Weld line strength testing device
By designing a weld line strength testing device and using an interference fit between the indenter and the hole of the weld line test sample, the problem of difficulty in evaluating weld line strength in injection molding is solved, fast and accurate testing is achieved, and the product quality is improved. mechanical properties and service life, and reduce costs.
Patent Information
- Application Number
- CN202420252909.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-01
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-02-01
AI Technical Summary
During the injection molding process, it is difficult to accurately evaluate the strength of the weld line in an interference assembly state. Existing methods rely on theoretical formulas or simulations and lack actual test data, leading to the risk of cracking in the product during use.
A welding line strength testing device is designed, including a base and an indenter. Through the interference fit between the indenter and the hole of the welding line test sample, the welding line strength test in various assembly states is realized, and the welding line strength test is carried out automatically. Centering and locking connections limit translational rigid body displacements to ensure test stability.
It achieves rapid and accurate assessment of weld line strength, optimizes structural design, improves the mechanical properties and service life of the product, and reduces development and production costs.
Smart Images

Figure CN221925913U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of injection molding, in particular to a weld line strength testing device. Background Art
[0002] The contents of this section merely provide background information related to the present invention and may not constitute prior art.
[0003] During the injection molding process of composite materials (especially fiber-filled composite materials), the molten plastic in the cavity will usually produce weld lines at the intersection of multiple streams due to the presence of holes, holes, inserts, cores and other obstacles, as well as multiple gates, different flow lengths or uneven wall thickness. The weld line is usually the weakest area of the injection molded product structure. Therefore, the evaluation of the strength reliability of the weld line is crucial to the reliability design of the product.
[0004] In some applications, in order to improve the mechanical properties and service life of injection molded products or other functional requirements, it is necessary to embed pre-molded parts in injection molded parts. There are inevitably weld lines around the holes of injection molded parts for press-fitting inserts, and there is a risk of cracking when the weld lines are press-fitted. At present, the weld line strength based on this working condition can only be evaluated by theoretical formula approximate calculation or simulation methods, but the actual weld line strength of injection molded products in the interference assembly state is not clear. Utility Model Content
[0005] One purpose of the utility model is to provide a weld line strength testing device, which can test the weld line strength of a weld line test sample under an assembly state of interference.
[0006] Another object of the present invention is to provide a weld line strength testing device, which can test the weld line strength of a weld line test sample under various interference assembly conditions.
[0007] Another object of the utility model is to provide a weld line strength testing device, which can automatically align the weld line test sample.
[0008] Another object of the present utility model is to provide a weld line strength testing device, which can limit the translational rigid body displacement of the weld line test sample.
[0009] The utility model provides a weld line strength testing device. The weld line strength testing device comprises: a base, the base having a receiving groove for receiving at least a part of a weld line test sample; and a pressure head, the pressure head is arranged above the base; wherein, when performing a weld line strength test, when the at least a part of the weld line test sample is placed in the receiving groove of the base, the pressure head can move toward the base under the action of pressure so that the lower end of the pressure head and the hole in the at least a part of the weld line test sample have an interference fit.
[0010] In some embodiments, the press head can be detachably connected to the pressure applying device.
[0011] In some embodiments, the lower end of the press head has a tapered shape.
[0012] In some embodiments, a protrusion protruding along the thickness direction of the base is provided at a substantially central position of the bottom of the receiving groove.
[0013] In some embodiments, the lower end of the pressure head has a tapered shape, and the protrusion is provided with a tapered groove at a central position.
[0014] In some embodiments, the bottom of the receiving groove is provided with one or more protrusions protruding along the thickness direction of the base, and the one or more protrusions are configured to form a shape-fitting locking connection with one or more grooves of the weld line test specimen.
[0015] In some embodiments, the weld line strength testing device further includes a cover plate, and the cover plate is detachably connectable to the base.
[0016] In some embodiments, a connector hole is provided at the upper end of the pressing head, so that the pressing head can be detachably connected to the pressure applying device through the connector.
[0017] In some embodiments, the pressure applying device is a universal tensile testing machine.
[0018] In some embodiments, base fastener holes for accommodating base fasteners are provided at both ends of the base, so that the base can be fixed by the base fasteners.
[0019] According to the weld line strength testing device disclosed in the present invention, by making the lower end of the pressure head produce an interference fit with the hole portion of the weld line test sample, it is possible to test the weld line strength of the weld line test sample under an assembly state with a certain amount of interference; by replacing the pressure head with a lower end portion having a different diameter or adopting a pressure head with a tapered lower end portion, so that the lower end portion of the pressure head and the hole portion of the weld line test sample produce an interference fit with different amounts of interference, it is possible to test the weld line strength of the weld line test sample under assembly states with a variety of amounts of interference; the bottom of the accommodating groove of the base is provided with a protrusion protruding in the thickness direction of the base at a substantially central position, so that the weld line test sample can be automatically centered; and the bottom of the accommodating groove is provided with one or more protrusions protruding in the thickness direction of the base, and these protrusions are configured to form a shape-fitting locking connection with one or more grooves of the weld line test sample, so that the translational rigid body displacement of the weld line test sample can be limited. In addition, by means of the weld line strength testing device according to the present disclosure, the weld line strength of the weld line test sample (such as glass fiber reinforced injection molded parts) can be quickly tested, so as to more accurately and effectively evaluate the reliability of the weld line strength, which is convenient for optimizing the structural design of glass fiber reinforced injection molded parts, improving mechanical properties, and thus increasing the service life of the product. Moreover, by adopting the weld line strength testing device of the utility model, the weld line failure analysis capability can be improved, the development cost can be reduced, and a more comprehensive, accurate, and efficient weld line failure solution can be provided to product manufacturers. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The following will describe the embodiments of the present invention by way of example only with reference to the accompanying drawings. In the accompanying drawings, the same features or components are represented by the same reference numerals, and the drawings are not necessarily drawn to scale. In the accompanying drawings:
[0021] Figure 1 A three-dimensional schematic diagram of a weld line strength testing device according to an embodiment of the present disclosure is shown;
[0022] Figure 2 A top view of a weld line strength testing device according to an embodiment of the present disclosure is shown;
[0023] Figure 3 shows a side view of a weld line strength testing device according to an embodiment of the present disclosure;
[0024] Figure 4 A perspective schematic diagram showing a base of a weld line strength testing device according to an embodiment of the present disclosure; and
[0025] Figure 5 A three-dimensional schematic diagram of a pressure head of a weld line strength testing device according to an embodiment of the present disclosure is shown. DETAILED DESCRIPTION
[0026] The following description is merely exemplary in nature and is not intended to limit the present invention, its application and use. It should be understood that in all of the accompanying drawings, similar reference numerals indicate the same or similar parts and features. The various drawings only schematically represent the concepts and principles of the embodiments of the present invention, and do not necessarily show the specific dimensions and proportions of the various embodiments of the present invention. Specific parts in specific drawings may be exaggerated to illustrate the relevant details or structures of the embodiments of the present invention.
[0027] In the description of the embodiments of the present invention, the directional terms related to "upper" and "lower" are used to describe the upper and lower positions of the views shown in the accompanying drawings. In practical applications, the positional relationship of "upper" and "lower" used in this article can be defined according to actual conditions, and these relationships can be reversed.
[0028] The following will be combined Figures 1 to 5 The weld line strength testing device 1 according to the embodiment of the present disclosure will be described in detail. Figure 1 A three-dimensional schematic diagram of a weld line strength testing device 1 according to an embodiment of the present disclosure is shown. Figure 2 A top view of a weld line strength testing device 1 according to an embodiment of the present disclosure is shown. Figure 3 A side view of a weld line strength testing device 1 according to an embodiment of the present disclosure is shown. Figure 4 A three-dimensional schematic diagram of a base 10 of a weld line strength testing device 1 according to an embodiment of the present disclosure is shown. Figure 5 A three-dimensional schematic diagram of a pressing head 20 of a weld line strength testing device 1 according to an embodiment of the present disclosure is shown.
[0029] The weld line strength testing device 1 of the present invention is used to perform weld line strength testing on a weld line testing sample 4. The weld line testing sample 4 refers to a sample or product to be tested having a weld line, such as a glass fiber reinforced injection molded part having a weld line.
[0030] like Figure 1 As shown, the weld line strength testing device 1 of the present invention comprises a base 10 and a pressure head 20. Figure 4 As shown, the base 10 has a receiving groove 11 for receiving at least a portion of the weld line test sample 4. In particular, the receiving groove 11 is at least used to receive the hole portion of the weld line test sample 4. Figure 1 and Figure 3As shown in FIG. 1 , the pressure head 20 is disposed above the base 10. When the weld line strength testing device 1 is used to test the weld line strength of the weld line test specimen 4, when at least a portion of the weld line test specimen 4 (at least the portion including the hole portion) is placed in the receiving groove 11 of the base 10, the pressure head 20 can move toward the base 10 under the action of pressure so that the lower end portion 21 (see FIG. 2 ) of the pressure head 20 is moved toward the base 10. Figure 5 ) generates an interference fit with the hole portion in at least a portion of the weld line test sample 4. In a state where the lower end portion of the pressure head 20 generates an interference fit with the hole portion of the weld line test sample 4, by observing whether the hole portion of the weld line test sample 4 is cracked, it is possible to test the weld line strength of the weld line test sample 4 in an assembly state with an interference amount.
[0031] It should be noted that, in this embodiment, both ends of the weld line test specimen 4 have the same structure, that is, the end of the weld line test specimen 4 inserted into the weld line strength test device 1 and the end of the weld line test specimen 4 not inserted into the weld line strength test device 1 have the same structure, such as Figure 1 and Figure 2 As shown, the end of the weld line test specimen 4 that is not inserted into the weld line strength testing device 1 has a hole portion 41 and one or more grooves 42, so the end of the weld line test specimen 4 that is inserted into the weld line strength testing device 1, that is, the at least a portion of the weld line test specimen 4 also has a hole portion and one or more grooves of the same structure. However, it is also conceivable that both ends of the weld line test specimen do not have the same structure, and only the end of the weld line test specimen that is inserted into the weld line strength testing device 1 has a hole portion and one or more grooves.
[0032] like Figure 1 As shown, the weld line strength testing device 1 may further include a cover plate 30, which can be detachably connected to the base 10. Figure 1 , Figure 3 and Figure 4As shown, the cover plate 30 is provided with a cover plate fastener hole (not shown), and correspondingly, the base 10 is provided with a fastener hole 14, and the cover plate 30 is detachably connected to the base 10 by passing the cover plate fastener 50 through the cover plate fastener hole of the cover plate 30 and the fastener hole 14 of the base 10. Preferably, the fastener hole 14 has an internal thread, and the cover plate fastener 50 has an external thread, such as a bolt or a screw, and the cover plate 30 is threadedly connected to the base 10 by passing the cover plate fastener hole of the cover plate 30 and screwing it into the fastener hole 14 of the base 10. By providing the cover plate 30, after placing at least a portion of the weld line test specimen 4 (at least the portion including the hole portion) in the receiving groove 11 of the base 10, the cover plate 30 can be connected to the base 10, thereby confining the weld line test specimen 4 in the receiving groove 11 of the base 10, thereby preventing the weld line test specimen 4 from escaping from the receiving groove 11 of the base 10 when performing the weld line strength test, thereby ensuring the stability of the weld line strength test.
[0033] Preferably, one or more of the base 10, the pressure head 20 and the cover plate 30 of the weld line strength testing device 1 can be made by a 3D printing (additive manufacturing) method, so that the size of these components is more accurate, and materials are saved, and the manufacturing cost is reduced. However, it is conceivable that these components of the weld line strength testing device 1 can be made by any other suitable method, such as by die casting, injection molding, stamping, etc.
[0034] Preferably, the pressure head 20 can be connected to a pressure applying device (not shown) in a detachable manner. The pressure applying device can be any device that can apply pressure to the pressure head 20, for example, it can be a universal tensile testing machine. The pressure head 20 can be connected to the pressure applying device in a detachable manner, so that the pressure head 20 can be easily assembled on the existing pressure applying device and can be easily removed from the existing pressure applying device. Moreover, the pressure head 20 can be easily replaced with another pressure head, the diameter of the lower end of the other pressure head is different from the diameter of the lower end of the pressure head 20, so that the lower ends of different pressure heads with different diameters can produce interference fits with different interference amounts with the hole portion of the weld line test sample 4. By observing the assembly state under which the hole portion of the weld line test sample 4 cracks, the weld line strength of the weld line test sample 4 can be determined. Therefore, the weld line strength testing device 1 of the present invention can test the weld line strength of the weld line test specimen 4 under various interference assembly conditions, and further provide data basis for the study of the weld line strength of specific weld line test specimens (such as glass fiber reinforced injection molding parts).
[0035] Preferably, if Figure 5As shown, the lower end 21 of the pressure head 20 has a tapered shape, so that when the pressure head 20 moves toward the base 10 under the action of pressure and contacts the hole of the weld line test sample 4, by controlling the downward movement of the pressure head 20, the periphery of the tapered lower end 21 with different diameters can produce interference fits with different interference amounts with the hole of the weld line test sample 4, and by observing the assembly state of the hole of the weld line test sample 4 under which the interference amount is cracked, the weld line strength of the weld line test sample 4 can be determined. Therefore, by using the pressure head 20 with a tapered lower end 21, it is not necessary to prepare multiple pressure heads with different diameters of the lower end, and only a single pressure head 20 with a tapered lower end 21 can achieve interference fits with multiple interference amounts, so that the weld line strength of the weld line test sample 4 can be tested under assembly states of multiple interference amounts. In addition, the tapered lower end 21 of the pressure head 20 is also conducive to the active centering of the weld line strength testing device 1. Specifically, after the weld line test piece 4 is mounted on the base 10, the base 10 with the weld line test piece 4 is roughly manually aligned with the pressure head 20, that is, the hole portion of the weld line test piece 4 is roughly aligned with the pressure head 20. Then, as the pressure head 20 is pressed down, the side surface of the tapered lower end portion 21 of the pressure head 20 interacts with the inner wall of the hole portion of the weld line test piece 4, so that the base 10 with the weld line test piece 4 moves slightly, and complete alignment is automatically achieved.
[0036] Preferably, if Figure 4As shown, a protrusion 12 protruding along the thickness direction of the base 10 is provided at a substantially central position of the bottom of the receiving groove 11 of the base 10 . After the pressure head 20 is connected to the pressure applying device, the pressure head 20 can be moved downward so that the lower end portion 21 of the pressure head 20 contacts the protrusion 12, and the position of the base 10 is adjusted so that the central axis of the lower end portion 21 of the pressure head 20 is aligned with the central axis of the protrusion 12. Then, the base 10 is fixed, and the pressure head 20 is moved upward, and at least a portion of the weld line test specimen 4 (at least including the hole portion) is placed in the accommodating groove 11 of the base 10, that is, the hole portion of the weld line test specimen 4 is directly sleeved on the outer periphery of the protrusion 12, so that the central axis of the hole portion of the weld line test specimen 4 is aligned with the central axis of the lower end portion 21 of the pressure head 20, so that the weld line test specimen 4 can be automatically aligned without manually adjusting the position of the weld line test specimen 4 and the pressure head 20, so that the lower end portion 21 of the pressure head 20 and the hole portion of the weld line test specimen 4 can be interference fit when aligned, so that the test of the weld line strength of the weld line test specimen 4 is more accurate. It should be noted that the height of the protrusion 12 is relatively low, and when the pressure head 20 moves toward the base 10 under the action of pressure so that the lower end 21 of the pressure head 20 and the hole of the weld line test sample 4 have an interference fit, the lower end 21 of the pressure head 20 does not contact the protrusion 12, thereby not interfering with the interference fit between the pressure head 20 and the weld line test sample 4. Since the weld line test sample 4 can be automatically centered, there is no need to repeat the positioning process of the weld line test sample 4, thereby improving the test efficiency and test accuracy.
[0037] Preferably, if Figure 4As shown, in the case where the lower end 21 of the press head 20 has a conical shape, the protrusion 12 is provided with a conical groove 121 at the central position. After the press head 20 is connected to the pressure applying device, the press head 20 can be moved downward so that the conical lower end 21 of the press head 20 contacts the conical groove 121 of the protrusion 12, and the position of the base 10 is adjusted so that the tip of the conical lower end 21 of the press head 20 is aligned with the bottom of the conical groove 121 of the protrusion 12, and then the base 10 is fixed, and the press head 20 is moved upward, and at least a portion of the weld line test specimen 4 (at least the portion including the hole portion) is placed in the receiving groove 11 of the base 10, that is, , the hole of the weld line test sample 4 is directly sleeved on the outer periphery of the protrusion 12, so that the central axis of the hole of the weld line test sample 4 is aligned with the tip of the tapered lower end 21 of the pressure head 20, so that the weld line test sample 4 can be automatically centered without manually adjusting the positions of the weld line test sample 4 and the pressure head 20, so that the lower end 21 of the pressure head 20 and the hole of the weld line test sample 4 can be interference fit when aligned, so that the test of the weld line strength of the weld line test sample 4 is more accurate. By providing the pressure head 20 with the tapered lower end 21 and the protrusion 12 with the tapered groove 121, the weld line test sample 4 can be automatically centered more accurately, thereby making the test of the weld line strength of the weld line test sample 4 more accurate.
[0038] Preferably, if Figure 4 As shown, the bottom of the receiving groove 11 is provided with one or more protrusions 13 protruding along the thickness direction of the base 10, and the one or more protrusions 13 are configured to form a shape-fitting locking connection with one or more grooves of the weld line test sample 4. The one or more protrusions 13 can have any suitable shape, such as a triangle, a circle, a rectangle, a rhombus or an irregular polygon, etc. Correspondingly, the one or more grooves have a shape corresponding to the shape of the one or more protrusions 13, so that the one or more protrusions 13 of the receiving groove 11 form a shape-fitting locking connection with the one or more grooves 42 of the weld line test sample 4, thereby limiting the translational rigid body displacement of the weld line test sample 4, and being able to stably position and lock the weld line test sample 4 in a suitable test position.
[0039] Preferably, if Figure 1 , Figure 3 and Figure 5 As shown, a connector hole 22 is provided at the upper end of the pressure head 20, so that the pressure head 20 can be detachably connected to the pressure applying device through a connector. The connector can be any commonly used connector, such as a pin, a bolt, etc.
[0040] Preferably, if Figure 1 and Figure 4As shown, both ends of the base 10 are stepped, that is, each end of the base 10 has a step portion 15, and the step portion 15 is provided with a base fastener hole 16 for accommodating a base fastener (not shown), so that the base 10 can be fixed by the base fastener. The base fastener can be any commonly used fastener, such as a bolt, a screw, a pin, a rivet, etc.
[0041] Preferably, when the pressure applying device is a universal tensile testing machine, the pressure head 20 is fixed to the upper clamping end of the universal tensile testing machine through a connecting piece, and the base 10 is fixed to the lower clamping end of the universal tensile testing machine through a base fastener. Since the weld line strength testing device of the utility model can be adapted to an existing pressure applying device, such as a universal tensile testing machine, and can be tested using an existing weld line test specimen, it is possible to test the weld line strength of the weld line test specimen without investing in additional testing equipment and additional mold costs, thereby reducing the testing cost.
[0042] In addition, according to the weld line strength testing device 1 of the present invention, by quickly testing the weld line strength of the weld line test sample (such as glass fiber reinforced injection molded parts), the reliability of the weld line strength is more accurately and effectively evaluated, which is convenient for optimizing the structural design of glass fiber reinforced injection molded parts, improving mechanical properties, and thus increasing the service life of the product. Moreover, by adopting the weld line strength testing device 1 of the present invention, the weld line failure analysis capability can be improved, the development cost can be reduced, and a more comprehensive, accurate, and efficient weld line failure solution can be provided to product manufacturers.
[0043] Here, an exemplary embodiment of the weld line strength testing device according to the utility model has been described in detail, but it should be understood that the utility model is not limited to the specific embodiments described and shown in detail above. Without departing from the main purpose and scope of the utility model, those skilled in the art can make various modifications and variations to the utility model. All these modifications and variations fall within the scope of the utility model. Moreover, all the components described herein can be replaced by other technically equivalent components.
Claims
1. A weld line strength testing device, characterized in that: The weld line strength testing device comprises: a base having a receiving groove for receiving at least a portion of the weld line test specimen; and A pressure head, the pressure head is arranged above the base; Wherein, when performing a weld line strength test, when at least a portion of the weld line test specimen is placed in the receiving groove of the base, the pressure head can move toward the base under the action of pressure so that the lower end of the pressure head and the hole portion in the at least a portion of the weld line test specimen produce an interference fit.
2. The weld line strength testing device according to claim 1, characterized in that: The pressure head can be detachably connected to the pressure applying device.
3. The weld line strength testing device according to claim 1, characterized in that: The lower end portion of the pressure head has a tapered shape.
4. The weld line strength testing device according to claim 1, characterized in that: A protrusion protruding in the thickness direction of the base is provided at a substantially central position of the bottom of the accommodating groove.
5. The weld line strength testing device according to claim 4, characterized in that: The lower end portion of the pressure head has a tapered shape, and the protrusion is provided with a tapered groove at a central position.
6. The weld line strength testing device according to any one of claims 1 to 5, characterized in that: The bottom of the receiving groove is provided with one or more protrusions protruding along the thickness direction of the base, and the one or more protrusions are configured to form a shape-fitting locking connection with one or more grooves of the weld line test specimen.
7. The weld line strength testing device according to any one of claims 1 to 5, characterized in that: The weld line strength testing device further includes a cover plate, which can be detachably connected to the base.
8. The weld line strength testing device according to any one of claims 1 to 5, characterized in that: The upper end portion of the pressure head is provided with a connector hole, so that the pressure head can be detachably connected to the pressure applying device through the connector.
9. The weld line strength testing device according to claim 8, characterized in that: The pressure applying device is a universal tensile testing machine.
10. The weld line strength testing device according to any one of claims 1 to 5, characterized in that: Both ends of the base are provided with base fastener holes for accommodating base fasteners, so that the base can be fixed by the base fasteners.