. The mold according to claim 1, It is characterized in that The die is annularly provided with rib grooves matching the two drawing ribs.
5. The mold according to claim 1, It is characterized in that A plurality of positioning pins are arranged around the material holding surface of the blank holding ring; The plurality of positioning pins are used to limit the position of the automotive galvanized steel sheet test piece placed on the lower die.
6. The mold according to claim 1, It is characterized in that The two draw beads include a first annular draw bead close to the punch and a second annular draw bead close to the blank holder; The resistance coefficient of the first annular drawbead is 0.45-0.5, and the resistance coefficient of the second annular drawbead is 0.35-0.
45.
7. The mold according to claim 6, It is characterized in that The first annular drawbead and the second annular drawbead are both semicircular drawbeads; The spacing between the first annular draw bead and the second annular draw bead is 20 mm-30 mm.
8. The mold according to claim 1, It is characterized in that The material inflow of the two draw beads is 30mm-50mm.
9. The mold according to claim 1, It is characterized in that The upper die is detachably mounted on a slide block of a press, and the lower die is detachably mounted on a workbench of the press.